A molding process for bio-based composite automotive interior parts
By constructing a piecewise linear function and analyzing competitive factors in real time, the problem of real-time identification and adjustment of damage state during the injection filling process of bio-based composite materials was solved, enabling efficient molding of automotive interior parts and ensuring product consistency and production efficiency.
Patent Information
- Application Number
- CN202611553159.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-09
- Publication Date
- 2026-11-17
AI Technical Summary
Existing technologies make it difficult to determine the timing of process adjustments in a timely manner based on the damage status of different areas during the injection filling process of bio-based composite materials. This results in a delayed adjustment response, making it easy to miss effective adjustment opportunities and increase production debugging time.
A piecewise polygonal function is constructed to represent the changes in interfacial debonding resistance, fiber fracture resistance, and melt flow resistance with temperature. Combined with the regional segmented injection speed curve, the driving forces of fiber fracture and interfacial debonding are analyzed in real time. The competition factor and effective window period are calculated. Real-time monitoring and regulation of damage modes are achieved through feedforward control and adjustment of process parameters.
It enables real-time identification and differentiation control of damage states in various regions during the injection filling process of bio-based composite materials, avoiding adjustment response lag, ensuring the final performance requirements of automotive interior parts, and reducing adjustment lag and repeated diagnostic and debugging time.
Smart Images

Figure CN123103998A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of material injection molding technology, specifically a molding process for bio-based composite automotive interior parts. Background Technology
[0002] With the increasing demands for lightweighting and environmental protection in automobiles, bio-based composite materials are being used more and more widely in automotive interior parts. These materials typically use thermoplastic resins as the matrix and natural fibers as the reinforcing phase, and are manufactured into automotive interior parts with complex structures through injection molding.
[0003] However, during the injection filling process of bio-based composite materials, the natural fibers experience significantly different flow effects as the melt passes through different regions. Temperature also affects the interfacial bearing capacity between the natural fibers and the resin matrix, which may cause fiber breakage or interfacial debonding in different regions. Existing technologies typically adjust the damage state as a whole based on process parameters such as injection speed and molding temperature, making it difficult to differentiate and control the actual damage state of different regions. When local damage approaches the critical state, if the conventional diagnosis and adjustment method is still used, it is easy to miss the effective adjustment opportunity due to the lag in adjustment response. Moreover, after parameter adjustment, the damage state needs to be re-diagnosed, resulting in repeated adjustments and increased production debugging time. Existing technologies cannot determine the timing and method of process adjustment in a timely manner based on the damage evolution state of different regions during the injection filling process.
[0004] Therefore, the present invention provides a molding process for bio-based composite automotive interior parts. Summary of the Invention
[0005] In order to overcome the shortcomings of the prior art, at least one technical problem raised in the background art is solved.
[0006] The technical solution adopted by this invention to solve its technical problem is: a molding process for bio-based composite automotive interior parts, comprising the following steps:
[0007] Collect multiple sets of historical injection filling process parameters and corresponding batch material performance parameters, construct piecewise linear functions of interface anti-debonding ability with temperature, fiber breaking ability with temperature, melt flow resistance with temperature, and regional segmented injection speed curves as the basic relational library.
[0008] Real-time process parameters during the injection filling process of this batch are collected. Combined with the basic relational database, the fiber breakage driving amount and interface debonding driving amount of each region at the current moment are analyzed in real time to obtain the competition factor. At the same time, the effective window period of each region is calculated to determine whether the corresponding region belongs to the long window region or the short window region.
[0009] If it is a short window area, the target damage mode is set according to the final performance requirements of the automotive interior parts. The target damage mode is used as the feedforward control target to make the competing factors reach the target state and preserve the final performance requirements of the automotive interior parts. If it is a long window area, the competing factors are adjusted to enter the safe range according to the competing factors and the basic relation library.
[0010] Real-time monitoring of the evolution status of each region, and iterative updates of the basic relational database and historical database.
[0011] The beneficial effects of this invention are as follows:
[0012] By collecting real-time process parameters during the injection filling process of this batch and combining them with the basic relationship database, the fiber fracture driving amount and interface debonding driving amount of each region at the current moment are analyzed in real time. Then, the ratio of the interface debonding driving amount to the fiber fracture driving amount is calculated to obtain the competition factor, so that the competition relationship between interface debonding and fiber fracture can be distinguished. This allows for the differentiation of damage status in each region and the identification of the dominant damage mode. At the same time, it provides a basis for comparison in the selection of adjustment direction, providing a foundation for subsequent real-time zone control.
[0013] By calculating the effective window period of each region, it is determined whether the corresponding region belongs to the long window region or the short window region. The effective window period is obtained by calculating the rate of change and margin of the competitive factor. This allows the remaining adjustable stroke of each region to be quantified and predicted in advance, so that the timing of process adjustment can be determined in a timely manner during the injection filling process. At the same time, the adjustment method can be distinguished and selected according to the long window region or the short window region, avoiding missing the effective adjustment opportunity due to the lag in adjustment response.
[0014] In the process of injection filling damage control based on competition factors and effective window period, the dominant relationship between interface debonding and fiber breakage represented by competition factors and the remaining adjustable stroke of the region represented by the effective window period are jointly judged. Through the joint decision of damage control timing and adjustment direction, the effect of actively selecting the target damage mode according to the final performance requirements of automotive interior parts in the short window area and suppressing the dominant damage and intervening in another type of damage in the long window area is achieved. At the same time, the process adjustment is transformed from remediation after damage occurs to prediction before damage occurs, reducing adjustment lag and repeated diagnosis and debugging. Attached Figure Description
[0015] The invention will now be further described with reference to the accompanying drawings.
[0016] Figure 1 This is a flowchart of the steps in an embodiment of the present invention;
[0017] Figure 2 This is a step logic judgment diagram of an embodiment of the present invention;
[0018] Figure 3This is a flowchart of step S30 in an embodiment of the present invention. Detailed Implementation
[0019] To make the technical means, creative features, objectives and effects of this invention easier to understand, the invention will be further described below in conjunction with specific embodiments.
[0020] Example
[0021] Please see Figures 1-3 As shown in the embodiment of the present invention, a molding process for a bio-based composite automotive interior part includes the following steps:
[0022] Step S10: Collect multiple sets of historical injection filling process parameters, construct piecewise linear functions of interface anti-debonding ability with temperature, fiber breakage resistance with temperature, melt flow resistance with temperature, and regional segmented injection speed curves as the basic relational library.
[0023] The specific process of step S10 is as follows:
[0024] Collect process parameters for injection filling from multiple historical batches from the historical database, as well as the corresponding material performance parameters for each batch;
[0025] Ideally, sixty sets of historical batch data should be collected to reduce the risk of misjudgment. If there are fewer than sixty sets of historical batch data, the number of temperature ranges or the number of batches in each temperature range can be reduced accordingly. However, the number of batches in each temperature range should not be less than three sets to ensure that there are still sufficient statistical samples after removing the maximum and minimum values.
[0026] The process parameters include melt temperature, mold temperature, injection speed, and screw position, while the material performance parameters include interfacial debonding resistance, fiber breakage resistance, melt flow resistance, and fiber length.
[0027] The interface resistance to debonding can be determined by the single fiber pull-out method or the micro-debonding method; the fiber resistance to breakage can be determined by the single fiber tensile method; the melt flow resistance can be determined by the capillary rheometer or the rotational rheometer; and the fiber length can be determined by the fiber length distribution test method.
[0028] Interfacial debonding resistance: characterizes the ultimate load-bearing capacity of the interface between natural fibers and resin matrix against mutual peeling and separation; Fiber fracture resistance: characterizes the ultimate load-bearing capacity of natural fibers against fracture.
[0029] For any historical batch, calculate the arithmetic mean of the melt temperature at all times to obtain the average melt temperature, calculate the arithmetic mean of all mold temperatures to obtain the average mold temperature, and then calculate the arithmetic mean of the average melt temperature and the average mold temperature to obtain the interface temperature corresponding to the batch.
[0030] For all historical batches, sort them from low to high interface temperature, and divide all batches into six temperature ranges, with each temperature range containing ten historical batches.
[0031] For any temperature range, the interfacial anti-debonding ability of all historical batches is sorted in ascending order of numerical value. The maximum and minimum values are removed, and the arithmetic mean of the remaining interfacial anti-debonding ability is calculated as the representative value of interfacial anti-debonding ability.
[0032] Using the same method as the method for calculating the representative value of the interface anti-debonding ability, the representative values of the fiber breaking ability and melt flow resistance were calculated.
[0033] For any temperature range, the median value of the interface temperature of all historical batches is taken as the representative value of the interface temperature.
[0034] The representative values of interface temperature across all temperature ranges are mapped one-to-one with the representative values of interface anti-debonding ability.
[0035] Plotting the interface temperature as the abscissa and the corresponding interface anti-debonding ability as the ordinate in a two-dimensional coordinate system and connecting them with a straight line, we obtain a piecewise polygonal function of the interface anti-debonding ability changing with temperature.
[0036] Plotting the interface temperature as the abscissa and the corresponding fiber breaking strength as the ordinate in a two-dimensional coordinate system and connecting them with a straight line, we obtain a piecewise polygonal function of fiber breaking strength as a function of temperature.
[0037] Plotting the interface temperature as the abscissa and the corresponding melt flow resistance as the ordinate in a two-dimensional coordinate system and connecting them with a straight line, we obtain a piecewise polygonal function of melt flow resistance as a function of temperature.
[0038] The specific process for constructing the regional segmented injection velocity curve is as follows:
[0039] The interior of the mold is divided into three zones: a high-tension zone, a weak-bonding zone, and a normal zone.
[0040] Among them, the high tensile zone includes at least the gate, variable cross-section, thin wall, converging flow channel and near sharp corners; the weak bonding zone includes at least the weld line, around the insert, flow end and rib root; and the ordinary zone includes at least the straight flow channel, flow middle section and large cross-section area.
[0041] The classification is based on the following criteria: Gates, areas with varying cross-sections, thin walls, converging channels, and sharp corners cause localized acceleration, convergence, directional changes, and strong shearing or stretching of the melt, making fibers prone to breakage due to concentrated loads; these areas are classified as high-strength zones. Weld lines, areas around inserts, flow ends, and rib roots cause melt convergence, flow around, stagnation, or insufficient pressure transmission, weakening interfacial bonding; these areas are classified as weak-bonding zones. Straight channels, the middle section of the flow, and large cross-section areas have continuous and stable flow, gentle cross-sectional changes, and relatively uniform shearing and stretching effects, making fiber breakage and interfacial debonding less likely to dominate; these areas are classified as ordinary zones.
[0042] Historical batches that meet the performance acceptance criteria for automotive interior parts are selected as qualified batches.
[0043] Among them, the performance acceptance index of automotive interior parts refers to the process where, after the interior parts are formed, the inspectors take samples and conduct quality tests based on industry standards. If the samples meet the requirements, they are considered qualified, and the batch represented by the samples is considered a qualified batch.
[0044] For each region, determine the corresponding screw position region, extract all injection speed values within the screw position region from the qualified batch, and take the arithmetic mean as the speed segment value corresponding to the region;
[0045] Connect the speed segment values corresponding to the high tensile zone, weak bonding zone and normal zone to obtain the regional segmented injection speed curve;
[0046] The piecewise polygonal functions of interface anti-debonding ability with temperature, fiber breaking ability with temperature, melt flow resistance with temperature, and regional segmented injection speed curves are stored in the basic relational database.
[0047] Step S20: Collect real-time process parameters during the injection filling process of this batch, combine them with the basic relationship database, analyze the fiber breakage driving amount and interface debonding driving amount of each region at the current moment, obtain the competition factor, and calculate the effective window period of each region to determine whether the corresponding region belongs to the long window region or the short window region.
[0048] The specific process of step S20 is as follows:
[0049] Collect the current melt temperature, current mold temperature, current injection speed, and current screw position at the current moment during the injection filling process of this batch;
[0050] The current screw position is used to record the corresponding change of the current injection speed of this batch with the current screw position, and is stored in the historical database for subsequent updates of the regional segmented injection speed curve;
[0051] For any region, calculate the current interface temperature based on the current melt temperature and the current mold temperature;
[0052] Based on the piecewise linear function of interface anti-debonding ability as a function of temperature: the process of solving for the current interface anti-debonding ability at the current interface temperature is as follows:
[0053] Determine the range of representative values of adjacent interface temperatures where the current interface temperature is located. Divide the difference between the current interface temperature and the lower representative value of the adjacent temperature range by the difference between the higher and lower representative values of the adjacent temperature range to obtain the interface interpolation ratio.
[0054] If the current interface temperature is lower than the representative value of the lowest interface temperature or higher than the representative value of the highest interface temperature, then the closest boundary temperature range is used for linear extrapolation (i.e., the slope of the broken line closest to the boundary is used to extend outward to calculate the current interface anti-debonding ability, current fiber anti-breakage ability and current melt flow resistance corresponding to the current interface temperature).
[0055] When calculating the current interface anti-debonding capacity, add the interface anti-debonding capacity representative value corresponding to the lower interface temperature representative value, and multiply the interface interpolation ratio by the difference between the interface anti-debonding capacity representative values corresponding to the higher and lower interface temperatures to obtain the current interface anti-debonding capacity.
[0056] An example of calculating the interface's resistance to debonding is as follows:
[0057] Assuming the representative values of adjacent interface temperatures are 180℃ (lower interface temperature) and 190℃ (higher interface temperature), the representative value of the interface anti-debonding ability corresponding to the lower interface temperature is 2.0 MPa, and the representative value of the interface anti-debonding ability corresponding to the higher interface temperature is 2.2 MPa, and the interface temperature is 185℃, then the formula for calculating the interface anti-debonding ability F at the interface temperature is as follows:
[0058] =2.1MPa;
[0059] To calculate the current fiber breaking capacity, first obtain the fiber interpolation ratio using the same method as calculating the interface interpolation ratio. Then, add the fiber breaking capacity representative value corresponding to the lower interface temperature representative value, and multiply the fiber interpolation ratio by the difference between the fiber breaking capacity representative values corresponding to the higher and lower interface temperatures to obtain the current fiber breaking capacity.
[0060] To calculate the current melt flow resistance, first obtain the melt interpolation ratio using the same method as calculating the interface interpolation ratio. Then, add the melt flow resistance representative value corresponding to the lower interface temperature representative value, and multiply the melt interpolation ratio by the difference between the melt flow resistance representative values corresponding to the higher and lower interface temperatures to obtain the current melt flow resistance.
[0061] For any region, the local shear rate is obtained by dividing the current injection rate by the region's flow channel thickness.
[0062] The thickness of the flow channel in the region is read from the mold geometry parameters;
[0063] Multiply the current melt flow resistance by the local shear rate to obtain the local shear force, and then divide the local shear force by the current interface anti-debonding capacity to obtain the interface debonding driving amount corresponding to the region.
[0064] It should be noted that the interface debonding driving force represents the ratio of the actual shear load generated by the melt flow on the interface between the natural fiber and the resin matrix at the current interface temperature and local shear rate to the current interface debonding resistance. The larger the ratio, the closer the shear force on the interface is to or exceeds the current interface debonding resistance, and the higher the risk of interface debonding. The smaller the ratio, the larger the interface bearing capacity, and the lower the risk of debonding.
[0065] Multiply the current fiber breaking strength by the fiber diameter, and then divide by twice the current interfacial debonding strength to obtain the critical fiber length.
[0066] The fiber diameter is derived from the quality inspection report provided by the material supplier.
[0067] The reason for using twice the current interface anti-debonding capacity as the denominator is: based on the symmetrical relationship that the interface anti-debonding capacity acts from both ends of the fiber to the middle of the fiber at the same time, that is, the interface anti-debonding capacity acts once at each end of the fiber. Therefore, twice the current interface anti-debonding capacity is used to characterize the total load-bearing capacity of the interfaces at both ends of the fiber to jointly resist debonding.
[0068] Extract the fiber length of all historical batches, divide each region into three corresponding groups, calculate the arithmetic mean of the corresponding groups after removing the maximum and minimum values, and obtain the representative fiber length value of the region.
[0069] Divide the representative value of the fiber length corresponding to the region by the critical fiber length to obtain the fiber breakage driving force corresponding to the region.
[0070] Among them, the fiber breakage driving amount represents the ratio of the representative value of the fiber length in the region to the critical fiber length under the current interface temperature and local shear rate. The larger the ratio, the closer the fiber length is to or exceeds the critical fiber length, and the higher the risk of fiber breakage. The smaller the ratio, the larger the fiber length margin and the lower the risk of breakage.
[0071] For any region, divide the interface debonding driving amount by the fiber fracture driving amount to obtain the competition factor corresponding to the region at the current time.
[0072] Among them, the role of the competition factor is: not only to participate in the calculation of the effective window period, but also to be used to determine the dominant damage mode in the corresponding region, providing a basis for the subsequent selection of adjustment strategies, and to a certain extent realizing the quantitative discrimination of the competitive relationship between interface debonding and fiber fracture;
[0073] Take the maximum value of all historical competition factors as the upper limit of the safe interval, and take the minimum value of all historical competition factors as the lower limit of the safe interval.
[0074] It should be noted that the historical competition factor is not a data collection parameter under the traditional method. Instead, it is calculated by backtracking all historical batch data in order to construct a safety range.
[0075] Compare the competition factor with the safe interval:
[0076] If the competition factor is greater than the upper limit of the safe interval, then the margin is equal to the competition factor minus the upper limit of the safe interval;
[0077] If the competition factor is less than the lower limit of the safe interval, then the margin is equal to the lower limit of the safe interval minus the competition factor;
[0078] If the competition factor is within the safe range, the corresponding region is determined to be in a safe state, and no further adjustments are made; the region waits for the next collection cycle.
[0079] Subtract the previous competition factor from the competition factor to obtain the competition factor difference;
[0080] Among them, the competition factor is the competition factor of the region corresponding to the current time, and the competition factor of the previous time is the competition factor of the region corresponding to the previous time.
[0081] It should be noted that the previous moment refers to the time before one acquisition cycle, and the duration of one acquisition cycle is preferably 0.05 seconds. The reason is that since the speed response time of common injection molding machines is between 0.02 seconds and 0.05 seconds, and the sensor signal acquisition and processing lag time is between 0.01 seconds and 0.02 seconds, the acquisition response lag time is between 0.03 seconds and 0.07 seconds. The preferred value of 0.05 seconds takes into account both advance prediction and computational burden.
[0082] Divide the difference in competition factors by the duration of the acquisition period to obtain the rate of change of competition factors. Then divide the margin by the rate of change of competition factors to obtain the theoretical adjustable time corresponding to the region.
[0083] Multiply the theoretical adjustable time by the current injection speed to obtain the theoretical adjustable screw stroke;
[0084] Multiply the response lag time by the current injection speed to obtain the lag screw stroke;
[0085] Among them, the response lag time is: during the equipment debugging stage, it is obtained by adding the injection molding machine speed response time, sensor signal acquisition and processing lag time, valve gate opening and closing response time and melt pressure transmission lag time obtained by actual measurement;
[0086] Subtracting the lag screw stroke from the theoretical adjustable screw stroke yields the effective adjustable screw stroke, which is the effective window period.
[0087] In this embodiment, the effective adjustable screw stroke is referred to as the effective window period, and the physical quantity is the screw stroke (length), which represents the amount of adjustable screw stroke remaining from the current moment until the damage occurs;
[0088] If the effective window period is longer than the lag screw stroke, the corresponding area is determined to be a long window area;
[0089] If the effective window period is less than or equal to the lag screw stroke, the corresponding area is determined to be a short window area.
[0090] The purpose of calculating the effective window period is to: quantify the remaining adjustable hysteresis screw stroke in the corresponding region from the current moment to before the damage occurs, determine whether the adjustment is timely, avoid missing the best adjustment opportunity due to response lag, change the process adjustment from remediation after the damage occurs to prediction before the damage occurs, and determine the length of the effective window period so as to select different control strategies in subsequent steps based on the long or short window area.
[0091] Step S20 calculates the competition factors of each region in real time, and then calculates the effective window period based on the rate of change of the competition factors and the margin. This clarifies the degree of deviation of each region from the safe state at the current moment and the remaining adjustable stroke, thus optimizing the problems of difficulty in differentiating control for different regions, lag in adjustment response, and repeated diagnosis and debugging. It also provides a basis for subsequent steps to select different control strategies based on long or short window areas.
[0092] Step S30: If the corresponding area is a short window area, set the target damage mode according to the final performance requirements of the automotive interior parts, use the target damage mode as the feedforward control target, and adjust it to make the competing factors reach the target state to preserve the final performance requirements of the automotive interior parts. If the corresponding area is a long window area, adjust it according to the competing factors and the basic relation library to make the competing factors enter the safe range.
[0093] The specific process of step S30 is as follows:
[0094] If the corresponding region is determined to be a short window area, the target damage mode of the corresponding region is determined as follows:
[0095] The target damage mode in the high tensile zone is to protect fiber length and allow interface debonding first.
[0096] The target damage mode for the weakly bonded region is to protect the integrity of the interface while allowing for local fiber breakage.
[0097] The target damage mode in the general area is determined based on the final performance requirements of automotive interior components.
[0098] The significance of determining the target damage mode is that since interface debonding and fiber breakage may occur simultaneously or switch randomly, setting a target damage mode means that, under the premise that damage is unavoidable, we can actively select the damage that minimizes the damage to the final performance. The other type of damage will naturally be suppressed. When damage has not occurred, it is a competitive mechanism; once it has occurred, it will suppress the other type of damage.
[0099] For the high-stretch zone, subtract the speed segment value corresponding to the zone in the segmented injection speed curve from the current injection speed to obtain the high-zone speed difference;
[0100] Add half the absolute value of the high-zone speed difference to the current injection speed to obtain the new high-zone injection speed;
[0101] By using the principle of allowing the interface to debond first as the target damage mode, and controlling the high tensile zone with the injection speed in the new high zone, the local shear effect can be improved, so that the competition factor reaches the target state (i.e., the competition factor is greater than one), and the interface debonding driving amount reaches one, allowing the interface to debond first, thereby protecting the fiber from breakage.
[0102] It should be noted that the principle of protecting the fiber from breakage is that both interface debonding and fiber breakage require stress transmission through the interface. Once interface debonding occurs, the channel for stress transmission is cut off, the fiber cannot obtain sufficient load transmission, the fiber breakage driving force is suppressed and cannot continue to rise, thereby preserving the fiber length.
[0103] For weakly bound regions, the velocity difference is obtained by subtracting the velocity segment value corresponding to the region in the regional segmented injection velocity curve from the current injection velocity.
[0104] The new weak zone injection speed is obtained by subtracting the absolute value of half of the weak zone speed difference from the current injection speed.
[0105] By allowing local fiber breakage as the target damage mode and controlling the weak bonding area with the injection speed of the new weak area, the local shear force can be reduced, the competition factor can reach the target state (i.e., the competition factor is less than one), and the fiber breakage driving amount can reach one, so that the local fibers break first, thereby protecting the interface integrity and preventing debonding.
[0106] It should be noted that the principle of protecting the interface integrity and preventing debonding is as follows: both interface debonding and fiber breakage are related to the stress transmitted at the interface. After the fiber breaks first, the fiber changes from a long fiber to a short fiber. The stress concentration at the fiber end is released, and the fiber can no longer transmit high stress to the interface. The driving force of interface debonding is suppressed and cannot continue to rise, thereby preserving the integrity of the interface.
[0107] For the general area, read the final performance requirements of the automotive interior components:
[0108] If the final performance requirement of automotive interior parts is mainly stiffness, the target damage mode in the normal area is set to protect the fiber length, allowing the interface to debond first.
[0109] A calculation and adjustment method for the high tensile zone is adopted to protect fiber length;
[0110] If the final performance requirement of automotive interior parts is mainly surface quality, the target damage mode of the ordinary area should be set to protect the integrity of the interface, allowing local fiber breakage.
[0111] A calculation and adjustment method for the weak bonding region is adopted to protect the integrity of the interface;
[0112] If the final performance requirements for automotive interior parts include both rigidity and surface quality, then the filling process should be paused, a prompt message should be displayed, and manual intervention should be initiated.
[0113] It should be noted that the short window area only adjusts the current injection speed, because speed is a fast variable and the adjustment takes effect immediately;
[0114] For any region, if the corresponding region is determined to be a long window region, the regulatory direction is determined based on the competition factor to suppress damage:
[0115] If the competition factor is greater than the upper limit of the safe range, it means that the amount of interface debonding is too large relative to the amount of fiber breakage, and the tendency to debond is stronger than the tendency to breakage. At the same time, the interface debonding can be quickly suppressed by adjusting the current injection speed, and the fiber breakage can be intervened by using the current mold temperature.
[0116] The first injection rate was obtained by using the same method as calculating the injection rate of the new weak region in the weak binding region;
[0117] Extract the mold temperatures of all batches in the corresponding region from the historical database, calculate the arithmetic mean, and obtain the average mold temperature of the region.
[0118] The difference between the regional average mold temperature and the current mold temperature is taken as the absolute value of the mold temperature difference.
[0119] Add half of the mold temperature difference to the current mold temperature to obtain the new mold temperature;
[0120] By controlling the corresponding area with the first injection speed and the new mold temperature, the competition factor can be reduced and fall back into the safe range, while avoiding interface debonding and fiber breakage.
[0121] If the competition factor is less than the lower limit of the safe range, it means that the fiber fracture driving force is too large relative to the interface debonding driving force, and the fracture tendency is stronger than the debonding tendency. At the same time, the fiber fracture can be quickly suppressed by adjusting the current injection speed, and the interface debonding can be intervened by using the current melt temperature.
[0122] The second injection speed was obtained by using the same method as calculating the injection speed in the new high-tension zone in the high-tension zone;
[0123] Extract all batch melt temperatures of the corresponding region from the historical database, calculate the arithmetic mean, and obtain the regional average melt temperature;
[0124] The difference between the regional average melt temperature and the current melt temperature is taken as the absolute value of the melt temperature difference.
[0125] The new melt temperature is obtained by subtracting half of the melt temperature difference from the current melt temperature.
[0126] By controlling the corresponding area with a second injection speed and a new melt temperature, the competition factor can be improved and brought back into the safe range, while avoiding fiber breakage and interface debonding.
[0127] It should be noted that if the absolute value of the difference between the competition factor and one is less than the preset threshold (preferably 0.05, because 0.05 is a commonly used tolerance or significance level in engineering control and statistical judgment), it is considered that the degree of interface debonding and fiber breakage damage is equivalent. The dominant mode is easy to switch with process fluctuations and cannot be widened by bias adjustment. It is treated as the target damage mode of the short window area.
[0128] For long window areas, the competition factor of the corresponding area is recalculated after adjustment, provided that the effective window period of the corresponding area has not been exceeded. If the competition factor does not enter the safe range, the adjustment is repeated until the competition factor enters the safe range.
[0129] If the effective window period is shortened to less than or equal to the lag screw stroke during the adjustment process, the corresponding area will be converted to the target damage mode of the short window area.
[0130] Step S30, through the synergistic effect of the effective window period and the competitive factor, realizes the timing and direction decision of damage control during the injection filling process. The effective window period determines whether the region has sufficient adjustable stroke, thereby distinguishing between long and short window areas. The competitive factor determines the dominant relationship between interface debonding and fiber breakage, thereby determining the priority direction of damage suppression. This allows the short window area to actively select the target damage mode based on the final performance requirements of automotive interior parts, ensuring the final performance, even when the adjustment response is lagging and closed-loop correction is not possible. The long window area can suppress the dominant damage within the effective window period and intervene in another type of damage, causing the competitive factor to return to the safe range. This simultaneously avoids interface debonding and fiber breakage, effectively reducing adjustment lag and repeated debugging time, and improving the process robustness and product consistency of the bio-based composite automotive interior parts molding process.
[0131] Step S40: Monitor the evolution status of each region in real time, iteratively update the basic relational database, and realize the self-expansion and self-learning of the historical database and basic relational database with production batches;
[0132] The specific process of step S40 is as follows:
[0133] Store the current melt temperature, current mold temperature, current injection speed, and current screw position of this batch into the historical database;
[0134] For this batch of samples, the material performance parameters of this batch of samples were tested offline using the same testing method as the historical batches, including interfacial debonding ability, fiber breaking ability, melt flow resistance and fiber length, as new historical samples for this batch;
[0135] It should be noted that the current interface anti-debonding ability, current fiber anti-breakage ability, and current melt flow resistance in step S20 are real-time calculated values obtained by interpolation ratio calculation or linear extrapolation based on the current interface temperature and combined with the basic relation library. They are used for judgment and adjustment in the injection filling process of this batch and cannot replace the actual material performance parameters obtained by offline detection in this step.
[0136] Simultaneously, the competition factors corresponding to each region are also stored in the historical database. The reason for adding and storing the competition factors when updating the basic relational database and the historical database is that: before this, the competition factors were not directly collected historical process parameters, but were derived parameters calculated based on the real-time process parameters of this batch and the basic relational database after the basic relational database was built. However, during the injection filling process of this batch, the competition factors have been calculated in real time in step S20 and used for adjustment in step S30. Therefore, storing the competition factors in the historical database after the completion of this batch can update the construction data source of the upper and lower limits of the safety interval and provide a data basis for subsequent calculation of the effective window period.
[0137] Based on the historical database, the piecewise linear functions of interface anti-debonding ability with temperature, fiber breaking ability with temperature, melt flow resistance with temperature, and regional segmented injection speed curves are reconstructed to obtain an updated basic relational library, which is used for relevant calculations and adjustments for the next batch of injection filling.
[0138] The foregoing has shown and described the basic principles, main features, and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The embodiments and descriptions in the specification are merely illustrative of the principles of the invention. Various changes and modifications can be made to the invention without departing from its spirit and scope, and all such changes and modifications fall within the scope of the present invention as claimed. The scope of protection of the present invention is defined by the appended claims and their equivalents.
Claims
1. A molding process for bio-based composite automotive interior parts, characterized in that: Includes the following steps: Collect multiple sets of historical injection filling process parameters and corresponding batch material performance parameters, construct piecewise linear functions of interface anti-debonding ability with temperature, fiber breaking ability with temperature, melt flow resistance with temperature, and regional segmented injection speed curves as the basic relational library. Real-time process parameters during the injection filling process of this batch are collected. Combined with the basic relational database, the fiber breakage driving amount and interface debonding driving amount of each region at the current moment are analyzed in real time to obtain the competition factor. At the same time, the effective window period of each region is calculated to determine whether the corresponding region belongs to the long window region or the short window region. If it is a short window area, the target damage mode is set according to the final performance requirements of the automotive interior parts. The target damage mode is used as the feedforward control target to make the competing factors reach the target state and preserve the final performance requirements of the automotive interior parts. If it is a long window area, the competing factors are adjusted to enter the safe range according to the competing factors and the basic relation library. Real-time monitoring of the evolution status of each region, and iterative updates of the basic relational database and historical database.
2. The molding process for a bio-based composite automotive interior part according to claim 1, characterized in that: The process of constructing piecewise linear functions for the interfacial anti-debonding ability as a function of temperature, the fiber breaking strength as a function of temperature, and the melt flow resistance as a function of temperature is as follows: The arithmetic mean of the average melt temperature and the average mold temperature is used to obtain the interface temperature corresponding to the batch. All interface temperatures are then divided into temperature ranges. Extract the interfacial anti-debonding ability, fiber fracture resistance and melt flow resistance from all corresponding batches of material performance parameters; Arrange all interfaces with anti-debonding capabilities corresponding to the temperature range in ascending order, and take the arithmetic mean after removing the maximum and minimum values as the representative value of the interface anti-debonding capability. Using the same method as the method for calculating the representative value of the interface's anti-debonding ability, the representative values of the fiber's breaking ability and the melt flow resistance were calculated; In a two-dimensional coordinate system, with the interface temperature as the representative value on the horizontal axis and the corresponding interface anti-debonding ability as the representative value on the vertical axis, plotting points and connecting them yields a piecewise polygonal function of the interface anti-debonding ability changing with temperature. Using the same method as that used to obtain the piecewise broken line function of the interfacial anti-debonding ability as a function of temperature, we obtained the piecewise broken line function of the fiber breaking ability as a function of temperature and the piecewise broken line function of the melt flow resistance as a function of temperature.
3. The molding process for a bio-based composite automotive interior part according to claim 1, characterized in that: The specific process for constructing the regional segmented injection velocity curve is as follows: The mold interior is divided into three regions: high tension zone, weak bonding zone and normal zone. The corresponding screw position regions are determined. All injection speed values within the screw position regions are extracted from all qualified batches, and the arithmetic mean is taken as the speed segment value corresponding to the region. Connecting the corresponding velocity segments of the three regions yields the region-segmented injection velocity curve.
4. The molding process for a bio-based composite automotive interior part according to claim 1, characterized in that: The process of obtaining the competitive factor is as follows: The local shear rate is obtained by dividing the current injection rate by the thickness of the flow channel in the region. The current melt flow resistance is multiplied by the local shear rate and then divided by the current interface debonding capacity to obtain the interface debonding driving force. Multiply the current fiber breaking strength by the fiber diameter, and divide by twice the current interfacial debonding strength to obtain the critical fiber length; The fiber lengths of all historical batches are grouped by region. After removing the maximum and minimum values of each group, the arithmetic mean of each group is calculated to obtain the representative fiber length value of each group. Then, the fiber breakage driving force is obtained by dividing by the critical fiber length. The competition factor is the ratio of the interfacial debonding driving force to the fiber fracture driving force.
5. The molding process for a bio-based composite automotive interior part according to claim 4, characterized in that: The process for obtaining the current interface anti-debonding ability, current fiber breaking resistance, and current melt flow resistance is as follows: Determine the range of representative values of adjacent interface temperatures where the current interface temperature is located, and divide the difference between the current interface temperature and the smaller representative value of the adjacent interface temperature by the difference between the representative values of the adjacent interface temperatures to obtain the interface interpolation ratio. The current interface anti-debonding ability is obtained by adding the interpolation ratio to the interface anti-debonding ability representative value corresponding to the smaller adjacent interface temperature representative value and multiplying it by the difference between the interface anti-debonding ability representative values corresponding to the adjacent interface temperature representative values. According to the method for calculating the current interface anti-debonding ability, the fiber interpolation ratio is obtained, and then the representative value of interface anti-debonding ability in the method is replaced with the representative value of fiber breaking ability to calculate the current fiber breaking ability. Based on the method for calculating the current interface's anti-debonding ability, the melt interpolation ratio is obtained. Then, the representative value of the interface's anti-debonding ability in the method is replaced with the representative value of the melt flow resistance, and the current melt flow resistance is calculated.
6. The molding process for a bio-based composite automotive interior part according to claim 1, characterized in that: The process of calculating the effective window period is as follows: The rate of change of the competition factor is obtained by subtracting the competition factor from the previous moment and then dividing by the duration of the acquisition period. The margin is obtained by comparing the competition factor with the safety interval; Divide the margin by the rate of change of the competition factor, and then multiply by the current injection speed to obtain the theoretical adjustable screw stroke; Multiplying the response lag time by the current injection speed yields the lag screw stroke. The effective window period is obtained by subtracting the lag screw stroke from the theoretically adjustable screw stroke. If the effective window period is greater than the lag screw travel, it is a long window area; otherwise, it is a short window area.
7. The molding process for a bio-based composite automotive interior part according to claim 6, characterized in that: The process of comparing and calculating the competition factor and the safe interval is as follows: Take the maximum value of all historical competition factors as the upper limit of the safe interval, and take the minimum value of all historical competition factors as the lower limit of the safe interval. If the competition factor is greater than the upper limit of the safe interval, then the margin is the competition factor minus the upper limit of the safe interval; If the competition factor is less than the lower limit of the safe interval, the margin is the lower limit of the safe interval minus the competition factor.
8. The molding process for a bio-based composite automotive interior part according to claim 1, characterized in that: The adjustment process for a short window region is as follows: Determine the target damage pattern for the corresponding area; For the high tensile zone, increase the current injection speed to enhance local shearing action, bring the competition factor to the target state, and make the interface debonding driving amount reach one, thus protecting the fiber from breakage. For weakly bonded areas, reduce the current injection speed to reduce local shearing, so that the competition factor reaches the target state and the fiber fracture driving amount reaches one, thus protecting the interface from debonding. For the ordinary area, the adjustment method of high tension area or weak bonding area is adopted according to the final performance requirements of automotive interior parts.
9. The molding process for a bio-based composite automotive interior part according to claim 8, characterized in that: The process of determining the target damage mode in the corresponding area is as follows: The target damage mode in the high tensile zone is to protect fiber length and allow interface debonding first. The target damage mode for the weakly bonded region is to protect the integrity of the interface while allowing for local fiber breakage. The target damage mode in the general area is determined based on the final performance requirements of automotive interior components.
10. The molding process for a bio-based composite automotive interior part according to claim 1, characterized in that: The adjustment process for a long window area is as follows: If the competition factor is greater than the upper limit of the safe range, the current injection speed is reduced to quickly suppress interface debonding, while the current mold temperature is increased to intervene in fiber breakage. If the competition factor is less than the lower limit of the safe range, the current injection speed is increased to quickly suppress fiber breakage, while the current melt temperature is reduced to intervene in interface debonding. If the absolute value of the difference between the competition factor and one is less than the preset threshold, it means that the degree of interface debonding and fiber breakage damage is equivalent, and it is processed according to the short window area target damage mode.