Layered modeling system
By detecting the temperature or shape of the weld bead and calculating the EN ratio and welding current, the problem of weld bead height deviation in consumable electrode arc welding was solved, achieving stable layering and constant deposition amount, thus improving welding stability.
Patent Information
- Application Number
- CN202580028373.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-04-18
- Filing Date
- 2025-04-11
- Publication Date
- 2026-11-10
AI Technical Summary
In consumable electrode arc welding, it is difficult to control the wire feed speed and welding current separately, which causes the height of the weld bead to deviate from the planned height and makes it impossible to stably stack the weld bead.
A layered molding system is adopted, which uses a detection device to detect the temperature or shape of the weld bead in real time, and uses a control device to calculate the appropriate EN ratio and welding current, and adjusts the welding wire melting speed and heat input to stabilize the layering of the weld bead.
It achieves stable stacking of weld beads while consuming electrode welding wire, prevents burn-through, ensures constant deposition amount and heat input, and improves welding stability.
Smart Images

Figure CN123076459A_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to a layered modeling system. Background Technology
[0002] Japanese Patent Application Publication No. 2022-106172 (Patent Document 1) discloses a technique for shaping an object by layering weld beads. Japanese Patent Application Publication No. 2022-106172 (Patent Document 1) also discloses a method for changing welding conditions when the height of the weld beads deviates from the planned height.
[0003] Existing technical documents
[0004] Patent documents
[0005] Patent Document 1: Japanese Patent Application Publication No. 2022-106172 Summary of the Invention
[0006] The problem that the invention aims to solve
[0007] In Japanese Patent Application Publication No. 2022-106172 (Patent Document 1), a consumable electrode is used in the deposition of weld beads, and the welding speed is changed according to the height of the deposit. In addition to the welding speed, the feed rate of the filler material and the amount of heat input used to generate the arc can also be controlled. However, in non-consumable electrode arc welding, the feed rate of the filler wire and the value of the welding current as heat input can be controlled independently, but in the case of consumable electrode arc welding, it is difficult to control them independently.
[0008] In consumable electrode systems, the wire feed rate and the wire melting rate are the same, thus stabilizing the welding process. Furthermore, the wire feed rate and the wire melting rate have a one-to-one relationship with the welding current and cannot be set independently. That is, Japanese Patent Application Publication No. 2022-106172 (Patent Document 1) does not consider the use of consumable electrodes; therefore, if the height of the weld bead deviates from the planned height, it is impossible to change to optimal welding conditions, and thus it cannot be considered sufficient for stably stacked weld beads.
[0009] The purpose of this disclosure is to provide a technique for stably stacking weld beads when using consumable electrode welding wire.
[0010] Methods for solving problems
[0011] This disclosure relates to a stacking molding system for molding an object by supplying welding current to a consumable electrode welding wire and stacking weld beads. The stacking molding system includes: a welding torch that performs the stacking of weld beads using a consumable electrode welding wire; a drive device that moves the welding torch; a detection device that detects the temperature or shape of the weld bead preceding the one being stacked during the stacking process; a welding power source that supplies alternating current (AC) to the consumable electrode welding wire as welding current; and a control device that controls the EN ratio of the AC. The control device calculates an EN ratio suitable for stacking weld beads based on at least one of the temperature and shape of the weld beads detected by the detection device.
[0012] Invention Effects
[0013] The stacking system of this disclosure calculates an EN ratio suitable for stacking weld beads based on at least one of the temperature and shape of the weld bead detected by the detection device. The amount of weld bead deposited can be easily changed independently of the current by changing the EN ratio. Therefore, the stacking system of this disclosure can stably stack weld beads when using consumable electrode welding wire. Attached Figure Description
[0014] Figure 1 This is a diagram that schematically illustrates the layered modeling system of Implementation Method 1.
[0015] Figure 2 This is a graph used to illustrate the EN ratio.
[0016] Figure 3 This is a graph used to illustrate an example of the relationship between welding current and wire melting speed for each EN ratio.
[0017] Figure 4 It is a graph used to illustrate the relationship between the temperature of the weld bead and the set EN ratio.
[0018] Figure 5 This is a flowchart illustrating the control content of Implementation Method 1.
[0019] Figure 6 This is a diagram that schematically illustrates the layered modeling system of Embodiment 2.
[0020] Figure 7 This is a graph used to illustrate an example of the relationship between welding current and wire melting speed for each EN ratio.
[0021] Figure 8 This is a graph used to illustrate the relationship between the height of the weld bead and the set EN ratio.
[0022] Figure 9 This is a flowchart illustrating the control content of Implementation Method 2.
[0023] Figure 10This is a flowchart representing the control content of a variant example. Detailed Implementation
[0024] Hereinafter, embodiments of the present disclosure will be described in detail with reference to the accompanying drawings. It should be noted that the same or equivalent parts in the drawings are labeled with the same reference numerals, and their descriptions will not be repeated.
[0025] [Implementation Method 1]
[0026] Figure 1 This is a schematic diagram illustrating the stacked modeling system 1 of Embodiment 1. The stacked modeling system 1 includes a robotic arm 40, a welding torch 20, a welding power source 10, a welding wire feed device 50, a temperature sensor 61, and a control device 30.
[0027] The robotic arm 40 is a multi-jointed arm, such as a six-axis multi-joint arm. The robotic arm 40 functions as a drive device to move the welding torch 20 at a set welding speed. By moving the welding torch 20 with the robotic arm 40, weld beads 70 containing molten consumable electrode wire 51 are stacked. The robotic arm 40 operates in a manner that shapes an object by stacking weld beads 70. It should be noted that the layer preceding the currently stacked layer of weld beads 70 is called the preceding layer.
[0028] In the welding torch 20, a welding current is supplied to the consumable electrode wire 51 through a power supply nozzle (not shown) located inside the nozzle 21. The consumable electrode wire 51 melts due to the electric arc 22 generated between it and the base material 80 or the already stacked weld beads 70, as well as the resistance heating caused by the current supply. The melting of the consumable electrode wire 51 forms the weld beads 70. The welding torch 20 performs the stacking of weld beads 70 using the consumable electrode wire 51. A shielding gas is supplied to the welding torch 20 through a shielding gas supply section (not shown), which exits from the nozzle 21 and reaches the electric arc 22 and the melting section. The shielding gas may be, for example, argon, CO2, or a mixture thereof.
[0029] The welding power source 10 supplies alternating current (AC) as the welding current to the consumable electrode welding wire 51. The magnitude of the welding current output from the welding power source 10 and the EN ratio are set by the control device 30. Here, the EN ratio refers to the proportion of the time of the welding wire's negative polarity period in one AC cycle to the total time. Alternatively, the EN ratio can also be set as the ratio of the value obtained by integrating the negative polarity current in one AC cycle to the value obtained by integrating the current in one AC cycle (the sum of the values obtained by integrating the positive polarity current and the negative polarity current).
[0030] Figure 2This is a diagram used to illustrate the EN ratio. The welding power source 10 switches the polarity of the electrode supplied to the consumable electrode wire 51 in the welding torch 20, specifying both positive and negative polarities. Positive electrode polarity refers to the polarity state where the consumable electrode wire 51 side in the current path supplied from the welding power source 10 is the anode and the base material 80 or weld bead 70 side is the cathode. Negative electrode polarity refers to the polarity state where the base material 80 or weld bead 70 side in the current path supplied from the welding power source 10 is the anode and the consumable electrode wire 51 side is the cathode.
[0031] For example, in Figure 2 In the case of the pulse waveform shown, the ratio of the positive electrode polarity to the total polarity of the negative electrode polarity is called the EP ratio, and the ratio of the negative electrode polarity is called the EN ratio. For example... Figure 2 As shown, the welding power source 10, for example, can output positive electrode polarity (S) during one cycle of an AC pulse. EP ) and electrode negative polarity (S EN Alternating welding current. It should be noted that this is not a pulse waveform; the EN ratio can also be set in the waveform of short-circuit welding accompanied by short-circuit transition.
[0032] It is known that the melting rate of the consuming electrode wire 51 increases during the period of negative electrode polarity. This is because the heat input from the arc 22 to the consuming electrode wire 51 increases during the period of negative electrode polarity, and the heat input from the arc 22 to the base material 80 or the weld bead 70 increases during the period of positive electrode polarity. Therefore, the wire melting rate can be adjusted by the EN ratio.
[0033] The heat input from arc 22 to the molten section is also increased. Figure 2 The amplitude of the welding current increases. However, in the arc 22, if the heat input to the molten part is excessively increased by increasing the welding current, the state of the weld bead 70 becomes unstable, which can lead to burn-through. Therefore, the control device 30 sets the state of the weld bead 70 to a suitable stacking state by controlling the magnitude of the welding current output by the welding power source 10 and the EN ratio.
[0034] return Figure 1 The wire feeding device 50 includes a roller (not shown) and a motor. The wire feeding device 50 feeds the consumable electrode wire 51 to the welding torch 20 by driving the motor and rotating the roller.
[0035] Temperature sensor 61 functions as a detection device, relative to the temperature of the deposited weld beads 70 during the stacking process. Figure 1The temperature sensor 61 detects the temperature of the weld bead 70 at position T, which is the position preceding the currently stacked layer, according to the welding direction indicated by the arrow. The temperature sensor 61 is preferably a non-contact sensor such as a thermal imager. Position T corresponds to the layer preceding the currently stacked layer (the previous layer). The temperature information of the weld bead 70 detected by the temperature sensor 61 is sent to the control device 30. Alternatively, the temperature sensor 61 may be a point-based pyrometer, rather than a thermal imager that captures images of an area.
[0036] Here, the structure formed by stacking weld beads 70 is in the following relationship: the lower the layer, the closer it is to the base material 80, so heat dissipates easily; the higher the layer, the further it is from the base material 80, so heat dissipates more difficultly. Under such circumstances, if welding current is supplied to the consuming electrode wire 51 under the same welding conditions, the heat in the upper weld beads 70 becomes too high, and the weld beads 70 may burn through. The stacking structure system 1 of Embodiment 1 changes the welding conditions based on the temperature information of the weld beads 70 detected by the temperature sensor 61.
[0037] The control device 30 includes a computing unit 31, a memory 32, a storage device 33, and an input / output interface 34. These components are connected via a bus.
[0038] The arithmetic unit 31 is a computing entity (computer) that performs the prescribed processing. The arithmetic unit 31 may be composed of processors such as CPU (Central Processing Unit), MPU (Micro-Processing Unit), TPU (Tensor Processing Unit), or GPU (Graphics Processing Unit). The arithmetic unit 31 may also be read as a processing circuitry that performs the prescribed processing.
[0039] The memory 32 includes a storage area (e.g., a working area) for storing program code or working memory when the computing device 31 executes various programs.
[0040] The storage device 33 functions as a storage unit for storing various programs or data executed by the arithmetic unit 31. For example, the storage device 33 stores the control program 330 executed by the arithmetic unit 31.
[0041] The input / output interface 34 receives values obtained from the temperature sensor 61, etc. The control device 30 sets the welding current output by the welding power source 10 based on the temperature information obtained from the temperature sensor 61. Specifically, the control device 30 calculates the EN ratio based on the temperature of the weld bead 70 detected by the temperature sensor 61, and calculates the welding current set for the welding power source 10 based on the calculated EN ratio.
[0042] Next, the relationship between welding current and welding wire melting speed will be explained. Figure 3 This is a graph illustrating an example of the relationship between welding current and wire melting rate for each EN ratio. Figure 3 In the diagram, the horizontal axis represents the welding current, and the vertical axis represents the wire melting rate. The wire melting rate refers to the speed at which the consumed electrode wire 51 melts and transforms into the weld bead 70. For example... Figure 3 As shown, it has the characteristic that the melting speed of the welding wire increases with the increase of welding current.
[0043] To stably stack the weld beads 70, it is important to maintain a constant weld bead formation rate, thereby ensuring a constant amount of weld beads 70. Furthermore, to stably stack the weld beads 70, it is important to maintain a constant temperature of the weld beads 70 (molten portion). Thus, for stable stacking of weld beads 70, welding conditions requiring a constant weld bead melting rate and a constant actual heat input (obtained by subtracting the heat exiting the molten portion from the heat input to the molten portion) are required. It should be noted that the weld bead melting rate cannot be directly controlled; therefore, the control device 30 indirectly adjusts the weld bead melting rate by sending a command to the weld bead feed device 50 to adjust the weld bead feed rate.
[0044] For example, it is assumed that when the temperature of the preceding layer is high, the heat transferred from the weld bead 70 (molten portion) to the preceding layer becomes smaller. Therefore, it is considered to reduce the heat input based on energization to keep the actual heat input to the molten portion constant. However, in the case of electrode consumption, such as Figure 3 As shown, there is a positive correlation between welding current and wire melting speed. Therefore, if only DC (EN ratio 0%) is considered, the wire melting speed will decrease as the current is reduced, making it impossible to keep the wire melting speed constant. Therefore, this study investigated reducing the current by adjusting the EN ratio of AC, thus keeping the actual heat input to the molten section constant while maintaining a constant wire melting speed.
[0045] Figure 3 This is an example illustrating the relationship between the welding current for each EN ratio and the melting rate of the consumed electrode wire 51. For example... Figure 3 As shown, the relationship between welding current and wire melting speed is as follows: When the wire melting speed of the consuming electrode wire 51 is set to constant at V0, the welding current decreases from I1 to I3 as the EN ratio increases. That is, it can be seen that the arc heat input can be changed by adjusting the EN ratio and changing the magnitude of the welding current, thus keeping the actual heat input constant while keeping the deposition amount constant by setting the wire melting speed to constant at V0.
[0046] Next, the EN ratio set according to the temperature of the weld bead 70 will be explained. Figure 4 This is a graph used to illustrate the relationship between the temperature of the weld bead 70 and the set EN ratio. Figure 4 In the diagram, the horizontal axis represents the temperature of the weld bead at 70°C, and the vertical axis represents the set EN ratio. For example... Figure 4 As shown, the EN ratio is set to increase as the temperature of the weld bead 70 increases.
[0047] exist Figure 4 In this process, because the deposition amount is kept constant, therefore, as Figure 3 In accordance with the corresponding relationship, an EN ratio is set to adjust the heat input by changing the welding current while maintaining a constant welding wire melting speed. Specifically, when the temperature of the preceding weld bead 70 is high, a higher EN ratio is set to reduce the heat input from the arc 22 to the weld bead 70, thereby decreasing the welding current. Conversely, when the temperature of the preceding weld bead 70 is low, a lower EN ratio is set to increase the heat input from the arc 22 to the weld bead 70, thereby increasing the welding current. Figure 4 The corresponding relationship is used to calculate the appropriate EN ratio based on the temperature of the weld bead at 70°C.
[0048] like Figure 4 As shown, based on the temperature of the previous layer's weld bead 70, an EN ratio suitable for the stacked weld bead 70 is set. Then, as... Figure 3 As shown, by changing the EN ratio according to the temperature of the previous weld bead 70 while keeping the welding wire melting speed constant, the welding current can be adjusted to keep the heat input of the molten portion constant. This allows for the stable stacking of weld beads 70.
[0049] Figure 3 , Figure 4 Such a relationship is stored in storage device 33 in advance based on experiments, etc. Figure 3 , Figure 4 The correspondence shown is an example. Information related to multiple correspondences can be stored in the storage device 33 according to the type of consuming electrode wire 51 of the stacked object. It should be noted that... Figure 3 , Figure 4 The correspondence shown can also be derived from calculation formulas, etc., without relying on experiments.
[0050] Next, the processing performed by the control device 30 in Embodiment 1 will be described in detail. Figure 5 This is a flowchart illustrating the control content of Implementation Method 1. Figure 5The flowchart processing is repeatedly invoked and executed as a subroutine from the main routine in the control unit 30. First, in step S (hereinafter simply referred to as "S") 11, the control unit 30 determines whether temperature information of the weld bead 70 sent from the temperature sensor 61 has been obtained. The temperature information can be sent, for example, at constant intervals. If the control unit 30 determines that no temperature information has been obtained (S11 "No"), the processing returns from the subroutine to the main routine.
[0051] When the control device 30 determines that temperature information has been obtained (S11 "Yes"), it uses the data stored in the storage device 33 to... Figure 4 The corresponding relationship is shown, and the EN ratio (S12) corresponding to the temperature information of the weld bead 70 detected by the temperature sensor 61 is calculated. Next, the control device 30, based on the data stored in the storage device 33... Figure 3 The corresponding relationship is shown, and the welding current corresponding to the EN ratio calculated in S12 when the melting rate of the consuming electrode welding wire 51 is set to constant is calculated (S13). Through the processing in S13, the control device 30 can calculate the optimal welding current by changing the EN ratio while keeping the melting rate constant (keeping the welding wire feed rate constant) based on the temperature information of the weld bead 70. Then, the control device 30 sends the information related to the welding current and the EN ratio to the welding power source 10 (S14), causing the processing to return from the subroutine to the main routine. It should be noted that the calculation of the EN ratio and the welding current can also be performed directly in the welding power source 10. In this way, part or all of the control device 30 can be assembled into the control device of the welding power source 10 or the robotic arm 40.
[0052] In the stacking molding system 1 of Embodiment 1, the control device 30 calculates an EN ratio suitable for stacking the weld beads 70 based on the temperature of the weld beads 70 detected by the temperature sensor 61. Then, the control device 30 calculates the welding current set for the welding power source 10 based on the calculated EN ratio. By calculating the welding current set for the welding power source 10 based on the EN ratio in this way, the weld beads 70 can be stably stacked when using the consumable electrode wire 51. It should be noted that the welding power source 10 outputs a corresponding current waveform based on the EN ratio and the welding current.
[0053] The control device 30, based on the data stored in the storage device 33, Figure 4 The control device 30 calculates the EN ratio corresponding to the temperature of the weld bead 70 detected by the temperature sensor 61, based on the corresponding relationship. Figure 3The corresponding relationship is used to calculate the magnitude of the welding current corresponding to the EN ratio when the melting rate of the consumable electrode wire 51 is set constant (the wire feed rate is set constant). Therefore, based on the EN ratio optimal for the temperature of the weld bead 70, by setting the melting rate of the consumable electrode wire 51 constant and varying the magnitude of the welding current, a stacking process can be performed that maintains a constant deposition amount in the weld bead 70. By setting this welding current, the stacking system 1 can prevent burn-through of the weld bead 70 and stabilize the stack.
[0054] [Implementation Method 2]
[0055] Next, the layered modeling system 1A of Embodiment 2 will be described. Figure 6 This is a schematic diagram illustrating the stacked modeling system 1A of Embodiment 2. The stacked modeling system 1A of Embodiment 2 differs from the stacked modeling system 1 of Embodiment 1 in that it has a shape sensor 62 instead of a temperature sensor 61.
[0056] The shape sensor 62 functions as a detection device, which, when stacking the weld beads 70, relative to... Figure 7 The shape sensor 62 detects the shape of the weld bead 70 at position T, which is the position preceding the currently stacked layer, according to the welding direction indicated by the arrow. The shape sensor 62 is preferably a non-contact sensor such as a laser scanner. Position T corresponds to the layer preceding the currently stacked layer (the previous layer). The shape sensor 62 sends the height information of the weld bead 70 as shape information to the control device 30.
[0057] Next, the relationship between welding current and wire melting speed for each EN ratio will be explained. Figure 7 This is a graph illustrating an example of the relationship between welding current and wire melting rate for each EN ratio. Figure 7 In the diagram, the horizontal axis represents the welding current, and the vertical axis represents the melting speed of the welding wire. For example... Figure 7 As shown, it has the characteristic that the melting speed of the welding wire increases with the increase of welding current.
[0058] To stably stack the weld beads 70, it is important to maintain a constant heat input to the molten portion by setting the welding current constant. Furthermore, to stably stack the weld beads 70, it is important to vary the wire melting speed of the weld beads 70 according to the shape of the preceding weld beads 70, thereby maintaining a constant amount of weld beads 70 formed. Thus, in the stable stacking of weld beads 70, as welding conditions, it is required to maintain a constant heat input to the molten portion and a constant amount of weld beads 70 formed by varying the wire melting speed.
[0059] For example, when the height of the front layer is low, consider increasing the welding wire melting rate while keeping the heat input to the molten section constant. However, in the case of electrode consumption, such as... Figure 7 As shown, there is a positive correlation between welding current and wire melting speed. Therefore, if only DC (EN ratio 0%) is considered, increasing the wire melting speed will also increase the welding current, which cannot keep the heat input to the molten part constant. Therefore, this study investigated how to change the wire melting speed while keeping the heat input to the molten part constant by adjusting the EN ratio of AC.
[0060] exist Figure 7 The relationship between welding current and the melting rate of the consuming electrode wire 51 is specified according to each EN ratio. For example... Figure 7 As shown, the relationship between welding current and wire melting speed is as follows: When the welding current is set to a constant I0, as the EN ratio increases, the wire melting speed of the electrode welding wire 51 increases from V1 to V3. That is, it can be seen that in order to stably deposit the weld bead 70, it is only necessary to change the EN ratio and the wire melting speed while keeping the heat input constant by setting the welding current to a constant I0.
[0061] Next, the relationship between the height of the weld bead 70 and the EN ratio will be explained. Figure 8 This is a diagram illustrating the relationship between the height of the weld bead 70 and the set EN ratio. Figure 8 In the diagram, the horizontal axis represents the height of the weld bead at 70°, and the vertical axis represents the set EN ratio. For example... Figure 8 As shown, the EN ratio is set to decrease as the height of the weld bead 70 increases.
[0062] exist Figure 8 In this case, because the heat input is kept constant, therefore, as Figure 7 In accordance with the corresponding relationship, an EN ratio is set to adjust the deposition amount by changing the wire melting speed while keeping the welding current constant. Specifically, when the height of the preceding weld bead 70 is high, a lower EN ratio is set to reduce the deposition amount, thus slowing down the wire melting speed. Conversely, when the height of the preceding weld bead 70 is low, a higher EN ratio is set to increase the deposition amount, thus speeding up the wire melting speed. Figure 8 The corresponding relationship is used to calculate the appropriate EN ratio based on the height of the weld bead 70.
[0063] like Figure 8 As shown, the EN ratio suitable for the stacked weld beads 70 is set according to the height of the previous weld bead 70. Furthermore, as... Figure 7As shown, by changing the EN ratio according to the height of the previous weld bead 70 while keeping the welding current constant, it is possible to keep the heat input to the molten portion constant and adjust the wire melting speed while keeping the welding current constant. This allows for the stable stacking of weld beads 70.
[0064] Figure 7 , Figure 8 Such a relationship is stored in storage device 33 in advance based on experiments, etc. Figure 7 , Figure 8 The correspondence shown is an example. Information related to multiple correspondences can be stored in the storage device 33 according to the type of the consuming electrode wire 51 of the stacked object.
[0065] Next, the processing performed by the control device 30 in Embodiment 2 will be described in detail. Figure 9 This is a flowchart illustrating the control content of Implementation Method 2. Figure 9 The flowchart processing is repeatedly invoked and executed as a subroutine from the main routine in the control unit 30. First, in step S21, the control unit 30 determines whether it has obtained height information of the weld bead 70, which is shape information sent from the shape sensor 62. The height information can be sent, for example, at constant intervals. If the control unit 30 determines that shape information has not been obtained (S21 "No"), the processing returns from the subroutine to the main routine.
[0066] When the control device 30 determines that altitude information has been obtained (S21 "Yes"), it uses the information stored in the storage device 33... Figure 8 The corresponding relationship is shown, and the EN ratio corresponding to the height information of the weld bead 70 detected by the shape sensor 62 is calculated (S22). Next, the control device 30 calculates the EN ratio based on the height information of the weld bead 70 detected by the shape sensor 62. Figure 7 The corresponding relationship is shown, and the melting rate of the consumed electrode wire 51 is calculated (S23) according to the EN ratio obtained in S22 when the welding current is set to constant. Through the processing of S23, the control device 30 can calculate the optimal wire melting rate by changing the EN ratio while keeping the welding current constant, based on the height information of the weld bead 70.
[0067] Next, the control device 30 sends information related to the magnitude of the welding current and the EN ratio to the welding power source 10 (S24). Then, the control device 30 sends information related to the melting speed of the consuming electrode wire 51 to the wire feed device 50 (S25), causing the process to return from the subroutine to the main routine. The wire feed device 50 is adjusted to a wire feed speed that matches the wire melting speed.
[0068] In the stacked molding system 1A of Embodiment 2, the control device 30 calculates an EN ratio suitable for stacking the weld beads 70 based on the height of the weld beads 70 detected by the shape sensor 62. Then, the control device 30 adjusts the welding wire melting speed by setting the welding wire feed speed set to the welding wire feed device 50 according to the calculated EN ratio. Thus, by keeping the welding current constant and changing the welding wire melting speed based on the EN ratio optimal for the height of the weld beads 70, the heat input can be kept constant and the amount of weld deposited can be adjusted.
[0069] The control device 30, based on the data stored in the storage device 33, Figure 8 The control device 30 calculates the EN ratio corresponding to the height of the weld bead 70 detected by the shape sensor 62 based on the corresponding relationship. Figure 7 Based on the corresponding relationship, the melting rate of the consumable electrode wire 51 is calculated to correspond to the EN ratio when the welding current is set to constant. Therefore, based on the EN ratio optimal for the height of the weld bead 70, by setting the welding current to constant and varying the wire melting rate, a stacking process can be performed that maintains constant heat input and adjusts the deposition amount of the weld bead 70. The stacking system 1A can prevent burn-through of the weld bead 70 and stabilize the stack by setting the welding current and the feed rate of the consumable electrode wire 51 set for the wire feed device 50.
[0070] [Variation Example]
[0071] Next, the processing performed by the control device 30 in the modified example will be explained in detail. Figure 10 This is a flowchart representing the control content of a variant example. Figure 10 The flowchart processing is repeatedly invoked and executed as a subroutine from the main routine in the control unit 30. First, in step S31, the control unit 30 determines whether it has obtained molten pool size information, which is the shape information of the weld bead 70 sent from the shape sensor 62. The molten pool size information is related to the size of the molten metal accumulation when the consuming electrode wire 51 melts. The storage device 33 stores the correspondence between the molten pool size and the approximate temperature information of the weld bead 70. This correspondence is determined in advance through experiments and stored in the storage device 33.
[0072] If the control device 30 determines that the molten pool size information has not been obtained (S31 "No"), the processing returns from the subroutine to the main routine. If the control device 30 determines that the molten pool size information has been obtained (S31 "Yes"), the control device 30 calculates the temperature information of the weld bead 70 corresponding to the molten pool size information stored in the storage device 33 (S32). Next, the control device 30 calculates the EN ratio corresponding to the temperature information of the weld bead 70 (S33). Next, the control device 30 calculates the welding current corresponding to the EN ratio calculated in S33 when the melting speed of the consuming electrode wire 51 is set to constant (the wire feed speed is set to constant) (S34). Next, the control device 30 sends information related to the magnitude of the welding current and the EN ratio to the welding power source 10 (S35), and the processing returns from the subroutine to the main routine.
[0073] As shown in the variation example, the temperature information of the weld bead 70 is indirectly obtained based on the size of the molten pool, thus enabling stable stacking of the weld bead 70 even when temperature measurement is difficult. It should be noted that, alternatively, the temperature information can be used instead of converting it into temperature information, and a direct correspondence can be established between the size of the molten pool and the EN ratio, which is optimal for the size of the molten pool, for control.
[0074] The layered modeling system 1 can also include both a temperature sensor 61 and a shape sensor 62. In this case, the EN ratio corresponding to the temperature information and shape information can be calculated.
[0075] In the above embodiments, the temperature or shape information of the weld bead 70 can also be obtained layer by layer in the stacking of the model.
[0076] In the above embodiments, a drive device for moving the detection device independently can also be provided. This drive device is preferably controlled to move the detection device to an appropriate position according to the movement of the welding torch 20.
[0077] In the above embodiments, the welding torch 20 may also be moved by an orthogonal robot instead of a multi-jointed robotic arm 40.
[0078] Summary
[0079] (1) This disclosure relates to a stacking molding system 1 for molding an object by supplying welding current to a consumable electrode welding wire 51 and stacking weld beads 70. The stacking molding system 1 includes: a welding torch 20 for stacking weld beads 70 using the consumable electrode welding wire 51; a drive device (robotic arm 40) for moving the welding torch 20; a detection device (temperature sensor 61) for detecting the temperature or shape of the weld beads 70 preceding the stacked weld beads 70 during stacking; a welding power source 10 for supplying alternating current as welding current to the consumable electrode welding wire 51; and a control device 30 for controlling the EN ratio of the alternating current. The control device 30 calculates an EN ratio suitable for stacking the weld beads 70 based on at least one of the temperature and shape of the weld beads 70 detected by the detection device (temperature sensor 61).
[0080] According to the stacking system 1 of this disclosure, the control device 30 calculates an EN ratio suitable for stacking the weld beads 70 based on at least one of the temperature and shape of the weld beads 70 detected by the detection device (temperature sensor 61). The amount of weld deposited in the weld beads 70 can be easily changed independently of the current by changing the EN ratio. Thus, the stacking system 1 of this disclosure can stably stack weld beads 70 when using consumable electrode wire 51.
[0081] (2) Based on the stacked modeling system 1 of (1), it also includes a storage unit (storage device 33), which stores a first correspondence between the temperature of the weld bead 70 and the EN ratio, and a second correspondence between the welding current and the melting rate of the consuming electrode wire 51 according to each EN ratio. The control device 30 calculates the first EN ratio corresponding to the temperature of the weld bead 70 detected by the detection device (temperature sensor 61) according to the first correspondence, and calculates the welding current corresponding to the first EN ratio when the melting rate of the consuming electrode wire 51 is set to constant according to the second correspondence.
[0082] According to the stacking system 1 disclosed herein, stacking can be performed with the melting rate of the consuming electrode wire 51 set to a constant, based on the EN ratio of the temperature most suitable for the weld bead 70.
[0083] (3) Based on the layered modeling system 1 of (1) or (2), the first correspondence is that the EN ratio increases as the temperature of the weld bead 70 increases.
[0084] According to the layered modeling system 1 disclosed herein, the most suitable EN ratio corresponding to the first correspondence can be calculated.
[0085] (4) Based on the stacked modeling system 1 in any one of (1) to (3), the second correspondence is that when the melting speed of the consuming electrode welding wire 51 is set to constant, the welding current decreases as the EN ratio increases.
[0086] According to the layered molding system 1 of this disclosure, an appropriate welding current can be calculated based on the EN ratio to set the melting rate of the consuming electrode welding wire 51 to a constant.
[0087] (5) Based on the stacking modeling system 1A of (1), the detection device (shape sensor 62) can detect the shape of the weld bead 70 in front of the stack as height information when stacking the weld beads 70. It also includes a storage unit (storage device 33), which stores a third correspondence between the specified height information and the EN ratio and a second correspondence between the welding current and the melting rate of the consuming electrode wire 51 according to each EN ratio. The control device 30 calculates the EN ratio corresponding to the height information detected by the detection device (shape sensor 62) according to the third correspondence, and calculates the melting rate of the consuming electrode wire 51 corresponding to the EN ratio when the welding current is set to constant according to the second correspondence.
[0088] According to the stacking system 1A of this disclosure, stacking can be performed with the welding current set to constant based on the EN ratio, which is optimal for the height of the weld bead 70. The stacking system 1A can stack the weld bead 70 with a constant welding current, thus preventing burn-through and stabilizing the stack.
[0089] (6) In the layered modeling system 1A of (5), the third correspondence is that the EN ratio decreases as the height of the weld bead 70 increases.
[0090] According to the layered modeling system 1A of this disclosure, the most appropriate EN ratio corresponding to the third correspondence can be calculated.
[0091] (7) In the stacked modeling system 1A of (5) or (6), the second correspondence is that when the welding current is set to constant, the melting rate of the electrode welding wire 51 increases as the EN ratio increases.
[0092] According to the layered molding system 1A of this disclosure, the appropriate melting rate of the consuming electrode wire 51 when the welding current is set to constant can be calculated based on the EN ratio.
[0093] The embodiments disclosed herein should be considered illustrative in all respects and not restrictive. The scope of this disclosure is not defined by the description of the embodiments above, but by the technical solutions, and is intended to include all equivalents and modifications within the scope of the technical solutions.
[0094] Explanation of reference numerals in the attached figures
[0095] 1.1A Layered Modeling System, 10 Welding Power Source, 20 Welding Torch, 21 Nozzle, 22 Arc, 30 Control Device, 31 Computing Device, 32 Memory, 33 Storage Device, 34 Input / Output Interface, 40 Robotic Arm, 50 Welding Wire Feeding Device, 51 Consumable Electrode Welding Wire, 61 Temperature Sensor, 62 Shape Sensor, 70 Weld Bead, 80 Base Material, 330 Control Program.
Claims
1. A layered molding system that supplies welding current to a consumable electrode welding wire to layer weld beads to shape an object, wherein, The layered modeling system has the following features: A welding torch that performs a stacking of weld beads using the consumable electrode wire; A drive device that moves the welding torch; A detection device that detects the temperature or shape of the weld bead preceding the layer during the stacking of the weld beads. A welding power source that supplies alternating current as the welding current to the consumable electrode wire; and Control device, which controls the EN ratio of the AC, The control device calculates the EN ratio suitable for stacking the weld beads based on at least one of the temperature and shape of the weld beads detected by the detection device.
2. The layered modeling system according to claim 1, wherein, The layered molding system also includes a storage unit that stores a first correspondence specifying the relationship between the temperature of the weld bead and the EN ratio, and a second correspondence specifying the relationship between the welding current and the melting rate of the consuming electrode wire for each EN ratio. The control device calculates a first EN ratio corresponding to the temperature of the weld bead detected by the detection device based on the first correspondence, and calculates the welding current corresponding to the first EN ratio when the melting rate of the consuming electrode wire is set to constant based on the second correspondence.
3. The layered modeling system according to claim 2, wherein, The first correspondence is that the EN ratio increases as the temperature of the weld bead increases.
4. The layered modeling system according to claim 2, wherein, The second correspondence is that when the melting rate of the consuming electrode welding wire is set to constant, the welding current decreases as the EN ratio increases.
5. The layered modeling system according to claim 1, wherein, When the weld beads are stacked, the detection device can detect the shape of the weld bead closest to the stack as height information. The layered molding system also includes a storage unit that stores a third correspondence specifying the relationship between the height information and the EN ratio, and a second correspondence representing the relationship between the welding current and the melting rate of the consuming electrode wire for each EN ratio. The control device calculates the EN ratio corresponding to the height information detected by the detection device according to the third correspondence, and calculates the melting rate of the consumed electrode wire corresponding to the EN ratio when the welding current is set to constant according to the second correspondence.
6. The layered modeling system according to claim 5, wherein, The third correspondence is that the EN ratio decreases as the height of the weld bead increases.
7. The layered modeling system according to claim 5, wherein, The second correspondence is that when the welding current is set to constant, the melting rate of the electrode welding wire increases as the EN ratio increases.
Citation Information
Patent Citations
Laminate molded article manufacturing method
JP2022106172A