A method for wire feeding machining of shaped holes in the lower die of an extrusion die

By aligning the center coordinates of the locating pin hole in the CAD drawing and performing rotational correction, combined with the molybdenum wire cutting of the wire EDM machine, the problem that the wire EDM machine cannot directly cut the shaped hole was solved. This achieved precise positioning and rotational accuracy of the shaped hole and the locating pin hole, reduced processing costs, and improved mold assembly accuracy.

CN123103335APending Publication Date: 2026-11-17FUJIAN NANPING ALUMINUM
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611597525.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-15
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In the existing technology, wire EDM machines cannot directly align and cut the die hole according to the rotation angle based on the positioning pin hole on the lower die. This makes it difficult to guarantee the relative positional accuracy of the die hole, positioning pin hole, and mating stop, and the processing cost is relatively high.

Method used

The method of machining the lower model hole using a medium-speed wire EDM machine involves aligning the center coordinates of the locating pin hole in the CAD drawing, calculating the rotation angle and correcting the rotation, and combining this with molybdenum wire cutting to ensure the relative positional accuracy of the model hole and the locating pin hole. Finally, the mating stop and locating pin hole are precision machined in one setup on a machining center.

Benefits of technology

The relative positional accuracy of the die hole, locating pin hole, and mating stop reached ±0.01mm, which reduced processing costs, improved processing efficiency, and ensured the accuracy of mold assembly.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123103335A_ABST
    Figure CN123103335A_ABST
Patent Text Reader

Abstract

A method for machining a shaped hole in the lower die of an extrusion die using wire cutting, providing a lower die with a mating stop, two locating pin holes, a process hole, and a shaped hole to be machined. The advantages of this invention are: it uses a medium-speed wire EDM machine to machine the lower die hole, aligns the two locating pin holes with a molybdenum wire, calculates the rotation angle in CAD and rotates the shaped hole graphic, positions it according to the process hole, and then loads the program for cutting, solving the problem of the lack of rotation angle cutting function on medium-speed wire EDM machines; the molybdenum wire can be reused, reducing the machining cost of large-size lower die holes; the relative positional tolerance between the machined shaped hole, locating pin holes, and mating stop can reach ±0.01mm, the wall thickness tolerance of the upper and lower die assembly is -0.04 to 0mm, and the dimensional deviation of the shaped hole is -0.04 to 0mm. Furthermore, it can be combined with electrical discharge machining (EDM) and slow wire EDM to ensure machining quality.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of mold processing technology, and specifically to a method for wire-feed machining of shaped holes in the lower die of an extrusion mold. Background Technology

[0002] In extrusion die processing, the lower die typically requires the machining of a shaped hole. In existing technology, this shaped hole is generally machined on a wire EDM machine. Wire EDM machines use copper wire for cutting, resulting in high machining accuracy and meeting the relative positional accuracy requirements between the shaped hole, locating pin holes, and mating stops. However, for large-sized lower dies, due to the thick die and large circumference of the shaped hole, the copper wire consumption during wire EDM is high, leading to higher processing costs.

[0003] Medium-speed wire EDM machines use molybdenum wire for cutting, which can be reused, resulting in lower processing costs and making them suitable for machining thick mold holes. However, medium-speed wire EDM machines lack the pin hole alignment calculation and rotation angle cutting functions found in slow-speed wire EDM machines. They cannot directly align and cut the mold hole according to the rotation angle based on the locating pin holes on the lower die. Therefore, when machining the lower die hole using a medium-speed wire EDM machine, it is difficult to guarantee the positional and rotational accuracy of the mold hole relative to the locating pin holes and mating stops, thus affecting the wall thickness accuracy of the upper and lower die assembly and the dimensional accuracy of the mold hole.

[0004] In existing technologies, the wall thickness tolerance of the upper and lower die assemblies is typically required to be -0.04 to 0 mm, the dimensional deviation of the die hole is required to be -0.04 to 0 mm, and the dimensional and positional tolerance of the mating stop and locating pin hole is required to be ±0.01 mm. When machining the lower die hole using a wire EDM machine, how to ensure the relative positional accuracy of the die hole, locating pin hole, and mating stop without a rotary angle cutting function, while simultaneously reducing machining costs, is a technical problem that needs to be solved in this field. Summary of the Invention

[0005] The purpose of this invention is to address the shortcomings and defects of the prior art by providing a method for wire feeding machining of shaped holes in the lower die of an extrusion die.

[0006] To achieve the above objectives, the present invention adopts the following technical solution: a method for machining a shaped hole in the lower die of an extrusion die using wire cutting, comprising the following steps: providing a lower die of an extrusion die, wherein the lower die is provided with a mating stop, two locating pin holes, a process hole, and a shaped hole to be machined; the mating stop and the two locating pin holes are precision machined in one clamping on a machining center to ensure the dimensional accuracy and relative positional accuracy of the mating stop and the locating pin holes; placing the lower die on the worktable of a wire cutting machine and clamping the lower die; using the molybdenum wire of the wire cutting machine to align the two locating pin holes respectively, and recording the center coordinate values ​​of the two locating pin holes; determining the rotation angle of the lower die relative to the theoretical position in a CAD drawing based on the center coordinate values ​​of the two locating pin holes, and performing rotation correction on the lower die shaped hole pattern accordingly; determining the relative positional dimensions between the process hole and the locating pin holes in the CAD drawing, and moving the molybdenum wire to the actual position of the process hole according to the relative positional dimensions; loading the shaped hole pattern program after the rotation correction in the above steps, and controlling the wire cutting machine to cut the lower die along the shaped hole pattern to obtain the lower die shaped hole.

[0007] Furthermore, the manufacturing process of the lower mold includes: blanking → rough turning → die marking → CNC milling → drilling top holes → heat treatment → precision turning → grinding → finishing; wherein, finishing includes finishing the positioning stop, positioning pin holes and welding chamber.

[0008] Furthermore, in the finishing process, the stop and locating pin holes are machined in one go on a machining center, with dimensional and positional tolerances of ±0.01mm.

[0009] Furthermore, the lower die is placed on the worktable of the wire EDM machine, without requiring the lower die to be in the same position as the theoretical coordinates of the machine tool, and then clamped.

[0010] Furthermore, based on the actual center coordinates of the two locating pin holes, the rotation angle of the mold is calculated in the CAD drawing, and the mold hole pattern is rotated.

[0011] Furthermore, the relative position dimensions between the process hole and the locating pin hole are marked in the CAD drawing, and the cutting molybdenum wire is moved to the actual position of the process hole according to the relative position dimensions.

[0012] Furthermore, the method also includes: performing electrical discharge machining on the lower die to process the exit working strip or the empty cutter.

[0013] Furthermore, after the electrical discharge machining (EDM) is performed, a slow wire EDM is used to precisely cut the hole.

[0014] Furthermore, the wire EDM machine uses molybdenum wire for cutting, and the molybdenum wire is reused. This method is suitable for large-size lower dies, using a wire EDM machine for hole cutting to reduce processing costs.

[0015] Furthermore, the relative positional and rotational accuracy of the machined hole and the relative positional tolerance of the positioning pin hole and the mating stop are ±0.01mm; the wall thickness tolerance of the upper and lower mold assembly is -0.04 to 0mm, and the hole size deviation is -0.04 to 0mm.

[0016] After adopting the above technical solution, the beneficial effects of the present invention include at least the following: 1. Reduce processing costs: Use a medium-speed wire EDM machine instead of a slow-speed wire EDM machine for cutting the lower die hole. The medium-speed wire EDM machine uses molybdenum wire, which can be reused. It is especially suitable for large-size and thick lower dies, effectively reducing copper wire consumption and processing costs.

[0017] 2. Solving the problem of the lack of rotation angle cutting function in medium-speed wire EDM machines: By aligning the two positioning pin holes with molybdenum wire and recording the center coordinates, the actual rotation angle of the lower die is calculated in the CAD drawing, and the hole pattern is rotated and corrected. Thus, the hole can be cut according to the actual rotation angle on the medium-speed wire EDM machine, making up for the lack of rotation angle cutting function in medium-speed wire EDM machines.

[0018] 3. Ensure the positional and rotational accuracy of the hole: By determining the relative positional dimensions between the process hole and the locating pin hole, the molybdenum wire is moved to the actual position of the process hole, and then the hole pattern program after rotation correction is loaded for cutting, so that the positional and rotational accuracy of the machined hole and the relative positional tolerance of the locating pin hole and the mating stop reach ±0.01mm.

[0019] 4. Ensure mold assembly accuracy: The lower mold mating stop and locating pin hole are precision machined in one clamping on the machining center, ensuring their dimensional accuracy and relative positional accuracy; combined with the alignment and rotation compensation method of the wire EDM hole, the wall thickness tolerance of the upper and lower mold assembly is controlled within -0.04 to 0 mm, and the hole size deviation is controlled within -0.04 to 0 mm.

[0020] 5. Improved processing efficiency: The actual position of the mold on the machine tool is restored online using CAD software. The mold hole is directly processed on the wire EDM machine according to the CAD dimensions and angles. The operation is simple, the processing accuracy meets the drawing requirements, and the processing efficiency is improved.

[0021] 6. Flexible process combination: For thick mold holes, a combination process can be adopted, which includes wire EDM, electrical discharge machining, and final wire EDM for precision cutting. This ensures the quality of mold processing while further saving processing costs. Attached Figure Description

[0022] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0023] Figure 1 This is a schematic diagram of the lower mold in this invention.

[0024] Figure 2 This is a cross-sectional view of the lower mold in this invention.

[0025] Figure 3 This is a schematic diagram of the position of the mold on the wire EDM machine in this invention. Detailed Implementation

[0026] The following is combined Figures 1-3 The following examples further illustrate the present invention. These examples are for illustrative purposes only and are not intended to limit the scope of protection of the present invention. Example 1

[0027] This embodiment provides a method for machining a shaped hole in the lower die of an extrusion die using wire cutting, including lower die manufacturing, wire cutting of the shaped hole, and subsequent processing.

[0028] I. Lower mold manufacturing The manufacturing process of the lower mold is as follows: Material cutting → rough turning → pattern marking → CNC milling → drilling top hole → heat treatment → finish turning → grinding → finishing → wire cutting → electrical discharge machining → wire cutting → polishing → fitter work.

[0029] Specifically: 1. Blanking: Cutting the billet; 2. Rough turning: Turning the outer diameter, mating stop, and welding chamber; 3. Mark the mold number: Mark the mold number; 4. CNC milling: Milling the material outlet, welding chamber, process holes, screw holes, and locating pin holes; 5. Drill the top hole; 6. Heat treatment: Quenching + Tempering; 7. Finish turning: Finish turning the mating end face; 8. Grinding: Grinding end faces; 9. Finishing: Finish machining of the locating stop, locating pin hole, and welding chamber; 10. Wire EDM machining: Medium-speed wire EDM is used to machine the holes, and alignment is performed according to the positioning pin holes; 11. Electrical Discharge Machining: Machining the exit working zone or empty tool; 12. Wire EDM machining: precision cutting of die-shaped holes, specifically the method for wire EDM cutting of die-shaped holes: 1) The die is placed randomly on the wire EDM worktable and clamped. 2) Cut the copper wire to align the two positioning pin holes and obtain the mold rotation angle; 3) Set the rotation angle and move the copper wire to the process hole according to the process hole coordinates on the drawing; 4) Adjust the hole program and cut according to the rotation angle.

[0030] 13. Polishing; 14. Fitter.

[0031] In order to ensure the accuracy of the wall thickness fit of the mold assembly, the mating stop and positioning pin hole of the lower mold are precision machined in the finishing process of the lower mold. The mating stop and positioning pin hole are clamped and machined in one go on the machining center to ensure the dimensional accuracy and relative position accuracy of the mating stop and positioning pin hole. The dimensional and position tolerances are ±0.01mm.

[0032] II. Medium wire EDM machining of lower mold holes Reference Figure 1 and Figure 2 The lower die has a mating stop, two locating pin holes, a process hole, and a die hole to be machined. The method for machining the die hole on a medium-speed wire EDM machine is as follows: S1. Provide a lower die for extrusion, which has a mating stop, two locating pin holes, a process hole, and a shaped hole to be machined. The mating stop and the two locating pin holes are precision machined in one clamping on a machining center to ensure the dimensional accuracy and relative positional accuracy of the mating stop and the locating pin holes. S2. Place the lower die on the worktable of the wire EDM machine and clamp it. In this embodiment, the lower die can be placed arbitrarily on the wire EDM worktable, and it is not required that the lower die be consistent with the theoretical coordinate position of the machine tool. S3. Use the molybdenum wire of the wire EDM machine to align the two positioning pin holes respectively, and record the center coordinate values ​​of the two positioning pin holes; specifically, use the cutting molybdenum wire to align one positioning pin hole and record the center coordinate value of the pin hole; then align the other positioning pin hole and record the center coordinate value of the pin hole. S4. Based on the center coordinates of the two locating pin holes, determine the rotation angle of the lower mold relative to the theoretical position in the CAD drawing, and correct the rotation of the lower mold hole pattern accordingly; specifically, based on the center coordinates of the two pin holes, calculate the mold rotation angle in the CAD drawing and rotate the mold hole. S5. Determine the relative position dimensions between the process hole and the locating pin hole in the CAD drawing, and move the molybdenum wire to the actual position of the process hole according to the relative position dimensions; specifically, mark the relative position dimensions between the process hole and the locating pin hole in the CAD drawing, and move the cutting molybdenum wire to the actual position of the process hole according to the relative position dimensions. S6. Load the hole pattern program after rotation correction in step S4, and control the wire feed machine to cut the lower die along the hole pattern to obtain the lower die hole; specifically, load the rotating die hole pattern program to cut the die.

[0033] Through the above process, the positional and rotational accuracy of the die hole and the relative positional accuracy of the locating pin hole and the mating stop are guaranteed, with dimensional and positional tolerances of ±0.01mm.

[0034] The wall thickness tolerance of the upper and lower mold assembly is -0.04 to 0 mm; the deviation of the hole size is -0.04 to 0 mm.

[0035] III. Subsequent Processing After wire EDM cutting the shaped hole, the lower die is subjected to EDM to machine the exit working zone or empty cut. After EDM empty cut, a slow wire EDM is used to precision cut the shaped hole to further ensure the quality of die machining. Example 2

[0036] For large-sized lower dies, the cost of slow wire EDM is high due to the relatively thick hole thickness. To reduce the processing cost of copper wire, a medium-speed wire EDM machine is used. Because medium-speed wire EDM uses molybdenum wire, it can be reused, resulting in lower processing costs.

[0037] The process is as follows: 1. Hole cutting is performed using a medium-speed wire EDM machine; 2. Since the wire EDM machine does not have the functions of pin hole alignment calculation and rotation angle cutting, the following process is adopted to ensure the positional accuracy and rotational accuracy of the die hole and the relative positional accuracy of the positioning pin hole and mating stop. The dimensional and positional tolerances are ±0.01mm.

[0038] Method for cutting die holes using wire cutting: 1. The die is placed randomly on the wire EDM worktable and clamped. 2. Use a cutting molybdenum wire to align one locating pin hole and record the center coordinates of the pin hole. Then align the other locating pin hole and record the center coordinates of the pin hole. 3. Based on the center coordinates of the two pin holes, calculate the mold rotation angle on the CAD drawing and rotate the mold hole accordingly; 4. Mark the relative dimensions of the process holes and locating pin holes on the CAD drawings; 5. Based on the relative position dimensions of the process hole and the locating pin hole, move the cutting molybdenum wire to the actual position of the process hole; 6. Load the rotating mold hole graphic program to cut the mold.

[0039] In a further preferred embodiment, in order to ensure machining accuracy and reduce machining costs, for thick mold holes, a medium wire EDM method is first used, followed by electrical discharge machining of the blank, and finally a slow wire EDM precision cutting process is used, thereby ensuring the quality of mold machining and saving machining costs. Example 3

[0040] This embodiment provides a manufacturing process for the upper mold, the specific process of which is as follows: Material cutting → rough turning → pattern marking → CNC milling → polishing → tapping → heat treatment → finish machining → EDM → polishing → fitter work.

[0041] Specifically: 1. Blanking: Cutting the billet; 2. Rough turning: Turning the outer diameter and fitting the stop; 3. Mark the mold number: Mark the mold number; 4. CNC milling: Machining tongue cores and flow dividers; 5. Polishing: Grinding the diversion holes; 6. Tapping: Tapping locking teeth; 7. Heat treatment: Quenching + Tempering; 8. Finishing: Finish machining the tongue core working strip, mating cross-section, locating pin hole, and locating stop; 9. Electrical spark: Electrically striking the tongue core; 10. Polishing; 11. Fitter.

[0042] In the finishing process, the mating stop, locating pin hole and tongue core of the upper mold are finished in one operation on the machining center, which ensures the dimensional accuracy and relative positional accuracy of the mating stop, locating pin hole and tongue core, with a dimensional and positional tolerance of ±0.01mm.

[0043] The above are merely preferred embodiments of the present invention and are not intended to limit the scope of protection of the present invention. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.

[0044] The above is only used to illustrate the technical solution of the present invention and is not intended to limit it. Any other modifications or equivalent substitutions made by those skilled in the art to the technical solution of the present invention, as long as they do not depart from the spirit and scope of the technical solution of the present invention, should be covered within the scope of the claims of the present invention.

Claims

1. A method for machining a shaped hole in the lower die of an extrusion die, characterized in that: Includes the following steps: S1. Provide a lower die for extrusion, wherein the lower die is provided with a mating stop, two locating pin holes, a process hole and a shaped hole to be machined; the mating stop and the two locating pin holes are precision machined in one clamping on a machining center to ensure the dimensional accuracy and relative positional accuracy of the mating stop and the locating pin holes. S2. Place the lower die on the worktable of the wire EDM machine and clamp the lower die; S3. Use the molybdenum wire of the medium-speed wire EDM machine to align the two positioning pin holes respectively, and record the center coordinate values ​​of the two positioning pin holes; S4. Based on the center coordinates of the two locating pin holes, determine the rotation angle of the lower mold relative to the theoretical position in the CAD drawing, and make rotation corrections to the lower mold hole pattern accordingly. S5. Determine the relative position dimensions between the process hole and the locating pin hole in the CAD drawing, and move the molybdenum wire to the actual position of the process hole according to the relative position dimensions. S6. Load the hole pattern program after rotation correction in step S4, and control the wire feed machine to cut the lower die along the hole pattern to obtain the lower die hole.

2. The method for machining a shaped hole in the lower die of an extrusion die according to claim 1, characterized in that: The manufacturing process of the lower mold in step S1 includes: blanking → rough turning → mold numbering → CNC milling → drilling top hole → heat treatment → finish turning → grinding → finishing; wherein, finishing includes finishing the positioning stop, positioning pin hole and welding chamber.

3. The method for machining a shaped hole in the lower die of an extrusion die according to claim 2, characterized in that: During the finishing process, the stop and locating pin holes are machined in one go on a machining center machine tool, with dimensional and positional tolerances of ±0.01mm.

4. The method for machining a shaped hole in the lower die of an extrusion die according to claim 1, characterized in that: In step S2, the lower die is placed on the worktable of the wire EDM machine. It is not required that the lower die be aligned with the theoretical coordinate position of the machine tool, and then it is clamped.

5. The method for machining a shaped hole in the lower die of an extrusion die according to claim 1, characterized in that: In step S4, the rotation angle of the mold is calculated in the CAD drawing based on the actual center coordinates of the two locating pin holes, and the mold hole pattern is rotated.

6. The method for machining a shaped hole in the lower die of an extrusion die according to claim 1, characterized in that: In step S5, the relative position dimensions between the process hole and the locating pin hole are marked on the CAD drawing, and the cutting molybdenum wire is moved to the actual position of the process hole according to the relative position dimensions.

7. A method for machining a shaped hole in the lower die of an extrusion die according to claim 1, characterized in that: The step S6 is followed by: performing electrical discharge machining on the lower die to process the exit working strip or the empty cutter.

8. A method for machining a shaped hole in the lower die of an extrusion die according to claim 1, characterized in that: After the electrical discharge machining (EDM) is performed with a blank tool, a slow wire EDM is used to precisely cut the hole.

9. A method for machining a shaped hole in the lower die of an extrusion die according to claim 1, characterized in that: The described wire EDM machine uses molybdenum wire for cutting, and the molybdenum wire can be reused repeatedly. This method is suitable for large-size lower dies, using a wire EDM machine for hole cutting to reduce processing costs.

10. A method for machining a shaped hole in the lower die of an extrusion die according to claim 1, characterized in that: The relative positional and rotational accuracy of the machined hole and the relative positional tolerance of the positioning pin hole and the mating stop are ±0.01mm; the wall thickness tolerance of the upper and lower mold assembly is -0.04 to 0mm, and the hole size deviation is -0.04 to 0mm.