A method of compression molding thermoplastic tubing

By generating a cross-sectional softening gradient to adjust the cavity gap of the forming die and the temperature of the temperature control zone, and by combining the geometric characteristics of the folded tube, the problem of the disconnect between the die gap and temperature regulation and the softening state of the tube was solved, thus achieving higher forming accuracy and winding quality.

CN123104032APending Publication Date: 2026-11-17新疆鼎立环境科技有限公司 +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611640459.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-22
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In the existing thermoplastic pipe pressing process, the mold gap and temperature adjustment are out of sync with the actual softening state of the pipe, resulting in inconsistent sidewall spacing and fold curvature of the folded pipe, which affects the molding accuracy and winding quality.

Method used

By acquiring the circumferential wall thickness data and axial temperature data of the pipe, a cross-sectional softening gradient is generated and mapped to the cavity clearance correction amount of the forming die and the temperature of the temperature control zone. The side wall spacing and fold curvature of the folded pipe are collected, and the traction tension and winding parameters are set to adapt the forming process to the actual state of the pipe.

Benefits of technology

It improves the cross-sectional accuracy and winding quality of the pressing and forming process, reduces local over-pressure and under-pressure, avoids the corners from being straightened due to excessive tension or slipping due to insufficient tension, and maintains the shape and winding quality of U-shaped or I-shaped folded pipes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123104032A_ABST
    Figure CN123104032A_ABST
Patent Text Reader

Abstract

The application discloses a thermoplastic pipe pressing forming method and belongs to the technical field of thermoplastic pipe pressing forming. The method comprises the following steps: obtaining the circumferential wall thickness data and axial temperature data of the pipe; generating a cross-section softening gradient according to the circumferential wall thickness data and the axial temperature data, mapping the cross-section softening gradient into a pressing die cavity gap correction amount; driving the pressing die servo die lip according to the pressing die cavity gap correction amount, and setting the temperature of the circumferential temperature control zone of the pressing die; pressing the U-shaped or H-shaped folded pipe in the pressing die, collecting the side wall spacing and the corner curvature of the folded pipe; and setting the traction tension, the winding pitch and the reciprocating stroke according to the side wall spacing and the corner curvature. According to the method, the die gap and the temperature control are adjusted according to the actual wall thickness and the temperature distribution of the pipe, and the traction and the winding parameters are set according to the geometric characteristics of the folded pipe, so that the pressing forming quality and the winding stability are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of thermoplastic pipe compression molding technology, specifically to a thermoplastic pipe compression molding method. Background Technology

[0002] In the compression molding process, thermoplastic pipes need to be heated to a softened state before being fed into a molding die to be pressed into U-shaped or I-shaped folded pipes. In existing compression molding methods, the cavity clearance of the molding die is usually set to a fixed value before processing, and the temperature of the circumferential temperature control zone is also mostly controlled according to a uniform target value. Affected by extrusion, storage, and heating conditions, the wall thickness of the pipe fluctuates along the circumference, and the axial temperature distribution also changes with heating time, conveying speed, and ambient temperature. A fixed cavity clearance and a uniform circumferential temperature cannot adapt to the uneven distribution of the actual wall thickness and temperature of the pipe. Areas with larger wall thickness or lower temperature are prone to local overpressure due to insufficient softening during molding, while areas with smaller wall thickness or higher temperature are prone to local underpressure due to excessively soft material. This results in inconsistent sidewall spacing and fold curvature along the length of the U-shaped or I-shaped folded pipe. After compression molding, the folded pipe needs to be tension-controlled, pitch-controlled, and reciprocatedly wound by a traction mechanism and a winding machine.

[0003] Currently, the traction tension, winding pitch, and reciprocating stroke are typically set by operators based on experience or adjusted solely according to the tube's linear speed, without utilizing the sidewall spacing and fold curvature of the folded tube after pressing in real time. When the cross-sectional geometry of the folded tube changes, a fixed traction tension can easily straighten the fold or cause the tube to slip. A mismatch between the winding pitch and the sidewall spacing can also cause compression of adjacent tubes within the reel, uneven winding surfaces, and accumulation at the reciprocating reversal points. These problems lead to a disconnect between the die clearance and temperature control during thermoplastic tube pressing and the actual softening state of the tube, and a disconnect between the traction and winding parameters after pressing and the geometric characteristics of the folded tube. Summary of the Invention

[0004] This invention provides a method for pressing and molding thermoplastic pipes. By acquiring circumferential wall thickness data and axial temperature data of the pipe, a cross-sectional softening gradient is generated and mapped to the cavity clearance correction amount of the pressing die. The servo lip of the pressing die is driven and the temperature of the circumferential temperature control zone of the pressing die is set. By collecting the side wall spacing and fold curvature of the pressed U-shaped or I-shaped folded pipe, the traction tension, winding pitch and reciprocating stroke are set to adapt the pressing process to the actual softening state of the pipe and the traction winding process to the geometric characteristics of the folded pipe, thereby improving the cross-sectional accuracy and winding quality of the pressing process.

[0005] To achieve the above objectives, the present invention provides the following technical solution: a method for pressing and molding thermoplastic pipes, comprising: Obtain the circumferential wall thickness data and axial temperature data of the pipe; A cross-sectional softening gradient is generated based on the circumferential wall thickness data and the axial temperature data of the pipe, and the cross-sectional softening gradient is mapped to the cavity clearance correction amount of the forming die. Drive the servo lip of the forming mold according to the cavity clearance correction amount, and set the temperature of the circumferential temperature control zone of the forming mold; U-shaped or I-shaped folded tubes are pressed in a forming mold, and the side wall spacing and folding angle curvature of the U-shaped or I-shaped folded tubes are collected. The traction tension, winding pitch, and reciprocating stroke are set according to the sidewall spacing and the angle curvature.

[0006] Preferably, the step of generating a cross-sectional softening gradient based on the circumferential wall thickness data and the axial temperature data of the pipe, and mapping the cross-sectional softening gradient to a correction amount for the cavity clearance of the forming die, includes: Divide the pipe into sectors along its circumference and collect the wall thickness value of each sector; The pipe is divided into temperature zones along its axial direction, and the temperature value of each zone is collected. The wall thickness value of each sector is paired with the temperature value of the corresponding temperature zone to generate the cross-sectional softening gradient; The cross-sectional softening gradient is added to the preset cavity clearance of the forming mold to obtain the cavity clearance correction amount of the forming mold.

[0007] Preferably, the step of driving the servo die lip of the forming mold according to the cavity clearance correction amount and setting the temperature of the circumferential temperature control zone of the forming mold includes: The cavity clearance correction amount of the forming die is converted into a displacement command for the servo die lip of the forming die; Drive the servo die lip of the forming mold according to the displacement command; The temperature of the circumferential temperature control zone of the forming mold is divided into multiple target values ​​according to the cross-sectional softening gradient; The actual displacement of the servo die lip of the forming die is collected, and the actual displacement and the displacement command are converted into the displacement command for the next cycle.

[0008] Preferably, the step of pressing U-shaped or I-shaped folded tubes in a forming mold and collecting the sidewall spacing and fold angle curvature of the U-shaped or I-shaped folded tubes includes: A laser rangefinder and a contour scanning sensor are installed at the exit of the forming mold; The sidewall spacing of the U-shaped or I-shaped folded tube is collected by the laser ranging sensor; The contour scanning sensor collects the set of bend contour points of the U-shaped or I-shaped folded pipe. The set of points representing the bend contour is paired with the sidewall spacing according to the pipe length to obtain the sidewall spacing and bend curvature.

[0009] Preferably, the step of setting the traction tension, winding pitch, and reciprocating stroke according to the sidewall spacing and the curvature of the bend angle includes: The winding pitch is determined according to the sidewall spacing, the traction tension is determined according to the bend curvature, and the reciprocating stroke is determined according to the winding pitch and the reel width. The traction tension is sent to the constant tension control device, and the winding pitch and the reciprocating stroke are sent to the winding machine.

[0010] Preferably, the step of pairing the wall thickness value of each sector with the temperature value of the corresponding temperature zone to generate the cross-sectional softening gradient includes: Obtain the wall thickness value of each sector in the circumferential direction of the pipe sector position, and obtain the temperature value of each temperature zone in the axial direction of the pipe temperature zone position; The sector position and the temperature zone position are combined to form cross-sectional position data; The wall thickness values ​​of adjacent sectors are paired with the temperature values ​​of the corresponding temperature zones based on the cross-sectional location data to obtain the cross-sectional softening gradient.

[0011] Preferably, the step of acquiring the actual displacement of the servo die lip of the forming die and converting the actual displacement and the displacement command into a displacement command for the next cycle includes: A displacement sensor is installed on the servo die lip of the forming mold, and the actual displacement is collected by the displacement sensor at a set period. The actual displacement is converted into the opening data of the servo die lip of the forming die; The opening data and the cavity clearance correction amount of the forming die are arranged in chronological order to generate the displacement command for the next cycle.

[0012] Preferably, the corner profile point set is paired with the sidewall spacing according to the pipe length to obtain the sidewall spacing and corner curvature, including: The set of points representing the bend contour is connected in the order of collection to form a bend contour polyline. Extract the included angle between adjacent line segments in the polygonal outline; Map the included angle to the curvature of the bend angle; The bend curvature and the sidewall spacing are written into the same data frame according to the length of the pipe to obtain the sidewall spacing and bend curvature.

[0013] Preferably, the winding pitch is determined according to the sidewall spacing, the traction tension is determined according to the bend curvature, and the reciprocating stroke is determined according to the winding pitch and the reel width, including: Multiply the sidewall spacing by the winding overlap coefficient to obtain the winding pitch; Multiplying the curvature of the bending angle by the tension transmission coefficient yields the traction tension; Divide the reel width by the winding pitch to obtain the number of revolutions per stroke, and set the reciprocating stroke according to the number of revolutions per stroke.

[0014] Preferably, the step of pairing the wall thickness values ​​of adjacent sectors with the temperature values ​​of the corresponding temperature zones according to the cross-sectional position data includes: using a linear interpolation method to continuously fit the wall thickness values ​​of adjacent sectors with the temperature values ​​of the corresponding temperature zones according to the circumferential angle and axial distance to obtain the cross-sectional softening gradient.

[0015] The technical effects and advantages provided by the present invention in the above technical solution are as follows: A cross-sectional softening gradient is generated based on the circumferential wall thickness and axial temperature data of the pipe. This gradient is then added to a preset cavity clearance to obtain the die cavity clearance correction amount, which is converted into a die servo lip displacement command. Simultaneously, the circumferential temperature control zone temperature of the die is set according to the cross-sectional softening gradient. Wall thickness values ​​are collected by dividing the pipe circumferentially into sectors and temperature values ​​are collected by dividing it axially into temperature zones. The wall thickness value of each sector is paired with the temperature value of the corresponding temperature zone, and a linear interpolation method is used to continuously fit the values ​​based on the circumferential angle and axial distance to obtain the cross-sectional softening gradient. The die cavity clearance is corrected circumferentially and axially according to the softening degree caused by the local wall thickness and temperature of the pipe. The circumferential temperature control zone temperature is set according to the cross-sectional softening gradient. After the tube enters the forming mold, areas with larger wall thickness or lower temperature receive suitable cavity space and heat input, while areas with smaller wall thickness or higher temperature avoid excessive cavity space or excessive heat input, reducing local overpressure and underpressure. The consistency of the side wall spacing and fold curvature of U-shaped or I-shaped folded tubes along the length direction is improved.

[0016] At the exit of the forming die, a laser rangefinder sensor collects the sidewall spacing of the U-shaped or I-shaped folded tube, and a contour scanning sensor collects the corner contour point set. The corner contour point set is connected in the collection order to form a corner contour polyline. The included angle between adjacent line segments is extracted and mapped to the corner curvature. The corner curvature and sidewall spacing are written into the same data frame according to the tube length. The winding pitch is obtained by multiplying the sidewall spacing by the winding overlap coefficient, and the traction tension is obtained by multiplying the corner curvature by the tension transmission coefficient. The number of turns per stroke is obtained by dividing the reel width by the winding pitch, and the reciprocating stroke is set. The traction tension is sent to the constant tension control device, and the winding pitch and reciprocating stroke are sent to the winding machine. The sidewall spacing directly participates in the calculation of the winding pitch, and the curvature of the bend directly participates in the calculation of the traction tension. The traction tension and winding parameters are automatically adjusted according to the geometric changes of the cross-section of the folded tube, avoiding the bend from being straightened due to excessive tension or slipping due to insufficient tension. This reduces the squeezing of adjacent tubes and the accumulation at the reciprocating reversal points caused by the mismatch between the winding pitch and the sidewall spacing, and maintains the cross-sectional shape and winding quality of the U-shaped or I-shaped folded tube. Attached Figure Description

[0017] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in this invention. For those skilled in the art, other drawings can be obtained based on these drawings.

[0018] Figure 1 This is a flowchart of the thermoplastic pipe compression molding process; Figure 2 This is a flowchart illustrating the generation of softening gradient in the cross-section and correction of cavity gap in thermoplastic pipe compression molding. Figure 3 This is a flowchart of the servo die lip displacement and circumferential temperature control for forming molds. Detailed Implementation

[0019] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0020] See Figure 1This invention provides a method for pressing and molding thermoplastic pipes, comprising: acquiring circumferential wall thickness data and axial temperature data of the pipe; generating a cross-sectional softening gradient based on the circumferential wall thickness data and axial temperature data of the pipe, and mapping the cross-sectional softening gradient to a cavity clearance correction amount of the molding die; driving the servo die lip of the molding die according to the cavity clearance correction amount of the molding die, and setting the temperature of the circumferential temperature control zone of the molding die; pressing a U-shaped or I-shaped folded pipe in the molding die, and collecting the side wall spacing and fold curvature of the U-shaped or I-shaped folded pipe; and setting the traction tension, winding pitch and reciprocating stroke according to the side wall spacing and fold curvature.

[0021] In specific implementation, please refer to Figure 2 The pipe is divided into sectors along its circumference. The number of sectors is determined based on the pipe's circumferential length and the wall thickness measurement resolution. Sector boundaries are evenly distributed along the pipe's circumference, with each sector corresponding to a circular arc area of ​​the pipe. When collecting the wall thickness value for each sector, a circumferential wall thickness detection device is used to measure the wall thickness of each sector along the pipe's circumference, acquiring one wall thickness value within each sector.

[0022] Temperature zones are divided along the axial direction of the pipe. The number of axial temperature zones is determined based on the axial length of the pipe and the rate of temperature change. The axial temperature zones are arranged continuously along the pipe axis, with each zone corresponding to a specific axial section of the pipe. When collecting the temperature value of each zone, an axial temperature sensor is used to obtain the surface temperature value of the pipe within the corresponding axial temperature zone.

[0023] The wall thickness value of each sector is paired with the temperature value of the corresponding temperature zone to generate a cross-sectional softening gradient. For the same cross-sectional location of the pipe, the wall thickness value of the sector at that cross-sectional location and the temperature value of the corresponding temperature zone are taken as a data pair. Data pairs from multiple cross-sectional locations constitute the cross-sectional softening gradient. The sector position of each sector's wall thickness value in the circumferential direction of the pipe is obtained, and the sector position is represented by the sector's central angle or sector boundary angle. The temperature zone position of each temperature zone's temperature value in the axial direction of the pipe is obtained, and the temperature zone position is represented by the axial coordinates of the temperature zone's center or temperature zone boundary. The sector positions and temperature zone positions are combined to form cross-sectional position data, which includes circumferential angular coordinates and axial distance coordinates.

[0024] The wall thickness values ​​of adjacent sectors are paired with the temperature values ​​of their corresponding temperature zones based on cross-sectional location data. In the circumferential direction, the wall thickness values ​​of adjacent sectors are connected in sequence according to their sector positions; in the axial direction, the temperature values ​​of adjacent temperature zones are connected in sequence according to their temperature zone positions. A linear interpolation method is used to continuously fit the wall thickness values ​​of adjacent sectors with the temperature values ​​of their corresponding temperature zones based on circumferential angles and axial distances. For two sectors with adjacent circumferential angles, the linear interpolation method calculates the interpolated wall thickness value based on the circumferential angle of the interpolation location; for two temperature zones with adjacent axial distances, it calculates the interpolated temperature value based on the axial distance of the interpolation location. Through linear interpolation, continuously distributed wall thickness and temperature values ​​are obtained on the pipe surface, forming a cross-sectional softening gradient.

[0025] The cross-sectional softening gradient is added to the preset cavity clearance of the forming die to obtain the cavity clearance correction amount of the forming die. The preset cavity clearance of the forming die is the basic cavity clearance setting value of the forming die before cross-sectional softening gradient correction is performed. The softening gradient value corresponding to each cross-sectional position in the cross-sectional softening gradient is added to the value of the preset cavity clearance of the forming die at the corresponding cross-sectional position to obtain the cavity clearance correction amount of the forming die. The cavity clearance correction amount of the forming die is used to drive the servo die lip of the forming die in the subsequent process. Among them, the value corresponding to each cross-sectional position in the cross-sectional softening gradient represents the cavity clearance compensation amount required at that cross-sectional position due to the difference in pipe wall thickness and temperature distribution. This compensation amount uses the same length dimension as the preset cavity clearance; the preset cavity clearance is the basic clearance setting value of the forming die before cross-sectional softening gradient correction is performed. Adding the cross-sectional softening gradient to the preset cavity clearance involves algebraically superimposing the base clearance setting value and the corresponding clearance compensation amount at the cross-sectional position determined by the same circumferential angle and the same axial distance to obtain the target cavity clearance value at that cross-sectional position, i.e., the cavity clearance correction amount. When the cavity space needs to be increased at this cross-sectional position, the compensation amount takes a positive value; when the cavity space needs to be reduced, the compensation amount takes a negative value. This allows the cavity clearance correction amount to vary along the circumferential and axial directions with the cross-sectional softening gradient, and serves as the target displacement basis for subsequent driving of the servo mold lip.

[0026] In specific implementation, please refer to Figure 3 The process converts the die cavity clearance correction amount into a displacement command for the die servo lip. The die cavity clearance correction amount contains clearance correction values ​​corresponding to multiple cross-sectional positions, and the displacement command for the die servo lip is the amount of displacement the die servo lip needs to move. During the conversion, each clearance correction value in the die cavity clearance correction amount is used as the target displacement value of the die servo lip at the corresponding cross-sectional position, and this target displacement value is converted into a displacement signal for the die servo lip actuator.

[0027] The servo die lip of the forming die is driven according to the displacement command. After receiving the displacement signal, the drive motor of the servo die lip moves according to the displacement signal, causing the servo die lip to move to the position corresponding to the displacement target value. During the movement of the servo die lip, the displacement sensor of the servo die lip detects the position change of the servo die lip in real time.

[0028] The temperature of the circumferential temperature control zone of the forming die is divided into multiple target values ​​based on the cross-sectional softening gradient. The temperature of the circumferential temperature control zone is formed by multiple heating zones arranged circumferentially around the forming die, with each temperature corresponding to a circumferential position on the inner surface of the die. The cross-sectional softening gradient includes the softening gradient value corresponding to the circumferential angle of the pipe. Based on the differences in the softening gradient values ​​within the cross-sectional softening gradient, the temperature of the circumferential temperature control zone of the forming die is divided into multiple target values, with each target value corresponding to a heating zone circumferentially around the forming die. The target temperature of each temperature control zone is determined by the cross-sectional softening gradient values ​​as follows: The average softening gradient values ​​corresponding to each cross-sectional position within the circumferential coverage area of ​​each heating zone are taken as the representative softening gradient value for that heating zone. The representative softening gradient value is compared with a preset reference softening gradient value. When the representative value is lower than the preset reference softening gradient value, the difference between the representative value and the preset reference softening gradient value is multiplied by a preset temperature compensation coefficient to obtain the temperature increase, and the target temperature of that heating zone is set as the preset reference temperature plus the temperature increase. When the representative value is higher than the preset reference softening gradient value, the difference between the representative value and the preset reference softening gradient value is multiplied by a preset temperature compensation coefficient to obtain the temperature decrease, and the target temperature of that heating zone is set as the preset reference temperature minus the temperature decrease. The preset temperature compensation coefficient is pre-calibrated based on the thermal response characteristics of the heating zone, ensuring that the target temperature of heating zones with a representative softening gradient value lower than the preset reference softening gradient value is higher than the preset reference temperature, and that the target temperature of heating zones with a representative softening gradient value higher than the preset reference softening gradient value is lower than the preset reference temperature.

[0029] The actual displacement of the servo die lip of the forming die is collected, and the actual displacement and displacement command are converted into the displacement command for the next cycle. A displacement sensor is installed on the servo die lip of the forming die, and the sensor collects the actual displacement of the servo die lip at a set cycle. The actual displacement is the position that the servo die lip of the forming die actually moves to within the set cycle. The actual displacement is compared with the corresponding displacement target value in the displacement command to obtain the displacement deviation. The displacement command for the next cycle is generated based on the displacement deviation. The next cycle displacement command is used to drive the movement of the servo die lip of the forming die in the next control cycle, so that the actual displacement of the servo die lip of the forming die approaches the displacement target value in the displacement command.

[0030] In practical implementation, a displacement sensor is installed on the servo die lip of the forming mold. The servo die lip is a movable die lip component in the forming mold. The displacement sensor is mounted on the moving part of the servo die lip, and the detection direction of the displacement sensor is consistent with the movement direction of the servo die lip. The displacement sensor is a linear displacement sensor. The fixed part of the displacement sensor is connected to the fixed mold base of the forming mold, and the movable part of the displacement sensor is connected to the servo die lip.

[0031] The actual displacement of the servo die lip of the forming die is collected by a displacement sensor at a set period. The set period is generated by the timer of the forming die controller, and the length of the set period is the motion control cycle of the servo die lip. At the end of each set period, the displacement sensor outputs the current actual displacement signal of the servo die lip, and the forming die controller reads the actual displacement signal and stores it as actual displacement data.

[0032] The actual displacement is converted into the opening data of the servo die lip of the forming die. The opening data of the servo die lip represents the opening distance between the servo die lip and the fixed die lip of the forming die. The actual displacement is the amount of movement of the servo die lip relative to the reference position of the displacement sensor, and the opening data is obtained through the opening conversion formula. The opening conversion formula is:

[0033] in, This indicates the opening size of the servo die lip in the forming die, in millimeters. This indicates the actual displacement of the servo die lip in the forming die, in millimeters. This represents the opening displacement conversion factor. Determined based on the transmission mechanism of the servo die lip of the forming mold. The method of obtaining this value is through calculation of the geometric relationship of the transmission mechanism of the servo die lip of the forming die. The value range is from 0.5 to 2.0; This indicates the offset of the opening data, in millimeters. The calibration was obtained based on the installation position of the displacement sensor of the servo die lip of the forming die. The value range is from 0 mm to 20 mm. When the transmission mechanism of the servo die lip of the forming die is a screw drive mechanism, the opening displacement conversion coefficient is... This is the quotient of the lead screw pitch and the encoder line count. The calibration method for the displacement sensor installation position of the servo die lip of the forming die is as follows: record the displacement sensor output value when the servo die lip of the forming die is in the closed position, and use the actual displacement corresponding to the closed position as the opening data offset. .

[0034] The opening data and the die cavity clearance correction amount are arranged in chronological order to generate the next cycle displacement command. Both the opening data and the die cavity clearance correction amount are timestamped. Arranging them in chronological order means mapping the opening data and die cavity clearance correction amounts for the same set cycle to the same time coordinate. The die controller calculates the opening deviation based on the opening data and die cavity clearance correction amount on the same time coordinate; the opening deviation is the die cavity clearance correction amount minus the opening data. This opening deviation is used as the displacement adjustment amount in the next cycle displacement command. The die controller drives the die servo lip movement according to the next cycle displacement command, ensuring that the die servo lip reaches the opening position corresponding to the die cavity clearance correction amount in the next cycle.

[0035] In practice, a laser rangefinder and a contour scanning sensor are installed at the exit of the forming mold. The laser rangefinder is installed on one side of the forming mold exit, and its laser emission direction is perpendicular to the side wall of the U-shaped or I-shaped folded tube. The contour scanning sensor is installed on the other side of the forming mold exit, and its scanning plane is perpendicular to the axis of the U-shaped or I-shaped folded tube.

[0036] The sidewall spacing of a U-shaped or I-shaped folded tube is acquired using a laser rangefinder. The laser rangefinder emits a laser pulse towards one sidewall of the U-shaped or I-shaped folded tube. The laser pulse is reflected by the sidewall and received by the laser rangefinder. The laser rangefinder calculates the distance between itself and the sidewall of the U-shaped or I-shaped folded tube based on the laser pulse's time of flight. The sidewall spacing is the inner distance between two opposite sidewalls of the U-shaped or I-shaped folded tube, and it is calculated by combining the distance measured by the laser rangefinder with the distance from the laser rangefinder's installation position to the center line of the forming die exit.

[0037] A contour scanning sensor acquires the corner contour point set of U-shaped or I-shaped folded pipes. The contour scanning sensor projects structured light stripes onto the corner area of ​​the U-shaped or I-shaped folded pipe. The image sensor of the contour scanning sensor acquires the deformation image of the structured light stripes in the corner area of ​​the U-shaped or I-shaped folded pipe. The contour scanning sensor extracts the corner contour point set based on the deformation image. The corner contour point set contains the two-dimensional coordinates of multiple corner contour points, and the two-dimensional coordinates of the corner contour points are located in the scanning plane of the contour scanning sensor.

[0038] The corner contour points are connected in the order of acquisition to form a corner contour polyline. Each corner contour point in the corner contour point set is arranged sequentially according to the order in which the corner contour points are output by the contour scanning sensor. Adjacent corner contour points are connected by straight line segments to form a corner contour polyline. The corner contour polyline consists of multiple straight line segments, with each straight line segment connecting two adjacent corner contour points.

[0039] Extract the included angle between adjacent line segments in a polygonal line with a bend in its contour. Adjacent line segments in a polygonal line with a bend in its contour are two straight line segments sharing the same bend in its contour. The included angle between adjacent line segments is the interior angle between the two straight line segments at the shared bend in its contour. The method for extracting the included angle is as follows: For each bend in the polygonal line with a bend in its contour except for the first and last bend in its contour, obtain the first vector from the bend in its contour to the previous bend in its contour, and obtain the second vector from the bend in its contour to the next bend in its contour. Calculate the included angle between the first vector and the second vector as the included angle between adjacent line segments.

[0040] The included angle is mapped to the curvature of the bend. The curvature of the bend is the degree of curvature of the bend profile line at the bend profile point where the included angle is located. The curvature of the bend is obtained by mapping the included angle. The formula for mapping the curvature of the bend is:

[0041] in, This indicates the curvature of the angle, expressed in radians per millimeter. Indicates the angle between adjacent line segments, in radians; Represents the curvature mapping coefficient of the included angle, with dimensions of , The sampling interval of the contour scanning sensor and the segment length of the polygonal contour line are determined based on the sampling interval of the contour scanning sensor. The data was obtained through calibration experiments of the contour scanning sensor. The value range is from 0.1 to 10.0; This indicates the baseline offset of the bend curvature, expressed in radians per millimeter. Determined based on the preset bend angle curvature reference value of U-shaped or I-shaped folded tubing. The data is obtained by measuring the contour scanning sensor when there is no bending in the corner area of ​​the U-shaped or I-shaped folded tube. The value ranges from 0 radians per millimeter to 0.5 radians per millimeter. (Angle curvature mapping coefficient) The calibration experiment is as follows: A standard bend curvature block is placed in the scanning plane of the contour scanning sensor. The contour scanning sensor acquires the bend profile point set of the standard bend curvature block, extracts the included angle between adjacent line segments of the standard bend curvature block, and divides the actual bend curvature of the standard bend curvature block by the extracted included angle between adjacent line segments to obtain the included angle curvature mapping coefficient. Angular curvature baseline offset The acquisition method is as follows: when the bend area of ​​the U-shaped or I-shaped folded pipe is in a straight state, the contour scanning sensor collects the bend contour point set and extracts the included angle of adjacent line segments. The included angle of adjacent line segments is substituted into the bend curvature mapping formula and the bend curvature is set as follows. If the value is zero, the baseline offset of the bend curvature can be obtained by solving. .

[0042] The bend curvature and sidewall spacing are written into the same data frame according to the pipe length to obtain the sidewall spacing and bend curvature. The pipe length is the length coordinate along the axial direction of the U-shaped or I-shaped folded pipe, and the pipe length is output by the length encoder on the traction device of the forming die. The bend curvature and the sidewall spacing are labeled with the pipe length. The same data frame contains the bend curvature value and the sidewall spacing value corresponding to one pipe length label. The bend curvature and the sidewall spacing are aligned with the pipe length labels and written into the same data frame to obtain the sidewall spacing and bend curvature.

[0043] In practical implementation, the winding pitch is determined based on the sidewall spacing. The sidewall spacing is the inner distance between two opposite sidewalls of the U-shaped or I-shaped folded tube, obtained by a laser rangefinder. The winding pitch is obtained by multiplying the sidewall spacing by the winding overlap coefficient. The winding pitch is the distance between the centerlines of two adjacent turns of tube on the winding machine reel in the axial direction of the reel. The winding overlap coefficient is related to the surface friction characteristics of the tube, the cross-sectional shape of the tube, and the winding tension. The formula for calculating the winding pitch is:

[0044] in, Indicates the winding pitch, in millimeters; This indicates the distance between the side walls, in millimeters. Indicates the winding overlap coefficient. The value range is from 1.0 to 1.5. The coefficient of friction is obtained through a winding test. During the winding test, the winding overlap coefficient is varied, and the tightness of the pipe arrangement on the reel is observed. The winding overlap coefficient that does not cause pipe slippage or interlayer crushing is selected as the calibration value. When the surface friction coefficient of the pipe is between 0.2 and 0.4, the winding overlap coefficient is set to 1.2.

[0045] The traction tension is determined by the curvature of the bend angle. The curvature of the bend angle is a quantitative value of the degree of bending in the bend area of ​​the U-shaped or I-shaped folded tube. The curvature of the bend angle is obtained by extracting the angle mapping between adjacent line segments after the bend angle profile point set is collected by the profile scanning sensor. The traction tension is obtained by multiplying the curvature of the bend angle by the tension transfer coefficient. The traction tension is the axial tension applied to the U-shaped or I-shaped folded tube by the constant tension control device. The tension transfer coefficient is related to the elastic modulus of the U-shaped or I-shaped folded tube material, the moment of inertia of the section, and the distance from the die exit to the traction device. The value of the tension transfer coefficient ranges from 0.5 N·mm / radian to 20 N·mm / radian. The tension transfer coefficient is obtained by calibration through tube bending springback test. In the tube bending springback test, the residual curvature of the tube after springback is measured at different bend angle curvatures. The required traction tension is determined based on the difference between the residual curvature and the target curvature. The traction tension is then divided by the curvature of the bend angle to obtain the tension transfer coefficient.

[0046] The reciprocating stroke is determined by the winding pitch and the reel width. The reel width is the effective winding width of the winding machine reel, determined by the distance between the flanges at both ends of the reel. Dividing the reel width by the winding pitch yields the number of turns per stroke. The number of turns per stroke is the number of tube turns corresponding to one axial movement of the cable guide along the reel within the effective winding width. The reciprocating stroke is set according to the number of turns per stroke, and is the distance the cable guide moves along the reel axially, equal to the reel width. The cable guide reverses direction when it reaches one flange of the reel; the reversing position is determined by the number of turns per stroke.

[0047] The traction tension is sent to the constant tension control device. Upon receiving the traction tension, the constant tension control device adjusts the output torque of the traction drive motor so that the axial tension acting on the U-shaped or I-shaped folded tube reaches the traction tension. The winding pitch and reciprocating stroke are sent to the winding machine. Upon receiving the winding pitch, the winding machine adjusts the ratio of the winding shaft speed to the axial movement speed of the cable guide so that the distance between the center lines of two adjacent turns of tube in the axial direction of the reel is equal to the winding pitch. Upon receiving the reciprocating stroke, the winding machine sets the reversing position of the cable guide, causing the cable guide to reciprocate within the effective winding width of the reel.

[0048] The above description is merely a specific embodiment of this application, but the scope of protection of this application is not limited thereto. Any changes or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in this application should be included within the scope of protection of this application.

Claims

1. A method for pressing and molding thermoplastic pipes, characterized in that, include: Obtain the circumferential wall thickness data and axial temperature data of the pipe; A cross-sectional softening gradient is generated based on the circumferential wall thickness data and the axial temperature data of the pipe, and the cross-sectional softening gradient is mapped to the cavity clearance correction amount of the forming die. Drive the servo lip of the forming mold according to the cavity clearance correction amount of the forming mold, and set the temperature of the circumferential temperature control zone of the forming mold. The setting of the circumferential temperature control zone of the forming mold is: dividing the temperature of the circumferential temperature control zone of the forming mold into multiple target values ​​of temperature control zones according to the cross-sectional softening gradient. U-shaped or I-shaped folded tubes are pressed in a forming mold, and the side wall spacing and folding angle curvature of the U-shaped or I-shaped folded tubes are collected. The traction tension, winding pitch, and reciprocating stroke are set according to the sidewall spacing and the angle curvature.

2. The thermoplastic pipe compression molding method according to claim 1, characterized in that, The step of generating a cross-sectional softening gradient based on the circumferential wall thickness data and the axial temperature data of the pipe, and mapping the cross-sectional softening gradient to a correction amount for the cavity clearance of the forming die, includes: Divide the pipe into sectors along its circumference and collect the wall thickness value of each sector; The pipe is divided into temperature zones along its axial direction, and the temperature value of each zone is collected. The wall thickness value of each sector is paired with the temperature value of the corresponding temperature zone to generate the cross-sectional softening gradient; The cross-sectional softening gradient is added to the preset cavity clearance of the forming die to obtain the cavity clearance correction amount of the forming die. The value corresponding to each cross-sectional position in the cross-sectional softening gradient represents the cavity clearance compensation amount required at that position due to differences in pipe wall thickness and temperature distribution. The clearance compensation amount and the preset cavity clearance use the same length dimension. The preset cavity clearance is the basic clearance setting value of the forming die before cross-sectional softening gradient correction. The addition is performed by algebraically superimposing the basic clearance setting value and the corresponding clearance compensation amount at the cross-sectional position determined by the same circumferential angle and the same axial distance to obtain the target cavity clearance value at that cross-sectional position, i.e., the cavity clearance correction amount of the forming die. When the cavity space needs to be increased at that cross-sectional position, the clearance compensation amount is positive; when the cavity space needs to be decreased, the clearance compensation amount is negative.

3. The thermoplastic pipe compression molding method according to claim 1, characterized in that, The step of driving the servo lip of the forming mold according to the cavity clearance correction amount and setting the temperature of the circumferential temperature control zone of the forming mold includes: The cavity clearance correction amount of the forming die is converted into a displacement command for the servo die lip of the forming die; Drive the servo die lip of the forming mold according to the displacement command; The temperature of the circumferential temperature control zone of the forming mold is divided into multiple target values ​​according to the cross-sectional softening gradient; The actual displacement of the servo die lip of the forming die is collected, and the actual displacement and the displacement command are converted into the next cycle displacement command. The conversion of the actual displacement and the displacement command into the next cycle displacement command is as follows: the actual displacement is compared with the corresponding displacement target value in the displacement command to obtain the displacement deviation, and the next cycle displacement command is generated based on the displacement deviation to make the actual displacement approach the displacement target value.

4. The thermoplastic pipe compression molding method according to claim 1, characterized in that, The process of pressing U-shaped or I-shaped folded tubes in a forming mold, and collecting the sidewall spacing and fold angle curvature of the U-shaped or I-shaped folded tubes, includes: A laser rangefinder and a contour scanning sensor are installed at the exit of the forming mold; The sidewall spacing of the U-shaped or I-shaped folded tube is collected by the laser ranging sensor; The contour scanning sensor collects the set of bend contour points of the U-shaped or I-shaped folded pipe. The set of points representing the bend contour is paired with the sidewall spacing according to the pipe length to obtain the sidewall spacing and bend curvature.

5. The method for pressing and forming a thermoplastic pipe according to claim 1, characterized in that, The setting of traction tension, winding pitch, and reciprocating stroke according to the sidewall spacing and the curvature of the bend angle includes: The winding pitch is determined according to the sidewall spacing, the traction tension is determined according to the bend curvature, and the reciprocating stroke is determined according to the winding pitch and the reel width. The traction tension is sent to the constant tension control device, and the winding pitch and the reciprocating stroke are sent to the winding machine.

6. The method for pressing and forming a thermoplastic pipe according to claim 2, characterized in that, The step of pairing the wall thickness value of each sector with the temperature value of the corresponding temperature zone to generate the cross-sectional softening gradient includes: Obtain the wall thickness value of each sector in the circumferential direction of the pipe sector position, and obtain the temperature value of each temperature zone in the axial direction of the pipe temperature zone position; The sector position and the temperature zone position are combined to form cross-sectional position data; The wall thickness values ​​of adjacent sectors are paired with the temperature values ​​of the corresponding temperature zones based on the cross-sectional location data to obtain the cross-sectional softening gradient.

7. The method for pressing and forming a thermoplastic pipe according to claim 3, characterized in that, The process of acquiring the actual displacement of the servo die lip of the forming die and converting the actual displacement and the displacement command into a displacement command for the next cycle includes: A displacement sensor is installed on the servo die lip of the forming mold, and the actual displacement is collected by the displacement sensor at a set period. The actual displacement is converted into the opening data of the servo die lip of the forming die; The opening data and the cavity clearance correction amount of the forming die are arranged in chronological order to generate the displacement command for the next cycle.

8. The method for pressing and forming a thermoplastic pipe according to claim 4, characterized in that, The set of bend contour points is paired with the sidewall spacing according to the pipe length to obtain the sidewall spacing and bend curvature, including: The set of points representing the bend contour is connected in the order of collection to form a bend contour polyline. Extract the included angle between adjacent line segments in the polygonal outline; Map the included angle to the curvature of the bend angle; The formula for mapping the curvature of the bend is: in, This indicates the curvature of the angle, expressed in radians per millimeter. Indicates the angle between adjacent line segments, in radians; Represents the curvature mapping coefficient of the included angle, with dimensions of ; This indicates the baseline offset of the bend curvature, expressed in radians per millimeter. Determined based on the preset bend angle curvature reference value of U-shaped or I-shaped folded pipe; The bend curvature and the sidewall spacing are written into the same data frame according to the length of the pipe to obtain the sidewall spacing and bend curvature.

9. The method for pressing and forming a thermoplastic pipe according to claim 5, characterized in that, The winding pitch is determined according to the sidewall spacing, the traction tension is determined according to the bend curvature, and the reciprocating stroke is determined according to the winding pitch and the reel width, including: Multiply the sidewall spacing by the winding overlap coefficient to obtain the winding pitch; Multiplying the curvature of the bending angle by the tension transmission coefficient yields the traction tension; Divide the reel width by the winding pitch to obtain the number of single-stroke turns, and set the reciprocating stroke according to the number of single-stroke turns. The reciprocating stroke is set according to the number of single-stroke turns as follows: the reciprocating stroke is equal to the reel width, and the cable guide moves to the end of the reel and reverses direction. The reversing position is determined according to the number of single-stroke turns.

10. The method for pressing and forming a thermoplastic pipe according to claim 6, characterized in that, The step of pairing the wall thickness values ​​of adjacent sectors with the temperature values ​​of the corresponding temperature zones according to the cross-sectional position data includes: using a linear interpolation method to continuously fit the wall thickness values ​​of adjacent sectors with the temperature values ​​of the corresponding temperature zones according to the circumferential angle and axial distance to obtain the cross-sectional softening gradient.