Negative electrode plate and manufacturing method for non-aqueous electrolyte secondary batteries

By controlling the powder density and molding pressure of silicon and graphite particles, voids are formed inside the negative electrode binder layer, solving the problem of increased resistance in non-aqueous electrolyte secondary batteries, enabling smooth electrolyte flow, and improving battery performance.

CN123120620APending Publication Date: 2026-11-17PRIME PLANET ENERGY & SOLUTIONS INC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202610671923.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2025-05-16
Filing Date
2026-05-15
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In non-aqueous electrolyte secondary batteries, the volume of the Si-based active material in the negative electrode increases during charging, which makes it difficult for the electrolyte to flow and increases the resistance.

Method used

By controlling the powder density and molding pressure of silicon-containing particles and graphite particles, the internal voids of the negative electrode mixture layer are ensured. The average particle size ratio of graphite particles to silicon-containing particles is 1.00 to 8.00, forming a path that facilitates electrolyte flow.

Benefits of technology

It effectively suppressed the increase in resistance of non-aqueous electrolyte secondary batteries, ensured the fluidity of the electrolyte, and improved battery performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123120620A_ABST
    Figure CN123120620A_ABST
Patent Text Reader

Abstract

A negative electrode plate for a non-aqueous electrolyte secondary battery includes a negative electrode mixture layer containing an active material. The active material comprises silicon particles and graphite particles. The content of silicon particles in the active material is 10-60% by mass relative to the total mass of the active material. The powder density of the silicon particles when pressed to a molding pressure of 60 MPa in the uniaxial direction is 0.90 g / cm³. 3 The following graphite particles are pressed into powder to a density of 1.7 g / cm³. 3 The required molding pressure in the uniaxial direction is above 30 MPa.
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Anode material, anode of secondary battery using said anode material, and method of manufacturing the same

    JP2024159006A