Polylactic acid skin-friendly anti-allergic down-like material and preparation method thereof
A biodegradable polyester-based material mimics down's insulating properties with hypoallergenic and moisture-wicking features, addressing ethical concerns and improving user comfort through electrospinning technology.
Patent Information
- Application Number
- CN202510358837.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-03-25
- Publication Date
- 2025-07-15
AI Technical Summary
Traditional down materials are prone to carrying allergens, poor breathability, poor hygroscopicity and insufficient environmental protection, and rely on animal resources and unstable supply chains.
Alternating electrospinning technology is used, polylactic acid/pretreated poplar cellulose is used as the velvet core, and polylactic acid/maleic anhydride grafted polyolefin is the velvet rigid framework to form a down-like " velvet core- velvet branch" structure, and licorice extract is added to provide anti-allergic effect.
It realizes the high warmth, lightness, softness and anti-allergicity of imitation down materials, avoids the disadvantages of natural down, and improves environmental protection performance and supply chain stability.
Smart Images

Figure BDA0005328074320000071 
Figure BDA0005328074320000072 
Figure BDA0005328074320000081
Abstract
Description
Technical Field
[0001] The present invention relates to the field of functional fiber materials, and particularly to a polylactic acid skin-friendly and anti-allergic down-like material. Background Art
[0002] Traditional down materials occupy an irreplaceable position in the field of thermal insulation materials due to their core advantages such as lightweight, high warmth retention, and dynamic temperature regulation. The three-dimensional cluster structure (down clusters) of down can lock a large amount of static air, forming an efficient heat insulation layer; in addition, the surface of down fibers is covered with natural oils, which can adjust the breathability according to the change of environmental humidity, achieving a comfortable experience of "warm but not stuffy". The higher the fill power and down content of down, the stronger its thermal insulation performance, and at the same time, it is lighter in weight and softer in texture, providing comfortable wearing. However, down materials also have some disadvantages. First, down is prone to carrying allergens (such as dust, microorganisms), which may cause skin sensitivity or respiratory discomfort; second, down products are prone to feather leakage, and rely on high-density fabrics or chemical coating treatments, which affect breathability and environmental friendliness; in addition, down has poor moisture absorption, and its thermal insulation performance drops significantly in a humid environment and it is difficult to dry quickly; finally, down relies on animal resources, there are animal ethics disputes, and its price fluctuates greatly due to the breeding cycle and diseases (such as avian influenza), and the supply chain stability is insufficient. These disadvantages have led to an increasing demand in the market for the research and development of down-like materials. The research directions of down-like materials include improving their comprehensive properties such as warmth retention, lightness, softness, and fluffiness to replace natural down materials. For example, by using a mixture of ultra-fine fibers and thick fibers, optimizing the fiber fineness ratio, shape treatment, and process parameters, down-like materials with spherical or tufted shapes are developed, which not only retain the fluffiness of down but also avoid the problems associated with the use of natural down. In addition, down-like materials also focus on environmental performance, using highly fluffy fibers and combining the application of nanotechnology and new materials to further improve their performance. Although down materials have significant advantages in terms of thermal insulation performance, lightweight, and comfort, their disadvantages also limit their wide application. Therefore, it is necessary to develop new down-like materials to meet the market's demand for high-performance, environmentally friendly, and sustainable development materials. Summary of the Invention
[0003] Technical problems to be solved: The present invention provides a polylactic acid skin-friendly and anti-allergic down-like material, which uses polylactic acid / pretreated poplar cellulose as the down core, and polylactic acid / maleic anhydride-grafted polyolefin as the rigid framework raw material for the down branches, and obtains the polylactic acid skin-friendly and anti-allergic down-like material through alternating electrospinning.
[0004] Technical solutions: A polylactic acid skin-friendly and anti-allergic down-like material, the down-like material is obtained by alternating electrospinning, and the down-like material uses polylactic acid / pretreated poplar cellulose as the fluff core and polylactic acid / maleic anhydride-grafted polyolefin as the rigid skeleton of the fluff branches. Preferably, the preparation method comprises the following steps: S1. Add polylactic acid and pretreated poplar cellulose into a mixed solution of dichloromethane / N,N-dimethylformamide, and add LiCl to obtain solution A with a mass fraction of 15-25 wt%. S2. Add polylactic acid, maleic anhydride-grafted polyolefin and licorice extract into a mixed solution of toluene and tetrahydrofuran, and add sodium dodecyl sulfate to obtain solution B with a mass fraction of 20-25 wt%. S3. Perform alternating electrospinning on solution A and solution B, and cycle 10-20 times to obtain the polylactic acid skin-friendly and anti-allergic down-like material. Preferably, the mass ratio of polylactic acid to pretreated poplar cellulose in S1 is 1:0.1-0.25; In S1, the volume ratio of dichloromethane to N,N-dimethylformamide is 7:3-9:1; The addition amount of LiCl in S1 is 0.2-0.6 wt% of the mass of polylactic acid. Preferably, the preparation method of the pretreated poplar cellulose in S1 comprises the following steps: S11. Add poplar cellulose into the organic acid mixture to obtain a mixed solution with a solid-liquid ratio of 1:5-15; S12. Heat and react the solution obtained in S11 at 60-80 °C and perform ultrasonic treatment to obtain the pretreated poplar cellulose. Preferably, the mass ratio of polylactic acid, maleic anhydride-grafted polyolefin and licorice extract in S2 is 1:0.15-0.3:0.08-0.12; In S2, the volume ratio of toluene to tetrahydrofuran is 2-5:1-3; The addition amount of sodium dodecyl sulfate in S2 is 0.3-1.5 wt% of the mass of polylactic acid. Preferably, the electrospinning voltage of solution A in S3 is -25 to -15 kV; The electrospinning flow rate of solution A in S3 is 0.5-1.0 mL / h; The receiving distance of solution A in S3 is 12-18 cm. Preferably, the electrospinning voltage of solution B in S3 is 20-30 kV; The electrospinning flow rate of solution B in S3 is 1.0-1.5 mL / h; The receiving distance of solution B in S3 is 8-12 cm. Preferably, the organic acid mixed solution in S11 is any two of oxalic acid, citric acid or p-toluenesulfonic acid, and the volume ratio of the two organic acids is 1-4:2-5. Preferably, the temperature of the heating reaction in S12 is 60-80 °C, the time is 1-3 h, and the power of the ultrasonic treatment is 550-180 W. Beneficial effects: The present invention has the following advantages: 1. In the present invention, the alternating electrospinning forms a "down core-down branch" structure similar to down through the layer-by-layer deposition of solution A and solution B. Poly(lactic acid) and pretreated poplar cellulose serve as a fluffy core layer to provide a static air storage space, while the maleic anhydride polyolefin backbone locks air convection through a branched fiber network, thereby constructing a down-like structure; 2. In the present invention, the high crystallinity and rigid microfibril structure of the pretreated poplar cellulose reduce the energy barrier required for the crystallization of poly(lactic acid), promote the preferential formation of crystal nuclei on the surface of cellulose, and thus provide nucleation sites for poly(lactic acid), inducing the refinement of microcrystals and also forming a fluffy network for fiber skeleton support; 3. In the present invention, the chemical bonding between the maleic anhydride-grafted polyolefin and the non-polar poly(lactic acid) chain segment in solution B forms a "sea-island structure" interface, and then forms a down-like structure of "down branch-down barbule"; and the licorice extract can relieve allergic symptoms by inhibiting histamine release, regulating immune function and anti-inflammatory effects, thereby endowing the material with anti-allergic efficacy. Specific embodiments The present invention will be further described below in conjunction with embodiments. The following embodiments are explanations of the present invention, and the present invention is not limited to the following embodiments: Example 1 A poly(lactic acid) skin-friendly and anti-allergic down-like material, the down-like material is obtained by alternating electrospinning, and the down-like material uses poly(lactic acid) / pretreated poplar cellulose as the down core and poly(lactic acid) / maleic anhydride-grafted polyolefin as the rigid backbone of the down branch. Among them, the preparation method includes the following steps: S1. Poly(lactic acid) and pretreated poplar cellulose are added to a mixed solution of dichloromethane / N,N-dimethylformamide with a volume ratio of 7:9 according to a mass ratio of 1:0.1, and LiCl is added. The addition amount of LiCl is 0.2 wt% of the mass of poly(lactic acid), and a solution A with a mass fraction of 15 wt% is obtained; S2. Poly(lactic acid), maleic anhydride-grafted polyolefin and licorice extract with a mass ratio of 1:0.15:0.08 are added to a mixed solution of toluene and tetrahydrofuran with a volume ratio of 2:1, and sodium dodecyl sulfate is added. The addition amount of sodium dodecyl sulfate is 0.3 wt% of the mass of poly(lactic acid), and a solution B with a mass fraction of 20 wt% is obtained; S3. Alternately electrospin Solution A and Solution B. The electrospinning voltage of Solution A is -25 kV, the electrospinning flow rate is 0.5 mL / h, and the receiving distance is 12 cm. The electrospinning voltage of Solution B is 20 kV, the electrospinning flow rate is 1.0 mL / h, and the receiving distance is 8 cm. Cycle 10 times to obtain a polylactic acid skin-friendly and anti-allergic down-like material. Among them, the preparation method of the pretreated poplar cellulose in S1 includes the following steps: S11. Add poplar cellulose to a mixed solution of citric acid / p-toluenesulfonic acid with a volume ratio of 1:2 to obtain a mixed solution with a solid-liquid ratio of 1:5. S12. Heat the solution obtained in S11 at 60 °C for reaction and perform ultrasonic treatment at a power of 50 W for 1 h to obtain pretreated poplar cellulose. Example 2 A polylactic acid skin-friendly and anti-allergic down-like material. The down-like material is obtained by alternate electrospinning. The down-like material uses polylactic acid / pretreated poplar cellulose as the fluff core and polylactic acid / maleic anhydride-grafted polyolefin as the rigid framework of the fluff branches. Among them, the preparation method includes the following steps: S1. Add polylactic acid and pretreated poplar cellulose in a mass ratio of 1:0.25 to a mixed solution of dichloromethane / N,N-dimethylformamide with a volume ratio of 3:1 and add LiCl. The addition amount of LiCl is 0.6 wt% of the mass of polylactic acid to obtain Solution A with a mass fraction of 25 wt%. S2. Add polylactic acid, maleic anhydride-grafted polyolefin, and licorice extract in a mass ratio of 1:0.3:0.0.12 to a mixed solution of toluene and tetrahydrofuran with a volume ratio of 5:3 and add sodium dodecyl sulfate. The addition amount of sodium dodecyl sulfate is 1.5 wt% of the mass of polylactic acid to obtain Solution B with a mass fraction of 22 wt%. S3. Alternately electrospin Solution A and Solution B. The electrospinning voltage of Solution A is -15 kV, the electrospinning flow rate is 1.0 mL / h, and the receiving distance is 18 cm. The electrospinning voltage of Solution B is 30 kV, the electrospinning flow rate is 1.5 mL / h, and the receiving distance is 12 cm. Cycle 20 times to obtain a polylactic acid skin-friendly and anti-allergic down-like material. Among them, the preparation method of the pretreated poplar cellulose in S1 includes the following steps: S11. Add poplar cellulose to a mixed solution of oxalic acid / citric acid with a volume ratio of 4:5 to obtain a mixed solution with a solid-liquid ratio of 1:15. S12. Heat the solution obtained in S11 at 80 °C for reaction and perform ultrasonic treatment at a power of 180 W for 2 h to obtain pretreated poplar cellulose. Example 3 A polylactic acid skin-friendly and anti-allergic down-like material, the down-like material is obtained by alternating electrospinning, the down-like material uses polylactic acid / pretreated poplar cellulose as the fluff core, and polylactic acid / maleic anhydride grafted polyolefin as the rigid framework of the fluff branches. Among them, the preparation method includes the following steps: S1. Add polylactic acid and pretreated poplar cellulose according to a mass ratio of 1:0.2 to a mixed solution of dichloromethane / N,N-dimethylformamide with a volume ratio of 5:2, and add LiCl. The addition amount of LiCl is 0.3 wt% of the mass of polylactic acid to obtain solution A with a mass fraction of 18 wt%; S2. Add polylactic acid, maleic anhydride grafted polyolefin and licorice extract with a mass ratio of 1:0.18:0.10 to a mixed solution of toluene and tetrahydrofuran with a volume ratio of 3:1, and add sodium dodecyl sulfate. The addition amount of sodium dodecyl sulfate is 0.8 wt% of the mass of polylactic acid to obtain solution B with a mass fraction of 22 wt%; S3. Perform alternating electrospinning on solution A and solution B. The electrospinning voltage of solution A is -20 kV, the electrospinning flow rate is 0.8 mL / h, and the receiving distance is 15 cm. The electrospinning voltage of solution B is 25 kV, the electrospinning flow rate is 1.2 mL / h, and the receiving distance is 10 cm. Cycle 15 times to obtain the polylactic acid skin-friendly and anti-allergic down-like material. Among them, the preparation method of the pretreated poplar cellulose in S1 includes the following steps: S11. Add poplar cellulose to a mixed solution of oxalic acid / citric acid with a volume ratio of 3:4 to obtain a mixed solution with a solid-liquid ratio of 1:10; S12. Heat the solution obtained in S11 at 60 °C for reaction and perform ultrasonic treatment at a power of 110 W for 1.5 h to obtain the pretreated poplar cellulose. Example 4 A polylactic acid skin-friendly and anti-allergic down-like material, the down-like material is obtained by alternating electrospinning, the down-like material uses polylactic acid / pretreated poplar cellulose as the fluff core, and polylactic acid / maleic anhydride grafted polyolefin as the rigid framework of the fluff branches. Among them, the preparation method includes the following steps: S1. Add polylactic acid and pretreated poplar cellulose according to a mass ratio of 1:0.2 to a mixed solution of dichloromethane / N,N-dimethylformamide with a volume ratio of 5:9, and add LiCl. The addition amount of LiCl is 0.4 wt% of the mass of polylactic acid to obtain solution A with a mass fraction of 22 wt%; S2. Add polylactic acid, maleic anhydride-grafted polyolefin, and licorice extract with a mass ratio of 1:0.20:0.08 to a mixed solution of toluene and tetrahydrofuran with a volume ratio of 4:3, and add sodium dodecyl sulfate. The addition amount of sodium dodecyl sulfate is 1 wt% of the mass of polylactic acid to obtain solution B with a mass fraction of 22 wt%. S3. Perform alternating electrospinning on solution A and solution B. The electrospinning voltage of solution A is -18 kV, the electrospinning flow rate is 0.8 mL / h, and the receiving distance is 15 cm. The electrospinning voltage of solution B is 25 kV, the electrospinning flow rate is 1.1 mL / h, and the receiving distance is 10 cm. Cycle 15 times to obtain a polylactic acid skin-friendly and anti-allergic down-like material. Among them, the preparation method of the pretreated poplar cellulose in S1 includes the following steps: S11. Add poplar cellulose to a mixed solution of oxalic acid / p-toluenesulfonic acid with a volume ratio of 3:2 to obtain a mixed solution with a solid-liquid ratio of 1:14. S12. Heat the solution obtained in S11 at 65 °C for reaction and perform ultrasonic treatment at a power of 80 W for 2 h to obtain pretreated poplar cellulose. Example 5 A polylactic acid skin-friendly and anti-allergic down-like material, the down-like material is obtained by alternating electrospinning, the down-like material uses polylactic acid / pretreated poplar cellulose as the fluff core, and uses polylactic acid / maleic anhydride-grafted polyolefin as the rigid fluff branch framework. Among them, the preparation method includes the following steps: S1. Add polylactic acid and pretreated poplar cellulose according to a mass ratio of 1:0.24 to a mixed solution of dichloromethane / N,N-dimethylformamide with a volume ratio of 5:8, and add LiCl. The addition amount of LiCl is 0.4 wt% of the mass of polylactic acid to obtain solution A with a mass fraction of 18 wt%. S2. Add polylactic acid, maleic anhydride-grafted polyolefin, and licorice extract with a mass ratio of 1:0.25:0.09 to a mixed solution of toluene and tetrahydrofuran with a volume ratio of 3:2, and add sodium dodecyl sulfate. The addition amount of sodium dodecyl sulfate is 1.2 wt% of the mass of polylactic acid to obtain solution B with a mass fraction of 22 wt%. S3. Perform alternating electrospinning on solution A and solution B. The electrospinning voltage of solution A is -20 kV, the electrospinning flow rate is 0.8 mL / h, and the receiving distance is 15 cm. The electrospinning voltage of solution B is 25 kV, the electrospinning flow rate is 1.2 mL / h, and the receiving distance is 10 cm. Cycle 15 times to obtain a polylactic acid skin-friendly and anti-allergic down-like material. Among them, the preparation method of the pretreated poplar cellulose in S1 includes the following steps: S11. Add poplar cellulose into a mixed solution of oxalic acid / p-toluenesulfonic acid with a volume ratio of 3:2 to obtain a mixed solution with a solid-liquid ratio of 1:11; S12. Heat and react the solution obtained in S11 at 70 °C and perform ultrasonic treatment at a power of 150 W for 1.5 h to obtain pretreated poplar cellulose. Example 6 A polylactic acid skin-friendly and anti-allergic down-like material, the down-like material is obtained by alternating electrospinning, the down-like material uses polylactic acid / pretreated poplar cellulose as the fluff core, and polylactic acid / maleic anhydride-grafted polyolefin as the rigid framework of the fluff branches. Among them, the preparation method includes the following steps: S1. Add polylactic acid and pretreated poplar cellulose into a mixed solution of dichloromethane / N,N-dimethylformamide with a volume ratio of 5:8 according to a mass ratio of 1:0.22 and add LiCl. The addition amount of LiCl is 0.4 wt% of the mass of polylactic acid to obtain solution A with a mass fraction of 18 wt%; S2. Add polylactic acid, maleic anhydride-grafted polyolefin and licorice extract with a mass ratio of 1:0.25:0.12 into a mixed solution of toluene and tetrahydrofuran with a volume ratio of 4:1 and add sodium dodecyl sulfate. The addition amount of sodium dodecyl sulfate is 0.5 wt% of the mass of polylactic acid to obtain solution B with a mass fraction of 22 wt%; S3. Perform alternating electrospinning on solution A and solution B. The electrospinning voltage of solution A is -18 kV, the electrospinning flow rate is 0.9 mL / h, and the receiving distance is 15 cm. The electrospinning voltage of solution B is 25 kV, the electrospinning flow rate is 1.2 mL / h, and the receiving distance is 12 cm. Cycle 15 times to obtain a polylactic acid skin-friendly and anti-allergic down-like material. Among them, the preparation method of the pretreated poplar cellulose in S1 includes the following steps: S11. Add poplar cellulose into a mixed solution of citric acid / oxalic acid with a volume ratio of 3:2 to obtain a mixed solution with a solid-liquid ratio of 1:8; S12. Heat and react the solution obtained in S11 at 70 °C and perform ultrasonic treatment at a power of 120 W for 1.5 h to obtain pretreated poplar cellulose. Comparative Example 1 The difference between this comparative example and Example 6 is that pretreated poplar cellulose was not added in S1. Comparative Example 2 The difference between this comparative example and Example 6 is that unpretreated poplar cellulose was added in S1. Comparative Example 3 The difference between this comparative example and Example 6 is that the maleic anhydride-grafted polyolefin was not added in S2. Comparative Example 4 The difference between this comparative example and Example 6 is that the licorice extract was not added in S2. Comparative Example 5 The difference between this comparative example and Example 6 is that in S3, electrospinning was first carried out with Solution A and then with Solution B, the electrospinning voltage was 25 kV, the electrospinning flow rate was 1.2 mL / h, and the receiving distance was 12 cm. Performance Test The materials obtained in Examples 1 to 6 of the present invention and Comparative Examples 1 to 4 were subjected to performance tests. Table 1 Thermal Insulation Performance Test Table 2 Antibacterial Performance Test Obviously, the above examples are only for clear illustration and not limitations on the implementation manners. For those of ordinary skill in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to enumerate all the implementation manners here. And the obvious changes or modifications derived therefrom are still within the protection scope of the present invention.
Claims
1. A polylactic acid skin-friendly and anti-allergic down-like material, characterized in that: The down-like material is obtained by alternating electrospinning. The down-like material uses polylactic acid / pretreated poplar cellulose as the fluff core and polylactic acid / grafted polyolefin maleic anhydride as the rigid fluff branch skeleton.
2. The preparation method of the polylactic acid skin-friendly and anti-allergic down-like material according to claim 1, wherein: The preparation method includes the following steps: S1. Add polylactic acid and pretreated poplar cellulose into a mixed solution of dichloromethane / N,N-dimethylformamide, and add LiCl to obtain solution A with a mass fraction of 15-25 wt%. S2. Add polylactic acid, grafted polyolefin maleic anhydride and licorice extract into a mixed solution of toluene and tetrahydrofuran, and add sodium dodecyl sulfate to obtain solution B with a mass fraction of 20-25 wt%. S3. Perform alternating electrospinning on solution A and solution B for 10-20 cycles to obtain a polylactic acid skin-friendly and anti-allergic down-like material.
3. The preparation method of the polylactic acid skin-friendly and anti-allergic down-like material according to claim 1, characterized in that: In S1, the mass ratio of polylactic acid to pretreated poplar cellulose is 1:0.1-0.25; and / or, in S1, the volume ratio of dichloromethane to N,N-dimethylformamide is 7:3-9:1; and / or, in S1, the addition amount of LiCl is 0.2-0.6 wt% of the mass of polylactic acid.
4. The preparation method of the polylactic acid skin-friendly and anti-allergic down-like material according to claim 1, wherein: The preparation method of the pretreated poplar cellulose in S1 includes the following steps: S11. Add poplar cellulose into the organic acid mixture to obtain a mixed solution with a solid-liquid ratio of 1:5-15; S12. Heat and react the solution obtained in S11 at 60-80 °C and perform ultrasonic treatment to obtain pretreated poplar cellulose.
5. The preparation method of the polylactic acid skin-friendly and anti-allergic down-like material according to claim 1, wherein: In S2, the mass ratio of polylactic acid, grafted polyolefin maleic anhydride and licorice extract is 1:0.15-0.3:0.08-0.12; and / or, in S2, the volume ratio of toluene to tetrahydrofuran is 2-5:1-3; and / or, in S2, the addition amount of sodium dodecyl sulfate is 0.3-1.5 wt% of the mass of polylactic acid.
6. The preparation method of the polylactic acid skin-friendly and anti-allergic down-like material according to claim 1, wherein: In S3, the electrospinning voltage of solution A is -25 to -15 kV; and / or, in S3, the electrospinning flow rate of solution A is 0.5-1.0 mL / h; and / or, in S3, the receiving distance of solution A is 12-18 cm.
7. The preparation method of the polylactic acid skin-friendly and anti-allergic down-like material according to claim 1, characterized in that: In S3, the electrospinning voltage of solution B is 20-30 kV; and / or, in S3, the electrospinning flow rate of solution B is 1.0-1.5 mL / h; and / or, in S3, the receiving distance of solution B is 8-12 cm.
8. The preparation method of the polylactic acid skin-friendly and anti-allergic down-like material according to claim 4, characterized in that: In S11, the organic acid mixed solution is any two of oxalic acid, citric acid or p-toluenesulfonic acid, and the volume ratio of the two organic acids is 1-4:2-5.
9. The preparation method of the polylactic acid skin-friendly and anti-allergic down-like material according to claim 4, characterized in that: In S12, the temperature of the heating reaction is 60-80 °C, the time is 1-3 h, and the power of the ultrasonic treatment is 550-180 W.