Double-layer tempered glass clamping structure

By designing a double-layer tempered glass clamping structure with detachable clamping structure and cushioning mechanism, the problems of high repair cost and insufficient sound insulation and thermal insulation effect of double-layer tempered glass are solved, and lower maintenance costs and higher Heat insulation and sound insulation performance.

CN119434812APending Publication Date: 2025-02-14HAINAN ZHONGRONG GLASS TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411582881.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-11-07
Publication Date
2025-02-14

AI Technical Summary

Technical Problem

The repair cost of double-layer tempered glass is high when it is damaged and needs to be replaced as a whole. At the same time, the sound insulation and heat insulation effect are insufficient in extreme climates, and lack flexibility and practicality.

Method used

A double-layer tempered glass clamping structure is designed, including a base and a cover plate. The removable replacement of tempered glass is achieved through the movable clamping of the clamping plate and the sliding groove, and a cushioning mechanism and air intake hole are provided in the vertical plate. Allow the intermediate layer to inflate to improve heat and sound insulation.

Benefits of technology

The double-layer tempered glass side removable and flexible replacement of the sandwich structure is realized, reducing repair costs, improving thermal, sound and ultraviolet resistance, and enhancing safety guarantees and flexibility in use.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119434812A_ABST
    Figure CN119434812A_ABST
Patent Text Reader

Abstract

The double-layer tempered glass clamping structure comprises a base and a cover plate, the middle of the base and the middle of the cover plate are each provided with two sets of fixing grooves, the two ends of each fixing groove are each provided with a sliding groove, and first tempered glass and second tempered glass are installed in the two fixing grooves correspondingly; sliding blocks matched with the sliding grooves are arranged in the fixing grooves, clamping plates are connected to the upper portions of the sliding blocks, the two sides of the first tempered glass and the two sides of the second tempered glass are fixed into the fixing grooves through the clamping plates, and an air inlet hole is formed in the middle of the outer side of the vertical plate on one side; the simple double-layer tempered glass clamping structure is used for realizing the double-layer tempered glass of which the side surfaces are detachable and the internal structure of the interlayer can be freely changed, the problems that the repair cost is relatively high and the whole replacement is required when the double-layer tempered glass is damaged are solved, and meanwhile, the same structure is used for improving the heat insulation and sound insulation effects and the flexible usability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of double-layer tempered glass, in particular to a double-layer tempered glass clamping structure. Background Art

[0002] Double-layer glass is widely used in door and window buildings. It has sound insulation and heat insulation effects. It is a hollow glass structure. Its structure is to seal and separate two pieces of glass through the structure, and set dry air or structural glass components between the two pieces of glass. If the tempered glass is hit and broken, its glass fragments will not fly. Therefore, the hollow glass window using double-layer tempered glass is a safety glass window. Double-layer tempered glass is more expensive than general hollow glass, but due to the structure of double-layer glass, once a single piece is damaged, the repair cost is high and it needs to be replaced as a whole. At the same time, under extreme climatic conditions, the sound insulation and heat insulation effects of double-layer tempered glass cannot be changed, lacking flexibility and practicality. Therefore, a simple double-layer tempered glass clamping structure is provided to realize detachable and replaceable tempered glass and arbitrarily change the internal structure of the sandwich. Summary of the invention

[0003] The present invention proposes a simple double-layer tempered glass clamping structure to achieve double-layer tempered glass with detachable sides and arbitrarily changeable interlayer internal structure, thereby solving the problem of high cost of repairing damaged glass and requiring overall replacement. At the same time, the same structure is used to improve the heat insulation and sound insulation performance and flexible use.

[0004] In order to achieve the above object, the present invention adopts the following technical solutions:

[0005] A double-layer tempered glass clamping structure comprises a base and a cover plate, wherein two groups of fixing grooves are arranged in the middle of the base and the cover plate, and sliding grooves are arranged at both ends of the fixing grooves, a first tempered glass and a second tempered glass are respectively installed in the two fixing grooves, a sliding block (4) matching the sliding block (3) is arranged in the fixing groove (2), a clamping plate (5) is connected above the sliding block (4), and the first tempered glass (10) and the second tempered glass (11) are fixed in the fixing groove (2) on both sides through the clamping plate (5).

[0006] A vertical plate is arranged on the outer side of the cover plate, and a shock absorbing mechanism is arranged between the vertical plate and the first tempered glass and the second tempered glass.

[0007] The base and the cover plate are both provided with threaded holes at both ends of their outer sides, the bolts penetrate through the threaded holes and are connected to the clamping plates, and the clamping plates are slidably contracted by rotating the bolts.

[0008] Preferably, the vertical plate is connected to the upper cover plate by long bolts, and a group of vertical grooves are provided in the middle of the vertical plate, and a shock absorbing mechanism is provided inside the grooves.

[0009] Preferably, the shock absorbing mechanism comprises a damping rod, a spring, and a pressure plate, and damping rods are installed at both ends above the groove, a spring is sleeved on the outer side of the damping rod, and a pressure plate is connected to the top end of the damping rod.

[0010] Preferably, the first tempered glass and the second tempered glass are inserted between the clamping plate and the inner side of the fixing groove through one side of the vertical plate, and an air inlet hole is provided in the middle of the outer side of the vertical plate on one side.

[0011] Preferably, the air inlet hole on the other side extends between the inner grooves of the vertical plate, and a cover is provided on the outer side of the air inlet hole.

[0012] Preferably, replaceable protective films are provided on the inner and outer sides of the first tempered glass and the second tempered glass, and the protective films include nano self-cleaning films, explosion-proof films, and sound-insulating cotton strips. The nano self-cleaning films are provided on the outer sides of the first tempered glass and the second tempered glass, and explosion-proof films are provided on the inner sides of the first tempered glass and the second tempered glass.

[0013] Preferably, the gaps between the outer sides of the first tempered glass and the second tempered glass and the base, the cover plate and the vertical plate are filled with sound insulation cotton strips.

[0014] Compared with the prior art, the beneficial effects of the present invention are:

[0015] A clamping structure for the detachable side of double-layer tempered glass is realized. The first tempered glass and the second tempered glass are inserted between the clamping plate and the inner side of the fixing groove through one side of the vertical plate. The clamping plate is movably clamped. When the tempered glass is broken, the single glass can be replaced and repaired, which reduces the cost of the double-layer tempered glass and facilitates the replacement of the protective film due to aging. At the same time, an air inlet is arranged in the middle of the outer side of the vertical plate to fill the middle of the double-layer tempered glass with dry air or argon gas. The content can be flexibly filled at any time to be suitable for use in different places. The treatment of the middle layer plays a significant role in the heat insulation, sound insulation and UV protection of the double-layer tempered glass. A damping rod, a spring and a pressure plate are arranged inside the groove of the vertical plate. The shock-absorbing mechanism effectively prevents the double-layer tempered glass from extruding too much and causing self-explosion, which can significantly reduce the risk of injury caused by window breakage, provide users with higher safety protection, and is very flexible to use.

[0016] The first tempered glass and the second tempered glass are both provided with explosion-proof films on the inside, so that the glass can more effectively resist shattering when impacted by external force. Even if shattering occurs, the fragments will form uniform small particles, greatly reducing the risk of harm to the human body. At the same time, a nano self-cleaning film is provided. The self-cleaning ability of the nano self-cleaning film can make the glass surface cleaner, giving people a better visual effect, while also further improving the sound insulation and heat insulation effects. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 This is a schematic diagram of the structure of removing one side of the vertical plate of the present invention.

[0018] Figure 2 It is a schematic diagram of the end surface structure of the tempered glass installation of the present invention.

[0019] Figure 3 It is a schematic diagram of the explosion structure of the present invention.

[0020] Figure 4 It is a schematic diagram of the base structure of the present invention.

[0021] Figure 5 For the present invention Figure 4 Enlarged structural diagram at A in the middle.

[0022] Figure 6 For the present invention Figure 3 Enlarged structural diagram of point B in the middle

[0023] Numbers in the figure: 1. Base; 2. Fixing groove; 3. Slide groove; 4. Slider; 5. Clamp; 6. Cover plate; 7. Vertical plate; 8. Groove; 9. Long bolt; 10. First tempered glass; 11. Second tempered glass; 12. Air inlet; 13. Bolt; 14. Threaded hole; 15. Damping rod; 16. Spring; 17. Pressure plate; 18. Cover; 19. Nano self-cleaning film; 20. Explosion-proof film; 21. Sound insulation cotton strip. DETAILED DESCRIPTION

[0024] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.

[0025] Reference Figure 1-Figure 6 The present invention provides a technical solution: a double-layer tempered glass clamping structure, comprising a base 1 and a cover plate 6, wherein two groups of fixing grooves 2 are arranged in the middle of the base 1 and the cover plate 6, and slide grooves 3 are arranged at both ends of the fixing grooves 2, and sliders 4 matching the slide grooves 3 are arranged inside the fixing grooves 2, and a clamping plate 5 is connected above the slider 4, and the first tempered glass 10 and the second tempered glass 11 are fixed in the fixing grooves 2 by the clamping plates 5 on both sides, and vertical plates 7 are arranged on both sides of the base 1 and are connected to the upper cover plate 6 by long bolts 9, so as to facilitate the disassembly of the cover plate 6 and the installation of subsequent tempered glass, and a group of vertical grooves 8 are arranged in the middle of the vertical plate 7, and a shock absorbing mechanism is arranged inside the groove 8, and the first tempered glass 10 and the second tempered glass 11 are inserted between the clamping plate 5 and the inner side of the fixing groove 2 through one side of the vertical plate 7, and an air inlet 12 is arranged in the middle of the outer side of one side of the vertical plate 7, and replaceable protective films are arranged inside and outside the first tempered glass 10 and the second tempered glass 11.

[0026] Reference Figure 3 , Figure 4 , threaded holes 14 are provided at both ends of the outer sides of the base 1 and the cover plate 6, and bolts 13 penetrate the threaded holes 14 and are connected to the clamping plate 5, and by rotating the bolts 13, the clamping plate 5 slides and contracts, and the end of the bolt 13 is embedded in the clamping plate 5 and is connected in a movable limit position, and the clamping plate 5 can be driven to move forward and backward by screwing the bolts 13 to meet the installation requirements of tempered glass of different models, thicknesses and specifications, and single-piece glass can be replaced and repaired at the same time, which is convenient to operate and reduces the cost of double-layer tempered glass, and is also convenient for the replacement of aging protective film.

[0027] Reference Figure 1 , Figure 5 The shock absorbing mechanism includes a damping rod 15, a spring 16, and a pressure plate 17, and the damping rods 15 are installed at both ends above the groove 8, the spring 16 is sleeved on the outside of the damping rod 15, and the top of the damping rod 15 is connected to the pressure plate 17, which effectively avoids the self-explosion phenomenon caused by excessive extrusion pressure, can significantly reduce the risk of injury caused by window breakage, and provide higher safety protection for users; the air inlet 12 on the other side extends to between the grooves 8 inside the vertical plate 7, and a cover 18 is arranged on the outside of the air inlet 12, which improves the integrity of the double-layer tempered glass.

[0028] Reference Figure 1 , Figure 2 The protective film includes a nano self-cleaning film 19, an explosion-proof film 20, and sound-insulating cotton strips 21, and the outer sides of the first tempered glass 10 and the second tempered glass 11 are both provided with the nano self-cleaning film 19. The self-cleaning ability of the nano self-cleaning film 19 can make the glass surface cleaner. In addition to the tempered glass body, the first tempered glass 10 and the second tempered glass 11 are both provided with an explosion-proof film 20 on the inner side of both glasses, so that the glass can more effectively resist breaking when impacted by external force. Even if breaking occurs, it is further ensured that the fragments will form uniform small particles, greatly reducing the risk of injury to the human body; the gaps between the outer sides of the first tempered glass 10 and the second tempered glass 11 and the base 1, the cover plate 6, and the vertical plate 7 are filled with sound-insulating cotton strips 21, which ensure the sealing and sound insulation effect of the double-layer tempered glass.

[0029] When the double-layer tempered glass is used, firstly, a suitable base 1, cover plate 6 and vertical plate 7 are selected for tempered glass of different models, thicknesses and specifications, and the vertical plate 7 is connected to the upper base 1 and the side of the cover plate 6 through the long bolt 9, and then the first tempered glass 10 and the second tempered glass 11 with the explosion-proof film 20 attached inside are respectively inserted between the clamping plate 5 and the inner side of the fixing groove 2 through one side of the vertical plate 7, and then the bottom slide groove 3 of the fixing groove 2 and the matching slider 4 are passed through the bolts 13 and threaded holes 14 of the outer base 1 and the cover plate 6, and the bolt 13 is turned to shrink the clamping plate 5 connected above the slider 4, so as to clamp the first tempered glass 10 and the second tempered glass 11;

[0030] Secondly, a damping rod 15, a spring 16 and a pressure plate 17 are arranged inside the groove 8 of the side vertical plate 7. The shock-absorbing mechanism effectively prevents the double-layer tempered glass from extruding excessively and causing self-explosion, which can significantly reduce the risk of injury caused by window breakage and provide users with higher safety protection. Then, an air inlet 12 is arranged in the middle of the outer side of the vertical plate 7 to fill dry air or argon gas in the middle of the double-layer tempered glass. The treatment of the middle layer has a significant effect on the heat insulation, sound insulation and UV protection properties of the double-layer tempered glass. Then, nano self-cleaning films 19 are affixed to the outer sides of the first tempered glass 10 and the second tempered glass 11. Finally, sound insulation cotton strips 21 are filled in the gaps between the outer sides of the first tempered glass 10 and the second tempered glass 11 and the base 1, the cover plate 6 and the vertical plate 7 to ensure the sealing and sound insulation effect of the double-layer tempered glass.

[0031] The above-mentioned structural connection realizes a clamping structure for the detachable side of the double-layer tempered glass. The first tempered glass and the second tempered glass are inserted between the clamping plate and the inner side of the fixing groove through one side of the vertical plate. The clamping plate is movably clamped. When the tempered glass is broken, the single piece of glass can be replaced and repaired, which reduces the cost of the double-layer tempered glass and facilitates the replacement of the aging protective film. At the same time, an air inlet is provided in the middle part of the outer side of the vertical plate to fill the middle of the double-layer tempered glass with dry air or argon gas. The content can be flexibly filled at any time to suit the use in different places. The treatment of the middle layer plays a significant role in the heat insulation, sound insulation and UV protection of the double-layer tempered glass. Damping rods, springs and pressure plates are provided inside the vertical plate groove. The shock-absorbing mechanism effectively prevents the double-layer tempered glass from extruding too much and causing self-explosion, which can significantly reduce the risk of injury caused by window breakage, provide users with higher safety protection, and is very flexible to use.

[0032] A simple double-layer tempered glass clamping structure is used to realize double-layer tempered glass with detachable sides and arbitrarily changeable sandwich internal structure.

[0033] The above are only preferred specific implementation modes of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical solutions and inventive concepts of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A double-layer tempered glass clamping structure, comprising a base (1) and a cover plate (6), characterized in that: The base (1) and the cover plate (6) are both provided with two groups of fixing grooves (2) in the middle, and the two ends of the fixing grooves (2) are both provided with sliding grooves (3), the first tempered glass (10) and the second tempered glass (11) are respectively installed inside the two fixing grooves (2), the fixing grooves (2) are provided with sliding blocks (4) matching the sliding blocks (3), the upper part of the sliding blocks (4) is connected with a clamping plate (5), and the first tempered glass (10) and the second tempered glass (11) are fixed in the fixing grooves (2) at both sides by the clamping plates (5).

2. The double-layer tempered glass clamping structure according to claim 1, characterized in that: A vertical plate (7) is arranged on the outer side of the cover plate (6), and a shock absorbing mechanism is arranged between the vertical plate (7) and the first tempered glass (10) and the second tempered glass (11).

3. The double-layer tempered glass clamping structure according to claim 1, characterized in that: The base (1) and the cover plate (6) are provided with threaded holes (14) at both ends of the outer sides, and are connected to the clamping plate (5) by bolts (13) passing through the threaded holes (14), and the clamping plate (5) is slidably contracted by rotating the bolts (13).

4. The double-layer tempered glass clamping structure according to claim 2, characterized in that: The vertical plate (7) is connected to the upper cover plate (6) via long bolts (9), and a group of vertical grooves (8) are provided in the middle of the vertical plate (7), and a shock absorbing mechanism is provided inside the grooves (8).

5. The double-layer tempered glass clamping structure according to claim 4, characterized in that: The shock absorbing mechanism comprises a damping rod (15), a spring (16), and a pressure plate (17), and the damping rods (15) are installed at both ends above the groove (8), the spring (16) is sleeved on the outer side of the damping rod (15), and the top end of the damping rod (15) is connected to the pressure plate (17).

6. The double-layer tempered glass clamping structure according to claim 1, characterized in that: The first tempered glass (10) and the second tempered glass (11) are inserted between the clamping plate (5) and the inner side of the fixing groove (2) through one side of the vertical plate (7), and an air inlet hole (12) is provided in the middle of the outer side of the vertical plate (7) on one side.

7. The double-layer tempered glass clamping structure according to claim 6, characterized in that: The air inlet hole (12) on the other side extends between the inner grooves (8) of the vertical plate (7), and a sealing cover (18) is arranged outside the air inlet hole (12).

8. The double-layer tempered glass clamping structure according to claim 1, characterized in that: Replaceable protective films are arranged on the inner and outer sides of the first tempered glass (10) and the second tempered glass (11), and the protective films include a nano self-cleaning film (19), an explosion-proof film (20), and a sound insulation cotton strip (21). The nano self-cleaning film (19) is arranged on the outer sides of the first tempered glass (10) and the second tempered glass (11), and the explosion-proof film (20) is arranged on the inner sides of the first tempered glass (10) and the second tempered glass (11).

9. The double-layer tempered glass clamping structure according to claim 8, characterized in that: The gaps between the outer sides of the first tempered glass (10) and the second tempered glass (11) and the base (1), the cover plate (6), and the vertical plate (7) are filled with sound insulation cotton strips (21).