Cosmetic coating component, manufacturing method of cosmetic coating component, and cosmetic coating tool
By using cosmetic coating components made of sintered porous plastic and synthetic fiber porous bodies, the problem of wear and tear on the shape and pattern of cosmetic coating tools during use has been solved, achieving stability of shape and pattern and a good skin feel.
Patent Information
- Application Number
- CN202580022835.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-05-01
- Filing Date
- 2025-04-08
- Publication Date
- 2026-11-10
AI Technical Summary
Existing cosmetic application tools cannot maintain their shape or pattern before and after use. In particular, the markings, bevels, and corners of stick cosmetic application parts, such as lipsticks, are easily worn away and disappear.
The outer component is made of sintered porous plastic with a porosity of 30% to 70%, while the inner shaft component is made of porous synthetic fiber and/or synthetic resin with a greater porosity than the outer component. The inner shaft component is molded and inserted to form a cosmetic coating component with bevels and decorative patterns.
It achieves the maintenance of the shape and decorative pattern of the cosmetic coating component before and after use, provides a good skin feel and a stable coating amount, and improves the service life of the cosmetic coating tool.
Smart Images

Figure CN123076331A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to a cosmetic coating component, a method for manufacturing the cosmetic coating component, and a cosmetic coating tool. More particularly, it relates to a rod-shaped cosmetic coating component that maintains its shape both before and after use. Background Technology
[0002] The following manufacturing method is used for stick-shaped cosmetic coating parts such as lipsticks: a material containing oil or pigment is poured into an Ogive mold or a mold as described in Patent Document 1 and then cured.
[0003] In particular, Augiev molds are made of elastically deformable resin materials, so even shapes that cannot be demolded in the mold can be formed, and three-dimensional patterns can be applied. They are mostly used to form rod-shaped cosmetic coating parts.
[0004] On the other hand, by using a mold, as in Patent Document 2, fine irregularities are also formed on the front end of the cosmetic coating component. The mold has the advantage of not requiring frequent replacements like Augie molds.
[0005] However, regardless of the molding method, typical stick-shaped cosmetic applicators color the surface by transferring pigments along with the oil components in the raw material onto the skin or other objects. Therefore, with each use, the cosmetic applicator material wears away and is shaved off, changing its shape, and engravings and other patterns quickly wear away and disappear. Regarding cosmetic applicators such as lipsticks, many consumers prioritize brand when purchasing them, demanding that logos and other engraved patterns not be easily shaved off. Furthermore, they require that the beveled, angled, or polygonal shapes of the tip of the lipstick or similar product not be simply round bars.
[0006] Existing technical documents
[0007] Patent documents
[0008] Patent Document 1: Japanese Patent Application Publication No. 2014-045985
[0009] Patent Document 2: Japanese Patent Application Publication No. 2008-278976 Summary of the Invention
[0010] The technical problem to be solved by the invention
[0011] The present invention was made in view of the above situation, and it solves the problem that the shape or pattern cannot be maintained before and after the use of conventional cosmetic application tools such as lipstick.
[0012] Means for solving technical problems
[0013] To address the aforementioned issues, a cosmetic coating component is provided, comprising an outer component and an inner shaft component. The outer component is generally rod-shaped and has an axial recess extending from its rear end toward its front end. The inner shaft component is configured to abut against the inner surface of the recess in the outer component. The outer component is made of sintered porous plastic with a porosity of 30% to 70%, maintaining its shape before and after use. The inner shaft component is made of a porous body of synthetic fibers and / or synthetic resin, and its porosity is greater than that of the outer component.
[0014] The sintered porous plastic of the outer component can be sintered polyethylene.
[0015] The cosmetic coating component may have a bevel formed relative to the axial direction at the front end portion of the surface of the outer component.
[0016] The cosmetic coating component may have fine concave or fine convex decorative patterns on the surface of the outer component.
[0017] The manufacturing method of the cosmetic coating component of the present invention is characterized by comprising the following steps: preparing a mold having the shape of the surface of the outer component and the shape of the recess of the outer component; filling the mold with particulate plastic material; heating the particulate plastic material to form the outer component; removing the outer component formed in the forming step; and inserting the inner shaft component into the recess of the outer component.
[0018] Preferably, the mold is formed by combining a first mold having the shape of the front end portion of the outer component and a second mold having the shape of the side portion other than the front end portion of the outer component and the shape of the recess.
[0019] The cosmetic coating tool of the present invention uses the above-described cosmetic coating component.
[0020] The cosmetic coating tool of the present invention is manufactured by the above-described method for manufacturing cosmetic coating components.
[0021] Invention Effects
[0022] According to the present invention, a rod-shaped cosmetic coating component and a cosmetic coating tool are provided that can maintain a three-dimensional shape that is easily applied to the object to be coated, such as a shape or mark. Attached Figure Description
[0023] Figure 1 An example of the cosmetic coating component of the present invention is shown. Figure 1 (a) is an example of a front view. Figure 1 (b) is an example of a diagram showing the axial rear end portion viewed from the side. Figure 1(c) is an example of a longitudinal section view.
[0024] Figure 2 This illustrates another example of the cosmetic coating component of the present invention. Figure 2 (a) is an example of a mark engraved in the central part of the outer component. Figure 2 (b) is an example of marking the front end of the outer part.
[0025] Figure 3 An example of a mold representing the present invention. Figure 3 (a) is an example of a longitudinal section view. Figure 3 (b) is based on Figure 3 Example of a longitudinal section view with the axis of (a) rotated 90° around the center. Figure 3 (c) is an example of a diagram showing the rear end of the mold viewed from the side.
[0026] Figure 4 An example of a cosmetic coating tool of the present invention is shown. Figure 4 (a) is an example of a cosmetic application component installed and contained in a screw-out container. Figure 4 (b) is an example of when the cosmetic coating part is unscrewed from the container. Detailed Implementation
[0027] Hereinafter, the coating tool of the present invention will be described with reference to the accompanying drawings and using appropriate symbols, but the embodiments are not limited thereto.
[0028] In addition, in this application specification, "front end" refers to the foremost end (position) of the coating side of the cosmetic coating tool in each part or section, "rear end" refers to the last end (position) of the cosmetic coating tool on the side opposite to the coating side in each part or section, "front end portion" refers to the front end and the portion near the front end in each part, "rear end portion" refers to the portion near the rear end and the rear end in each part, and "central portion" refers to the portion near the center in the axial direction of each part between the front end portion and the rear end portion. Furthermore, "front end side" refers to the coating side, and "rear end side" refers to the side opposite to the coating side.
[0029] The cosmetic coating component 1 of the present invention includes an outer component 2 and an inner shaft component 3.
[0030] The outer component 2 is generally rod-shaped and has a recess along the axial direction from the rear end toward the front end. An inner shaft component 3 is provided on the inner side of this recess in an abutting manner. The shape of the recess is not limited to cylindrical or polygonal prism shapes, as long as it allows for demolding using the mold described later. However, a cylindrical shape is preferred for ease of insertion of the inner shaft component 3 into the recess.
[0031] Furthermore, the front end of the recess, when viewed in longitudinal section, can be perpendicular to the axial direction or have an arc shape. It can be any shape as long as the inner shaft component 3 can be inserted.
[0032] Within the range of maintaining the shape of the outer component 2 before and after use, the depth of the recess only needs to be within the axial length of the outer component 2, and the diameter of the recess only needs to be within the outer diameter of the outer component 2. The inner shaft component 3, inserted into the recess of the outer component 2, holds the cosmetic material and supplies the cosmetic material to the outer component 2 appropriately by generating a difference in capillary force with the outer component 2. Therefore, it is adjusted according to the required volume of the recess and the capillary force of the outer component 2.
[0033] The front end portion of the surface of the outer component 2 is preferably formed with a bevel to facilitate the application of cosmetics. The angles, lines, and surfaces formed by the bevel allow the cosmetics to be applied along the subtle shape of the object being coated.
[0034] Furthermore, in addition to the aforementioned inclined surface, a polygonal or asymmetrical / symmetrical spherical surface can also be formed on the front end portion of the surface of the outer component 2. However, a shape that can be demolded using the mold described later is preferred.
[0035] Furthermore, the surface of the outer component 2 can have fine concave or fine convex decorative patterns. For example... Figure 2 As shown in (a), a fine, recessed decorative pattern, such as an identifier, can be added, engraved from the front end of the outer component 2 to the central portion. Figure 2 As shown in (b), a fine concave decorative pattern, such as the logo, can also be added to the bevel of the front end of the outer part 2.
[0036] If it is an engraving method, it is concave, but it can also be a fine convex decorative pattern. However, when applying a fine pattern to the bevel of the front end of the outer part 2, it is preferable to make it concave to avoid friction with the object being coated.
[0037] The outer component 2 is made of sintered porous plastic. That is, it is formed by sintering plastic particles. Specific examples include polyethylene, polyolefins such as polypropylene, polyamides such as nylon (registered trademark), polyphenylene sulfide, acrylic resin, etc. Among them, sintered polyethylene formed by sintering polyethylene particles is preferred.
[0038] When the outer component 2 is sintered polyethylene, the particle size of the polyethylene particles in the material is preferably in the range of 30μm to 330μm, more preferably 30μm to 200μm or 50μm to 200μm.
[0039] The molecular weight of the polyethylene particles is preferably in the range of 200,000 to 5,000,000, more preferably 1,000,000 to 4,500,000 or 1,500,000 to 1,900,000.
[0040] The porosity of the outer component 2 is preferably 30% to 70%, more preferably 30% to 60% or 30% to 50%.
[0041] The inner shaft component 3 is made of a porous body using synthetic fibers and / or synthetic resins.
[0042] Examples of synthetic fiber systems include those formed by bundling synthetic fibers and curing them with polyurethane resin or the like, and those formed by mixing low-melting-point synthetic fibers and bonding high-melting-point synthetic fibers together with low-melting-point synthetic fibers. Examples of synthetic resin systems include those formed by melt extrusion molding thermoplastic resin into the desired cross-sectional shape and size, and those formed by partially fusing thermoplastic resin granules together to form interconnected continuous pores between the granules and molding them by sintering.
[0043] Examples include synthetic fibers such as nylon, polyester, acrylic fibers or blends thereof; synthetic resins such as polyethylene terephthalate (PET), polybutylene terephthalate, polyoxymethylene, polyamides such as nylon, polyethylene, olefin resins such as polypropylene, acrylic resins, polyvinyl chloride, polystyrene, polyvinyl acetate, polyurethane, TEFLON (registered trademark), ABS resin, AS resin, polyphenylene sulfide, polysulfone, polyethersulfone, polyetheretherketone, polyimide, etc.
[0044] The porosity of the porous body in the inner shaft component 3 is greater than that in the outer component 2. Therefore, if the liquid such as cosmetic in the outer component 2 decreases due to coating or slight evaporation, the liquid such as cosmetic stored in the inner shaft component 3 will move to the outer component 2 through capillary force. The porosity of the inner shaft component 3 is preferably adjusted to a range of 65% to 95%, more preferably to a range of 75% to 95% or 80% to 95%.
[0045] The cosmetic applicator 1 can be installed in various cosmetic containers depending on the application, and can also be designed to be installed in screw-on containers. When installed in a lipstick screw-on container, the dimensions of the cosmetic applicator 1 depend on the shape of the container, but examples include an outer diameter of 12 mm and a length of 36 mm. Furthermore, the dimensions of the recess in the outer component 2 can include an inner diameter of 8 mm and a length of 28 mm. That is, in this example, the inner shaft component 3 has an outer diameter of 8 mm and a length of 28 mm.
[0046] Furthermore, the shape of the rear end portion of the cosmetic coating component 1 can be appropriately processed to allow it to be installed in a cosmetic container for its intended use. In this case, the rear end of the outer component 2 and the rear end of the inner shaft component 3 can be located at the same position in the axial direction, or the rear end of the outer component 2 can be located further back, or the rear end of the inner shaft component 3 can be located further back.
[0047] By constructing the outer component 2 and the inner shaft component 3 with the materials and dimensions described above, when the cosmetic coating component 1 is used for lipstick, it has basic properties such as providing a skin feel that is at least as good as conventional oil-based lipsticks, being able to adjust the amount of cosmetic coating to the same degree, maintaining the shape or embossed pattern 4 of the cosmetic coating component 1 before and after use, and being reusable.
[0048] The manufacturing method of the cosmetic coating component 1 of the present invention includes the following steps: preparing a mold K having the shape of the surface of the outer component 2 and the shape of the recess of the outer component 2; filling the mold K with particulate plastic material; heating the particulate plastic material to form it; taking out the outer component 2 formed in the forming step; and inserting the inner shaft component 3 into the recess of the outer component 2.
[0049] like Figure 3 of (a) Figure 3 As illustrated in (b), mold K is preferably a mold composed of a first mold K1 having a front end portion with the outer component 2 and a second mold K2 having a side portion and a recess other than the front end portion with the outer component 2. The method of combining the first mold K1 and the second mold K2, or their position (the dividing position), is not limited as long as the formed outer component 2 can be removed from mold K. Furthermore, as... Figure 3 As shown in (c), it is preferable to have a filling port so that particulate plastic material can be filled from the rear end portion of the mold K.
[0050] Particle-shaped plastic material is filled into the mold K through the opening by vibration, and then heated. The heating conditions are adjusted to form a sintered porous plastic. In the case of sintered porous plastic being sintered polyethylene, an example is a heating temperature of 180°C and a heating time of 30 minutes.
[0051] After cooling mold K, the outer part 2 is removed from mold K1 and mold K2.
[0052] Additionally, an inner shaft component 3 is formed. The inner shaft component 3 is a porous body made of synthetic fibers and / or synthetic resins. The porous body is obtained by adjusting the molding conditions using raw materials of synthetic fibers or synthetic resins.
[0053] The molded inner shaft component 3 is inserted into the molded outer component 2 to manufacture the cosmetic coating component 1.
[0054] In addition, a method for manufacturing a cosmetic coating component 1 by inserting the inner shaft component 3 into the outer component 2 is described, but other manufacturing methods that can produce a cosmetic coating component 1 with the above-mentioned features are not excluded.
[0055] The cosmetic coating tool 5 of the present invention includes the cosmetic coating component 1 described above. In addition to the cosmetic coating component 1, the cosmetic coating tool 5 may also include any container or a component for impregnating the cosmetic with the inner shaft component 3.
[0056] As an example of any container, one could cite a spin-out container 6 (see reference). Figure 4 of (a) Figure 4 (b)
[0057] The cosmetic material only needs to be able to impregnate the inner shaft component 3 and be supplied to the outer component 2. The cosmetic material may contain water, polyols, glycerin, emollients, setting agents, preservatives, dyes, pigments, fragrances, etc.
[0058] Furthermore, the cosmetic coating tool 5 of the present invention is manufactured using the aforementioned method for manufacturing the cosmetic coating component 1. Alternatively, other manufacturing methods may also be used to produce the cosmetic coating component 1 having the aforementioned characteristics.
[0059] Example
[0060] The embodiments of the present invention were evaluated by comparing them with conventional lipsticks and the like.
[0061] A mold K was prepared in the shape of a rod-shaped cosmetic coating component 1. The outer diameter of the mold K is 12 mm and the length is 36 mm. The mold K has a protrusion with a diameter of 8 mm and a length of 28 mm corresponding to the concave portion of the outer component 2, and a filling port for filling granular plastic material. In addition, the mold K is formed by combining a first mold K1 with the shape of the front end portion of the outer component 2 and a second mold K2 with the shape of the side portion and the concave portion of the outer component 2 excluding the front end portion. After filling the filling port with ultra-high molecular weight polyethylene (molecular weight 1.7 million) with a particle size of 115 μm, the mold was heated at 180°C for about 30 minutes, cooled, and the outer component 2 with a porosity of 40% was removed. The inner shaft component 3, a porous body made of 5 denier polyester fiber with a diameter of 8 mm, a length of 28 mm, and a porosity of 83%, was inserted into the concave portion of the outer component 2 to obtain the cosmetic coating component 1. The cosmetic coating component 1 was installed in the unscrewing container 6, and the cosmetic coating tool 5 was used as Example 1.
[0062] In contrast, a commercially available lipstick (manufactured by ERATO INC., Lipstick Tint) is used as Comparative Example 1.
[0063] Furthermore, a cosmetic coating component with the porosity of the outer component adjusted to 80% and the porosity of the inner shaft component adjusted to 83% was used as Comparative Example 2.
[0064] Furthermore, a mold with a shape that does not have an outer part and a cosmetic coating component with a porosity of 40% that does not have an inner shaft component was used as Comparative Example 3.
[0065] Regarding Example 1 and Comparative Examples 1-3, 10 people conducted evaluations. The applied material was evaluated as lips, with Comparative Example 1, which was a conventional lipstick, as the benchmark (○). 8 or more people considered it excellent, ◎ was selected; 5 or more people considered it excellent, ○ was selected; and less than 5 people considered it excellent, △ was selected.
[0066] Here, in "Shape Retention," the shape of the lipstick surface was maintained; in "Application Amount," the amount of cosmetic material was evaluated as too much or too little; in "Skin Feel," the skin feel of the applied material when used as lips was evaluated; in "Stability Over Time," the ability of the cosmetic material to be stably applied to the applied material over many days was evaluated; and in "Strength," the coating part of the cosmetic material application component was evaluated for any damage after repeated use.
[0067] The evaluation results are shown in Table 1.
[0068] [Table 1]
[0069] As shown in Table 1, based on Comparative Example 1, which is a conventional lipstick, it was found that Example 1 not only has a good skin feel and the amount of application is not excessive, but also excels in shape retention and strength. In particular, regarding shape retention, it was found that it can continue to be used while maintaining the shape of the front end portion of the outer part 2 or the fine embossed decorative pattern.
[0070] In contrast, according to the results of Comparative Example 2, if the porosity of the outer part is high, the skin feel is poor and the strength is reduced, resulting in excessive leakage of cosmetic material. Due to the excessive leakage of cosmetic material, the amount of coating decreases relatively quickly, thus resulting in poor stability over time.
[0071] Furthermore, according to the results of Comparative Example 3, when the cosmetic coating component was made only of the material of the outer component, cosmetic sedimentation occurred, and a significant reduction in coating amount was observed.
[0072] The present invention may have the structure shown below.
[0073] [Item 1]
[0074] A cosmetic coating component includes an outer component and an inner shaft component, wherein, The outer component is generally rod-shaped and has an axial recess extending from the rear end toward the front end. The inner shaft component is configured to abut against the inner side surface of the recess of the outer component. The outer component is made of sintered porous plastic with a porosity of 30% to 70%, and maintains its shape before and after use. The inner shaft component is made of a porous body of synthetic fibers and / or synthetic resin. The porosity of the inner shaft component is greater than that of the outer component.
[0075] [Item 2]
[0076] According to the cosmetic coating component described in item 1 above, the sintered porous plastic of the outer component is sintered polyethylene.
[0077] [Item 3]
[0078] According to item 1 or 2 above, the cosmetic coating component has an inclined surface formed relative to the axial direction at the front end portion of the surface of the outer component.
[0079] [Item 4]
[0080] The cosmetic coating component according to any one of items 1 to 3 above, wherein the surface of the outer component has a fine concave or fine convex decorative pattern.
[0081] [Item 5]
[0082] A method for manufacturing a cosmetic coating component, which is the method for manufacturing a cosmetic coating component as described in item 1 above, comprising the following steps: Prepare a mold having the shape of the surface of the outer component and the shape of the recess of the outer component; The mold is filled with granular plastic material; The outer component is formed by heating the granular plastic material. Remove the outer component formed in the molding step; and Insert the inner shaft component into the recess of the outer component.
[0083] [Item 6]
[0084] According to the method for manufacturing a cosmetic coating component as described in item 5 above, the mold is formed by combining a first mold having the shape of a front end portion of the outer component and a second mold having the shape of a side portion other than the front end portion of the outer component and the shape of the recess.
[0085] [Item 7]
[0086] A cosmetic coating tool that uses the cosmetic coating component described in any one of items 1 to 4 above.
[0087] [Item 8]
[0088] A cosmetic coating tool, which is manufactured by the method for manufacturing cosmetic coating components described in item 5 or 6 above.
[0089] Symbol Explanation
[0090] 1-Cosmetic coating component, 2-Outer component, 3-Inner shaft component, 4-Embossing pattern, 5-Cosmetic coating tool, 6-Screwing container, K-Mold, K1-First mold, K2-Second mold.
Claims
1. A cosmetic coating component, comprising an outer component and an inner shaft component, characterized in that, The outer component is generally rod-shaped and has an axial recess extending from the rear end toward the front end. The inner shaft component is configured to abut against the inner side surface of the recess of the outer component. The outer component is made of sintered porous plastic with a porosity of 30% to 70%, and maintains its shape before and after use. The inner shaft component is made of a porous body of synthetic fibers and / or synthetic resin. The porosity of the inner shaft component is greater than that of the outer component.
2. The cosmetic coating component according to claim 1, characterized in that, The sintered porous plastic of the outer component is sintered polyethylene.
3. The cosmetic coating component according to claim 1 or 2, characterized in that, The front end portion of the surface of the outer component has an inclined surface formed relative to the axial direction.
4. The cosmetic coating component according to claim 3, characterized in that, The surface of the outer component has fine concave or fine convex decorative patterns.
5. A method for manufacturing a cosmetic coating component, which is the method for manufacturing a cosmetic coating component as described in claim 1, characterized in that, Includes the following steps: Prepare a mold having the shape of the surface of the outer component and the shape of the recess of the outer component; The mold is filled with granular plastic material; The outer component is formed by heating the granular plastic material. Remove the outer component formed in the molding step; and Insert the inner shaft component into the recess of the outer component.
6. The method for manufacturing the cosmetic coating component according to claim 5, characterized in that, The mold is formed by combining a first mold having the shape of the front end portion of the outer component and a second mold having the shape of the side portion other than the front end portion of the outer component and the shape of the recess.
7. A cosmetic application tool, characterized in that, The cosmetic coating component according to claim 1 was used.
8. A cosmetic application tool, characterized in that, Manufactured using the manufacturing method of the cosmetic coating component as described in claim 5.
Citation Information
Patent Citations
Stick-like cosmetic and its manufacturing method
JP2008278976A
Manufacturing device and manufacturing method of rod-like cosmetic
JP2014045985A