A process for producing silicon-rich improved soil

By using a mechanical-liquid phase synergistic dissociation process to convert inert crystalline silicon into citrate-soluble silicon and active monosilicic acid precursors, combined with heavy metal passivation and organic functional group grafting, the high energy consumption and strong alkalinity of existing silicon-based soil amendment materials are solved. This achieves a continuous supply of effective silicon and stable soil structure, reduces the risk of heavy metals, and is suitable for various types of arable land improvement.

CN123107697APending Publication Date: 2026-11-17SHANDONG WOPT BIOTECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611443850.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-17
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing silicon-based soil amendment materials suffer from problems such as high energy consumption at high temperatures, strong alkalinity of finished products, low effective silicon conversion rate, single amendment function, and high risk of heavy metals. They are difficult to simultaneously achieve continuous supply of effective silicon, soil structure reshaping, heavy metal passivation, and microecological stability.

Method used

A mechanical-liquid phase synergistic dissociation process was adopted to convert inert crystalline silicon into citrate-soluble silicon and active monosilicic acid precursors through mechanical grinding and liquid phase reaction. Combined with heavy metal passivation and organic functional group grafting, an organic-inorganic composite interface layer was formed to prepare silicon-rich improved soil.

Benefits of technology

It reduces production energy consumption, achieves continuous and slow release of effective silicon, stabilizes soil structure, reduces heavy metal risks, promotes indigenous microbial communities, is applicable to the improvement of different types of arable land, and avoids the alkalinity problem caused by traditional high-temperature calcination.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123107697A_ABST
    Figure CN123107697A_ABST
Patent Text Reader

Abstract

This invention discloses a process for producing silicon-rich improved soil, specifically including the following steps: S1, raw material pretreatment; S2, mechanical-liquid phase synergistic dissociation activation; S3, liquid phase phase-modification passivation; S4, organic functional group grafting modification; S5, solid-liquid separation and low-temperature maturation; S6, mixing and molding. This invention relates to the field of soil amendment material preparation technology. This silicon-rich improved soil production process achieves silicon mineral lattice destruction through mechanical-liquid phase synergistic dissociation, significantly reducing production energy consumption. Through the phase-modification passivation process, the proportions of water-soluble silicon, citrate-soluble silicon, and lattice-controlled-release silicon are controlled in stages, ensuring an effective silicon supply in the initial stage of soil application and achieving continuous slow release in the medium and long term, preventing rapid silicon leaching and loss. By simultaneously completing in-situ co-precipitation passivation of heavy metals in the liquid phase system, an aluminosilicate passivation shell is formed on the outer layer of mineral particles, fixing the heavy metals inherent in the raw materials and reducing the risk of the finished product returning to the field.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of soil amendment material preparation technology, specifically a process for producing silicon-rich soil amendments. Background Technology

[0002] my country's arable land generally suffers from soil compaction, shallow topsoil, lack of available silicon, pH imbalance, and high heavy metal activity. Long-term continuous cropping and excessive fertilizer application further exacerbate topsoil degradation. Most existing silicon-based soil amendments employ high-temperature calcination and hydrothermal synthesis processes using single minerals, which present several prominent practical problems: First, high-temperature calcination is energy-intensive, and the finished product is excessively alkaline, easily disrupting the original pH balance of the soil and posing a risk of root irritation to slightly acidic arable land. Second, most processes only pursue total silicon content, resulting in a high proportion of crystalline inert silicon, leading to a slow conversion rate to plant-available silicon in the soil environment, poor initial effectiveness, and a short release period. Third, ordinary silicon amendments lack a coupling structure compatible with local soil organic matter and indigenous microorganisms, making the particles prone to pulverization and loss after application, with limited aggregate formation capacity. Fourth, some slag-based silicon amendment products may introduce trace amounts of harmful heavy metals, lacking an in-situ pre-passivation process, posing potential risks when directly applied to the field.

[0003] Most existing patents focus on the formulation and compounding of silicon-calcium-magnesium fertilizers and silicon-based conditioners. These typically involve direct mixing, high-temperature activation, and granulation, lacking an integrated process route encompassing "mineral pre-dissociation - mild phase transformation - organic matter grafting - simultaneous formation of indigenous microbial colonization carriers." This makes it difficult to simultaneously achieve multiple objectives, including continuous supply of effective silicon, soil structure reshaping, in-situ passivation of heavy metals, and maintenance of soil microecological stability. Therefore, developing a low-energy-consumption, silicon-controlled phase production process suitable for different types of arable land has practical production value. Summary of the Invention

[0004] (a) Technical problems to be solved To address the shortcomings of existing technologies, this invention provides a silicon-rich soil improvement production process that solves the problems of high energy consumption at high temperatures, low effective silicon conversion rate, strong alkalinity of the finished product, and limited improvement functions. This process does not rely on traditional high-temperature calcination but employs a mechanical-liquid phase synergistic dissociation method to gradually convert inert crystalline silicon into citric acid-soluble silicon and active monosilicic acid precursors. Simultaneously, it completes heavy metal pre-passivation and organic functional group grafting, resulting in a finished improved soil product. The finished product offers multiple benefits, including slow-release silicon supply, promotion of soil aggregate formation, stabilization of indigenous microbial communities, and reduction of heavy metal activity. It can be directly applied to the field for the improvement of compacted, acidified, and lightly heavy metal-contaminated farmland.

[0005] (II) Technical Solution To achieve the above objectives, the present invention is implemented through the following technical solution: a process for producing improved soil rich in silicon, specifically including the following steps; S1. Raw material pretreatment: The raw materials are 60-75 parts by weight of high-silica weathered rock ore, 12-20 parts of calcium-magnesium base mineral auxiliary material, 8-15 parts of biochar and 2-5 parts of weak alkaline buffer additive. The high-silica weathered rock ore and calcium-magnesium base mineral auxiliary material are crushed and ball-milled to 200-320 mesh, and the biochar is screened through a 100-mesh sieve to remove impurities. S2. Mechanical-liquid phase synergistic dissociation and activation: The ore from step S1 is put into a horizontal stirred ball mill reactor with a solid-liquid ratio of 1:2.2-2.8. Deionized water is added, and a weak complexing activation aid is added. The temperature inside the reactor is controlled at 55-65℃, and the stirring speed is 280-350 r / min. The ball milling dissociation is carried out for 2.5-4 hours. The mineral lattice is destroyed by grinding and shearing to generate amorphous silicon precursors. In this process, the mineral crystal lattice is destroyed by grinding and shearing. At the same time, in a weak complexing environment, the silicon-oxygen bonds on the mineral surface are partially broken, generating a large amount of amorphous silicon precursors. High-temperature calcination is not performed to avoid the formation of strong alkaline silicates. S3. Liquid-phase passivation: Maintain the temperature inside the reactor at 50-60℃, add calcium hydroxide suspension dropwise to adjust the pH of the system to 8.2-8.8, and stir at a constant temperature and low speed for 90-130 minutes. Heavy metal ions will co-precipitate and form an aluminosilicate passivation shell on the surface of silicon mineral particles. Aluminum ions, lead, and cadmium heavy metal ions dissolved in the system will co-precipitate with silicate and hydroxide ions and form an aluminosilicate passivation shell on the surface of silicon mineral particles. This achieves in-situ pre-fixation of heavy metals inside the raw materials, while controlling the silicon phase to ensure that water-soluble silicon accounts for 8%-13% of the total silicon, citric acid-soluble silicon accounts for 28%-36% of the total silicon, and the remainder is lattice-released silicon. S4. Organic functional group grafting modification: Add pretreated biochar powder, maintain the temperature at 45-55℃, stir at 150-200 r / min, and react for 1.5-2.5 h. The surface groups of biochar graft with the silanol groups of mineral particles to construct an organic-inorganic composite interface layer. This interface layer can delay the rapid dissolution of silicon elements when they come into contact with water, realize graded slow release, and provide attachment sites for soil native microorganisms, thereby improving the colonization ability of microorganisms after the finished product is put into the soil. S5. Solid-liquid separation and low-temperature maturation: The slurry is filtered by plate and frame filter press to obtain a filter cake with a moisture content of 32%-38%. The filter cake is placed in a micro-permeable sealed maturation chamber and maturated at 28-35℃ for 48-72 hours. The pH of the material drops to 7.3-8, and a silicon-based modified matrix is ​​obtained. During the maturation process, the unreacted silicon phase inside the material continues to slowly transform, eliminating local strong alkaline sites. S6. Mixing and Molding: The silicon-based modified matrix is ​​mixed with a weakly alkaline buffering agent, and then rolled and granulated at low temperature. The granulation temperature is not higher than 65℃, the particle size is 2-6mm, and the mixture is air-dried and sieved at low temperature to obtain a silicon-rich improved soil product.

[0006] Preferably, in step S3, the mass concentration of the calcium hydroxide suspension is 4-6 wt%, and the dropping rate is 25-40 mL / min.

[0007] Preferably, in step S5, the curing chamber is kept slightly permeable, allowing a small amount of air to circulate.

[0008] Preferably, the high-silica weathered rock ore in step S1 is weathered rhyolite or weathered dacite, with a silica mass fraction ≥62%.

[0009] Preferably, the calcium-magnesium ore auxiliary material in step S1 is serpentine weathered powder.

[0010] Preferably, the weakly alkaline buffering agent in step S1 is fine natural magnesite powder.

[0011] Preferably, the weak complexing activator in step S2 is sodium citrate, and the amount of sodium citrate added is 0.8%-1.5% of the total mass of the mineral.

[0012] Preferably, during the screening process in step S1, the heavy metal content of each raw material is tested, and batches exceeding the control limits for agricultural soil are eliminated.

[0013] (III) Beneficial Effects This invention provides a process for producing silicon-rich improved soil. Compared with existing technologies, it has the following advantages: (1) The production process of this silicon-rich improved soil relies on mechanical liquid phase synergistic dissociation to destroy the silicon mineral lattice, which significantly reduces production energy consumption. Through the phase-adjusting passivation process, the proportion of water-soluble silicon, citric acid-soluble silicon and lattice-released silicon is controlled in stages, which not only ensures an effective silicon supply in the early stage of soil entry, but also achieves continuous slow release in the medium and long term, and will not cause the problem of rapid leaching and loss of silicon.

[0014] (2) The production process of this silicon-rich improved soil involves the simultaneous in-situ co-precipitation and passivation of heavy metals in a liquid phase system, forming an aluminosilicate passivation shell on the outer layer of mineral particles. The heavy metals in the raw materials are fixed, resulting in low risk of the finished product returning to the field. Subsequently, organic-inorganic grafting is used to construct a composite interface, which improves the mechanical properties of the particles and prevents them from instantly disintegrating and pulverizing when soaked in water.

[0015] (3) The soil amendment produced by this silicon-rich process has a pH value in the neutral to slightly alkaline range, avoiding the root burn problem caused by the strong alkalinity of traditional high-temperature silicon fertilizers. It can improve acidified soils and can also be used in neutral arable land without excessively raising the soil pH. The organic-inorganic composite interface can provide attachment sites for native soil microorganisms, which is conducive to the formation of soil aggregate structure after application, and simultaneously achieves multiple functions such as silicon supplementation, conditioning properties, maintenance of soil micro-ecology, and passivation of heavy metals.

[0016] (4) The production process of this silicon-rich improved soil is completed in a continuous process flow, with the reaction, passivation and grafting completed in the same reactor in stages, reducing material transfer loss; the final product is granular improved soil, which can be directly spread and tilled, and is suitable for various scenarios such as field, orchard and facility cultivation. Attached Figure Description

[0017] Figure 1 This is a flowchart of the process of the present invention. Detailed Implementation

[0018] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0019] Please see Figure 1 The present invention provides three technical solutions: a process for producing improved soil rich in silicon, specifically including the following embodiments: Example 1: A process for producing silicon-rich improved soil, specifically including the following steps; S1. Raw material pretreatment: The raw materials, by weight, consist of 68 parts of high-silica weathered rock ore, 16 parts of calcium-magnesium-based mineral auxiliary material, 12 parts of biochar, and 3 parts of weakly alkaline buffering agent. The high-silica weathered rock ore and calcium-magnesium-based mineral auxiliary material are crushed and ball-milled to 280 mesh. The biochar is sieved through a 100-mesh sieve to remove impurities. The high-silica weathered rock ore is weathered rhyolite or weathered dacite with a silica mass fraction ≥62%. The calcium-magnesium-based mineral auxiliary material is weathered serpentine powder. The weakly alkaline buffering agent is fine natural magnesite powder. During the screening process, the heavy metal content of each raw material is tested, and batches exceeding the control limits for agricultural soil are rejected. S2. Mechanical-Liquid Phase Synergistic Dissociation and Activation: The ore from step S1 is added to a horizontal stirred ball mill reactor with a solid-liquid ratio of 1:2.5. Deionized water is added, along with a weak complexing activation aid. The reactor temperature is controlled at 60℃, and the stirring speed is 300 r / min. Ball milling and dissociation are carried out for 3.2 hours. The mineral lattice is broken by grinding and shearing to generate amorphous silicon precursors. This process relies on grinding and shearing to break the mineral crystal lattice. At the same time, under a weak complexing environment, some silicon-oxygen bonds on the mineral surface are broken, generating a large amount of amorphous silicon precursors. High-temperature calcination is not performed to avoid the formation of strongly alkaline silicates. The weak complexing activation aid is sodium citrate, and the amount of sodium citrate added is 1.2% of the total mass of the ore. S3. Liquid-phase passivation: Maintain the temperature inside the reactor at 55℃, add calcium hydroxide suspension dropwise to adjust the pH of the system to 8.5, and stir at a constant temperature and low speed for 110 min. Heavy metal ions will co-precipitate and form an aluminosilicate passivation shell on the surface of silicon mineral particles. Aluminum ions, lead, and cadmium heavy metal ions dissolved in the system will co-precipitate with silicate and hydroxide ions and form an aluminosilicate passivation shell on the surface of silicon mineral particles. This achieves in-situ pre-fixation of heavy metals inside the raw materials, while controlling the silicon phase to ensure that water-soluble silicon accounts for 10% of the total silicon, citrate-soluble silicon accounts for 32% of the total silicon, and the remainder is lattice-released silicon. The mass concentration of calcium hydroxide suspension is 5wt%, and the dropping rate is 32mL / min. S4. Organic functional group grafting modification: The pretreated biochar powder is added, the temperature is maintained at 50℃, the stirring speed is 180r / min, and the reaction is carried out for 2h. The surface groups of biochar graft with the silanol groups of mineral particles to construct an organic-inorganic composite interface layer. This interface layer can delay the rapid dissolution of silicon elements when they come into contact with water, realize the graded slow release, and provide attachment sites for soil native microorganisms, thereby improving the colonization ability of microorganisms after the finished product is put into the soil. S5. Solid-liquid separation and low-temperature maturation: The slurry is filtered by plate and frame filter press to obtain a filter cake with a moisture content of 35%. The filter cake is placed in a micro-permeable and sealed maturation chamber and maturated at 31°C for 58 hours. The pH of the material drops to 7.6, and a silicon-based modified matrix is ​​obtained. During the maturation process, the unreacted silicon phase inside the material continues to slowly transform, eliminating local strong alkaline points. The maturation chamber is kept micro-permeable, allowing a small amount of air to circulate. S6. Mixing and Molding: The silicon-based modified matrix is ​​mixed with a weakly alkaline buffering agent, and then rolled and granulated at low temperature. The granulation temperature is not higher than 65℃, the particle size is 4mm, and the mixture is air-dried and sieved at low temperature to obtain a silicon-rich improved soil product.

[0020] Example 2: A process for producing silicon-rich improved soil, specifically including the following steps; S1. Raw material pretreatment: The raw materials, by weight, consist of 60 parts of high-silica weathered rock ore, 12 parts of calcium-magnesium-based mineral auxiliary material, 8 parts of biochar, and 2 parts of weakly alkaline buffering agent. The high-silica weathered rock ore and calcium-magnesium-based mineral auxiliary material are crushed and ball-milled to 200 mesh. The biochar is sieved through a 100-mesh sieve to remove impurities. The high-silica weathered rock ore is weathered rhyolite or weathered dacite with a silica mass fraction ≥62%. The calcium-magnesium-based mineral auxiliary material is weathered serpentine powder. The weakly alkaline buffering agent is fine powder of natural magnesite. During the screening process, the heavy metal content of each raw material is tested, and batches exceeding the control limits for agricultural soil are rejected. S2. Mechanical-Liquid Phase Synergistic Dissociation and Activation: The ore from step S1 is added to a horizontal stirred ball mill reactor with a solid-liquid ratio of 1:2.2. Deionized water is added, along with a weak complexing activator. The reactor temperature is controlled at 55℃, and the stirring speed is 280 r / min. The ball milling dissociation is carried out for 2.5 hours. The mineral lattice is broken by grinding and shearing to generate amorphous silicon precursors. In this process, the mineral crystal lattice is broken by grinding and shearing. At the same time, in a weak complexing environment, some silicon-oxygen bonds on the mineral surface are broken, generating a large amount of amorphous silicon precursors. High-temperature calcination is not performed to avoid the formation of strongly alkaline silicates. The weak complexing activator is sodium citrate, and the amount of sodium citrate added is 0.8% of the total mass of the ore. S3. Liquid-phase passivation: Maintain the temperature inside the reactor at 50℃, add calcium hydroxide suspension dropwise to adjust the pH of the system to stabilize at 8.2, and stir at a constant temperature and low speed for 90 min. Heavy metal ions will co-precipitate and form an aluminosilicate passivation shell on the surface of silicon mineral particles. Aluminum ions, lead, and cadmium heavy metal ions dissolved in the system will co-precipitate with silicate and hydroxide ions and form an aluminosilicate passivation shell on the surface of silicon mineral particles. This achieves in-situ pre-fixation of heavy metals inside the raw materials, while controlling the silicon phase to ensure that water-soluble silicon accounts for 8% of the total silicon, citrate-soluble silicon accounts for 28% of the total silicon, and the remainder is lattice-released silicon. The mass concentration of calcium hydroxide suspension is 4wt%, and the dropping rate is 25mL / min. S4. Organic functional group grafting modification: The pretreated biochar powder is added, the temperature is maintained at 45℃, the stirring speed is 150r / min, and the reaction is carried out for 1.5h. The surface groups of biochar graft with the silanol groups of mineral particles to construct an organic-inorganic composite interface layer. This interface layer can delay the rapid dissolution of silicon elements when they come into contact with water, so as to achieve graded slow release. On the other hand, it provides attachment sites for soil native microorganisms and improves the colonization ability of microorganisms after the finished product is put into the soil. S5. Solid-liquid separation and low-temperature maturation: The slurry is filtered by plate and frame filter press to obtain a filter cake with a moisture content of 32%. The filter cake is placed in a micro-permeable and sealed maturation chamber and maturated at 28°C for 48 hours. The pH of the material drops to 7.3, and a silicon-based modified matrix is ​​obtained. During the maturation process, the unreacted silicon phase inside the material continues to slowly transform, eliminating local strong alkaline points. The maturation chamber is kept micro-permeable, allowing a small amount of air to circulate. S6. Mixing and Molding: The silicon-based modified matrix is ​​mixed with a weakly alkaline buffering agent, and then rolled and granulated at a low temperature. The granulation temperature is not higher than 65℃, the particle size is 2mm, and the mixture is air-dried and sieved at a low temperature to obtain a silicon-rich improved soil product.

[0021] Example 3: A process for producing silicon-rich improved soil, specifically including the following steps; S1. Raw material pretreatment: The raw materials, by weight, consist of 75 parts of high-silica weathered rock ore, 20 parts of calcium-magnesium-based mineral auxiliary material, 15 parts of biochar, and 5 parts of weakly alkaline buffering agent. The high-silica weathered rock ore and calcium-magnesium-based mineral auxiliary material are crushed and ball-milled to 320 mesh. The biochar is sieved through a 100-mesh sieve to remove impurities. The high-silica weathered rock ore is weathered rhyolite or weathered dacite with a silica mass fraction ≥62%. The calcium-magnesium-based mineral auxiliary material is weathered serpentine powder. The weakly alkaline buffering agent is fine powder of natural magnesite. During the screening process, the heavy metal content of each raw material is tested, and batches exceeding the control limits for agricultural soil are rejected. S2. Mechanical-liquid phase synergistic dissociation and activation: The ore from step S1 is put into a horizontal stirred ball mill reactor with a solid-liquid ratio of 1:2.8. Deionized water is added, and a weak complexing activation aid is added. The temperature inside the reactor is controlled at 65℃, and the stirring speed is 350 r / min. The ball milling dissociation is carried out for 4 hours. The mineral lattice is destroyed by grinding and shearing to generate amorphous silicon precursors. In this process, the mineral crystal lattice is destroyed by grinding and shearing. At the same time, in a weak complexing environment, the silicon-oxygen bonds on the mineral surface are partially broken, generating a large amount of amorphous silicon precursors. High-temperature calcination is not performed to avoid the formation of strong alkaline silicates. The weak complexing activation aid is sodium citrate, and the amount of sodium citrate added is 1.5% of the total mass of the ore. S3. Liquid-phase passivation: Maintain the temperature inside the reactor at 60℃, add calcium hydroxide suspension dropwise to adjust the pH of the system to 8.8, and stir at a constant temperature and low speed for 130 min. Heavy metal ions will co-precipitate and form an aluminosilicate passivation shell on the surface of silicon mineral particles. Aluminum ions, lead, and cadmium heavy metal ions dissolved in the system will co-precipitate with silicate and hydroxide ions and form an aluminosilicate passivation shell on the surface of silicon mineral particles. This achieves in-situ pre-fixation of heavy metals inside the raw materials and controls the silicon phase, ensuring that water-soluble silicon accounts for 13% of the total silicon, citrate-soluble silicon accounts for 36% of the total silicon, and the remainder is lattice-released silicon. The mass concentration of calcium hydroxide suspension is 6wt%, and the dropping rate is 40mL / min. S4. Organic functional group grafting modification: The pretreated biochar powder is added, the temperature is maintained at 55℃, the stirring speed is 200r / min, and the reaction is carried out for 2.5h. The surface groups of biochar graft with the silanol groups of mineral particles to construct an organic-inorganic composite interface layer. This interface layer can delay the rapid dissolution of silicon elements when they come into contact with water, so as to achieve graded slow release. On the other hand, it provides attachment sites for soil native microorganisms and improves the colonization ability of microorganisms after the finished product is put into the soil. S5. Solid-liquid separation and low-temperature maturation: The slurry is filtered by plate and frame filter press to obtain a filter cake with a moisture content of 38%. The filter cake is placed in a micro-permeable and sealed maturation chamber and maturated at 35°C for 72 hours. The pH of the material drops back to 8, and a silicon-based modified matrix is ​​obtained. During the maturation process, the unreacted silicon phase inside the material continues to slowly transform, eliminating local strong alkaline points. The maturation chamber is kept micro-permeable, allowing a small amount of air to circulate. S6. Mixing and Molding: The silicon-based modified matrix is ​​mixed with a weakly alkaline buffering agent, and then rolled and granulated at a low temperature. The granulation temperature is not higher than 65℃, the particle size is 6mm, and the mixture is air-dried and sieved at a low temperature to obtain a silicon-rich improved soil product.

[0022] In summary, this invention achieves silicon mineral lattice destruction through mechanical liquid-phase synergistic dissociation, significantly reducing production energy consumption. Through a phase-adjusting passivation process, the proportions of water-soluble silicon, citrate-soluble silicon, and lattice-released silicon are controlled in stages, ensuring an effective silicon supply in the initial soil application stage and achieving sustained slow release in the medium to long term, preventing rapid silicon leaching and loss. Simultaneous in-situ co-precipitation passivation of heavy metals in the liquid-phase system forms an aluminosilicate passivation shell on the outer layer of mineral particles, fixing the heavy metals inherent in the raw materials and minimizing the risk of the finished product returning to the field. Subsequent organic-inorganic grafting constructs a composite interface, improving particle mechanical properties, preventing instantaneous disintegration and pulverization upon immersion in water. The prepared amendment has a pH in the neutral to slightly alkaline range, avoiding the root burn problem associated with traditional high-temperature silicon fertilizers. It can improve acidified soils and can also be used in neutral arable land without excessively raising the soil pH. The organic-inorganic composite interface can provide attachment sites for soil native microorganisms. After application, it is conducive to the formation of soil aggregate structure and simultaneously achieves multiple functions such as silicon supplementation, conditioning properties, maintenance of soil micro-ecology, and passivation of heavy metals. Through the entire process flow, the reaction, passivation and grafting are completed in the same reactor in stages, reducing material transfer loss. The final product is granular improved soil that can be directly spread and tilled, and is suitable for various scenarios such as field, orchard and facility cultivation.

[0023] Furthermore, any content not described in detail in this specification is existing technology known to those skilled in the art.

[0024] It should be noted that, in this document, relational terms such as "first" and "second" are used only to distinguish one entity or operation from another, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Furthermore, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such process, method, article, or apparatus.

[0025] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.

Claims

1. A process for producing silicon-rich improved soil, characterized in that: Specifically, it includes the following steps; S1. Raw material pretreatment: The raw materials are 60-75 parts by weight of high-silica weathered rock ore, 12-20 parts of calcium-magnesium base mineral auxiliary material, 8-15 parts of biochar and 2-5 parts of weak alkaline buffer additive. The high-silica weathered rock ore and calcium-magnesium base mineral auxiliary material are crushed and ball-milled to 200-320 mesh, and the biochar is screened through a 100-mesh sieve to remove impurities. S2. Mechanical-liquid phase synergistic dissociation and activation: The ore from step S1 is put into a horizontal stirred ball mill reactor with a solid-liquid ratio of 1:2.2-2.

8. Deionized water is added, and a weak complexing activation aid is added. The temperature inside the reactor is controlled at 55-65℃, the stirring speed is 280-350 r / min, and the ball milling dissociation is carried out for 2.5-4 hours. The mineral lattice is destroyed by grinding and shearing to generate an amorphous silicon precursor. S3. Liquid phase passivation: Maintain the temperature inside the reactor at 50-60℃, add calcium hydroxide suspension dropwise to adjust the pH of the system to 8.2-8.8, and stir at a constant temperature and low speed for 90-130 minutes. Heavy metal ions will co-precipitate and form an aluminosilicate passivation shell on the surface of silicon mineral particles. At the same time, the silicon phase will be controlled to ensure that water-soluble silicon accounts for 8%-13% of the total silicon, citric acid-soluble silicon accounts for 28%-36% of the total silicon, and the remainder is lattice-released silicon. S4. Organic functional group grafting modification: Add pretreated biochar powder, maintain the temperature at 45-55℃, stir at 150-200r / min, and react for 1.5-2.5h. The surface groups of biochar graft with the silanol groups of mineral particles to construct an organic-inorganic composite interface layer. S5. Solid-liquid separation and low-temperature maturation: The slurry is filtered by plate and frame filter press to obtain filter cake with a moisture content of 32%-38%. The filter cake is placed in a micro-permeable sealed maturation chamber and maturated at 28-35℃ for 48-72 hours. The pH of the material drops back to 7.3-8, and a silicon-based modified matrix is ​​obtained. S6. Mixing and Molding: The silicon-based modified matrix is ​​mixed with a weakly alkaline buffering agent, and then rolled and granulated at low temperature. The granulation temperature is not higher than 65℃, the particle size is 2-6mm, and the mixture is air-dried and sieved at low temperature to obtain a silicon-rich improved soil product.

2. The process for producing silicon-rich improved soil according to claim 1, characterized in that: In step S3, the mass concentration of the calcium hydroxide suspension is 4-6 wt%, and the dropping rate is 25-40 mL / min.

3. The process for producing silicon-rich improved soil according to claim 1, characterized in that: In step S5, the curing chamber is kept slightly permeable, allowing a small amount of air to circulate.

4. The process for producing silicon-rich improved soil according to claim 1, characterized in that: In step S1, the high-silica weathered rock ore is weathered rhyolite or weathered dacite, with a silica mass fraction ≥62%.

5. The process for producing silicon-rich improved soil according to claim 1, characterized in that: In step S1, the calcium-magnesium ore auxiliary material is serpentine weathered powder.

6. The process for producing silicon-rich improved soil according to claim 1, characterized in that: The weakly alkaline buffering agent in step S1 is fine natural magnesite powder.

7. The process for producing silicon-rich improved soil according to claim 1, characterized in that: In step S2, the weak complexing activator is sodium citrate, and the amount of sodium citrate added is 0.8%-1.5% of the total mass of the mineral.