Metal-insulator-metal device and manufacturing method thereof
By using a cover layer of a tetragonal lattice phase and a zirconium-rich oxide composition in the MIM structure, the performance deterioration caused by thermal annealing is solved, and the robustness and performance indicators of the MIM structure are improved, especially for ferroelectric MIM. structure, achieving higher collapse voltage and lower leakage.
Patent Information
- Application Number
- CN202411064420.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-08-11
- Filing Date
- 2024-08-05
- Publication Date
- 2024-12-06
AI Technical Summary
The existing metal-insulator-metal (MIM) structures have deteriorated performance during thermal annealing, especially in terms of collapse voltage, time-dependent dielectric breakdown and leakage, and the ferroelectric MIM structure is unstable for orthogonal crystallization annealing.
By using a cover layer with a predominantly tetragonal lattice phase in the MIM structure, the lower and upper cover layers are formed, respectively, containing at least 80% of the tetragonal dielectric material, deterioration during thermal annealing and by appropriate zirconium and oxidation The zirconium-rich version of compositions such as Hf1-xZrxO2 and ZrO2 improves the performance of the insulator layer.
The performance indicators of MIM structures are significantly improved, such as time-dependent dielectric breakdown, collapse voltage and leakage, which improves the robustness and output of the device, especially for ferroelectric MIM structures, and reduces the impact of orthogonal crystallization annealing.
Smart Images

Figure CN119092496A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a metal-insulator-metal device and a method for manufacturing the same. Background Art
[0002] The following relates to metal-insulator-metal (MIM) devices, integrated circuit (IC) technology, ferroelectric device technology, and related technologies. Summary of the invention
[0003] According to some embodiments of the present disclosure, a method for manufacturing a metal-insulator-metal (MIM) device includes the following steps: forming a first capping layer on a first metal, wherein the first capping layer includes a composition including at least zirconium and oxygen and having a tetragonal lattice phase; forming Hf on the first capping layer; 1-x Zr x O2 insulator layer. In Hf 1-x Zr x A second capping layer is formed on the O2 insulator layer, and the second capping layer includes a composition containing at least zirconium and oxygen and having a tetragonal lattice phase. A second metal is formed on the second capping layer.
[0004] According to some embodiments of the present disclosure, a method for manufacturing a metal-insulator-metal (MIM) device includes the following steps: forming a first capping layer on a first metal, wherein the first capping layer includes a dielectric material having a tetragonal phase percentage of at least 80%. forming a second capping layer on the insulator layer, wherein the second capping layer includes a dielectric material having a tetragonal phase percentage of at least 80%. forming a second metal on the second capping layer.
[0005] According to some embodiments of the present disclosure, a metal-insulator-metal (MIM) device includes a first metal, a first capping layer disposed on the first metal, an insulator layer disposed on the first capping layer, a second capping layer disposed on the insulator layer, and a second metal disposed on the second capping layer. The first capping layer includes a dielectric material having a tetragonal lattice phase, and the second capping layer includes a dielectric material having a tetragonal lattice phase. BRIEF DESCRIPTION OF THE DRAWINGS
[0006] The embodiments of the present disclosure may be better understood from the following detailed description when read in conjunction with the accompanying drawings. It is noteworthy that, in accordance with standard practice in practice, the features are not drawn to scale. In fact, the dimensions of the various features may be arbitrarily increased or decreased for clarity of discussion.
[0007] Figure 1 , Figure 2 and Figure 3depicts a side cross-sectional view of a metal-insulator-metal (MIM) device including a high-k insulator with a capping structure according to various embodiments;
[0008] Figure 4 Hf 1-x Zr x The relationship between the composition and crystal structure of O2;
[0009] Figure 5 depicts a side cross-sectional view of a MIM device including a high-k insulator with a capping structure according to another embodiment;
[0010] Figure 6 Some experimental results are presented, demonstrating that the leakage of MIM devices decreases with increasing ZrO2 coverage thickness;
[0011] Figure 7 depicts a side cross-sectional view of a MIM device including a high-k insulator with a capping structure according to another embodiment;
[0012] Figure 8 A flow chart illustrating a suitable manufacturing process for manufacturing a MIM device including a high-k insulator with a capping structure is depicted;
[0013] Fig. 9 depicts a side cross-sectional view of a MIM device including a high-k insulator with a capping structure according to another embodiment; and
[0014] Fig.10 and Fig.11 Two exemplary applications of the MIM device of the present disclosure are illustrated for reducing noise fluctuations in signals transmitted between an integrated circuit (IC) die and bonding bumps of a redistribution layer.
[0015]
Explanation of symbols
[0016] 10: First Metal / Lower Metal
[0017] 12: First covering layer / lower covering layer / covering layer
[0018] 12 Zr-rich :Lower covering layer / first covering layer / covering layer
[0019] 12 ZrO :Lower covering layer / first covering layer / covering layer
[0020] 12 d :Lower cover layer / Lower doped cover layer / cover layer
[0021] 14: High-k insulator layer / HK layer / insulator layer / ferroelectric layer
[0022] 14FE :Insulator layer / Ferroelectric insulator layer / FE layer
[0023] 14 HZO :Insulator layer / HZO layer / HZO insulator layer
[0024] 16: Second covering layer / upper covering layer / covering layer
[0025] 16 Zr-rich :Upper cover layer / Second cover layer / Cover layer
[0026] 16 ZrO :Upper cover layer / Second cover layer / Cover layer
[0027] 16 d :Upper cover layer / Upper doped cover layer / Cover layer
[0028] 18: Second Metal / Upper Metal
[0029] 30,32,34,36,38,40: Steps
[0030] 40: Thermal annealing
[0031] 50: High-k buffer layer
[0032] 60:Semiconductor wafer / wafer
[0033] 62: Top metallization layer / top patterned metallization layer
[0034] 64: Dielectric materials
[0035] 66: Dielectric layer / dielectric material
[0036] 70:MIM structure
[0037] 72:Through hole
[0038] 74: Redistribution Layer / RDL
[0039] 75: Bonding pad
[0040] 76: Dielectric layer
[0041] 78: Passivation layer
[0042] 80: Engagement bump
[0043] 82: Interface Materials
[0044] 84: Polyimide layer
[0045] a,b,c: edge
[0046] d:Thickness
[0047] dtop :thickness
[0048] d HK :thickness
[0049] d bot :thickness DETAILED DESCRIPTION
[0050] The following disclosure provides many different embodiments or examples for implementing the different features of the present disclosure. Specific examples of components and configurations are described below to simplify the present disclosure. Of course, these specific examples are only examples and are not intended to be limiting. For example, in the following description, the formation of a first feature above or on a second feature may include an embodiment in which the first feature and the second feature are directly contacted, and may also include an embodiment in which an additional feature may be formed between the first feature and the second feature so that the first feature and the second feature may not be directly in contact. In addition, the present disclosure may repeat reference numerals and / or letters in various examples. This repetition is for the purpose of simplicity and clarity, and does not itself indicate the relationship between the various embodiments and / or configurations discussed.
[0051] Additionally, for ease of description, spatially relative terms (e.g., "below," "overlying," "lower," "above," "upper," and the like) may be used herein to describe the relationship of one component or feature to another component or feature as illustrated in the accompanying figures. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein interpreted accordingly.
[0052] The term "about" can be used to include any value that can be varied without changing the basic function of the value. When used with a range, "about" also discloses a range defined by the absolute value of one or both endpoints, for example, "about 0.2 nanometers to about 5 nanometers" also discloses the range "0.2 nanometers to 5 nanometers". And, similarly, a range of "at least about 25% lower" also discloses a range of "at least about 25% lower". The term "about" can mean plus or minus 10% of the specified number.
[0053] Metal-insulator-metal (MIM) devices are used in various integrated circuit (IC) designs. The basic MIM structure includes an insulator layer disposed between first and second metal layers and can be used, for example, for capacitors for frequency filtering, noise reduction, direct current (DC) isolation, etc. The insulator layer has a high dielectric constant to facilitate providing high capacitance to the MIM structure. In common notation, high-k (high κ, or high relative permittivity ε) is used to represent the dielectric constant of the MIM structure. r ) The dielectric material has a dielectric constant κ(=εr ) a dielectric material with a dielectric constant greater than that of silicon dioxide (SiO2, κ = 3.9). The capacitance C of the MIM structure is obtained by the following formula, where κ and d are the dielectric constant and thickness of the insulator layer, respectively, and ε0 is the dielectric constant of free space (i.e., vacuum). Accordingly, it can be seen that by reducing the thickness d of the insulator layer and / or by increasing the dielectric constant κ of the insulator layer, the capacitance C (for a given area A of the MIM) can be increased. Therefore, there is a motivation to make the MIM structure have a high dielectric constant and a reduced thickness d of the insulator layer.
[0054] In some applications, the insulator layer of the MIM structure may need to be a ferroelectric material. For example, an MIM with a ferroelectric insulator layer can be used to implement a ferroelectric memory (i.e., storage) device. For example, an array of MIM devices with a ferroelectric insulator layer and a suitable transistor-based drive circuit can thus serve as a compact ferroelectric memory array. A suitable high-k dielectric material that can be made into a ferroelectric material is hafnium zirconium oxide (Hf 1-x Zr x O2), which is also denoted as HZO in the disclosure. The x in Hf 1-x Zr x O2 represents the number of zirconium molecules, where 0 < x < 1. The binary oxide ZrO2 corresponds to x = 1, and the binary oxide HfO2 corresponds to x = 0. The orthorhombic lattice phase of HZO is non-centrosymmetric, and the arrangement of oxygen atoms can respond to an external electric field to form polarization, and thus can be switched between the positive polarization and negative polarization states by applying an electric field. The ferroelectric property of the orthorhombic lattice phase of HZO is the result of the non-centrosymmetric crystal structure of the orthorhombic lattice phase of HZO.
[0055] The performance of the MIM structure is usually characterized by metrics such as breakdown voltage (VBD), time-dependent dielectric breakdown (TDDB), and leakage (LK). The performance of the MIM structure measured by such metrics degrades due to the thermal annealing of the MIM structure. However, annealing may be performed, such as a high-temperature treatment performed after forming the MIM structure, or an orthorhombic crystallization annealing induced in the case of the MIM structure used as a ferroelectric device.
[0056] In the MIM structure and corresponding manufacturing method disclosed herein, degradation is reduced by using a capping layer having a predominantly tetragonal lattice phase. As described herein, the capping layer improves the indicators (e.g., TDDB, VBD, LK) of the MIM structure and thus increases the device yield. The capping layer having a predominantly tetragonal lattice phase reduces the degradation produced by the annealing process. For a ferroelectric MIM structure, the MIM structure is more robust to orthorhombic crystallization annealing.
[0057] See also Figure 1 , depicts a side cross-sectional view of a MIM device according to a first embodiment. The MIM structure includes a first metal 10, a first capping layer 12 disposed on the first metal 10, a high-k insulator layer (high-k, HK layer) 14 disposed on the first capping layer 12, a second capping layer 16 disposed on the HK layer, and a second metal 18 disposed on the second capping layer 16. In one suitable manufacturing process (see Figure 8 ), the order of formation is: forming a first metal 10; then forming a first capping layer 12; then forming an HK layer 14; then forming a second capping layer 16; then forming a second metal 18. Therefore, the first metal 10 is also referred to as the lower metal 10 in the present disclosure; the first capping layer 12 is also referred to as the lower capping layer 12 in the present disclosure; the second capping layer 16 is also referred to as the upper capping layer 16 in the present disclosure; and the second metal 18 is also referred to as the upper metal 18 in the present disclosure. The use of "upper" and "lower" does not indicate any specific spatial positioning.
[0058] The lower metal 10 suitably includes a conductive material, such as titanium nitride (TiN); tantalum nitride (TaN); an elemental metal, such as titanium (Ti), aluminum (Al), tungsten (W), platinum (Pt), molybdenum (Mo), or alloys thereof, etc. As shown by these non-limiting illustrative examples, the term "metal" used in the present disclosure is not limited to elemental metals or alloys thereof; on the contrary, the term "metal" used herein also covers other materials commonly used as electrical conductors in the semiconductor industry, such as TiN or TaN. The upper metal 18 also suitably includes a conductive material such as TiN, TaN, an elemental metal such as Ti, Al, W, Pt, Mo, or alloys thereof, etc. The upper metal 18 can be the same type of metal as the lower metal 10 (for example, both are TiN); or, the upper metal 18 and the lower metal 10 can be different types of metals (for example, the lower metal 10 can be W, and the upper metal 18 can be TaN).
[0059] The upper cover layer 12 and the lower cover layer 16 each include a dielectric material having a tetragonal lattice phase. For example, in some embodiments, the upper cover layer 12 and the lower cover layer 16 have a tetragonal phase percentage of at least 80%; or in other words, the upper cover layer 12 and the lower cover layer 16 have a tetragonal phase percentage of at least 80%. In various embodiments, the tetragonal phase percentage of the upper cover layer 12 and the lower cover layer 16 can be achieved by selecting appropriate components, or by appropriately doping the upper cover layer 12 and the lower cover layer 16. The tetragonal phase has mutually orthogonal (i.e., mutually perpendicular) sides a, b, and c, and has a unit cell with two sides (e.g., sides a and b) of equal length. If the three sides of the unit cell have the same length (i.e., a=b=c), the tetragonal phase is specifically a cubic phase. The cubic phase is also a tetragonal phase, i.e., the cubic phase is one example of a tetragonal phase.
[0060] The insulator layer 14 includes a high-k dielectric material and is therefore also referred to as the HK layer 14 in the present disclosure. The insulator layer 14 has a dielectric constant greater than that of silicon dioxide (SiO2, κ=3.9). In some non-limiting exemplary embodiments, the insulator layer 14 is a high-k dielectric material with a dielectric constant κ in the range of 30≤κ≤40. In some non-limiting illustrative examples, the insulator layer 14 has an orthorhombic lattice phase percentage of at least 70%. In some non-limiting illustrative embodiments, the insulator layer 14 is a ferroelectric material, and in some cases, is obtained by having an orthorhombic lattice phase percentage of at least 70%. In some non-limiting exemplary embodiments, the thickness d of the lower cover layer 12 is bot Less than or equal to the thickness d of the insulator layer 14 HK 0.1 times (i.e., ); the thickness d of the upper cover layer 16 top Less than or equal to the thickness d of the insulator layer 14 HK 0.1 times (i.e. ). and The advantage of the relatively thin capping layer is that the total thickness of the dielectric material disposed between the lower metal 10 and the upper metal 18 is reduced, thereby maintaining a low total thickness d and thus maintaining a high capacitance.
[0061] In some embodiments, the capping layers 12 and 16 are made of the same high-k dielectric material as the HK layer 14, although they may have different compositional ingredients and / or be doped to enhance the tetragonal phase percentage as described in some illustrative embodiments of the present disclosure. For example, in one non-limiting illustrative example, the capping layers 12 and 16 and the HK layer 14 may all be made of hafnium zirconium oxide with the same or different zirconium molecular numbers.
[0062] Without being limited to any particular theory of operation, the lower capping layer 12 is believed to improve the properties of the insulator layer 14 (e.g., TDDB, VBD, LK) by at least one or more of the following mechanisms. If the insulator layer 14 is a binary, ternary, or quaternary oxide, and the lower capping layer 12 is also a (possibly different) binary, ternary, or quaternary oxide, then the lower capping layer 12 is believed to reduce defects in the insulator layer 14 due to oxygen deficiency or holes. The lower capping layer 12 can also provide an improved crystallographic template for the subsequently formed insulator layer 14. In particular, if the bottom layer 12 and the insulator layer 14 are made of materials with similar crystal structures (e.g., the lower capping layer 12 is ZrO2 or Hf 1-x Zr x O2, and the insulator layer 14 is Hf 1-x Zr x In the case of O2 (as a non-limiting example), in some embodiments, the lower capping layer 12 has a thickness of at least 0.4 nanometers to provide a stable and uniform film.
[0063] Without being limited to any particular theory of operation, the upper capping layer 16 is believed to protect the insulator layer 14 at least during one or more processes to improve the properties (e.g., TDDB, VBD, LK) of the insulator layer 14. Heat treatment performed after the MIM structure is formed. For example, if the MIM structure is intended to be a ferroelectric, the heat treatment may include annealing to crystallize the insulator layer into a crystallization of a predominantly ferroelectric orthorhombic phase. In other examples, one or more thermal processes may include increasing the temperature when depositing the material after the MIM structure is formed.
[0064] Since the lower cover layer 12 and the upper cover layer 16 perform different functions, the lower cover layer 12 and the upper cover layer 16 may have different thicknesses and / or different compositions. As a non-limiting example, in one embodiment, the thickness of the lower cover layer 12 is 0.4 nanometers, and the thickness of the upper cover layer 16 is 1.0 nanometers.
[0065] In applications, such as Figure 1The MIM structure or the MIM structure of other embodiments of the present disclosure can be used as a capacitor for frequency filtering, noise reduction, DC isolation, etc. In some embodiments, the MIM structure can be formed during the back end-of-line (BEOL) processing of the IC chip, but is not limited to this configuration. The lower metal 10 and the upper metal 18 are configured to serve as electrodes or electrode plates of the capacitive MIM structure, and the insulator layer 14 (followed by the dielectric cover layers 12 and 16) are configured to serve as the insulator structure of the MIM capacitor. In an embodiment where the insulator layer 14 is a ferroelectric material, the MIM structure can be used as a ferroelectric tunnel junction (FTJ), or conversely, the MIM structure can be used as a storage element of a ferroelectric random access memory (FeRAM), where the FeRAM includes a FTJ and a transistor. For example, the transistor can be a field-effect transistor (FET), and is suitable for reading bit values from and writing bit values to the FTJ, and the FTJ serves as a non-volatile memory of the FeRAM.
[0066] See also Figure 2 , depicts an embodiment of the MIM structure. Figure 1 As described in the embodiment of the present invention, the MIM structure includes a lower metal 10, a lower cover layer 12, an upper cover layer 16 and an upper metal 18. And, further includes the above Figure 1 The insulator layer 14, but Figure 1 The insulating layer 14 is Figure 2 In the embodiment of the present invention, the ferroelectric insulator layer 14 is specifically FE . Ferroelectric insulator layer 14 FE The ferroelectric phase includes an asymmetric central orthorhombic lattice phase having oxygen atoms configured to form polarization in response to an external electric field, and thus capable of switching between positive and negative polarization states by applying an electric field. The ferroelectric properties of the orthorhombic lattice phase are a result of the asymmetric central crystal structure of the orthorhombic lattice phase. In some non-limiting illustrative embodiments, the ferroelectric insulator layer 14 FE may include an oxide, and the oxide is selected from Hf 1-x Zr x O2, SrBi2Ta2O9, PbZr x Ti 1- x In some embodiments, the insulator layer 14 FEComprises a ternary or quaternary oxide having a ferroelectric orthorhombic lattice phase, and the phase percentage in the insulator layer 14FE is at least 70%; the lower cover layer 12 comprises a ternary or quaternary oxide doped with a dopant, and the upper cover layer 16 comprises a ternary or quaternary oxide doped with a dopant. Moreover, the dopant makes the tetragonal phase percentage of the lower cover layer 12 at least 80%, and also makes the tetragonal phase percentage of the upper cover layer 16 at least 80%.
[0067] Please refer to Figure 3 , which shows an embodiment of the MIM structure. The insulator layer is a hafnium zirconium oxide (Hf 1-x Zr x O2 or HZO) layer 14 HZO , the lower cover layer is the lower (or first) cover layer 12 Zr-rich , the lower (or first) cover layer 12 Zr-rich contains more zirconium molecules (i.e., a larger x value) of HZO than the HZO layer 14 HZO contains, and the upper (or second) cover layer 14 Zr-rich contains more zirconium molecules (i.e., a larger x value) of HZO than the HZO layer 14 HZO contains. In other words, compared with the HZO layer 14 HZO , the lower and upper cover layers 12 Zr-rich and 14 Zr-rich are HZO materials richer in zirconium. As mentioned above, in some embodiments, the thickness of each of the lower cover layer 12 Zr-rich and the upper cover layer 14 Zr-rich is 1 / 10 or less of the thickness of the HZO layer 14 HZO .
[0068] Next, please refer to Figure 3 and further refer to Figure 4 , which describes the reason why making the lower cover layer 12 Zr-rich and the upper cover layer 16 Zr-rich richer in zirconium than the HZO layer 14 HZO can promote the formation of the desired crystal structure in the corresponding layers. Figure 4 Exemplarily shows the molecular formula of the zirconium molecule number of the stable crystal structure, and the range of x is from x = 0 (i.e., the binary oxide HfO2) to x = 1 (the binary oxide ZrO2). Conceptually, the ternary composition (HZO, where 0 < x < 1) can be regarded as a mixture of HfO2 and ZrO2. As Figure 4As shown, the stable crystal phase of ZrO2 is a tetragonal lattice phase, while the stable crystal phase of HfO2 is a monoclinic phase (where the angle β between the side a and the side c is not equal to 90°, β≠90°). As for the intermediate value of zirconium composition (i.e., an intermediate mixture of HfO2 and ZrO2), the stable phase of the ternary oxide HZO is an orthorhombic lattice phase.
[0069] The stable orthorhombic phase of HZO is asymmetrically centered, with oxygen atoms arranged in such a way that they can form polarization in response to an external electric field, and can then switch between positive and negative polarization states by applying an electric field. The ferroelectric properties of the orthorhombic phase of HZO are a result of the asymmetric centered crystal structure. On the other hand, by enriching HZO with zirconium (e.g. Figure 4 As shown in FIG. 1 , the stable crystalline phase is transformed into a tetragonal lattice phase. Therefore, by forming a lower cover layer 12 with a zirconium-rich HZO composition Zr-rich and the upper covering layer 16 Zr-rich , and a lower cover layer 12 having a tetragonal phase percentage of at least 80% may be formed Zr-rich and the upper covering layer 16 Zr-rich . Covering layer 12 Zr-rich and 16 Zr-rich and the insulator layer 14 HZO The number of Zr molecules in the cover layer 12 is appropriately determined by experimental testing (in order to Zr-rich and 16 Zr-rich The desired tetragonal phase percentage of 80% or more is achieved in the insulator layer 14 HZO The desired 70% or higher orthorhombic phase is achieved in the overlying layer 12 (possibly after annealing), wherein the experimental test is characterized by X-ray diffraction (XRD), electron backscatter diffraction (EBSD) or other characterization techniques to evaluate the phase percentages of each layer. In some non-limiting illustrative examples, a zirconium molecular number x greater than about 20% is suitable for the overlying layer 12 Zr-rich and 16 Zr-rich The desired tetragonal phase percentage of 80% or more is obtained.
[0070] In this embodiment, the deposited HZO layer 14 HZO It may be amorphous or may have an undesirable mixture of crystalline phases. Specifically, the deposited insulator layer 14 HZO may not have the desired orthorhombic lattice phase percentage of 70% or more. Therefore, in some embodiments, the formation of each layer in the MIM structure includes performing annealing so that the deposited insulator layer 14 HZOThe crystallization is mainly an orthorhombic lattice phase (e.g., an orthorhombic lattice phase percentage of 70% or more). The annealing is performed at a suitably high temperature for a sufficient time (e.g., as a non-limiting example, in some cases, 5 minutes at 550° C. may be sufficient). According to the IC manufacturing process including the MIM structure, when forming the insulator layer 14 having HZO HZO After the MIM device is formed, the IC manufacturing steps performed may provide sufficient annealing to obtain the desired orthorhombic lattice phase of 70% or more, so it may not be necessary to perform a special anneal to perform orthorhombic crystallization of HZO. XRD, EBSD or other characterization methods can be performed in experimental testing of different annealing methods to experimentally determine the insulator layer 14 HZO Suitable annealing method.
[0071] See also Figure 5 , according to another embodiment similar to Figure 3 However, Figure 5 The MIM structure is respectively the lower (i.e. the first) ZrO2 capping layer 12 ZrO and the upper (i.e. second) ZrO2 capping layer 16 ZrO Alternative Figure 3 The cover layer 12 of the embodiment Zr-rich and 16 Zr-rich Please return to Figure 4 This embodiment corresponds to the limiting case where the zirconium-rich capping layer is a binary oxide ZrO2 (ie, the number of zirconium molecules x=1).
[0072] See also Figure 6 , basically presents the following Figure 5 The experimental results of the MIM structure shown in FIG. 1 include a lower ZrO2 capping layer 12 ZrO and the upper ZrO2 capping layer 16 ZrO Covering HZO layer 14 HZO . Figure 6 The measured leakage (LK) of the MIM structure is plotted as a function of the ZrO2 thickness. As shown in the figure, the leakage decreases with increasing ZrO2 capping layer thickness, demonstrating the effectiveness of the capping layer in improving leakage.
[0073] exist Figures 3 to 6 In the described embodiments, by making the capping layer rich in zirconium (or Figure 5 In some embodiments, the coating layer 12 is deposited in a single deposition chamber of a continuous deposition process. Zr-rich and 16 Zr-richThe ratio of zirconium and hafnium precursors is appropriately changed during the deposition of zirconium (ie, a higher zirconium precursor / hafnium precursor ratio during zirconium deposition), and during the deposition of the insulator layer 14 HZO The zirconium precursor / hafnium precursor ratio is reduced during the Figure 5 In the embodiment of the present invention, the ZrO2 cover layer 12 ZrO and 16 ZrO During the deposition of the HZO layer 14, the supply of the hafnium precursor may be completely stopped. The deposition chamber may be, for example, a chemical vapor deposition (CVD) chamber or a physical vapor deposition (PVD) chamber. Although from a manufacturing perspective, it is more convenient to use a single deposition chamber to deposit the capping layer and the HZO insulator layer 14. HZO It is possible, but optional, to use different deposition chambers to deposit the capping layer and the batch of HZO insulator layers 14 separately. HZO .
[0074] See now Figure 7 In some embodiments, doping with a dopant is employed to obtain lower and upper capping layers having a desired high tetragonal phase percentage (eg, greater than or equal to 70%). Figure 7 The MIM structure is similar to Figure 3 The structure includes a HZO insulator layer 14 sandwiched therebetween. HZO The lower metal 10 and the upper metal 18. However, in Figure 7 In the embodiment of the present invention, the lower cover layer includes a doped HZO cover layer 12 d , doped HZO cap layer 12 d The lower doped HZO cap layer 12 is doped with d Similarly, the upper cap layer includes a doped HZO cap layer 16 d , doped HZO cap layer 16 d The upper doped HZO cap layer 16 is doped with d The dopant with a tetragonal phase percentage of at least 80% is used. The dopant used may be, for example, silicon (Si), germanium (Ge), aluminum (Al), yttrium (Y), scandium (Sc), gadolinium (Gd) or a combination thereof. Table 1 provides the HZO stable phases expected to be achieved by the minimum doping concentrations (expressed as percentages) of the aforementioned different dopants. As previously mentioned, the stable cubic phases obtainable using Y, Sc or Gd are specific examples of tetragonal phases. The minimum doping concentration values listed in Table 1 are theoretical estimates, and in practice lower concentrations (e.g., close to about 5% to 10%) may be sufficient to obtain the lower doped HZO cap layer 12 d and the upper doped HZO capping layer 16 dThe lower HZO capping layer 12 may be doped d and the upper doped HZO capping layer 16 d The different doping levels of the HZO capping layer 12 are experimentally tested (by performing XRD, EBSD or other characterization methods) to determine the appropriate doping level according to the experiment to obtain the desired tetragonal phase of the aforementioned layers. In addition, it should be understood that Table 1 provides some exemplary suitable dopants, and other dopant types may also be suitable for doping the HZO capping layer 12. d and 16 d To obtain the desired tetragonal phase. Figure 7 An example of describing the ferroelectric insulator layer 14 HZO It is HZO, and the lower doped cap layer 12 d and the upper doped cap layer 16 d Also HZO, but more generally this doping can be configured to obtain other types of ferroelectric materials (such as Hf 1- x Zr x O2, SrBi2Ta2O9, PbZr x Ti 1-x O3 or BaTiO3) of the MIM structure of the tetragonal lower and upper covering layers.
[0075] Table 1
[0076] Dopant Stable phase Minimum doping concentration Silicon (Si) Tetragonal lattice phase 11% Germanium (Ge) Tetragonal lattice phase 19% Aluminum (Al) Tetragonal lattice phase 11% Yttrium (Y) cube 11% Scandium (Sc) cube 13% Gadolinium (Gd) cube 10%
[0077] See now Figure 8 , through a flow chart presenting manufacturing e.g. Figures 1 to 3 , Figure 5 or Figure 7 illustrative example of a method for forming a MIM structure. In step 30, a lower (or first) metal 10 is formed. In some embodiments, the lower metal 10 may be deposited as, for example, a conductive material, such as TiN, TaN, an elemental metal (e.g., Ti, Al, W, Pt, Mo, etc.) or an alloy thereof. The lower metal 10 may be formed, for example, by physical vapor deposition (PVD), atomic layer deposition (atomic layer deposition, ALD), electrolysis, or other suitable techniques. In some embodiments of manufacturing a MIM structure during back-end process (BEOL) processing, the lower metal 10 may include a patterned metallization layer of a metallization stack formed during BEOL processing. In such an embodiment, step 30 may involve depositing a capping metal layer on an underlying intermetal dielectric (IMD) material and forming a patterned metallization layer by patterned etching using lithography techniques to form a patterned metallization layer including the lower metal 10.
[0078] In step 32, a lower (or first) capping layer is formed, for example, by PVD, ALD, chemical vapor deposition (CVD), or another suitable deposition technique. The specific formation method depends on the type of capping layer. For example, in order to achieve the formation Figure 3 The MIM structure of the embodiment is appropriately formed by depositing HZO having an appropriately high number of zirconium molecules to form the lower cover layer 12 Zr-rich , as mentioned above Figure 3 In order to achieve the formation Figure 5 The MIM structure of the embodiment, the lower cover layer 12 ZrO It is suitably formed by depositing ZrO2. Figure 7 The MIM structure of the embodiment, the lower cover layer 12 d Suitably the HZO is formed doped with a tetragonal phase inducing dopant.
[0079] In step 34, a high-k insulator layer is formed. For example, to achieve the formation Figure 3 , Figure 5 or Figure 7 In one embodiment of the MIM structure, the insulator layer is suitably formed as a HZO layer 14. HZO , for example by PVD, ALD, CVD or other suitable deposition technique.
[0080] In step 36, an upper (or second) capping layer is formed, for example, by PVD, ALD, CVD or other suitable deposition techniques. Similar to step 32, the specific formation method depends on the type of the capping layer.
[0081] In some embodiments, steps 32, 34, and 36 can be performed by using the same deposition tool (e.g., the same PVD chamber, the same ALD chamber, or the same CVD chamber, etc.). In such embodiments, in the execution of the consecutive steps 32, 34, and 36, it is necessary to appropriately adjust, turn on or off the precursor flow. For example, in order to achieve Figure 3 The MIM structure of the embodiment can adjust the zirconium precursor flow and / or the hafnium precursor flow to control each layer (lower cover layer 12 Zr-rich、 Insulator layer 14 HZO and the upper covering layer 12 Zr-rich ) of zirconium molecules. Figure 5 The MIM structure of the embodiment can be in the cover layer 12 ZrO and 16 ZrO The zirconium precursor flow was shut off during the deposition of Figure 7 The MIM structure of the embodiment can be deposited at the lower doped capping layer 12 d During this period, the dopant precursor flow is turned on, and then, during the deposition of the HZO insulator layer 14 HZOThe dopant precursor flow is turned off at this time, and then the dopant precursor flow is turned on again to deposit the upper doped capping layer 16 d Using a single deposition tool to perform the three steps 32, 34, and 36 has some advantages, such as workflow efficiency and minimizing the possibility of surface contamination during wafer transfer between deposition tools. However, steps 32, 34, and 36 may also be performed by using two or even three different deposition tools.
[0082] In step 38, an upper (or second) metal 18 is formed. In some embodiments, the upper metal 18 may be deposited as, for example, a conductive material such as TiN, TaN, an elemental metal (e.g., Ti, Al, W, Pt, Mo, etc.), or an alloy thereof. The upper metal 18 may be formed, for example, by PVD, ALD, electrolysis, or other suitable techniques. In embodiments where the MIM structure is fabricated during BEOL processing, the upper metal 18 may include a second patterned metallization layer of a metallization stack formed during BEOL processing. The lower (or first) metal 10 formed in step 30 and the upper (or second) metal 18 formed in step 38 may be formed of the same material, or may be formed of different materials.
[0083] Next, see Figure 8 , the MIM structure manufacturing process may optionally include a thermal anneal 40. For example, as discussed above, the formation of a portion of the ferroelectric material may include a thermal anneal 40 to crystallize the material (e.g., HZO) into a ferroelectric orthorhombic phase. If the thermal anneal 40 is performed, it may be a dedicated thermal anneal specifically performed to crystallize the insulator layer into a ferroelectric orthorhombic phase (e.g., so that the orthorhombic phase percentage of the HZO insulator layer after annealing is at least 70%, so that the HZO insulator layer is ferroelectric). Alternatively, the thermal anneal 40 may be performed after step 38 in the process of the entire IC manufacturing workflow, and the further process includes sufficient heating to perform the desired crystallization in the orthorhombic phase. For example, as one of the non-limiting illustrative examples, the thermal anneal 40 may include a high temperature interval for depositing subsequent layers (e.g., silicon nitride, oxide insulators, etc.). Generally speaking, the thermal annealing 40 may be performed by rapid thermal annealing (RTA), forming gas annealing (forming gas annealing), high pressure annealing (HPA), or various combinations thereof.
[0084] Figures 1 to 3 , Figure 5 and Figure 7 The exemplary MIM structure includes a lower metal 10, a lower capping layer 12, and aZr-rich , 12 ZrO or 12 d , insulator layers 14, 14 FE or 14 HZO , upper covering layer 16, 16 Zr-rich , 16 ZrO or 16 d , and an upper metal layer 18. However, the MIM structure may optionally include additional layers.
[0085] See also Fig. 9 , for example, a diagram similar to Figure 1 The MIM structure of the MIM structure includes a lower metal 10, a lower cover layer 12, an insulator layer 14, an upper cover layer 16 and an upper metal layer 18. However, Fig. 9 The MIM structure also includes a high-k buffer layer 50 inserted between the lower metal 10 and the lower cap layer 12. For example, the high-k buffer layer 50 can increase the total thickness of the total dielectric inserted between the metal layers 10 and 18 to increase the breakdown voltage (VBD) of the MIM structure. As a more specific example, if the insulator layer 14 is a ferroelectric layer and the high-k buffer layer 50 is a non-ferroelectric layer, this combination can provide a larger insulator thickness to increase the VBD while keeping the ferroelectric layer 14 thinner to maintain a high switching speed of the FTJ or other ferroelectric device.
[0086] As previously mentioned, in some embodiments, the MIM structure may be formed during a BEOL process, for example as a BEOL capacitor or FTJ formed in a BEOL process.
[0087] See also Fig.10 and Fig.11 , two of the illustrative embodiments of examples of incorporating MIM structures into IC devices are depicted by way of cross-sectional views. A processed semiconductor wafer 60 is also depicted as an example. In front-end-of-line (FEOL) processing, a silicon wafer is processed through steps such as dopant diffusion, epitaxy, etching, and / or deposition controlled by lithography patterning to form electronic devices in a silicon wafer, silicon-on-insulator (SOI) wafer, or other semiconductor substrate to form a processed semiconductor wafer 60. Subsequently, BEOL processing forms a metallization stack on the IC chip or wafer 60. BEOL processing typically involves a repetitive process of depositing a blanket metal layer, performing lithography patterning on the blanket metal layer to form a patterned metallization layer, depositing an intermetal dielectric material (IMD), and repeating the aforementioned steps to form a continuous patterned metallization layer to form a metallization stack. Fig.10 and Fig.11Only the topmost metallization layer 62 of the metallization stack and the surrounding dielectric material 64 are shown by way of example. The surfaces of the metallization stack and the surrounding dielectric material 64 are suitably planarized, for example, by chemical-mechanical polishing (CMP).
[0088] Then, under-bump metallization (UBM) is formed to enable the IC to be bonded to another wafer, printed circuit board (PCB) or other electrical or electronic component via a ball grid array (BGA). The UBM includes a dielectric layer 66, and a MIM structure 70 is embedded in the dielectric material 66. In order to form a through hole 72 to contact the topmost patterned metallization layer 62, etching is controlled by lithography to pass through the dielectric material 66 to form a through hole opening, and the through hole opening is filled with an electrically conductive material (such as tungsten, as a non-limiting example). The MIM structure 70 is included to help provide noise fluctuation suppression for signals passing through the UBM. The UBM further includes a redistribution layer (RDL) 74 and (multiple) bonding pads 75 ( Fig.10 and Fig.11 A bonding pad 75 is shown respectively, and a redistribution layer (RDL) 74 and the bonding pad 75 are coated with another dielectric layer 76 and a passivation layer 78 .
[0089] exist Fig.10 In the illustrative example of FIG. 1 , etch openings are defined in dielectric layer 76 and passivation layer 78 by lithography techniques to bond exemplary bonding bumps (i.e., balls) 80 to exemplary bonding pads 75. Prior to bonding bonding bumps 80, an optional interface material 82 (e.g., pre-solder, flux material, or organic solderability preservative, etc.) may be applied to bonding pads 75. In a general sequence, bonding bumps 80 include solder and are heated to form a bond.
[0090] exist Fig.11 In addition to forming an additional polyimide layer 84 on the passivation layer 78, Fig.11 The UBM for the example is similar to Fig.10 The polyimide layer 84 may serve as, for example, a solder mask or the like.
[0091] It should be understood that Fig.10 and Fig.11The exemplary noise fluctuation suppression application of the MIM structure is only a non-limiting illustrative example. More generally, the MIM structure of the present disclosure can be employed in any application using a MIM structure, and the embodiments using a ferroelectric insulator layer can be employed in any other application of FTJ, FE-RAM or ferroelectric MIM structure.
[0092] In the following, some further embodiments are described.
[0093] In a non-limiting illustrative embodiment, a method for manufacturing a metal-insulator-metal (MIM) device is disclosed. The method includes: forming a first capping layer on a first metal, wherein the first capping layer includes a composition including at least zirconium and oxygen and having a tetragonal lattice phase; forming Hf on the first capping layer; 1-x Zr x O2 insulator layer; in Hf 1-x Zr x A second capping layer is formed on the O2 insulator layer, and the second capping layer includes a composition including at least zirconium and oxygen and having a tetragonal lattice phase; and a second metal is formed on the second capping layer. In some embodiments, the tetragonal phase percentage of the first capping layer is at least 80%, and the tetragonal phase percentage of the second capping layer is at least 80%. In some embodiments, Hf 1-x Zr x The orthorhombic lattice phase percentage of the O2 insulator layer is at least 70%, so that the Hf 1-x Zr x The O2 insulator layer is a ferroelectric. In some embodiments, the first capping layer includes Hf 1-x Zr x O2 composition, and Hf 1-x Zr x O2 composition ratio Hf 1-x Zr x The O2 insulator layer is richer in zirconium; and the second capping layer includes Hf 1-x Zr x O2 composition, and Hf 1-x Zr x O2 composition ratio Hf 1-x Zr x The O2 insulator layer is richer in zirconium. In some embodiments, the first capping layer comprises ZrO2 and the second capping layer comprises ZrO2. In some embodiments, the first capping layer comprises Hf doped with a dopant. 1-x Zr x O2 composition, and the second capping layer includes Hf doped with the dopant 1-x Zr xO2 composition; and the dopant makes the tetragonal phase percentage of the first capping layer at least 80%, and the dopant makes the tetragonal phase percentage of the second capping layer at least 80%. In some embodiments, the dopant includes silicon (Si), germanium (Ge), aluminum (Al), yttrium (Y), scandium (Sc), gadolinium (Gd), or a combination thereof. In some embodiments, Hf 1-x Zr x O2 insulator layer, the Hf of the first cap layer 1-x Zr x O2 composition and Hf of the second capping layer 1-x Zr x O2 compositions have the same number of zirconium molecules x. In some embodiments, the first capping layer and the Hf 1-x Zr x The ratio of the thickness of the O2 insulator layer is 0.1 or less, and the second cap layer and the Hf 1-x Zr x The ratio of the thickness of the O2 insulator layer is 0.1 or less. In some embodiments, the thickness of the first capping layer is less than the thickness of the second capping layer. In some embodiments, the method further includes forming a buffer dielectric layer on the first metal to form the first capping layer on the buffer dielectric layer before forming the first capping layer on the first metal.
[0094] In a non-limiting illustrative embodiment, a method of manufacturing a metal-insulator-metal (MIM) device is disclosed. The method includes: forming a first capping layer on a first metal, wherein the first capping layer includes a dielectric material having a tetragonal phase percentage of at least 80%; forming a second capping layer on the insulator layer, wherein the second capping layer includes a dielectric material having a tetragonal phase percentage of at least 80%; and forming a second metal on the second capping layer. In some embodiments, the insulator layer includes a ferroelectric phase. In some embodiments, the insulator layer includes a dielectric material selected from Hf 1-x Zr x O2, SrBi2Ta2O9, PbZr x Ti 1-x In some embodiments, the insulator layer comprises a ternary or quaternary oxide having a ferroelectric orthorhombic lattice phase, the percentage of the ferroelectric orthorhombic lattice phase in the insulator layer is at least 70%, the first capping layer comprises a ternary or quaternary oxide doped with a dopant, the second capping layer comprises a ternary or quaternary oxide doped with a dopant, and the dopant makes the first capping layer have a tetragonal phase percentage of at least 80%, and makes the second capping layer have a tetragonal phase percentage of at least 80%. In some embodiments, the insulator layer comprises a ferroelectric Hf 1-x Zr x O2 composition, and the first covering layer comprises ZrO2 or Hf 1-x Zrx O2 composition, and Hf 1-x Zr x O2 composition is richer in zirconium than the insulator layer, and the second capping layer comprises ZrO2 or Hf 1-x Zr x O2 composition, and Hf 1-x Zr x The O2 composition is richer in zirconium than the insulator layer. In some embodiments, a ratio of the thickness of the first capping layer to the insulator layer is 0.1 or less, and a ratio of the thickness of the second capping layer to the insulator layer is 0.1 or less. In some embodiments, the method further includes forming a buffer dielectric layer on the first metal to form the first capping layer on the buffer dielectric layer before forming the first capping layer on the first metal.
[0095] In a non-limiting illustrative embodiment, a metal-insulator-metal (MIM) device includes: a first metal; a first capping layer disposed on the first metal, the first capping layer comprising a dielectric material having a tetragonal lattice phase; an insulator layer disposed on the first capping layer; a second capping layer disposed on the insulator layer, the second capping layer comprising a dielectric material having a tetragonal lattice phase; and a second metal disposed on the second capping layer. In some embodiments, the insulator layer comprises a ferroelectric Hf 1-x Zr x O2 material, and the first capping layer contains ZrO2 or Hf 1-x Zr x O2 composition, and Hf 1-x Zr x O2 composition is richer in zirconium than the insulator layer, and the second capping layer comprises ZrO2 or Hf 1-x Zr x O2 composition, and Hf 1-x Zr x The O2 composition is richer in zirconium than the insulator layer.
[0096] The foregoing summarizes the features of several embodiments so that those skilled in the art can better understand the aspects of the present disclosure. Those skilled in the art should understand that they can easily use the present disclosure as a basis for designing or modifying other processes and structures to achieve the same purposes and / or achieve the same advantages of the embodiments introduced herein. Those skilled in the art should also recognize that such equivalent constructions do not depart from the spirit and scope of the present disclosure, and that those skilled in the art can make various changes, substitutions and modifications without departing from the spirit and scope of the present disclosure.
Claims
1. A method of manufacturing a metal-insulator-metal device, It is characterized in that include: forming a first capping layer on a first metal, wherein the first capping layer comprises a composition including at least zirconium and oxygen and having a tetragonal lattice phase; A Hf 1-x Zr x O 2 Insulator layer; In this Hf 1-x Zr x O 2 forming a second capping layer on the insulator layer, wherein the second capping layer comprises a composition at least containing zirconium and oxygen and having the tetragonal lattice phase; and A second metal is formed on the second capping layer.
2. The method according to claim 1, It is characterized in that The Hf 1-x Zr x O 2 The insulator layer has an orthorhombic lattice phase percentage of at least 70%, so that the Hf 1-x Zr x O 2 The insulator layer is a ferroelectric.
3. The method according to claim 1, It is characterized in that The first covering layer includes a Hf 1-x Zr x O 2 composition, and the Hf 1-x Zr x O 2 The composition is higher than that of Hf 1-x Zr x O 2 The insulator layer is richer in zirconium; and The second covering layer includes a Hf 1-x Zr x O 2 composition, and the Hf 1-x Zr x O 2 The composition is higher than that of Hf 1-x Zr x O 2 The insulator layer is richer in zirconium.
4. The method according to claim 1, It is characterized in that The first capping layer comprises ZrO 2 , and the second covering layer comprises ZrO 2 .
5. The method according to claim 1, It is characterized in that The Hf 1-x Zr x O 2 The insulating layer, the first cover layer, a Hf 1-x Zr x O 2 Composition and the second covering layer of Hf 1-x Zr x O 2 The compositions all have the same number x of zirconium molecules.
6. A method of manufacturing a metal-insulator-metal device, It is characterized in that include: forming a first capping layer on a first metal, wherein the first capping layer comprises a dielectric material having a tetragonal phase percentage of at least 80%; forming an insulator layer on the first covering layer; forming a second covering layer on the insulator layer, wherein the second covering layer comprises a dielectric material having a tetragonal phase percentage of at least 80%; as well as A second metal is formed on the second capping layer.
7. The method according to claim 6, It is characterized in that The insulator layer includes a selected from Hf 1-x Zr x O 2 、SrBi 2 Ta 2 O 9 、PbZr x Ti 1-x O 3 , or BaTiO 3 Groups composed of.
8. The method according to claim 6, It is characterized in that The insulator layer includes a ferroelectric Hf 1-x Zr x O 2 composition, and the first covering layer comprises ZrO 2 or Hf 1-x Zr x O 2 composition, and the Hf 1-x Zr x O 2 The composition is richer in zirconium than the insulator layer, and the second capping layer comprises ZrO 2 or Hf 1-x Zr x O 2 composition, and the Hf 1-x Zr x O 2 The composition is richer in zirconium than the insulator layer.
9. The method according to claim 6, It is characterized in that Further including: Before forming the first capping layer on the first metal, a buffer dielectric layer is formed on the first metal to form the first capping layer on the buffer dielectric layer.
10. A metal-insulator-metal device, It is characterized in that include:
1. First metal; a first capping layer disposed on the first metal, wherein the first capping layer comprises a dielectric material having a tetragonal lattice phase; an insulator layer disposed on the first covering layer; a second covering layer disposed on the insulator layer, wherein the second covering layer comprises a dielectric material having the tetragonal lattice phase; as well as A second metal is disposed on the second covering layer.