Production method of environment-friendly pigment yellow 83

By improving the production process of Pigment Yellow 83, removing harmful substances and improving crystal stability, the problem of excessive toxic substances in existing pigments has been solved, realizing the production of environmentally friendly pigments suitable for various environmental protection fields.

CN121873575APending Publication Date: 2026-04-17JIANGSU CAIRUI IND CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202511748900.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2025-05-21
Filing Date
2025-11-26
Publication Date
2026-04-17

AI Technical Summary

Technical Problem

Existing Pigment Yellow 83 products contain toxic aromatic amines and heavy metals, which cannot meet the requirements of the EU REACH regulation. Furthermore, the production process is environmentally polluting and cannot be used in food packaging and high-end decoration.

Method used

By improving the production process, including steps such as diazotization, coupling, pressure filtration, washing, and post-treatment, and using special additives and high-temperature pressure treatment, organic impurities and salts are removed, ensuring that the pigments do not contain prohibited aromatic amines and heavy metals. Furthermore, the unique post-treatment process improves the crystal stability and dispersibility of the pigments.

Benefits of technology

We produce an environmentally friendly pigment yellow 83 that is bright, light- and heat-resistant, and free of harmful substances. It is suitable for environmentally friendly water-based pigments, inkjet printing, powder coatings, and high-grade anti-corrosion paints, and is especially suitable for the food industry. It is environmentally friendly.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN121873575A_ABST
    Figure CN121873575A_ABST
Patent Text Reader

Abstract

According to the production method of the brand new environment-friendly pigment yellow 83 in the aspect of application, on the basis of a traditional production process, materials obtained after coupling reaction are subjected to filter pressing and washing, organic impurities and salt are removed, then a special high-speed beating machine is used for conducting high-speed beating on a filter cake, high-temperature and pressure treatment is conducted in a pressure kettle, and the pigment yellow 83 is obtained. According to the process, pigment particles are more sufficient in crystal transformation, more stable in crystal form and narrower in particle size distribution, and the obtained pigment yellow 83 is higher than industrial standards in terms of high gloss, high transparency and the like and does not contain forbidden aromatic amine or toxic substances.
Need to check novelty before this filing date? Find Prior Art

Claims

1. A method for producing environmentally friendly Pigment Yellow 83, characterized by, The method includes the following steps: S1, Diazotization reaction After diluting hydrochloric acid and acetic acid with water, 3,3'-dichlorobenzidine hydrochloride is added and stirred until completely dissolved. Then, ice is added to lower the temperature to 0-3°C, and sodium nitrite aqueous solution is added to carry out a medium diazotization reaction for 1-3 hours. The gas generated during the reaction is treated as waste gas. After the reaction is completed, aminosulfonic acid is added to remove excess sodium nitrite. Ice and water are added to maintain the temperature at 3-8°C to obtain a diazo solution for later use. S2, Coupling reaction After diluting the alkali with water, add 4-chloro-2,5-dimethoxyacetylaniline. After the solution is completely dissolved by stirring at room temperature, add water and ice to adjust the temperature to 25°C. Then add a dilute acetic acid solution prepared by dissolving 60% glacial acetic acid and 58% sodium acetate in water and perform acid precipitation for 0.5 to 1.5 hours until the pH value is between 6.0 and 6.

5. Add ice and water to adjust the temperature to 15-25°C, add emulsifier OS, and the coupling solution is ready for use. Add the resulting coupling solution to the diazo solution obtained in step S1 and carry out the coupling reaction for 3-3.5 hours. During the reaction, maintain the reaction temperature at 20-25℃ and control the reaction pH to 4-5 with liquid alkali. After coupling is complete, stir for 0.5 hours, then raise the temperature to 80-85℃ by heating with steam and keep it at that temperature for 0.5 hours before use. S3, Filtration, Washing The coupling product obtained in S2 is filtered by a filter press to separate the water from the obtained pigment. The wastewater generated by the filter press is sent to the sewage treatment plant for treatment. Water is added to the filter press to rinse the material until it is neutral. The wastewater generated after rinsing is sent to the sewage treatment plant for treatment. The filter cake is ready for use. S4, Post-processing Add the filter cake obtained from S3 to the reactor, add water to make up to 70-80% of the reactor volume, then add xylene, and slurry at 1000-1500 rpm for 30 minutes. Seal the reactor, raise the temperature to 110℃-125℃, keep it at that temperature for 2 hours, and recover the xylene for reuse. S5, pressure filtration, fine washing The product obtained from S4 is filtered again through a filter press. The wastewater generated from the filter press is treated in a sewage treatment plant. Water is added to the filter press to rinse the material until it is neutral. After rinsing, the material is blown off and set aside for use. The wastewater generated after rinsing and blowing off is treated in a sewage treatment plant. S6. Drying and pulverizing The filter cake obtained from S5 is dried at a temperature of 80-85℃ for 12 hours. The gas generated during drying is treated by dust removal. The collected dust is mixed with the filter cake and then dried until the moisture content is 0.5-1.5%. The gas that is not collected is treated as waste gas. After drying, the finished pigment yellow 83 is obtained.

2. The production method according to claim 1, characterized by, The molar ratio of dichlorobenzidine hydrochloride, sodium nitrite, and hydrochloric acid in S1 is 1:2-3:4-5.

3. The production method according to claim 1, characterized by, The molar ratio of cromoglycinate AS-IRG to alkali in S2 is 1:1 to 2.

4. The production method according to claim 1, characterized by, The alkali used in S2 is either liquid alkali or soda ash.

5. The production method according to claim 1, characterized by, In S2, the pH is adjusted by hydrochloric acid and liquid alkali, and the pH is stabilized by acetic acid.

6. The production method according to claim 1, characterized by, In S5, the material is rinsed until the conductivity is ≤100μs / cm.

7. The production method according to claim 1, characterized by, In S6, the filter cake is dried to a moisture content of ≤1.0%.

8. The production method according to claim 1, characterized by, The dried material obtained in S6 is then subjected to ultrafine pulverization.

9. The production method according to claim 1, characterized by, Huntsman L-207 and acetoacetanilide were heated at 85-90 degrees Celsius for 6 hours to prepare an auxiliary agent, which was added before the coupling reaction of the auxiliary agent S2.

10. The production method according to claim 9, characterized by, The molar ratio of the additive is 0.051.

Citation Information

Patent Citations

  • Industrial production method of low PCBs environmentally friendly yellow pigment PY83 for plastic cement

    CN109651836A