Electrolyte additives, gel polymer electrolyte compositions and their preparation methods
By introducing flexible segments and flame-retardant groups into the electrolyte through chemical modification of lignin additives, the problems of lignin dispersion and high-pressure decomposition were solved, the electrochemical stability and safety of the battery were improved, and low-cost and high-efficiency electrolyte improvement was achieved.
Patent Information
- Application Number
- CN202611406048.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-10
- Publication Date
- 2026-11-17
AI Technical Summary
Existing gel polymer electrolytes suffer from poor lignin dispersion and easy decomposition under high pressure. Furthermore, traditional flame retardants are costly and have poor compatibility with electrolytes, resulting in insufficient battery safety and electrochemical stability.
Chemically modified lignin is used as an electrolyte additive. Flexible polymer segments are covalently linked to the lignin skeleton and flame-retardant groups of phosphorus, silicon, fluorine or boron are introduced. Phenolic hydroxyl and alcohol hydroxyl groups are blocked with end-capping groups to form an electrolyte additive that combines compatibility, flame retardancy and antioxidant properties.
It significantly improves the stability and safety of the electrolyte under high voltage, enhances the interface contact stability and long-term safety of the battery, and reduces production costs, meeting the needs of green and environmentally friendly industrialization.
Smart Images

Figure CN123120860A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of lithium secondary battery technology, specifically to electrolyte additives, gel polymer electrolyte compositions, and their preparation methods. Background Technology
[0002] Lithium-ion batteries are widely used in portable electronic devices, electric vehicles, and other fields due to their high energy density and long cycle life. However, traditionally used liquid organic electrolytes pose safety hazards such as flammability and leakage, and may cause thermal runaway under overcharging, short circuits, or high-temperature environments, leading to fire or explosion. Gel polymer electrolytes, by immobilizing the liquid electrolyte within a polymer matrix, can effectively reduce the risk of leakage and are considered an important way to improve battery safety.
[0003] Existing gel polymer electrolyte systems often improve performance by adding oligomers, ionic liquids, or flame retardants with specific structures. However, many synthetic oligomers or flame retardants suffer from high cost, poor compatibility with electrolytes, or insufficient electrochemical stability. Lignin, as an abundant natural aromatic polymer, is widely available, inexpensive, and biodegradable. However, when used directly as an additive in gel polymer electrolytes, its numerous active phenolic and aliphatic hydroxyl groups are easily oxidized and decomposed under high voltage, and its solubility and dispersibility in organic electrolytes are extremely poor, making it difficult to form homogeneous and stable gel polymer electrolytes.
[0004] Therefore, there is an urgent need to develop a new gel polymer electrolyte technology that can provide multiple benefits such as flame retardancy and high-temperature stability. Summary of the Invention
[0005] The purpose of this invention is to overcome the shortcomings of the prior art and provide an electrolyte additive, a gel polymer electrolyte composition and its preparation method, so as to solve the problems of poor lignin dispersibility and easy decomposition under high pressure, and to endow the gel polymer electrolyte with excellent electrochemical stability.
[0006] The specific technical solution of the present invention is as follows: In a first aspect, the present invention provides an electrolyte additive, wherein the electrolyte additive is chemically modified lignin, the chemically modified lignin comprising a lignin skeleton, a flexible polymer chain segment covalently connected to the lignin skeleton, the side ends or ends of the flexible polymer chain segment containing phosphorus, silicon, fluorine or boron flame retardant groups; and the phenolic hydroxyl and alcoholic hydroxyl groups remaining on the lignin skeleton are capped by end-capping groups.
[0007] Through the above structural design, the electrolyte additive combines the compatibility brought by the flexible chain segments, the safety brought by the flame retardant groups, and the antioxidant properties brought by the end-capped groups. The three work together to significantly improve the overall stability and safety of the electrolyte under high voltage.
[0008] Furthermore, the flexible polymer segments are homopolymer or copolymer segments formed from one or more of methyl methacrylate, butyl acrylate, and ε-caprolactone. This approach enables the modified lignin to form a good molecular-level intercompatible network with the organic solvent and polymer matrix in the electrolyte, effectively improving the interfacial contact stability of the battery during cycling.
[0009] Furthermore, the flame-retardant group is derived from the copolymerization of a vinyl monomer containing this group, wherein the vinyl monomer is selected from at least one of diethylphosphoryl methacrylate, vinyltrimethoxysilane, hexafluorobutyl methacrylate, and 4-vinylphenylboronic acid. This preferred embodiment anchors the flame-retardant elements (P, Si, F, B) to the polymer chain segments through copolymerization, avoiding the problems of easy precipitation and migration of small molecule flame retardants, thereby ensuring the long-term safety of the battery.
[0010] Furthermore, the end-capping group is acetyl or benzoyl. This preferred embodiment eliminates the active phenolic and alcoholic hydroxyl groups on the lignin backbone through chemical end-capping, blocking its oxidative degradation pathway under high voltage, further broadening the electrochemical stability window of the electrolyte, and suppressing side reactions under high voltage.
[0011] Furthermore, the lignin is selected from one or more of alkali lignin, sulfate lignin, lignin sulfonate, and organic solvent lignin. This preferred embodiment provides a wide range of raw material options, all of which are industrial by-products, widely available, and extremely low in cost, while also meeting the requirements of green and environmentally friendly industrialization.
[0012] In a second aspect, the present invention provides a method for preparing an electrolyte additive as described in any one of the first aspects, comprising the following steps: S1, Methacrylation: Lignin is dissolved in an organic solvent and reacted with a methacrylating agent in the presence of a catalyst and an acid-binding agent to introduce double bonds into the lignin skeleton; S2, Graft copolymerization: In the reaction system obtained in step S1, vinyl monomers containing phosphorus, silicon, fluorine or boron flame retardant groups, comonomers and polymerization initiators are added to carry out free radical copolymerization reaction to graft flexible polymer segments containing flame retardant groups onto the lignin skeleton. S3. End-capping treatment: Cool the reaction system obtained in step S2, add acetyl chloride or benzoyl chloride to carry out the end-capping reaction, and block the residual phenolic hydroxyl and alcoholic hydroxyl groups on the lignin skeleton. S4. Purification: Pour the reaction solution obtained in step S3 into a precipitant to precipitate the solid, and then wash and vacuum dry to obtain the electrolyte additive.
[0013] Further, in step S1, the catalyst is 4-dimethylaminopyridine, the acid-binding agent is triethylamine, and the methacrylating agent is methacryloyl chloride; in step S2, the polymerization initiator is azobisisobutyronitrile.
[0014] Furthermore, based on 10 parts by weight of lignin: In step S1, the amount of the methacrylamide reagent is 15-25 parts by weight, the amount of the catalyst is 0.3-0.8 parts by weight, and the amount of the acid-binding agent is 3-7 parts by weight. In step S2, the amount of the vinyl monomer containing phosphorus, silicon, fluorine or boron flame retardant groups is 10-20 parts by weight, the amount of the comonomer is 20-40 parts by weight, and the amount of the polymerization initiator is 0.2-1.0 parts by weight. In step S3, the amount of acetyl chloride or benzoyl chloride used is 1-3 parts by weight. This preparation method is simple and mild. By precisely limiting the amount of raw materials used in each step, it achieves precise control over the lignin grafting rate and end-capping rate, thereby ensuring that the obtained electrolyte additive has excellent dispersibility, flame retardancy, and high-pressure stability, and is easy to scale up for production.
[0015] Thirdly, the present invention provides a gel polymer electrolyte composition comprising a lithium salt, a non-aqueous organic solvent, a crosslinkable polymer or oligomer, a polymerization initiator, and the electrolyte additive described in any one of the first aspects. Through the synergistic effect of its components, this composition can form a gel electrolyte system with a uniform structure, stability, high ionic conductivity, and excellent antioxidant properties.
[0016] Furthermore, the mass ratio of the electrolyte additive to the crosslinkable polymer or oligomer is 0.05:1 to 2:1.
[0017] Furthermore, the mass ratio of the electrolyte additive to the crosslinkable polymer or oligomer is 1:1 to 2:1. Within this preferred ratio range, the modified lignin can fully participate in the construction of the gel network, providing sufficient flame-retardant groups and suppressing interfacial side reactions; excess or deficiency will lead to a decrease in performance (e.g., below 1:1, the flame-retardant and stabilizing effects are insufficient, and above 2:1 may lead to excessively high system viscosity and hindered ion conduction), thereby ensuring the optimal balance between electrochemical stability and mechanical strength of the gel electrolyte.
[0018] Furthermore, based on the total mass of the gel polymer electrolyte composition being 100%, the mass fraction of the electrolyte additive is 1% to 4%.
[0019] Furthermore, based on the total mass of the gel polymer electrolyte composition being 100%, the mass fraction of the electrolyte additive is 2% to 4%.
[0020] Further, the crosslinkable polymer or oligomer is polyethylene glycol diacrylate or ethoxylated trimethylolpropane triacrylate; the lithium salt is lithium hexafluorophosphate; and the polymerization initiator is azobisisobutyronitrile.
[0021] Furthermore, the non-aqueous organic solvent is a carbonate solvent.
[0022] Fourthly, the present invention provides a method for preparing a gel polymer electrolyte, comprising the following steps: S1. Mix and stir the components in the composition described in any one of the second aspects to form a homogeneous and transparent precursor solution; S2. Inject the precursor solution into a mold and polymerize it at 60-80°C under normal pressure for 1-6 hours to form a gel polymer electrolyte.
[0023] This preparation method is simple to operate, operates under mild conditions, and does not require high-pressure equipment. It can directly prepare a uniformly structured gel film through in-situ thermal polymerization without the need for additional solvent removal processes, which greatly improves process efficiency and product yield. This enhances the applicability and safety of the preparation method in large-scale production and reduces production costs.
[0024] Compared with the prior art, the beneficial technical effects of this invention are reflected in: This invention transforms lignin into a high-performance, high-safety gel polymer electrolyte functional additive through rational chemical modification. Grafting flexible solvated segments allows the modified lignin to be uniformly and stably dispersed in the organic electrolyte, preventing aggregation and precipitation. End-capping treatment eliminates the risk of oxidative decomposition of active hydroxyl groups under high pressure, broadening the electrochemical stability window of the electrolyte. Furthermore, lignin, as a natural and renewable resource, is green, inexpensive, and has enormous industrialization potential. Attached Figure Description
[0025] Figure 1 The linear sweep voltammetry curves of the gel polymer electrolytes prepared in Examples 1, 2, and 3 of this invention are compared with those of Comparative Example 1. Figure 2 The FTIR spectra of unmodified lignin and chemically modified lignin A are shown. Figure 3 a is a photograph of unmodified alkali lignin; Figure 3 b is a photograph of the chemically modified lignin A; Figure 3 c is a comparison photograph of the dissolution states of unmodified alkali lignin and chemically modified lignin A in the basic electrolyte; Figure 4 Photographs showing the appearance of the precursor solution; Figure 5 Photographs of the gel polymer electrolytes obtained in Examples 1, 2, 3 and Comparative Example 1; Figure 6 The battery cycle performance curves are for Examples 1, 2, 3 and Comparative Example 1. Detailed Implementation
[0026] To make the above-mentioned objects, features and advantages of the present invention more apparent and understandable, the specific embodiments of the present invention will be described in detail below with reference to the accompanying drawings.
[0027] Many specific details are set forth in the following description in order to provide a full understanding of the invention. However, the invention may also be practiced in other ways different from those described herein, and those skilled in the art can make similar extensions without departing from the spirit of the invention. Therefore, the invention is not limited to the specific embodiments disclosed below.
[0028] Secondly, the term "one embodiment" or "embodiment" as used herein refers to a specific feature, structure, or characteristic that may be included in at least one implementation of the present invention. The phrase "in one embodiment" appearing in different places in this specification does not necessarily refer to the same embodiment, nor is it a single or selective embodiment that excludes other embodiments. Where specific conditions are not specified in the embodiments, conventional conditions or conditions recommended by the manufacturer shall be followed. Where the manufacturers of reagents or instruments are not specified, they are all conventional products that can be purchased commercially.
[0029] The embodiments of the present invention will be described in detail below with reference to the accompanying drawings.
[0030] Preparation of modified lignin A Alkali lignin (manufacturer: Aladdin, CAS No.: 8068-05-1) was selected. Alkali lignin was vacuum-dried at 80℃ for 12 hours before use.
[0031] Step 1, Methacrylation Modification of the Lignin Framework: 10 parts by weight of alkali lignin were added to 50 parts by weight of anhydrous dimethyl sulfoxide and pre-stirred at room temperature for 30 minutes under nitrogen protection. Then, 0.5 parts by weight of 4-dimethylaminopyridine and 5 parts by weight of triethylamine were added, and the temperature was raised to 40°C. 20 parts by weight of methacrylamide chloride were slowly added dropwise over a period of 30–60 minutes. After the addition was complete, the reaction was continued for 24 hours under nitrogen protection and mechanical stirring at 40°C using a reflux condenser. The purpose of this step is to introduce polymerizable double-bond functional groups into the lignin framework, providing reaction sites for subsequent graft copolymerization.
[0032] Step 2, flexible segment graft copolymerization with flame-retardant groups: After the reaction in Step 1 is completed, 15 parts by weight of diethylphosphoryl methacrylate, 30 parts by weight of methyl methacrylate, and 0.5 parts by weight of azobisisobutyronitrile are added, and nitrogen gas is continuously purged for 10-20 minutes. The temperature is then raised to 70°C, and the reaction is carried out for 12 hours under nitrogen protection and continuous stirring. The purpose of this step is to graft polymer segments with both flexible and flame-retardant functions onto the lignin backbone via free radical copolymerization, thereby improving its compatibility with organic electrolytes and imparting flame retardancy.
[0033] Step 3, End-capping treatment of residual active hydroxyl groups: After the polymerization in Step 2 is completed, the system is cooled to 25°C, and 2 parts by weight of acetyl chloride are added under nitrogen protection. The addition rate is controlled so that the system temperature does not exceed 30°C. After the addition is complete, the reaction is continued at 25°C with stirring for 6 hours. The purpose of this step is to use acetyl groups to block the unreacted phenolic and alcoholic hydroxyl groups on the lignin backbone, eliminate the risk of oxidative decomposition under high voltage, and broaden the electrochemical stability window.
[0034] Step 4, Product Separation and Purification: After the reaction in Step 3 is completed, the reaction solution is slowly added to 5-10 times its volume of deionized water, allowed to stand for 30 minutes, and then filtered. The resulting solid is washed three times with a mixed solvent of ethanol / deionized water (ethanol to deionized water mass ratio of 8:2). The washed solid is then dried in a vacuum oven at 60-80℃ for 12-24 hours until constant weight is achieved, yielding modified lignin A. The purpose of this step is to remove unreacted monomers, homopolymers, and byproducts through precipitation, washing, and drying, thereby obtaining pure chemically modified lignin A.
[0035] Example 1 (The ratio of modified lignin A weight to total electrolyte weight is 0.02:1) In a nitrogen-filled glove box, 1.0 mol / L lithium hexafluorophosphate was dissolved in a mixed solvent of ethylene carbonate / ethyl methyl carbonate to prepare a basic electrolyte. 95.95 parts by weight of the basic electrolyte were taken, and 2 parts by weight of polyethylene glycol diacrylate (PEGDA, manufacturer: McLean, CAS No.: 26570-48-9) with a number-average molecular weight of approximately 575, 2 parts by weight of modified lignin A, and 0.05 parts by weight of azobisisobutyronitrile were added. The mixture was magnetically stirred at 25°C for 2 hours at a stirring speed of 500–800 rpm to obtain a homogeneous and transparent precursor solution (appearance as shown in the image). Figure 4 (As shown). The precursor solution was injected into the electrode assembly, sealed, and polymerized at 70°C under normal pressure for 2 hours to form a gel polymer electrolyte in situ (see actual photograph). Figure 5 a).
[0036] Example 2 (the ratio of modified lignin A weight to total electrolyte weight is 0.01:1) In a nitrogen-filled glove box, 1.0 mol / L lithium hexafluorophosphate was dissolved in a mixed solvent of ethylene carbonate / ethyl methyl carbonate to prepare a basic electrolyte. 96.95 parts by weight of the basic electrolyte were taken, and 2 parts by weight of polyethylene glycol diacrylate (number-average molecular weight approximately 575), 1 part by weight of modified lignin A, and 0.05 parts by weight of azobisisobutyronitrile were added. The mixture was magnetically stirred at 25°C for 2 hours at a stirring speed of 500–800 rpm to obtain a homogeneous and transparent precursor solution (appearance as shown in the image). Figure 4 (As shown). The precursor solution was injected into the electrode assembly, sealed, and polymerized at 70°C under normal pressure for 2 hours to form a gel polymer electrolyte in situ (see actual photograph). Figure 5 b).
[0037] Example 3 (The ratio of modified lignin A weight to total electrolyte weight is 0.04:1) In a nitrogen-filled glove box, 1.0 mol / L lithium hexafluorophosphate was dissolved in a mixed solvent of ethylene carbonate / ethyl methyl carbonate to prepare a basic electrolyte. 93.95 parts by weight of the basic electrolyte were taken, and 2 parts by weight of polyethylene glycol diacrylate (number-average molecular weight approximately 575), 4 parts by weight of modified lignin A, and 0.05 parts by weight of azobisisobutyronitrile were added. The mixture was magnetically stirred at 25°C for 2 hours at a stirring speed of 500–800 rpm to obtain a homogeneous and transparent precursor solution (appearance as shown in the image). Figure 4 (As shown). The precursor solution was injected into the electrode assembly, sealed, and polymerized at 70°C under normal pressure for 2 hours to form a gel polymer electrolyte in situ (see actual photograph). Figure 5 c) Comparative Example 1 (without added modified lignin) Without adding modified lignin A, only 94 parts by weight of basic electrolyte, 5 parts by weight of polyethylene glycol diacrylate, and 0.05 parts by weight of azobisisobutyronitrile were used, with the remaining steps being the same as in Example 1. See the actual product photograph. Figure 5 d.
[0038] Performance testing and characterization Chemical structure characterization The structures of unmodified alkali lignin and chemically modified lignin A were characterized by Fourier transform infrared spectroscopy (FTIR), and the results are as follows: Figure 2 As shown. The results indicate that unmodified alkali lignin at approximately 3430 cm⁻¹ - The ¹ position shows an absorption peak for the hydroxyl stretching vibration at 2925 cm⁻¹. - ¹ It has an absorption peak for aliphatic CH stretching vibration at 1600 cm⁻¹. - ¹ and 1510cm -The characteristic absorption of the lignin aromatic ring skeleton is observed at ¹. After chemical modification, the hydroxyl absorption peak of lignin changes, and a new absorption peak appears at approximately 1725 cm⁻¹. - A distinct absorption peak for the ester carbonyl C=O group appears at approximately 1635 cm⁻¹. - A characteristic absorption peak for methacrylate C=C appears at ¹; additionally, a peak appears at approximately 1240 cm⁻¹. - ¹ and 1045cm - A characteristic absorption peak related to the P=O and POC vibrations appears at position ¹. The changes in the above characteristic peaks indicate that the lignin hydroxyl groups have undergone a chemical reaction, and methacrylate and phosphate structures have been successfully introduced, indicating that chemically modified lignin A has been successfully prepared.
[0039] Electrochemical stability test The electrochemical stability window of the electrolyte was determined using linear sweep voltammetry. A stainless steel sheet was used as the working electrode, and a lithium sheet was used as both the counter and reference electrode. The scan range was 2.5–6.0 V, the scan rate was 1 mV / s, and the test temperature was 25 °C. The oxidation initiation potential was defined as the potential at which the current density significantly deviated from the baseline. The oxidative decomposition potentials of the gel polymer electrolytes prepared in Examples 1–3 and Comparative Example 1 were tested. The results are as follows: Figure 1 As shown in Table 1.
[0040] Ion conductivity test The ionic conductivity of each gel polymer electrolyte was tested using the AC impedance method. The precursor solution was injected into a stainless steel blocking electrode mold. After polymerization, AC impedance testing was performed at 25°C, with a frequency range of 1 Hz to 1 MHz and an AC amplitude of 10 mV. The ionic conductivity was calculated using the following formula: σ = L / (Rb × A), where σ is the ionic conductivity, L is the gel electrolyte thickness, Rb is the bulk resistance determined by the intersection of the high-frequency region of the AC impedance spectrum and the real axis, and A is the effective contact area between the electrode and the electrolyte. The test results are shown in Table 1.
[0041] Precursor solution dispersion stability test The precursor solutions of Examples 1-3 and Comparative Example 1 were left to stand at room temperature for 24 hours, and the appearance changes of the solutions (whether precipitation, layering, or aggregation occurred) were observed to evaluate the dispersion stability of modified lignin in the organic electrolyte. The results are as follows: Figure 3 , Figure 4 As shown. Figure 3 c represents the dissolution of 0.2g of alkali lignin (unmodified) and 0.2g of lignin A (modified) in 20g of basic electrolyte. The unmodified alkali lignin ( Figure 3 a, Figure 3 c (left side) can only partially dissolve in the basic electrolyte, with a large amount of black particulate precipitate and extremely poor dispersibility; while the lignin A modified by this invention ( Figure 3b、 Figure 3 (c on the right) can completely dissolve, forming a homogeneous, transparent, dark-colored solution. Further... Figure 4 It is evident that the precursor solutions containing different amounts of modified lignin A remained uniform, transparent, and free of precipitation and stratification after standing at room temperature for 24 hours, indicating that the modified lignin has excellent compatibility and dispersion stability with the electrolyte system.
[0042] The precursor solutions obtained in Examples 1-3 and Comparative Example 1 were subjected to in-situ polymerization, and the resulting gel polymer electrolytes are shown in the following photographs. Figure 5 As shown in the figure. As can be seen from the figure, Example 1 (with added modified lignin A) Figure 5 a) Example 2 ( Figure 5 b) and Example 3 ( Figure 5 c) Both can form self-supporting, structurally complete flexible gel films with uniform film surfaces. However, Comparative Example 1 ( Figure 5 Although d (without modified lignin) can also form a gel, its macroscopic state differs significantly from that of the lignin-added examples. This indicates that modified lignin A has good compatibility with the crosslinkable polymer matrix and can successfully copolymerize in situ to form a uniform gel electrolyte.
[0043] Battery cycle performance test The gel polymer electrolytes prepared in Examples 1-3 and Comparative Example 1 were assembled into CR2032 coin cells, using lithium iron phosphate (LiFePO4) as the positive electrode and lithium metal sheets as the negative electrode. The battery cycle test conditions were as follows: charge / discharge voltage window of 3.0–4.2V, charging method of constant current-constant voltage (CC-CV), formation rate of 0.1C, constant voltage cutoff current of 0.05C; formal cycle charge rate of 0.5C, formal cycle discharge rate of 0.5C, cycle temperature of 25°C, and 500 cycles (rated capacity is calculated as 1C = 168 mAh·g). - ¹Calculation). Record the initial discharge specific capacity, discharge specific capacity after 500 cycles, and capacity retention for each battery. Results are as follows: Figure 6 (Examples 1, 2, 3 and Comparative Example 1) and Table 1 are shown. Table 1
[0044] Depend on Figure 6As shown in Table 1, different amounts of modified lignin A significantly affect the battery cycle performance. Example 1 (modified lignin A to PEGDA mass ratio 1:1, 2 parts by weight) exhibited the highest capacity retention and the slowest discharge capacity decay after 500 cycles, demonstrating the best cycle stability; Comparative Example 1 (without modified lignin) had a capacity retention of only 88.2%. Example 2 (mass ratio 0.5:1, 1 part by weight) showed a capacity retention of only 80.5% due to insufficient modified lignin addition, which prevented the formation of sufficient flame-retardant groups and end-capping components in the gel network, leading to decreased interfacial stability. This further demonstrates that a modified lignin content of 1:1 or higher is a necessary condition for ensuring the technical effect of this invention. Furthermore, Example 3 (mass ratio 2:1, 4 parts by weight) showed a capacity retention of 89.7%, also superior to Comparative Example 1. In summary, the modification of lignin by grafting flexible flame-retardant segments and hydroxyl end-capping effectively enhances the interfacial stability of the gel electrolyte under high pressure, thereby improving the long cycle life of the battery. It also clearly shows that the preferred mass ratio of the modified lignin A to the crosslinkable polymer of the present invention is in the range of 1:1 to 2:1.
[0045] The above detailed description is a specific description of one of the feasible embodiments of the present invention. This embodiment is not intended to limit the patent scope of the present invention. All equivalent implementations or modifications that do not depart from the present invention should be included within the scope of the technical solution of the present invention.
[0046] It should be particularly noted that the various embodiments listed in this specification and accompanying drawings are intended to illustrate the technical solutions and advantages of the present invention, and not to limit the scope of protection of the present invention. Without departing from the core ideas and technical effects of the present invention, those skilled in the art can make any form of improvement, substitution, combination, or modification to the structural arrangement, process parameters, material selection, control logic, etc., of the described embodiments; any obvious changes based on the same concept should be considered equivalent solutions of the present invention and should be included within the scope of protection defined by the claims of the present invention. The actual scope of protection of the present invention is determined by the appended claims and should be correctly understood in conjunction with the specification and accompanying drawings.
Claims
1. An electrolyte additive characterized in that, The electrolyte additive is chemically modified lignin, which comprises a lignin skeleton. Flexible polymer segments are covalently linked to the lignin skeleton, and the side ends or ends of the flexible polymer segments contain phosphorus, silicon, fluorine or boron flame-retardant groups. Furthermore, the residual phenolic and alcoholic hydroxyl groups on the lignin skeleton are capped by end-capping groups.
2. The electrolyte additive according to claim 1, characterized in that, The flexible polymer segment is a homopolymer or copolymer segment formed from one or more of methyl methacrylate, butyl acrylate, and ε-caprolactone.
3. The electrolyte additive according to claim 1, characterized in that, The flame-retardant group is derived from the copolymerization of a vinyl monomer containing the group, wherein the vinyl monomer is selected from at least one of diethylphosphoryl methacrylate, vinyltrimethoxysilane, hexafluorobutyl methacrylate, and 4-vinylphenylboronic acid.
4. The electrolyte additive according to claim 1, characterized in that, The end-capping group is acetyl or benzoyl.
5. The electrolyte additive according to claim 1, characterized in that, The lignin is selected from one or more of alkali lignin, sulfate lignin, lignin sulfonate, and organic solvent lignin.
6. A process for the preparation of the electrolyte additive according to any one of claims 1 to 5, characterized in that, Includes the following steps: S1, Methacrylation: Lignin is dissolved in an organic solvent and reacted with a methacrylating agent in the presence of a catalyst and an acid-binding agent to introduce double bonds into the lignin skeleton; S2, Graft copolymerization: In the reaction system obtained in step S1, vinyl monomers containing phosphorus, silicon, fluorine or boron flame retardant groups, comonomers and polymerization initiators are added to carry out free radical copolymerization reaction to graft flexible polymer segments containing flame retardant groups onto the lignin skeleton. S3. End-capping treatment: Cool the reaction system obtained in step S2, add acetyl chloride or benzoyl chloride to carry out the end-capping reaction, and block the residual phenolic hydroxyl and alcoholic hydroxyl groups on the lignin skeleton. S4. Purification: Pour the reaction solution obtained in step S3 into a precipitant to precipitate the solid, and then wash and vacuum dry to obtain the electrolyte additive.
7. The production method according to claim 6, wherein In step S1, the catalyst is 4-dimethylaminopyridine, the acid-binding agent is triethylamine, and the methacrylating agent is methacryloyl chloride; in step S2, the polymerization initiator is azobisisobutyronitrile.
8. The preparation method according to claim 6, characterized in that, Based on 10 parts by weight of lignin: In step S1, the amount of the methacrylamide reagent is 15-25 parts by weight, the amount of the catalyst is 0.3-0.8 parts by weight, and the amount of the acid-binding agent is 3-7 parts by weight. In step S2, the amount of the vinyl monomer containing phosphorus, silicon, fluorine or boron flame retardant groups is 10-20 parts by weight, the amount of the comonomer is 20-40 parts by weight, and the amount of the polymerization initiator is 0.2-1.0 parts by weight. In step S3, the amount of acetyl chloride or benzoyl chloride used is 1-3 parts by weight.
9. A gel polymer electrolyte composition characterized in that, It comprises lithium salt, non-aqueous organic solvent, crosslinkable polymer or oligomer, polymerization initiator, and electrolyte additive as described in any one of claims 1-5.
10. The composition of claim 9, wherein, The mass ratio of the electrolyte additive to the crosslinkable polymer or oligomer is 0.05:1 to 2:
1.
11. The composition of claim 10, wherein, The mass ratio of the electrolyte additive to the crosslinkable polymer or oligomer is 1:1 to 2:
1.
12. The composition of claim 9, wherein, The cross-linkable polymer or oligomer is polyethylene glycol diacrylate or ethoxylated trimethylolpropane triacrylate; the lithium salt is lithium hexafluorophosphate; and the polymerization initiator is azobisisobutyronitrile.
13. The composition of claim 9, wherein, The non-aqueous organic solvent is a carbonate solvent.
14. A method for producing a gel polymer electrolyte, characterized by, The method comprises the following steps: S1, mixing and stirring the components in the composition according to any one of claims 9-13 to form a uniform transparent precursor solution; S2, injecting the precursor solution into a mold and polymerizing at 60-80°C under normal pressure for 1-6 hours to form a gel polymer electrolyte.