A method for removing perfluorinated compounds from water.
By using a foam concentration method formed by the synergistic addition of surfactants and sodium sulfate, combined with electrochemical oxidation treatment by a three-dimensional microporous REM-BDD electrode, the problem of low removal efficiency of perfluorinated compounds in water was solved, achieving a high-efficiency and low-cost removal effect for perfluorinated compounds.
Patent Information
- Application Number
- CN202611320317.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-28
- Publication Date
- 2026-11-17
AI Technical Summary
Existing technologies are insufficient for efficiently removing perfluorinated compounds from water bodies. Traditional methods suffer from problems such as low adsorption efficiency, high energy consumption, high cost, and difficulty in treating byproducts, and lack scalable treatment solutions.
A foam concentration method is formed by synergistic addition of surfactant solution and sodium sulfate, combined with electrochemical oxidation treatment by three-dimensional microporous REM-BDD electrode, to first enrich and then deeply degrade perfluorinated compounds, and improve removal efficiency by utilizing the synergistic effect of foam layer and electrode.
It achieves a high efficiency removal rate of perfluorinated compounds, reduces the volume of foam concentrate to 6% of the original water, reduces the concentration of perfluorinated compounds in the effluent to below 80 ng/L, achieves a removal rate of over 85%, and significantly improves degradation efficiency.
Abstract
Description
Technical Field
[0001] This invention belongs to the field of wastewater treatment technology, specifically relating to a method for removing perfluorinated compounds from water. Background Technology
[0002] Perfluorinated compounds (PFAS) are chemically stable due to their carbon-fluorine bonds, making them difficult to degrade naturally. They can accumulate in organisms and be transferred through the food chain, posing a long-term risk to human health. Furthermore, these substances can persist in water, soil, and air, and can migrate over long distances, hence they are called permanent chemicals. Current global efforts to manage PFAS are shifting from detection and regulation to comprehensive remediation and green alternatives.
[0003] The main sources of perfluorinated compounds (PFOCs) include wastewater containing PFOCs discharged from industrial processes such as chemical plants, textile mills, and paint factories; linear and branched perfluorohexane, perfluorooctanoic acid, perfluorohexane sulfonic acid, and perfluorooctanoic acid contained in aqueous film-forming foam fire extinguishing agents; and effluent from wastewater treatment plants. Because conventional wastewater treatment processes have limited removal efficiency for PFOCs, the concentration of these substances in the effluent is sometimes higher than in the influent, making it one of the main direct sources of PFOC emissions into the aquatic environment.
[0004] Traditional water treatment systems struggle to effectively break carbon-fluorine bonds, and existing treatment technologies can be broadly categorized into two types. Physical methods include granular activated carbon adsorption, ion exchange, and membrane filtration. Granular activated carbon adsorption is currently the most widely used method, effective for long-chain perfluorinated compounds such as perfluorooctanoic acid (PFOA) and perfluorooctane sulfonic acid (PFOS), but its adsorption efficiency for short-chain substances like perfluorobutyric acid (PFBA) is very low. PFBA is prone to penetrating the filter bed, and once saturated, it requires frequent replacement or high-temperature regeneration. Ion exchange resins offer higher selectivity but are susceptible to interference from other anions such as sulfate in the water. The high-concentration wastewater generated during regeneration requires safe disposal. Membrane filtration technologies, such as nanofiltration and reverse osmosis, offer high removal rates, but produce a significant proportion of high-concentration perfluorinated compound wastewater in the influent. This concentrated wastewater is extremely difficult to treat, and membrane fouling leads to a continuous increase in energy consumption and operating costs.
[0005] Another type is advanced oxidation, which aims to directly destroy the molecular structure of perfluorinated compounds to achieve harmlessness. However, these methods usually require specific reaction conditions and often face limitations in practical applications, such as incomplete degradation, low mineralization rates, easy generation of more difficult-to-treat short-chain fluorinated byproducts, high energy consumption, or insufficient selectivity. Currently, most advanced oxidation technologies are still in the laboratory research stage, lacking feasible, low-cost, and scalable remediation solutions. Summary of the Invention
[0006] In view of the shortcomings of the prior art, the first objective of the present invention is to provide a method for removing perfluorinated compounds from water.
[0007] To achieve the above objectives, the present invention adopts the following technical solution:
[0008] This invention discloses a method for removing perfluorinated compounds from water. A surfactant solution and sodium sulfate are added to PFAS-contaminated water, and gas is introduced to generate micro-nano bubbles. A foam layer containing PFAS is formed on the top of the water, and the lower layer is purified water. The foam layer is collected to obtain foam concentrate, and the lower purified water is obtained. The foam concentrate is subjected to electrochemical oxidation treatment to obtain the treated liquid.
[0009] The surfactant in the surfactant solution is selected from at least one of carboxymethyl cellulose, hexadecyltrimethylammonium bromide, and hexadecyltrimethylammonium chloride, preferably carboxymethyl cellulose;
[0010] The anode used in the electrochemical oxidation treatment is a three-dimensional microporous REM-BDD electrode; the three-dimensional microporous REM-BDD electrode is composed of a porous substrate and a BDD film disposed on the surface of the porous substrate.
[0011] The method for removing perfluorinated compounds from water provided by this invention first employs a foam concentration method. By adding a surfactant solution and sodium sulfate, a foam concentrate with highly enriched PFAS can be obtained. The volume of the collected PFAS concentrate is reduced to less than 6% of the original PFAS-contaminated water volume, and the PFAS removal rate in the lower purified water is greater than 90%. Then, the foam concentrate is subjected to deep degradation using REM electrochemical method, which can achieve a perfluorinated compound removal rate of more than 80% in the foam concentrate.
[0012] In actual operation, depending on the pollutant concentration of the PFAS-contaminated water body, if the pollutant indicators in the lower-level purified water body do not meet the discharge standards, surfactant solution and sodium sulfate can be added to the lower-level purified water body again for foam concentration to further purify the lower-level purified water body.
[0013] Experiments have shown that adding carboxymethyl cellulose to PFAS-contaminated water can increase the viscosity of the liquid phase of the solution, form a protective film at the gas-liquid interface, and inhibit liquid film drainage, thereby delaying foam breakage. At the same time, the addition of sodium sulfate can reduce the solubility of surfactants in water, thereby enhancing their adsorption affinity at the bubble-water interface and further increasing the stability of the foam. Therefore, with the synergistic addition of surfactant solution and sodium sulfate, the removal rate of pollutants in PFAS-contaminated water during the foam concentration process is significantly improved.
[0014] In addition, the added sodium sulfate can increase conductivity, reduce energy consumption in the subsequent electrochemical oxidation treatment of foam concentrate, and improve the effect. At the same time, a small amount of sodium persulfate is generated during the electrochemical oxidation treatment, which greatly increases the removal effect of perfluorinated compounds. Furthermore, the electrode used in the electrochemical oxidation treatment of this invention is a three-dimensional microporous REM-BDD electrode, which has a higher specific surface area and more accessible active sites compared to a planar BDD electrode. The reactants will form forced convection mass transfer in the pores, thereby compressing the diffusion layer thickness and strengthening the interfacial mass transfer process, thereby greatly improving the removal efficiency of PFAS.
[0015] In a preferred embodiment, the surfactant solution contains a surfactant mass fraction of 0.1% to 0.2 wt%.
[0016] In a preferred embodiment, the mass-to-volume ratio of the surfactant solution to the PFAS-contaminated water is 2-20 mg:1 L, preferably 5-10 mg:1 L. Experiments have shown that controlling the amount of surfactant solution added within this range yields optimal performance. Too little surfactant significantly reduces the foam concentration effect, while too much not only affects the foam concentration effect but also increases the difficulty of subsequent degradation.
[0017] In a preferred embodiment, the amount of sodium sulfate added is such that the concentration of sodium sulfate in the PFAS-polluted water body is 2-10 mM, preferably 6-10 mM.
[0018] In a preferred embodiment, the gas is air.
[0019] In the preferred embodiment, the gas-liquid volume ratio of the introduced gas to the PFAS-contaminated water body is 1:2~4.
[0020] In a preferred embodiment, the pore size of the micropores in the three-dimensional microporous REM-BDD electrode is 5~100μm, preferably 7-34μm, and more preferably 7-11μm.
[0021] Experiments have shown that the micropore treatment efficiency is optimal among the three-dimensional microporous REM-BDD electrodes with the above-mentioned pore size. The appropriate small pore size structure shortens the mass transfer path length, improves current utilization efficiency and interfacial reaction rate. Of course, the pore size cannot be too small. If it is too small, diffusion will be hindered, reducing the utilization rate of active sites and thus reducing the treatment efficiency.
[0022] In a preferred embodiment, the specific surface area of the three-dimensional microporous REM-BDD electrode is 0.01~0.12 m². 2 g -1 .
[0023] In a preferred embodiment, the porous substrate is made of SiC and / or metal, preferably SiC. Experiments have shown that the three-dimensional microporous REM-BDD electrode using a porous SiC substrate exhibits the best electrochemical oxidation effect.
[0024] In a preferred embodiment, the fabrication process of the three-dimensional microporous REM-BDD electrode is as follows: immersing a porous substrate in an acid solution for etching to obtain a porous etched substrate, then planting a seed crystal on the surface of the porous etched substrate, and then performing boron-doped diamond by chemical vapor deposition.
[0025] Experiments have shown that depositing BDD on porous substrates is significantly more difficult than depositing it on smooth planar electrodes. This invention combines acid etching with nanodiamond seed crystals on porous SiC substrates, effectively solving the problems of difficult nucleation and poor film adhesion in HFCVD on non-diamond substrates.
[0026] In a further preferred embodiment, the acid solution is obtained by mixing sulfuric acid and nitric acid, wherein the volume ratio of sulfuric acid to nitric acid in the acid solution is 1:2~4.
[0027] In a further preferred embodiment, the soaking time is 1 to 2 minutes.
[0028] The above-mentioned acid solution can remove organic impurities from the surface and perform slight etching on the surface. In actual operation, after soaking, the surface is rinsed three times with deionized water, and then ultrasonically cleaned in deionized water and acetone (≥99.5%) for 20-30 minutes each.
[0029] Further preferred, the seed crystal planting process involves immersing the porous etched substrate in a nanodiamond suspension and ultrasonically treating it for 30-45 minutes, wherein the mass fraction of nanodiamonds in the nanodiamond suspension is 0.03-0.08 wt.%.
[0030] In a further preferred embodiment, the chemical vapor deposition (CVD) is hot-filament CVD. The CVD process is as follows: a porous etched substrate with a seed crystal is placed in a CVD furnace, and a mixed gas of H2, CH4, and B2H6 is introduced. The flow rate ratio of H2, CH4, and B2H6 is controlled at 90-110:3-5:1.0-2.0, the tungsten filament temperature is 2000-2200℃, the substrate temperature is 800-940℃, the chamber pressure is 3.5-5.5 kPa, and the deposition time is 10-16 hours. Through acid etching and seed crystal implantation, the CVD deposition time is short and the deposition effect is good.
[0031] In a preferred embodiment, during the electrochemical oxidation treatment, the cathode is selected from one of copper mesh, titanium mesh, or 316L stainless steel mesh.
[0032] In a preferred embodiment, the current density during the electrochemical oxidation treatment is 5–50 mA / cm². 2 The electrochemical oxidation treatment time is 30~90 min.
[0033] In a further preferred embodiment, during the electrochemical oxidation treatment, the flow mode of the foam concentrate is either a flow-through mode or a circulation mode, preferably a circulation mode.
[0034] Experiments have shown that in the flow mode, the foam concentrate passes through the internal channels of the three-dimensional microporous REM electrode under external pressure. The reactants form forced convection mass transfer within the channels, thereby compressing the thickness of the diffusion layer and enhancing the interfacial mass transfer process, which can further improve the degradation effect.
[0035] Further optimization involves controlling the water flux at 2.0~6.0×10⁻⁶ when the electrochemical oxidation treatment is performed in flow mode. 4 Lm 2 h -1 .
[0036] Beneficial effects
[0037] The method for removing perfluorinated compounds from water provided by this invention first uses a foam concentration method to obtain a foam concentrate with highly enriched PFAS. The volume of the collected PFAS concentrate is reduced to less than 6% of the original PFAS-contaminated water volume. Then, a REM electrochemical method is used for deep degradation, which can achieve a perfluorinated compound removal efficiency of more than 85%, reduce the PFOA content in the effluent to below 80 ng / L, and reduce the total PFAF content to below 300 ng / L. Detailed Implementation
[0038] Example 1
[0039] Step 1: Fabrication of four three-dimensional microporous REM-BDD electrodes with different pore sizes
[0040] Porous SiC substrates with pore sizes of 7 μm, 11, 21, and 34 μm were selected. First, the substrates were immersed in a mixed acid solution of sulfuric acid and nitric acid (volume ratio of sulfuric acid to nitric acid 1:3) for 1 min to remove surface organic impurities and perform light etching. Subsequently, the substrates were ultrasonically cleaned sequentially in deionized water and acetone for 20 min each. The cleaned substrates were then ultrasonically seeded in a 0.05 wt.% nanodiamond suspension for 30 min. The seeded porous SiC substrates were then placed in a hot-filament chemical vapor deposition (HFCVD) apparatus. The deposition atmosphere consisted of H2, CH4, and B2H6 with flow rates of 97 sccm, 3 sccm, and 1.2 sccm, respectively. The deposition was performed at a substrate temperature of 800°C and a chamber pressure of 4 kPa for 10 h, yielding four three-dimensional microporous REM-BDD electrodes, named BDD7μm, BDD11μm, BDD11μm, and BDD11μm.
[0041] Step 2: Formation of foam concentrate and purification of PFAS-contaminated water.
[0042] Carboxymethyl cellulose solution and sodium sulfate were added to a 50L volume of PFAS-contaminated water (PFOA concentration of 0.002μM (815ng / L)). The mass-to-volume ratio of carboxymethyl cellulose to PFAS-contaminated water was 10mg:1L. The concentration of sodium sulfate in the PFAS-contaminated water was controlled at 10mM. Air was introduced simultaneously, and the gas-liquid ratio of air to PFAS-contaminated water was controlled at 1:3. Bubbles were generated, and a stable foam rich in PFAS was formed on the top of the water. At the same time, the PFAS molecules on the surface of the bubbles were further concentrated during the drainage process. After the concentration was completed, 2.75L of foam concentrate was obtained by skimming off the foam and then collecting it by suction. 47.25L of purified water was obtained from the lower layer.
[0043] Four portions of foam concentrate were obtained using the method described above.
[0044] Step 3: Purification of foam concentrate
[0045] The four foam concentrates were subjected to electrochemical oxidation treatment. For all four foam concentrates, a three-dimensional microporous REM-BDD electrode was used as the anode and a copper mesh as the cathode. The only difference was that the three-dimensional microporous REM-BDD electrodes used were 7μm, 11μm, 21μm, and 34μm BDD, respectively. During the electrochemical oxidation treatment, the current density was controlled at 30 mA / cm². 2 The foam concentrate flows through a three-dimensional microporous REM-BDD electrode in a flow-through mode, with the water flux controlled at 4.0 × 10⁻⁶. 4 Lm 2After 60 minutes of electrochemical oxidation treatment, four post-treatment solutions were obtained and named REM-BDD7μm post-treatment solution, REM-BDD11μm post-treatment solution, REM-BDD11μm post-treatment solution and REM-BDD11μm post-treatment solution, respectively.
[0046] Performance Results
[0047] In this embodiment, the PFOA concentration in the PFAS-contaminated water was 0.002 μM (815 ng / L). After foam concentration treatment in step two, the resulting lower purified water volume was 2.75 L, which was only 5.5% of the original PFAS-contaminated water volume. The concentration of the concentrated solution was 0.0333 μM (7576 ng / L), a concentration of 16.66 times. The PFOA concentration in the lower purified water was 74.1 ng / L, and the PFOA removal rate was 91%.
[0048] Four foam concentrates were electro-purified using BDD7μm, BDD11μm, BDD21μm, and BDD34μm electrodes, respectively. The PFOA concentrations in the resulting REM-BDD7μm, REM-BDD11μm, REM-BDD11μm, and REM-BDD34μm treated solutions were 75.76 ng / L, 333.34 ng / L, 962.15 ng / L, and 1469.74 ng / L, respectively, with PFOA removal rates of 99.0%, 95.6%, 87.3%, and 80.6%. It can be seen that the pore size of the three-dimensional microporous REM-BDD electrode has a significant impact on the degradation effect; a smaller pore size increases the reaction rate. This is because the smaller pore size shortens the mass transfer path length, improving current utilization efficiency and interfacial reaction rate.
[0049] Comparative Example 1
[0050] Other conditions were the same as in Example 1, except that sodium sulfate was not added. As a result, the concentration of PFOA in the foam concentrate was 0.0261 μM, which was 13.1 times concentrated. The concentration of PFOA in the lower purified water was 246 ng / L, and the removal efficiency was 71.9%.
[0051] And using BDD 7μm After electrochemical oxidation, the concentration of PFOA in the treated solution of REM-BDD7μm electrode was 2.74μg / L, and the PFOA removal rate was 74.6%.
[0052] Comparative Example 2
[0053] Other conditions were the same as in Example 1, except that methylcellulose was not added. As a result, the concentration of PFOA in the foam concentrate was 0.0188 μM, which was 9.4 times concentrated. The concentration of PFOA in the lower purified water was 424 ng / L, and the removal efficiency was 51.61%.
[0054] Comparative Example 3
[0055] Other conditions were the same as in Example 1, except that the gas-liquid volume ratio of the introduced gas to the PFAS-contaminated water was 1:1. As a result, the PFOA concentration in the foam concentrate was 0.0214 μM, which was 10.7 times concentrated. The PFOA concentration in the lower purified water was 361 ng / L, and the removal efficiency was 58.8%.
[0056] Comparative Example 4
[0057] Other conditions were the same as in Example 1, except that a flat SiCBDD electrode was used in the electrochemical oxidation process. As a result, the PFOA concentration in the treated solution was 3318.3 ng / L, and the removal efficiency was 56.2%.
Claims
1. A method for removing perfluorinated compounds from water, characterized in that: A surfactant solution and sodium sulfate are added to PFAS-contaminated water, and gas is introduced to generate micro-nano bubbles. A foam layer containing PFAS is formed on the top of the water, and the lower layer is purified water. The foam layer is collected to obtain foam concentrate, and the foam concentrate is subjected to electrochemical oxidation treatment to obtain the treated liquid. The surfactant in the surfactant solution is selected from one of carboxymethyl cellulose, hexadecyltrimethylammonium bromide, and hexadecyltrimethylammonium chloride. The anode used in the electrochemical oxidation treatment is a three-dimensional microporous REM-BDD electrode; the three-dimensional microporous REM-BDD electrode is composed of a porous substrate and a BDD film disposed on the surface of the porous substrate.
2. The method for removing perfluorinated compounds from water according to claim 1, characterized in that: The surfactant solution contains a surfactant mass fraction of 0.1% to 0.2 wt%.
3. The method for removing perfluorinated compounds from water according to claim 1, characterized in that: The mass-to-volume ratio of the surfactant solution to the PFAS-contaminated water is 2-20 mg: 1 L; The amount of sodium sulfate added is such that, after being added to the PFAS-polluted water body, the concentration in the PFAS-polluted water body is 2~10 mM.
4. The method for removing perfluorinated compounds from water according to claim 1, characterized in that: The gas is air; The gas-liquid volume ratio of the introduced gas to the PFAS-contaminated water body is 1:2~4.
5. The method for removing perfluorinated compounds from water according to claim 1, characterized in that: The pore size of the micropores in the three-dimensional microporous REM-BDD electrode is 5~100μm; The specific surface area of the three-dimensional microporous REM-BDD electrode is 0.01~0.12m². 2 g -1 .
6. The method for removing perfluorinated compounds from water according to claim 1, characterized in that: The porous substrate is made of SiC and / or metal.
7. A method for removing perfluorinated compounds from water according to claim 1 or 5, characterized in that: The fabrication process of the three-dimensional microporous REM-BDD electrode is as follows: a porous substrate is immersed in an acid solution for etching to obtain a porous etched substrate, then a seed crystal is planted on the surface of the porous etched substrate, and then boron-doped diamond is deposited by chemical vapor deposition.
8. The method for removing perfluorinated compounds from water according to claim 7, characterized in that: The acid solution is obtained by mixing sulfuric acid and nitric acid, wherein the volume ratio of sulfuric acid to nitric acid in the acid solution is 1:2~4. The soaking time is 1-2 minutes; The seed crystal planting process involves immersing a porous etched substrate in a nanodiamond suspension and ultrasonically treating it for 30-45 minutes. The nanodiamond suspension contains 0.03-0.08 wt.% nanodiamonds. The chemical vapor deposition is hot-filament chemical vapor deposition. The chemical vapor deposition process is as follows: a porous etched substrate after seeding is placed in a chemical vapor deposition furnace, and a mixed gas of H2, CH4 and B2H6 is introduced. The flow rate ratio of H2, CH4 and B2H6 is controlled at 90-110:3-5:1.0-2.0, the temperature of the tungsten filament is 2000-2200℃, the temperature of the substrate is 800-940℃, the chamber pressure is 3.5-5.5kPa, and the deposition time is 10-16h.
9. The method for removing perfluorinated compounds from water according to claim 1, characterized in that: During the electrochemical oxidation treatment, the cathode is selected from one of copper mesh, titanium mesh, and 316L stainless steel mesh. During the electrochemical oxidation treatment, the current density is 5–50 mA / cm². 2 The electrochemical oxidation treatment time is 30~90 min.
10. The method for removing perfluorinated compounds from water according to claim 9, characterized in that: During the electrochemical oxidation treatment, the flow pattern of the foam concentrate is either a flow-through pattern or a flow-through pattern. When electrochemical oxidation treatment is performed in flow mode, the water flux is controlled at 2.0~6.0×10⁻⁶. 4 Lm 2 h -1 .