A 3D printed coil structure based on self-supporting design and its molding method
The 3D printed coil structure with a self-supporting design features a flow channel cross-section consisting of a rounded top and a rectangular bottom. Combined with a solid thickened layer or support feet, this design solves the problems of molding quality and post-processing difficulties in coil manufacturing, achieving efficient and reliable coil production.
Patent Information
- Application Number
- CN202611100103.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-07-23
- Publication Date
- 2026-11-17
AI Technical Summary
In the existing technology, there is a contradiction between forming quality and post-processing difficulty in metal additive manufacturing of coils. In particular, the internal support is difficult to remove and easily damages the inner wall of the flow channel, the separation process of the coil and the substrate can easily lead to damage to the functional tube wall, and the cleaning of unmelted powder is difficult.
The 3D printed coil structure adopts a self-supporting design. The flow channel cross section is composed of a combination of a circular arc top and a rectangular bottom. The local tilt angle of the circular arc top is greater than or equal to 45°. The connection between the coil body and the substrate is provided with a solid thickened layer or support feet, and is connected into one piece through a smooth transition. It is printed by combining partition scanning and contour offset strategies, and then separated by wire cutting.
It achieves stable molding without internal support, avoids damage to the inner wall of the flow channel and the effects of cutting heat, improves the yield of finished products and manufacturing reliability, simplifies post-processing procedures, and reduces material waste and costs.
Smart Images

Figure CN123102997A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of metal additive manufacturing technology, and in particular to a 3D printed coil structure based on a self-supporting design and its forming method. Background Technology
[0002] Metal additive manufacturing technology, with its advantage of being able to integrally mold complex internal flow channel structures without molds, has been widely used in high-end manufacturing fields such as electromagnetic coils and liquid cooling heat dissipation components. In this technological direction, to obtain specific electromagnetic properties or fluid heat transfer efficiency, coils are typically designed as tubular structures with complex, circuitous paths. Current mainstream technologies for manufacturing such coils usually employ processes such as selective laser melting, building the part by layering metal powder. During the specific process implementation, to cope with the influence of gravity on the molten metal and to ensure the forming stability of the suspended structure, technicians generally design and print auxiliary support structures below the suspended area based on the spatial orientation of the part, or adjust the placement angle of the part on the printing substrate to minimize the area of the horizontally suspended surface, thereby ensuring the continuity of the printing process and the basic geometric integrity of the part.
[0003] However, in long-term industrial practice, the manufacturing of this type of coil still faces a significant contradiction between molding quality and post-processing difficulty. On the one hand, for flow channel structures with specific cross-sectional shapes, insufficient local tilt angles during printing can easily lead to top collapse or rough inner walls. Relying on internal supports presents the dilemma of being difficult to remove and easily damaging the inner walls of the flow channels. On the other hand, after the metallurgical bonding between the coil body and the printing substrate, the separation process often carries a high risk of scrap, and functional tube walls are easily damaged due to cutting deviations or thermal effects. In addition, physical dead corners left by traditional cross-sectional designs also make it difficult to clean unmelted powder, thus affecting the final performance of the coil. These problems together constitute the key bottleneck restricting the yield and cost control of mass production of this type of high-precision coil. Summary of the Invention
[0004] This application provides a 3D printed coil structure based on self-supporting design and its molding method, which can solve the significant contradiction between molding quality and post-processing difficulty in the prior art coil manufacturing, especially the technical problems that internal supports are difficult to remove and easily damage the inner wall of the flow channel, the separation process of coil and substrate easily leads to damage to the functional tube wall, and the difficulty in cleaning unmelted powder.
[0005] To achieve the above objectives, this application provides a 3D printed coil structure based on a self-supporting design, including a coil body. The coil body has a flow channel, the cross-section of which is composed of a circular arc top and a rectangular bottom. The local tilt angle of any point on the circular arc top is greater than or equal to 45°. A solid thickened layer or a support foot is provided at the connection between the coil body and the substrate. The solid thickened layer or the support foot is smoothly transitioned to and connected to the flow channel as a whole.
[0006] Optionally, the arc-shaped top is a semicircle, and the diameter of the semicircle is equal to the width of the bottom of the rectangle.
[0007] Optionally, the solid thickening layer extends continuously along the bottom contour of the coil body, the outer surface of the solid thickening layer forms a bonding plane, and the thickness T of the solid thickening layer satisfies T ≥ A, where A is the single-sided machining allowance of the wire cutting separation process.
[0008] Optionally, the arc-shaped top is a parabolic arc, an elliptical arc, or an approximate arc surface formed by splicing together multiple continuous straight line segments.
[0009] Optionally, the coil body is formed in a horizontal position, and the major axis of the flow channel is parallel to the plane of the printing substrate.
[0010] Optionally, the local tilt angle at any point on the arc-shaped top is 45°-90°.
[0011] Furthermore, to achieve the above objectives, this application also provides a method for forming the aforementioned 3D printed coil structure based on a self-supporting design, comprising the following steps: A three-dimensional model of the target coil is constructed in a three-dimensional modeling software, the three-dimensional model is cross-sectioned, and the data of the three-dimensional model is imported into a 3D printing device; The printing parameters of the 3D printing equipment are set, and the printing is carried out using a partitioned scanning and contour offset strategy to obtain the blank of the target coil; After printing is completed, the blank is removed from the substrate of the 3D printing equipment, and after grinding, polishing and stress relief treatment, the target coil is obtained.
[0012] Optionally, the method for constructing the three-dimensional model of the target coil includes: A preliminary model of the target coil is constructed, the preliminary model including a coil body having a square flow channel; In the preliminary model, the upper surface of the flow channel constituting the target coil is surfaced, so that the cross-section of the flow channel forms a combination of an arc-shaped top and a rectangular bottom; In the preliminary model, the bottom of the target coil is offset and extended along the forming height direction and filled into a solid to form a solid thickened layer or support foot, and allowance is reserved for wire cutting processing.
[0013] Optionally, the printing parameters of the 3D printing equipment are set as follows: The laser power is 500W-700W, the scanning speed is 600mm / s-1000mm / s, and the layer thickness is set to 55μm-65μm.
[0014] Optionally, the partitioned scanning includes: dividing each layer of the three-dimensional model into multiple different printing areas, and setting a scanning direction rotation angle between each area; The contour offset strategy includes: first completing the closed scan of the outer contour of the target coil, then filling the inner area, and for the arc-shaped top area of the target coil, using a 5%-10% increase in laser power to perform dynamic energy compensation printing.
[0015] Compared with the prior art, this application has the following beneficial effects: This application provides a 3D printed coil structure based on a self-supporting design and its forming method. This scheme designs the coil flow channel cross-section as a combination of a circular arc top and a rectangular bottom, ensuring that the local tilt angle at any point on the circular arc top is greater than or equal to 45°. This allows each layer of molten metal to directly overlap the solidified inclined surface of the lower layer during the layer-by-layer printing process. Self-supporting forming is achieved through the balance of gravity and surface tension, thus completely eliminating the dependence on sacrificial support structures inside the flow channel. This avoids internal wall damage and residue problems caused by support removal. Simultaneously, the smooth, continuous circular arc surface eliminates right-angle dead corners, facilitating the cleaning of unmelted powder. Based on this, by setting a solid thickened layer or support foot that is integrated with the flow channel at the connection between the coil body and the substrate, and separating it along the thickened area by wire cutting after molding, the cutting path is completely located within the reserved non-functional solid material area, effectively isolating the heat-affected zone of cutting from the functional tube wall. Therefore, it avoids the significant contradiction between molding quality and post-processing difficulty faced by coil manufacturing in the prior art, especially the technical problems of internal support being difficult to remove and easily damaging the inner wall of the flow channel, the functional tube wall being easily damaged during the separation process of the coil and the substrate, and the difficulty in cleaning unmelted powder. This significantly improves the yield of finished coils, the consistency of internal flow channels, and the overall manufacturing reliability. Attached Figure Description
[0016] Figure 1 A schematic diagram of a 3D printed coil structure based on a self-supporting design is provided for this application; Figure 2 A schematic diagram of the cross-sectional structure of the coil body with a semi-circular top arc shape, provided for this application; Figure 3 A side view of the coil body with a continuously extending solid thickened layer provided for this application; Figure 4 A schematic diagram of the cross-section of the coil body with a parabolic arc, elliptical arc, or multiple continuous straight line segments spliced together for the purpose of this application; Figure 5 A schematic diagram of the mating structure between the coil body and the substrate in a horizontally shaped manner provided in this application; Figure 6 Enlarged detail views of the flow channel cross-section with a local tilt angle of 45°-90° provided for this application; Figure 7 This is a schematic flowchart illustrating a molding method for a 3D printed coil structure based on a self-supporting design, as provided in this application.
[0017] Figure Labels 1-Coil body; 2-Flow channel; 3-Arc-shaped top; 4-Rectangular bottom; 5-Solid thickened layer; 6-Support foot; 7-Substrate; 8-Lamination plane. Detailed Implementation
[0018] The technical solutions in the embodiments of this application will be clearly and completely described below. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments. Based on the embodiments in this application, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of this application.
[0019] Example 1 like Figure 1 As shown, this embodiment provides a 3D-printed coil structure based on a self-supporting design. The 3D-printed coil structure includes: a coil body 1, a flow channel 2, an arc-shaped top 3, a rectangular bottom 4, a solid thickening layer 5, supporting feet 6, and a substrate 7. The coil body 1 has a flow channel 2, the cross-section of which is formed by a combination of the arc-shaped top 3 and the rectangular bottom 4. In this embodiment, the flow channel 2 constitutes the core channel inside the coil body 1 for the flow of cooling medium or electrical connection. This cross-sectional shape is designed to adapt to the process characteristics of additive manufacturing, particularly solving the printing challenges of suspended structures. The combination of the arc-shaped top 3 and the rectangular bottom 4 ensures that the top has a smooth curvature to facilitate fluid flow or electrical performance, while the rectangular structure at the bottom provides a larger contact area to enhance stability.
[0020] Specifically, the arc-shaped top 3 can adopt a semi-circular, superior, or inferior arc structure, and its radius of curvature can be optimized according to the coil size and printed layer thickness; the rectangular bottom 4 provides a flat bottom surface for easy contact with the substrate or other structures. It should be understood that this combined cross-sectional shape is not a simple geometric splicing, but a smooth transition connection to avoid stress concentration and fluid resistance.
[0021] The local tilt angle at any point on the top arc of the 3rd arc is greater than or equal to 45°. Specifically, this feature is a key geometric constraint for achieving self-supporting printing. During 3D printing, molten material needs support from the underlying solid layer when stacking; if the tilt angle is too small, the suspended portion is prone to collapse or sagging. The local tilt angle can be defined as the angle between the tangent at any point on the top curve of the flow channel and the horizontal plane. When this angle satisfies... At an angle ≥45°, based on experience in materials mechanics and additive manufacturing processes, the adhesion force between material layers is sufficient to overcome the slippage component caused by gravity, thereby ensuring molding quality. This indicates a local tilt angle, expressed in degrees (°). In actual printing path planning, this geometry ensures that each new layer of material can be directly laid on top of the solidified underlying material during the movement of the print head or laser energy source, without relying on additional support structures. This not only simplifies the printing process but also eliminates the subsequent step of removing support structures, avoiding surface damage caused by support removal.
[0022] A solid thickened layer 5 or a support foot 6 is provided at the connection point between the coil body 1 and the substrate 7. In this embodiment, this design aims to solve the problem of easy damage when the coil is separated from the substrate 7 after printing. In 3D printing, the coil body 1 is usually printed directly on the substrate 7, and the two are metallurgically bonded through a molten pool, resulting in extremely high connection strength. If separation is performed directly using methods such as wire cutting, the tube wall of the flow channel 2 is easily damaged due to cutting errors or heat-affected zone, leading to coil scrap. The solid thickened layer 5 or the support foot 6 serves as a sacrificial layer or process reinforcement structure at the connection point.
[0023] Specifically, the solid thickening layer 5 can be a region of increased thickness, either entirely or partially, at the bottom of the coil body 1; the support feet 6 can be discretely distributed columnar or block-shaped protrusions. Their function is to reserve additional material thickness, ensuring that the wire cutting processing path lies within the solid thickening layer 5 or the support feet 6, thus maintaining a safe physical distance from the wall of the flow channel 2. It should be understood that the solid thickening layer 5 and the support feet 6 can be used individually or in combination, depending on the actual printing layout and stress requirements. Their specific dimensions and distribution density should be set according to the weight of the coil, the cutting process parameters, and the material properties of the substrate 7.
[0024] The solid thickened layer 5 or support foot 6 smoothly transitions and connects to the flow channel 2 as a single unit. In this structure, a smooth transition can mean that the surface of the solid thickened layer 5 or support foot 6 is connected to the outer wall of the flow channel 2 through rounded corners, bevels, or continuously curved surfaces, without sharp edges or abrupt steps. Being connected as a single unit means that during the printing process, the solid thickened layer 5 or support foot 6 and the coil body 1 are made of the same material and printed synchronously, forming a unified structure through interatomic metallurgical bonding. Specifically, this smooth transition can be achieved through chamfering operations or Boolean operation optimization during CAD modeling. For example, the radius of the rounded corners in the transition area... The settings can be based on the minimum resolution and stress concentration factor of the printing equipment; a typical relationship can be expressed as follows: ,in The wall thickness of channel 2. It is an empirical coefficient greater than 0 (usually taken as 0.5 to 1). This design not only ensures the mechanical strength of the connection and avoids the initiation of cracks caused by stress concentration, but more importantly, it ensures the continuity and smoothness of the inner wall of the flow channel 2, preventing steps or depressions in the transition area, thereby avoiding the accumulation of cooling medium or the deterioration of electrical performance.
[0025] The core innovation of this application lies in constructing a self-supporting structure system for 3D printed coils based on specific geometric constraints. This system eliminates the risk of collapse during the printing process by designing the flow channel cross-section as a combination of a circular arc top and a rectangular bottom, and strictly limiting the local tilt angle at any point on the top curve to be greater than or equal to 45°, thus achieving true self-supporting molding. Simultaneously, by introducing a solid thickened layer or support foot at the connection between the coil body and the substrate, and designing it as a smoothly transitioning integrated structure with the flow channel, the system cleverly combines the requirements of the printing process with the requirements of post-processing separation, providing a physical basis for non-destructive separation while ensuring structural integrity.
[0026] The working process and principle of this application are as follows: During 3D printing, the equipment first deposits material layer by layer according to the slice data. When printing to the flow channel area, since the inclination angle of the arc-shaped top 3 is always maintained above 45°, each layer of molten metal is effectively supported by the solidified metal below before solidification. The material remains stable under the combined action of surface tension and interlayer bonding force, and will not collapse or deform, thus naturally forming a closed or open flow channel cross-section. As printing continues, the coil body 1 gradually takes shape and is firmly bonded to the substrate 7 at the bottom. In the area of the solid thickened layer 5 or support foot 6, the material is also deposited layer by layer to form a solid structure thicker than the flow channel wall, and naturally merges with the outer wall of the flow channel through a smooth transition surface. After printing is completed, a demolding operation is performed, and the solid thickened layer 5 or support foot 6 is cut along the predetermined path using processing methods such as wire cutting. Since the thickened layer or support foot provides sufficient material allowance, the sparks and heat-affected zone generated during the cutting process only act on these sacrificial structures and will not affect the tube wall of the flow channel 2, thus achieving safe separation of the coil from the substrate.
[0027] Through the above technical solution, this application achieves the following beneficial effects: Since the flow channel cross-section adopts a combination of an arc-shaped top and a rectangular bottom with a local tilt angle of 45° or greater at the top, it can be stably formed without adding any internal support structure during the 3D printing process. This effectively avoids flow channel blockage and inner wall damage caused by residual support material or removal of support, while also significantly reducing material waste and post-processing time, thus improving manufacturing efficiency. Since a solid thickened layer or support foot is set at the connection between the coil body and the substrate, and both are smoothly transitioned and connected to the flow channel, when the coil and substrate are separated by wire cutting in the subsequent process, the cutting path is located in the thickened area, physically away from the functional flow channel wall. This completely solves the problem that traditional cutting methods easily damage the tube wall, leading to coil scrapping, and significantly improves the product yield and reliability.
[0028] Example 2 like Figure 2 As shown, this application embodiment provides a 3D printed coil structure based on a self-supporting design. The coil body 1 has a flow channel 2, the cross-section of which is composed of an arc-shaped top 3 and a rectangular bottom 4. The arc-shaped top 3 is semi-circular, and the diameter of the semi-circle is equal to the width of the rectangular bottom 4.
[0029] The specific geometric dimensions described above define the cross-section of channel 2 as a standard D-shaped structure. In this embodiment, the arc-shaped top 3 adopts a semi-circular design, ensuring that the angle between the tangent at any point on the arc surface and the horizontal plane is greater than or equal to 45°. This geometric characteristic allows the molten metal powder to obtain continuous solid support from the underlying material during the cooling and solidification process when using metal 3D printing processes, such as Selective Laser Melting (SLM) or Laser Engineered Net Shaping (LENS), for layer-by-layer deposition manufacturing. This satisfies the critical angle requirement for self-supporting molding, eliminating the need for additional auxiliary support structures inside the channel.
[0030] Meanwhile, the fact that the width of the rectangular bottom 4 is equal to the diameter of the semicircle ensures that the width of the flow channel 2 remains consistent in the horizontal direction. This design not only guarantees that the flow channel 2 has sufficient cross-sectional area to meet the needs of cooling medium flow or current conduction, but also simplifies the parametric modeling process of the 3D model, facilitating precise control of the overall dimensions of the flow channel 2 through a single width parameter. Furthermore, this standardized cross-sectional shape helps maintain the structural consistency of the coil body 1 during the printing process, avoiding thermal stress concentration caused by abrupt changes in cross-sectional dimensions, thereby improving the coil's molding yield and mechanical properties.
[0031] Through the above technical solution, this application achieves further optimization of the flow channel cross-sectional shape, constructing a standard D-shaped cross-section with defined geometric parameters. This structure not only geometrically ensures that the tilt angle at each point of the arc surface meets the self-support condition, completely eliminating the need to add support structures inside the flow channel, reducing printing costs and post-processing difficulties, but also simplifies the manufacturing process through dimensional co-design, improving the stability and repeatability of the coil structure in the 3D printing process.
[0032] Example 3 like Figure 3As shown, this embodiment provides a 3D printed coil structure based on a self-supporting design. The solid thickening layer 5 extends continuously along the bottom contour of the coil body 1, and the outer surface of the solid thickening layer 5 forms a bonding plane 8. The thickness T of the solid thickening layer 5 satisfies T≥A, where A is the single-sided machining allowance of the wire cutting separation process. Unlike conventional designs, this application innovatively designs the solid thickening layer 5 as a structure that extends continuously along the bottom contour of the coil body 1, rather than only making local point contact. This continuous extension layout allows the coil body 1 to be tightly bonded to the substrate 7 through the large-area bonding plane 8 during the printing process, thereby significantly enhancing the adhesion and thermal conductivity stability during the printing process and effectively suppressing the risk of printing deformation caused by local warping or thermal stress concentration. Simultaneously, the bonding plane 8 formed by the outer surface provides a flat mounting reference for the printing substrate 7, which helps ensure the coil's posture accuracy in the printing space.
[0033] The design of the bonding plane 8 allows the coil body 1 to be placed stably on the printing substrate 7, ensuring the flatness of the printing start layer. In practical applications, the bonding plane 8 should maintain good surface contact with the substrate 7 to avoid printing defects caused by poor contact. The surface roughness of the bonding plane 8 can be appropriately adjusted according to the printing process requirements; for example, it can be the original surface after printing or a surface that has undergone slight polishing. This application embodiment does not impose any special limitations on this.
[0034] This thickness design is a key technical feature of this application in solving the problem of wire EDM damage to the coil tube wall. Specifically, the mathematical relationship between the thickness T and the single-sided machining allowance A during wire EDM can be expressed as follows: .in, This indicates the geometric thickness of the solid thickening layer 5 in the direction perpendicular to the bonding plane 8, usually expressed in millimeters (mm). This represents the minimum machining allowance per side required in wire EDM to ensure complete cut and compensate for tool deviation and heat-affected zone. Its value depends on the wire diameter, discharge gap, and material properties; for example, it can be 0.5mm, 1.0mm, or other process-defined values. By strictly meeting these requirements... This design ensures that during wire EDM separation, the cutting path remains entirely within the solid material of the thickened layer 5, without intruding into the functional tube wall area of the coil body 1. This design overcomes the limitations of traditional direct bonding of coils to the substrate, which results in insufficient cutting allowance and easy damage to the tube wall. It completely confines the heat-affected zone and the risk of mechanical overcutting within the sacrificial thickened layer material, thus fundamentally avoiding damage to the coil body 1 while ensuring smooth separation, significantly improving the yield and safety of the finished product. It should be understood that the specific value of the thickness T can vary depending on the wire EDM process parameters, as long as the condition T≥A is met; this embodiment does not impose any special limitations on this.
[0035] Through the above technical solution, this application achieves the following: by setting a continuously extending solid thickening layer 5 with a thickness meeting specific requirements at the bottom of the coil body 1, the printing stability is enhanced by using the bonding plane 8, while providing sufficient machining allowance for wire cutting separation. Because the thickness T of the solid thickening layer 5 is designed to be greater than or equal to the single-sided machining allowance A of wire cutting, the technical problem of cutting the bottom wall of the coil due to positioning deviation or thermal effects during wire cutting separation in the prior art is completely solved, thereby achieving the technical effect of significantly improving separation safety and finished product yield, and reducing scrap costs.
[0036] Example 4 like Figure 4 As shown, this embodiment provides a 3D printed coil structure based on a self-supporting design. This structure mainly involves the further design of the geometry at the top of the flow channel. The arc-shaped top 3 is an approximate arc surface formed by a parabolic arc, an elliptical arc, or multiple continuous straight line segments. As the upper boundary structure of the flow channel 2 cross-section, the arc-shaped top 3's core function is to replace traditional planar or right-angled structures, utilizing specific curved surface geometric characteristics to meet the self-supporting molding requirements in metal 3D printing. In this embodiment, the specific contour curve of the arc-shaped top 3 is not limited to a standard semicircle, but can be flexibly adjusted according to the actual application scenario's requirements for fluid dynamics performance, structural strength, or spatial layout. For example, when using a parabolic arc, its radius of curvature varies with height, providing different guiding characteristics than a circular arc. When using an elliptical arc, the flatness or aspect ratio of the cross-section can be optimized while maintaining the self-supporting angle by adjusting the ratio of the major and minor axes of the ellipse. When using an approximate arc surface formed by splicing multiple continuous straight line segments, a trapezoidal or polygonal top structure can be constructed through polygon approximation. This structure may have better adaptability in mold processing or certain specific slicing algorithms. It should be understood that regardless of the specific geometry used, the design must follow a common physical constraint: the local tilt angle at any point on the arc-shaped top 3 must be greater than or equal to 45° to ensure the stable forming of the molten metal material during printing.
[0037] Through the above technical solution, this application effectively expands the design freedom of the top structure of the flow channel. By limiting the arc-shaped top 3 to a parabolic arc, elliptical arc, or an approximate arc surface formed by splicing multiple continuous straight line segments, it breaks the single design mode that relies solely on the standard semi-circular structure. This allows designers to optimize the flow channel cross-section according to the specific operating conditions of the coil (such as coolant flow rate requirements, electromagnetic field distribution requirements, or geometric constraints of the installation space). This diversified structural design, while ensuring compliance with the self-supporting process requirements of 3D printing and eliminating the need for internal supports, further improves the overall performance of the coil structure, taking into account both manufacturing feasibility and functional optimization.
[0038] Example 5 like Figure 5 As shown, this embodiment provides a forming posture for a 3D printed coil structure based on a self-supporting design. This forming posture mainly involves the spatial orientation of the coil body 1 relative to the printing substrate 7. Specifically, the coil body 1 is formed in a horizontal posture, and the major axis of the flow channel 2 is parallel to the plane of the printing substrate 7.
[0039] The aforementioned coil body 1 is formed in a horizontal orientation, which means that the overall length direction or main extension plane of the coil body 1 is placed horizontally, allowing it to be stacked layer by layer in the horizontal direction during the printing process. This horizontal placement method differs from the existing technology that places the coil vertically. In the horizontal orientation, the long axis of the flow channel 2 is parallel to the plane of the printing substrate 7, meaning that the longest dimension of the flow channel 2 remains horizontal, i.e., perpendicular to the direction of gravity or the movement direction of the printing powder spreading blade. For the aforementioned flow channel 2 cross-section composed of the arc-shaped top 3 and the rectangular bottom 4, its long axis usually corresponds to the width direction of the rectangular bottom 4 or the span direction of the arc-shaped top 3.
[0040] This orientation fully utilizes the self-supporting characteristics of the arc-shaped top 3. Since the local tilt angle at any point on the arc-shaped top 3 is greater than or equal to 45°, during horizontal printing, the suspended surface at the top of the flow channel 2 can receive continuous support from the lower layer of molten metal, thus avoiding top collapse or deformation defects caused by large-area horizontal suspension. Simultaneously, by placing the coil body 1 horizontally, the printing height is significantly reduced, the number of printing layers is decreased, thereby shortening the forming time, reducing equipment energy consumption, and improving production efficiency.
[0041] Furthermore, this horizontal orientation, combined with the design of the solid thickened layer 5, allows the solid thickened layer 5 to adhere smoothly to the printing substrate 7. This structure not only facilitates heat conduction and stress distribution during the printing process but also provides a stable processing benchmark and sufficient processing allowance for the subsequent wire cutting separation process, effectively avoiding the problem of difficult separation of the bottom fusion caused by vertical printing. It should be understood that although this embodiment preferably adopts a completely horizontal orientation, in other embodiments, the coil body 1 can be tilted at a small angle (e.g., within 15°) relative to the plane of the printing substrate 7, depending on the actual operating conditions of the printing equipment, as long as the long axis of the flow channel 2 is basically parallel to the plane of the printing substrate 7 and the arc-shaped top 3 meets the self-support angle requirements. This application embodiment does not impose any special limitations on this.
[0042] Through the above technical solution, this application optimizes the coil printing process. Because the coil body 1 is formed in a horizontal orientation and the long axis of the flow channel 2 is parallel to the plane of the printing substrate 7, combined with the self-supporting design of the arc-shaped structure at the top of the flow channel 2, the technical problems of high printing height, long cycle time, and difficulty in separating the bottom fusion caused by traditional vertical placement are solved. This horizontal printing strategy effectively reduces printing height and forming time while ensuring molding quality and eliminating the need for internal support. Furthermore, the thickened bottom design enables safe separation, thereby achieving the technical effects of improving production efficiency, reducing manufacturing costs, and increasing product yield.
[0043] Example 6 like Figure 6 As shown, this embodiment provides a 3D printed coil structure based on a self-supporting design. This coil structure primarily further defines the geometric parameters of the arc-shaped top 3 of the flow channel 2. Specifically, the local tilt angle at any point on the arc-shaped top is 45°-90°.
[0044] The local tilt angle mentioned here refers to the angle between the tangent at the point of the arc-shaped top 3 of the flow channel 2 and the horizontal plane. This angle reflects the degree of tilt of the arc surface during the printing process. Limiting the local tilt angle to the range of 45°-90° is based on the self-supporting characteristics of molten powder or filament in metal 3D printing. When the local tilt angle is greater than or equal to 45°, the molten material can obtain effective support from the solidified layer below during layer-by-layer deposition, thus avoiding collapse and ensuring molding quality. Simultaneously, limiting the upper limit of the angle to 90° avoids excessive steepness leading to reduced space utilization and also helps maintain the overall structural strength and hydrodynamic performance of the flow channel 2 cross-section. Within this angle range, the arc-shaped top 3 can form a smoothly transitioned surface, maximizing the effective flow cross-sectional area of the flow channel 2 while ensuring the feasibility of unsupported printing, thereby improving the cooling efficiency or conductivity of the coil. It should be understood that 45°-90° is the preferred range. In practical applications, the specific value of the local tilt angle can be flexibly selected within this range according to the specific characteristics of the printing material, layer thickness parameters or scanning strategy, such as setting it to 60°, 75°, etc. The embodiments of this application do not impose any special limitations on this.
[0045] Through the above technical solution, this application achieves precise control over the self-supporting capability of the arc-shaped top 3 of the flow channel 2. By strictly limiting the local tilt angle to between 45° and 90°, it ensures that the arc-shaped top 3 can be stably formed without internal support during horizontal printing, eliminating the risk of damage to the inner wall due to difficulty in removing the support. Furthermore, by optimizing the flow channel cross-sectional shape through a reasonable angle range, it avoids wasted flow channel space due to excessive angle or forming defects due to excessive angle. Thus, while ensuring printing yield and structural stability, it improves the overall performance of the coil.
[0046] Example 7 In another alternative embodiment, such as Figure 7 The diagram shown is a flowchart illustrating a method for forming a 3D printed coil structure based on a self-supporting design, according to an embodiment of this application. The method includes the following steps: Step S701: Construct a 3D model of the target coil in 3D modeling software, cross-section the 3D model, and import the data of the 3D model into the 3D printing equipment.
[0047] A 3D model of the target coil is constructed in Computer-Aided Design (CAD) software to digitize the self-supporting coil structure defined in the aforementioned embodiments. This model must accurately reflect the geometric features of the flow channel cross-section, which consists of a circular arc top and a rectangular bottom, as well as the solid thickened layer or support leg structure at the connection between the coil body and the substrate. Considering dimensional deviations during 3D printing, such as correcting and compensating for the original design dimensions, the cross-sectional dimensions of the coil are appropriately enlarged to offset printing shrinkage and ensure dimensional accuracy after molding.
[0048] The slicing algorithm performs faceting processing on the 3D model, converting the continuous 3D digital model into 2D layer data recognizable by the printing equipment. Based on the preset printing layer thickness, the model is segmented layer by layer along the height direction, generating the contour information and infill path for each layer. The generated slice data is then imported into the 3D printing equipment to prepare for subsequent printing operations, ensuring that the printing equipment can control the movement of the laser or electron beam according to precise path instructions, thereby depositing material layer by layer on the substrate.
[0049] Step S702: Set the printing parameters of the 3D printing equipment, and use the partition scanning and contour offset strategy to print to obtain the blank of the target coil.
[0050] Configure printing parameters such as laser power, scanning speed, and layer thickness to ensure molding quality. In this embodiment, the laser power is set to, for example, 500W to 700W, the scanning speed is set to, for example, 600mm / s to 1000mm / s, and the layer thickness is set to, for example, 60μm. Properly configuring these process parameters ensures that the copper alloy powder is fully fused during the melting process, while avoiding deformation or warping caused by overheating.
[0051] To reduce thermal stress accumulation during printing, a partitioned scanning strategy is employed. Each layer's sliced area is divided into multiple rectangular sub-regions, such as blocks measuring 50mm × 50mm. During printing, adjacent sub-regions are scanned with a rotational angle difference, for example, a 67° rotation. This staggered scanning method breaks the directional accumulation of heat, effectively reducing residual stress and preventing the blank from cracking or deforming due to excessive thermal stress.
[0052] To improve the forming accuracy and surface quality of the part edges, a contour offset strategy is employed for printing. This strategy prioritizes scanning the outer contour of the part before filling the internal areas. The contour scan, for example, involves offsetting the outer contour line inward by a certain distance (e.g., 0.1 mm) to form the scanning path. This method first solidifies a clear boundary, enhancing the stability of the edge portion and preventing edge collapse during subsequent filling scans. Through the combination of this partitioned scanning and contour offset strategy, the printed target coil blank possesses a dense internal structure and precise geometric shape.
[0053] Step S703: After printing is completed, the blank is removed from the substrate of the 3D printing equipment, and after grinding, polishing and stress relief treatment, the target coil is obtained.
[0054] The blank is removed from the substrate of the 3D printing equipment by utilizing the solid thickened layer or the machining allowance reserved in the support legs designed at the bottom of the coil. For example, the blank is separated from the substrate along a predetermined path of the solid thickened layer by wire cutting or milling. This separation method makes full use of the protective function of the bottom thickened layer, ensuring that the functional tube wall of the coil body is not damaged during the cutting process, thereby obtaining an independent part.
[0055] The blank is ground step by step using sandpaper of different grits until the surface roughness meets the design requirements, in order to eliminate melt lines, powder adhesion defects, and support removal marks on the blank surface. This process not only improves the appearance quality of the coil, but more importantly, it removes microscopic protrusions and burrs on the surface, avoiding local electric field concentration or increased fluid resistance caused by uneven surface.
[0056] The preform is held at a specific temperature for a period of time and then cooled in the furnace or in the air to release the residual stress accumulated inside the material during the printing process. Through stress relief treatment, the microstructure of the material can be improved, the part dimensions can be stabilized, and the coil can be prevented from deforming due to stress release during use, thus ultimately obtaining a target coil with stable performance and accurate dimensions.
[0057] By achieving precise digitization of the self-supporting structure through 3D modeling, and combining partitioned scanning and contour offset strategies to control thermal stress and molding accuracy, and by optimizing the bottom structure and releasing stress in the post-processing stage, the above steps work together to effectively solve the problems of low molding yield, difficult post-processing and high manufacturing cost of traditional 3D printed copper coils, and realize the integrated manufacturing of high-quality coils.
[0058] Example 8 In one alternative implementation, the method for constructing a three-dimensional model of the target coil includes: Step S801: Construct a preliminary model of the target coil. The preliminary model includes the coil body, which has a square flow channel.
[0059] Based on the overall design parameters of the target coil, such as the number of turns, loop routing, and center diameter, a basic geometric framework, or preliminary model, is established in a 3D modeling environment. This preliminary model includes the coil body, whose internal flow channels are configured with a conventional square cross-section structure. Specifically, this square flow channel is enclosed by four mutually perpendicular planes, with the top being a horizontal plane and the sidewalls being vertical planes. This preliminary model establishes the geometric benchmark for subsequent structural optimization and clarifies the initial spatial morphology of the flow channels.
[0060] Step S802: In the preliminary model, the upper surface of the flow channel constituting the target coil is surfaced, so that the cross-section of the flow channel forms a combination of a circular arc top and a rectangular bottom.
[0061] To address the limitations of additive manufacturing processes on suspended structures, the upper surface of the flow channel in the preliminary model was geometrically reconstructed. By replacing the horizontal plane at the top of the original square flow channel with an arc surface of specific curvature, the horizontal suspended area during printing was eliminated. After this surface treatment, the cross-sectional shape of the flow channel evolved into a composite structure consisting of an arc-shaped top and a rectangular bottom. The arc-shaped top replaced the original horizontal upper surface, while the rectangular bottom retained the straight lower part of the original square flow channel. During this process, the radius of curvature of the arc was precisely controlled to ensure that the angle between the tangent at any point on the arc surface and the horizontal plane met the requirements of the self-supporting printing process. This geometric adjustment allows the molten metal to naturally form based on the underlying material during deposition, eliminating the need for additional auxiliary support structures, thereby optimizing the printing path and improving the forming quality.
[0062] Step S803: In the preliminary model, the bottom of the target coil is offset and extended along the forming height direction and filled into a solid to form a solid thickened layer or support foot, and allowance is reserved for wire cutting processing.
[0063] To ensure structural integrity when the coil separates from the printing substrate, the connection area between the bottom of the model and the substrate is reinforced. Specifically, the outline of the bottom of the target coil is offset downwards along the molding height direction, and the extended area is solidly filled to create a solid thickened layer or support foot that smoothly transitions with the coil body. During the construction of this solid structure, the thickness of the thickened layer is set according to the characteristics of the wire cutting process, making it greater than the single-sided machining allowance required for wire cutting. This design ensures that the subsequent wire cutting separation path is entirely within the solid thickened layer, thereby effectively isolating the heat-affected zone and mechanical action zone generated by cutting from the working tube wall of the coil body in physical space. This not only achieves safe separation of the coil from the substrate but also avoids damage to the flow channel wall caused by the cutting operation, ensuring the sealing and overall performance of the finished coil.
[0064] Example 9 In another optional embodiment, the method provided in this application further includes: the printing parameters of the 3D printing equipment are set as follows: laser power is 500W-700W, scanning speed is 600mm / s-1000mm / s, and layer thickness is set to 55μm-65μm.
[0065] The laser power was set to 500W-700W. Laser power characterizes the energy output of the laser beam per unit time and is a key heat source parameter determining whether the metal powder can be fully melted. Within this power range, the laser energy density is sufficient to instantly melt the copper alloy powder and form a stable molten pool, avoiding both poor fusion or spheroidization caused by insufficient energy and overheating and splattering caused by excessive power. This parameter range is the optimal process window determined through experimental optimization, taking into account the high reflectivity and high thermal conductivity characteristics of copper alloy materials.
[0066] The scanning speed is configured between 600 mm / s and 1000 mm / s. The scanning speed determines the movement rate of the laser spot on the powder layer, directly controlling the energy input per unit length. This speed range provides good energy matching with the aforementioned laser power, ensuring an appropriate residence time for the molten pool. This allows for complete powder melting while simultaneously refining the grains using a relatively fast cooling rate. This configuration balances printing efficiency and forming quality, effectively avoiding thermal accumulation deformation caused by excessively slow speeds or insufficient interlayer bonding due to excessively fast speeds.
[0067] The layer thickness is set to 55μm-65μm. Layer thickness refers to the thickness of each powder layer, which directly determines the resolution and surface roughness of the formed part in the Z-axis direction. Controlling this parameter between 55μm and 65μm can provide fine forming accuracy while ensuring printing efficiency. This layer thickness range ensures that the laser energy can completely penetrate the current powder layer and melt part of the underlying formed entity, thereby obtaining good interlayer metallurgical bonding and avoiding problems such as interlayer separation or excessive porosity.
[0068] By coordinating the above printing parameters, a stable thermal cycle can be established during the printing process, thereby obtaining a coil blank with high density, few internal defects, and excellent surface quality.
[0069] Example 10 In another optional embodiment, the method provided in this application further includes the following steps: Partition scanning includes dividing each layer of the 3D model into multiple different printing areas, and setting the scanning direction rotation angle between each area; Each layer to be printed is divided into multiple independent printing sub-regions. This division aims to disperse heat input by changing the direction of the laser scanning path, thereby reducing the accumulation of thermal stress caused by continuous scanning in a single direction. In practice, each layer can be divided into a grid area of fixed size, such as a 50mm × 50mm square grid, or adaptively divided according to the geometric characteristics of the coil structure. After determining each sub-region, the scanning direction rotation angle between adjacent or specific regions is set, causing the laser scanning vector to deflect in different regions. For example, the scanning direction rotation angle between adjacent regions can be set to 67°, or it can be randomly selected within the range of 0° to 90° according to a preset rule.
[0070] The contour offset strategy includes: first completing the closed scan of the outer contour of the target coil, then filling the inner area, and for the arc-shaped top area of the target coil, using a 5%-10% increase in laser power to perform dynamic energy compensation printing.
[0071] Before performing internal filling, the outer contour of the target coil is first closed-loop scanned. The laser beam scans once or multiple times along the outermost boundary path of the part's cross-section, forming a dense, closed outer frame. This process preferentially melts and solidifies the edge contour of the part, enhancing the bonding force between the edge and the substrate or lower molten pool, effectively preventing edge collapse or spheroidization that may occur during subsequent internal filling. After completing the outer contour scan, the remaining internal area is filled. For the arc-shaped top area of the target coil, due to the inclined surface, the energy density distribution of the laser beam on the inclined surface is attenuated compared to the horizontal surface, and the heat dissipation conditions are more complex, which can easily lead to poor fusion or step effects. To address this, a dynamic energy compensation mechanism is introduced, increasing the laser power by 5%-10% from the reference power when printing the arc-shaped top area. For example, when the reference laser power is set to 600W, the laser power for scanning the arc-shaped top area is dynamically adjusted to between 630W and 660W. This dynamic compensation ensures that the curved area receives sufficient linear energy input, achieving full metallurgical bonding between the molten pool and the underlying material or adjacent molten channels. It avoids weak interlayer bonding or porosity defects caused by insufficient energy, thereby ensuring the compactness and surface smoothness of the inner wall of the coil flow channel.
[0072] By combining the above-mentioned partitioned scanning and contour offset strategies, residual stress during the printing process is effectively reduced. At the same time, targeted energy optimization is carried out for the special arc top structure, ensuring high-quality forming of the coil as a whole.
[0073] The above are merely preferred embodiments of this application and do not limit the patent scope of this application. Any equivalent structural or procedural transformations made using the content of this application's specification and drawings, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of this application.
Claims
1. A 3D printed coil structure based on a self-supporting design comprising a coil body, characterized in that, The coil body has a flow channel, the cross-section of which is composed of a circular arc top and a rectangular bottom. The local tilt angle of any point on the circular arc top is greater than or equal to 45°. The connection between the coil body and the substrate is provided with a solid thickened layer or a support foot. The solid thickened layer or the support foot is smoothly transitioned to the flow channel and connected as a whole.
2. The 3D-printed coil structure based on a self-supporting design according to claim 1, characterized in that, The top of the arc is a semicircle, and the diameter of the semicircle is equal to the width of the bottom of the rectangle.
3. The 3D printed coil structure based on a self-supporting design according to claim 1, characterized in that, The solid thickening layer extends continuously along the bottom contour of the coil body, and the outer surface of the solid thickening layer forms a bonding plane. The thickness T of the solid thickening layer satisfies T ≥ A, where A is the single-sided machining allowance of the wire cutting separation process.
4. The 3D-printed coil structure based on a self-supporting design according to claim 1, characterized in that, The arc-shaped top is an approximate arc surface formed by a parabolic arc, an elliptical arc, or multiple continuous straight line segments.
5. The 3D-printed coil structure based on a self-supporting design according to claim 1, characterized in that, The coil body is formed in a horizontal position, and the long axis of the flow channel is parallel to the plane of the printing substrate.
6. The 3D-printed coil structure based on a self-supporting design according to any of claims 1-5, characterized in that, The local tilt angle at any point on the arc-shaped top is 45°-90°.
7. A forming method of a 3D printed coil structure based on a self-supporting design according to any one of claims 1-6, characterized in that, Includes the following steps: A three-dimensional model of the target coil is constructed in a three-dimensional modeling software, the three-dimensional model is cross-sectioned, and the data of the three-dimensional model is imported into a 3D printing device; The printing parameters of the 3D printing equipment are set, and the printing is carried out using a partitioned scanning and contour offset strategy to obtain the blank of the target coil; After printing is completed, the blank is removed from the substrate of the 3D printing equipment, and after grinding, polishing and stress relief treatment, the target coil is obtained.
8. The molding method according to claim 7, characterized by The method for constructing the three-dimensional model of the target coil includes: A preliminary model of the target coil is constructed, the preliminary model including a coil body having a square flow channel; In the preliminary model, the upper surface of the flow channel constituting the target coil is surfaced, so that the cross-section of the flow channel forms a combination of an arc-shaped top and a rectangular bottom; In the preliminary model, the bottom of the target coil is offset and extended along the forming height direction and filled into a solid to form a solid thickened layer or support foot, and allowance is reserved for wire cutting processing.
9. The molding method according to claim 7, characterized by, The printing parameters of the 3D printing equipment are set as follows: The laser power is 500W-700W, the scanning speed is 600mm / s-1000mm / s, and the layer thickness is set to 55μm-65μm.
10. The molding method according to claim 7, wherein The partitioned scanning includes: dividing each layer of the three-dimensional model into multiple different printing areas, and setting a scanning direction rotation angle between each area; The contour offset strategy includes: first completing the closed scan of the outer contour of the target coil, then filling the inner area, and for the arc-shaped top area of the target coil, using a 5%-10% increase in laser power to perform dynamic energy compensation printing.