Battery
By incorporating temperature-sensitive insulating components into all-solid-state batteries, allowing them to flow or become conductive at specific temperatures, the battery can be forced to discharge before thermal runaway, thus solving the thermal runaway problem of all-solid-state batteries. This method is suitable for high-energy-density batteries such as lithium-ion batteries.
Patent Information
- Application Number
- CN202511999507.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2025-05-15
- Filing Date
- 2025-12-29
- Publication Date
- 2026-11-17
AI Technical Summary
Existing all-solid-state batteries are prone to thermal runaway at high temperatures, and the risk of thermal runaway is low for batteries in an uncharged state, lacking effective prevention and control measures.
The battery incorporates first and second insulating components that flow or become conductive when a specific temperature is reached, thereby forcing discharge before the battery reaches thermal runaway and connecting to the outer casing through the positive and negative current collector layers.
It effectively suppresses thermal runaway of electrode stacks, reduces battery temperature through forced discharge, and reduces the risk of thermal runaway. It is suitable for high energy density batteries such as lithium-ion batteries.
Smart Images

Figure CN123120905A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to a battery. Background Technology
[0002] Batteries are manufactured by housing electrode stacks within an outer casing. The outer casing is primarily used to protect the electrode stacks. Various suggestions have been made regarding the structure of the outer casing to improve battery quality.
[0003] Patent Document 1 discloses an all-solid-state battery comprising: an all-solid-state battery element having one or more unit cells having a negative electrode current collector layer, a negative electrode active material layer, a solid electrolyte layer, a positive electrode active material layer, and a positive electrode current collector layer sequentially arranged therein; a metal casing having an opening at at least one end and housing the all-solid-state battery element; a resin sealant sealing the opening and contacting the surface of the all-solid-state battery element opposite to the opening; and negative electrode current collector layer protrusions and positive electrode current collector layer protrusions from the resin sealant toward a side opposite to the all-solid-state battery element, wherein the resin sealant penetrates into at least a portion of the gap between the outer periphery of the all-solid-state battery element and the inner periphery of the metal casing to form a gap filler. According to the invention of Patent Document 1, an all-solid-state battery that suppresses degradation of the all-solid-state battery can be provided.
[0004] Patent Document 1: Japanese Patent Application Publication No. 2018-116917 Summary of the Invention
[0005] If a charged battery becomes excessively hot due to overcharging or thermal cascading from other connected batteries, for example, the positive electrode active material may thermally decompose, releasing oxygen and generating heat, potentially leading to thermal runaway. On the other hand, the risk of thermal runaway in an uncharged battery is extremely low compared to that of a charged battery.
[0006] Therefore, in order to suppress thermal runaway and prevent further cascading to other connected batteries, it is preferable to force the battery to discharge before reaching the temperature that would cause thermal runaway.
[0007] Therefore, the object of the present invention is to provide a battery capable of suppressing thermal runaway.
[0008] The present invention achieves the above objectives through the following solutions.
[0009] <Method 1>
[0010] A battery having an electrode stack and an outer casing housing the electrode stack, wherein the battery,
[0011] The aforementioned electrode stack comprises, in sequence, a positive current collector layer, a positive active material layer, a solid electrolyte layer or a separator layer, a negative active material layer, and a negative current collector layer.
[0012] (i) The positive current collector layer contacts the outer casing via the first insulating member, and when the first insulating member reaches a first predetermined temperature or above, the first insulating member flows and / or becomes conductive, thereby making the positive current collector layer electrically contact the outer casing, and thus the positive current collector layer and the negative current collector layer are connected via the outer casing, and / or (ii) The negative current collector layer contacts the outer casing via the second insulating member, and when the second insulating member reaches a second predetermined temperature or above, the second insulating member flows and / or becomes conductive, thereby making the negative current collector layer electrically contact the outer casing, and thus the positive current collector layer and the negative current collector layer are connected via the outer casing.
[0013] <Method 2>
[0014] According to the battery of method 1, the first specified temperature and / or the second specified temperature is 140°C or higher and less than 200°C.
[0015] <Method 3>
[0016] According to the battery described in method 1 or 2, wherein,
[0017] The aforementioned electrode stack has, sequentially on both sides of the aforementioned positive electrode current collector layer, the aforementioned positive electrode active material layer, the aforementioned solid electrolyte layer, the aforementioned negative electrode active material layer, and the aforementioned negative electrode current collector layer, or
[0018] The electrode stack has, in sequence, the negative electrode active material layer, the solid electrolyte layer, the positive electrode active material layer, and the positive electrode current collector layer on both sides of the negative electrode current collector layer.
[0019] <Method 4>
[0020] The battery according to any one of methods 1 to 3, wherein,
[0021] (i) The first insulating component is made of a first resin material, whereby when the first insulating component reaches or exceeds the first specified temperature, the first insulating component flows, thereby making electrical contact between the positive current collector layer and the outer casing, thus enabling the positive current collector layer and the negative current collector layer to conduct through the outer casing, and / or
[0022] (ii) The second insulating component is made of a second resin material, whereby when the second insulating component reaches or exceeds the second specified temperature, the second insulating component flows, thereby making electrical contact between the positive current collector layer and the outer casing, and thus the positive current collector layer and the negative current collector layer are connected through the outer casing.
[0023] <Method 5>
[0024] The battery according to any one of methods 1 to 4, wherein,
[0025] The temperature specified in section 1 above is different from the temperature specified in section 2 above.
[0026] Invention Effects
[0027] According to the present invention, a battery capable of suppressing thermal runaway of the electrode stack can be provided. Attached Figure Description
[0028] Figure 1 This is a side sectional view used to illustrate the battery of the present invention. Detailed Implementation
[0029] The embodiments of the present invention will now be described in detail. However, the present invention is not limited to the following embodiments, and various modifications can be made within the scope of the spirit of the invention.
[0030] "Battery"
[0031] A battery having an electrode stack and an outer casing housing the electrode stack, wherein the battery,
[0032] The aforementioned electrode stack comprises, in sequence, a positive current collector layer, a positive active material layer, a solid electrolyte layer or a separator layer, a negative active material layer, and a negative current collector layer.
[0033] (i) The positive current collector layer contacts the outer casing via the first insulating member, and when the first insulating member reaches a first predetermined temperature or above, the first insulating member flows and / or becomes conductive, thereby making the positive current collector layer electrically contact the outer casing, and thus the positive current collector layer and the negative current collector layer are connected via the outer casing, and / or (ii) The negative current collector layer contacts the outer casing via the second insulating member, and when the second insulating member reaches a second predetermined temperature or above, the second insulating member flows and / or becomes conductive, thereby making the negative current collector layer electrically contact the outer casing, and thus the positive current collector layer and the negative current collector layer are connected via the outer casing.
[0034] According to the present invention, a battery capable of suppressing thermal runaway of the electrode stack can be provided.
[0035] The inventors have discovered that by making the positive current collector layer contact the outer casing via a first insulating member and / or making the negative current collector layer contact the outer casing via a second insulating member, it is possible to force the battery to discharge before it reaches a temperature that would cause thermal runaway.
[0036] Specifically, for example, such as Figure 1 As shown in (a), the battery 100 has an electrode stack 200 and an outer casing 300 that houses the electrode stack 200. The electrode stack 200 sequentially comprises a positive current collector layer 210, a positive active material layer 220, a solid electrolyte layer 230, a negative active material layer 240, and a negative current collector layer 250. The positive current collector layer 210 is in contact with the outer casing 300 via a first insulating member 400. The negative current collector layer 250 is in contact with the outer casing 300 via a second insulating member 500.
[0037] In Figure 1 In the battery 100 shown in (a), when the temperature of the positive electrode active material layer 220 is lower than the first predetermined temperature, the first insulating member 400 exhibits insulation properties, thus insulating the positive electrode current collector layer 210 from the outer casing 300. Furthermore, when the temperature of the first insulating member 400 reaches or exceeds the first predetermined temperature, the first insulating member 400 melts and flows. As a result, the positive electrode current collector layer 210 makes electrical contact with the outer casing 300.
[0038] Furthermore, when the temperature of the negative electrode active material layer 240 is lower than the second predetermined temperature, the second insulating component 500 exhibits insulation properties, thus insulating the negative electrode current collector layer 250 from the outer casing 300. Moreover, when the temperature of the second insulating component 500 of the battery 100 reaches or exceeds the second predetermined temperature, the second insulating component 500 melts and flows. As a result, the negative electrode current collector layer 250 makes electrical contact with the outer casing 300.
[0039] Here, the first and second specified temperatures can be set to be lower than the temperature at which the positive active material in the positive active material layer 220 and / or the negative active material in the negative active material layer 240 reach thermal runaway.
[0040] Therefore, when the temperature of the first insulating component 400 of the battery 100 becomes higher than the first predetermined temperature and the temperature of the second insulating component 500 of the battery 100 becomes higher than the second predetermined temperature, the positive current collector layer 210 and the negative current collector layer 250 become connected via the outer casing 300, thus forcing the battery 100 to discharge. Furthermore, during this discharge, the outer casing 300 becomes hot, but because the outer casing 300 has more contact with the outside air, it can be easily cooled.
[0041] The constituent elements of the present invention will be described below.
[0042] The battery of the present invention has an electrode stack and an outer casing for accommodating the electrode stack. Furthermore, the battery has a first insulating member and / or a second insulating member. That is, the battery may have only one of the first insulating member and the second insulating member. Moreover, the battery may arbitrarily have a sealing body and a gap filler.
[0043] The battery of this invention can be a solid-state battery. Regarding this invention, a "solid-state battery" refers to a battery that uses at least a solid electrolyte as the electrolyte; therefore, a solid-state battery uses a combination of a solid electrolyte and a liquid electrolyte as the electrolyte. Furthermore, in this invention, a "solid-state battery" can be an all-solid-state battery, that is, a battery that uses only a solid electrolyte as the electrolyte. Solid-state batteries do not have a shut-off function in the event of abnormal heating, unlike the separator layer in liquid-state batteries; therefore, thermal runaway countermeasures are highly necessary.
[0044] The battery of the present invention can be applied, for example, to lithium-ion batteries. Lithium-ion batteries have high energy density, therefore, they release high energy during thermal runaway, making thermal runaway countermeasures highly necessary.
[0045] <Insulating Components>
[0046] The first insulating component is disposed in contact between the positive current collector layer and the outer casing of the electrode laminate. Furthermore, the second insulating component is disposed in contact between the negative current collector layer and the outer casing of the electrode laminate.
[0047] The first insulating component exhibits non-conductivity below a first specified temperature and flows and / or exhibits conductivity above the first specified temperature. Flow is transmitted through the first insulating component, which is absent in at least a portion between the positive current collector layer and the outer casing. Thus, the positive current collector layer is in direct contact with the outer casing. Furthermore, the second insulating component exhibits non-conductivity below a second specified temperature and flows and / or exhibits conductivity above the second specified temperature. The first and second insulating components may be made of the same material or different materials.
[0048] The first insulating component may be made of a first resin material. The first resin material flows when it reaches or exceeds a first predetermined temperature. Furthermore, the second insulating component may be made of a second resin material. The second resin material flows when it reaches or exceeds a second predetermined temperature. Here, the first and second resin materials can flow by melting.
[0049] The first and second resin materials can be, for example, high-density polyethylene (melting point: 141°C), polypropylene (melting point: 160°C), etc.
[0050] The first and second insulating components can be made of materials that exhibit conductivity at high temperatures. An anisotropic conductive film (ACF) is an example of such a material. Therefore, the first insulating component is conductive above a first predetermined temperature. Thus, the positive current collector layer and the outer casing are electrically connected via the first insulating component. Similarly, the second insulating component is conductive above a second predetermined temperature, thus the negative current collector layer and the outer casing are electrically connected via the second insulating component.
[0051] Anisotropic conductive film (ACF) is a film composed of a thermosetting resin containing multiple conductive particles. Normally, the conductive particles are insulated by the thermosetting resin, thus the anisotropic conductive film (ACF) exhibits insulating properties. However, if pressure is applied in a direction perpendicular to the film surface, the thermosetting resin is compressed, the insulation of the conductive particles is disrupted, and conductivity appears in that direction. The electrode stack expands at high temperatures and is constrained by an outer casing; therefore, the anisotropic conductive film (ACF) exhibits conductivity when pressure is applied at high temperatures. Examples of conductive particles include nickel particles, gold particles, and silver particles; examples of thermosetting resins include epoxy resin and acrylic resin.
[0052] The shapes of the first and second insulating components are not particularly limited; for example, they can be membrane-like or gasket-like.
[0053] The thickness of the first and second insulating components in the stacking direction of the electrode stack can be appropriately determined at high temperatures to a thickness that enables the positive current collector layer and / or the negative current collector layer to conduct electricity with the outer casing. The aforementioned thickness can be, for example, 0.1 mm or more, 0.3 mm or more, 0.5 mm or more, or less than 10 mm, less than 5 mm, or less than 1 mm.
[0054] The first specified temperature is a temperature lower than the temperature at which the positive electrode active material layer of the electrode laminate reaches thermal runaway, and preferably higher than the temperature range typically used by the positive electrode active material layer. For example, the aforementioned temperature can be 100°C or higher, 120°C or higher, 140°C or higher, 150°C or higher, or 160°C or higher, or it can be 240°C or lower, 220°C or lower, 200°C or lower, 180°C or lower, or 170°C or lower.
[0055] The second specified temperature is a temperature lower than the temperature at which the negative electrode active material layer of the electrode laminate reaches thermal runaway, and preferably higher than the temperature range typically used by the negative electrode active material layer. For example, the aforementioned temperature can be 100°C or higher, 120°C or higher, 140°C or higher, 150°C or higher, or 160°C or higher, or it can be 220°C or lower, 200°C or lower, 180°C or lower, or 170°C or lower.
[0056] The first specified temperature and the second specified temperature may be different. Preferably, the first and second specified temperatures are determined based on the respective heating tendencies of the positive and negative active material layers of the electrode laminate, and the first and second insulating components are selected accordingly.
[0057] <Exterior body>
[0058] The outer casing houses the electrode stack. From the viewpoint of enabling conductivity between the positive and negative current collector layers via the outer casing, the outer casing preferably has electrical conductivity. The outer casing can be, for example, a metallic material. Examples of metallic materials include aluminum, aluminum alloys, steel, and stainless steel, as well as combinations thereof.
[0059] The outer casing can be a molded body formed by plastic processing of sheet metal, a welded body formed by joining sheet metal, or a composite welded body formed by joining a molded body and a sheet metal. An insulating coating can be applied to the surface of the outer casing.
[0060] The outer casing may have an opening. The opening is provided for inserting the electrode stack. Furthermore, the opening may be sealed by a sealing body. The sealing body may be a curable resin. Examples of curable resins include epoxy resin and acrylic resin.
[0061] The outer casing preferably has a thickness that does not deform during normal use of the battery. The thickness of the outer casing can be, for example, 0.5 mm or more, 1.0 mm or more, 1.5 mm or more, 2.0 mm or more, or 3.0 mm or more, or less than 10.0 mm, 9.0 mm or less, 8.0 mm or less, 7.0 mm or less, or 6.0 mm or less.
[0062] The gap between the outer casing and the electrode stack is preferably set to a level that allows a first insulating member and / or a second insulating member to be disposed between the outer casing and the electrode stack. The gap may be, for example, 0.1 mm or more, 0.3 mm or more, 0.5 mm or more, or less than 10 mm, less than 5 mm, or less than 1 mm.
[0063] In the gap between the outer casing and the electrode stack, a gap filler can be disposed within a range that does not impede the conductivity between the positive and / or negative current collector layers of the electrode stack and the outer casing when heated. This suppresses short circuits or battery damage caused by movement of the electrode stack within the outer casing. The gap filler can be a curable resin. Examples of curable resins include epoxy resin and acrylic resin.
[0064] <Electrode stack>
[0065] The electrode stack sequentially comprises a positive electrode current collector layer, a positive electrode active material layer, and a solid electrolyte layer or a solid electrolyte layer, a negative electrode active material layer, and a negative electrode current collector layer. The electrode stack may also optionally include a liquid electrolyte. Here, in the case of a solid-state battery, the electrode stack has a solid electrolyte layer; in the case of a liquid-system battery, the electrode stack has a separator layer.
[0066] The positive current collector layer is in contact with the outer casing via a first insulating member, and / or the negative current collector layer is in contact with the outer casing via a second insulating member. With both the first and second insulating members configured, the outer casing is not charged within the temperature range during normal battery operation.
[0067] When the positive current collector layer and the outer casing are in contact via the first insulating component, the first insulating component becomes fluid and / or becomes conductive when it reaches a temperature above the first specified temperature, thereby making electrical contact between the positive current collector layer and the outer casing, and connecting the positive current collector layer and the negative current collector layer via the outer casing.
[0068] When the negative current collector layer and the outer casing are in contact via the second insulating component, the second insulating component becomes fluid and / or becomes conductive when it reaches a second specified temperature, thereby making electrical contact between the negative current collector layer and the outer casing, and connecting the positive current collector layer and the negative current collector layer via the outer casing.
[0069] like Figure 1 As shown in (b), the electrode stack may have a positive active material layer 220, a solid electrolyte layer 230, a negative active material layer 240 and a negative current collector layer 250 on both sides of the positive current collector layer 210, respectively.
[0070] like Figure 1 As shown in (c), the electrode stack may have a negative electrode active material layer 240, a solid electrolyte layer 230, a positive electrode active material layer 220 and a positive electrode current collector layer 210 on both sides of the negative electrode current collector layer 250, respectively.
[0071] (Positive current collector layer)
[0072] The material used in the positive electrode current collector layer is not particularly limited, and materials commonly used as positive electrode current collectors in solid-state batteries can be appropriately adopted. Examples of materials used in the positive electrode current collector layer include Cu, Ni, Cr, Au, Pt, Ag, Al, Fe, Ti, Zn, Co, and stainless steel, but are not limited to these. Furthermore, the positive electrode current collector layer may have a coating layer on its surface for purposes such as adjusting resistance. Moreover, the positive electrode current collector layer may be a layer on which the aforementioned metals are deposited or vapor-deposited onto a metal foil or substrate.
[0073] The shape of the positive current collector layer is not particularly limited, and can be, for example, foil, plate, or mesh. Among these, foil is preferred. The thickness of the positive current collector layer is not particularly limited, and can be 0.1 μm or more, 1 μm or more, 1 mm or less, or 100 μm or less.
[0074] like Figure 1 As shown in (b), the positive current collector layer can be disposed through the outer casing 300. Furthermore, the conductive material connected to the positive current collector layer can penetrate the outer casing.
[0075] (Positive electrode active material layer)
[0076] The positive electrode active material layer contains at least positive electrode active material, and may optionally also contain binders, solid electrolytes, and conductive additives. The positive electrode active material may also contain various additives. The content of positive electrode active material, binders, solid electrolytes, conductive additives, etc., in the positive electrode active material layer can be appropriately determined based on the target battery performance.
[0077] The materials used for the positive electrode active material are not particularly limited as long as they can adsorb and release lithium ions. Examples of positive electrode active materials include lithium cobalt oxide (LiCoO2), lithium nickel oxide (LiNiO2), lithium manganese oxide (LiMn2O4), lithium iron phosphate (LFP), lithium manganese iron phosphate (LMFP), and lithium nickel cobalt manganese oxide (NCM:LiCO3). 1 / 3 Ni 1 / 3 Mn 1 / 3 O2), Lithium nickel cobalt aluminate (LiNi) 0.8 (CoAl) 0.2 O2), Li 1+x Mn 2-x-y M y O4 (where M is one or more metallic elements selected from Al, Mg, Co, Fe, Ni and Zn) represents heteroelemental substitutions for Li-Mn spinel, etc., but is not limited to these.
[0078] The shape of the positive electrode active material is not particularly limited as long as it is a typical shape used for positive electrode active materials in batteries. For example, the positive electrode active material can be in particle form. It can be primary particles or secondary particles formed by the aggregation of multiple primary particles. The average particle size D of the positive electrode active material... 50 For example, it can be 1 nm or larger, 5 nm or larger, or 10 nm or larger, and it can also be less than 500 μm, less than 100 μm, less than 50 μm, or less than 30 μm. Additionally, the particle size D... 50 The median particle size is the particle size at 50% of the cumulative value in the particle size distribution of the volume reference obtained by laser diffraction / scattering.
[0079] The material of the adhesive is not particularly limited. Adhesives can be, for example, polyvinylidene fluoride (PVdF), butadiene rubber (BR), polytetrafluoroethylene (PTFE), styrene-butadiene rubber (SBR), etc., but are not limited to these. There are no particular limitations on the adhesive; only one type can be used, or two or more types can be used in combination.
[0080] The material of a solid electrolyte is not particularly limited; for example, it can be a sulfide solid electrolyte, an oxide solid electrolyte, or a polymer electrolyte.
[0081] Examples of sulfide solid electrolytes include amorphous sulfide solid electrolytes, crystalline sulfide solid electrolytes, and sulfide-germanium ore type solid electrolytes, but are not limited to these. Specific examples of sulfide solid electrolytes include the Li₂S-P₂S₅ system (Li₇P₃S₅). 11 , Li3PS4, Li8P2S9, etc.), Li2S-SiS2, LiI-Li2S-SiS2, LiI-Li2S-P2S5, LiI-LiBr-Li2S-P2S5, Li2S-P2S5-GeS2 (Li 13 GeP3S 16 Li 10 GeP2S 12 etc.), LiI-Li2S-P2O5, LiI-Li3PO4-P2S5, Li 7-x PS 6-x Cl x etc.; or combinations thereof, but not limited to these.
[0082] Examples of oxide solid electrolytes include Li7La3Zr2O 12 Li 7-x La3Zr 1-x Nb x O 12 Li 7- 3x La3Zr2Al x O 12 Li 3x La 2 / 3-x TiO3, Li 1+x Al x Ti 2-x (PO4)3, Li 1+x Al x Ge 2-x (PO4)3, Li3PO4 or Li 3+x PO 4-x N x (LiPON), etc.; or combinations thereof, but not limited to these.
[0083] Sulfide solid electrolytes and oxide solid electrolytes can be glass or crystallized glass (glass ceramics).
[0084] Examples of polymer electrolytes include polyethylene oxide (PEO), polypropylene oxide (PPO), and their copolymers, but are not limited to these.
[0085] The conductive additive is not particularly limited. Examples of conductive additives include vapor-grown carbon fiber (VGCF), acetylene black (AB), Ketjen black (KB), carbon nanotubes (CNT), and carbon nanofibers (CNF), but are not limited to these. The conductive additive can be in particle or fibrous form, and its size is not particularly limited. The conductive additive is not particularly limited; only one type can be used, or two or more types can be used in combination.
[0086] The positive electrode active material layer can be manufactured using known methods. For example, it can be manufactured by dry or wet molding a composite material containing the positive electrode active material layer onto the positive electrode current collector layer.
[0087] (Diaphragm layer)
[0088] There are no particular limitations on the separator layer; any separator commonly used as a battery separator can be used. For example, nonwoven fabrics such as polyolefin-based, polyamide-based, and polyimide-based separators can be used as separators.
[0089] (Solid electrolyte layer)
[0090] The solid electrolyte layer contains at least a solid electrolyte and may optionally also contain a binder. The solid electrolyte layer may also contain various additives. The content of the solid electrolyte, binder, etc., in the solid electrolyte layer can be appropriately determined based on the target battery performance. For information on solid electrolytes and binders, please refer to the relevant descriptions of the positive electrode active material layer described above.
[0091] Solid electrolyte layers can be manufactured using known methods. For example, they can be manufactured by dry or wet molding of a composite material containing a solid electrolyte layer onto a substrate.
[0092] (Negative electrode active material layer)
[0093] The negative electrode active material layer contains at least negative electrode active material, and may optionally also contain binders, solid electrolytes, and conductive additives. The negative electrode active material layer may also contain various additives. The content of negative electrode active material, binders, solid electrolytes, conductive additives, etc., in the negative electrode active material layer can be appropriately determined based on the target battery performance. For information on binders, solid electrolytes, and conductive additives, please refer to the relevant descriptions of the positive electrode active material layer described above.
[0094] As the negative electrode active material, it can be a material whose lithium ion adsorption / release potential (charge / discharge potential) is lower than that of the positive electrode active material of the present invention. The material of the negative electrode active material is not particularly limited; it can be metallic lithium or a material capable of adsorbing and releasing metal ions such as lithium ions. Examples of materials capable of adsorbing and releasing metal ions such as lithium ions include alloy-based negative electrode active materials, carbon materials, or lithium titanate (Li4Ti5O). 12 (etc.), but not limited to these.
[0095] There are no particular limitations on alloy-based anode active materials; examples include Si alloy-based and Sn alloy-based anode active materials. Si alloy-based anode active materials include silicon, silicon oxides, silicon carbides, silicon nitrides, or their solid solutions. Furthermore, Si alloy-based anode active materials can contain metallic elements other than silicon, such as Fe, Co, Sb, Bi, Pb, Ni, Cu, Zn, Ge, In, Sn, and Ti. Sn alloy-based anode active materials include tin, tin oxides, tin nitrides, or their solid solutions. Furthermore, Sn alloy-based anode active materials can contain metallic elements other than tin, such as Fe, Co, Sb, Bi, Pb, Ni, Cu, Zn, Ge, In, Ti, and Si.
[0096] There are no particular limitations on carbon materials; examples include hard carbon, soft carbon, and graphite.
[0097] There are no particular limitations on the shape of the negative electrode active material; any shape commonly used as a negative electrode active material in batteries is acceptable. For example, the negative electrode active material can be in particle or sheet form.
[0098] The negative electrode active material layer can be manufactured using known methods. For example, it can be manufactured by dry or wet molding a composite material containing the negative electrode active material layer onto the negative electrode current collector layer.
[0099] (Negative electrode current collector layer)
[0100] The materials used in the negative electrode current collector layer are not particularly limited, and materials commonly used as negative electrode current collectors in solid-state batteries can be appropriately adopted. Examples of materials used in the negative electrode current collector layer include Cu, Ni, Cr, Au, Pt, Ag, Al, Fe, Ti, Zn, Co, stainless steel, or carbon sheets, but are not limited to these. The negative electrode current collector layer may have a coating layer on its surface for purposes such as adjusting resistance.
[0101] The shape of the negative electrode current collector layer is not particularly limited, and can be, for example, foil, plate, or mesh. Among these, foil is preferred. The thickness of the negative electrode current collector layer is not particularly limited, and can be 0.1 μm or more, 1 μm or more, or less than 1 mm or less than 100 μm.
[0102] like Figure 1 As shown in (c), the negative current collector layer can be disposed through the outer casing 300. Furthermore, the conductive material connected to the positive current collector layer can penetrate the outer casing.
[0103] <Liquid Electrolytes>
[0104] There are no particular limitations on liquid electrolytes, but it is preferred that they contain a supporting salt and a solvent.
[0105] Lithium salts, which serve as supporting salts for liquid electrolytes with lithium-ion conductivity, are not particularly limited and can include inorganic lithium salts and organic lithium salts. Examples of inorganic lithium salts include LiPF6, LiBF4, LiClO4, and LiAsF6, but are not limited to these. Examples of organic lithium salts include LiCF3SO3, LiN(CF3SO2)2, LiN(C2F5SO2)2, LiN(FSO2)2, and LiC(CF3SO2)3, but are not limited to these.
[0106] There are no particular limitations on the solvent used in the liquid electrolyte, and examples include cyclic carbonates and chain carbonates. Examples of cyclic carbonates include ethylene carbonate (EC), propylene carbonate (PC), and butene carbonate (BC), but these are not limited to these. Examples of chain carbonates include dimethyl carbonate (DMC), diethyl carbonate (DEC), and methyl ethyl carbonate (EMC), but these are not limited to these. There are no particular limitations on the liquid electrolyte; only one type can be used, or two or more types can be used in combination.
[0107] The battery of the present invention can be manufactured using known methods. For example, it can be manufactured by placing a first or second insulating member on the positive current collector layer and / or the negative current collector layer of the electrode stack, inserting it into the outer casing through the opening of the outer casing, and then sealing the opening with a sealing part.
[0108] Symbol Explanation
[0109] 100 - Battery, 200 - Electrode stack, 210 - Positive current collector layer, 220 - Positive active material layer, 230 - Solid electrolyte layer, 240 - Negative active material layer, 250 - Negative current collector layer, 300 - Outer casing, 400 - First insulating component, 500 - Second insulating component.
Claims
1. A battery having an electrode stack and an outer casing housing the electrode stack, characterized in that, The electrode stack comprises, in sequence, a positive current collector layer, a positive active material layer, a solid electrolyte layer or a separator layer, a negative active material layer, and a negative current collector layer. (i) The positive current collector layer contacts the outer casing via a first insulating member, and when the first insulating member reaches a first predetermined temperature or above, the first insulating member flows and / or becomes conductive, thereby making electrical contact between the positive current collector layer and the outer casing, thus establishing a connection between the positive current collector layer and the negative current collector layer via the outer casing, and / or (ii) The negative current collector layer is in contact with the outer casing via the second insulating component, and when the second insulating component reaches a second specified temperature or above, the second insulating component flows and / or becomes conductive, thereby making the negative current collector layer electrically contact the outer casing, and thus the positive current collector layer and the negative current collector layer are connected via the outer casing.
2. The battery according to claim 1, characterized in that, The first specified temperature and / or the second specified temperature are above 140°C and below 200°C.
3. The battery according to claim 1 or 2, characterized in that, The electrode stack has, sequentially on both sides of the positive electrode current collector layer, the positive electrode active material layer, the solid electrolyte layer, the negative electrode active material layer, and the negative electrode current collector layer, or The electrode stack has, in sequence, the negative electrode active material layer, the solid electrolyte layer, the positive electrode active material layer, and the positive electrode current collector layer on both sides of the negative electrode current collector layer.
4. The battery according to claim 1 or 2, characterized in that, (i) The first insulating component is made of a first resin material, whereby the first insulating component flows when it reaches above the first predetermined temperature, thereby making electrical contact between the positive current collector layer and the outer casing, thus enabling the positive current collector layer and the negative current collector layer to conduct through the outer casing, and / or (ii) The second insulating component is made of a second resin material, whereby the second insulating component flows when it reaches or exceeds the second specified temperature, thereby making electrical contact between the positive current collector layer and the outer casing, and thus the positive current collector layer and the negative current collector layer are connected via the outer casing.
5. The battery according to claim 1 or 2, characterized in that, The first specified temperature is different from the second specified temperature.