Core winding, core winding device, core winding method and battery
By designing straight and arc-shaped sections in the wound electrode core, and optimizing the spacing between the negative electrode sheet and the arc apex, as well as the position of the electrode sheet's end, the problem of electrode sheet wrinkling during the hot pressing process of the wound battery cell was solved, thus improving the quality and safety performance of the battery cell.
Patent Information
- Application Number
- CN202611290126.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-24
- Publication Date
- 2026-11-17
AI Technical Summary
During the hot pressing process, wound battery cells are prone to electrode wrinkling, which leads to a decrease in battery performance and a shortened cycle life. Existing technologies are unable to effectively solve this problem.
The cross-section of the wound electrode core is designed to have a straight section and a circular arc section. The negative electrode sheet maintains a distance from the arc apex of the circular arc section before hot pressing. By optimizing the thickness of the feeding clamp and the position of the electrode sheet's tail end, it is ensured that the electrode sheet does not interfere with each other during the hot pressing process.
It effectively prevents electrode wrinkling, improves the quality and safety performance of battery cells, reduces production costs, and avoids performance degradation and lithium plating problems caused by electrode wrinkling.
Smart Images

Figure CN123120813A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of wound battery cells, and more specifically, to a wound electrode core, an electrode core winding device, an electrode core winding method, and a battery. Background Technology
[0002] With the development of the new energy vehicle industry, lithium batteries, as its core component, are also booming. With the widespread application of lithium batteries, the demand for batteries with high energy density, high performance, and high safety is becoming increasingly urgent.
[0003] Currently, lithium battery cells are classified into three types: prismatic, cylindrical, and pouch. Their structure or manufacturing process is divided into two types: lamination and winding. Lamination cells offer high space utilization, low internal resistance, and good rate performance, but they suffer from prominent burr issues during manufacturing, making process control more difficult. In contrast, winding cells represent a mature process with high automation, fast production speed, good continuity, lower equipment requirements, and easier control over battery consistency. Most battery cell manufacturers currently employ the winding process.
[0004] However, as the pursuit of battery capacity and energy density continues to increase, the size of wound battery cells is becoming larger, with more and more layers and greater thickness. This has led to increasingly prominent wrinkling issues in battery cells, especially the wrinkling of the inner and outer rings, which is very difficult to resolve. Besides the internal S-shaped wrinkles caused by the continuous expansion and contraction of the positive and negative electrode sheets after multiple cycles of the finished battery cell, wrinkling of the electrode sheets also occurs during the winding and hot pressing process in battery cell manufacturing. If this wrinkling is not addressed promptly, it will lead to brown spots and lithium plating during subsequent battery cell formation, capacity grading, and charge / discharge cycles, affecting the battery's cycle life performance. Furthermore, lithium plating can further form lithium dendrites in subsequent charge / discharge cycles, impacting battery performance. Summary of the Invention
[0005] The purpose of this application is to prevent the coiled electrode core from wrinkling during the hot pressing process in a cost-effective manner, thereby eliminating the performance problems that may be caused by the coiled electrode.
[0006] Furthermore, the purpose of this application is to solve or at least alleviate one or more problems existing in the prior art.
[0007] This application solves the above problems by providing a wound electrode core, an electrode core winding device, an electrode core winding method, and a battery. Specifically, according to one aspect of this application, the following is provided: A wound electrode core, wherein the wound electrode core has a negative electrode sheet, and the cross-section of the wound electrode core has a structure including a straight section and an arc section connecting the straight section. Before the wound electrode core is hot-pressed, the negative electrode sheet has a gap relative to the arc apex of the arc section, so that the negative electrode sheet and the arc apex do not interfere when the wound electrode core is hot-pressed.
[0008] Optionally, according to one embodiment of this application, the negative electrode sheet has an infeed end that is first fed to the winding needle of the core winding device when the core is wound. Before the core is hot-pressed, the infeed end is spaced apart from the interior of the arc apex, so that the infeed end does not interfere with the interior of the arc apex when the core is hot-pressed.
[0009] Optionally, according to one embodiment of this application, before the wound electrode core is hot-pressed, the distance between the insert end and the arc apex is a', and the thickness of the unloading clamp of the electrode core winding device is A', satisfying the following relationship: a'≥A' / 2.
[0010] Optionally, according to one embodiment of this application, the negative electrode sheet has a tail end when the wound electrode core is wound on the winding needle of the electrode core winding device. Before the wound electrode core is hot-pressed, the tail end is spaced apart from the outside of the arc apex, so that the tail end does not interfere with the outside of the arc apex when the wound electrode core is hot-pressed.
[0011] Optionally, according to one embodiment of this application, before the wound pole core is hot-pressed, the tail end is located upstream of the arc apex in the winding direction of the wound pole core, and the tail end is located between the junction between the straight segment and the arc segment and a quarter of the arc length of the arc segment.
[0012] According to another aspect of this application, a core winding device is provided, wherein the core winding device is used to wind any of the above-mentioned wound cores.
[0013] Optionally, according to one embodiment of this application, the electrode core winding device includes a feeding clamp and a hot plate. The feeding clamp is used to clamp and stretch the wound electrode core after it has been fed into the hot plate. The hot plate is used to hot press the wound electrode core. The thickness of the feeding clamp is A', the plate spacing of the hot plate after hot pressing is B', and the arc angle of the arc segment of the wound electrode core is α', satisfying the following relationship: Sin(0.5α')=A' / B'.
[0014] Optionally, according to one embodiment of this application, the thickness of the feed clamp is 1 to 5 mm.
[0015] According to another aspect of this application, a method for winding an electrode core is provided, wherein the method is used to wind any of the above-mentioned wound electrode cores, and the method includes the following steps: The winding needle of the electrode core winding device retracts from the wound electrode core. The electrode core winding device uses a clamping pin to hold and stretch the wound electrode core, wherein the negative electrode sheet has a gap relative to the apex of the arc segment. The hot plate of the electrode core winding device hot-presses the wound electrode core into shape, wherein the negative electrode sheet does not interfere with the arc apex.
[0016] Optionally, according to one embodiment of this application, the electrode core winding method includes the following steps: The feeding clamp needle opens and retracts from the wound electrode core. The hot plate presses the wound electrode core together, wherein the negative electrode sheet does not interfere with the arc apex.
[0017] According to another aspect of this application, a battery is provided, wherein the battery includes any of the above-described wound electrode cores. Attached Figure Description
[0018] Referring to the accompanying drawings, the above and other features of this application will become apparent, wherein, Figure 1 This shows a schematic diagram of the electrode insert end of a wound electrode core according to this application at the start of hot pressing; Figure 2 This invention provides a schematic diagram of the electrode insert end of a wound electrode core after hot pressing is completed. Figure 3 The diagram shows the stress analysis of the wound pole core at the beginning of hot pressing. Figure 4 This invention provides a schematic diagram of the electrode tail end at the start of hot pressing of a wound electrode core according to the present application. Figure 5 This invention provides a schematic diagram of the electrode sheet tail end of a wound electrode core after hot pressing is completed. Figure 6 This diagram shows a wound pole core and a feeding clamping pin according to the present application at the start of hot pressing; Figure 7 A schematic diagram of a wound pole core and a feeding clamping pin according to this application during the hot pressing process is shown; Figure 8 This diagram illustrates a wound pole core according to the present application when the feeding clamp needle retracts; Figure 9 A schematic diagram of a wound pole core according to this application is shown when hot pressing is completed; Figure 10 A flowchart of a core winding method according to this application is shown. Detailed Implementation
[0019] It is readily understood that, based on the technical solution of this application, those skilled in the art can propose various interchangeable structural methods and implementations without altering the essential spirit of this application. Therefore, the following detailed embodiments and accompanying drawings are merely illustrative examples of the technical solution of this application and should not be considered as the entirety of this application or as limitations or restrictions on the technical solution of this application.
[0020] The directional terms such as up, down, left, right, front, back, front, back, top, and bottom mentioned or possibly used in this specification are defined relative to the structures shown in the accompanying drawings. These are relative concepts and may therefore vary depending on their location and usage. Therefore, these or other directional terms should not be interpreted as restrictive. Furthermore, the terms "first," "second," "third," and similar expressions are used for descriptive and distinguishing purposes only and should not be construed as indicating or implying the relative importance of the corresponding components.
[0021] Figure 1 This shows a schematic diagram of the electrode insert end of a wound electrode core according to this application at the start of hot pressing; Figure 2 This invention provides a schematic diagram of the electrode insert end of a wound electrode core after hot pressing is completed. Figure 3 The diagram shows the stress analysis of the wound pole core at the beginning of hot pressing. Figure 4 This invention provides a schematic diagram of the electrode tail end at the start of hot pressing of a wound electrode core according to the present application. Figure 5 A schematic diagram of the electrode sheet tail end of a wound electrode core according to this application after hot pressing is completed is shown.
[0022] This disclosure relates to a wound electrode core 1, wherein the wound electrode core 1 has a negative electrode sheet, and the cross-section of the wound electrode core 1 has a structure including a straight section 11 and an arc section 12 connecting the straight section 11. Before the wound electrode core 1 is hot-pressed, the negative electrode sheet has a gap relative to the arc apex of the arc section 12, so that the negative electrode sheet and the arc apex do not interfere when the wound electrode core 1 is hot-pressed.
[0023] It is understood that the electrode core includes a positive electrode plate, a negative electrode plate, and a separator that insulates the two. The positive and negative electrode plates are respectively constructed with a positive electrode tab 15 and a negative electrode tab 16. The positive electrode tab is, for example, an aluminum electrode tab, and the negative electrode tab is, for example, a copper electrode tab.
[0024] For example, the width of the battery cell is 1 mm-500 mm, the height of the battery cell is 1 mm-500 mm, the thickness of the battery cell is 0-300 mm, or the diameter of the battery cell is 1 mm-100 mm; the shape of the battery cell includes but is not limited to square, cylindrical, etc., the shell type includes but is not limited to soft pack, steel shell, etc., and the chemical system of the battery cell product includes but is not limited to lithium cobalt oxide, lithium iron phosphate, ternary materials, etc.
[0025] The hot pressing process here should be understood broadly, including the situation where the hot plate of the core winding device presses down to contact the core during hot pressing, the situation where the hot plate has not yet contacted the core but its heat has already affected the core (this is also called preheating or pre-pressing), and the situation where the hot plate is pressed down to the limit position after the feeding clamp opens and retracts to press the core tightly.
[0026] It is also understandable that before the wound electrode core is hot-pressed, it first undergoes winding by the winding needles of the electrode core winding device, followed by the winding needles exiting the winding electrode core (also known as unwinding), and being clamped by the unwinding clamps of the electrode core winding device (for example, two unwinding clamps clamp the two ends of the wound electrode core's arc) and stretching (stretching outwards). At this time, the wound electrode core is elliptical in shape. When the wound electrode core is hot-pressed, it gradually takes on a racetrack shape due to the action of hot pressing, including straight sections and arc sections.
[0027] This technical solution specifies a distance between the negative electrode sheet and the apex of the arc segment before hot pressing, and ensures that the negative electrode sheet does not interfere with the apex during hot pressing. This prevents the negative electrode sheet from wrinkling due to interference with the apex, thus eliminating all performance impacts caused by wrinkling. In other words, this spacing design provides the electrode sheet with sufficient space to move during the hot pressing process.
[0028] In contrast, other technical methods known to the applicant employ methods such as diaphragm baking to improve electrode wrinkling, optimizing winding tension parameters (including the tension of positive and negative electrodes and diaphragm) to improve diaphragm internal stress, and high-temperature hot pressure drop rebound, as well as pre-composite electrodes and diaphragms. While these methods do alleviate diaphragm internal stress and electrode wrinkling caused by electrode expansion, they still cannot eliminate wrinkling on the inner and outer rings. Furthermore, diaphragm baking requires additional steps, impacting production capacity and increasing manufacturing costs; winding tension optimization involves parameters such as the parallelism of the positive and negative electrodes, diaphragm, and multiple rollers on the winding machine, making adjustments very cumbersome and resulting in insufficient production stability; high-temperature hot pressing increases diaphragm thermal shrinkage and reduces diaphragm porosity, thus affecting the subsequent electrolyte retention and kinetic performance of the battery cell; and pre-composite electrodes and diaphragms only increase the complexity of the production process, significantly impacting production efficiency, and are currently not feasible with winding equipment.
[0029] Therefore, this application solves the problem of wrinkling of electrode sheets during hot pressing in a cost-effective manner.
[0030] Combination Figure 1 and Figure 2 It can be seen that (among them, Figure 1 and Figure 2 (The drawn arrows indicate the winding direction). The negative electrode sheet has an inlet end 13 that is first fed to the winding needle of the electrode core winding device when the winding electrode core 1 is wound. Before the winding electrode core 1 is hot-pressed, the inlet end 13 is spaced apart from the interior of the arc apex, so that the inlet end 13 does not interfere with the interior of the arc apex when the winding electrode core 1 is hot-pressed.
[0031] The insert end can be understood as the inner ring head electrode insert position. This technical solution can address situations where the inner ring electrode is not stretched properly during pre-pressing or hot pressing (e.g., the inner ring electrode springs back and shifts when the clamping needle is released) or where the inner ring electrode still slips or shifts within the crease position fluctuation range. It provides sufficient space for electrode extension and avoids the problem of wrinkling of the inner ring electrode caused by interference between the inner ring electrode head and the inner ring R-angle (i.e., the arc of the arc segment) (double insurance against inner ring wrinkling).
[0032] In terms of quantitative design, before the wound pole core 1 is hot-pressed, the distance between the insert end 13 and the arc apex is a', and the thickness of the unloading clamp 2 of the pole core winding device is A', satisfying the following relationship: a'≥A' / 2.
[0033] The units for each parameter in this formula are, for example, millimeters. The following section explains in detail why this technical solution can prevent wrinkling of the inner electrode sheet.
[0034] W is defined as the length of the innermost electrode sheet of the wound core before design optimization, that is, from the head of the innermost electrode sheet as the starting point to the center point of the innermost R-angle on the negative electrode tab side as the ending point; a is defined as the distance between the head of the innermost electrode sheet of the wound core before design optimization and the innermost R-angle on the positive electrode tab side, that is, from the head of the innermost electrode sheet as the starting point to the center point of the innermost R-angle on the positive electrode tab side as the ending point. Generally, a is approximately 0 (considering flatness); X is defined as the distance between the center points of the innermost R-angles on both sides of the positive and negative electrode tabs of the wound core, that is, from the center point of the innermost R-angle on the positive electrode tab side as the starting point to the center point of the innermost R-angle on the negative electrode tab side as the ending point.
[0035] Furthermore, W' is defined as the length of the innermost electrode sheet after the design optimization of the wound electrode core, that is, from the head b' of the innermost electrode sheet as the starting point to the center point f of the innermost R-angle on the negative electrode tab side as the ending point. a' is defined as the distance between the head of the innermost electrode sheet and the innermost R-angle on the positive electrode tab side after the design optimization of the wound electrode core, that is, from the head b' of the innermost electrode sheet as the starting point to the center point e of the innermost R-angle on the positive electrode tab side as the ending point. After optimization, a'≥A' / 2, where A' is the thickness of the feeding clamp after thinning.
[0036] T is defined as the thickness of the wound electrode core after pre-pressing or hot-pressing, and Δ is defined as the redundancy of the innermost electrode sheet, where: (W'+Δ)<X<(W+Δ), Δ<A' / 2.
[0037] Before optimization, during the descent of the pre-pressing or hot-pressing plate, the inner ring electrode sheet may slip or shift due to insufficient tension of the feeding clamping pin lever (e.g., the inner ring electrode sheet springs back and shifts when the clamping pin is released) or fluctuation of the crease position within a certain arc range. This results in electrode sheet redundancy, where the length of the inner ring electrode sheet changes from W to (W+Δ). The head of the inner ring electrode sheet moves closer to the center point e of the R-angle on the positive electrode tab side. At this point, the distance X between the center points e / f of the R-angles on both sides of the positive and negative electrode tabs is greater than the distance (W+Δ) between the inner ring electrode sheet and the center point e of the R-angle on both sides of the positive and negative electrode tabs. However, in general design, a is approximately 0, meaning the distance between the initial head point of the inner ring electrode sheet and the center point e of the R-angle on the positive electrode tab side is close to 0. Therefore, the resulting electrode sheet redundancy does not have enough space to release or flatten the electrode sheet, leading to wrinkling of the inner ring electrode sheet.
[0038] After optimization, the distance a' between the initial head of the inner circle electrode and the inner circle positive electrode ear-side R-angle is increased to ≥ A' / 2, that is, the distance between the head b' of the inner circle electrode and the center point e of the inner circle positive electrode ear-side R-angle must be ≥ A' / 2. The reason for this design is that, under extreme conditions, the innermost circle can be regarded as a semi-circular arc with the thickness of the clamping pin as its diameter. The minimum redundancy of the electrode sliding forward during the pressing process is A' / 2. Therefore, the distance from the electrode insertion position to the arc must be at least greater than this minimum redundancy.
[0039] Therefore, during the descent of the pre-pressing or hot-pressing plate, if the inner ring electrode sheet is not stretched properly due to insufficient tension of the feeding clamping pin (e.g., the inner ring electrode sheet springs back and shifts when the clamping pin is released) or the crease position fluctuates within a certain range of arc, the electrode sheet may slip or shift, resulting in electrode sheet redundancy. That is, the length of the inner ring electrode sheet changes from W' to (W'+Δ), and the head point b' of the inner ring electrode sheet moves closer to the center point e of the inner ring positive electrode ear side R angle. However, at this time, there is a space margin a' (≥A' / 2) between the head of the inner ring electrode sheet and the inner ring positive electrode ear side R angle. After the slip or electrode sheet shifts, the length W'+Δ of the inner ring electrode sheet is still smaller than the distance X between the center points e / f of the inner ring positive and negative electrode ear sides R angles. In other words, there is enough space to release the electrode sheet redundancy or flatten the electrode sheet. Even if the inner ring electrode sheet slips and shifts, it will not interfere with the arc apex, so the inner ring electrode sheet will not wrinkle.
[0040] Combination Figure 3 , Figure 4 and Figure 5 The negative electrode sheet has a tail end 14 when the wound electrode core 1 is wound on the winding needle of the electrode core winding device. Before the wound electrode core 1 is hot-pressed, the tail end 14 is spaced apart from the outside of the arc apex, so that the tail end 14 does not interfere with the outside of the arc apex when the wound electrode core 1 is hot-pressed.
[0041] It should be understood, for reference Figure 3 After the feeding clamps connect to the electrode core, the outer ring of the wound electrode sheet will sag due to gravity, while the diaphragm is in a flat state. When the preheating or hot pressing plate begins to descend, the diaphragm shrinks first due to heat, causing the outer ring electrode sheet to slip or shift, resulting in electrode redundancy. When the pressing plate presses down and contacts the electrode core, the outer ring electrode sheets at the corners on both sides of the electrode core (the end electrode sheet is designed to pass through the corner) are clamped by the feeding clamps on both sides. The two ends of the outer ring electrode sheet are also subjected to the pressure F1 / F2 of the top pressing plate. After the force is decomposed, there is a squeezing force F12 / F22 that pushes the outer ring electrode sheet towards the middle of the electrode core (the remaining force components are F11 / F21), which further aggravates the slippage or shift of the outer ring electrode sheet, increasing electrode redundancy. When the pressing plate descends further and locks the electrode core crease, the redundant electrode sheet is restricted by the corners on both sides and cannot be released or extended, leading to the problem of electrode wrinkling caused by interference between the end negative electrode sheet and the outer ring R-angle.
[0042] Therefore, according to this scheme, the end of the negative electrode, i.e. the end position of the electrode, is optimized. This can eliminate the problem of electrode wrinkling caused by interference between the outer negative electrode and the outer R-angle when the end position of the outer negative electrode passes the corner and the outer electrode slips or is displaced during pre-pressing or hot pressing. This is because the corners on both sides are restricted by the redundancy of the electrode and cannot be released or the electrode cannot be flattened. This ensures that the electrode next to the arc apex is not stressed.
[0043] In terms of quantitative design, according to one embodiment of this application, before the wound pole core 1 is hot-pressed, the tail end 14 is located upstream of the arc apex in the winding direction of the wound pole core 1, and the tail end 14 is located between the junction of the straight segment 11 and the arc segment 12 and a position where the distance between the tail end 14 and the arc apex is greater than or equal to one-quarter of the arc length of the arc segment 12.
[0044] The following explains in detail why this technical solution can solve the problem of wrinkling in the outer ring negative electrode sheet.
[0045] L is defined as the length of the final electrode sheet of the wound core before the end position optimization, that is, from the center point E of the outermost R-angle on the positive electrode tab side to the end point C of the electrode sheet; D is defined as the length between the center points of the outermost R-angles on both sides of the wound core, that is, from the center point E of the outermost R-angle on the positive electrode tab side to the center point F of the outermost R-angle on the negative electrode tab side; L' is defined as the length of the final electrode sheet of the wound core after the end position optimization, that is, from the center point E of the outermost R-angle on the positive electrode tab side to the end point C' of the electrode sheet; A' is the thickness of the feeding clamp after thinning; the arc corresponding to the fluctuation of the inner electrode sheet fold position is approximately equal to the thickness A of the feeding clamp; Δ' is defined as the redundancy of the outermost electrode sheet.
[0046] Where (L'+Δ')<D<(L+Δ'), Δ'<1 / 4 arc length (1 / 4 arc length=πT / 8).
[0047] Before optimization, (L+Δ')>D, meaning that when the end point of the tail electrode exceeds 1 / 2 of the arc corresponding to the outermost R angle on the negative electrode ear side (1 / 2 arc length = πT / 4), and reaches below point F, when the pre-pressing or hot-pressing plate descends, the outermost tail electrode will slide or the electrode will shift, resulting in electrode redundancy. However, due to the corner stress at points E and F, the redundant electrode can only randomly shift between points E and F. The redundant electrode cannot be flattened, and there is a gap between it and the lower electrode. When the pressing plate compacts the electrode core, it causes the outermost tail electrode to wrinkle.
[0048] After optimization, (L'+Δ')<D, the end point C' of the terminal electrode is above point F, and it is stipulated that the end point C' of the terminal electrode is not allowed to exceed 1 / 4 of the arc corresponding to the outermost R angle on the negative electrode ear side (1 / 4 arc length = πT / 8). When the pre-pressing or hot-pressing plate descends, the outermost electrode is only subjected to stress at point E. The end point C' of the terminal electrode will slide or displace the electrode towards point F, resulting in redundancy. However, since point C' is above point F and does not exceed 1 / 4 of the arc corresponding to the outermost R angle on the negative electrode ear side, there is enough space between point C' and point F (≥1 / 4 arc length) to allow the redundancy of the terminal electrode (Δ'<1 / 4 arc length) to be released or extended, so that the outermost electrode will not wrinkle.
[0049] What we know is that the selection of the quarter-length position strikes a balance between the flatness of the electrode core and the risk of exceeding the arc apex. In other words, if the end point is upstream of the junction, it may affect the flatness of the electrode core; if the end point is downstream of the quarter-length of the arc segment, there may be a risk of exceeding the arc apex. This value can be fine-tuned based on the feed position.
[0050] It is also known that the position of the tail electrode can be adjusted by shortening the length of the tail electrode or by adjusting the insertion position of the inner ring head (the optimized design of the inner ring head electrode to the inner ring R-angle has already left sufficient space). For example, if the insertion end is closer to the (left) arc apex, the distance between the tail end and the (right) arc apex will be greater. This also saves on the use of electrode foil, reducing the cost of the battery cell.
[0051] This application also relates to a core winding device, wherein the core winding device is used to wind any of the above-mentioned wound cores 1.
[0052] Therefore, the electrode core winding device of this application can inherit various implementation methods and corresponding technical effects of winding electrode cores, which will not be elaborated here.
[0053] Figure 6 This diagram shows a wound pole core and a feeding clamping pin according to the present application at the start of hot pressing; Figure 7 A schematic diagram of a wound pole core and a feeding clamping pin according to this application during the hot pressing process is shown; Figure 8 This diagram illustrates a wound pole core according to the present application when the feeding clamp needle retracts; Figure 9 A schematic diagram of a wound electrode core according to this application after hot pressing is shown. Figure 9 The short horizontal lines at both ends of the arc of the wound pole core represent creases.
[0054] The electrode core winding device includes a feeding clamp 2 and a hot plate 3. The feeding clamp 2 is used to clamp and stretch the wound electrode core 1 after it is fed into the hot plate. The hot plate 3 is used to hot press the wound electrode core 1. The thickness of the feeding clamp 2 is A', the plate spacing of the hot plate 3 after hot pressing is B', and the arc angle of the arc segment 12 of the wound electrode core 1 is α', satisfying the following relationship: Sin(0.5α')=A' / B'.
[0055] The hot plate may include, for example, two parallel and opposite plates, with the wound electrode core disposed between the two hot plates.
[0056] In contrast, theoretically, the arc angle α that improves the fluctuation of the pre-crease position has the following relationship with the thickness A of the blanking clamp and the plate spacing B after the pre-pressing plate descends: Sin(0.5α)=A / B, where 0°<α'<α<90°, A-A'>B-B'.
[0057] This technical solution can lock the crease fluctuation amplitude or crease position of the inner electrode sheet, thus making it difficult for wrinkles to occur in other parts of the electrode core during subsequent processes. The formula shows the ratio of A' / B'. When the clamping pin thickness A' is less than the original value A, the pressure plate can be lowered to a lower position, meaning B' is smaller, and the crease fluctuation angle α' also decreases accordingly.
[0058] In other words, this solution recognizes the relationship between the thickness of the feeding clamp needle and the arc angle corresponding to the crease, as well as its impact on the spacing between the hot plates. By utilizing this relationship, the size of the arc angle of the pole core can be controlled by adjusting the thickness of the feeding clamp needle.
[0059] For example, by reducing the thickness of the winding and unloading clamping needle (the thickness of the winding needle is, for example, 1-10 mm), the pressure plate can be lowered to a lower position during pre-pressing or hot pressing. This makes it easier to lock the crease position of the inner ring electrode in advance and significantly reduces the fluctuation range of the crease position. This avoids the problem of uneven distribution of the upper and lower half of the electrode core during hot pressing, which can cause slippage or electrode displacement in the inner ring, and thus lead to wrinkling of the inner ring electrode.
[0060] Specifically, it is feasible for the thickness of the feed clamp 2 to be 1 to 5 mm.
[0061] For example, the original thickness of the winding and unwinding clamp is 9-10 mm (A is the initial clamp thickness). In this regard, according to this technical solution, when the winding needle exits the electrode core and the unwinding clamp takes over the electrode core to begin stretching, the inner ring R-angle is tightly fitted with the unwinding clamp. The arc range corresponding to the fluctuation of the inner ring electrode crease position is approximately equal to the thickness A of the unwinding clamp. Therefore, as the thickness A of the unwinding clamp decreases, the arc range of the crease position fluctuation also decreases. That is, the thinner the unwinding clamp, the earlier the crease position of the inner ring electrode can be locked. Furthermore, in the pre-pressing process, because the unwinding clamp is thinned, the pre-pressing plate can also be reduced from the original spacing B to a lower spacing B' (where B' > (electrode core + clamp thickness)), further locking the inner ring electrode crease position. This can avoid the problem of uneven distribution of the upper and lower half of the electrode core due to the large fluctuation range of the inner ring crease when the pre-pressing plate descends to press the electrode core, which would cause the inner ring to slip or the electrode to shift, thus leading to the problem of wrinkling of the inner ring electrode.
[0062] Figure 10 A flowchart of a core winding method according to this application is shown.
[0063] This application also relates to a method for winding an electrode core, wherein the method is used to wind any of the above-mentioned wound electrode cores 1, and the method includes the following steps: S1: The winding needle of the electrode core winding device retracts from the wound electrode core 1. S2: The feeding pin 2 of the electrode core winding device clamps and stretches the wound electrode core 1, wherein the negative electrode sheet has a gap relative to the arc apex of the arc segment 12. S3: The hot plate 3 of the electrode core winding device hot-presses the winding electrode core 1 into shape, wherein the negative electrode sheet does not interfere with the arc apex.
[0064] Therefore, the electrode core winding method of this application can inherit various implementation methods and corresponding technical effects of winding electrode cores, which will not be elaborated here.
[0065] However, it should be understood that the electrode core winding method may also include the following steps: S4: The feeding clamp 2 opens and retracts from the winding electrode core 1. S5: The hot plate 3 presses the wound electrode core 1 tightly, wherein the negative electrode sheet does not interfere with the arc apex. At this time, the feeding clamp needle rises back to its initial position.
[0066] Therefore, the hot pressing of the wound electrode core by the hot plate is divided into two stages, with the withdrawal of the feeding clamp pin as the dividing line. Throughout the entire stage of hot pressing of the wound electrode core by the hot plate, wrinkling of the negative electrode sheet can be prevented.
[0067] The hot plate pressing the wound electrode core can be understood as compressing the wound electrode core to a preset thickness (final forming thickness) and heat-setting it.
[0068] This application also relates to a battery, wherein the battery includes any of the above-described wound electrode cores 1.
[0069] Similarly, the battery of this application can inherit various implementation methods and corresponding technical effects of wound electrode cores.
[0070] It should be understood that the battery cell products targeted in this application include, but are not limited to, lithium-ion batteries, sodium-ion batteries, etc.
[0071] In summary, by addressing electrode wrinkling in three aspects (thickness of the feeding clamp, design of the insert end, and design of the termination end) in this application, the problem of wrinkling of the inner and outer ring electrodes in lithium-ion battery cells can be eliminated, thereby improving cell quality, reducing cell cost, avoiding performance degradation and lithium plating caused by wrinkling of the inner and outer rings of the battery cell, and further enhancing the safety performance of the battery cell.
[0072] The following experimental data further illustrates the effectiveness of this application in preventing wrinkles based on these three aspects. Product Parameters Specification Base group Control group 1 Control group 2 Control group 3 Core thickness / mm T 16.94 16.96 16.99 16.95 Thickness of the feeding clamp before thinning / mm A 9.0 / / / Thickness of the feed clamp after thinning / mm A’ / 5.0 4 2 Height between clamping pins and pressure plates before thinning / mm B 27.80 / / / Height between pressure plates after thinning of clamping needles / mm B’ / 23.82 22.85 20.81 The arc corresponding to the angle / ° for improving the crease fluctuation of the inner electrode sheet. α 37.8 / / / The angle corresponding to the arc of the improved inner electrode crease fluctuation / ° α’ / 24.3 20.1 11.0 Before improvement, the inner electrode length was 2 mm. W 225.50 / / / Distance between the center points of the inner R-angles on both sides of the pole core / mm X 225.56 225.54 225.51 225.57 Improved inner electrode length / mm W’ / 223 223.5 224.5 Inner ring electrode redundancy / mm Δ 1.2 1.2 1 0.5 Improved outer electrode length / mm L 258 / / / Length between the center points of the outer R-angles on both sides of the pole core / mm D 252 252.2 252.3 251.9 Improved outer electrode length / mm L’ / 245 244.5 243.5 Outer electrode redundancy / mm Δ' 3.2 3.3 2.7 1.8 Wrinkle condition of inner and outer rings / pcs NG 36 / 50 0 / 50 0 / 50 0 / 50
[0073] In summary, based on the experimental data above, the wrinkle rate of the Base group was 72% (36 / 50), while the wrinkle rate of all three control groups was 0% (0 / 50), demonstrating excellent anti-wrinkle effects.
[0074] Specifically, regarding the design of the feed clamp thickness, the base group had a feed clamp thickness of 9 mm and an arc angle of 37.8 degrees, with a large range of fluctuation in the crease and strong randomness; while the control group had feed clamp thicknesses of 5.0, 4, and 2 mm, and arc angles of 24.3, 20.1, and 11.0 degrees, respectively, which were reduced by 36, 47, and 71% compared to the original arc angle.
[0075] Regarding the design of the insert end, the distance between the length of the inner ring electrode and the center point of the inner ring R-angle on both sides of the electrode core is almost the same before the improvement, which cannot meet the 1.2 mm redundancy of the inner ring electrode. Therefore, the insert end of the inner ring electrode is prone to interference with the arc apex during hot pressing. In the three control groups, the distance between the insert end and the arc apex is approximately 2.54, 2.01, and 1.07 mm, respectively, which meet the inner ring electrode redundancy requirements of 1.2, 1, and 0.5 mm, respectively.
[0076] Regarding the design of the termination end, the outer ring electrode length in the Base group is 258 mm, which is longer than the length between the center points of the outer ring R-angles on both sides of the electrode core. Therefore, whether the termination extends beyond the R-angle vertex can easily cause interference with the R-angle during hot pressing, resulting in wrinkles. In the three control groups, the outer ring electrode length is shorter than the length between the center points of the outer ring R-angles on both sides of the electrode core, and the difference is sufficient to meet the redundancy of the outer ring electrode, allowing the electrode to extend and release smoothly without wrinkles caused by interference.
[0077] It should be understood that all the above preferred embodiments are exemplary and not restrictive, and various modifications or variations made by those skilled in the art to the specific embodiments described above under the concept of this application should be within the scope of legal protection of this application.
Claims
1. A wound electrode core (1), characterized in that The wound core (1) has a negative electrode sheet. The cross-section of the wound core (1) is a structure including a straight section (11) and an arc section (12) connecting the straight section (11). Before the wound core (1) is hot-pressed, the negative electrode sheet has a gap relative to the arc apex of the arc section (12) so that the negative electrode sheet does not interfere with the arc apex when the wound core (1) is hot-pressed.
2. The wound pole core (1) according to claim 1, characterized in that, The negative electrode sheet has an inlet end (13) that is first fed to the winding needle of the core winding device when the core (1) is wound. Before the core (1) is hot-pressed, the inlet end (13) is spaced apart from the interior of the arc apex, so that the inlet end (13) does not interfere with the interior of the arc apex when the core (1) is hot-pressed.
3. The wound pole core (1) according to claim 2, characterized in that, Before the wound pole core (1) is hot-pressed, the distance between the insert end (13) and the arc apex is a', and the thickness of the unloading clamp (2) of the pole core winding device is A', satisfying the following relationship: a'≥A' / 2.
4. The wound pole core (1) according to claim 1, characterized in that, The negative electrode sheet has a tail end (14) when the wound electrode core (1) is wound on the winding needle of the electrode core winding device. Before the wound electrode core (1) is hot-pressed, the tail end (14) is spaced apart from the outside of the arc apex, so that when the wound electrode core (1) is hot-pressed, the tail end (14) does not interfere with the outside of the arc apex.
5. The wound pole core (1) according to claim 4, characterized in that, Before the wound pole core (1) is hot-pressed, the tail end (14) is located upstream of the arc apex in the winding direction of the wound pole core (1), and the tail end (14) is located between the junction between the straight section (11) and the arc section (12) and a quarter of the arc length of the arc section (12).
6. A core winding device, characterized in that, The pole core winding device is used to wind the wound pole core (1) according to any one of claims 1 to 5.
7. The electrode core winding device according to claim 6, characterized in that, The electrode core winding device includes a feeding clamp (2) and a hot plate (3). The feeding clamp (2) is used to clamp and stretch the winding electrode core (1) after it is fed. The hot plate (3) is used to hot press the winding electrode core (1). The thickness of the feeding clamp (2) is A'. The plate spacing of the hot plate (3) after hot pressing is B'. The arc angle of the arc segment (12) of the winding electrode core (1) is α', which satisfies the following relationship: Sin(0.5α')=A' / B'.
8. The core winding device according to claim 7, characterized in that, The thickness of the feeding clamp (2) is 1 to 5 mm.
9. A method for winding an electrode core, characterized in that, The electrode core winding method is used to wind a wound electrode core (1) according to any one of claims 1 to 5, and the electrode core winding method includes the following steps: The winding needle of the core winding device exits the wound core (1). The feeding pin (2) of the electrode core winding device clamps and stretches the wound electrode core (1), wherein the negative electrode sheet has a gap relative to the arc apex of the arc segment (12). The hot plate (3) of the core winding device hot-presses the wound core (1) into shape, wherein the negative electrode sheet does not interfere with the arc apex.
10. The electrode core winding method according to claim 9, characterized in that, The pole core winding method includes the following steps: The feeding clamp (2) opens and retracts the winding pole core (1). The hot plate (3) presses the wound electrode core (1) together, wherein the negative electrode sheet does not interfere with the arc apex.
11. A battery, characterized in that, The battery includes a wound electrode core (1) according to any one of claims 1 to 5.