Battery management system, battery pack comprising same, and method for establishing charging protocol of lithium secondary battery

By measuring voltage and calculating internal resistance values, drawing internal resistance curves, and determining the limit charging state, the heating and internal resistance problems during fast charging in large-capacity battery cells are solved, and the charging protocol establishment and battery without the need for three-electrode singles are realized The identification of single-unit deterioration optimizes charging efficiency.

CN119096448APending Publication Date: 2024-12-06LG ENERGY SOLUTION LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380038989.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-11-08
Filing Date
2023-11-08
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

The prior art is difficult to reflect the heating and internal resistance during fast charging in large-capacity battery cells, and it is necessary to manufacture difficult three-electrode monomers to derive the charging protocol. It is difficult to deviate the battery cells due to the subjectivity of the experimenter. Establish a charging protocol with similar voltage curves in the case.

Method used

By measuring closed and open circuit voltages, calculating internal resistance values, drawing internal resistance curves, determining the limit charging state, establishing a charging protocol, and updating the protocol during repeated charging and discharging of the battery cell, reflecting the degree of deterioration of the battery cell.

Benefits of technology

A charging protocol is realized that the resistance of the large-capacity battery cell and the heating state during fast charging is derived without the need to manufacture a three-electrode single, the charging protocol is not destructively identified, and the charging protocol is updated to optimize the charging efficiency. .

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119096448A_ABST
    Figure CN119096448A_ABST
Patent Text Reader

Abstract

A method for establishing a charging protocol of a lithium secondary battery and a battery management system according to the present invention, in which, for a dual-electrode battery cell, a closed-circuit voltage (CCVSOCx) and an open-circuit voltage (OCVSOCx) according to a state of charge (SOCx) during charging with each charging current (I) are measured according to the following formula 1, and the closed-circuit voltage (CCVSOCx) and the open-circuit voltage (OCVSOCx) are measured according to the state of charge (SOCx) during charging with each charging current (I). And determining a limit state of charge corresponding to each charging current from an internal resistance curve by collecting the internal resistance curve drawing the internal resistance value (RSOCx) according to the state of charge for each charging current (I). [Formula 1] An internal resistance value (RSOCx) according to a state of charge = (CCVSOCx-OCVSOCx) / I.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application claims the benefit of priority of Korean Patent Application No. 10-2022-0147912, filed on November 8, 2022.

[0002] The present invention relates to a method for establishing a fast charging protocol that reflects heat generation and internal resistance caused by charging and discharging of a large-capacity battery cell, a battery management system capable of establishing such a fast charging protocol, and a battery pack including the battery management system. Background Art

[0003] In recent years, the demand for portable electronic products such as laptop computers and portable phones has increased dramatically, and the demand for electric carts, electric wheelchairs, and electric bicycles has also increased, and research on high-performance batteries that can be repeatedly charged and discharged has also been actively conducted. In recent years, with the gradual depletion of carbon energy and the increase in environmental awareness, the demand for hybrid electric vehicles (HEV) and electric vehicles (EV) has also been increasing worldwide. Therefore, more and more attention and research are focused on vehicle batteries, which are core components of HEVs and EVs, and there is an urgent need to develop fast charging technology that can quickly recharge batteries. Fast charging is a crucial capability, especially for EVs without additional energy sources.

[0004] The process of charging a battery involves introducing an electric current into the battery to accumulate charge and energy, and this process must be carefully controlled. Generally speaking, excessive charging current (C-rate) or charging voltage can permanently degrade the performance of the battery and eventually cause the battery to fail completely, or cause sudden failures such as leakage or explosion of highly corrosive chemicals.

[0005] When charging a battery with a constant current, if the current rate of the charging current is low, it will take a long time to fully charge the battery. On the other hand, if the current rate of the charging current is too high, the battery will age quickly. Therefore, during constant current charging, the current rate of the charging current needs to be gradually adjusted according to the state of the battery.

[0006] A charging map with a "multi-stage constant current charging protocol" is typically utilized to adjust the current rate during constant current charging in a stepwise manner. The charging map includes at least one data array in which the relationship between multiple current rates and multiple transition conditions is recorded. Whenever each transition condition is met, the following current rate sequence may be provided to the battery as the charging current. The current rate (also referred to as a "C rate") is the charging current divided by the maximum capacity of the battery, using the unit "C".

[0007] Conventionally, in order to derive such a multi-stage constant current charging protocol, a 50 mAh single-cell type three-electrode cell is manufactured, and the state of charge (SOC) at which lithium deposition occurs at the negative electrode for each charging current is set as the charging limit.

[0008] However, three-electrode cells are difficult to manufacture and require dedicated chargers and dischargers for charging and discharging, so there are many constraints such as the integrity of the three-electrode cells, the manufacturing time of the three-electrode cells, and the preparation of dedicated chargers and dischargers. In addition, when the extreme charging states identified in these three-electrode cells are applied to large-capacity battery cells with a capacity range of 40-200Ah, there is no technology that reflects the resistance of the large-capacity battery cells or the heat generation during fast charging. In addition, the method of establishing a charging protocol using a three-electrode cell is subject to the subjectivity of the experimenter because as the charging current becomes smaller and the negative electrode composition becomes more conducive to fast charging, the lithium deposition area is no longer clearly distinguished, so it is difficult to establish a charging protocol that exhibits a similar voltage curve in the case of deviations in the battery cells.

[0009] Therefore, it is necessary to develop a technology that does not require the manufacture of three-electrode cells and derive a charging protocol that can produce similar voltage curves in the presence of battery cell differences while taking into account the resistance of large-capacity battery cells and the heating state during fast charging. Summary of the invention

[0010] [Technical issues]

[0011] The present invention is designed to solve the above-mentioned problems and aims to provide a method for deriving a charging protocol that does not require pre-manufacturing of a three-electrode cell to derive a limit charging state through a charging current, a method for deriving a charging protocol that takes into account the resistance of a large-capacity battery cell and the heating state during rapid charging, and a battery management system capable of establishing such a charging protocol and a battery pack equipped with the system.

[0012] [Technical solution]

[0013] According to one embodiment of the present invention, a battery management system is provided. The battery management system includes: a measuring unit configured to measure, for a dual-electrode battery cell having a positive electrode and a negative electrode, a closed-circuit voltage (CCV) according to a state of charge (SOCx) when charged with different charging currents (I). SOCx ) and open circuit voltage (OCV SOCx ); a memory unit configured to collect and store an internal resistance curve, the internal resistance curve is obtained by dividing the measured CCV SOCx and OCV SOCx Substitute into the following formula 1 to calculate the internal resistance value (R SOCx) to plot the internal resistance value (R) according to the charging state for each charging current (I) SOCx ); and a control unit, which is configured to determine the limit charging state corresponding to each charging current according to the internal resistance curve and establish a charging protocol based on this.

[0014] [Formula 1]

[0015] According to the internal resistance value (R SOCx ) = (CCV SOCx -OCV SOCx ) / I

[0016] In an exemplary embodiment, the control portion may be configured to determine, as the limit charge state, a state of charge (SOCx) value at a point where a graph shape of the internal resistance curve changes from a flat shape to a downward trend.

[0017] In an exemplary embodiment, the control portion may be configured to re-establish the charging protocol by periodically deriving a new limit state of charge corresponding to each charging current during repeated charging and discharging of the battery cells.

[0018] In an exemplary embodiment, the battery management system further includes a connection portion configured to be connected with a charging device to supply a charging current to the battery cell according to a charging protocol established by the control portion.

[0019] In an exemplary embodiment, the measuring part is configured to measure state information of the battery cell, the state information including at least one of a voltage and a charging state of the battery cell.

[0020] In an exemplary embodiment, the charging current (I) is selected from a range of 0.33C to 6.0C.

[0021] According to another exemplary embodiment of the present invention, a battery pack including the above-mentioned battery management system is provided.

[0022] In an exemplary embodiment, the battery pack may include a plurality of battery cells having a capacity of 40 to 200 Ah.

[0023] According to another exemplary embodiment of the present invention, a method for establishing a charging protocol for a lithium secondary battery is provided. The method for establishing a charging protocol for a lithium secondary battery comprises: (a) for a dual-electrode battery cell having a positive electrode and a negative electrode, when charging with different charging currents (I), respectively measuring a closed circuit voltage (CCV) according to a state of charge (SOCx); SOCx ) and open circuit voltage (OCV SOCx );

[0024] (b) The measured CCV SOCx and OCV SOCxSubstitute into the following formula 1 to calculate the internal resistance value (R SOCx ), and collect the internal resistance curve, which plots the internal resistance value (R) according to the charging state for each charging current (I) SOCx );as well as

[0025] (c) determining the limit charging state corresponding to each charging current based on the collected internal resistance curve;

[0026] [Formula 1]

[0027] According to the internal resistance value (R SOCx ) = (CCV SOCx -OCV SOCx ) / I

[0028] In the exemplary embodiment, in process (c), the limit state of charge is determined as a state of charge (SOC) value at a point where the graph shape of the internal resistance curve changes from a flat shape to a downward trend.

[0029] In an exemplary embodiment, the dual electrode battery cell has a capacity of 40 to 200 Ah.

[0030] In an exemplary embodiment, in process (a), the charging current (I) is selected from a range of 0.33C to 6.0C.

[0031] In an exemplary embodiment, in process (a), the charging current (I) is set at intervals of 0.1C to 1.0C.

[0032] The method of establishing a charging protocol according to an exemplary embodiment further includes mapping the charging protocol based on the limit charging state according to the charging current, wherein the mapping process maps so that each charging current is charged with a corresponding charging current to reach the limit charging state, but as the charging state increases, the charging current decreases.

[0033] [Beneficial Effects]

[0034] The battery management system and the charging protocol setting method according to the present invention have the effect of providing a charging protocol that reflects the resistance and heat generation directly from a large-capacity battery cell without manufacturing a three-electrode cell that is difficult to manufacture.

[0035] Furthermore, the battery management system and the charging protocol setting method according to the present invention have the effect of non-destructively identifying the degree of degradation of the battery cells even during operation of the battery cells, and updating the charging protocol to reflect the degradation of the battery cells.

[0036] Furthermore, the battery management system and charging protocol setting method according to the present invention can derive a limit charging state even at a charging current as low as 1.0C, thereby providing a charging protocol that is conducive to fast charging. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1 is a schematic diagram illustrating an exemplary configuration of a battery pack including a battery management system according to an exemplary embodiment of the present invention.

[0038] Figure 2 is a diagram schematically illustrating a battery pack including a battery management system according to an exemplary embodiment of the present invention.

[0039] Figure 3 is an internal resistance curve of charging current (I) collected according to an exemplary embodiment of the present invention.

[0040] Figure 4 is a graph showing limiting state of charge for charging currents derived according to the present invention and prior art methods of establishing a charging protocol.

[0041] Figure 5 is a SOC-OCV curve of each of the battery cells charged using the charging protocol established according to the present invention and the prior art method.

[0042] Figure 6 is a flowchart of a method of establishing a charging protocol for a lithium secondary battery according to an exemplary embodiment of the present invention.

[0043] Figure 7 is an internal resistance curve of a charging current (I) of a degraded battery cell after 500 charge and discharge cycles collected according to an exemplary embodiment of the present invention.

[0044] Figure 8 It is shown Figure 4 The charging current (I) is the limit of the charging state and Figure 7 Graph of the charging current (I) and the limit state of charge of a degraded battery cell. DETAILED DESCRIPTION

[0045] The terms and words used in this specification and claims should not be interpreted in their ordinary or dictionary meanings, but should be interpreted according to the meanings and concepts consistent with the technical ideas of the present invention, based on the principle that the inventor can appropriately define the concepts of the terms to best describe his invention.

[0046] Therefore, it should be understood that the embodiments described herein and the configurations shown in the accompanying drawings are merely the most preferred embodiments of the present invention and do not represent the entire technical concept of the present invention, and that various equivalents and modifications that can replace them may exist when the application is submitted.

[0047] Furthermore, in describing the present invention, if it is determined that a detailed description of a related known configuration or feature would obscure the essence of the present invention, such a detailed description will be omitted.

[0048] Throughout the specification, when it is said that a part “includes” components, it means that the part may further include other components, rather than excluding other components, unless explicitly stated otherwise.

[0049] In addition, terms such as a control unit used in this specification refer to a unit that processes at least one function or operation, which can be implemented by hardware or software, or a combination of hardware and software.

[0050] Furthermore, throughout the specification, when it is said that a part is “connected” to another part, this includes not only “direct connection” but also “indirect connection” with other elements therebetween.

[0051] The preferred embodiments of the present invention will be described in detail below with reference to the accompanying drawings.

[0052] Figure 1 is a schematic diagram illustrating an exemplary configuration of a battery pack including a battery management system according to an exemplary embodiment of the present invention. Figure 2 is a diagram schematically illustrating an exemplary configuration of a battery pack including a battery management system according to an exemplary embodiment of the present invention.

[0053] See also Figure 1 The battery pack 1 may include a battery cell 10 and a battery management system 100. The battery management system 100 is a battery management system that monitors the voltage, current, temperature, etc. of the battery cell 10 and controls and manages them to prevent overcharging, overdischarging, etc.

[0054] Here, the battery cell 10 is a double-electrode battery cell having a negative electrode and a positive electrode, which is a single physically separable cell. In one example, a pouch-type lithium polymer cell may be regarded as the battery cell 10. In addition, the battery cell 10 may be a large-capacity battery cell having a capacity in the range of 40 to 200 Ah.

[0055] The battery pack 1 may also include a battery module including one or more battery cells 10 connected in series and / or in parallel.

[0056] As the positive electrode active material constituting the positive electrode of the battery cell 10, a lithium-containing transition metal oxide can be used. For example, LiCoC2, LiNiO2, LiMnO2, LiMn2O4, Li(Ni a Co b Mn c )O2(0 <a<1,0<b<1,0<c<1,a+b+c=1)、Li x (Ni a Co b Mn c Ald )O2 (0.5 < x < 1.3, 0.6 < a < 1, 0 < b < 0.2, 0 < c < 0.1, 0 < d < 0.1, a + b + c + d = 1), LiNi 1-y Co y O2, LiCo 1-y Mn y O2, LiNi 1-y Mn y O2 (0 ≤ y < 1), Li(Ni a Co b Mn c )O4 (0 < a < 2, 0 < b < 2, 0 < c < 2, a + b + c = 2), LiMn 2-z Ni z O4, LiMn 2-z Co z O4 (0 < z < 2), LiCoPO4, LiFePO4, or two or more of these. In addition to these oxides, sulfides, selenides, halides, etc. may also be used.

[0057] As the negative electrode active material constituting the negative electrode, carbon-based materials such as graphite and activated carbon, or materials such as silicon oxide (SiO x ) can be used.

[0058] For the negative electrode active material using a carbon-based material, the potential is very low and similar to that of lithium. Therefore, an increase in resistance or an increase in current will cause lithium deposition, which forms a metal coating film on the negative electrode due to the properties of lithium ions. Therefore, a safe charging protocol is established by defining the charging state at which lithium deposition occurs on the negative electrode as the limit charging state.

[0059] When establishing a fast charging protocol, the present invention derives the lithium deposition point for setting the limit charging state from the internal resistance curve that plots the internal resistance values according to the charging state of the battery cell.

[0060] Referring to Figure 1 , the battery management system 100 according to the present invention may include a measurement unit 110, a memory unit 120, and a control unit 130.

[0061] In Figure 2 's embodiment, the battery management system 100 according to the present invention may further include a connection unit 140 configured to connect to a charging device 200 that can supply a charging current to the battery cell according to the charging protocol established by the control unit 130.

[0062] The charging device 200 may be connected to the battery pack 1. And the charging device 200 connected to the battery pack 1 may supply a charging current to the battery cell 10 according to the charging protocol established by the control unit 130 for the battery cell 10.

[0063] Also, the battery management system 100 may control the operation of the switch part SW to control the charge and discharge of the battery cell 10 and / or the battery module.

[0064] The measuring unit 110 is configured to measure the state information of the battery cell, which includes at least one of the voltage and the state of charge of the battery cell 10. According to an embodiment of the present invention, the measuring unit 110 is configured to measure the closed circuit voltage (CCV) according to the state of charge (SOCx). SOCx ) and the open circuit voltage (OCV SOCx ), in order to calculate the internal resistance of the battery cell 10. The closed circuit voltage (CCV) measured by the measuring unit 110 SOCx ) and open circuit voltage (OCV SOCx ) is the basic data for calculating the internal resistance value under the corresponding charging state (SOCx).

[0065] The measuring unit 110 is configured to measure the closed circuit voltage (CCV) of the battery cell 10 according to the charging state at different charging currents (I). SOCx ) and open circuit voltage (OCV SOCx ). In an exemplary embodiment, the charging current (I) may be selected multiple times within the range of 0.2C to 6C, more specifically, 0.33C to 6C, and more specifically, 0.5C to 5C. In addition, the interval of the charging current (I) may be set to an interval of 0.1C to 1.0C. For example, for the battery cell 10, various values ​​of the charging current (I) are set at intervals of 0.25C, such as 0.25C-0.5C-0.75C…-2.75C-3.0C, charging is performed to reach SOC 100%, and the measuring unit 110 is configured to measure the closed circuit voltage (CCV) according to the state of charge (SOCx) at each charging current (I). SOCx ) and open circuit voltage (OCV SOCx ), where the closed circuit voltage (CCV SOCx ) and open circuit voltage (OCV SOCx ) can be set at intervals of SOC 2.5%, at intervals of SOC 5%, or at intervals of SOC 10%.

[0066] The memory unit 120 is configured to store the CCV measured by the measuring unit 110 SOCx and OCV SOCx Substitute into the following formula 1 to calculate the internal resistance value R according to the charging state SOCx SOCx , and for each charging current I, collect and store the internal resistance value R according to the charging state SOCx The internal resistance curve.

[0067] [Formula 1]

[0068] According to the internal resistance value (R SOCx ) = (CCV SOCx -OCV SOCx ) / I

[0069] Since the difference between the closed-circuit voltage and the open-circuit voltage is caused by the voltage drop across the internal resistance, the actual internal resistance of the battery cell can be calculated by dividing the difference between the closed-circuit voltage and the open-circuit voltage by the (fast) charging current.

[0070] At this time, the closed circuit voltage (CCV SOCx ) within 1 second to 30 seconds, or 1 second to 15 seconds, or 1 second to 10 seconds, or 2 seconds to 9 seconds from the start time of measurement. SOCx ).

[0071] The control section 130 is configured to determine a limit charging state corresponding to each charging current (I) stored in the memory section according to the internal resistance curve, and establish a charging protocol based thereon.

[0072] The control unit 130 of the present invention may be configured to determine the value of the state of charge (SOCx) at a point where the shape of the graph in the internal resistance curve changes from a flat shape to a downward trend as the limit state of charge.

[0073] Figure 3 1 shows an internal resistance curve according to a state of charge (SOCx) according to an exemplary embodiment of the present invention, which is obtained by measuring a closed circuit voltage (CCV) according to a state of charge (SOCx) through a charging current (I) respectively. SOCx ) and the open circuit voltage (OCV SOCx ), calculate the internal resistance value (R SOCx ) and plotting the internal resistance value (R SOCx ) and export.

[0074] refer to Figure 3 , for a charging current (I) range of 0.5C to 3C, an internal resistance curve plotting the internal resistance value according to the charging state is shown for various charging current values ​​set at intervals of 0.25C.

[0075] It can be observed from these internal resistance curves that there is a point in the graph where the arc becomes flat and then drops sharply. That is, for almost the entire charging current range (1C to 3C), there is a constant internal resistance value of about 1.4mΩ, and then the internal resistance value changes to a downward trend, which can be considered as the point where lithium deposition occurs.

[0076] In the case of lithium deposition, lithium ions are inserted into the graphite layer of the negative electrode during the charging rest period and are coupled with the lithium deposition part at the same time. In other words, in the charging state interval before lithium deposition occurs, lithium ions are inserted into the negative electrode and exist in the form of series resistance, but in the charging state interval after lithium deposition occurs, the situation of lithium ions inserted into the negative electrode and the situation of lithium deposition occur to form a parallel resistance, resulting in a decrease in the overall resistance. Therefore, in the internal resistance curve according to the charging state, the decrease in the internal resistance value is an indicator that lithium deposition has occurred.

[0077] Therefore, the control unit 130 of the present invention determines the value of the state of charge (SOCx) at the point where the graph of the internal resistance curve of the charging current changes from a flat trend to a downward trend as the limit charging state. After the control unit 130 determines the limit charging state corresponding to each charging current I as described above, the control unit 130 can establish a charging protocol based on this.

[0078] The battery management system 100 according to the present invention has the effect that the measuring part 110 , the memory part 120 , and the control part 130 can charge the battery cells according to the charging protocol reflecting the resistance of the large-capacity battery cells 10 and the heat generated by rapid charging.

[0079] At the same time, the control unit 130 may be configured to re-establish the charging protocol by periodically deriving a new limit state of charge corresponding to each charging current during repeated charging and discharging of the battery cells. This is to reflect the aging of the battery cells in repeated charging and discharging cycles.

[0080] For example, the control unit 130 controls the measuring unit 110 to measure the closed circuit voltage (CCV) according to the state of charge (SOCx) for each 100 cycles when the battery cells are charged with different charging currents (I). SOCx ) and the open circuit voltage (OCV SOCx ), controls the memory unit 120 to pass the measured CCV SOCx and OCV SOCx Substitute the following formula 1 to calculate the internal resistance value (R SOCx ), controls the memory unit 120 to collect and store an internal resistance curve that plots the internal resistance value according to the charging state for each charging current I, and derives a new limit charging state corresponding to each charging current from the internal resistance curve stored in the memory unit 120, and based on the above, establishes a new charging protocol that reflects aging.

[0081] Therefore, the battery management system according to the present invention has the effect of non-destructively identifying the degree of aging of the battery cells even when the battery cells are in operation, and updating the charging protocol to reflect the aging of the battery cells.

[0082] Figure 6 is a flowchart of a method of establishing a charging protocol for a lithium secondary battery according to an exemplary embodiment of the present invention.

[0083] (a) For a two-electrode battery cell with a positive electrode and a negative electrode, the closed-circuit voltage (CCV) according to the state of charge (SOCx) is measured when charged at different charging currents (I). SOCx ) and open circuit voltage (OCV SOCx );

[0084] (b) The measured CCV SOCx and OCV SOCx Substitute the following formula 1 to calculate the internal resistance value (R SOCx ), and collect the internal resistance value (R) according to the charging state for each charging current (I) SOCx )’s internal resistance curve; and

[0085] (c) Determine the limit charging state corresponding to each charging current based on the collected internal resistance curve.

[0086] [Formula 1]

[0087] According to the internal resistance value (R SOCx ) = (CCV SOCx -OCV SOCx ) / I

[0088] When establishing a charging protocol according to the present invention, the limit state of charge may be a state of charge (SOC) value at a point where the shape of the internal resistance curve changes from flat to a downward trend.

[0089] And, in process (a), the charging current (I) may be set at a certain interval ranging from 0.2C to 6C, more specifically, from 0.33C to 6C, more specifically, from 0.5C to 5C. In this case, the interval may be from 0.1C to 1.0C.

[0090] In the prior art method of establishing a charging protocol, a three-electrode cell with a capacity of 50 mAh has been pre-manufactured to derive the limit charging state, and the lithium deposition point according to the negative electrode potential has been derived as the limit charging state, while the present invention does not require the manufacture of a three-electrode cell, and for a large-capacity two-electrode cell with a capacity of 40 to 200 Ah, the limit charging state can be derived directly by calculating the internal resistance value.

[0091] According to an exemplary embodiment, the method of establishing a charging protocol may further include mapping the charging protocol based on a limit charging state of the charging current.

[0092] The mapping process can make each charging current be mapped to charging with the corresponding charging current to reach the limit charging state, but the charging current decreases as the charging state increases. For example, if the limit charging state corresponding to the 3.0C charging current may be SOC 40%, the limit charging state corresponding to the 2.5C charging current may be SOC 45%, the limit charging state corresponding to the 2.0C charging current may be SOC 55%, and the limit charging state corresponding to the 5C charging current is SOC65%, then it can be mapped so that for SOC 40% or less, charging can be performed with a charging current of 3.0C, for SOC45% or less, charging can be performed with a charging current of 2.5C, for SOC 55% or less, charging can be performed with a charging current of 2.0C, and for SOC 65% and below, charging can be performed with a charging current of 1.5C.

[0093] Hereinafter, a battery management system of the present invention for deriving a limit charging state corresponding to a charging current and establishing a charging protocol according to the present invention will be described in detail using a specific example.

[0094] Example 1

[0095] For a battery cell with a capacity of 40Ah and a SOC of 2.5%, the battery cell is charged at a charging current of 0.5C. The measurement unit measures the closed circuit voltage (CCV) of the battery cell at the charging state interval of SOC 2.5%. SOCx ) and open circuit voltage (OCV SOCx ), and substitute the measurement result into the following formula 1 to calculate the internal resistance value in this charging state.

[0096] [Formula 1]

[0097] According to the internal resistance value (R SOCx ) = (CCV SOCx -OCV SOCx ) / I

[0098] Then, by plotting the charge state on the x-axis and the internal resistance on the y-axis, Figure 3 The internal resistance curve shown, which plots the internal resistance value according to the state of charge, is stored in the memory section.

[0099] This process is then repeated for each of the following charging currents: 0.75C, 1.0C, 1.25C, 1.5C, 1.75C, 2.0C, 2.25C, 2.5C, 2.75C, and 3.0C, and the internal resistance curve for each charging current is stored in the memory section.

[0100] Then, the control unit performs the control according to the Figure 3The internal resistance curve of the charging state is used to determine the charging degree when the shape of the graph changes from flat to a downward trend as the limit charging state of the charging current. The results are as follows Figure 4 And as shown in Table 1.

[0101] [Table 1]

[0102]

[0103] Comparative Example 1

[0104] Using a three-electrode monomer, a conventional method of establishing a charging protocol was used to perform charging and discharging at a temperature of 25 degrees Celsius to derive the limiting charge state of the charging current, and the results are shown in Tables 2 and Figure 4 In this case, the limit charge state is determined by measuring the negative electrode potential (CCV) according to the state of charge (SOC) of the three-electrode unit when charging at a charging current set at intervals of 0.25C in the range of 1.0C to 2.75C for a single cell of 50mAh, and determining the charge state at the point where the negative electrode potential begins to stabilize instead of decreasing as the limit charge state.

[0105] Comparative Example 2

[0106] The same method as in Comparative Example 1 was used to derive the limit charge state of the charging current, except that the temperature was set to 35 degrees Celsius, and the results are shown in Tables 2 and Figure 4 shown.

[0107] [Table 2]

[0108]

[0109] Will Figure 4 Comparing the results of Table 1 and Table 2, it can be seen that the value of the limit state of charge of the charging current according to the present invention is consistent with or similar to the value of the limit state of charge of the charging current derived using a conventional three-electrode cell at 35 degrees Celsius. Therefore, it can be confirmed that the limit state of charge of the charging current derived according to the present invention fully reflects the resistance of the large-capacity battery cell and the heat generated by rapid charging.

[0110] Experimental Example 1

[0111] The battery cell used in Example 1 was prepared (Preparation Example 1), and a battery cell in which the negative electrode composition was changed to provide excellent fast charging capability was prepared from the battery cell of Preparation Example 1 (Preparation Example 2).

[0112] For the battery cells of Preparation Example 1 and Preparation Example 2, a charging protocol was established by deriving the limit state of charge by the charging current in the same manner as in the example. As a result, a charging protocol was established in which the charging protocol of the battery cell of Preparation Example 1 required 28.4 minutes to charge (first charging protocol), and the charging protocol of the battery cell of Preparation Example 2 required 21.7 minutes to charge (second charging protocol).

[0113] For the battery cell of Preparation Example 1, charging was performed according to the first charging protocol, and the open circuit voltage according to the charging state was measured, and the results were as follows: Figure 5 For the battery cell of Preparation Example 2, charging was performed according to the second charging protocol, and the open circuit voltage according to the charging state was measured, and the results are as follows: Figure 5 shown.

[0114] See also Figure 5 It can be seen that the battery cell of Preparation Example 1 presents a similar voltage curve to the battery cell of Preparation Example 2. Therefore, it can be seen that the method for establishing a charging protocol according to the present invention has the effect of being able to establish a protocol using a similar charging state for battery cells with different electrode compositions.

[0115] Experimental Example 2

[0116] The same battery cell as that used in Example 1 was subjected to 500 cycles of charge and discharge, and for a battery cell (capacity: 40 Ah) that had undergone aging, an internal resistance curve according to the state of charge was derived under the same conditions and method, and the results are as follows: Figure 7 Then, in Figure 7 In the internal resistance curve shown in FIG. 1 , the state of charge at the point where the shape of the graph is flat and then decreases is determined as the limit state of charge for each charging current, and the limit state of charge of the charging current of the battery cell that has experienced aging is added to the limit state of charge of the charging current of the battery cell that has undergone aging. Figure 4 The figure shown in the figure is as follows Figure 8 shown.

[0117] Will Figure 7 and Figure 3 For comparison, an aged cell that has been subjected to 500 charge and discharge cycles and experienced aging has an increased internal resistance from about 1.4 mΩ to about 1.6 mΩ compared to a battery cell at the initial life (BOL) that has not been subjected to repeated charge and discharge (Example 1). This is considered to reflect aging due to repeated charge and discharge cycles. It was also found that the rate of increase in the internal resistance value varies depending on the charging current. In addition, in Figure 7 The x-axis coordinate (SOC) of the point where the arc in the figure flattens and starts to decline is Figure 3The x-axis coordinate of the point where the arc line in the middle figure flattens and starts to drop moves more to the left. It can be seen that in the cell where aging has progressed, the limit charge state of the charging current decreases.

[0118] Therefore, the charging protocol establishing method of the present invention and the battery management system according to the present invention are expected to have the effect of updating a new charging protocol reflecting the degradation of the battery cells during operation.

[0119] Example 2

[0120] A battery cell (capacity: 40 Ah) of the same specification as the battery cell used in Example 1 was connected to an electrochemical charger and discharger. Based on the limit charge state of the charging current listed in Table 1 of Example 1, the charging protocol was mapped as shown in Table 3 below, and the battery cell was fully charged to SOC 100% according to the mapped charging protocol, and the fully charged battery cell was fully discharged to SOC 0% at a constant current of 0.33C.

[0121] [Table 3]

[0122]

[0123] Comparative Example 3

[0124] A battery cell (capacity: 40 Ah) of the same specifications as the battery cell used in Example 1 was connected to an electrochemical charger and fully charged to SOC 100% at a constant current of 0.33C, and the fully charged battery cell was fully discharged to SOC 0% at a constant current of 0.33C.

[0125] Experimental Example 2: Measuring charging and discharging time

[0126] For each of the case of charging according to the method of Example 2 and charging according to the method of Comparative Example 3, the time required for charging was measured, and the results are shown in Table 4.

[0127] Experimental Example 3: Evaluation of Capacity Retention Rate

[0128] Charging and discharging were performed according to the methods of Example 2 and Comparative Example 3, respectively, but 200 cycles of charging and discharging were repeated, and then the capacity retention ratio calculated according to the following Formula 1 is shown in Table 4.

[0129] Formula 1: (discharge capacity at 200 cycles × 100) / discharge capacity at the first cycle

[0130] [Table 4]

[0131]

[0132] Referring to Table 4, when charging is performed according to the charging protocol of Example 2, the time required for charging is significantly reduced compared to charging according to the charging method according to Comparative Example 3. In addition, when charging is performed according to the charging protocol according to Example 2, the capacity retention rate is equal to the capacity retention rate of charging according to the charging method according to Comparative Example 3, thereby confirming that the charging protocol derived according to the present invention does not cause capacity aging of the battery cells.

[0133] [reference numerals]

[0134] 1: Battery Pack

[0135] 10: Battery Cell

[0136] 100: Battery Management System

[0137] 110: Measurement Department

[0138] 120: Memory unit

[0139] 130: Control Department

[0140] 200: Charging equipment

Claims

1. A battery management system, comprising: The measuring unit is configured to measure the closed circuit voltage (CCV) according to the state of charge (SOCx) when charging the double-electrode battery cell having a positive electrode and a negative electrode with different charging currents (I). SOCx ) and open circuit voltage (OCV SOCx ); A memory unit configured to collect and store an internal resistance curve by converting the measured CCV SOCx and OCV SOCx Substitute into the following formula 1 to calculate the internal resistance value (R SOCx ) to plot the internal resistance value (R) according to the charging state for each charging current (I) SOCx );as well as a control unit configured to determine a limit charging state corresponding to each charging current according to the internal resistance curve, and establish a charging protocol based on the limit charging state. [Formula 1] According to the internal resistance value (R SOCx ) = (CCV SOCx -OCV SOCx ) / I.

2. The battery management system according to claim 1, wherein: The control portion is configured to determine a state of charge (SOCx) value at a point where a graph shape of the internal resistance curve changes from a flat shape to a downward trend as a limit state of charge.

3. The battery management system according to claim 1, wherein: The control portion is configured to reestablish the charging protocol by periodically deriving a new limit state of charge corresponding to each charging current during repeated charging and discharging of the battery cells. 4 . The battery management system according to claim 1 , further comprising a connection portion configured to be connected with a charging device to supply a charging current to the battery cells according to a charging protocol established by the control portion.

5. The battery management system according to claim 1, wherein: The measuring section is configured to measure state information of the battery cell, the state information including at least one of a voltage and a charging state of the battery cell.

6. The battery management system according to claim 1, wherein: The charging current (I) is selected from the range of 0.33C to 6.0C.

7. A battery pack comprising the battery management system according to claim 1.

8. The battery pack according to claim 7, wherein: The battery pack includes a plurality of battery cells having a capacity of 40 to 200 Ah.

9. A method for establishing a charging protocol for a lithium secondary battery, comprising: (a) For a two-electrode battery cell with a positive electrode and a negative electrode, the closed circuit voltage (CCV) according to the state of charge (SOCx) is measured when charged at different charging currents (I). SOCx ) and open circuit voltage (OCV SOCx ); (b) The measured CCV SOCx and OCV SOCx Substitute into the following formula 1 to calculate the internal resistance value (R SOCx ), and collect an internal resistance curve, which plots the internal resistance value (R) according to the charging state for each charging current (I) SOCx );as well as (c) determining the limit charging state corresponding to each charging current based on the collected internal resistance curve; [Formula 1] According to the internal resistance value (R SOCx ) = (CCV SOCx -OCV SOCx ) / I.

10. The method for establishing a lithium secondary battery charging protocol according to claim 9, wherein: In process (c), the limit state of charge is determined as a state of charge (SOC) value at a point where a graph shape of the internal resistance curve changes from a flat shape to a downward trend.

11. The method for establishing a lithium secondary battery charging protocol according to claim 9, wherein: The dual-electrode battery cell has a capacity of 40 to 200 Ah.

12. The method for establishing a lithium secondary battery charging protocol according to claim 9, wherein: In process (a), the charging current (I) is selected from the range of 0.33C to 6.0C.

13. The method for establishing a lithium secondary battery charging protocol according to claim 12, wherein: In process (a), the charging current (I) is set at intervals of 0.1C to 1.0C.

14. The method for establishing a lithium secondary battery charging protocol according to claim 9, further comprising mapping the charging protocol based on a limit charging state according to a charging current, wherein: The mapping process maps so that each charging current is charged with a corresponding charging current to reach a limit charging state, but as the charging state increases, the charging current decreases.