Circuit board, display device and manufacturing method of circuit board

CN119073018APending Publication Date: 2024-12-03BOE TECHNOLOGY GROUP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380008396.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-21
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

Among existing three-dimensional display technologies, IC packaging technology faces the challenge of high-channel-count driver chip packaging, which results in poor uniformity of chip-on-film (COF) plating and cannot meet the accuracy and product yield requirements of high-channel-count bonding processes.

Method used

An auxiliary pattern is set in the non-pattern area of ​​the circuit board, the pad and auxiliary pattern are formed through the electroplating process, and a protective layer is formed on the surface of the pad and a solder resist layer is formed in the non-pattern area to improve the uniformity of electroplating.

Benefits of technology

It effectively improves the uniformity of metal thickness at the pad, improves the yield of the circuit board during back-end bonding, and improves the plating uniformity of COF and the pattern uniformity of the bonding area.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119073018A_ABST
    Figure CN119073018A_ABST
Patent Text Reader

Abstract

The embodiment of the invention provides a circuit board, a display device and a manufacturing method of the circuit board. The manufacturing method of the circuit board comprises the following steps: providing a precursor substrate; a seed pattern and an auxiliary seed pattern are formed on one side of the precursor substrate, the seed pattern is located in the pattern area, the auxiliary seed pattern is located in the non-pattern area, and the seed pattern and the auxiliary seed pattern are spaced from each other; and through an electroplating process, a bonding pad is formed at the seed pattern, and an auxiliary pattern is formed at the auxiliary seed pattern.
Need to check novelty before this filing date? Find Prior Art

Description

Circuit board, display device, and method for manufacturing circuit board Technical Field

[0001] The present disclosure relates to the field of semiconductor technology, and in particular to a circuit board, a display device, and a method for manufacturing the circuit board. Background Art

[0002] Three-dimensional (3D) display technology is developing rapidly, with intelligent and portable electronics being the key trends. 3D display products require an increase in the number of data channels from 4k to 10k+, placing new demands on IC packaging technology. High-channel-count driver IC packaging technology, which supports more functions, is becoming a limiting factor in the future development of 3D display products. Therefore, the development of ultra-high-resolution chip-on-film (COF) packaging technology is needed to develop high-channel-count IC packaging technology. Due to the structural characteristics of COFs, the plating patterns in different bonding areas (e.g., the bonding area for display substrates (OLB Bonding), the bonding area for flexible circuit boards (FOF Bonding), and the bonding area for ICs (ILB Bonding)) vary. This leads to poor plating uniformity after thick Cu plating, which cannot meet the precision and product yield requirements of the subsequent COF bonding process.

[0003] Summary of the Invention

[0004] An embodiment of the present disclosure provides a method for manufacturing a circuit board having a plurality of pattern areas and a non-pattern area outside the pattern areas, wherein the manufacturing method includes:

[0005] providing a precursor substrate;

[0006] forming a seed pattern and an auxiliary seed pattern on one side of the precursor substrate, wherein the seed pattern is located in the pattern area, the auxiliary seed pattern is located in the non-pattern area, and the seed pattern and the auxiliary seed pattern are spaced apart from each other;

[0007] Through an electroplating process, a pad is formed at the seed pattern, and an auxiliary pattern is formed at the auxiliary seed pattern.

[0008] In a possible implementation, forming a seed pattern and an auxiliary seed pattern on one side of the precursor substrate includes:

[0009] forming a plurality of seed patterns in the pattern area of ​​the precursor substrate;

[0010] forming an auxiliary film having an auxiliary seed pattern and a hollow area, wherein the auxiliary seed pattern comprises: a first flexible substrate, and a first auxiliary seed film layer located on one side of the first flexible substrate;

[0011] The side of the auxiliary film having the first flexible base is laminated to the side of the precursor substrate having the seed pattern, wherein the pattern area of ​​the precursor substrate is laminated to the hollow area of ​​the auxiliary film.

[0012] In a possible implementation, forming the auxiliary film having the auxiliary seed pattern and the hollow area includes:

[0013] providing a rigid substrate;

[0014] forming a first flexible substrate and a first auxiliary seed film layer in sequence on one side of the rigid substrate;

[0015] cutting the first flexible substrate and the first auxiliary seed film layer to remove the area outside the auxiliary seed pattern to form the hollow area;

[0016] The rigid substrate is removed.

[0017] In a possible implementation, laminating the side of the auxiliary film having the first flexible base to the side of the precursor substrate having the seed pattern includes:

[0018] The side of the auxiliary film having the first flexible base is bonded to the side of the precursor substrate having the seed pattern by rolling.

[0019] In a possible implementation, after forming a pad at the seed pattern and forming an auxiliary pattern at the auxiliary seed pattern through an electroplating process, the manufacturing method further includes:

[0020] Remove the auxiliary film.

[0021] In a possible implementation manner, after removing the auxiliary film, the manufacturing method further includes:

[0022] forming a protective layer on the surface of the pad;

[0023] A solder resist layer is formed in the non-pattern area.

[0024] In a possible implementation, forming a seed pattern and an auxiliary seed pattern on one side of the precursor substrate includes:

[0025] forming a second seed film layer on the precursor substrate through a sputtering process;

[0026] By performing a patterning process on the second seed film layer, a plurality of seed patterns are formed in the pattern area, and at the same time, the auxiliary seed pattern is formed in the non-pattern area, wherein a gap exists between the auxiliary seed pattern and the seed pattern.

[0027] In a possible implementation, after forming a pad at the seed pattern and forming an auxiliary pattern at the auxiliary seed pattern through an electroplating process, the manufacturing method further includes:

[0028] forming a protective layer on the surfaces of the pad and the auxiliary pattern;

[0029] A solder resist layer is formed in the area where the auxiliary pattern is located.

[0030] In one possible implementation, providing a precursor substrate includes:

[0031] providing a substrate;

[0032] forming a plurality of leads on one side of the base substrate;

[0033] A planar layer is formed on a side of the lead facing away from the base substrate, wherein the planar layer has a via hole exposing a portion of the lead.

[0034] The present disclosure also provides a circuit board, comprising:

[0035] A base substrate having a pattern area and a non-pattern area outside the pattern area;

[0036] A plurality of pads are located on one side of the base substrate and in the pattern area;

[0037] An auxiliary pattern is located on the same side of the base substrate as the pad, and the auxiliary pattern is located in the non-pattern area.

[0038] In a possible implementation manner, there is a gap between the auxiliary pattern and the pad.

[0039] In a possible implementation manner, the auxiliary pattern and the pad are made of the same layer and material.

[0040] In a possible implementation manner, a surface of the auxiliary pattern facing away from the base substrate and a surface of the pad facing away from the base substrate are located in the same plane.

[0041] In a possible implementation manner, the circuit board further includes:

[0042] a plurality of leads located between the substrate and the pad;

[0043] a flat layer, located between the leads and the pads, and having vias exposing portions of the leads, wherein the leads are electrically connected to the pads in a one-to-one correspondence through the vias;

[0044] a protective layer, located on a side of the pad facing away from the planar layer and covering the pad and the auxiliary pattern;

[0045] The solder resist layer is located on a side of the auxiliary pattern away from the planar layer and covers the auxiliary pattern.

[0046] The present disclosure also provides a display device, comprising: a display panel, a flexible circuit board, a control chip, and the circuit board obtained by the manufacturing method provided by the embodiment of the present disclosure, or comprising the circuit board provided by the embodiment of the present disclosure; wherein the multiple pattern areas of the circuit board include: a first pattern area, a second pattern area, and a third pattern area;

[0047] The display panel includes a plurality of first pins, and the first pins of the display panel are bound to the pads of the first pattern area in a one-to-one correspondence;

[0048] The flexible circuit board includes a plurality of second pins, and the second pins of the flexible circuit board are bound to the pads of the second pattern area in a one-to-one correspondence;

[0049] The control chip has a plurality of third pins, and the third pins of the control chip are bound to the pads of the third pattern area in a one-to-one correspondence. BRIEF DESCRIPTION OF THE DRAWINGS

[0050] Figure 1 is a schematic diagram of the distribution of electric force lines of an electroplated sample;

[0051] FIG2 is a second schematic diagram of the distribution of electric force lines of an electroplated sample;

[0052] FIG3 is a schematic diagram of a manufacturing process of a circuit board provided in an embodiment of the present disclosure;

[0053] FIG4A is a schematic diagram of a precursor substrate for forming leads according to an embodiment of the present disclosure;

[0054] FIG4B is a schematic top view of forming leads according to an embodiment of the present disclosure;

[0055] FIG4C is a schematic diagram of a precursor substrate for forming a flat layer according to an embodiment of the present disclosure;

[0056] FIG4D is a schematic diagram of a precursor substrate for forming an insulating layer according to an embodiment of the present disclosure;

[0057] FIG4E is a schematic diagram of a precursor substrate for forming a seed pattern according to an embodiment of the present disclosure;

[0058] FIG5A is a top view of a first alignment mark when forming an auxiliary film according to an embodiment of the present disclosure;

[0059] FIG5B is a cross-sectional view of a first alignment mark when forming an auxiliary film according to an embodiment of the present disclosure;

[0060] FIG5C is a schematic diagram of the first seed film layer when forming an auxiliary film according to an embodiment of the present disclosure;

[0061] FIG5D is a schematic diagram of removing the periphery of the first alignment mark when forming an auxiliary film according to an embodiment of the present disclosure;

[0062] FIG5E is a schematic diagram of the auxiliary film after the periphery of the first alignment mark is removed when forming the auxiliary film according to an embodiment of the present disclosure;

[0063] FIG5F is a schematic diagram of a motherboard including multiple COFs provided by an embodiment of the present disclosure;

[0064] FIG5G is a schematic diagram of a hollow area formed on an auxiliary film according to an embodiment of the present disclosure;

[0065] FIG5H is a schematic diagram of peeling the auxiliary film from the rigid substrate according to an embodiment of the present disclosure;

[0066] FIG5I is a schematic diagram of an auxiliary film obtained according to an embodiment of the present disclosure;

[0067] FIG5J is a top view of an auxiliary film corresponding to a single COF obtained in an embodiment of the present disclosure;

[0068] FIG5K is a schematic cross-sectional view of an auxiliary film corresponding to a single COF obtained in an embodiment of the present disclosure;

[0069] FIG6A is a top view schematically illustrating laminating an auxiliary film to a precursor substrate having a seed pattern formed thereon, according to an embodiment of the present disclosure;

[0070] FIG6B is a cross-sectional view of laminating an auxiliary film to a precursor substrate having a seed pattern formed thereon, according to an embodiment of the present disclosure;

[0071] FIG7 is a schematic cross-sectional view of a plated pad according to an embodiment of the present disclosure;

[0072] FIG8 is a schematic cross-sectional view of a chip-on-film after the auxiliary film is removed according to an embodiment of the present disclosure;

[0073] FIG9 is a schematic cross-sectional view of a COF formed with a protective layer and a solder resist layer according to an embodiment of the present disclosure;

[0074] FIG10 is a cross-sectional schematic diagram of simultaneously forming a seed pattern and an auxiliary seed pattern according to an embodiment of the present disclosure;

[0075] FIG11 is a second cross-sectional schematic diagram of a chip-on-film (COF) having a protective layer and a solder mask layer formed thereon according to an embodiment of the present disclosure;

[0076] FIG12 is a schematic diagram of a display device provided by an embodiment of the present disclosure;

[0077] FIG13 is a schematic diagram of the connection between the pad and the lead provided by an embodiment of the present disclosure;

[0078] FIG. 14 is a diagram showing a comparison of uniformity between a device with and without auxiliary patterns provided in an embodiment of the present disclosure. DETAILED DESCRIPTION

[0079] In order to make the purpose, technical solutions and advantages of the embodiments of the present disclosure more clear, the technical solutions of the embodiments of the present disclosure will be clearly and completely described below in conjunction with the drawings of the embodiments of the present disclosure. Obviously, the described embodiments are part of the embodiments of the present disclosure, not all of the embodiments. Based on the described embodiments of the present disclosure, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present disclosure.

[0080] Unless otherwise defined, the technical or scientific terms used in this disclosure should have the usual meanings understood by persons of ordinary skill in the field to which this disclosure belongs. The words "first", "second" and similar terms used in this disclosure do not indicate any order, quantity or importance, but are only used to distinguish different components. Words such as "include" or "comprise" mean that the elements or objects appearing before the word include the elements or objects listed after the word and their equivalents, without excluding other elements or objects. Words such as "connect" or "connected" are not limited to physical or mechanical connections, but may include electrical connections, whether direct or indirect. "Up", "down", "left", "right" and the like are only used to indicate relative positional relationships. When the absolute position of the object being described changes, the relative positional relationship may also change accordingly.

[0081] As used herein, "about" or "approximately the same" is inclusive of the stated value and means within an acceptable range of deviation for the particular value as determined by one of ordinary skill in the art taking into account the measurement in question and the errors associated with the measurement of the particular quantity (i.e., the limitations of the measurement system). For example, "approximately the same" can mean that the difference relative to the stated value is within one or more standard deviations, or within ±30%, 20%, 10%, 5%.

[0082] In the accompanying drawings, the thickness of layers, films, panels, regions, etc. are exaggerated for clarity. Exemplary embodiments are described herein with reference to cross-sectional views that are schematic representations of idealized embodiments. As such, deviations from the shapes of the figures are to be expected as a result of, for example, manufacturing techniques and / or tolerances. Thus, the embodiments described herein should not be construed as limited to the specific shapes of the regions as shown herein, but rather include deviations in shape that result from, for example, manufacturing. For example, a region illustrated or described as flat may typically have rough and / or nonlinear features. Furthermore, sharp corners illustrated may be rounded. Thus, the regions illustrated in the figures are schematic in nature, and their shapes are not intended to illustrate the precise shape of the regions and are not intended to limit the scope of the claims.

[0083] In order to keep the following description of the embodiments of the present disclosure clear and concise, the present disclosure omits detailed descriptions of known functions and known components.

[0084] When the entire plate is electroplated, the schematic diagram of the electric force line distribution of the electroplated sample is shown in Figure 1. The electric force lines are evenly distributed from the anode to the cathode, and the thickness of the electroplated position is relatively uniform. When the patterned sample is electroplated with Cu, the schematic diagram of the electroplating force line distribution is shown in Figure 2. The electric force lines in some areas of the cathode are too concentrated, and burrs and other problems occur during the electroplating process, resulting in poor electroplating uniformity.

[0085] As shown in FIG3 , an embodiment of the present disclosure provides a method for manufacturing a circuit board, wherein the circuit board has multiple pattern areas and non-pattern areas outside the pattern areas. Specifically, in the embodiment of the present disclosure, the circuit board can be a chip on film (COF), having a bonding area (OLB Bonding) for bonding a display substrate, a bonding area (FOF Bonding) for bonding a flexible circuit board, and a bonding area (ILB Bonding) for bonding an IC; the patterns of different bonding areas can be different. Specifically, the manufacturing method provided in the embodiment of the present disclosure can also be applied to other circuit boards formed using an electroplating process. The manufacturing method provided in the embodiment of the present disclosure includes:

[0086] Step S100: providing a precursor substrate;

[0087] Specifically, step S100 of providing a precursor substrate may include:

[0088] Step S111 , providing a base substrate 11 ; specifically, the material of the base substrate 11 may be a rigid substrate, specifically, a glass substrate, and the base substrate 11 may be removed after the circuit board is finally formed.

[0089] Specifically, as shown in FIG4A , a flexible film 12 (which may be polyimide, PI) may be coated or laminated on one side of the base substrate 11, with a thickness of 10 μm to 40 μm. A water-resistant inorganic film SiO2 or SiN may be deposited on the flexible film 12 as a water-blocking layer 13, with a thickness of 100 nm to 500 nm. Specifically, the flexible film 12 may be a single layer or a composite laminate structure. When the flexible film 12 is a single layer, the material of the flexible film 12 may be polyimide (PI), polyethylene naphthalate, or polyethylene terephthalate. When the flexible film 12 is a composite laminate structure, it may include a first organic layer, a barrier layer, and a second organic layer stacked in sequence. The first organic layer may be made of polyimide, polyethylene naphthalate, or polyethylene terephthalate, and the second organic layer may be made of polyimide, polyethylene naphthalate, or polyethylene terephthalate.

[0090] Step S112, forming a plurality of leads 14 on one side of the base substrate 11, specifically, forming a plurality of leads 14 on the side of the water-blocking layer 13 away from the flexible film 12; specifically, forming a plurality of leads 14 may include: first depositing a layer of metal film, the metal film may be Mo, Al, or Ti / Al / Ti laminated metal, for example, Ti / Al / Ti metal, the thickness may be 500nm to 1000nm, and patterning, to achieve a smaller size (pitch), the etching process may be dry etching. The cross-sectional view is shown in Figure 4A, the schematic diagram of the lead 14 of the binding pad 3 may be shown in Figure 4B, and the top view schematic diagram of the lead 14 and the subsequently formed pad 3 may be shown in Figure 13; limited by the accuracy of the binding equipment, the size of the binding pad 3 needs to be greater than 20μm, so the line width of the lead 14 in the densest wiring area between the pads 3 needs to be (pitch) <4μm;

[0091] Step S113: Form a planar layer 16 on the side of the lead 14 facing away from the base substrate 11, as shown in FIG4C . The planar layer 16 includes a via K that exposes a portion of the lead 14. Specifically, an organic insulating layer is applied to the side of the lead 14 facing away from the base substrate 11 as the planar layer 16. A resin material of 2 μm to 5 μm thickness can be used. A transfer via K is provided at the location of the pad 3. One or more transfer vias K can be provided on the pad 3; the schematic diagram shows one as an example.

[0092] Specifically, an inorganic insulating layer SiN or SiO stack may be deposited on the side of the flat layer 16 away from the lead 14 as the insulating layer 17 , as shown in FIG4D , with a thickness of 100 nm to 500 nm, and a transfer hole may be provided at the pad 3 .

[0093] Specifically, as shown in FIG4D , the formed precursor substrate may include a base substrate 11, leads 14 located on one side of the base substrate 11, and a planar layer 16 located on a side of the leads 14 facing away from the base substrate 11. Specifically, a flexible film 12 may be provided between the base substrate 11 and the leads 14, a water-blocking layer 13 may be provided between the flexible film 12 and the leads 14, and an insulating layer 17 may be provided on the side of the planar layer 16 facing away from the leads 14.

[0094] Step S200: forming a seed pattern and an auxiliary seed pattern on one side of a precursor substrate, wherein the seed pattern is located in a pattern area, the auxiliary seed pattern is located in a non-pattern area, and the seed pattern and the auxiliary seed pattern are spaced apart from each other. Specifically, as shown in FIG6B , the seed pattern 21 and the auxiliary seed pattern 60 may be spaced apart by a first flexible substrate T1; or, as shown in FIG11 , the seed pattern 21 and the auxiliary seed pattern 60 may be spaced apart by a gap;

[0095] Specifically, regarding step S200, a seed pattern and an auxiliary seed pattern are formed on one side of the precursor substrate. The seed pattern and the auxiliary seed pattern may be formed in a variety of ways. In one possible embodiment, the following methods may be used:

[0096] Step S211: forming a plurality of seed patterns 21 in the pattern area of ​​the precursor substrate, as shown in FIG4E . Specifically, the seed patterns 21 may be formed at the via holes K of the precursor substrate after the precursor substrate is formed.

[0097] Step S212: forming an auxiliary film having an auxiliary seed pattern and a hollow area, wherein the auxiliary seed pattern includes: a first flexible substrate, and a first auxiliary seed film layer located on one side of the first flexible substrate; specifically, step S212: forming the auxiliary film having the auxiliary seed pattern and the hollow area may include:

[0098] Step a, providing a rigid substrate; specifically, the rigid substrate can be a glass substrate, specifically, referring to FIG5A and FIG5B, a first alignment mark M1 can be made on the rigid substrate G, specifically, a sputtering device can be used to first deposit a layer of a thickness of (Specifically, for example, ) of the metal Mo, and then use a photolithography device to perform a photoresist coating process, and then use a dry etching process to retain only the first alignment mark M1 around it. The specific plan schematic diagram and cross-sectional schematic diagram are shown in Figures 5A and 5B below;

[0099] Step b, as shown in FIG5C, a first flexible substrate T1 and a first auxiliary seed film layer T2 are sequentially formed on one side of the rigid substrate G; specifically, a laminator device can be used to accurately and completely attach the entire TPF film (as the first flexible substrate T1) to the rigid substrate G marked with the first alignment mark M1, and a layer of a thickness of 1000 nm can be deposited on the TPF film (first flexible substrate T1) using a Sputter device. Cu (as the first auxiliary seed film layer T2), as shown in FIG5C;

[0100] Step c: cutting the first flexible substrate T1 and the first auxiliary seed film layer T2 to remove the area outside the auxiliary seed pattern to form a hollow area;

[0101] Specifically, first, laser cutting can be used to accurately align the inner side of the first alignment mark M1 and cut the TPF film (first flexible substrate T1) outside the inner side of the first alignment mark M1. 5D ; laser cutting and peeling of a portion of the TPF film (first flexible substrate T1) and the first auxiliary seed film layer T2 is performed, as shown in FIG5E ; secondly, based on the second alignment mark (not shown) of the motherboard having multiple precursor substrates and the third alignment mark (not shown) in a single precursor substrate (e.g., COF) and the distance between the ILB, OLB, and FOF in a single COF and the fourth alignment mark (not shown) (wherein a schematic diagram of the distribution of the precursor substrates on the entire motherboard is shown in FIG5F ), the TPF film (first flexible substrate T1) and the first auxiliary seed film layer T2 are precisely cut to form a hollow area L (the hollow area L may specifically include a first hollow area L1 corresponding to the OLB binding area on the precursor substrate in FIG5F , a second hollow area L2 corresponding to the ILB binding area, and a third hollow area L3 corresponding to the FOF binding area). The remaining pattern serves as the auxiliary seed pattern 60. The upper substrate after laser cutting is shown in FIG5G ;

[0102] Step d: Remove the rigid substrate. Specifically, remove the TPF film (first flexible substrate T1) and the first auxiliary seed film layer T2 from the rigid substrate G, as shown in Figure 5H below. The resulting auxiliary film is shown in Figure 5I. The single COF is shown in Figure 5J, and its cross-sectional view at the arrow is shown in Figure 5K.

[0103] Step S213, the side of the auxiliary film having the first flexible substrate T1 is laminated to the side of the precursor substrate having the seed pattern 21, as shown in FIG6B , wherein the pattern area of ​​the precursor substrate (for example, OLB, ILB or FOF in FIG6A ) is laminated to the hollow area L of the auxiliary film. Specifically, the side of the auxiliary film having the first flexible substrate can be laminated to the side of the precursor substrate having the seed pattern by rolling with a roller. Specifically, the precursor substrate 1 formed with the seed pattern 21 and the auxiliary film 22 are precisely and tightly laminated by rolling with two laminating rollers, as shown in FIG6A . A cross-sectional view of the precursor substrate after adding the auxiliary seed pattern 60 is shown in FIG6B .

[0104] Step S300 : forming a pad 3 at the seed pattern 21 and forming an auxiliary pattern 6 at the auxiliary seed pattern 60 through an electroplating process, as shown in FIG. 7 .

[0105] Specifically, after step S300 , that is, after forming the pad 3 at the seed pattern 21 and the auxiliary pattern 6 at the auxiliary seed pattern 60 through the electroplating process, the manufacturing method further includes: removing the auxiliary film 22 , as shown in FIG. 8 .

[0106] Specifically, after removing the auxiliary film, the manufacturing method further includes:

[0107] A protective layer 4 is formed on the surface of the pad 3, as shown in FIG9 . Specifically, a tinning treatment is performed to form the protective layer 4 to prevent the pad 3 from being oxidized.

[0108] A solder resist layer 5 is formed in the non-patterned area, as shown in FIG9 . Specifically, a solder resist layer 5 (e.g., green oil) is applied to the non-patterned area (e.g., non-ILB, OLB, FOF area) to a thickness of 10 μm to 20 μm. In an embodiment of the present invention, the auxiliary pattern 6 may not be retained in the final COF.

[0109] In another possible implementation, regarding step S200, forming a seed pattern and an auxiliary seed pattern on one side of the precursor substrate includes:

[0110] Step S221: Form a second seed film layer 61 on the precursor substrate by sputtering, as shown in FIG10 ; Specifically, a sputtering device is used to deposit a Cu seed layer on the precursor substrate with a thickness of (For example, it can be Specifically, in the embodiment of the present invention, the process of forming the precursor substrate is the same as the process of forming the precursor substrate described above, and will not be repeated here.

[0111] Step S222: Patterning the second seed film layer 61 to form a plurality of seed patterns 21 in the pattern area and forming auxiliary seed patterns 60 in the non-pattern area, wherein a gap exists between the auxiliary seed patterns 60 and the seed patterns 21. Specifically, the patterning process can be performed using a photolithography process, as shown in FIG10 ;

[0112] Specifically, after forming a pad at the seed pattern and forming an auxiliary pattern at the auxiliary seed pattern through an electroplating process, the manufacturing method further includes:

[0113] A protective layer 4 is formed on the surface of the pad 3 and the auxiliary pattern 6; as shown in FIG11 , specifically, a tin treatment is performed to form the protective layer 4 to achieve an anti-oxidation effect on the pad 3; the material of the protective layer 4 can be tin (Sn) metal, etc. In some embodiments, the protective layer 4 can be formed by a chemical plating process, and the thickness of the protective layer 4 is greater than or equal to 0.5 μm and less than or equal to 2 μm, for example, 0.5 μm, 1 μm, 1.5 μm, 2 μm, etc.; in addition, the surface of the pad 3 can also be covered with indium tin oxide (ITO) to prevent the pad 3 from being oxidized.

[0114] A solder resist layer 5 is formed in the area where the auxiliary pattern 6 is located. The solder resist layer 5 is formed on the auxiliary pattern 6, as shown in FIG11. Specifically, a solder resist layer 5 (for example, green oil) is applied to the non-pattern area (for example, non-ILB, OLB, FOF area). The thickness of the solder resist layer 5 can be greater than or equal to 10 μm and less than or equal to 20 μm. Optionally, the thickness of the solder resist layer 5 is 10 μm, 15 μm, 20 μm, etc. Specifically, in the embodiment of the present invention, the auxiliary pattern 6 can be left on the final COF.

[0115] In the embodiment of the present disclosure, the electroplating uniformity of the case without and with the auxiliary pattern is shown in FIG14 , from which it can be concluded that:

[0116] 1. Adding auxiliary patterns can effectively improve the plating uniformity of a motherboard containing multiple COFs (uniformity here can be understood as the uniformity between the same patterns. The lower the uniformity, the smaller the thickness difference between the same patterns, which better meets the requirements of the back-end bonding process). Compared with the 40% plating uniformity of a motherboard containing multiple COFs without auxiliary patterns, the addition of auxiliary patterns in the embodiment of the present disclosure can reduce the plating uniformity of the entire motherboard to 4%;

[0117] 2. Adding auxiliary patterns can also improve the pattern uniformity of the COF in the bonding area. Compared with the 23% electroplating uniformity of the bonding area without auxiliary patterns, the addition of auxiliary patterns in the embodiment of the present disclosure can reduce the electroplating uniformity of the entire motherboard to 17%, which is a good improvement in electroplating uniformity.

[0118] It should be noted that in the embodiment of the present disclosure, the electroplating uniformity is divided into the electroplating uniformity of the motherboard containing multiple COFs and the uniformity of the binding area (for example, the ILB binding point); the uniformity of the entire motherboard is to test the electroplating thickness of Cu at the fixed position of each single COF on the motherboard, and calculate the uniformity of the electroplated Cu; and the electroplating uniformity at the ILB is to select the electroplated Cu thickness at different positions of the ILB binding point in a single COF, and calculate the ILB electroplating Cu uniformity.

[0119] The disclosed embodiments can replace existing COF product structures and solutions. Existing COF structures utilize additive electroplating, with a flat layer (resin) acting as a barrier. As the thickness of the plated Cu increases, the uniformity of the Cu thickness decreases. Existing COF pads suffer from poor Cu thickness uniformity, which results in varying resistance across pads and reduces bonding yield, impacting device performance.

[0120] The circuit board manufacturing method provided in the embodiment of the present disclosure can be applied to the manufacturing process of high-resolution COF device structures in the display field, as well as the patterned electroplating thick Cu technology in mini light-emitting diode (Mini-LED) and micro light-emitting diode (Micro-LED) technologies.

[0121] The beneficial effects of the embodiments of the present disclosure are as follows: by setting an auxiliary pattern in the non-pattern area of ​​the circuit board, the uniformity of the distribution of the electric field lines is improved when thick metal (for example, thick Cu greater than 8 μm) is electroplated on the pad, thereby improving and enhancing the thickness uniformity of the metal at the pad, and improving the yield of the circuit board during the later binding.

[0122] Based on the same inventive concept, an embodiment of the present invention further provides a circuit board, comprising:

[0123] A base substrate 11, the base substrate 11 having a pattern area and a non-pattern area outside the pattern area;

[0124] A plurality of pads 3 are located on one side of the base substrate 11 and in the pattern area;

[0125] The auxiliary pattern 6 is located on the same side of the base substrate 11 as the pad 3 and is located in the non-pattern area. Specifically, the auxiliary pattern 6 can be a whole pattern surrounding the pattern area.

[0126] In a possible embodiment, as shown in FIG11 , there is a gap between the auxiliary pattern 6 and the pad 3 to prevent the auxiliary pattern 6 from causing other unnecessary adverse effects on the COF circuit board.

[0127] In a possible implementation, as shown in Figure 11 , the auxiliary pattern 6 and the pad 3 are made of the same layer and material. Specifically, the auxiliary pattern 6 and the pad 3 may be made of copper.

[0128] In a possible implementation, as shown in FIG. 11 , the surface of the auxiliary pattern 6 facing away from the base substrate 11 and the surface of the pad 3 facing away from the base substrate 11 are located in the same plane.

[0129] In a possible implementation, as shown in FIG11 , the circuit board further includes:

[0130] A plurality of leads 14 are located between the substrate 1 and the pads 3;

[0131] The flat layer 16 is located between the leads 14 and the pads 3 and has vias exposing portions of the leads 14 . The leads 14 are electrically connected to the pads 3 in a one-to-one correspondence through the vias.

[0132] The protective layer 4 is located on the side of the pad 3 facing away from the planar layer 16 and covers the pad 3 and the auxiliary pattern 6;

[0133] The solder resist layer 5 is located on a side of the auxiliary pattern 6 facing away from the planar layer 16 and covers the auxiliary pattern 6 .

[0134] Based on the same inventive concept, an embodiment of the present invention further provides a display device, as shown in FIG12 , comprising: a display panel 002, a flexible circuit board FPC, a control chip IC, and a circuit board 001 obtained by the manufacturing method provided by an embodiment of the present disclosure, or comprising the circuit board 001 provided by an embodiment of the present disclosure; wherein the multiple pattern areas of the circuit board 001 include: a first pattern area OLB, a second pattern area FOF, and a third pattern area ILB;

[0135] The display panel includes a plurality of first pins, and the first pins of the display panel are bound to the pads of the first pattern area OLB in a one-to-one correspondence;

[0136] The flexible circuit board includes a plurality of second pins, and the second pins of the circuit board are bound to the pads of the second pattern area FOF in a one-to-one correspondence;

[0137] The control chip has a plurality of third pins, and the third pins of the control chip are bound to the pads of the third pattern area ILB in a one-to-one correspondence.

[0138] The beneficial effects of the embodiments of the present disclosure are as follows: The beneficial effects of the embodiments of the present disclosure are as follows: By setting an auxiliary pattern in the non-pattern area of ​​the circuit board, the uniformity of the distribution of the electric field lines is improved when thick metal (for example, thick Cu greater than 8μm) is electroplated at the pad, thereby improving and enhancing the thickness uniformity of the metal at the pad, and improving the yield of the circuit board during the later binding.

[0139] In some embodiments, the display device provided by the embodiments of the present disclosure may be a liquid crystal display device, which includes a backlight module and a liquid crystal display panel located on the light-emitting side of the backlight module. The liquid crystal display panel may be a twisted nematic (TN) liquid crystal display panel, an advanced dimension switch (ADS) liquid crystal display panel, a high-aperture ratio advanced dimension switch (HADS) liquid crystal display panel, an in-plane switch (IPS) liquid crystal display panel, or the like.

[0140] In some embodiments, the display device provided by the embodiments of the present disclosure may be a 3D display device. In this case, the display device may further include a liquid crystal grating located between the backlight module and the liquid crystal display panel, and the liquid crystal grating may be fixed to the liquid crystal display panel via an adhesive layer. Optionally, based on the current position of the viewer's eyes, the liquid crystal grating may be controlled to form alternating light-transmitting areas and light-blocking areas, so that the viewer's left eye sees the left-eye image displayed on the display panel through the light-transmitting areas of the liquid crystal grating, and the right eye sees the right-eye image displayed on the display panel through the light-transmitting areas. By arranging the liquid crystal grating on the light-incident side of the liquid crystal display panel, when the liquid crystal display panel includes touch electrodes, the liquid crystal grating will not shield the touch electrodes in the liquid crystal display panel, thereby avoiding the problem of touch failure, thereby improving the touch sensitivity and accuracy of the liquid crystal display panel.

[0141] In some embodiments, the display panel in the above-mentioned display device provided by the embodiment of the present disclosure may also be an electroluminescent display panel (Organic Light Emitting Diodes, OLED) or a quantum dot display panel (Quantum Dot Light Emitting Diodes, QLED), which is not limited here. The OLED display panel or QLED display panel includes a light-emitting device and a pixel driving circuit electrically connected to the light-emitting device; wherein the light-emitting device may include a cathode and an anode opposite to each other, and a light-emitting functional layer between the cathode and the anode; the pixel driving circuit may include a thin film transistor, a storage capacitor, etc., and may be implemented in various different types, such as a 2TIC type (i.e., including two thin film transistors and a storage capacitor), and may further include more transistors and / or capacitors on the basis of the 2T1C type to have functions such as compensation, reset, light-emitting control, and detection. The embodiment of the present disclosure does not limit the pixel driving circuit. For example, in some embodiments, the thin film transistor directly electrically connected to the light-emitting element may be a driving transistor (Td) or a light-emitting control transistor (EM), etc.

[0142] In some embodiments, the above-mentioned display device provided by the embodiment of the present disclosure may be any product or component with a display function, such as a mobile phone, a tablet computer, a television, a monitor, a laptop computer, a digital photo frame, a navigator, a smart watch, a fitness wristband, a personal digital assistant, etc. Optionally, the above-mentioned display device provided by the embodiment of the present disclosure includes but is not limited to components such as a radio frequency unit, a network module, an audio output & input unit, a sensor, a display unit, a user input unit, an interface unit, and a control chip. Optionally, the control chip is a central processing unit, a digital signal processor, a system-on-chip (SoC), etc. For example, the control chip may also include a memory, a power module, etc., and realize power supply and signal input and output functions through additionally provided wires, signal lines, etc. For example, the control chip may also include hardware circuits and computer executable codes, etc. The hardware circuit may include conventional very large scale integration (VLSI) circuits or gate arrays and existing semiconductors or other discrete components such as logic chips and transistors; the hardware circuit may also include field programmable gate arrays, programmable array logic, programmable logic devices, etc. In addition, those skilled in the art will understand that the above structure does not constitute a limitation on the above display device provided in the embodiment of the present disclosure. In other words, the above display device provided in the embodiment of the present disclosure may include more or fewer of the above components, or a combination of certain components, or different component arrangements.

[0143] Although the preferred embodiments of the present invention have been described, those skilled in the art may make additional changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the present invention.

[0144] Obviously, those skilled in the art may make various changes and modifications to the embodiments of the present invention without departing from the spirit and scope of the embodiments of the present invention. Thus, if such changes and modifications of the embodiments of the present invention fall within the scope of the claims and their equivalents, the present invention is intended to include such changes and modifications.

Claims

1. A method for manufacturing a circuit board, comprising a plurality of pattern areas and a non-pattern area outside the pattern areas, wherein: The production method comprises: Providing a precursor substrate; forming a seed pattern and an auxiliary seed pattern on one side of the precursor substrate, wherein the seed pattern is located in the pattern area, the auxiliary seed pattern is located in the non-pattern area, and the seed pattern and the auxiliary seed pattern are spaced apart from each other; Through an electroplating process, a pad is formed at the seed pattern, and an auxiliary pattern is formed at the auxiliary seed pattern.

2. The method according to claim 1, wherein: The step of forming a seed pattern and an auxiliary seed pattern on one side of the precursor substrate comprises: forming a plurality of seed patterns in the pattern area of ​​the precursor substrate; Forming an auxiliary film having an auxiliary seed pattern and a hollow area, wherein the auxiliary seed pattern includes: a first flexible substrate, and a first auxiliary seed film layer located on one side of the first flexible substrate; The side of the auxiliary film having the first flexible substrate is laminated to the side of the precursor substrate having the seed pattern, wherein the pattern area of ​​the precursor substrate is laminated to the hollow area of ​​the auxiliary film.

3. The method according to claim 2, wherein: The method of forming an auxiliary film having an auxiliary seed pattern and a hollow area includes: providing a rigid substrate; forming a first flexible substrate and a first auxiliary seed film layer in sequence on one side of the rigid substrate; Cutting the first flexible substrate and the first auxiliary seed film layer to remove the area outside the auxiliary seed pattern to form the hollow area; The rigid substrate is removed.

4. The method according to claim 3, wherein: The step of laminating the side of the auxiliary film having the first flexible substrate to the side of the precursor substrate having the seed pattern comprises: The side of the auxiliary film having the first flexible substrate is bonded to the side of the precursor substrate having the seed pattern by rolling with a roller.

5. The method according to any one of claims 2 to 4, wherein: After forming a pad at the seed pattern and forming an auxiliary pattern at the auxiliary seed pattern through an electroplating process, the manufacturing method further includes: The auxiliary film is removed.

6. The method according to claim 5, wherein: After removing the auxiliary film, the manufacturing method further includes: forming a protective layer on the surface of the pad; A solder resist layer is formed in the non-pattern area.

7. The method according to claim 1, wherein: The step of forming a seed pattern and an auxiliary seed pattern on one side of the precursor substrate comprises: Forming a second seed film layer on the precursor substrate through a sputtering process; By performing a patterning process on the second seed film layer, a plurality of seed patterns are formed in the pattern area, and at the same time, the auxiliary seed pattern is formed in the non-pattern area, wherein a gap exists between the auxiliary seed pattern and the seed pattern.

8. The method according to claim 7, wherein: After forming a pad at the seed pattern and forming an auxiliary pattern at the auxiliary seed pattern through an electroplating process, the manufacturing method further includes: forming a protective layer on the surfaces of the pad and the auxiliary pattern; A solder resist layer is formed in the area where the auxiliary pattern is located.

9. The method according to any one of claims 1 to 8, wherein: The method provides a precursor substrate, comprising: Providing a substrate; forming a plurality of leads on one side of the base substrate; A planar layer is formed on a side of the lead facing away from the base substrate, wherein the planar layer has a via hole exposing a portion of the lead.

10. A circuit board, wherein: include: A base substrate, wherein the base substrate has a pattern area and a non-pattern area outside the pattern area; A plurality of pads are located on one side of the base substrate and in the pattern area; An auxiliary pattern is provided, wherein the auxiliary pattern and the pad are located on the same side of the base substrate, and the auxiliary pattern is located in the non-pattern area.

11. The circuit board according to claim 10, wherein: There is a gap between the auxiliary pattern and the pad.

12. The circuit board according to claim 10 or 11, wherein: The auxiliary pattern and the pad are formed in the same layer and made of the same material.

13. The circuit board according to any one of claims 10 to 12, wherein: A surface of the auxiliary pattern facing away from the base substrate and a surface of the pad facing away from the base substrate are located in the same plane.

14. The circuit board according to any one of claims 10 to 13, wherein: The circuit board also includes: A plurality of leads are located between the substrate base and the pad; A flat layer, located between the lead and the pad, having a via hole exposing a portion of the lead, wherein the lead is electrically connected to the pad in a one-to-one correspondence through the via hole; A protective layer, located on a side of the pad away from the flat layer and covering the pad and the auxiliary pattern; The solder resist layer is located on a side of the auxiliary pattern away from the flat layer and covers the auxiliary pattern.

15. A display device, wherein: include: A display panel, a flexible circuit board, a control chip, and the circuit board obtained by the manufacturing method according to any one of claims 1 to 9, or the circuit board according to any one of claims 10 to 14; wherein the multiple pattern areas of the circuit board include: a first pattern area, a second pattern area, and a third pattern area; The display panel comprises a plurality of first pins, and the first pins of the display panel are bound to the pads of the first pattern area in a one-to-one correspondence; The flexible circuit board includes a plurality of second pins, and the second pins of the flexible circuit board are bound to the pads of the second pattern area in a one-to-one correspondence; The control chip has a plurality of third pins, and the third pins of the control chip are bound to the pads of the third pattern area in a one-to-one correspondence.