A wind- and earthquake-resistant self-damping concrete utility pole and its vibration-damping base
By introducing a self-damping design into concrete utility poles, and utilizing damping components and self-healing components, the problem of microcrack propagation in the pole body under alternating loads was solved, achieving effective vibration energy dissipation and improved structural durability.
Patent Information
- Application Number
- CN202611462226.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-20
- Publication Date
- 2026-11-17
AI Technical Summary
Existing concrete utility poles are prone to developing microcracks inside the pole body under long-term exposure to alternating wind vibrations and seismic loads. These cracks continue to expand, leading to pole cracking and stiffness reduction. Furthermore, existing damping components are complex to assemble or have limited vibration reduction effects.
The design of the self-damping concrete utility pole utilizes damping components welded to the surface of the reinforcing cage assembly. This allows for the dissipation of vibrational energy through the controllable micro-slip friction between the damping elastic particles and the cement stone interface, as well as the hybrid reinforcing fibers. Furthermore, the design repairs micro-cracks through self-healing components. Combined with multiple damping units arranged in segments along the pole height, the design achieves a synergistic effect between the intrinsic damping of the material and the damping of the pre-embedded structure.
It effectively dissipates vibration energy, reduces fatigue damage to the base material, improves the wind and earthquake resistance of utility poles, extends service life, and simplifies the assembly process of damping components.
Smart Images

Figure CN123109451A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of concrete utility pole technology, and in particular to a wind- and earthquake-resistant self-damping concrete utility pole and its shock-absorbing base. Background Technology
[0002] Concrete utility poles are widely used load-bearing structures for power transmission and distribution lines. They are extensively used in outdoor environments and are subjected to alternating wind vibrations and repeated earthquake loads over a long period of time. Under the continuous action of alternating loads, the concrete pole body is repeatedly bent, and micro-cracks are prone to appear inside the pole body. As the cracks continue to expand, they will cause the pole body to crack and its stiffness to decrease. In severe cases, pole breakage and collapse will occur, threatening the safe operation of the power grid.
[0003] The existing technical approaches to improving the wind and earthquake resistance of concrete utility poles are mainly divided into two categories: The first category is simple structural improvement, which increases the bending capacity of the utility pole by increasing the cross-section of the pole, improving the strength grade of concrete, and increasing the amount of reinforcement. This method only improves the static load-bearing capacity of the component. However, ordinary cement concrete has a low damping loss factor, and the vibration energy cannot be effectively dissipated after vibration occurs. Alternating stress will continue to accumulate in the pole, and the risk of fatigue cracking remains prominent. At the same time, increasing the cross-section will significantly increase the material cost and the self-weight of the component.
[0004] The second category involves adding external or internal damping components, relying on friction damping and tuned mass damping to dissipate vibration energy. Most existing damping components are assembled later, requiring insertion into the hollow cavity from the pole end after the pole is formed. On the one hand, the deformation of damping components is very small under wind vibration conditions with small to medium amplitude, resulting in limited vibration reduction effect. On the other hand, the later-assembled damping components have the drawback of complex assembly process. Summary of the Invention
[0005] The purpose of this invention is to provide a wind- and earthquake-resistant self-damping concrete utility pole and its vibration-damping base, which solves the problem that existing utility poles are subjected to alternating wind vibration and earthquake loads over a long period of time; under the continuous action of alternating loads, the concrete pole body is repeatedly bent, and micro-cracks are easily generated inside the pole body. The continuous expansion of cracks will cause the pole body to crack and the stiffness to decrease.
[0006] To achieve the above objectives, the present invention provides a wind- and earthquake-resistant self-damping concrete utility pole, comprising a steel cage assembly, a damping assembly, and a pole body cast from concrete material, wherein the damping assembly is welded onto the surface of the steel cage assembly. The concrete material is made from the following raw materials in parts by weight: It includes 128-140 parts of cementitious material, which is composed of 100 parts of silicate cement and 28-40 parts of mineral admixture; it also includes 130-160 parts of river sand, 205-245 parts of crushed stone, 8-16 parts of damping elastic particles, 6-12 parts of mixed reinforcing fibers, 2-4 parts of self-healing component, 2.5-5.5 parts of functional additives, 0.05-0.15 parts of thickening stabilizer, and 39-47 parts of water; The hybrid reinforcing fiber comprises steel fiber and PVA synthetic fiber, with a mass ratio of steel fiber to PVA synthetic fiber of (2-3):1; the self-healing component is compounded from hydrated calcium silicate seed crystals and ettringite-type expansion component in a mass ratio of (1-2):1, wherein the ettringite-type expansion component accounts for 3%-6% of the total mass of the cementitious material; the concrete material dissipates vibration energy by undergoing controllable micro-slip friction under cyclic loading through the interface between damping elastic particles and cement paste, and the interface between the hybrid reinforcing fiber and the matrix.
[0007] Preferably, the river sand is the net amount after deducting the volume substitution of damping elastic particles, with a fineness modulus of 2.4-3.0 and a mud content of ≤1.5%; the crushed stone has a continuous gradation of 5-13mm, a needle-like and flaky content of ≤8%, and a crushing index of ≤12%; the damping elastic particles are surface-modified EPDM rubber particles, with an ethylene content of 50%-60%, an ethylene-based norbornene third monomer content of 2%-5%, a Shore A hardness of 58-72, and a density of 0.86-0.92 g / cm³. 3 The surface is coated with a silane-modified layer with a thickness of 5-15 μm, which is formed by coating with silane coupling agent KH-550 or KH-560 after hydrolysis; the damping elastic particles include 60%-75% coarse particles with a particle size of 0.6-1.2 mm and 25%-40% fine particles with a particle size of 0.3-0.6 mm by mass percentage; the mineral admixture is a mixture of ultrafine mineral powder and silica fume in a mass ratio of (4-6):1, or a mixture of ultrafine mineral powder, silica fume and Class I fly ash, wherein Class I fly ash accounts for 20%-30% of the total amount of mineral admixture.
[0008] Preferably, the specific surface area of the ultrafine mineral powder is ≥450m². 2 / kg, 7-day activity index ≥75%; the silica fume has a SiO2 mass fraction ≥92% and a specific surface area ≥15000m². 2 / kg; the fineness of the Class I fly ash is ≤12%, and the water requirement ratio is ≤95%; the river sand is Class II graded medium sand, and the crushed stone is a continuous graded mixture of 5-10mm and 10-13mm grades in a mass ratio of (3-4):(6-7).
[0009] Preferably, the steel fiber is a hook-shaped steel fiber with a length of 12-18 mm, a diameter of 0.2-0.4 mm, an aspect ratio of 40-60, and a tensile strength ≥1000 MPa; the PVA synthetic fiber has a length of 6-12 mm, a diameter of 15-30 μm, and a breaking elongation of 6%-8%; basalt fiber may also be incorporated into the hybrid reinforcing fiber, with basalt fiber accounting for 10%-20% of the total mass of the hybrid reinforcing fiber, and the basalt fiber has a length of 12-18 mm and a diameter of 13-17 μm.
[0010] Preferably, the hydrated calcium silicate seed crystals have a Ca / Si molar ratio of 0.8-1.2 and a particle size of 5-20 μm, and are commercially available nanocrystalline seed additives; the ettringite-type expansion component is a calcium sulfoaluminate-calcium oxide expansion agent with a fineness ≤5% and a 7-day restricted expansion rate in water of 0.025%-0.050%; the self-healing component may also contain 5%-10% sodium carbonate activator by mass of the self-healing component.
[0011] Preferably, the functional admixture comprises a polycarboxylate-based high-efficiency water-reducing agent, a retarding component, an defoamer, and an amino alcohol-based steel reinforcement corrosion inhibitor; the polycarboxylate-based high-efficiency water-reducing agent has a water reduction rate ≥30% and is added at a dosage of 1.0%-1.8% of the total mass of the cementitious material; the retarding component is sodium gluconate or citric acid, and is added at a dosage of 0.05%-0.15% of the total mass of the cementitious material; the defoamer is an organosilicon defoamer, and is added at a dosage of 0.02%-0.08% of the total mass of the cementitious material; the amino alcohol-based steel reinforcement corrosion inhibitor is dimethylethanolamine or an amino alcohol complex salt, and is added at a dosage of 0.5%-1.0% of the total mass of the cementitious material; the thickening and stabilizing agent is hydroxypropyl methylcellulose with a viscosity specification of 40000-100000 mPa·s.
[0012] Preferably, the utility pole is a hollow cone shape, cast from concrete, with a wall thickness of 40-70mm. The steel cage assembly includes a lower base, an upper base, and a steel cage. The steel cage is connected between the lower base and the upper base, and the steel cage is bound to the surface of the steel cage.
[0013] Preferably, the damping assembly includes symmetrically arranged flanges and annular high-damping manganese-copper alloy sheets. The annular high-damping manganese-copper alloy sheets are alternately stacked between the two flanges. Each annular high-damping manganese-copper alloy sheet has a thickness of 1.5-2.5 mm, a Mn mass fraction of 60%-70%, a Cu mass fraction of 20%-30%, and the balance being Fe, Ni, and Al. The flanges are welded to the reinforcing steel frame to clamp the annular high-damping manganese-copper alloy sheets. An annular high-damping rubber pad is filled between adjacent annular high-damping manganese-copper alloy sheets. The annular high-damping rubber pad is made of polyurethane damping adhesive or asphalt-based damping paste, with a thickness of 0.8-1.5 mm and a Shore A hardness of 55-70. Several anchors are welded to the surface of the outermost annular high-damping manganese-copper alloy sheet. The anchoring bars are 5-15mm long and are embedded in the concrete to enhance mechanical bonding with the concrete. Multiple sets of damping components are arranged in sections along the pole's height, including a lower damping unit group and an upper damping unit group. The lower damping unit group is located in the lower 1 / 3 of the pole's height area, with a unit length of 400-500mm, a diameter of 60-80mm, and 8-12 layers, designed to dissipate energy from seismic reciprocating loads. The upper damping unit group is located in the upper 1 / 3 of the pole's height area, with a unit length of 200-300mm, a diameter of 40-60mm, and 4-6 layers, designed to dissipate energy from wind-induced reciprocating vibrations. The damping components are axially aligned with the pole's axis and radially located in the middle layer of the wall thickness, with a concrete protective layer thickness ≥15mm.
[0014] Preferably, the manufacturing process of the utility pole includes the following steps: S1. Prefabrication of the main body of the utility pole: The steel frame is fixed between the lower base and the upper base. The annular high-damping manganese copper alloy sheet and the annular high-damping rubber pad are alternately stacked and clamped and fixed by the flanges on both sides. The steel frame is then welded to the surface of the steel frame by the flanges. Finally, the steel cage is welded to the surface of the steel frame. S2. Mold assembly and concrete pouring: Place the tied pole body into the centrifugal mold and close the mold; pour concrete material using a three-speed centrifugal system: low speed 250-300 r / min for 2-3 minutes, medium speed 600-700 r / min for 3-4 minutes, and high speed 900-1100 r / min for 6-8 minutes. Under the action of centrifugal force, the concrete material densely wraps the pole body. S3. Curing and demolding: Static pre-curing for 2-4 hours, steam curing at 65-80℃ for 8-12 hours, and natural wet curing for 7-14 days after demolding.
[0015] A shock-absorbing base for a wind-resistant and earthquake-resistant self-damping concrete utility pole, wherein the shock-absorbing base is applicable to any one of the wind-resistant and earthquake-resistant self-damping concrete utility poles described herein, and the utility pole is installed on the shock-absorbing base for limiting and fixing the lower base.
[0016] The advantages and positive effects of the wind-resistant and earthquake-resistant self-damping concrete utility pole and its shock-absorbing base described in this invention are as follows: 1. This invention uses silane-modified EPDM rubber damping elastic particles to replace part of the river sand by volume; the silane-modified layer constructs a controllable interface between the rubber particles and cement stone; under cyclic loads, the interface undergoes controllable micro-slip friction to dissipate vibration energy; EPDM rubber is resistant to aging in high-alkali environments of concrete, and its batch performance is stable; combined with ultrafine mineral powder-silica fume compound mineral admixtures, it compensates for the strength loss caused by the elastic particles, and the composite material meets the strength grade requirements of C50 and above for concrete poles. Under small to medium wind vibration and small to medium earthquake conditions, most of the vibration energy can be dissipated by the material itself, reducing fatigue damage to the matrix.
[0017] 2. In this invention, the damping components are directly welded and fixed to the steel cage components and centrifugally cast together with the concrete. The damping components rely on the flanges on both sides to clamp the annular manganese copper alloy sheet and the rubber pad to form a friction pair. Multiple damping units are arranged in segments along the height of the pole. The lower unit is for energy dissipation of large bending moments during earthquakes, and the upper unit is for energy dissipation of high-frequency wind vibrations during strong winds. The intrinsic damping of the material and the damping of the pre-embedded structure work together to further dissipate vibration energy under extreme conditions of large amplitude.
[0018] 3. The present invention combines hydrated calcium silicate seed crystals and ettringite-type expansion components as self-healing components; when microcracks with a width ≤0.2mm are generated in the pole body, and environmental moisture enters the cracks, the CSH seed crystals induce secondary hydration of unhydrated cement, and the ettringite expansion components fill the cracks, realizing the self-repair of microcracks, blocking the channels for water and chloride ion erosion, delaying steel corrosion, and improving the service life of the utility pole throughout its entire life cycle.
[0019] The technical solution of the present invention will be further described in detail below with reference to the accompanying drawings and embodiments. Attached Figure Description
[0020] Figure 1 A frontal perspective view provided for an embodiment of the present invention; Figure 2 A perspective view of a flange provided for an embodiment of the present invention; Figure 3 A cross-sectional view of a ring-shaped high-damping manganese-copper alloy sheet provided for an embodiment of the present invention; Figure 4 A process flow diagram provided for embodiments of the present invention.
[0021] Figure Labels 1. Reinforcing cage assembly; 11. Lower base; 12. Upper base; 13. Reinforcing steel skeleton; 14. Reinforcing steel cage; 2. Damping assembly; 21. Flange; 22. Annular high-damping manganese-copper alloy sheet; 23. Annular high-damping rubber pad; 24. Anchor bar. Detailed Implementation
[0022] In this application, unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application pertains. In case of any inconsistency, the meaning set forth in this specification or derived from the content described herein shall prevail. Furthermore, the terminology used herein is for the purpose of describing embodiments of this application only and is not intended to limit the scope of this application.
[0023] The embodiments of the present invention will be described in detail below with reference to examples.
[0024] Reference Figures 1-4 As shown, the present invention provides a technical solution: a wind-resistant and earthquake-resistant self-damping concrete utility pole, comprising a reinforcing cage assembly 1, a damping assembly 2, and a pole body cast from concrete. The damping assembly 2 is welded onto the surface of the reinforcing cage assembly 1. The utility pole is in the shape of a hollow cone, cast from concrete, with a wall thickness of 40-70mm. The reinforcing cage assembly 1 includes a lower base 11, an upper base 12, and a reinforcing cage 13. The reinforcing cage 13 is connected between the lower base 11 and the upper base 12, and a reinforcing cage 14 is bound to the surface of the reinforcing cage 13.
[0025] Reference Figures 1-4As shown, the damping component 2 includes symmetrically arranged flanges 21 and annular high-damping manganese-copper alloy sheets 22. The annular high-damping manganese-copper alloy sheets 22 are alternately stacked between the two flanges 21. The thickness of a single annular high-damping manganese-copper alloy sheet 22 is 1.5-2.5 mm, with a Mn mass fraction of 60%-70%, a Cu mass fraction of 20%-30%, and the balance being Fe, Ni, and Al. The flanges 21 are welded to the steel frame 13 to clamp the annular high-damping manganese-copper alloy sheets 22. An annular high-damping rubber pad 23 is filled between adjacent annular high-damping manganese-copper alloy sheets 22. The annular high-damping rubber pad 23 is made of polyurethane damping adhesive or asphalt-based damping paste, with a thickness of 0.8-1.5 mm and a Shore A hardness of 55-70. The outermost annular high-damping manganese-copper alloy sheet 22 is welded to the surface. Several anchor bars 24 are attached, each 5-15mm long, and are embedded in the concrete material to enhance mechanical bonding with it. Multiple damping components 2 are arranged in sections along the pole's height, including a lower damping unit group and an upper damping unit group. The lower damping unit group is located in the lower 1 / 3 height region of the pole, with a unit length of 400-500mm, a diameter of 60-80mm, and 8-12 laminated layers, designed to dissipate energy from seismic reciprocating loads. The upper damping unit group is located in the upper 1 / 3 height region of the pole, with a unit length of 200-300mm, a diameter of 40-60mm, and 4-6 laminated layers, designed to dissipate energy from wind reciprocating vibrations. The damping component 2 is axially aligned with the pole's axis and radially located in the middle layer of the wall thickness, with a concrete protective layer thickness ≥15mm.
[0026] The concrete material is made from the following raw materials in parts by weight: 128-140 parts of cementitious material, which consists of 100 parts of silicate cement and 28-40 parts of mineral admixtures; it also includes 130-160 parts of river sand, 205-245 parts of crushed stone, 8-16 parts of damping elastic particles, 6-12 parts of mixed reinforcing fibers, 2-4 parts of self-healing component, 2.5-5.5 parts of functional admixture, 0.05-0.15 parts of thickening stabilizer, and 39-47 parts of water. The hybrid reinforcing fiber contains steel fiber and PVA synthetic fiber, with a mass ratio of steel fiber to PVA synthetic fiber of (2-3):1; the self-healing component is a compound of hydrated calcium silicate seed crystals and ettringite-type expansion component in a mass ratio of (1-2):1, wherein the ettringite-type expansion component accounts for 3%-6% of the total mass of the cementitious material; the concrete material dissipates vibration energy by undergoing controllable micro-slip friction under cyclic loading through the interface between the damping elastic particles and cement paste, and the interface between the hybrid reinforcing fiber and the matrix.
[0027] The river sand is the net amount after deducting the volume substitution of damping elastic particles, with a fineness modulus of 2.4-3.0 and a mud content of ≤1.5%; the crushed stone is a continuous gradation of 5-13mm, with a needle-like and flaky content of ≤8% and a crushing index of ≤12%; the damping elastic particles are surface-modified EPDM rubber particles, with an ethylene content of 50%-60%, an ethylene-based norbornene third monomer content of 2%-5%, a Shore A hardness of 58-72, and a density of 0.86-0.92 g / cm³. 3 The surface is coated with a silane-modified layer with a thickness of 5-15 μm, which is formed by coating after hydrolysis of silane coupling agent KH-550 or KH-560; the damping elastic particles include 60%-75% coarse particles with a particle size of 0.6-1.2 mm and 25%-40% fine particles with a particle size of 0.3-0.6 mm by mass percentage; the mineral admixture is a mixture of ultrafine mineral powder and silica fume in a mass ratio of (4-6):1, or a mixture of ultrafine mineral powder, silica fume and Class I fly ash, wherein Class I fly ash accounts for 20%-30% of the total amount of mineral admixture.
[0028] The specific surface area of ultrafine mineral powder is ≥450m². 2 / kg, 7-day activity index ≥75%; SiO2 mass fraction of silica fume ≥92%, specific surface area ≥15000m² 2 / kg; Grade I fly ash fineness ≤12%, water requirement ratio ≤95%; River sand is Zone II graded medium sand, and crushed stone is a continuous gradation formed by mixing two grades of 5-10mm and 10-13mm in a mass ratio of (3-4):(6-7).
[0029] The steel fibers are hook-shaped, with a length of 12-18 mm, a diameter of 0.2-0.4 mm, an aspect ratio of 40-60, and a tensile strength ≥1000 MPa; the PVA synthetic fibers are 6-12 mm long, 15-30 μm in diameter, and have a breaking elongation of 6%-8%; basalt fibers can also be incorporated into the hybrid reinforcing fibers, accounting for 10%-20% of the total mass of the hybrid reinforcing fibers, with a length of 12-18 mm and a diameter of 13-17 μm.
[0030] The Ca / Si molar ratio of the hydrated calcium silicate seed crystals is 0.8-1.2, and the particle size is 5-20 μm. It is a commercially available nanocrystalline seed additive. The ettringite-type expansion component is a calcium sulfoaluminate-calcium oxide expansion agent with a fineness ≤5% and a 7-day restricted expansion rate in water of 0.025%-0.050%. The self-healing component may also contain 5%-10% sodium carbonate activator by mass of the total self-healing component.
[0031] The functional admixtures include polycarboxylate-based high-efficiency water-reducing agents, retarding components, defoamers, and amino alcohol-based steel reinforcement corrosion inhibitors. The polycarboxylate-based high-efficiency water-reducing agent has a water reduction rate of ≥30% and is added at a dosage of 1.0%-1.8% of the total mass of the cementitious materials. The retarding component is sodium gluconate or citric acid, and is added at a dosage of 0.05%-0.15% of the total mass of the cementitious materials. The defoamer is an organosilicon defoamer, and is added at a dosage of 0.02%-0.08% of the total mass of the cementitious materials. The amino alcohol-based steel reinforcement corrosion inhibitor is dimethylethanolamine or amino alcohol complex salt, and is added at a dosage of 0.5%-1.0% of the total mass of the cementitious materials. The thickening and stabilizing agent is hydroxypropyl methylcellulose with a viscosity specification of 40,000-100,000 mPa·s.
[0032] The manufacturing process of utility poles includes the following steps: S1. Prefabrication of the main body of the utility pole: The steel frame 13 is fixed between the lower base 11 and the upper base 12. The annular high-damping manganese copper alloy sheet 22 and the annular high-damping rubber pad 23 are alternately stacked and clamped and fixed by the flanges 21 on both sides. The steel frame 13 is welded and fixed by the flanges 21. Finally, the steel cage 14 is welded to the surface of the steel frame 13. S2. Mold assembly and concrete pouring: Place the tied pole body into the centrifugal mold and close the mold; pour concrete material using a three-speed centrifugal system: low speed 250-300 r / min for 2-3 minutes, medium speed 600-700 r / min for 3-4 minutes, and high speed 900-1100 r / min for 6-8 minutes. Under the action of centrifugal force, the concrete material densely wraps the pole body. S3. Curing and demolding: Static pre-curing for 2-4 hours, steam curing at 65-80℃ for 8-12 hours, and natural wet curing for 7-14 days after demolding.
[0033] A shock-absorbing base for a wind-resistant and earthquake-resistant self-damping concrete utility pole, the shock-absorbing base being applicable to any one of the wind-resistant and earthquake-resistant self-damping concrete utility poles, the utility pole being installed on the shock-absorbing base for limiting and fixing the lower base 11.
[0034] Example 1 A wind- and earthquake-resistant self-damping concrete utility pole comprises the following materials per cubic meter of concrete: 440 kg of silicate cement; 125 kg of mineral admixtures, including 100 kg of ultrafine mineral powder and 25 kg of silica fume in a mass ratio of 4:1; 620 kg of river sand; 1030 kg of crushed stone, a continuous gradation of 5-10 mm and 10-13 mm aggregates mixed in a mass ratio of 3.5:6.5; 40 kg of damping elastic particles; 36 kg of hybrid reinforcing fibers, including 26 kg of steel fibers and 10 kg of PVA fibers in a mass ratio of 2.6:1; and a self-healing component. 14 kg of cementitious material, including 9 kg of hydrated calcium silicate seed crystals and 5 kg of ettringite-type expansion component, with a mass ratio of 1.8:1 and the expansion component accounting for 3.0% of the cementitious material; 13 kg of functional admixtures, including 7.3 kg of polycarboxylate superplasticizer, accounting for 1.3% of the total mass of the cementitious material, 4.5 kg of dimethyl ethanolamine rust inhibitor, accounting for 0.8% of the total mass of the cementitious material, 0.5 kg of sodium gluconate, and 0.7 kg of organosilicon defoamer; 0.5 kg of thickening and stabilizing agent hydroxypropyl methylcellulose; 175 kg of water; the water-cement ratio is 0.31, and the sand ratio is 37.6%.
[0035] The damping elastic particles are surface-modified EPDM rubber particles with 55% ethylene content, 3.5% ethylene-methylnorbornene content, a Shore A hardness of 65, and a density of 0.89 g / cm³. 3 The silane-modified layer is 10 μm thick and is formed by hydrolysis and coating with KH-550 silane coupling agent; the damping elastic particles consist of 65% coarse particles with a particle size of 0.6-1.2 mm and 35% fine particles with a particle size of 0.3-0.6 mm by mass, and the ultrafine mineral powder has a specific surface area of 480 m². 2 / kg, 7-day activity index 80%; silica fume SiO2 content 94%, specific surface area 18000m² 2 / kg; River sand is zone II graded medium sand with a fineness modulus of 2.6 and a mud content of 1.0%; Crushed stone crushing index is 10%, and needle-like and flaky content is 6%. Steel fibers are hook-shaped, 15mm long, 0.3mm in diameter, with an aspect ratio of 50 and a tensile strength of 1200MPa; PVA fibers are 9mm long, 22μm in diameter, and have an elongation at break of 7%; Hydrated calcium silicate seed crystals have a Ca / Si molar ratio of 0.8-1.2 and a particle size of 10μm, and are commercially available nanocrystalline seed additives; Erythrite-type expanding agent has a fineness of 3% and a 7-day restricted expansion rate of 0.035% in water; Polycarboxylate superplasticizer has a water reduction rate of 32%; Hydroxypropyl methylcellulose has a viscosity specification of 60000mPa·s.
[0036] Concrete pole structure: The hollow cone-shaped pole has a wall thickness of 55mm and is cast from the above-mentioned concrete material; multiple damping components 2 are arranged in sections along the height of the pole. The lower damping unit group is arranged in the lower 1 / 3 height of the pole, with a unit length of 450mm, a diameter of 70mm, and 10 layers of laminated plates; the upper damping unit group is arranged in the upper 1 / 3 height of the pole, with a unit length of 250mm, a diameter of 50mm, and 5 layers of laminated plates; each damping unit is axially along the pole axis, circumferentially uniform and symmetrical, and radially located in the middle layer of the cylinder wall, with a protective layer thickness of 20mm; Damping component 2 structure: the anchor bar 24 is 10mm long; the annular high-damping manganese-copper alloy sheet 22 is 2.0mm thick, with a Mn mass fraction of 65% and a Cu mass fraction of 25%; the annular high-damping rubber pad layer 23 is 1.2mm thick and has a Shore A hardness of 62.
[0037] The manufacturing process of utility poles includes the following steps: S1. Prefabrication of the main body of the utility pole: The steel frame 13 is fixed between the lower base 11 and the upper base 12. The annular high-damping manganese copper alloy sheet 22 and the annular high-damping rubber pad 23 are alternately stacked and clamped and fixed by the flanges 21 on both sides. The steel frame 13 is welded and fixed by the flanges 21. Finally, the steel cage 14 is welded to the surface of the steel frame 13. S2. Mold Assembly and Concrete Pouring: Place the tied-up main body of the utility pole into the centrifugal mold and close the mold; pour concrete material. The concrete material preparation method is as follows: dry mix silicate cement, mineral admixtures, and self-healing components for 1.5 min, add damping elastic particles and mixed reinforcing fibers and mix for 1.5 min, add river sand and crushed stone and dry mix for 1.5 min, add water containing functional admixtures and thickening stabilizers and stir for 4 min; then use a three-speed centrifugal system: low speed 280 r / min for 2.5 min, medium speed 650 r / min for 3.5 min, and high speed 1000 r / min for 7 min. Under the action of centrifugal force, the concrete material densely wraps the main body of the utility pole; S3. Curing and demolding: Static pre-curing for 3 hours, steam curing at 72℃ for 10 hours, and natural wet curing for 10 days after demolding.
[0038] Example 2 A wind- and earthquake-resistant self-damping concrete utility pole comprises the following materials per cubic meter of concrete: 450 kg of silicate cement; 130 kg of mineral admixtures, including 105 kg of ultrafine mineral powder, 25 kg of silica fume, and 640 kg of river sand; 1050 kg of crushed stone; 38 kg of damping elastic particles; 28 kg of mixed reinforcing fibers, including 20 kg of steel fibers and 8 kg of PVA fibers; 11 kg of self-healing component; 12 kg of functional admixtures; 0.35 kg of thickening and stabilizing agent hydroxypropyl methylcellulose; 178 kg of water; a water-cement ratio of 0.307; and a sand ratio of 37.9%.
[0039] The damping elastic particles are made of EPDM rubber, with an ethylene content of 52%, an ethylene-based norbornene content of 2.5%, a Shore A hardness of 65, and a density of 0.87 g / cm³. 3 The silane-modified layer is 8 μm thick and is formed by hydrolysis and coating with KH-560 silane coupling agent; the damping elastic particles consist of 70% coarse particles with a particle size of 0.6-1.2 mm and 30% fine particles with a particle size of 0.3-0.6 mm by mass, and the ultrafine mineral powder has a specific surface area of 460 m². 2 / kg, 7-day activity index 80%; silica fume SiO2 content 93%; river sand is zone II graded medium sand, fineness modulus 2.4, mud content 1.2%; crushed stone crushing index 11%, needle-like and flaky content 7%. Steel fibers are hook-shaped, 12mm long, 0.25mm in diameter; PVA fibers are 6mm long, 18μm in diameter; hydrated calcium silicate seed crystals have a Ca / Si molar ratio of 0.8-1.2, a particle size of 8μm, and are commercially available nanocrystalline seed additives; ettringite-type expanding agent has a fineness of 3%, and a 7-day restricted expansion rate in water of 0.028%; polycarboxylate high-efficiency water-reducing agent has a water reduction rate of 30%; hydroxypropyl methylcellulose viscosity specification 40000mPa·s.
[0040] Concrete pole structure: The hollow cone-shaped pole has a wall thickness of 50mm and is cast from the above-mentioned concrete material; multiple damping components 2 are arranged in sections along the height of the pole. The lower damping unit group is arranged in the lower 1 / 3 height of the pole, with a unit length of 400mm, a diameter of 60mm, and 8 layers of laminated plates; the upper damping unit group is arranged in the upper 1 / 3 height of the pole, with a unit length of 200mm, a diameter of 40mm, and 4 layers of laminated plates; each damping unit is axially along the pole axis, circumferentially uniform and symmetrical, and radially located in the middle layer of the cylinder wall, with a protective layer thickness of 20mm; Damping component 2 structure: the anchor bar 24 is 8mm long; the annular high-damping manganese-copper alloy sheet 22 is 1.8mm thick, with a Mn mass fraction of 65% and a Cu mass fraction of 25%; the annular high-damping rubber pad layer 23 is 1.0mm thick and has a Shore A hardness of 58.
[0041] The manufacturing process of utility poles includes the following steps: S1. Prefabrication of the main body of the utility pole: The steel frame 13 is fixed between the lower base 11 and the upper base 12. The annular high-damping manganese copper alloy sheet 22 and the annular high-damping rubber pad 23 are alternately stacked and clamped and fixed by the flanges 21 on both sides. The steel frame 13 is welded and fixed by the flanges 21. Finally, the steel cage 14 is welded to the surface of the steel frame 13. S2. Mold Assembly and Concrete Pouring: Place the tied-up main body of the utility pole into the centrifugal mold and close the mold; pour concrete material. The concrete material preparation method is as follows: dry mix silicate cement, mineral admixtures, and self-healing components for 1.5 min, add damping elastic particles and mixed reinforcing fibers and mix for 1.5 min, add river sand and crushed stone and dry mix for 1.5 min, add water containing functional admixtures and thickening stabilizers and stir for 4 min; then use a three-speed centrifugal system: low speed 260 r / min for 2 min, medium speed 620 r / min for 3 min, and high speed 950 r / min for 6 min. Under the action of centrifugal force, the concrete material densely wraps the main body of the utility pole; S3. Curing and demolding: Static pre-curing for 3 hours, steam curing at 68℃ for 9 hours, and natural wet curing for 7 days after demolding.
[0042] Example 3 A wind- and earthquake-resistant self-damping concrete utility pole comprises the following materials per cubic meter of concrete: 430 kg of silicate cement; 155 kg of mineral admixtures, including 90 kg of ultrafine mineral powder, 20 kg of silica fume, 45 kg of Class I fly ash, and 590 kg of river sand; 1000 kg of crushed stone; 60 kg of damping elastic particles; 45 kg of hybrid reinforcing fibers, including 28 kg of steel fibers and 8 kg of PVA fibers; 9 kg of basalt fibers; 16 kg of self-healing components; 1 kg of sodium carbonate activator; 16 kg of functional admixtures; 0.55 kg of thickening and stabilizing agent hydroxypropyl methylcellulose; and 185 kg of water. The water-cement ratio is 0.316, and the sand ratio is 37.1%.
[0043] The damping elastic particles are made of EPDM rubber, with an ethylene content of 58%, an ethylene-based norbornene content of 4.5%, a Shore A hardness of 70, and a density of 0.91 g / cm³. 3 The silane-modified layer is 12 μm thick and is formed by hydrolysis and coating with KH-550 silane coupling agent; the damping elastic particles consist of 60% coarse particles with a particle size of 0.6-1.2 mm and 40% fine particles with a particle size of 0.3-0.6 mm by mass, and the ultrafine mineral powder has a specific surface area of 500 m². 2 / kg, 7-day activity index 80%; silica fume SiO2 content 95%, fly ash fineness 10%, water requirement ratio 92%; river sand is zone II graded medium sand, fineness modulus 2.9, mud content 0.8%; crushed stone crushing index 9%, needle-like and flaky content 5%. Steel fibers are hook-shaped, 18mm long, 0.35mm in diameter; PVA fibers are 12mm long, 28μm in diameter, basalt fibers are 15mm long, 15μm in diameter; hydrated calcium silicate seed crystals have a Ca / Si molar ratio of 0.8-1.2, a particle size of 15μm, and are commercially available nanocrystalline seed additives; ettringite-type expanding agent has a fineness of 3%, and a 7-day restricted expansion rate in water of 0.045%; polycarboxylate high-efficiency water-reducing agent has a water reduction rate of 35%; hydroxypropyl methylcellulose viscosity specification 100000mPa·s.
[0044] Concrete pole structure: The hollow cone-shaped pole has a wall thickness of 65mm and is cast from the above-mentioned concrete material; multiple damping components 2 are arranged in sections along the height of the pole. The lower damping unit group is arranged in the lower 1 / 3 height of the pole, with a unit length of 500mm, a diameter of 80mm, and 12 layers of laminated plates; the upper damping unit group is arranged in the upper 1 / 3 height of the pole, with a unit length of 300mm, a diameter of 60mm, and 6 layers of laminated plates; each damping unit is axially along the pole axis, circumferentially uniform and symmetrical, and radially located in the middle layer of the cylinder wall, with a protective layer thickness of 20mm; Damping component 2 structure: the anchor bar 24 is 15mm long; the annular high-damping manganese-copper alloy sheet 22 is 2.2mm thick, with a Mn mass fraction of 65% and a Cu mass fraction of 25%; the annular high-damping rubber pad layer 23 is 1.4mm thick and has a Shore A hardness of 68.
[0045] The manufacturing process of utility poles includes the following steps: S1. Prefabrication of the main body of the utility pole: The steel frame 13 is fixed between the lower base 11 and the upper base 12. The annular high-damping manganese copper alloy sheet 22 and the annular high-damping rubber pad 23 are alternately stacked and clamped and fixed by the flanges 21 on both sides. The steel frame 13 is welded and fixed by the flanges 21. Finally, the steel cage 14 is welded to the surface of the steel frame 13. S2. Mold Assembly and Concrete Pouring: Place the tied-up main body of the utility pole into the centrifugal mold and close the mold; pour concrete material. The concrete material preparation method is as follows: dry mix silicate cement, mineral admixtures, and self-healing components for 1.5 min, add damping elastic particles and mixed reinforcing fibers and mix for 1.5 min, add river sand and crushed stone and dry mix for 1.5 min, add water containing functional admixtures and thickening stabilizers and stir for 4 min; then use a three-speed centrifugal system: low speed 300 r / min for 3 min, medium speed 700 r / min for 4 min, and high speed 1100 r / min for 8 min. Under the action of centrifugal force, the concrete material densely wraps the main body of the utility pole; S3. Curing and demolding: Static pre-curing for 3 hours, steam curing at 78℃ for 12 hours, and natural wet curing for 14 days after demolding.
[0046] Comparative Example 1 The only difference between this comparative example and Example 1 is that ordinary utility pole concrete material is used, without the addition of damping elastic particles, mixed reinforcing fibers, self-healing components, and thickening stabilizers; and no damping component 2 is pre-embedded in the wall of the utility pole. The materials used per cubic meter of ordinary concrete are: 460 kg of cement, 120 kg of mineral powder, 680 kg of river sand, 1080 kg of crushed stone, 6 kg of polycarboxylate superplasticizer, and 180 kg of water; the remaining preparation process parameters are the same as in Example 1.
[0047] Comparative Example 2 The only difference between this comparative example and Example 1 is that the damping elastic particles are not subjected to silane surface modification treatment, but are directly incorporated into unmodified EPDM rubber particles. The remaining formulation, structure and preparation process parameters are the same as those in Example 1.
[0048] Comparative Example 3 The only difference between this comparative example and Example 1 is that the damping component 2 is not pre-embedded in the wall of the utility pole, and the damping relies solely on the intrinsic damping of the material; the rest of the material formulation and preparation process parameters are the same as in Example 1.
[0049] Comparative Example 4 The only difference between this comparative example and Example 1 is that no self-healing component is added to the material formulation; the rest of the formulation, structure, and preparation process parameters are the same as in Example 1.
[0050] Comparative Example 5 The only difference between this comparative example and Example 1 is that the thickening and stabilizing agent hydroxypropyl methylcellulose is not added in the preparation method, and the high-speed centrifugation speed is a conventional 1200 r / min. All other formulations, structures, and process parameters are the same as in Example 1.
[0051] For the utility poles prepared in Examples 1-3 and Comparative Examples 1-5, the 28-day compressive strength of cubic specimens was tested according to GB / T50081-2019 "Standard for Test Methods of Physical and Mechanical Properties of Concrete"; the flexural strength of 400×100×100mm prisms was tested according to GB / T50081-2019; the damping loss factor of the materials was tested according to GB / T18258-2026 "Damping Materials and Damping Performance Test Methods"; the overall structural damping ratio was tested according to JGJ / T101-2015 "Code for Seismic Testing of Buildings"; the self-healing rate of microcracks was tested according to T / CECS913-2021 "Standard for Test Methods of Self-Healing Performance of Cement Concrete"; the chloride ion diffusion coefficient was tested with reference to GB / T50082-2024 "Standard for Test Methods of Long-Term Performance and Durability of Ordinary Concrete"; and the fatigue performance was tested according to T / CECS1499-2023 "Code for Test of Fatigue Performance of Railway Concrete". The performance test results of the utility poles are shown in Table 1.
[0052] Table 1 Performance test results of utility poles
[0053] As shown in Table 1, the 28-day compressive strength of the concrete materials in Examples 1-3 is ≥55MPa and the flexural strength is ≥8.0MPa, meeting the C50 strength grade requirements of GB / T4623-2014 for ring concrete poles; the material damping loss factor is ≥0.118, which is more than 2.6 times that of the ordinary concrete in Comparative Example 1; the overall structural damping ratio is ≥0.049, which is more than 2.7 times that of Comparative Example 1, proving that the intrinsic damping of the material and the built-in damping component 2 synergistically significantly improve the overall vibration reduction performance of the pole.
[0054] Comparative Example 2 uses unmodified EPDM rubber particles. Although the material damping loss factor reaches 0.132, the compressive strength is only 45.2 MPa and the flexural strength is 5.4 MPa, which is far below the C50 strength requirement for electric poles. This proves that silane surface modification is a key technical means to achieve both high damping and high strength.
[0055] Comparative Example 1: Ordinary concrete without material damping or built-in damping units has an overall structural damping ratio of only 0.018 and a fatigue cycle count of only 42,000. Example 1: Overall structural damping ratio of 0.058 and fatigue cycle count of 142,000, which is 3.4 times that of Comparative Example 1, proving that the dual damping system effectively improves fatigue resistance.
[0056] Comparing Example 1 and Comparative Example 3, the material formula is the same, but Comparative Example 3 does not have a pre-embedded damping component 2. The overall structural damping ratio decreased from 0.058 to 0.032, and the number of fatigue cycles decreased from 142,000 to 102,000. This proves that the pre-embedded damping component 2 effectively supplements the structural damping, and the sealed shell ensures that the friction damping mechanism still works effectively after the integral casting.
[0057] Comparative Example 4, without the addition of self-healing components, showed a microcrack self-healing rate of only 7%, while Example 1 achieved 92%, demonstrating that the self-healing components enabled automatic repair of microcracks.
[0058] Comparative Example 5, without the addition of thickening stabilizer and centrifuged at high speed of 1200 r / min, showed a high difference rate of 19.2% in the strength of the inner and outer surfaces, while Example 1 showed only 4.0%, demonstrating that the thickening stabilizer effectively inhibited the centrifugal migration and stratification of low-density components.
[0059] Example 3: With the addition of fly ash and basalt fiber, the chloride ion diffusion coefficient is only 1.4 × 10⁻⁶. -12 m 2 / s, overall structural damping ratio 0.065, fatigue cycle count 158,000, with optimal comprehensive performance.
[0060] Therefore, the wind-resistant and earthquake-resistant self-damping concrete utility pole and its vibration-damping base described in this invention achieve intrinsic material damping through silane-modified EPDM rubber particles, and additional structural damping through the damping component 2. The two work together to solve the problems in the prior art where utility poles are subjected to alternating wind vibration and earthquake loads over a long period of time; under the continuous action of alternating loads, the concrete pole body is repeatedly bent, and micro-cracks are easily generated inside the pole body. The continuous expansion of cracks will cause the pole body to crack and the stiffness to decrease. This invention achieves a unity of high damping, high strength, self-healing and high durability.
[0061] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention and not to limit them. Although the present invention has been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can still be made to the technical solutions of the present invention, and these modifications or equivalent substitutions cannot cause the modified technical solutions to deviate from the spirit and scope of the technical solutions of the present invention.
Claims
1. A wind- and earthquake-resistant self-damping concrete utility pole, characterized in that, It includes a steel cage assembly (1), a damping assembly (2) and a rod made of concrete material, wherein the damping assembly (2) is welded onto the surface of the steel cage assembly (1); The concrete material is made from the following raw materials in parts by weight: It includes 128-140 parts of cementitious material, which is composed of 100 parts of silicate cement and 28-40 parts of mineral admixture; it also includes 130-160 parts of river sand, 205-245 parts of crushed stone, 8-16 parts of damping elastic particles, 6-12 parts of mixed reinforcing fibers, 2-4 parts of self-healing component, 2.5-5.5 parts of functional additives, 0.05-0.15 parts of thickening stabilizer, and 39-47 parts of water; The hybrid reinforcing fiber comprises steel fiber and PVA synthetic fiber, with a mass ratio of steel fiber to PVA synthetic fiber of (2-3):1; the self-healing component is compounded from hydrated calcium silicate seed crystals and ettringite-type expansion component in a mass ratio of (1-2):1, wherein the ettringite-type expansion component accounts for 3%-6% of the total mass of the cementitious material; the concrete material dissipates vibration energy by undergoing controllable micro-slip friction under cyclic loading through the interface between damping elastic particles and cement paste, and the interface between the hybrid reinforcing fiber and the matrix.
2. The wind-resistant and earthquake-resistant self-damping concrete utility pole according to claim 1, characterized in that: The river sand is the net amount after deducting the volume substitution of damping elastic particles, with a fineness modulus of 2.4-3.0 and a mud content of ≤1.5%; the crushed stone has a continuous gradation of 5-13mm, with a needle-like and flaky content of ≤8% and a crushing index of ≤12%; the damping elastic particles are surface-modified EPDM rubber particles, with an ethylene content of 50%-60%, an ethylene-based norbornene third monomer content of 2%-5%, a Shore A hardness of 58-72, and a density of 0.86-0.92 g / cm³. 3 The surface is coated with a silane-modified layer with a thickness of 5-15 μm, which is formed by coating with silane coupling agent KH-550 or KH-560 after hydrolysis; the damping elastic particles include 60%-75% coarse particles with a particle size of 0.6-1.2 mm and 25%-40% fine particles with a particle size of 0.3-0.6 mm by mass percentage; the mineral admixture is a mixture of ultrafine mineral powder and silica fume in a mass ratio of (4-6):1, or a mixture of ultrafine mineral powder, silica fume and Class I fly ash, wherein Class I fly ash accounts for 20%-30% of the total amount of mineral admixture.
3. A wind-resistant and earthquake-resistant self-damping concrete utility pole according to claim 2, characterized in that: The specific surface area of the ultrafine mineral powder is ≥450m². 2 / kg, 7-day activity index ≥75%; the silica fume has a SiO2 mass fraction ≥92% and a specific surface area ≥15000m². 2 / kg; the fineness of the Class I fly ash is ≤12%, and the water requirement ratio is ≤95%; the river sand is Class II graded medium sand, and the crushed stone is a continuous graded mixture of 5-10mm and 10-13mm grades in a mass ratio of (3-4):(6-7).
4. A wind-resistant and earthquake-resistant self-damping concrete utility pole according to claim 3, characterized in that: The steel fiber is a hook-shaped steel fiber with a length of 12-18 mm, a diameter of 0.2-0.4 mm, an aspect ratio of 40-60, and a tensile strength ≥1000 MPa; the PVA synthetic fiber has a length of 6-12 mm, a diameter of 15-30 μm, and a breaking elongation of 6%-8%; basalt fiber may also be incorporated into the hybrid reinforcing fiber, accounting for 10%-20% of the total mass of the hybrid reinforcing fiber, with a length of 12-18 mm and a diameter of 13-17 μm.
5. A wind-resistant and earthquake-resistant self-damping concrete utility pole according to claim 4, characterized in that: The hydrated calcium silicate seed crystals have a Ca / Si molar ratio of 0.8-1.2 and a particle size of 5-20 μm, and are commercially available nanocrystalline seed additives; the ettringite-type expansion component is a calcium sulfoaluminate-calcium oxide expansion agent with a fineness ≤5% and a 7-day restricted expansion rate in water of 0.025%-0.050%; the self-healing component may also contain 5%-10% sodium carbonate activator by mass of the total self-healing component.
6. A wind-resistant and earthquake-resistant self-damping concrete utility pole according to claim 5, characterized in that: The functional admixture comprises a polycarboxylate-based high-efficiency water-reducing agent, a retarding component, an defoamer, and an amino alcohol-based steel reinforcement corrosion inhibitor; the polycarboxylate-based high-efficiency water-reducing agent has a water reduction rate ≥30%, and its dosage is 1.0%-1.8% of the total mass of the cementitious material; the retarding component is sodium gluconate or citric acid, and its dosage is 0.05%-0.15% of the total mass of the cementitious material; the defoamer is an organosilicon defoamer, and its dosage is 0.02%-0.08% of the total mass of the cementitious material; the amino alcohol-based steel reinforcement corrosion inhibitor is dimethylethanolamine or an amino alcohol complex salt, and its dosage is 0.5%-1.0% of the total mass of the cementitious material; the thickening and stabilizing agent is hydroxypropyl methylcellulose, with a viscosity specification of 40000-100000 mPa·s.
7. A wind-resistant and earthquake-resistant self-damping concrete utility pole according to claim 6, characterized in that: The utility pole is a hollow cone shape, cast from concrete, with a wall thickness of 40-70mm. The steel cage assembly (1) includes a lower base (11), an upper base (12), and a steel cage (13). The steel cage (13) is connected between the lower base (11) and the upper base (12), and a steel cage (14) is tied to the surface of the steel cage (13).
8. A wind-resistant and earthquake-resistant self-damping concrete utility pole according to claim 7, characterized in that: The damping component (2) includes symmetrically arranged flanges (21) and annular high-damping manganese-copper alloy sheets (22). The annular high-damping manganese-copper alloy sheets (22) are alternately stacked between the two flanges (21). The thickness of a single annular high-damping manganese-copper alloy sheet (22) is 1.5-2.5 mm, with a mass fraction of Mn of 60%-70%, a mass fraction of Cu of 20%-30%, and the balance being Fe, Ni, and Al. The flanges (21) are welded to the reinforcing steel frame (13) to clamp the annular high-damping manganese-copper alloy sheets (22). An annular high-damping rubber pad (23) is filled between adjacent annular high-damping manganese-copper alloy sheets (22). The annular high-damping rubber pad (23) is a polyurethane damping adhesive or an asphalt-based damping paste. The thickness of the annular high-damping rubber pad (23) is 0.8-1.5 mm, and the Shore A hardness is 55-70. The outermost annular high-damping... The surface of the manganese-copper alloy sheet (22) is welded with several anchor bars (24), the anchor bars (24) are 5-15mm long, and the anchor bars (24) penetrate into the concrete material to enhance the mechanical interlocking with the concrete material; multiple sets of the damping components (2) are arranged in sections along the height direction of the pole, including a lower damping unit group and an upper damping unit group. The lower damping unit group is arranged in the lower 1 / 3 height area of the pole, the unit length is 400-500mm, the diameter is 60-80mm, and the number of laminated layers is 8-12, which is for energy dissipation of seismic reciprocating load; the upper damping unit group is arranged in the upper 1 / 3 height area of the pole, the unit length is 200-300mm, the diameter is 40-60mm, and the number of laminated layers is 4-6, which is for energy dissipation of reciprocating vibration of strong wind; the axial direction of the damping component (2) is along the pole axis, and the radial direction is located in the middle layer of the cylinder wall thickness, and the concrete protective layer thickness is ≥15mm.
9. A wind-resistant and earthquake-resistant self-damping concrete utility pole according to claim 8, characterized in that: The manufacturing process of the utility pole includes the following steps: S1. Prefabrication of the main body of the utility pole: The steel frame (13) is fixed between the lower base (11) and the upper base (12). The annular high-damping manganese copper alloy sheet (22) and the annular high-damping rubber pad (23) are alternately stacked and clamped by the flanges (21) on both sides. The steel frame (13) is welded to the surface of the steel frame (13) by the flanges (21). Finally, the steel cage (14) is welded to the surface of the steel frame (13). S2. Mold assembly and concrete pouring: Place the tied pole body into the centrifugal mold and close the mold; pour concrete material using a three-speed centrifugal system: low speed 250-300 r / min for 2-3 minutes, medium speed 600-700 r / min for 3-4 minutes, and high speed 900-1100 r / min for 6-8 minutes. Under the action of centrifugal force, the concrete material densely wraps the pole body. S3. Curing and demolding: Static pre-curing for 2-4 hours, steam curing at 65-80℃ for 8-12 hours, and natural wet curing for 7-14 days after demolding.
10. A shock-absorbing base for a wind- and earthquake-resistant self-damping concrete utility pole, characterized in that: The shock-absorbing base is applicable to a wind-resistant and earthquake-resistant self-damping concrete utility pole as described in any one of claims 1-9. The utility pole is installed on the shock-absorbing base for limiting and fixing the lower base (11).