Battery formation method and device, battery and production method, system and device thereof

During the formation process of lithium-ion batteries, the target film forming voltage determined by the differential voltage-voltage change curve is used to extend the film forming reaction time of the solid electrolyte interface film, and the problem of poor film forming quality of the battery is solved and the improvement of battery performance and life is achieved.

CN119725824AActive Publication Date: 2025-03-28CONTEMPORARY AMPEREX TECHNOLOGY CO LTD
6 Cites 6 Cited by

Patent Information

Application Number
CN202510222683.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-02-27
Publication Date
2025-03-28
Estimated Expiration
2045-02-27

AI Technical Summary

Technical Problem

During the first charging process of lithium-ion batteries, the film formation quality of the solid electrolyte interface film is poor, resulting in oxidative decomposition and re-repairing processes during recycling, affecting the performance and life of the battery.

Method used

In the battery formation method, the battery is charged and constant voltage charging using the target film forming voltage determined by the differential voltage-voltage change curve, and the film forming reaction time of the solid electrolyte interface film is extended to improve its film forming quality.

Benefits of technology

It effectively improves the film formation quality of the solid electrolyte interface film, extends the service life of the battery, and improves the performance of the battery.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention provides a battery formation method and device, a battery and a production method, system and device of the battery, and belongs to the technical field of batteries. A first target film forming voltage is determined by characterizing a differential voltage-voltage change curve of an organic phase film forming reaction of the solid electrolyte interfacial film. In the battery formation method, the first target film forming voltage determined by the differential voltage-voltage change curve is used for constant-voltage charging, so that the film forming quality of the solid electrolyte interfacial film can be improved.