A processing method for open-end folding of a coreless hot coil box
By detecting sudden changes in the thickness of the intermediate billet and adjusting the shearing length of the flying shear system, the problem of opening and closing folds in the mandrel-less hot coil box was solved, equipment accidents were avoided, and production efficiency was improved.
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- ANGANG STEEL CO LTD
- Filing Date
- 2026-03-10
- Publication Date
- 2026-05-29
AI Technical Summary
Existing technologies have failed to effectively solve the problem of folding at the opening and closing of mandrel-less hot coil boxes, resulting in the inability of the inner end of the steel coil to open normally, causing the tail steel plate to fold, affecting production efficiency and potentially leading to serious equipment accidents.
By detecting sudden changes in the thickness of the intermediate billet, and utilizing the coordinated operation of the hot rolling box and the flying shear system, the shearing length is automatically adjusted to avoid the folded parts, enabling rapid shearing and notifying the operator.
This effectively avoids accidents such as blade breakage of flying shears and roll breakage in rolling mills caused by folding, thus improving production continuity and equipment protection.