Integrated injection molding wireless heat conduction type charging assembly and production process thereof

Through gradient temperature control, nano-level titanium nitride coating treatment, twin-screw blending injection molding and visual positioning technology, the problems of brittle connection between the soft magnetic layer and the thermal conductive layer and inaccurate coil positioning in traditional wireless charging components have been solved, achieving high-precision and stable wireless charging component production, and improving heat dissipation performance and electromagnetic conversion efficiency.

CN120620688APending Publication Date: 2025-09-12SUZHOU BOTAO NEW MATERIALS TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510762027.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-06-09
Publication Date
2025-09-12

AI Technical Summary

Technical Problem

Traditional wireless charging components adopt a layered assembly structure, in which the soft magnetic layer and the thermal conductive layer are connected by a gluing process. The glue layer is prone to aging and cracking under long-term thermal cycles, resulting in an increase of more than 30% in the interface thermal resistance and a decay in heat dissipation performance over time. The coil positioning relies on mechanical fixtures, with large assembly tolerances, uneven electromagnetic field distribution, and fluctuating energy transmission efficiency. The interface bonding strength between the soft magnetic material and the polymer matrix is ​​insufficient, and the layers are easily peeled off under mechanical impact.

Method used

A gradient temperature control process and nano-scale titanium nitride coating are used to generate high-precision molds. The twin-screw co-blending injection molding process is combined to achieve uniform distribution of the soft magnetic matrix. The Litz coil is accurately embedded using a visual positioning-assisted process, and AlN/PA66 composite materials are injected in stages. The crystallinity and cross-linking density are controlled through a gradient curing process, and the surface functionalization process is used to improve component performance.

Benefits of technology

The mold precision and thermal stability are improved, ensuring that the dimensional tolerance of the soft magnetic matrix structure layer is within ±0.05mm, the magnetic permeability is increased to 120μ, the Litz coil position deviation is less than 0.1mm, the continuity of the heat conduction path is enhanced, the thermal conductivity is increased to 5.8W/m·K, the bending strength reaches 180MPa, the surface hardness is increased to HV1200, the heat dissipation area is increased by 40%, the electromagnetic conversion efficiency is increased by 12%, the temperature rise is reduced by 25℃, and the mechanical vibration tolerance is increased by 3 times.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120620688A_ABST
    Figure CN120620688A_ABST
Patent Text Reader

Abstract

The invention provides an integrated injection molding wireless heat conduction type charging assembly and a production process thereof, and relates to the technical field of wireless charging. The integrated injection molding wireless heat conduction type charging assembly and the production technology thereof comprise the following steps that S1, based on the mold pretreatment requirement, a gradient temperature control technology is adopted, a mold is preheated to 80 + / -2 DEG C and kept for 30 min, meanwhile, nanoscale titanium nitride surface coating treatment is carried out, and a high-precision pretreatment mold is generated; the gradient temperature control technology is combined with nanoscale titanium nitride coating treatment, the surface precision and thermal stability of a mold are remarkably improved, material shrinkage deformation in the injection molding process is reduced, it is ensured that the dimensional tolerance of a soft magnetic matrix structure layer is controlled within + / -0.05 mm, and in the double-screw blending injection molding technology, FeSiAl soft magnetic powder and a PA6 base material are subjected to melt blending, so that the stability of the mold is improved. Uniform distribution of a soft magnetic phase in a matrix is achieved, the magnetic conductivity is improved to 120 mu or above, and meanwhile the eddy current loss is reduced by 15% through the coating effect of PA6.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of wireless charging, and in particular to an integrated injection-molded wireless thermally conductive charging component and a production process thereof. Background Art

[0002] The field of wireless charging technology mainly involves a technical system that realizes wireless transmission of electric energy through electromagnetic induction, magnetic resonance or radio frequency. This field covers key technical directions such as energy conversion efficiency optimization, electromagnetic interference suppression, thermal management design and new material application. It focuses on solving problems such as interface wear, poor environmental adaptability and space limitations in traditional wired charging. Among them, an integrated injection-molded wireless thermal conductive charging component and its production process refer to an integrated component manufactured by integrating soft magnetic materials, conductive coils and thermal conductive media through innovative injection molding technology. This technology uses an in-mold composite injection molding process to achieve one-time molding of the electromagnetic conversion unit and the heat dissipation structure. It is mainly used in the manufacture of wireless charging modules for electronic products such as smart phones, smart wearable devices and Internet of Things terminals. It can effectively improve charging efficiency and solve the heat accumulation and mechanical reliability problems of traditional layered structures.

[0003] Traditional wireless charging components use a layered assembly structure, where the soft magnetic layer and the thermal conductive layer are connected by gluing. The glue layer is prone to aging and brittle cracking under long-term thermal cycles, resulting in an increase in interfacial thermal resistance of more than 30%, and the heat dissipation performance decays over time. The coil positioning relies on mechanical fixtures, and the assembly tolerance generally exceeds 0.5mm, resulting in uneven electromagnetic field distribution and energy transmission efficiency fluctuations of up to ±8%. At the same time, there is a micron-level gap between the coil and the soft magnetic substrate, generating high-frequency vibration noise during operation. The single temperature and pressure parameters in the injection molding process result in insufficient interfacial bonding strength between the soft magnetic material and the polymer matrix. Interlayer delamination is prone to occur in mechanical impact tests, with a peel strength of only 15MPa. Summary of the Invention

[0004] In response to the shortcomings of the existing technology, the present invention provides an integrated injection-molded wireless thermal conductive charging component and its production process, which solves the problem that traditional wireless charging components adopt a layered assembly structure, the soft magnetic layer and the thermal conductive layer are connected by a gluing process, and the glue layer is prone to aging and brittle cracking under long-term thermal cycles, resulting in an increase in interface thermal resistance by more than 30% and the heat dissipation performance decaying over time.

[0005] To achieve the above objectives, the present invention is implemented through the following technical solutions: a one-piece injection-molded wireless thermal conductive charging component production process, characterized by comprising the following steps: S1: Based on the mold pretreatment requirements, a gradient temperature control process is used to preheat the mold to 80±2℃ and maintain it for 30 minutes. At the same time, nano-scale titanium nitride surface coating treatment is applied to generate a high-precision pretreated mold; S2: Based on the pre-treated mold, a twin-screw blending injection molding process was used to melt-blend FeSiAl soft magnetic powder and PA6 substrate at 280°C, and injected into the mold cavity at a pressure of 100 MPa with a holding time of 18 seconds to form a soft magnetic matrix structure layer; S3: Based on the soft magnetic matrix structure layer, a visual positioning-assisted process is used to guide the precise embedding of the Litz coil through the CCD imaging system, and 5kPa vacuum adsorption is simultaneously applied to fix it to form a coil-embedded matrix; S4: Based on the coil-embedded matrix, a gradient injection molding process is implemented to inject AlN / PA66 composite materials in two stages: the first stage: 280℃ / 80MPa injection molding to fill the coil gap, and the second stage: 300℃ / 120MPa to complete the overall coating to form a thermal conductive-electromagnetic composite; S5: Based on the thermal conductive-electromagnetic composite, a gradient curing process is adopted and performed under nitrogen protection: 0-30 minutes: 80°C low-temperature setting, 30-60 minutes: 120°C crystallization strengthening, 60-90 minutes: 160°C cross-linking curing to generate a three-dimensional stable structure; S6: Based on the three-dimensional stable structure, a surface functionalization process is implemented, including: plasma surface treatment; nano-aluminum oxide coating deposition; laser microstructure etching, to generate a multifunctional integrated component.

[0006] Preferably, generating a high-precision pre-processed mold based on S1 includes the following steps: S101: Based on the mold surface cleaning requirements, a plasma cleaning process is used to generate argon plasma through a radio frequency power supply. The treatment time was 15 minutes, and the surface energy was increased to 72 mN / m, generating a clean mold matrix; S102: Based on the clean mold substrate, a physical vapor deposition process is performed to deposit a titanium nitride coating using a magnetron sputtering method with a target current of 3.5 A, a deposition rate of 0.8 nm / s, and a vacuum degree of 5×10-3 Pa to generate a coated mold substrate; S103: Based on the coated mold substrate, perform a gradient preheating process, raise the temperature to 80±2℃ at a rate of 5℃ / min, keep warm for 30 minutes, and the mold temperature uniformity is ≤±0.5℃ to generate a high-precision pretreated mold.

[0007] Preferably, the generation of the soft magnetic matrix structure layer based on S2 comprises the following steps: S201: Based on the pre-treated mold, a material pre-mixing process is implemented to melt-blend FeSiAl powder and PA6 particles in a twin-screw extruder. The temperature is controlled in zones: feeding section 240°C → compression section 260°C → homogenization section 280°C to generate a soft magnetic composite melt. S202: Based on the soft magnetic composite material melt, a high-speed injection molding process is used with an injection speed of 120 mm / s, a V / P switching point of 95% of the mold cavity volume, a peak pressure of 100 MPa, and a holding pressure curve of 80 MPa in the first 10 seconds → 60 MPa in the last 8 seconds to generate a preliminary soft magnetic structure; S203: Based on the initially formed soft magnetic structure, perform an in-mold annealing process, maintain 120°C / 15 minutes in the mold, cool at a rate of 2°C / min to 60°C for demoulding, and generate a soft magnetic matrix structure layer.

[0008] Preferably, the generation of the coil embedded matrix based on S3 comprises the following steps: S301: Based on the soft magnetic matrix structure layer, a visual positioning process is implemented, using a 5MP industrial camera and the Halcon algorithm to achieve a positioning accuracy of ±0.03mm, generate three-dimensional coordinate data, and generate a digital model for coil positioning; S302: Based on the positioning digital model, the robot guidance process is executed. The six-axis robot carries the Litz coil to the specified position, and the vacuum suction cup pressure is -85kPa to generate a pre-positioned coil assembly. S303: Based on the pre-positioned coil assembly, a hot pressing embedding process is used, with local heating to 180°C, a downward pressure of 25N maintained for 10 seconds, and a coil embedding depth of 0.5±0.05mm to generate a coil embedded matrix.

[0009] Preferably, the generation of the thermal conductive-electromagnetic composite based on S4 comprises the following steps: S401: Based on the coil embedded matrix, a material drying process is performed to vacuum dry the AlN / PA66 composite material at 120°C for 4 hours with a moisture content of ≤0.02%, thereby generating a dry thermal conductive material; S402: Based on the dry thermal conductive material, a two-stage injection molding process is performed: the first stage: injection speed 80mm / s, pressure 80MPa, filling the coil gap; the second stage: injection speed 40mm / s, pressure 120MPa, completing the overall coating; generating the initial thermal conductive structure; S403: Based on the initially formed thermal conductive structure, an in-mold embossing process is used, maintained at 120°C / 15MPa for 30 seconds, to replicate the mold surface microstructure and generate a thermal conductive-electromagnetic composite.

[0010] Preferably, the generation of a three-dimensional stable structure based on S5 comprises the following steps: S501: Based on the thermal conductive-electromagnetic composite, a low-temperature shaping process is implemented, which is maintained in a nitrogen environment at 80°C for 30 minutes to eliminate internal stress and generate a stress-relieved matrix; S502: Based on the stress-relieved matrix, a crystallization strengthening process is performed, wherein the temperature is raised to 120°C at 3°C / min and kept at this temperature for 60 minutes, and the crystallinity is increased to 45%, thereby generating a semi-crystalline structure. S503: Based on the semi-crystalline structure, a high-temperature cross-linking process is used, maintained at 160℃ / 0.5MPa pressure for 30 minutes to form a three-dimensional cross-linked network and generate a three-dimensional stable structure.

[0011] Preferably, generating a multifunctional integrated component based on S6 includes the following steps: S601: Based on the three-dimensional stable structure, plasma treatment is performed using atmospheric pressure plasma and Ar / O2 mixed gas for 120 seconds to generate an activated surface matrix; S602: Based on the activated surface substrate, an atomic layer deposition process is performed to deposit a nano-aluminum oxide layer, with a precursor TMA / H2O, a cycle number of 200 times, and a growth rate of 0.11 nm / cycle to generate a nano-coating substrate; S603: Based on a nano-coated substrate, femtosecond laser etching is used with a wavelength of 1030nm, a pulse energy of 50μJ, and a processing groove depth of 50μm / width of 100μm, with a spacing of 200μm, to generate a multifunctional integrated component.

[0012] An integrated injection-molded wireless thermal conductive charging component, characterized in that: it includes an integrated injection-molded wireless thermal conductive charging component production process as described in any one of claims 1-7, the integrated injection-molded wireless thermal conductive charging component includes a first shell, the inner upper surface of the first shell is fixedly connected to a magnetic shield, the upper surface of the magnetic shield is fixedly connected to a coil, and the upper surface of the first shell is fixedly connected to a second shell.

[0013] The present invention provides an integrated injection-molded wireless thermally conductive charging assembly and its production process. It has the following beneficial effects: The present invention significantly improves the mold surface accuracy and thermal stability through a gradient temperature control process combined with nano-scale titanium nitride coating treatment, reduces material shrinkage and deformation during the injection molding process, and ensures that the dimensional tolerance of the soft magnetic matrix structure layer is controlled within ±0.05mm. In the twin-screw co-blending injection molding process, FeSiAl soft magnetic powder and PA6 substrate are melt-blended to achieve a uniform distribution of the soft magnetic phase in the matrix, increasing the magnetic permeability to above 120μ. At the same time, the coating effect of PA6 reduces eddy current loss by 15%. The visual positioning auxiliary process uses the CCD imaging system and vacuum adsorption to achieve a Litz coil embedding position deviation of less than 0.1mm. Combined with the gradient injection molding process, the AlN / PA66 composite material is filled in stages, and the coil gap filling rate exceeds 98%. The continuity of the thermal conductivity path is enhanced, and the thermal conductivity is increased to 5.8W / m·K. The gradient curing process regulates the crystallinity and cross-linking density in stages under nitrogen protection, raising the material's heat deformation temperature to 160°C and the flexural strength to 180MPa, avoiding structural deformation under high-temperature conditions. In the surface functionalization process, plasma treatment and nano-aluminum oxide coating work synergistically to increase the surface hardness to HV1200. The micro-groove structure formed by laser etching increases the heat dissipation area by 40%, achieving the comprehensive technical effects of increasing electromagnetic conversion efficiency by 12%, reducing temperature rise by 25°C, and increasing mechanical vibration tolerance by 3 times. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 It is a schematic diagram of the main steps of the present invention; Figure 2 This is a schematic diagram of the refinement of S1 of the present invention; Figure 3 This is a schematic diagram of the refinement of S2 of the present invention; Figure 4 This is a schematic diagram of the refinement of S3 of the present invention; Figure 5 This is a schematic diagram of the refinement of S4 of the present invention; Figure 6 This is a schematic diagram of the refinement of S5 of the present invention; Figure 7 This is a schematic diagram of the refinement of S6 of the present invention; Figure 8 It is a schematic diagram of the three-dimensional structure of the present invention; Figure 9 It is a split diagram of the present invention.

[0015] Among them, 1. first shell; 2. magnetic isolation; 3. coil; 4. first shell. DETAILED DESCRIPTION

[0016] The following will clearly and completely describe the technical solutions in the embodiments of the present invention in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of the present invention.

[0017] Example: like Figure 1-9 As shown, an embodiment of the present invention provides a production process for an integrated injection-molded wireless thermal conductive charging assembly, which is characterized by comprising the following steps: S1: Based on the mold pretreatment requirements, a gradient temperature control process is used to preheat the mold to 80±2℃ and maintain it for 30 minutes. At the same time, nano-scale titanium nitride surface coating treatment is applied to generate a high-precision pretreated mold; Gradient temperature control parameters: Preheating curve: 40℃→60℃(3℃ / min)→constant temperature 10min→60℃→80℃(1℃ / min) Titanium nitride coating process: Magnetron sputtering power: 3.2kW Deposition pressure: 0.3Pa Coating thickness: 1.5μm Surface hardness: HV2200 Comparative data: index Traditional molds This solution mold Demolding force (kN) 12.5 7.2 Surface roughness Ra (μm) 1.8 0.4 Service life (times) 3000 15000 S2: Based on the pre-treated mold, a twin-screw blending injection molding process was used to melt-blend FeSiAl soft magnetic powder and PA6 substrate at 280°C, and injected into the mold cavity at a pressure of 100 MPa with a holding time of 18 seconds to form a soft magnetic matrix structure layer; Material system: FeSiAl powder: particle size D50 = 15 μm (85 wt%) PA6 substrate: melt index 12g / 10min (230℃ / 2.16kg) Coupling agent: Silane KH560 (0.8wt%) Process parameters: Temperature of each zone of twin screw: Segment Zone 1 Zone 2 Zone 3 die head Temperature (℃) 235 255 275 270 Injection molding pressure holding curve: Performance testing: Magnetic permeability: 128μ (1MHz) Eddy current loss: 13W / kg (100kHz, 0.5T).

[0018] S3: Based on the soft magnetic matrix structure layer, a visual positioning-assisted process is used to guide the precise embedding of the Litz coil through the CCD imaging system, and 5kPa vacuum adsorption is simultaneously applied to fix it to form a coil-embedded matrix; Device configuration: Vision system: Basler ace 5MP camera + Schott cold light source Positioning algorithm: Feature matching based on deep learning (accuracy 99.7%) Robot: EPSON C4-A601S (repeat accuracy ±0.01mm) Accuracy verification: Test conditions X-axis error (μm) Y-axis error (μm) Angular error (°) normal temperature ≤±3 ≤±3 ≤0.02 Vibration environment ≤±5 ≤±5 ≤0.05 S4: Based on the coil-embedded matrix, a gradient injection molding process is implemented to inject AlN / PA66 composite materials in two stages: the first stage: 280℃ / 80MPa injection molding to fill the coil gap, and the second stage: 300℃ / 120MPa to complete the overall coating to form a thermal conductive-electromagnetic composite; Material formula: PA66: viscosity 2.8 (275°C) AlN filler: particle size 0.5 μm (oxygen content ≤ 0.5%) Dispersant: Titanate LICA38 (1.5wt%) Process control: parameter Phase 1 Phase II Melt temperature (℃) 275±3 295±3 Injection speed (mm / s) 85 45 Holding pressure (MPa) 35 55 Cooling time (s) 18 22 Microscopic analysis: SEM shows that AlN forms a three-dimensional network structure in the PA66 matrix, with the volume fraction near the coil area reaching 48%.

[0019] S5: Based on the thermal conductive-electromagnetic composite, a gradient curing process is used under nitrogen protection: 0-30 minutes: 80℃ low temperature setting, 30-60 minutes: 120℃ crystallization strengthening, 60-90 minutes: 160℃ cross-linking curing to form a three-dimensional stable structure; Phase change control: Low temperature stage: β crystal nucleation (crystallinity 18%→25%) Medium temperature stage: α crystal growth (spherulite size 8μm→15μm) High temperature stage: amide cross-linking (cross-linking density 2.8×10 -4 mol / cm 3 ) Mechanical properties: index Numerical Test standards Flexural strength (MPa) 185 ASTM D790 Heat deformation temperature (℃) 162 ASTM D648 <![CDATA[Coefficient of linear expansion (10 -6 / °C)]]> 28 ASTM E831 S6: Based on the three-dimensional stable structure, implement surface functionalization process, including: plasma surface treatment; nano-aluminum oxide coating deposition; laser microstructure etching to generate multifunctional integrated components.

[0020] Composite treatment process: Plasma treatment: Power density: 3W / cm 2 Gas ratio: Ar:O2=3:1 Processing time: 150s Atomic layer deposition: Precursor pulse time: TMA 0.1s / H2O 0.2s Number of cycles: 250 times Coating thickness: 35nm Laser etching: Wavelength: 1064nm Pulse frequency: 100kHz Etching pattern: Hexagonal honeycomb structure (cell size 200μm) Functional test: Comprehensive performance comparison: Performance indicators Traditional crafts This program Improvement Charging efficiency (%) 78 89 +14.1% Temperature rise (Δ℃) 42 23 -45.2% Vibration tolerance (g) 6 18 3 times Production cycle (min) 7.5 4.2 -44% <![CDATA[Power density (W / cm 3 )]]> 0.75 2.1 +180% Generating a high-precision pre-processed mold based on S1 includes the following steps: S101: Based on the mold surface cleaning requirements, a plasma cleaning process is used. Argon plasma is generated by a radio frequency power supply. The treatment time is 15 minutes, and the surface energy is increased to 72mN / m to generate a clean mold substrate. Plasma cleaning system: RF power parameters: 13.56MHz / 800W Processing chamber structure: parallel plate electrodes (spacing 50mm) Argon flow control: 20-50sccm (mass flow meter accuracy ±1%) Surface energy test: Using the hanging drop method, the contact angle was reduced from 105° to 12°. Process verification: After 15 minutes of treatment, XPS detection showed that the surface carbon contamination was reduced from 28at% to 3at%.

[0021] S102: Based on the clean mold substrate, a physical vapor deposition process is implemented to deposit a titanium nitride coating using magnetron sputtering. The target current is 3.5A, the deposition rate is 0.8nm / s, and the vacuum degree is 5×10 -3 Pa, generates the coating mold substrate; Magnetron sputtering device: parameter Numerical Control method Target purity 99.99% Ti GDMS testing Substrate rotation speed 5rpm Servo motor control Deposition uniformity ≤±3% Multi-point film thickness meter monitoring Coating analysis: AFM shows surface roughness Ra = 8.2nm, scratch test critical load LC2 = 45N.

[0022] S103: Based on the coated mold substrate, perform a gradient preheating process, raise the temperature to 80±2℃ at a rate of 5℃ / min, keep warm for 30 minutes, and the mold temperature uniformity is ≤±0.5℃ to generate a high-precision pretreated mold.

[0023] Gradient preheating system: Heating element: ceramic infrared heating plate (response time <3s); Temperature monitoring: 16-channel thermocouple (accuracy ±0.1°C); Thermal balance algorithm: PID + feedforward control. Effect verification: Mold temperature uniformity test shows a maximum temperature difference of 0.3°C.

[0024] The generation of a soft magnetic matrix structure layer based on S2 includes the following steps: S201: Based on the pre-treated mold, a material pre-mixing process is implemented to melt-blend FeSiAl powder and PA6 particles in a twin-screw extruder. The temperature is controlled in zones: feeding section 240°C → compression section 260°C → homogenization section 280°C to generate a soft magnetic composite melt. Twin screw configuration: Screw diameter: 35mm Aspect ratio: 40:1 Mixing element: kneading block + reverse thread combination Material properties: FeSiAl powder: oxygen content <0.1% (LECO analysis) PA6 moisture content: <0.05% (Karl Fischer method) Melt flow index: 25g / 10min (275℃ / 5kg).

[0025] S202: Based on the soft magnetic composite material melt, a high-speed injection molding process is used with an injection speed of 120 mm / s, a V / P switching point of 95% of the mold cavity volume, a peak pressure of 100 MPa, and a holding pressure curve of 80 MPa in the first 10 seconds → 60 MPa in the last 8 seconds to generate a preliminary soft magnetic structure; Injection molding machine parameters: Clamping force: 3500kN Screw diameter: 45mm V / P switching control: pressure sensor (accuracy ±0.5% FS) Molding quality: Three-dimensional measurement shows that the dimensional tolerance is ±0.05mm.

[0026] S203: Based on the initially formed soft magnetic structure, perform an in-mold annealing process, maintain 120°C / 15 minutes in the mold, cool at a rate of 2°C / min to 60°C for demoulding, and generate a soft magnetic matrix structure layer.

[0027] In-mold annealing system: Mold heating: Oil temperature machine temperature control (fluctuation ± 0.5 ℃) Cooling channel design: Conformal water channel (spacing 15mm) Demolding mechanism: Nitrogen spring ejection (pressure adjustable 0-20MPa) Metallographic analysis: After annealing, the grain size increases from 5μm to 15μm.

[0028] Generating a coil-embedded matrix based on S3 includes the following steps: S301: Based on the soft magnetic matrix structure layer, a visual positioning process is implemented, using a 5MP industrial camera and the Halcon algorithm to achieve a positioning accuracy of ±0.03mm, generate three-dimensional coordinate data, and generate a digital model for coil positioning; Vision system configuration: Camera: 5MP CMOS (pixel size 3.45μm) Lens: Bi-telecentric lens (depth of field ±1mm) Lighting: coaxial light + diffuse light combination Positioning algorithm: Halcon's shape-based matching is used, with a matching score > 0.85.

[0029] S302: Based on the positioning digital model, the robot guidance process is executed. The six-axis robot carries the Litz coil to the specified position, and the vacuum suction cup pressure is -85kPa to generate a pre-positioned coil assembly. Robot parameters: Repeatability: ±0.005mm Maximum acceleration: 15m / s 2 Tool center point calibration: Laser tracker (accuracy ±2μm) Vacuum system: Multi-stage Roots pump (ultimate vacuum 5×10 -3 Pa) + molecular pump group.

[0030] S303: Based on the pre-positioned coil assembly, a hot pressing embedding process is used, with local heating to 180°C, a downward pressure of 25N maintained for 10 seconds, and a coil embedding depth of 0.5±0.05mm to generate a coil embedded matrix.

[0031] Hot pressing device: Heating method: Pulse resistance heating (temperature control accuracy ±1°C) Pressure control: servo electric cylinder (resolution 0.1N) Depth detection: Laser displacement sensor (accuracy ±1μm) Embedding Quality: Confocal microscopy showed an embedding depth of 0.48 ± 0.03 mm.

[0032] The S4-based generation of a thermal-electromagnetic complex includes the following steps: S401: Based on the coil embedded matrix, a material drying process is performed to vacuum dry the AlN / PA66 composite material at 120°C for 4 hours with a moisture content of ≤0.02%, thereby generating a dry thermal conductive material; Drying equipment: Vacuum degree: <1<100Pa (two-stage rotary vane pump) Material layer thickness <3 <30mm (vibration laying mechanism) Humidity monitoring: dew point meter (-80℃ DP) Moisture content test: A halogen moisture meter (accuracy ±0.002%) was used.

[0033] S402: Based on the dry thermal conductive material, a two-stage injection molding process is performed: the first stage: injection speed 80mm / s, pressure 80MPa, filling the coil gap; the second stage: injection speed 40mm / s, pressure 120MPa, completing the overall coating; generating the initial thermal conductive structure; Two-stage injection molding parameters: parameter Phase 1 Phase II Melt temperature 275±3℃ 295±3℃ Injection time 1.8s 2.5s Cooling water temperature 60℃ 40℃ Flow analysis: Moldflow simulation shows that the shear stress is <0.8MPa (safety threshold).

[0034] S403: Based on the initially formed thermal conductive structure, an in-mold embossing process is used, maintained at 120°C / 15MPa for 30 seconds, to replicate the mold surface microstructure and generate a thermal conductive-electromagnetic composite.

[0035] In-mold embossing system: Imprinting pressure: 1515±0.2MPa (servo hydraulic) Microstructure mold: EDM (Ra = 0.1 μm) Release agent: Fluorine coating (contact angle>110°) Replication accuracy: The microstructure replication rate detected by white light interferometry is >98%.

[0036] Generating a three-dimensional stable structure based on S5 includes the following steps: S501: Based on the thermal conductive-electromagnetic composite, a low-temperature shaping process is implemented, which is maintained in a nitrogen environment at 80°C for 30 minutes to eliminate internal stress and generate a stress-relieved matrix; Low temperature setting equipment: Nitrogen purity: 99.999% (dew point <-70°C) Circulation wind speed: 0.5m / s (laminar flow control) Stress relief rate: 85% (measured by photoelastic method) DSC analysis: The glass transition temperature Tg increased from 65°C to 78°C.

[0037] S502: Based on the stress-relieved matrix, a crystallization strengthening process is performed, wherein the temperature is raised to 120°C at 3°C / min and kept at this temperature for 60 minutes, and the crystallinity is increased to 45%, thereby generating a semi-crystalline structure. Crystallinity control: Nucleating agent: nano talc (0.5wt%) Crystallization kinetics: Avrami index n = 2.8 Spherulite size: 15±2μm measured by polarized light microscope XRD analysis: The α crystal content increased from 30% to 75%.

[0038] S503: Based on the semi-crystalline structure, a high-temperature cross-linking process is used, maintained at 160℃ / 0.5MPa pressure for 30 minutes to form a three-dimensional cross-linked network and generate a three-dimensional stable structure.

[0039] Cross-linking system: Crosslinking agent: dicumyl peroxide (0.8 phr) Cross-linking agent: triallyl isocyanurate (0.3 phr) Network structure: TEM shows mesh size 20-50nm Mechanical properties: Impact strength from 8kJ / m 2 Increased to 22kJ / m 2 .

[0040] Generating a multifunctional integrated component based on S6 includes the following steps: S601: Based on the three-dimensional stable structure, plasma treatment is performed using atmospheric pressure plasma and Ar / O2 mixed gas for 120 seconds to generate an activated surface matrix; Plasma treatment: Electrode design: Rotating electric nozzle (speed 500rpm) Processing uniformity: ±5% (fluorescent dye test) Surface chemistry: XPS shows that the O content increases from 12at% to 28at% Adhesion test: Cross-cut method meets ASTM D3359 5B grade.

[0041] S602: Based on the activated surface substrate, an atomic layer deposition process is performed to deposit a nano-aluminum oxide layer, with a precursor TMA / H2O, a cycle number of 200 times, and a growth rate of 0.11 nm / cycle to generate a nano-coating substrate; ALD process parameters: parameter Numerical Control method Precursor pulse TMA 0.1s <![CDATA[H2O 0.2s]]> Purge time Nitrogen 20s Flow rate 10slm Growth monitoring Quartz crystal microbalance ±0.1nm Coating performance: Nanoindentation test hardness HV0.005=12GPa.

[0042] S603: Based on a nano-coated substrate, femtosecond laser etching is used with a wavelength of 1030nm, a pulse energy of 50μJ, and a processing groove depth of 50μm / width of 100μm, with a spacing of 200μm, to generate a multifunctional integrated component.

[0043] Laser processing system: Beam quality: M 2 <1.2 Scanning galvanometer: 8-bit resolution Focus control: Dynamic Z axis (response time <1ms) Functional testing: Infrared thermal imaging shows that heat dissipation efficiency has increased by 42%.

[0044] An integrated injection-molded wireless thermal conductive charging component, characterized in that: it includes an integrated injection-molded wireless thermal conductive charging component production process as described in any one of claims 1-7, the integrated injection-molded wireless thermal conductive charging component includes a first shell, the inner upper surface of the first shell is fixedly connected to a magnetic shield, the upper surface of the magnetic shield is fixedly connected to a coil, and the upper surface of the first shell is fixedly connected to a second shell.

[0045] While embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions, and variations may be made to these embodiments without departing from the principles and spirit of the invention, and that the scope of the invention is defined by the appended claims and their equivalents.

Claims

1. A production process for an integrated injection-molded wireless thermally conductive charging component, characterized in that The following steps are involved: S1: Based on the mold pretreatment requirements, a gradient temperature control process is used to preheat the mold to 80±2℃ and maintain it for 30 minutes. At the same time, nano-scale titanium nitride surface coating treatment is applied to generate a high-precision pretreated mold; S2: Based on the pre-treated mold, a twin-screw blending injection molding process was used to melt-blend FeSiAl soft magnetic powder and PA6 substrate at 280°C, and injected into the mold cavity at a pressure of 100 MPa with a holding time of 18 seconds to form a soft magnetic matrix structure layer; S3: Based on the soft magnetic matrix structure layer, a visual positioning-assisted process is used to guide the precise embedding of the Litz coil through the CCD imaging system, and 5kPa vacuum adsorption is simultaneously applied to fix it to form a coil-embedded matrix; S4: Based on the coil-embedded matrix, a gradient injection molding process is implemented to inject AlN / PA66 composite materials in two stages: the first stage: 280℃ / 80MPa injection molding to fill the coil gap, and the second stage: 300℃ / 120MPa to complete the overall coating to form a thermal conductive-electromagnetic composite; S5: Based on the thermal conductive-electromagnetic composite, a gradient curing process is used under nitrogen protection: 0-30 minutes: 80℃ low temperature setting, 30-60 minutes: 120℃ crystallization strengthening, 60-90 minutes: 160℃ cross-linking curing to form a three-dimensional stable structure; S6: Based on the three-dimensional stable structure, implement surface functionalization process, including: plasma surface treatment; nano-aluminum oxide coating deposition; laser microstructure etching to generate multifunctional integrated components.

2. The production process of an integrated injection-molded wireless thermally conductive charging assembly according to claim 1, characterized in that: Generating a high-precision pre-processed mold based on S1 includes the following steps: S101: Based on the mold surface cleaning requirements, a plasma cleaning process is used. Argon plasma is generated by a radio frequency power supply. The treatment time is 15 minutes, and the surface energy is increased to 72mN / m to generate a clean mold substrate. S102: Based on the clean mold substrate, a physical vapor deposition process is implemented to deposit a titanium nitride coating using magnetron sputtering, with a target current of 3.5A, a deposition rate of 0.8nm / s, and a vacuum degree of 5×10⁻³Pa to generate a coated mold substrate; S103: Based on the coated mold substrate, perform a gradient preheating process, raise the temperature to 80±2℃ at a rate of 5℃ / min, keep warm for 30 minutes, and the mold temperature uniformity is ≤±0.5℃ to generate a high-precision pretreated mold.

3. The production process of an integrated injection-molded wireless thermally conductive charging assembly according to claim 1, characterized in that: The generation of a soft magnetic matrix structure layer based on S2 includes the following steps: S201: Based on the pre-treated mold, a material pre-mixing process is implemented to melt-blend FeSiAl powder and PA6 particles in a twin-screw extruder. The temperature is controlled in zones: feeding section 240°C → compression section 260°C → homogenization section 280°C to generate a soft magnetic composite melt. S202: Based on the soft magnetic composite material melt, a high-speed injection molding process is used with an injection speed of 120 mm / s, a V / P switching point of 95% of the mold cavity volume, a peak pressure of 100 MPa, and a holding pressure curve of 80 MPa in the first 10 seconds → 60 MPa in the last 8 seconds to generate a preliminary soft magnetic structure; S203: Based on the initially formed soft magnetic structure, perform an in-mold annealing process, maintain 120°C / 15 minutes in the mold, cool at a rate of 2°C / min to 60°C for demoulding, and generate a soft magnetic matrix structure layer.

4. The production process of an integrated injection-molded wireless thermally conductive charging assembly according to claim 1, characterized in that: Generating a coil-embedded matrix based on S3 includes the following steps: S301: Based on the soft magnetic matrix structure layer, a visual positioning process is implemented, using a 5MP industrial camera and the Halcon algorithm to achieve a positioning accuracy of ±0.03mm, generate three-dimensional coordinate data, and generate a digital model for coil positioning; S302: Based on the positioning digital model, the robot guidance process is executed. The six-axis robot carries the Litz coil to the specified position, and the vacuum suction cup pressure is -85kPa to generate a pre-positioned coil assembly. S303: Based on the pre-positioned coil assembly, a hot pressing embedding process is used, with local heating to 180°C, a downward pressure of 25N maintained for 10 seconds, and a coil embedding depth of 0.5±0.05mm to generate a coil embedded matrix.

5. The production process of an integrated injection-molded wireless thermally conductive charging assembly according to claim 1, characterized in that: The S4-based generation of a thermal-electromagnetic complex includes the following steps: S401: Based on the coil embedded matrix, a material drying process is implemented to vacuum dry the AlN / PA66 composite material at 120°C for 4 hours with a moisture content of ≤0.02%, thereby generating a dry thermal conductive material; S402: Based on the dry thermal conductive material, a two-stage injection molding process is performed: the first stage: injection speed 80mm / s, pressure 80MPa, filling the coil gap; the second stage: injection speed 40mm / s, pressure 120MPa, completing the overall coating; generating the initial thermal conductive structure; S403: Based on the initially formed thermal conductive structure, an in-mold embossing process is used, maintained at 120°C / 15MPa for 30 seconds, to replicate the mold surface microstructure and generate a thermal conductive-electromagnetic composite.

6. The production process of an integrated injection-molded wireless thermally conductive charging assembly according to claim 1, characterized in that: Generating a three-dimensional stable structure based on S5 includes the following steps: S501: Based on the thermal conductive-electromagnetic composite, a low-temperature shaping process is implemented, which is maintained in a nitrogen environment at 80°C for 30 minutes to eliminate internal stress and generate a stress-relieved matrix; S502: Based on the stress-relieved matrix, a crystallization strengthening process is performed, heating to 120°C at 3°C / min and holding for 60 minutes, increasing the crystallinity to 45%, generating a semi-crystalline structure; S503: Based on the semi-crystalline structure, a high-temperature cross-linking process is used, maintained at 160℃ / 0.5MPa pressure for 30 minutes to form a three-dimensional cross-linked network and generate a three-dimensional stable structure.

7. The production process of an integrated injection-molded wireless thermally conductive charging assembly according to claim 1, characterized in that: Generating a multifunctional integrated component based on S6 includes the following steps: S601: Based on the three-dimensional stable structure, plasma treatment is performed using atmospheric pressure plasma and Ar / O2 mixed gas for 120 seconds to generate an activated surface matrix; S602: Based on the activated surface substrate, an atomic layer deposition process is performed to deposit a nano-aluminum oxide layer, with a precursor TMA / H2O, a cycle number of 200 times, and a growth rate of 0.11 nm / cycle to generate a nano-coating substrate; S603: Based on a nano-coated substrate, femtosecond laser etching is used with a wavelength of 1030nm, a pulse energy of 50μJ, and a processing groove depth of 50μm / width of 100μm, with a spacing of 200μm, to generate a multifunctional integrated component.

8. One-piece injection-molded wireless thermally conductive charging assembly, characterized by: A production process for an integrated injection-molded wireless thermal conductive charging component comprising the process described in any one of claims 1 to 7, wherein the integrated injection-molded wireless thermal conductive charging component comprises a first shell (1), a magnetic shield (2) is fixedly connected to the inner upper surface of the first shell (1), a coil (3) is fixedly connected to the upper surface of the magnetic shield (2), and a second shell (4) is fixedly connected to the upper surface of the first shell (1).