A limiting baffle plate based on additive manufacturing and its manufacturing method

By using additive manufacturing technology to prepare the limiting baffle, the problems of large weight and complex manufacturing of existing baffles have been solved, and the uniformity of the gas passage and the thrust-to-weight ratio have been improved, ensuring the high reliability and rapid iteration capability of the engine.

CN123064602APending Publication Date: 2026-11-10YI BIN BEI FANG CHUAN AN HUA GONG YOU XIAN GONG SI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611534522.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-30
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

The existing propellant baffle is heavy and cannot effectively suppress the unilateral offset and accumulation of the propellant grain, resulting in asymmetrical gas passage, affecting thrust eccentricity and external ballistic performance. Moreover, the manufacturing process is complex and time-consuming, making it difficult to meet the needs of rapid iteration.

Method used

Using additive manufacturing technology, a limiting baffle plate is prepared by 3D printing. The limiting components and limiting bosses in the annular channel are designed to separate independent charging areas. Combined with GH4169 nickel-based high-temperature alloy powder and specific heat treatment, lightweight and high strength are achieved.

Benefits of technology

It achieves uniformity of gas flow, eliminates thrust eccentricity, improves thrust-to-weight ratio, shortens manufacturing cycle, and enhances material utilization and engine reliability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123064602A_ABST
    Figure CN123064602A_ABST
Patent Text Reader

Abstract

This invention discloses a propellant deflector plate based on additive manufacturing and its manufacturing method, belonging to the field of aerospace solid propulsion technology. The deflector plate is integrally printed using selective laser melting technology, including a central hole and an annular channel surrounding the central hole. The annular channel has a skeleton array structure, consisting of multiple circumferentially arranged deflector components and support arms connecting each deflector component. A flow channel for propellant gas is formed between the support arms. The deflector components include radial deflector partitions and deflector bosses. The deflector bosses are located between adjacent support arms and divide the annular channel into several independent propellant deflector regions of equal volume, used to physically isolate and prevent propellant from shifting and accumulating to one side. This invention fundamentally eliminates the thrust eccentricity problem of multi-nozzle engines through a cavity deflector structure, and the overall weight is reduced by combining it with a 3mm thin-walled skeleton design.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of solid propulsion technology in aerospace, specifically to a limiting baffle plate based on additive manufacturing and its manufacturing method. Background Technology

[0002] Solid rocket engines are widely used in tactical missiles, launch vehicles, and spacecraft orbit-changing engines due to their simple structure, high reliability, and long-term storage capability. The propellant baffle is a key component within the combustion chamber, primarily used to secure the propellant grain, preventing displacement under gravity, launch overload, and combustion pressure fluctuations, and providing insulation and blocking during the final stages of combustion.

[0003] With increasing demands for thrust-to-weight ratio and maneuverability in space missions, the application of porous annular propellant charges or multiple sub-charges is becoming more common. Existing propellant deflectors are mostly made of stainless steel or heat-resistant alloys, manufactured through CNC milling of forged blanks or by separate stamping followed by welding. The above structures and processes present the following problems in practical applications: Under lateral overload, propellant grains are prone to unilateral shift and accumulation. In annular charge structures, when a missile performs large maneuvers or experiences high lateral overloads at launch, multiple individual propellant grains or internal combustion chamber supports are prone to circumferential sliding within the annular space. Once the propellant grains shift and accumulate to one side of the circumference, the cross-sectional area of ​​the gas passage on that side decreases or even becomes blocked, while a larger flow passage is formed on the other side. For multi-nozzle annular engines, asymmetry in the gas passages will cause distortion of the total pressure at the inlet of each nozzle, resulting in an asymmetric thrust vector, i.e., thrust eccentricity, which in turn affects attitude control and external ballistic performance; in severe cases, it can lead to increased ballistic dispersion, increased miss distance, or even flight failure.

[0004] Existing detonator plates struggle to balance lightweight design with resistance to stacking. Solid metal or thick-walled detonator plates are too heavy, which is detrimental to improving the thrust-to-weight ratio. If the wall thickness is reduced or the structure is simplified to reduce weight, the constraint and insulation of the propellant grain are weakened, making it difficult to stably suppress unilateral stacking of the propellant grain.

[0005] Traditional manufacturing processes have poor adaptability. When machining complex integral structures using CNC machining, tool accessibility is limited. When using modular welding, coaxiality and connection accuracy are difficult to guarantee, and welds are prone to becoming crack initiation points and ablation weak points under the scouring of high-temperature combustion gases. Nickel-based superalloys are difficult to machine; material utilization in subtractive manufacturing is typically less than 30%, and manufacturing cycles can last for several weeks, making it difficult to meet the demands of rapid iteration.

[0006] Therefore, existing drug-blocking plates are insufficient to meet the requirements in terms of lightweight design, unilateral offset stacking of anti-drug columns, manufacturing cost, and cycle time. Summary of the Invention

[0007] To address the aforementioned problems, this invention provides a lightweight propellant anti-accumulation baffle plate based on additive manufacturing and its manufacturing method. The purpose is to overcome the shortcomings of existing baffle plates, such as large weight and difficulty in effectively suppressing unilateral displacement and accumulation of propellant grains. This invention reduces the weight of the baffle plate, blocks the unilateral accumulation channel of the propellant grain, ensures balanced gas supply to each nozzle, and eliminates the root cause of thrust eccentricity.

[0008] This invention is achieved through the following scheme: A limit baffle plate based on additive manufacturing is 3D printed in one piece. It includes a central hole and an annular channel around the central hole presents a skeleton array structure. The annular skeleton array structure includes multiple limit members arranged in a circumferential array. Each limit member is connected by a support arm. The gap between each support arm forms a guide channel for gas to pass through. The annular channel of the baffle plate is circumferentially distributed with at least one ring of limiting members. The limiting members include a radial limiting partition and a limiting boss that extends outward from the circumferential of the limiting partition. The limiting boss is disposed between adjacent support arms. The limiting members divide the annular channel inside the baffle plate into several independent charging limiting areas with equal volume, which are used to physically isolate and prevent multiple propellant charges or combustion chamber support members from displacing and accumulating to one side. The radial limiting partition, the support arm, and the bottom of the limiting boss are located on the same plane, and the top of the limiting boss is higher than the thickness of the support arm and the radial limiting partition.

[0009] Furthermore, the thickness of the radial limiting partition and the support arm is no more than 3mm.

[0010] Furthermore, the baffle plate includes a central inner ring, an outer outer ring, and multiple support arms connecting the inner and outer rings, with a ring-shaped skeleton array structure disposed between the outer and inner rings; the aperture of the central inner ring is 12mm-13mm.

[0011] Furthermore, the diameter of the central inner ring is 12.5 mm; the load-bearing wall thickness of the radial limiting partition and support arm is 3 mm.

[0012] Furthermore, the circumferential array arrangement consists of multiple rings of limiting members distributed circumferentially along the annular channel of the deflector plate. The supporting arms between the limiting members in the same ring form a structural ring, and the supporting arms between the limiting members in each ring are radially connected; the independent deflector limiting areas have equal volumes.

[0013] Furthermore, the limiting component is a ring, and the limiting boss is a cantilever structure with a lateral bayonet at the height position.

[0014] Furthermore, the powder raw materials for 3D printing are GH4169 nickel-based high-temperature alloy spherical metal powder or 17-4PH stainless steel spherical metal powder. The particle size of the spherical metal powder is distributed between 15μm and 53μm, and the flowability is controlled between 20S and 45S.

[0015] An additive manufacturing method for a medicine shield includes the following steps: Step S1: Based on the airflow mechanics and stress requirements of the engine cavity, construct a 3D model of a hollowed-out propellant baffle with a limiting partition, and import it into SLM slicing software. The preset printing layer thickness is 30μm~50μm. According to the cantilever structure characteristics of the propellant baffle, perform spatial deformation-prevention compensation design in CAD software, and adopt a partitioned staggered scanning strategy to reduce internal microscopic thermal stress.

[0016] Step S2: In a selective laser melting device protected by an inert atmosphere with an oxygen content of less than 500 ppm, spherical metal powder is used. The powder is laid layer by layer and laser melted layer by layer at a laser power of 200W–400W, a scanning speed of 700mm / s–1100mm / s, and a scanning interval of 0.08mm–0.12mm, forming a baffle plate blank in one piece. By controlling the solidification and cooling rate of the molten pool, the microstructure of the printed part exhibits fine cellular and columnar crystal morphologies, avoiding the macroscopic segregation and coarse grains commonly found in traditional casting.

[0017] Specifically, the metal powder is GH4169 nickel-based high-temperature alloy powder with a sphericity of ≥95%, and the particle size distribution is between 15μm and 53μm. The Hall flow rate is controlled within 20S to 45S, and the loose packing density is ≥4.4g / cm3, ensuring that there is no agglomeration or voids in the powder spreading process.

[0018] Step S3: After printing, the part cools to room temperature along with the substrate. The baffle blank is then cut off from the substrate using wire cutting. For any residual metal powder in the internal limit slits of the baffle, a combination of high-pressure air blowing and ultrasonic alcohol solution cleaning is used to thoroughly clean the inner cavity.

[0019] Step S4: Heat Treatment Strengthening. Since rapid cooling of the SLM leaves residual tensile stress along the printing direction inside the part, this invention performs specific heat treatment on the cleaned baffle blank. First, a solution treatment is performed: heating to 1020℃±15℃ and holding for 1 hour, followed by water cooling to room temperature, promoting the re-dissolution of solute elements into the matrix; then, a two-stage aging treatment is performed: first heating to 720℃±15℃ and holding for 8 hours, then slow cooling in the furnace to 620℃±15℃ and holding for 8 hours, and finally air cooling to room temperature.

[0020] This heat treatment process allows for the formation of nanoscale γ" and γ´ reinforcing phases in the fine-grained structure of 3D printed materials, resulting in a 15% to 20% increase in the strength of the parts at both room temperature and high temperature compared to traditional forged materials.

[0021] Step S5: Hot Isostatic Pressing After solution treatment and two-stage aging treatment, hot isostatic pressing (HIP) treatment can be optionally added to eliminate micropores inside the parts and further improve density and mechanical properties.

[0022] In summary, due to the adoption of the above technical solution, the beneficial effects of the present invention are: 1) Cavity-based limiting prevents accumulation and ensures coaxiality of thrust vectors across multiple nozzles. By arranging limiting components and protrusions within the annular cavity, the annular channel is divided into several independent propellant-limiting areas, physically limiting the circumferential displacement of the propellant column. Regardless of the direction of lateral overload, the propellant columns in each limiting compartment cannot cross the partition and converge to the same side, thus ensuring uniform gas flow and constant pressure in front of each nozzle. This eliminates thrust eccentricity caused by changes in gas flow between nozzles, ensuring the aircraft is not disturbed by lateral alternating moments during the active phase of flight, and improving external ballistic accuracy and impact point density.

[0023] (2) Lightweight design improves thrust-to-weight ratio. Using SLM additive manufacturing technology, the load-bearing wall thickness of the propellant baffle can be as thin as 3mm. Combined with the ring frame and limiting partition structure, the overall weight is reduced by about 40% to 60% compared with the traditional solid disc structure. The weight reduction is directly converted into a higher thrust-to-weight ratio, which improves the rocket's flight speed or carrying capacity.

[0024] (3) Seamless integral molding with strong thermal shock resistance. The parts have no welds, threads, or splicing gaps. The fine-grained structure generated by the rapid solidification of SLM, combined with the optimized heat treatment process, makes the density of the propellant baffle reach more than 99%, and the room temperature tensile strength is stable at more than 1450MPa. Under the working environment of 800℃ to 1000℃, the strength decay rate is low, and the propellant baffle will not fall off due to weld cracking after thermal cycling, thus improving the reliability of the engine.

[0025] (4) Short manufacturing cycle and high material utilization. Using additive manufacturing technology and metal powder as raw material, the parts can be manufactured in a few days, shortening the manufacturing cycle by about 70% compared with the traditional process; the remaining powder after printing can be recycled and reused, significantly improving the material utilization rate. Attached Figure Description

[0026] Figure 1 This is a table showing the mechanical and physical properties of the GH4169 metal 3D printing powder and molded parts used in the embodiments of the present invention under different conditions. Figure 2 This is a schematic diagram of a partial structure of the medicine-blocking plate of the present invention; Figure 3 This is a schematic diagram of the overall structure of the medicine-blocking plate of the present invention; Figure 4 This is a top cross-sectional view of the internal annular arrangement and circumferential limiting partition structure of the medicine baffle plate of the present invention.

[0027] Figure 5 This is a physical image of the integrated metal baffle plate of the present invention after SLM printing, heat treatment and surface treatment.

[0028] Figure label: 1-Inner ring; 2-Outer ring; 3-Support arm; 4-Limiting component; 41-Limiting partition; 42-Limiting boss; 5-Guide channel. Detailed Implementation

[0029] The present invention will be further described in detail below with reference to the accompanying drawings and specific embodiments. The following embodiments are for illustrative purposes only and are not intended to limit the scope of protection of the present invention.

[0030] Example 1 This embodiment provides a 3D-printed propellant baffle with anti-stacking limit, suitable for multi-channel annular solid rocket motors, especially multi-nozzle annular motors equipped with multiple nozzle assemblies.

[0031] like Figures 1 to 5 As shown, the baffle plate in this embodiment is integrally printed using selective laser melting (SLM) technology. The baffle plate has an overall annular thin-walled dot matrix structure with a through hole in the center, the diameter of which is 12.5 mm. In the annular channel of the baffle plate, limiting members 4 are distributed in a circumferential array. Each limiting member 4 is connected by a support arm 3, and the gap between each support arm 3 forms a guide channel 5 for the gas to pass through.

[0032] Each limiting member 4 includes a radial limiting partition 41 and a limiting boss 42 extending circumferentially outward from the radial limiting partition 41. The limiting boss 42 is located in the gap between adjacent support arms 3. The thickness of the radial limiting partition 41 is 3mm, and the wall thickness of the support arm 3 is also 3mm. The bottoms of the radial limiting partition 41, the support arm 3, and the limiting boss 42 are located on the same plane, and the top of the limiting boss 42 is higher than the thickness of the support arm 3 and the radial limiting partition 41.

[0033] The limiting component 4 evenly divides the entire annular propellant loading area into multiple independent fan-shaped propellant loading chambers, each with an equal volume.

[0034] The limiting boss 42 extends outward along the radial limiting partition 41 and is positioned in the gap between adjacent support arms 3. The limiting boss 42 is higher in height than the thickness of the support arm 3 and the limiting partition 41, forming a circumferential barrier. When the engine is subjected to high lateral overload, its shear strength directly blocks the inertial displacement of the propellant or internal support components. It disperses and constrains the accumulated force, which might otherwise slide to one side, within each independent limiting compartment, fundamentally ensuring the uniformity of the cross-sectional area of ​​the gas passages in all directions. This ensures a balanced gas supply flow in each nozzle of the multi-nozzle structure, ultimately achieving absolute axisymmetry of the engine thrust vector and eliminating the physical root cause of thrust eccentricity.

[0035] In this embodiment, the medicine-blocking plate includes a central inner ring 1, an outer outer ring 2, and multiple support arms 3 connecting the central inner ring 1 and the outer outer ring 2. The aperture of the central inner ring is preferably 12.5 mm. The support arms 3 connect the inner ring 1 and the outer ring 2 radially, and a ring-shaped skeleton array structure is arranged between the outer ring 2 and the inner ring 1.

[0036] Example 2 To further improve the limiting stability of the medicine baffle when subjected to severe bidirectional vibration, this embodiment provides a modified example of the limiting structure.

[0037] Based on the basic radial partition structure of Example 1, in this example, each limiting partition is designed with an outwardly protruding L-shaped or T-shaped slot structure at the top and bottom, and the slot depth is 2mm.

[0038] Building upon the existing blocking mechanism, a limiting latch function has been added. When the propellant charge experiences severe axial reciprocating vibrations in the lateral direction, the L-shaped slot physically engages the end region of the propellant charge, preventing it from veering over the baffle due to high-frequency vibrations under certain extreme conditions. This more complex slot-shaped limiting structure is still achieved through one-time molding using SLM additive manufacturing technology, eliminating the need for secondary assembly and further enhancing the safety redundancy of the propellant baffle.

[0039] Example 3 This embodiment provides an additive manufacturing method for the medicine-blocking plate described in the above embodiment, and the specific steps are as follows: GH4169 spherical powder was selected. The powder sphericity is ≥95%, the particle size distribution is 15μm~53μm, the surface is smooth and there are no satellite powders, the loose density is 4.4g / cm3, and the flowability measured by the Hall flowmeter is 45S, ensuring that there is no agglomeration or voids in the powder spreading process.

[0040] SLM equipment was selected. The printing layer thickness was preset to 40 μm in an argon-protected chamber with an oxygen content below 500 ppm. The laser power was set to 280 W, the scanning speed to 900 mm / s, and the scanning spacing to 0.10 mm. A partitioned, staggered scanning strategy was employed to control the heat input layer by layer. The cooling rate reached 10... 5 ~10 6 K / s results in extremely fine grains inside the printed state.

[0041] Heat treatment process. The printed baffle plate is strengthened in a vacuum heat treatment furnace: heated to 1020℃±5℃, held for 1 hour, and then rapidly water quenched; then heated to 720℃±5℃ and held for 8 hours; then slowly cooled to 620℃±5℃ at a cooling rate of ≤50℃ / h and held for 8 hours before air cooling. This heat treatment process promotes the uniform dispersion and precipitation of a large number of nano-scale γ" phase (Ni3Nb) at the grain boundaries, which plays a very strong pinning and strengthening role, resulting in a final part with a tensile strength >1450MPa, a yield strength >1000MPa, and a hardness of 455HB at room temperature.

[0042] Example 4 This embodiment uses 17-4PH martensitic precipitation-hardening stainless steel powder as the printing material. When the engine operating temperature is below 700℃, to reduce manufacturing costs, 17-4PH martensitic precipitation-hardening stainless steel powder is used as the printing material, supplemented by the same SLM process as in the above embodiment. After aging treatment at 475℃, the tensile strength of the baffle plate is ≥1250MPa, and the hardness is 32~42HRC, meeting the usage requirements. While maintaining the same limiting structure, material replacement using 3D printing technology is extremely convenient, requiring no changes to tooling molds, demonstrating the strong material compatibility of additive manufacturing.

[0043] This invention fundamentally solves the thrust eccentricity problem of multi-nozzle engines through an integrated limiting structure, effectively ensuring external ballistic accuracy. Simultaneously, the component boasts a density ≥99%, tensile strength ≥1450MPa, and an operating temperature exceeding 800℃, achieving a balance between lightweight design and high reliability under extreme conditions. It is applicable to multi-nozzle annular solid rocket motors or gas generators.

[0044] The structure of the baffle plate employs a 3mm thin-walled skeleton array, printed using SLM (Selective Laser Melting) equipment. This requires the molding material to meet two mutually restrictive technical specifications: high yield strength and excellent SLM molding flowability. For example... Figure 1As shown, this invention fully leverages the precipitation strengthening advantage of GH4169 powder through a specific SLM process and two-stage aging heat treatment. Its yield strength can reach over 1000 MPa, resisting the severe vibrations during engine operation and the shear forces from high overloads exceeding 20G. Simultaneously, it ensures the compactness of the 3mm thin-walled structure during printing, avoiding incomplete fusion defects at the limiting slits. This solves the technical problem of plastic deformation in thin-walled blast deflectors under high overloads, while simultaneously meeting the dual requirements of thin-walled formability and high overload bearing capacity.

[0045] All features disclosed in this specification, or all steps in all disclosed methods or processes, may be combined in any way, except for mutually exclusive features and / or steps.

[0046] Any feature disclosed in this specification (including any appended claims and abstract) may be replaced by other equivalent or similar features unless specifically stated otherwise.

[0047] In the description of this invention, it should be understood that the terms "upper", "lower", "left", "right", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this invention.

[0048] Furthermore, the terms “first,” “second,” etc., are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined with “first,” “second,” etc., may explicitly or implicitly include one or more of that feature.

Claims

1. A limiting baffle plate based on additive manufacturing, characterized in that, The baffle plate is 3D printed in one piece and includes a central hole. The annular channel around the central hole presents a skeleton array structure. The annular skeleton array structure includes multiple limiting members arranged in a circumferential array. Each limiting member is connected by a support arm. The gap between each support arm forms a guide channel for gas to pass through. The annular channel of the baffle plate has at least one ring of limiting members distributed around its circumference. The limiting members include a radial limiting partition and a limiting boss extending outward from the limiting partition. The limiting boss is disposed between adjacent support arms. The limiting members divide the annular channel inside the baffle plate into several independent charging limiting areas with equal volume, which are used to physically isolate and prevent multiple propellant charges or combustion chamber support members from shifting and accumulating to one side. The radial limiting partition, the support arm, and the bottom of the limiting boss are located on the same plane, and the top of the limiting boss is higher than the thickness of the support arm and the radial limiting partition.

2. A limiting baffle plate based on additive manufacturing according to claim 1, characterized in that, The thickness of the radial limiting partition and support arm is no more than 3mm.

3. A limiting baffle plate based on additive manufacturing according to claim 1, characterized in that, The medicine baffle includes a central inner ring, an outer outer ring, and multiple support arms connecting the inner ring and the outer ring. A ring-shaped skeleton array structure is disposed between the outer ring and the inner ring. The aperture of the central inner ring is 12mm-13mm.

4. A drug-stopping plate based on additive manufacturing according to claim 3, characterized in that, The diameter of the central inner ring is 12.5 mm; the load-bearing wall thickness of the radial limiting partition and support arm is 3 mm.

5. A drug-stopping plate based on additive manufacturing according to claim 1, characterized in that, The circumferential array arrangement consists of multiple rings of limiting members distributed circumferentially along the annular channel of the deflector plate. The supporting arms between the limiting members in the same ring are connected to form a structural ring, and the supporting arms between the limiting members in each ring are connected radially. The independent deflector areas have equal volumes.

6. A limiting baffle plate based on additive manufacturing according to claim 1, characterized in that, The limiting component is a ring, and the limiting boss is a cantilever structure with a lateral bayonet at the height position.

7. A drug-stopping plate based on additive manufacturing according to claim 1, characterized in that, The powder raw materials for 3D printing are GH4169 nickel-based high-temperature alloy spherical metal powder or 17-4PH stainless steel spherical metal powder. The particle size of the spherical metal powder is distributed between 15μm and 53μm, and the flowability is controlled between 20S and 45S.

8. A method for manufacturing a limiting baffle plate based on additive manufacturing as described in any one of claims 1 to 7, characterized in that, Includes the following steps: Construct a 3D model of the drug-blocking plate with a ring-shaped skeleton array structure and import it into slicing software; In a selective laser melting device protected by an inert atmosphere with an oxygen content of less than 500 ppm, spherical metal powder is used. With a laser power of 200W to 400W, a scanning speed of 700mm / s to 1100mm / s, and a scanning interval of 0.08mm to 0.12mm, powder is laid layer by layer and laser melting is performed layer by layer to form a baffle plate blank in one piece. After printing, the part is cooled to room temperature along with the substrate. The baffle blank is separated from the substrate using wire cutting, and residual powder in the gaps of the internal limiting structure of the part is removed. The cleaned baffle blanks are subjected to heat treatment: first, they are heated to 1020℃±15℃ and held for 1 hour for solution treatment and then water-cooled; then they are heated to 720℃±15℃ and held for 8 hours, furnace-cooled to 620℃±15℃ and held for 8 hours for two-stage aging treatment, and finally air-cooled to room temperature.

9. The method for manufacturing the limiting baffle plate according to claim 8, characterized in that, The preset printing layer thickness is 30μm to 50μm, and a partitioned block staggered scanning strategy is set to carry out spatial anti-deformation compensation design.

10. The method for manufacturing the limiting baffle plate according to claim 8, characterized in that, Following solution treatment and two-stage aging treatment, the process also includes hot isostatic pressing of the baffle plate.