Electromagnetic self-shielding packaging grounding structure and production process method thereof
The packaging grounding structure for FCBGA packages addresses electromagnetic interference and heat dissipation by using a substrate with a ground shielding wall, metal cover, and clip connection, achieving effective shielding and improved connectivity.
Patent Information
- Application Number
- CN202411200348.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-29
- Publication Date
- 2024-12-06
AI Technical Summary
Existing electromagnetic shielding technologies are inadequate for flip chip ball grid array (FCBGA) packages with metal shells, as they lack effective grounding and electromagnetic shielding, leading to electromagnetic interference and heat dissipation issues.
A packaging grounding structure comprising a substrate with a ground shielding wall, a main control chip, and a metal cover connected via a metal clip, forming a closed electromagnetic shielding environment by snapping the metal clip onto the metal cover, with additional features like a conductive column, thermal conductive adhesive, and solder balls for improved connectivity and heat dissipation.
The solution effectively blocks electromagnetic radiation, reduces interference, enhances heat dissipation, and protects surrounding devices from electromagnetic interference, while ensuring stable electrical connections and mechanical integrity.
Smart Images

Figure CN119092491A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of electromagnetic self-shielding package grounding, and in particular to an electromagnetic self-shielding package grounding structure and a production process method thereof. Background Art
[0002] At present, the design of package-level electromagnetic shielding mainly uses magnetron sputtering to sputter a metal coating on the outer surface of the package after the chip is plastic-sealed. It is generally a stainless steel-copper-stainless steel structure, and the metal copper layer absorbs and reflects the electromagnetic waves of high-frequency signals to achieve a package-level electromagnetic self-shielding effect; however, this solution is mainly suitable for FCCSP (flip chip level) packages with plastic-sealed shells, but is not applicable to FCBGA (flip chip ball grid array) packages with metal shell packages; on the other hand, the FCBGA package itself has a heat dissipation metal shell, but due to its large size, it is often bonded to the substrate through resin glue, so it is not grounded and cannot achieve the function of electromagnetic shielding. Summary of the invention
[0003] The purpose of the present invention is to overcome the deficiencies of the prior art and to provide an electromagnetic self-shielding package grounding structure and a production process method thereof.
[0004] In order to solve the above technical problems, the present invention adopts the following technical solutions:
[0005] In the first aspect, an embodiment of the present invention provides an electromagnetic self-shielding packaging grounding structure, comprising: a substrate, a main control chip and a metal cover, wherein the substrate is provided with a ground shielding wall, the main control chip is installed on the upper surface of the substrate, the metal cover is used to cover the main control chip and is connected to the substrate, and the upper surface of the substrate is also provided with a metal clip connected to the ground shielding wall, and the metal clip is clipped to the metal cover to form an electrical connection.
[0006] In a specific embodiment, the substrate is divided into several layers, and the exposed peripheral pads of one layer of the substrate are connected to the adjacent substrate wiring copper layer through punching to form a continuous and through-going ground wall structure, namely the ground shielding wall, at the outermost periphery of the substrate circuit layer.
[0007] In a specific embodiment, the main control chip is connected to the substrate through a conductive column.
[0008] In a specific embodiment, a bottom filling material is also filled between the main control chip and the substrate.
[0009] In a specific embodiment, the outer edge of the metal cover is a flat area, and the metal buckle is snapped onto the flat area.
[0010] In a specific embodiment, the metal cover is connected to the substrate via an adhesive, and the metal buckle is in a Z-shape.
[0011] In a specific embodiment, the metal cover is a hat-shaped metal cover.
[0012] In a specific embodiment, a thermal conductive adhesive layer is further provided between the hat-shaped metal cover and the main control chip.
[0013] In a specific embodiment, solder balls are disposed on the lower surface of the substrate.
[0014] The electromagnetic self-shielding packaging grounding structure of the present invention has the following beneficial effects compared with the prior art: by designing a packaging grounding structure including a substrate, a main control chip and a metal cover, and providing a metal clip connected to the ground shielding wall on the upper surface of the substrate, and the metal clip is snapped into the metal cover to form an electrical connection, a closed electromagnetic shielding environment is formed, which can effectively block or weaken the leakage of electromagnetic radiation generated by the main control chip and the substrate during operation, thereby protecting surrounding electronic devices from unnecessary electromagnetic interference.
[0015] In a second aspect, an embodiment of the present invention provides a production process method of an electromagnetic self-shielding package grounding structure, comprising the following steps:
[0016] making a substrate with a ground shielding wall;
[0017] Mounting the main control chip on the upper surface of the substrate and filling the bottom filling material between the main control chip and the substrate;
[0018] Fill a thermal conductive adhesive layer between the metal cover and the main control chip, and bond the metal cover to the substrate;
[0019] A metal clip is welded on the upper surface of the substrate located on the ground shielding wall and the metal clip is connected to the metal cover;
[0020] Perform solder balling on the bottom surface of the substrate to complete the production process.
[0021] The production process method of the electromagnetic self-shielding packaging grounding structure of the present invention has the following beneficial effects compared with the prior art: a packaging grounding structure including a substrate, a main control chip and a metal cover is manufactured through the production process of the electromagnetic self-shielding packaging grounding structure, and a metal clip connected to the ground shielding wall is provided on the upper surface of the substrate, and the metal clip is snapped with the metal cover to form an electrical connection, that is, a closed electromagnetic shielding environment is formed, which can effectively block or weaken the leakage of electromagnetic radiation generated by the main control chip and the substrate during operation, thereby protecting surrounding electronic devices from unnecessary electromagnetic interference.
[0022] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0024] Figure 1 A schematic front view of the electromagnetic self-shielding package grounding structure provided by the present invention;
[0025] Figure 2 A schematic top view of the electromagnetic self-shielding package grounding structure provided by the present invention;
[0026] Figure 3 A schematic flow chart of a production process method for an electromagnetic self-shielding packaged grounding structure provided by the present invention. DETAILED DESCRIPTION
[0027] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0028] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present invention.
[0029] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.
[0030] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0031] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be connected, detachably connected, or integrated; it can be mechanically connected or electrically connected; it can be directly connected or indirectly connected through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0032] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0033] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms should not be understood as necessarily referring to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification.
[0034] See also Figure 1 to Figure 2 As shown, the present invention discloses a specific embodiment of an electromagnetic self-shielding packaging grounding structure, including: a substrate 10, a main control chip 20 and a metal cover 30, the substrate 10 is provided with a ground shielding wall, the main control chip 20 is installed on the upper surface of the substrate 10, the metal cover 30 is used to cover the main control chip 20 and is connected to the substrate 10, and the upper surface of the substrate 10 is also provided with a metal clip 40 connected to the ground shielding wall, and the metal clip 40 is clipped with the metal cover 30 to form an electrical connection.
[0035] Specifically, by combining the ground shielding wall on the substrate 10, the main control chip 20 and the metal cover 30 covering the main control chip 20, and specially designing the electrical connection between the metal buckle 40 connected to the ground shielding wall and the metal cover 30, a complete electromagnetic shielding system is constructed, which can effectively block or weaken the electromagnetic radiation generated by the main control chip 20 and the substrate 10 during operation from leaking outward, which is crucial for reducing electromagnetic interference (EM I) because it can prevent these radiations from causing unnecessary interference or damage to other surrounding electronic devices. In addition, due to the reduction of electromagnetic radiation, the technology can protect sensitive electronic devices located around the packaging structure from the influence of electromagnetic interference, which is crucial for maintaining the stability and reliability of the entire electronic system, especially in modern electronic devices with high-density integration and high-frequency operation. In addition, by reducing the leakage of electromagnetic radiation, the technology helps to maintain the signal integrity and electromagnetic compatibility (EMC) of the electronic system, which can not only reduce signal distortion or loss caused by electromagnetic interference, but also improve the efficiency and accuracy of data transmission, thereby improving the performance of the system as a whole. In addition, the contact between the metal buckle 40 and the metal cover 30 not only forms an electrical connection, but also ensures good grounding of the entire packaging structure. Good grounding can provide a stable potential reference point, which helps to reduce noise and interference caused by potential differences and protect key electronic components such as the main control chip 20 from damage by transient overvoltages such as electrostatic discharge (ESD). In addition, the presence of the metal cover 30 and the metal shielding layer also helps to improve the heat dissipation performance of the package. Metal has good thermal conductivity and can quickly disperse and transfer the heat generated by heat sources such as the main control chip 20 to the external environment, thereby improving the stability and reliability of the entire electronic system. In addition, the metal cover 30 not only provides an electromagnetic shielding function, but also plays a certain physical protection role, which can effectively prevent external physical impacts, dust, moisture and other environmental factors from damaging internal components such as the main control chip 20, thereby extending the service life of electronic products.
[0036] In one embodiment, the substrate 10 is divided into several layers, and the exposed peripheral pads of one layer of the substrate 10 are connected to the adjacent substrate 10 routing copper layer through punching to form a continuous and through-going ground wall structure, i.e., the ground shielding wall, at the outermost periphery of the circuit layer of the substrate 10.
[0037] Specifically, the punching hole can be a through hole structure, or a blind hole or a buried hole. By forming a continuous and through ground wall structure (ground shielding wall) at the outermost periphery of the circuit layer of the substrate 10, it can effectively block and reflect electromagnetic radiation, reduce the leakage of electromagnetic energy from the inside of the substrate 10 to the outside, and this continuous ground wall structure provides an additional electromagnetic shielding layer for electronic equipment, which helps to reduce the risk of electromagnetic interference (EMI) and radio frequency interference (RFI). In addition, whether through holes, blind holes or buried holes are used, the ultimate goal is to form a continuous and through ground wall structure at the outermost periphery of the circuit layer of the substrate 10. These punching methods have their own advantages and disadvantages, but they can enhance the electromagnetic shielding effect to a certain extent; for example: blind holes and buried holes can save space on the circuit board, realize a more compact design, and reduce the length of the signal path and improve signal integrity. In addition, the design of the substrate 10 being divided into several layers allows wiring on different circuit layers, thereby improving the flexibility of the circuit layout. Designers can select the most suitable wiring layer as needed to optimize the signal transmission path and reduce signal attenuation and interference. In addition, with the continuous development of electronic technology, the complexity and integration of circuit boards are getting higher and higher. This multi-layer substrate 10 design can support higher-density wiring requirements and meet the requirements of modern electronic equipment for high performance and high integration. In addition, the multi-layer substrate 10 structure has higher mechanical strength than the single-layer substrate 10. By punching holes to connect the adjacent substrate 10 wiring copper layers, the overall structural stability of the substrate 10 can be further enhanced, so that it can better withstand external shocks and vibrations. In addition, the multi-layer substrate 10 design also helps to optimize the heat dissipation path. By reasonably setting the heat dissipation layer and the heat conduction path, it can ensure that the heat generated by the electronic equipment during operation can be dissipated in time to avoid performance degradation or damage caused by overheating.
[0038] In one embodiment, the main control chip 20 is connected to the substrate 10 via a conductive column 50 .
[0039] Specifically, the conductive column 50, as a connecting medium, realizes a direct electrical connection between the main control chip 20 and the substrate 10. This connection method reduces the attenuation and interference of the signal during the transmission process, and improves the stability and reliability of the electrical connection. In addition, the conductive column 50 can carry the current and signal transmitted between the main control chip 20 and the substrate 10, ensuring the accurate and rapid transmission of the current and signal, which is crucial for the normal operation of the main control chip 20 and the stable operation of the entire circuit system. In addition, the conductive column 50 is not only a part of the electrical connection, but also a path for heat conduction. When the main control chip 20 generates heat during operation, the heat can be transferred to the substrate 10 through the conductive column 50, and then dissipated through the heat dissipation structure on the substrate 10, which helps to reduce the operating temperature of the main control chip 20, improve the heat dissipation efficiency, and ensure the stability and life of the main control chip 20.
[0040] In one embodiment, a bottom filling material 60 is further filled between the main control chip 20 and the substrate 10 .
[0041] Specifically, the bottom filler 60 is usually a low-viscosity, low-temperature curing polymer composite material. In the chip packaging process, due to the difference in the coefficient of thermal expansion (CTE) of the material between the chip and the substrate 10, when the temperature changes, this difference will cause thermal stress between the interfaces. The addition of the bottom filler 60 can effectively alleviate this thermal stress mismatch, and reduce the stress concentration and failure risk caused by the CTE difference through its elasticity and mechanical strength after curing. In addition, after curing, the bottom filler 60 will form a firm adhesive layer and filling layer, which will tightly connect the main control chip 20 and the substrate 10 together. This connection not only enhances the overall mechanical strength of the package, but also improves the anti-drop, anti-vibration and other capabilities of the package structure, thereby extending the service life of the product. In addition, the bottom filler 60 can close the gap between the main control chip 20 and the substrate 10, forming a barrier to effectively prevent the intrusion of harmful substances such as external moisture and dust, which is crucial to protect the chip from corrosion and pollution and maintain its long-term stable performance. In addition, some bottom fillers 60 have good thermal conductivity. They can quickly conduct the generated heat to the substrate 10 when the chip is working, and dissipate it through the heat dissipation structure on the substrate 10, which helps to reduce the operating temperature of the chip and improve its working stability and reliability. In addition, the bottom filler 60 can be compatible with a variety of packaging processes, such as flip-chip packaging (Flip-Chip), ball grid array packaging (BGA), etc., which makes it play an important role in different packaging scenarios and improves the flexibility and adaptability of the packaging process. In addition, with the development of automated production technology, the filling and curing process of the bottom filler 60 can be highly automated. This not only improves production efficiency, but also reduces labor costs and error rates.
[0042] In one embodiment, the outer edge of the metal cover 30 is a flat area, and the metal buckle 40 is snapped onto the flat area.
[0043] Specifically, the flat area on the outer edge of the metal cover 30 provides a stable and reliable contact surface for the metal buckle 40. This design ensures that the metal buckle 40 can be firmly clamped on the metal cover 30 to form a stable electrical connection. In addition, the flat contact surface helps to reduce contact resistance and improve electrical conductivity, which helps to ensure the maximization of the electromagnetic shielding effect, because good electrical conductivity can more effectively guide electromagnetic radiation to the ground shielding wall and finally into the ground. In addition, the metal buckle 40 is clamped on the flat area of the metal cover 30, which helps to reduce or eliminate the gap between the two. The gap is a channel through which electromagnetic radiation may leak, so reducing the gap is crucial to improving the electromagnetic shielding effect. In addition, through the close connection between the metal buckle 40 and the metal cover 30, the entire packaging structure becomes more solid and tight. This design helps to form a more complete electromagnetic shielding environment, thereby more effectively blocking or reducing the leakage of electromagnetic radiation. In addition, the clamping design of the metal buckle 40 and the flat area makes the installation and maintenance process simpler and faster. If the components in the packaging structure need to be replaced or repaired, the staff can more easily disassemble and reassemble these components.
[0044] In one embodiment, the metal cover 30 is connected to the substrate 10 via an adhesive 80 , and the metal buckle 40 is in a Z-shape.
[0045] Specifically, the use of adhesive 80 to connect the metal cover 30 to the substrate 10 can provide a stable and durable connection method. The adhesive 80 can fill the small gap between the metal cover 30 and the substrate 10 to form a tight bonding surface, thereby preventing loosening or falling off. This connection method is essential for maintaining the integrity of the electromagnetic shielding environment. In addition, the design of the Z-shaped metal buckle 40 not only increases the contact area with the metal cover 30, but also provides additional locking force through its unique shape; when the metal buckle 40 is clamped on the flat area of the metal cover 30, its Z-shaped structure helps to resist deformation or displacement under the action of external forces, thereby further enhancing the stability and reliability of the connection.
[0046] Preferably, the metal buckle 40 can be interconnected with the substrate 10 and the metal cover 30 by welding. As a welding material, the conductive silver paste can tightly connect the metal buckle 40, the substrate 10 and the metal cover 30 to form a low-resistance conductive path. This electrical connection not only ensures the integrity of the electromagnetic shielding, but also helps to effectively guide the electromagnetic radiation into the ground, thereby reducing the leakage of electromagnetic radiation. In addition, the welding process of the conductive silver paste can fill the tiny gaps between the metal buckle 40, the substrate 10 and the metal cover 30, reducing the risk of electromagnetic leakage caused by the gaps, which is of great significance for improving the overall electromagnetic shielding effect. In addition, the connection formed by the conductive silver paste welding has high mechanical strength and durability, and can resist the influence of the external environment (such as temperature changes, vibrations, etc.) on the connection point, which helps to ensure the long-term stable connection between the metal buckle 40 and the substrate 10 and the metal cover 30. In addition, the conductive silver paste usually also has good thermal conductivity, which helps to quickly conduct the heat generated by the metal buckle 40, the substrate 10 and the metal cover 30 during work, reduce local temperature rise, and improve the stability and reliability of the system.
[0047] See also Figure 2 As shown, there are several metal buckles 40, and the number of installations is generally determined according to the shielding effectiveness of finite element EMI simulation (the grounding area, considering the grounding shielding effectiveness, at least two metal buckles 40 can be set for a single side of the package), and considering the risk control of warping, the metal buckles 40 are installed in a non-continuous manner, that is, they are evenly distributed in the edge area of the substrate 10 (that is, connected to the ground shielding wall). The material of the metal buckle 40 is mainly copper, and it can also be other conductive alloy materials. Copper is an excellent conductive material with low resistivity, so the copper metal buckle 40 can ensure the formation of a good conductive path in the electromagnetic shielding structure, effectively guide the electromagnetic radiation to the ground shielding wall or the ground, thereby reducing electromagnetic leakage. In addition to copper, other conductive alloy materials (such as brass, bronze, zinc alloy, etc.) also have good conductivity. These alloy materials may optimize conductivity, mechanical properties or corrosion resistance by adjusting the composition and proportion to meet different application requirements. In addition, the material of the metal buckle 40 is allowed to be mainly copper, and it can also be other conductive alloy materials. This design choice provides manufacturers with greater flexibility and allows them to choose the appropriate material of the metal buckle 40 based on specific application scenarios, cost budgets and performance requirements.
[0048] In one embodiment, the metal cover 30 is a hat-shaped metal cover.
[0049] Specifically, the cap-shaped metal cover usually has a larger coverage area and stronger structural strength, which can provide better protection. It can not only prevent external objects from directly impacting and damaging internal components, but also reduce the loosening or damage of internal components caused by vibration or impact. In addition, the cap-shaped metal cover can also be used as a decorative part of the product to increase the beauty and recognition of the product. At the same time, it can also be used as a product logo or label to distinguish products of different models or specifications.
[0050] In one embodiment, a thermal conductive adhesive layer 90 is further disposed between the cap-shaped metal cover and the main control chip 20 .
[0051] Specifically, the thermally conductive adhesive layer 90 is a material with excellent thermal conductivity, which can effectively conduct the heat generated by the main control chip 20 to the cap-shaped metal cover quickly. This efficient heat conduction mechanism helps to reduce the temperature of the main control chip 20 and prevent it from being damaged due to overheating, thereby improving the reliability and service life of the entire electronic component. In addition, the thermally conductive adhesive layer 90 fills the small gap between the cap-shaped metal cover and the main control chip 20, forming a continuous heat conduction channel. This design enables heat to be transferred to the external environment along a shorter and more efficient path, further improving the heat dissipation effect. In addition, the thermally conductive adhesive layer 90 not only has a heat conduction function, but also has a certain viscosity and strength. It can firmly bond the cap-shaped metal cover to the main control chip 20, providing additional structural support. This support function helps to reduce the looseness or damage of the structure caused by external factors such as vibration and impact. In addition, the thermally conductive adhesive layer 90, as an isolation layer between the main control chip 20 and the external environment, can prevent harmful substances such as moisture and corrosive gases from directly contacting the main control chip 20, thereby protecting it from erosion and damage. In addition, there are often tiny gaps or unevenness in the contact interface between the hat-shaped metal cover and the main control chip 20, which will increase the interface thermal resistance and affect the effective conduction of heat. The thermal conductive adhesive layer 90 can fill these tiny gaps to form a tight contact interface, thereby reducing the interface thermal resistance and improving the heat conduction efficiency.
[0052] In one embodiment, solder balls 70 are disposed on the lower surface of the substrate 10 .
[0053] Specifically, the solder ball 70, as a conductive medium, can form a reliable electrical connection between the lower surface of the substrate 10 and the corresponding electrical contact points. This connection method ensures the smooth transmission of electronic signals between the substrate 10 and other electronic components, and is the basis for the normal operation of electronic equipment. In addition, in high-speed data transmission and high-frequency applications, the solder ball 70 package can achieve a higher electrical signal transmission rate and lower signal loss. This is because the solder ball 70 has good electrical conductivity and low contact resistance, which can reduce the attenuation and distortion of the signal during transmission. In addition, tin has good thermal conductivity, so the solder ball 70 package helps to achieve good thermal management; when electronic equipment generates heat during operation, the solder ball 70 can effectively conduct heat, help dissipate heat and keep the temperature of electronic components within an acceptable range, which is particularly important for high-power electronic equipment and integrated circuits, and can prevent performance degradation or damage caused by overheating.
[0054] See also Figure 3 As shown, an embodiment of the present invention provides a production process method for an electromagnetic self-shielding package grounding structure, comprising the following steps:
[0055] S1, manufacturing a substrate with a ground shielding wall;
[0056] Specifically, when designing the substrate wiring, the metal wires at the outermost periphery of the substrate are connected through via holes, and their pins are defined as grounded, and finally interconnected with the mainboard through ground pads.
[0057] S2, mounting the main control chip on the upper surface of the substrate, and filling the bottom filling material between the main control chip and the substrate;
[0058] Specifically, a pad window structure is provided on the periphery of the upper surface of the substrate, a pad window structure is provided in the DIE Bump (chip flip-chip solder joint) area, and the remaining positions are covered by the solder resist layer.
[0059] S3, filling a thermal conductive adhesive layer between the metal cover and the main control chip, and bonding the metal cover to the substrate;
[0060] Specifically, since the metal cover is a cap-shaped metal cover, a thermal conductive adhesive layer needs to be coated between the cap-shaped metal cover and the main control chip, and then the metal cover is bonded to the substrate by an adhesive.
[0061] S4, welding a metal buckle on the upper surface of the substrate located on the ground shielding wall and making the metal buckle and the metal cover form a snap connection;
[0062] Specifically, first ensure that the surface of the substrate is clean, free of oil and oxide, and then select appropriate metal materials (such as copper, aluminum, etc.) and sizes according to design requirements to ensure that the surface of the metal buckle is also clean and free of defects. Then, according to the electromagnetic shielding requirements, determine the number, position, height and other parameters of the metal buckles, and then select appropriate welding methods and parameters according to the welding process plan. Use a welding gun or welding equipment to heat the metal buckle, and at the same time feed in welding wire for filling, control the welding speed and temperature, ensure that the weld quality is good and a firm connection is formed between the metal buckle and the substrate; after welding is completed, use measuring tools and visually inspect the quality of the weld to ensure that the weld is free of cracks, slag inclusions, unfused and other defects, so as to ensure that the metal buckle and the metal cover are tightly clamped without gaps or misalignment.
[0063] S5, performing a solder ball operation on the lower surface of the substrate to complete the production process.
[0064] Specifically, a packaging grounding structure including a substrate, a main control chip and a metal cover is manufactured through the production process of an electromagnetic self-shielding packaging grounding structure, and a metal clip connected to the ground shielding wall is provided on the upper surface of the substrate, and the metal clip is snapped into the metal cover to form an electrical connection, thereby forming a closed electromagnetic shielding environment, which can effectively block or weaken the leakage of electromagnetic radiation generated by the main control chip and the substrate during operation, thereby protecting surrounding electronic devices from unnecessary electromagnetic interference.
[0065] The above embodiments are preferred implementation schemes of the present invention. In addition, the present invention may also be implemented in other ways. Any obvious replacement without departing from the concept of the present technical solution is within the protection scope of the present invention.
Claims
1. An electromagnetic self-shielding package grounding structure, characterized in that: include: A substrate, a main control chip and a metal cover, wherein the substrate is provided with a ground shielding wall, the main control chip is installed on the upper surface of the substrate, the metal cover is used to cover the main control chip and is connected to the substrate, and the upper surface of the substrate is also provided with a metal clip connected to the ground shielding wall, and the metal clip is clipped with the metal cover to form an electrical connection.
2. The electromagnetic self-shielding encapsulated grounding structure according to claim 1, characterized in that: The substrate is divided into several layers, and the exposed peripheral pads of one layer of the substrate are connected to the adjacent substrate wiring copper layer through punching to form a continuous and through ground wall structure at the outermost periphery of the substrate circuit layer, namely the ground shielding wall.
3. The electromagnetic self-shielding encapsulated grounding structure according to claim 1, characterized in that: The main control chip is connected to the substrate through a conductive column.
4. The electromagnetic self-shielding encapsulated grounding structure according to claim 3, characterized in that: A bottom filling material is also filled between the main control chip and the substrate.
5. The electromagnetic self-shielding encapsulated grounding structure according to claim 1, characterized in that: The outer edge of the metal cover is a flat area, and the metal buckle is snap-connected to the flat area.
6. The electromagnetic self-shielding encapsulated grounding structure according to claim 1, characterized in that: The metal cover is connected to the substrate through an adhesive, and the metal buckle is in a Z shape.
7. The electromagnetic self-shielding encapsulated grounding structure according to claim 1, characterized in that: The metal cover is a cap-shaped metal cover.
8. The electromagnetic self-shielding encapsulated grounding structure according to claim 7, characterized in that: A heat-conducting adhesive layer is also provided between the cap-shaped metal cover and the main control chip.
9. The electromagnetic self-shielding encapsulated grounding structure according to claim 1, characterized in that: The lower surface of the substrate is provided with solder balls.
10. A production process for an electromagnetic self-shielding package grounding structure, characterized in that: The following steps are involved: making a substrate with a ground shielding wall; Mounting the main control chip on the upper surface of the substrate and filling the bottom filling material between the main control chip and the substrate; Fill a thermal conductive adhesive layer between the metal cover and the main control chip, and bond the metal cover to the substrate; A metal clip is welded on the upper surface of the substrate located on the ground shielding wall and the metal clip is connected to the metal cover; Perform solder balling on the bottom surface of the substrate to complete the production process.