Molten Salt Electrolytic Recycling System Based on Co-processing of Aluminosilicate Overhaul Slag in Alumina Electrolytic Cells

By using an aluminum electrolytic cell co-processing system, combined with solar thermal collection and molten salt thermal storage technology, the problems of low resource recovery rate and high energy consumption in the treatment of aluminum-silica overhaul slag have been solved, realizing efficient resource utilization and low-carbon operation of aluminum-silica overhaul slag.

CN123108592APending Publication Date: 2026-11-17CENT SOUTH UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202610460809.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-04-09
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing technologies for treating aluminum electrolytic cell overhaul slag have problems such as low resource recovery rate, high energy consumption, large carbon emissions, low system integration and high environmental pollution risk. In particular, it is difficult to achieve efficient resource utilization of aluminum-silica overhaul slag.

Method used

A collaborative treatment system based on aluminum electrolysis cells is adopted, which combines solar thermal collection, molten salt thermal storage, shell-type molten salt electrolysis cells, waste gas absorption and adsorption, and alloy sensible heat recovery system to achieve efficient resource utilization of aluminum-silicon overhaul slag.

Benefits of technology

This system achieves efficient recovery of Al2O3 and SiO2 from aluminosilicate overhaul slag, recycling of fluorides, significantly reducing system energy consumption and carbon emissions, improving resource utilization, and ensuring system stability and safety.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123108592A_ABST
    Figure CN123108592A_ABST
Patent Text Reader

Abstract

This invention relates to the field of solid waste resource utilization technology in the aluminum electrolysis industry, and particularly to a molten salt electrolytic recycling system for the co-processing of aluminum-silica overhaul slag in aluminum electrolysis cells. The system includes: a solar thermal collection system, a molten salt thermal storage system, a material and power supply system, a shell-type molten salt electrolysis cell system, a waste gas absorption and adsorption system, and an alloy sensible heat recovery system. Through the coupled design of the shell-type molten salt electrolysis cell and the molten salt thermal storage system, this invention achieves efficient recovery of valuable elements and recycling of fluorides in the overhaul slag, significantly improving resource utilization. During molten salt electrolysis, Al₂O₃ and SiO₂ in the aluminum-silica overhaul slag are reduced to an Al-Si intermediate alloy, achieving an aluminum recovery rate of up to 92% and a silicon recovery rate of up to 85%. Fluorides in the overhaul slag dissolve into the electrolyte system and are recycled as effective electrolyte components. Combined with the capture of fluorides by the waste gas absorption system, the overall fluoride recovery rate is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of solid waste resource utilization technology in the aluminum electrolysis industry, and in particular to a molten salt electrolytic recycling system based on the co-processing of aluminum-silica overhaul slag in aluminum electrolysis cells. Background Technology

[0002] Aluminum electrolytic cells generate a large amount of overhaul slag during long-term operation. This aluminum-silica overhaul slag contains components such as Al2O3, SiO2, fluorides, and small amounts of cyanide. Existing treatment technologies mainly include landfilling, wet leaching, and high-temperature roasting, all of which suffer from low resource recovery rates, incomplete cyanide detoxification, high energy consumption, and large carbon emissions. In recent years, although molten salt electrolysis has been attempted to treat this type of waste slag, it still faces significant drawbacks such as excessive power consumption, serious heat waste, inability to effectively couple clean energy sources, and low system integration.

[0003] Landfilling is currently the most primitive method for disposing of overhaul waste, directly sending it to hazardous waste landfills. The disadvantages of this method are: severe resource waste: large quantities of valuable Al2O3, SiO2, and fluorides in the overhaul waste are not recovered; high environmental risk: after landfilling, fluorides and cyanides may migrate with leachate, posing a long-term pollution hazard; and high economic cost: the cost of landfilling hazardous waste is typically 2,000 to 5,000 yuan per ton, and land resources are becoming increasingly scarce.

[0004] Wet treatment mainly includes processes such as water washing, acid leaching, and alkali leaching. For example: Water washing removes soluble fluorides and cyanides through multi-stage countercurrent washing, but cannot recover Al2O3 and SiO2, and generates a large amount of fluoride-containing wastewater, resulting in high treatment costs; Acid leaching uses sulfuric acid or hydrochloric acid to leach elements such as aluminum and sodium, but suffers from high acid consumption, severe equipment corrosion, and difficulty in disposing of waste acid; Alkali leaching uses sodium hydroxide solution to dissolve Al2O3 and SiO2, but has poor reaction selectivity, makes aluminum-silicon separation difficult, and generates a large amount of alkaline wastewater. Overall, wet treatment generally suffers from drawbacks such as long process flow, low recovery rate of valuable elements, high wastewater treatment pressure, and severe secondary pollution, making it difficult to achieve efficient resource utilization of overhaul slag.

[0005] Pyrometallurgical treatment mainly includes processes such as high-temperature roasting and melt solidification. For example, high-temperature roasting decomposes cyanide at temperatures above 1000℃, but fluorides are easily volatilized at high temperatures, causing secondary pollution; melt solidification involves co-melting overhaul slag with flux to form a glassy solid, but this method is extremely energy-intensive and fails to recover valuable elements. Although pyrometallurgical treatment can achieve the thermal decomposition of cyanide, it consumes a huge amount of energy, has high carbon emissions, and insufficient resource utilization, which does not conform to the green and low-carbon development direction. Therefore, a molten salt electrolytic recycling system based on aluminum electrolysis cells for the co-processing of aluminosilicate overhaul slag is needed to solve the above problems. Summary of the Invention

[0006] The purpose of this invention is to solve the problems mentioned in the background section.

[0007] To achieve the above objectives, the present invention adopts the following technical solution: A system for the molten salt electrolytic recycling of aluminum-silica overhaul slag based on the co-processing of aluminum electrolytic cells includes: Solar thermal collection system, molten salt thermal storage system, material and power supply system, shell-type molten salt electrolysis cell system, waste gas absorption and adsorption system, and alloy sensible heat recovery system; The shell-type molten salt electrolysis cell system includes an electrolysis cell body and a molten salt heating shell disposed outside the electrolysis cell body. The molten salt heating shell is connected to the molten salt heat storage system and is used to introduce high-temperature molten salt to provide external heating to the electrolysis cell.

[0008] Preferably, the molten salt thermal storage system includes a high-temperature molten salt storage tank and a low-temperature molten salt storage tank; The high-temperature molten salt storage tank is connected to the solar thermal collection system, the molten salt heating shell of the shell-type molten salt electrolysis cell system, and the Stirling unit, respectively. The low-temperature molten salt storage tank is connected to the discharge end of the shell-type molten salt electrolysis cell system and is used to receive the degraded molten salt produced by electrolysis.

[0009] Preferably, the discharge end of the shell-type molten salt electrolysis cell system is equipped with a molten salt separation device. The molten salt separation device consists of a connecting flange, an Archimedes screw, a filter screen, a shell, a deteriorated molten salt outlet, and an alloy outlet. The outlet of the molten salt separation device is connected to the alloy sensible heat recovery system, the low-temperature molten salt storage tank, and the electrolyte recovery pipeline, respectively.

[0010] Preferably, the main body of the electrolytic cell is made of ceramic fiber furnace, and the outside is wrapped with resistance wire as an auxiliary heating element; The main body of the electrolytic cell is also provided with a thermocouple interface, an inlet pipe and an outlet pipe, and the outlet pipe is connected to the waste gas absorption and adsorption system.

[0011] Preferably, the Stirling unit is electrically connected to the material and power supply system to convert the thermal energy of molten salt into electrical energy and provide part of the power to the electrolytic cell; The material and power supply system also includes a grid-connected switching switch, which is used to automatically switch to grid power supply when the Stirling unit's power supply is insufficient.

[0012] Preferably, the waste gas absorption and adsorption system includes a calcium-based absorption tower, the inlet of which is connected to the outlet pipeline of the shell-type molten salt electrolysis cell system, and the outlet is connected to the atmosphere via a fan.

[0013] Preferably, the alloy sensible heat recovery system includes an indirect heat exchanger, the hot side inlet of which is connected to the alloy outlet of the molten salt separation device, and the cold side is connected to the material preheating pipeline or the heating pipeline of the low-temperature molten salt storage tank.

[0014] Preferably, it also includes a central controller, which is electrically connected to the solar thermal acquisition system, the molten salt thermal storage system, the material and power supply system, the shell-type molten salt electrolysis cell system, the waste gas absorption and adsorption system, and the alloy sensible heat recovery system, respectively. The shell-type molten salt electrolysis cell system includes a ceramic fiber base, a furnace barrel installed at the top of the ceramic fiber base, and resistance wires installed on the outside of the furnace barrel. A furnace cover is provided at the top of the furnace barrel, and the top periphery of the furnace cover is connected to the furnace wall by nuts. A ceramic fiber furnace chamber is provided on the inner side of the furnace wall. A thermocouple is provided at the bottom left side of the furnace wall. An air inlet, a material feeding and discharging port, and an exhaust port are arranged sequentially from left to right on the top of the furnace cover. The central controller is configured to: prioritize adjusting the molten salt flow rate of the molten salt heating shell to maintain the electrolysis temperature based on the temperature of the electrolytic cell and the temperature of the high-temperature molten salt storage tank, and activate resistance wire auxiliary heating when the shell heating is insufficient.

[0015] Preferably, the central controller is further configured to: When the temperature of the high-temperature molten salt storage tank is ≥750℃, molten salt is preferentially allocated to the molten salt heating shell, and the remaining molten salt is allocated to the Stirling unit for power generation. When the temperature of the high-temperature molten salt storage tank is between 650°C and 750°C, reduce the flow rate of the molten salt heating shell and start the resistance wire auxiliary heating, while stopping the Stirling unit. When the temperature of the high-temperature molten salt storage tank is <650℃, the heating shell of the molten salt is shut off, and the electrolytic cell is heated at full power by the resistance wire.

[0016] Preferably, the central controller is further configured with emergency stop interlock logic, and the triggering conditions of the emergency stop interlock logic include at least one of the following: Electrolytic cell temperature > 980℃ or < 820℃; Molten salt leakage detection alarm for casing; The furnace internal pressure is >0.2MPa or <-0.08MPa; High-temperature molten salt storage tank temperature > 950℃; The concentration of toxic gases exceeded the standard; Overcurrent or short circuit fault in rectifier cabinet; The circulating cooling water supply was interrupted; When the emergency shutdown interlock logic is triggered, at least one of the following actions is performed: cutting off the electrolysis power supply, closing the shell molten salt inlet valve, opening the emergency exhaust pipeline, and starting emergency cooling.

[0017] The present invention has at least the following beneficial effects: 1. By coupling the shell-type molten salt electrolytic cell with the molten salt thermal storage system, the efficient recovery of valuable elements in the overhaul slag and the recycling of fluorides are achieved, significantly improving the resource utilization level. Al2O3 and SiO2 in the aluminosilicate overhaul slag are reduced to Al-Si intermediate alloy during molten salt electrolysis, with an aluminum recovery rate of up to 92% and a silicon recovery rate of up to 85%. Fluorides in the overhaul slag dissolve into the electrolyte system and are recycled as an effective component of the electrolyte. Combined with the capture of fluorides by the waste gas absorption system, the overall recovery rate of fluorides is improved.

[0018] 2. Through the coordinated operation of the solar thermal collection system, the molten salt thermal storage system, and the Stirling unit, as well as the waste heat utilization of the alloy sensible heat recovery system, the cascade utilization of energy and the significant reduction of system energy consumption are achieved. The degraded molten salt produced by electrolysis is introduced into the molten salt thermal storage system and recycled as a thermal storage medium. Combined with the solar thermal collection system, the degraded molten salt is reheated to above 750°C. Part of it is used for power generation by the Stirling unit to provide clean electricity for the electrolysis system, and part of it is fed into the shell-type molten salt electrolysis cell to heat the shell for external heating, reducing direct power consumption. At the same time, the alloy sensible heat recovery system recovers the sensible heat of the Al-Si alloy through an indirect heat exchanger for preheating materials or auxiliary heating of low-temperature molten salt.

[0019] 3. Through the configuration of the central controller and emergency shutdown interlock logic, intelligent control and safe operation of the system are achieved, ensuring the stability and reliability of the process. The central controller prioritizes adjusting the molten salt flow rate of the molten salt heating shell to maintain the electrolysis temperature based on the temperature of the electrolytic cell and the high-temperature molten salt storage tank. When the shell heating is insufficient, resistance wire auxiliary heating is activated to ensure continuous and stable operation of the system under varying solar radiation conditions. Attached Figure Description

[0020] To more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings used in the following description of the embodiments will be briefly introduced. Obviously, the drawings described below are some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0021] Figure 1 This is a system flow diagram of the molten salt electrolytic recycling system for the co-processing of aluminum-silica overhaul slag based on aluminum electrolytic cells proposed in this invention. Figure 2 This is a schematic diagram of the temperature control logic of the electrolytic cell in the molten salt electrolytic recycling system for the co-processing of aluminum-silica overhaul slag based on aluminum electrolytic cells proposed in this invention. Figure 3This is a schematic diagram of the molten salt allocation and scheduling logic in the molten salt electrolytic recycling system for the co-processing of aluminum-silica overhaul slag in aluminum electrolytic cells proposed in this invention. Figure 4 This is a schematic diagram of the material separation and recycling process in the molten salt electrolytic recycling system for the co-processing of aluminum-silica overhaul slag based on aluminum electrolytic cells, as proposed in this invention. Figure 5 This is a schematic diagram of the chemical element content distribution of overhaul slag in the molten salt electrolytic recycling system for the co-processing of aluminum-silica overhaul slag based on aluminum electrolytic cells, as proposed in this invention. Figure 6 This is a curve fitting diagram of the dissolution concentration of aluminum-silica overhaul slag in molten salt under different conditions according to the present invention; Figure 7 (a) and (b) SEM images of aluminosilicate overhaul slag and (c) XRD patterns of overhaul slag, which are the physical and chemical characteristics of the overhaul slag of the present invention. Figure 8 The following are SEM surface scans and elemental distribution diagrams of the electrolysis products of this invention: (a) and (b) respectively. Figure 9 This is a cross-sectional structural diagram of the shell-type molten salt electrolysis system equipment of the present invention.

[0022] Illustration: 1. Exhaust port; 2. Furnace cover; 3. Ceramic fiber furnace chamber; 4. Resistance wire; 5. Furnace barrel; 6. Ceramic fiber base; 7. Thermocouple; 8. Furnace wall; 9. Nut; 10. Air inlet; 11. Feeding and discharging port. Detailed Implementation

[0023] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative and not intended to limit the invention.

[0024] The comprehensive solution for the recycling system is as follows: Reference Figure 1-9 A system for the electrolytic recycling of molten salt in the co-processing of aluminum-silica overhaul slag from aluminum electrolysis cells includes: Solar thermal collection system, molten salt thermal storage system, material and power supply system, shell-type molten salt electrolysis cell system, waste gas absorption and adsorption system, and alloy sensible heat recovery system; The shell-type molten salt electrolysis cell system includes an electrolysis cell body and a molten salt heating shell disposed outside the electrolysis cell body. The molten salt heating shell is connected to the molten salt heat storage system and is used to introduce high-temperature molten salt to provide external heating to the electrolysis cell.

[0025] Molten salt thermal energy storage systems include high-temperature molten salt storage tanks and low-temperature molten salt storage tanks; The high-temperature molten salt storage tank is connected to the solar thermal collection system, the molten salt heating shell of the shell-type molten salt electrolysis cell system, and the Stirling unit, respectively. The low-temperature molten salt storage tank is connected to the discharge end of the shell-type molten salt electrolysis cell system to receive the deteriorated molten salt produced by electrolysis.

[0026] The shell-type molten salt electrolysis cell system is equipped with a molten salt separation device at the discharge end. The molten salt separation device consists of a connecting flange, an Archimedes screw, a filter screen, a shell, a deteriorated molten salt outlet, and an alloy outlet. The outlet of the molten salt separation device is connected to the alloy sensible heat recovery system, the low-temperature molten salt storage tank, and the electrolyte recovery pipeline, respectively.

[0027] The main body of the electrolytic cell is made of ceramic fiber furnace chamber, and the outside is wrapped with resistance wire as auxiliary heating element; The main body of the electrolytic cell is also equipped with a thermocouple interface, an inlet pipe and an outlet pipe, and the outlet pipe is connected to the waste gas absorption and adsorption system.

[0028] The Stirling unit is electrically connected to the material and power supply system to convert the thermal energy of molten salt into electrical energy and provide part of the power to the electrolyzer. The materials and power supply system also includes a grid-connected switching switch, which is used to automatically switch to grid power when the Stirling unit is underpowered.

[0029] The waste gas absorption and adsorption system includes a calcium-based absorption tower. The inlet of the calcium-based absorption tower is connected to the outlet pipeline of the shell-type molten salt electrolysis cell system, and the outlet is connected to the atmosphere via a fan.

[0030] The alloy sensible heat recovery system includes an indirect heat exchanger. The hot side inlet of the indirect heat exchanger is connected to the alloy outlet of the molten salt separation device, and the cold side is connected to the material preheating pipeline or the heating pipeline of the low-temperature molten salt storage tank.

[0031] It also includes a central controller, which is electrically connected to the solar thermal collection system, molten salt thermal storage system, material and power supply system, shell-type molten salt electrolysis cell system, waste gas absorption and adsorption system, and alloy sensible heat recovery system, respectively. The shell-type molten salt electrolysis cell system includes a ceramic fiber base 6, a furnace barrel 5 is installed on the top of the ceramic fiber base 6, and a resistance wire 4 is installed on the outside of the furnace barrel. A furnace cover 2 is set on the top of the furnace barrel 5, and the top periphery of the furnace cover 2 is connected to the furnace wall 8 by nuts 9. A ceramic fiber furnace chamber 3 is set on the inside of the furnace wall 8. A thermocouple 7 is set on the bottom left side of the furnace wall 8. From left to right, an air inlet 10, a material feeding and discharging port 11 and an exhaust port 1 are set on the top of the furnace cover 2. The central controller is configured to: prioritize adjusting the molten salt flow rate of the molten salt heating shell to maintain the electrolysis temperature based on the temperature of the electrolytic cell and the temperature of the high-temperature molten salt storage tank, and activate the resistance wire auxiliary heating when the shell heating is insufficient.

[0032] The central controller is also configured as follows: When the temperature of the high-temperature molten salt storage tank is ≥750℃, molten salt is preferentially allocated to the molten salt heating shell, and the remaining molten salt is allocated to the Stirling unit for power generation. When the temperature of the high-temperature molten salt storage tank is between 650°C and 750°C, reduce the flow rate of the molten salt heating shell and start the resistance wire auxiliary heating, while stopping the Stirling unit. When the temperature of the high-temperature molten salt storage tank is <650℃, the heating shell of the molten salt is shut off, and the electrolytic cell is heated at full power by the resistance wire.

[0033] The central controller is also equipped with emergency stop interlock logic, and the triggering conditions for the emergency stop interlock logic include at least one of the following: Electrolytic cell temperature > 980℃ or < 820℃; Molten salt leakage detection alarm for casing; The furnace internal pressure is >0.2MPa or <-0.08MPa; High-temperature molten salt storage tank temperature > 950℃; The concentration of toxic gases exceeded the standard; Overcurrent or short circuit fault in rectifier cabinet; The circulating cooling water supply was interrupted; When the emergency shutdown interlock logic is triggered, at least one of the following actions shall be performed: cut off the electrolysis power supply, close the shell molten salt inlet valve, open the emergency exhaust pipeline, and start the emergency cooling.

[0034] Degraded molten salt refers to molten salt whose composition deviates from the initial electrolyte composition after electrolytic cycling, resulting in an increased melting point, decreased conductivity, or impurity accumulation. The criteria for determining degraded molten salt are: when the total molar ratio of NaF+AlF3 in the molten salt is below 2.0 or above 2.8, or the carbon content is >1.5%, or the Al2O3 content is >8%, it is considered degraded molten salt and needs to be processed in the purification unit. Composition detection is performed using an X-ray fluorescence spectrometer, sampling and analysis are conducted every 4 hours at the degraded molten salt outlet of the molten salt separation unit.

[0035] The following is a detailed explanation using several embodiments: Example 1: This embodiment provides a system for the electrolytic recycling of molten salt slag from aluminum-silica overhaul slag using an aluminum electrolytic cell. Its specific structure is as follows: The solar thermal collection system uses a parabolic trough concentrator. The heat transfer medium inside the collector tube is a binary molten salt with a ratio of 60% NaNO3 + 40% KNO3. The designed collection temperature is 750℃~850℃. The molten salt thermal storage system includes a high-temperature molten salt storage tank and a low-temperature molten salt storage tank. The tank body is made of high-temperature resistant alloy steel and is covered with an external insulation layer. The high-temperature molten salt storage tank is connected to the outlet of the solar thermal collection system and is also connected to the molten salt heating shell inlet of the shell-type molten salt electrolysis cell and the heating end of the Stirling unit. The low-temperature molten salt storage tank is connected to the degraded molten salt outlet of the molten salt separation device at the discharge end of the shell-type molten salt electrolysis cell.

[0036] The material and power supply system includes a pretreatment unit for overhaul slag, an electrolyte mixing device, a screw feeder, a rectifier transformer, and an electrical control cabinet. The pretreatment unit for overhaul slag can preferably be a jaw crusher, a ball mill, or a screening machine. The rectifier transformer outputs a DC voltage of 0-5V that is adjustable and a rated current of 10kA, which is used to power the electrolytic cell.

[0037] The main body of the electrolytic cell is integrally cast from a high-purity alumina ceramic fiber furnace chamber. A molten salt heating shell is tightly attached to the outside of the main body of the electrolytic cell. The shell is made of heat-resistant stainless steel and has internal guide ribs to ensure uniform flow of molten salt. Resistance wires are also wrapped around the outside of the main body of the electrolytic cell as auxiliary heating elements. The furnace cover and the furnace body are sealed together by flange bolts. The furnace cover is equipped with three thermocouple interfaces, which are used to measure the temperature of the upper, middle and lower layers of molten salt, respectively. There is also an inlet pipe for high-purity nitrogen protection and an outlet pipe for connecting to the waste gas absorption system.

[0038] The waste gas absorption and adsorption system includes a calcium-based absorption tower. The tower body is a carbon steel-lined glass flake anti-corrosion structure. Three spray layers are set inside the tower. The absorbent is limestone slurry with a concentration of 15%. A demister is installed at the top of the tower. The gas outlet pipeline is connected to the inlet of the absorption tower. The outlet of the absorption tower is connected to the chimney via an induced draft fan.

[0039] The alloy sensible heat recovery system includes a plate indirect heat exchanger. The hot side inlet of the heat exchanger is connected to the alloy outlet of the molten salt separation device, and the hot side outlet is connected to the alloy storage tank. The cold side of the heat exchanger is connected to the material preheating pipeline. The alloy sensible heat is used to preheat the pretreated overhaul slag to 200°C before it is sent into the electrolytic cell.

[0040] During system operation, the aluminosilicate overhaul slag is crushed and ball-milled to a particle size ≤200 mesh, then mixed evenly with the recovered electrolyte at a mass ratio of 1:2. This mixture is continuously fed into the shell-type molten salt electrolysis cell by a screw feeder. During the cell startup phase, the temperature inside the cell is first raised to 850℃ by full-power heating with resistance wires. Subsequently, the inlet valve of the molten salt heating shell is opened, introducing molten salt at 780℃ from the high-temperature molten salt storage tank into the shell, with the flow rate controlled at 5 m³ / min. 3The electrolytic cell temperature was maintained between 850℃ and 950℃ per hour, the electrolysis voltage was set to 3.8V, and the current density was 0.8A / cm³. 2 Electrolysis continued for 5 hours.

[0041] After electrolysis is completed, the molten salt separation device is started to push the mixture at the bottom of the tank to the separation chamber. The separated Al-Si alloy is cooled to 200°C by the alloy sensible heat recovery system and then put into the storage tank. Clean electrolyte is returned to the electrolytic cell through the electrolyte recovery pipeline; degraded molten salt at a temperature of about 700°C is temporarily stored in a low-temperature molten salt storage tank. The degraded molten salt in the low-temperature molten salt storage tank is periodically pumped to a solar thermal collection system for reheating to above 780°C and then returned to the high-temperature molten salt storage tank for recycling.

[0042] The anode waste gas generated during the electrolysis process enters the calcium-based absorption tower through the outlet pipeline. After being absorbed by limestone slurry spray, the fluoride concentration in the waste gas decreases from the initial approximately 300 mg / m³. 3 Reduced to 5 mg / m 3 The fluorine-containing sludge discharged from the bottom of the absorption tower via the exhaust fan is regularly cleaned up and sold as raw material for fluoride salt production. Tests showed that this embodiment achieved a 92% aluminum recovery rate, an 85% silicon recovery rate, a 96% comprehensive fluoride recovery rate (combined with electrolyte reuse and waste gas absorption), and a cyanide decomposition rate of >99.9%. Compared with the traditional molten salt electrolysis process, the system's unit product power consumption was reduced by 32%, and carbon emissions were reduced by 28%.

[0043] SEM surface scanning, elemental distribution analysis, and XRD analysis were performed on the Al-Si alloy products obtained by electrolysis. The results showed that the characteristic brightness regions of Al and Si elements were concentrated and had high intensity. XRD detected the Al9Si hypoeutectic alloy phase, proving that SiO2 was successfully reduced and formed a stable alloy with Al. The comparison of alloy element content before and after electrolysis is as follows:

[0044] As shown in the table, the Si content increased from 0.042 wt% to 2.643 wt%, proving that SiO2 in the overhaul slag was efficiently reduced and recovered; the Fe content increased from 0.091 wt% to 0.321 wt%, realizing the resource utilization of impurity components; the contents of trace elements such as Cu, Ga, Zn, and V remained basically unchanged, and impurity elements such as Na and K were not significantly electrolyzed, and did not have an adverse effect on the core components of the alloy.

[0045] The above recovery rate and energy consumption data are averages from 30 continuous electrolysis cycles, each lasting 5 hours. The composition of the raw material, aluminum-silicon overhaul slag, ranges from 45% to 65% Al₂O₃, 15% to 35% SiO₂, 8% to 12% fluoride, and 0.1% to 0.5% cyanide. During the testing period, the aluminum recovery rate remained stable between 90% and 94%, the silicon recovery rate between 83% and 87%, and the overall fluoride recovery rate between 95% and 97%. The unit product power consumption was reduced by 30% to 35% compared to traditional processes. Statistical analysis shows that the confidence interval for the above data is 95%, indicating good consistency and repeatability.

[0046] Additional explanation regarding the shell structure: The molten salt heating shell is welded from heat-resistant stainless steel plates and is cylindrical, tightly covering the outer wall of the electrolytic cell. A 5-10mm annular flow channel is formed between the inner wall of the shell and the outer wall of the electrolytic cell. Six to eight longitudinal guide ribs are evenly distributed circumferentially inside the shell, with the rib height matching the flow channel gap. This divides the flow channel into multiple independent molten salt flow channels, ensuring that the molten salt enters from the bottom inlet and flows evenly upwards along the rib guide direction, exiting from the top outlet. A molten salt inlet pipe is located at the bottom of the shell, and a molten salt outlet pipe is located at the top, connected to the high-temperature molten salt storage tank and the low-temperature molten salt storage tank of the molten salt thermal storage system via flanges, respectively. A high-temperature resistant gasket is used to seal the shell and the electrolytic cell body to prevent molten salt leakage. The high-temperature resistant gasket is made of flexible graphite material.

[0047] Example 2: This embodiment further optimizes the energy scheduling and control logic based on Embodiment 1.

[0048] The system is equipped with a central controller, which can be a Siemens S7-1500 series PLC. It is electrically connected to the solar thermal acquisition system, molten salt thermal storage system, material and power supply system, shell-type molten salt electrolysis cell system, waste gas absorption and adsorption system, and alloy sensible heat recovery system. The central controller has a built-in temperature control module, energy scheduling module, and fault diagnosis module.

[0049] The temperature control module adjusts the opening of the inlet regulating valve of the molten salt heating shell through a PID algorithm based on the deviation between the average temperature T of the three thermocouples in the electrolytic cell and the set value of 900℃. When T < 850℃, prioritize increasing the molten salt flow rate of the shell and sleeve; If the shell flow rate has been adjusted to the maximum and the temperature of the high-temperature molten salt storage tank is ≥750℃, continue to maintain the maximum shell flow rate for heating; If the temperature of the high-temperature molten salt storage tank is <750℃, then the resistance wire auxiliary heating will be started, and the power will be adjusted according to the PID output.

[0050] When T > 950℃, reduce the molten salt flow rate in the shell. If the temperature still exceeds the limit even when the flow rate is reduced to 0, open the shell bypass cooling valve to discharge the molten salt in the shell back to the cryogenic storage tank.

[0051] The energy dispatch module switches operating modes based on the temperature T_h of the high-temperature molten salt storage tank: When T_h≥750℃, the system enters the priority heating and power generation mode: priority is given to meeting the heating demand of the electrolytic cell shell and the remaining molten salt flow is allocated to the Stirling unit for power generation. The output power of the Stirling unit is connected to the grid through the grid-connected switching switch and is given priority to the electrolytic cell. The insufficient part is supplemented by the grid. When 650℃≤T_h<750℃, the system enters the energy-saving and production-preserving mode: at this time, the flow rate of molten salt in the shell is halved, and the resistance wire auxiliary heating is started at the same time. The power of the resistance wire can be adjusted according to actual needs, and the Stirling unit automatically stops. When T_h < 650℃, the system enters the all-electric heating mode: the shell molten salt inlet valve is closed, the resistance wire heats the electrolytic cell at full power (150kW), and all power is provided by the power grid.

[0052] In this embodiment, the system can provide more than 80% of the electricity for electrolysis by solar-Stirling power generation during sunny days, and automatically switch to grid power supply at night or during consecutive cloudy days to ensure the system operates continuously and stably 24 hours a day.

[0053] The above temperature thresholds are set based on the verification results of the dissolution process parameters and thermodynamic calculations. As described in Example 6, the optimal dissolution temperature of SiO2 in molten salt is 960℃, and the operating temperature of the electrolytic cell needs to be maintained between 850℃ and 950℃ to ensure the full dissolution and reduction of Al2O3 and SiO2 in the overhaul slag. When the temperature of the high-temperature molten salt storage tank is ≥750℃, the molten salt has sufficient heat capacity to effectively convert the remaining heat into electrical energy while maintaining the heating of the electrolytic cell shell, and the power generation efficiency of the Stirling unit can reach more than 25%. When the temperature is between 650℃ and 750℃, the heat capacity of the molten salt is insufficient to support the efficient power generation of the Stirling unit, the shell heating capacity decreases, and resistance wire auxiliary heating needs to be started. When the temperature is <650℃, the molten salt can no longer meet the basic heating requirements of the electrolytic cell, and resistance wire heating must be relied upon entirely. The above threshold values ​​were calculated using thermodynamics based on a molten salt specific heat capacity of 1.5 kJ / (kg·K) and an electrolytic cell heat load of approximately 200 kW. Combined with multiple field tests, it was verified that the system has the best energy efficiency and stable operation within this threshold range.

[0054] Example 3: This embodiment, based on embodiment two, further includes a safety interlock and fault diagnosis system.

[0055] The central controller has a built-in emergency stop interlock logic module that monitors the following parameters in real time: 1. Electrolytic cell temperature (average value of three points and the highest value); 2. Condition of the molten salt pressure and leakage detection electrodes in the casing; 3. Furnace internal pressure (pressure transmitter); 4. Temperature of high-temperature molten salt storage tank; 5. Concentration of toxic gases at the outlet of the waste gas absorption tower (HF online analyzer, CO alarm); 6. Rectifier cabinet current, voltage, and protection device status; 7. Cooling water flow switch.

[0056] The central controller will immediately trigger an emergency stop interlock when any of the following conditions are detected: 1. Temperature at any point in the electrolytic cell > 980℃ or average temperature at three points < 820℃; 2. Sudden drop in molten salt pressure in the casing (>0.2MPa / s) or alarm at the leakage detection electrode; 3. The furnace internal pressure is >0.2MPa or <-0.08MPa; 4. The temperature of the high-temperature molten salt storage tank is >950℃; 5. HF concentration at the outlet of the waste gas absorption tower > 20 mg / m³ 3 Or the CO concentration exceeds the standard; 6. The rectifier cabinet trips due to overcurrent (>120% of rated value), overvoltage, or short circuit. 7. Circulating cooling water interrupted (flow switch activated).

[0057] After the interlock is triggered, the central controller automatically performs the following actions: First, a trip command is sent to the rectifier cabinet to cut off the electrolysis power supply; Secondly, close the electric valve at the molten salt inlet of the casing to prevent molten salt from continuing to flow into the casing; Next, open the solenoid valve on the emergency exhaust pipe on the electrolytic cell furnace cover to release the pressure inside the furnace; Immediately afterwards, the emergency cooling water pump (diesel engine driven standby pump) was started to maintain emergency cooling of the electrolytic cell casing and high-temperature tank; Next, an audible and visual alarm is triggered, and fault information is pushed to the central control room and maintenance personnel's mobile phones via industrial Ethernet.

[0058] Finally, after troubleshooting, the operator needs to confirm the system status on-site, that is, confirm the temperature, pressure, leak detection reset, etc., and manually reset the interlock signals on the central controller interface, and restart the system according to the normal startup procedure.

[0059] This embodiment effectively ensures the safety of equipment and personnel under abnormal operating conditions through the above-mentioned safety interlock design, which complies with the safety specifications of the chemical and metallurgical industries.

[0060] Example 4: This embodiment optimizes the alloy sensible heat recovery system based on Embodiment 1.

[0061] The alloy sensible heat recovery system includes two parallel plate heat exchangers, one for direct use and one as a backup. The hot-side inlet of the heat exchanger is connected to the alloy outlet of the molten salt separation device, and the hot-side outlet is connected to the alloy storage tank. A three-way regulating valve is installed on the cold side, which can distribute the waste heat to two branches according to the system requirements: Branch 1 connects to the material preheating pipeline to preheat the pretreated overhaul slag from room temperature to 250°C; Branch 2 connects to the heating coil of the low-temperature molten salt storage tank to assist in heating the low-temperature molten salt and increase its initial temperature when entering the solar collector.

[0062] The central controller automatically adjusts the opening of the three-way valve based on the material preheating demand signal and the temperature of the cryogenic molten salt storage tank. When the temperature of the low-temperature molten salt storage tank is <350℃ and there is no need for material preheating, all the waste heat is used to heat the low-temperature molten salt. When there is a need for material preheating and the temperature of the low-temperature molten salt storage tank is ≥400℃, the waste heat should be used for material preheating first. Under other operating conditions, waste heat is distributed according to a preset ratio.

[0063] The cold-side outlet temperature of the heat exchanger is controlled by adjusting the flow rate of the cooling medium (heat transfer oil) to ensure that the temperature of the alloy outlet heat exchanger is ≤200℃. When the pressure difference between the inlet and outlet of a heat exchanger is >0.3MPa, the system automatically switches to the standby heat exchanger and simultaneously initiates a backflushing procedure to remove blockages.

[0064] This embodiment improves the overall thermal efficiency of the system to 68% through the refined distribution of waste heat, which is about 25 percentage points higher than when there is no waste heat recovery.

[0065] The indirect heat exchanger uses a plate heat exchanger with a heat exchange area of ​​15m². 2 Design heat transfer coefficient ≥ 500 W / (m²) 2 The heat exchanger uses a high-temperature Al-Si alloy as the hot-side medium, with an inlet temperature of approximately 700°C. The cold-side medium is heat transfer oil, with a circulation flow rate of 10 m³ / s. 3 The cold-side outlet is equipped with a three-way regulating valve. A temperature sensor is installed before the valve to measure the alloy outlet temperature. After the valve, it splits into two branches: Branch 1 connects to the material preheater to preheat the pretreated overhaul slag from room temperature to 250℃; Branch 2 connects to the heating coil in the cryogenic molten salt storage tank to assist in heating the cryogenic molten salt. The central controller performs PID regulation based on the material preheating demand signal and the set value of 400℃ for the cryogenic molten salt storage tank. It samples every 30 seconds, and the valve opening step is 5%. When the material temperature is 10℃ lower than the target value, the flow is preferentially allocated to Branch 1.

[0066] Example 5: This embodiment optimizes the recycling of deteriorated molten salt based on Embodiment 1.

[0067] If the deteriorated molten salt in the low-temperature molten salt storage tank is tested for composition and the fluoride content still meets the electrolyte requirements (i.e., the total molar ratio of NaF+AlF3 is between 2.0 and 2.8), it is directly returned to the electrolyzer through the electrolyte recovery pipeline to replenish the electrolyte loss. If the composition deviates, it first enters the molten salt purification unit, which includes a gravity settling tank and a ceramic membrane filter to remove suspended carbon particles and insoluble impurities before being sent to the solar thermal collection system for reheating and circulation.

[0068] Meanwhile, the system is equipped with a new molten salt replenishment tank. When the liquid level in the low-temperature molten salt storage tank is 30% lower than the set value, new molten salt is automatically added. The new molten salt is a mixture of cryolite and sodium fluoride to maintain the stability of the total amount of molten salt in the system.

[0069] This embodiment achieves long-life operation of molten salt, with a single batch of molten salt being recycled ≥50 times, significantly reducing the consumption of new molten salt and the generation of waste salt.

[0070] Example 6: To further verify the adaptability and treatment effect of the system of the present invention on aluminosilicate overhaul slag, this embodiment systematically analyzes the physicochemical properties and key dissolution process parameters of the overhaul slag used.

[0071] refer to Figure 7 As shown, SEM (Scanning Electron Microscopy) analysis of the aluminosilicate overhaul slag particles revealed that the slag is mainly composed of irregular small particles with rough surfaces, sharp edges, and a dense structure. These physical characteristics indicate poor fluidity in electrolytes, necessitating forced conveying methods such as screw feeders in applications. The molten salt separation device and screw feeder used in this invention effectively solve this problem.

[0072] refer to Figure 5 As shown, XRD phase analysis and elemental content determination results indicate that the main phases of the overhaul slag include Al2O3, SiO2, NaF, NaAlF6, and Na3AlF6. Among them, valuable recoverable elements such as O, Al, Si, and Na account for 72%, and F accounts for approximately 2.63%. The remaining trace elements are inherent components of the aluminum electrolyte system, indicating that returning the overhaul slag to the electrolytic cell will not introduce harmful impurities and has high feasibility for resource utilization.

[0073] refer to Figure 6 As shown, this embodiment systematically investigated the effects of four key parameters—mixing ratio, molten salt molecular ratio, temperature, and particle size—on the dissolution performance of SiO2 in overhaul slag, which is characterized by low dissolution rate and easy clogging during feeding. The experimental results show that: When the mass ratio of Na3AlF6 to overhaul slag is 1:1.2 (i.e., the mass ratio of Al2O3 to SiO2 is close to 1:1), the dissolution rate and solubility of SiO2 reach their optimal levels. The molten salt ratio (CR) is positively correlated with the dissolution efficiency, and the dissolution effect is optimal when the CR is 2.7. The dissolution rate and solubility are optimal at a dissolution temperature of 960℃, and the dissolution effect decreases at 1000℃. The dissolution effect is optimal when the particle size of the overhaul residue is controlled between 100 and 200 mesh.

[0074] In summary, the optimal dissolution conditions were determined to be: a dissolution temperature of 960℃, a molten salt molecular ratio of 2.7, a Na3AlF6 to overhaul slag mixing ratio of 1:1.2, and a particle size of 100–200 mesh. Under these conditions, the dissolution rate of the aluminosilicate overhaul slag was significantly improved, the saturated solubility increased by 3 wt%, and the dissolution time was controlled to approximately 5 minutes. This embodiment verifies the operational adaptability of the system of the present invention under the above process parameters, providing data support for the continuous and stable operation of the system. The basic principles, main features, and advantages of the present invention have been shown and described above. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The embodiments and descriptions in the specification are merely the principles of the present invention. Various changes and modifications can be made to the present invention without departing from its spirit and scope, and all such changes and modifications fall within the scope of the present invention as claimed. The scope of protection claimed by the present invention is defined by the appended claims and their equivalents.

Claims

1. A system for the electrolytic recycling of molten salt in the co-processing of aluminum-silica overhaul slag using aluminum electrolytic cells, characterized in that, include: Solar thermal collection system, molten salt thermal storage system, material and power supply system, shell-type molten salt electrolysis cell system, waste gas absorption and adsorption system, and alloy sensible heat recovery system; The shell-type molten salt electrolysis cell system includes an electrolysis cell body and a molten salt heating shell disposed outside the electrolysis cell body. The molten salt heating shell is connected to the molten salt heat storage system and is used to introduce high-temperature molten salt to provide external heating to the electrolysis cell.

2. The molten salt electrolytic recycling system for co-processing aluminum-silica overhaul slag based on aluminum electrolytic cells according to claim 1, characterized in that, The molten salt thermal storage system includes a high-temperature molten salt storage tank and a low-temperature molten salt storage tank; The high-temperature molten salt storage tank is connected to the solar thermal collection system, the molten salt heating shell of the shell-type molten salt electrolysis cell system, and the Stirling unit, respectively. The low-temperature molten salt storage tank is connected to the discharge end of the shell-type molten salt electrolysis cell system and is used to receive the degraded molten salt produced by electrolysis.

3. The molten salt electrolytic recycling system for co-processing aluminum-silica overhaul slag based on aluminum electrolytic cells according to claim 2, characterized in that, The shell-type molten salt electrolysis cell system is equipped with an Archimedes screw separator at the discharge end. The outlet of the Archimedes screw separator is connected to the alloy sensible heat recovery system, the low-temperature molten salt storage tank, and the electrolyte recovery pipeline.

4. The molten salt electrolytic recycling system for co-processing aluminum-silica overhaul slag based on aluminum electrolytic cells according to claim 1, characterized in that, The main body of the electrolytic cell is made of ceramic fiber furnace chamber, and the outside is wrapped with resistance wire as an auxiliary heating element; The main body of the electrolytic cell is also provided with a thermocouple interface, an inlet pipe and an outlet pipe, and the outlet pipe is connected to the waste gas absorption and adsorption system.

5. The molten salt electrolytic recycling system for co-processing aluminum-silica overhaul slag based on aluminum electrolytic cells according to claim 2, characterized in that, The Stirling unit is electrically connected to the material and power supply system, and is used to convert the thermal energy of molten salt into electrical energy and provide part of the power to the electrolytic cell. The material and power supply system also includes a grid-connected switching switch, which is used to automatically switch to grid power supply when the Stirling unit's power supply is insufficient.

6. The molten salt electrolytic recycling system for co-processing aluminum-silica overhaul slag based on aluminum electrolytic cells according to claim 1, characterized in that, The waste gas absorption and adsorption system includes a calcium-based absorption tower. The inlet of the calcium-based absorption tower is connected to the gas outlet pipeline of the shell-type molten salt electrolysis cell system, and the outlet is connected to the atmosphere via a fan.

7. The molten salt electrolytic recycling system for co-processing aluminum-silica overhaul slag based on aluminum electrolytic cells according to claim 1, characterized in that, The alloy sensible heat recovery system includes an indirect heat exchanger, the hot side inlet of which is connected to the alloy outlet of the Archimedes screw separator, and the cold side is connected to the material preheating pipeline or the heating pipeline of the low-temperature molten salt storage tank.

8. The molten salt electrolytic recycling system for co-processing aluminum-silica overhaul slag based on aluminum electrolytic cells according to claim 1, characterized in that, It also includes a central controller, which is electrically connected to the solar thermal acquisition system, the molten salt thermal storage system, the material and power supply system, the shell-type molten salt electrolysis cell system, the waste gas absorption and adsorption system, and the alloy sensible heat recovery system, respectively. The shell-type molten salt electrolysis cell system includes a ceramic fiber base (6), a furnace barrel (5) is installed on the top of the ceramic fiber base (6), and a resistance wire (4) is installed on the outside of the furnace barrel. A furnace cover (2) is provided on the top of the furnace barrel (5), and the top periphery of the furnace cover (2) is connected to the furnace wall (8) by a nut (9). A ceramic fiber furnace chamber (3) is provided on the inside of the furnace wall (8). A thermocouple (7) is provided at the bottom left side of the furnace wall (8). An air inlet (10), a material feeding and discharging port (11) and an exhaust port (1) are arranged sequentially from left to right on the top of the furnace cover (2). The central controller is configured to: prioritize adjusting the molten salt flow rate of the molten salt heating shell to maintain the electrolysis temperature based on the temperature of the electrolytic cell and the temperature of the high-temperature molten salt storage tank, and activate resistance wire auxiliary heating when the shell heating is insufficient.

9. The molten salt electrolytic recycling system for co-processing aluminum-silica overhaul slag based on aluminum electrolytic cells according to claim 8, characterized in that, The central controller is also configured to: When the temperature of the high-temperature molten salt storage tank is ≥750℃, molten salt is preferentially allocated to the molten salt heating shell, and the remaining molten salt is allocated to the Stirling unit for power generation. When the temperature of the high-temperature molten salt storage tank is between 650°C and 750°C, reduce the flow rate of the molten salt heating shell and start the resistance wire auxiliary heating, while stopping the Stirling unit. When the temperature of the high-temperature molten salt storage tank is <650℃, the heating shell of the molten salt is shut off, and the electrolytic cell is heated at full power by the resistance wire.

10. The molten salt electrolytic recycling system for co-processing aluminum-silica overhaul slag based on aluminum electrolytic cells according to claim 8, characterized in that, The central controller is also configured with emergency stop interlock logic, and the triggering conditions of the emergency stop interlock logic include at least one of the following: Electrolytic cell temperature > 980℃ or < 820℃; Molten salt leakage detection alarm for casing; The furnace internal pressure is >0.2MPa or <-0.08MPa; High-temperature molten salt storage tank temperature > 950℃; The concentration of toxic gases exceeded the standard; Overcurrent or short circuit fault in rectifier cabinet; The circulating cooling water supply was interrupted; When the emergency shutdown interlock logic is triggered, at least one of the following actions is performed: cutting off the electrolysis power supply, closing the shell molten salt inlet valve, opening the emergency exhaust pipeline, and starting emergency cooling.