Semiconductor structure and its formation method
By forming a first sidewall on the sidewall of the peripheral gate structure and protecting the peripheral gate structure during the formation of the first dielectric layer, the problem of negative bias temperature instability of NAND flash memory devices is solved, and the yield of semiconductor structures is improved.
Patent Information
- Application Number
- CN202510639450.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-16
- Publication Date
- 2026-11-17
AI Technical Summary
NAND flash memory devices suffer from negative bias temperature instability, which affects the yield of semiconductor structures.
A first sidewall is formed on the sidewall of the peripheral gate structure, and a barrier layer is used to protect the peripheral gate structure. During the formation of the first dielectric layer, the influence on the peripheral gate structure is reduced, and an air gap is formed between adjacent word line gate structures.
It improves the negative bias temperature instability and increases the yield of semiconductor structures.
Smart Images

Figure CN123124355A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor manufacturing, and more particularly to a semiconductor structure and a method for forming the same. Background Technology
[0002] Flash memory, also known as flash storage, has become the mainstream of non-volatile memory (NVM). The main characteristics of flash memory are its ability to retain stored information for extended periods without power, and it offers advantages such as high integration density, fast access speed, and ease of erasing and rewriting. Therefore, it has been widely used in microcomputers, automation control, and many other fields.
[0003] Depending on their structure, flash memory can be divided into two types: NOR Flash and NAND Flash. NAND flash memory, due to its advantages such as higher cell density, higher storage density, and faster write and erase speeds, has gradually become the most commonly used structure in flash memory, currently mainly used in flash memory cards for digital cameras and MP3 players.
[0004] However, the performance of NAND flash memory devices still needs to be improved. Summary of the Invention
[0005] The problem solved by the embodiments of the present invention is to provide a semiconductor structure and a method for forming the same, which helps to improve the problem of negative bias temperature instability of semiconductor devices and improve the yield of semiconductor structures.
[0006] To address the aforementioned problems, embodiments of the present invention provide a method for forming a semiconductor structure, comprising: providing a substrate, the substrate including a cell region and a peripheral region, a peripheral gate structure formed on the substrate of the peripheral region, a word line gate structure formed on the substrate of the cell region, and a first sidewall formed on the sidewall of the peripheral gate structure and between adjacent word line gate structures; forming a barrier layer on top of the first sidewall of the peripheral region, the barrier layer having a first opening located in the cell region, and the first opening being located above the first sidewall between adjacent word line gate structures; under the blocking effect of the barrier layer, removing the first sidewall at the bottom of the first opening to form a trench between adjacent word line gate structures; after removing the first sidewall at the bottom of the first opening, forming a first dielectric layer on top of the word line gate structure, the first sidewall, and the peripheral gate structure, the first dielectric layer sealing the top of the trench to form an air gap between adjacent word line gate structures.
[0007] Accordingly, embodiments of the present invention also provide a semiconductor structure, comprising: a substrate, the substrate including a peripheral region and a cell region; a peripheral gate structure located on the substrate of the peripheral region; a word line gate structure located on the substrate of the cell region, and adjacent word line gate structures and the substrate forming a trench; a first sidewall located on the sidewall of the peripheral gate structure; and a first dielectric layer located on top of the word line gate structure, the first sidewall, and the peripheral gate structure, the first dielectric layer sealing the top of the trench, and the first dielectric layer, adjacent word line gate structures, and the substrate forming an air gap.
[0008] Compared with the prior art, the technical solution of the embodiments of the present invention has the following advantages:
[0009] This invention provides a method for forming a semiconductor structure, comprising: forming a first sidewall on the sidewall of a peripheral gate structure and between adjacent word line gate structures; forming a barrier layer on top of the first sidewall in the peripheral region, the barrier layer having a first opening located in the cell region, and the first opening being located above the first sidewall between adjacent word line gate structures; removing the first sidewall at the bottom of the first opening to form a trench between adjacent word line gate structures; after removing the first sidewall at the bottom of the first opening under the blocking effect of the barrier layer, forming a first dielectric layer on top of the word line gate structure, the first sidewall, and the peripheral gate structure, the first dielectric layer sealing the top of the trench to form an air gap between adjacent word line gate structures; in this embodiment, since the sidewall of the peripheral gate structure has the first sidewall, the first sidewall can protect the peripheral gate structure during the process of forming the first dielectric layer, reducing the impact of the process on the peripheral gate structure, thereby improving the problem of negative bias temperature instability (NBTI) and improving the yield of the semiconductor structure.
[0010] Accordingly, this embodiment of the invention also provides a semiconductor structure, including: a substrate, the substrate including a peripheral region and a cell region; a peripheral gate structure located on the substrate of the peripheral region; a word line gate structure located on the substrate of the cell region, and adjacent word line gate structures and the substrate forming a trench; a first sidewall located on the sidewall of the peripheral gate structure; a first dielectric layer located on top of the word line gate structure, the first sidewall and the peripheral gate structure, the first dielectric layer sealing the top of the trench, and the first dielectric layer, adjacent word line gate structures and the substrate forming an air gap; in this embodiment, since the sidewall of the peripheral gate structure has the first sidewall, the first sidewall can protect the peripheral gate structure during the process of forming the first dielectric layer, reducing the impact of the process on the peripheral gate structure, thereby improving the problem of negative bias temperature instability and improving the yield of the semiconductor structure. Attached Figure Description
[0011] Figures 1 to 6 This is a schematic diagram of the structure corresponding to each step in a method for forming a semiconductor structure.
[0012] Figure 7 Is adopted Figures 1 to 6 Log-normal distribution of negative bias temperature instability of the semiconductor structure formed by the formation method;
[0013] Figures 8 to 13 This is a schematic diagram of the structure corresponding to each step in one embodiment of the method for forming a semiconductor structure of the present invention;
[0014] Figure 14 This is a log-normal distribution diagram of the negative bias temperature instability of a semiconductor structure formed using a method according to an embodiment of the present invention;
[0015] Figure 15 This is a schematic diagram of a semiconductor structure according to an embodiment of the present invention. Detailed Implementation
[0016] Currently, the problem of negative bias temperature instability in semiconductor devices still needs to be improved. This paper analyzes the reasons why the performance of semiconductor structures needs improvement, using schematic diagrams of each step in a semiconductor structure formation method.
[0017] Figures 1 to 6 This is a schematic diagram of the structure corresponding to each step in a method for forming a semiconductor structure, wherein (a) represents a schematic diagram of the cell region and (b) represents a schematic diagram of the peripheral region.
[0018] refer to Figure 1 A substrate 10 is provided, the substrate 10 including cell regions i [e.g. Figure 1 (a) is shown] and the outer area ii [as shown in] Figure 1As shown in (b), a peripheral gate structure 11 is formed on the substrate 10 of the peripheral region ii, a word line gate structure 12 is formed on the substrate 10 of the cell region i, a first sidewall 14 is formed on the sidewall of the peripheral gate structure 11 and between adjacent word line gate structures 12, a gate mask layer 15 is formed on the top of the peripheral gate structure 11 and the word line gate structure 12, and a second sidewall 22 is formed between the peripheral gate structure 11 and the first sidewall 14 and between the word line gate structure 12 and the first sidewall 14.
[0019] refer to Figure 2 A barrier layer 16 is formed in the outer perimeter region ii, and the barrier layer 16 has a first opening 17 located in the unit region i [e.g. Figure 2 (a) shown] and the second opening 18 located in the outer area ii [as shown in] Figure 2 As shown in (b), the first opening 17 exposes the first sidewall 14 between adjacent word line gate structures 12 and the word line gate structure 12, and the second opening 18 exposes the first sidewall 14 on the sidewall of the peripheral gate structure 11 and the peripheral gate structure 11.
[0020] Continue to refer to Figure 2 Remove the first opening 17 [e.g.] Figure 2 (a) shows the bottom and the second opening 18 [as shown in] Figure 2 (b) shows the bottom gate mask layer 15.
[0021] It should be noted that the step of removing the gate mask layer 15 at the bottom of the first opening 17 and the bottom of the second opening 18 also includes: removing a portion of the thickness of the first sidewall 14 at the bottom of the first opening 17 [e.g.] Figure 2 [as shown in (a)] and the first sidewall 14 with part of the thickness removed from the bottom of the second opening 18 [as shown in] Figure 2 (b) shows the second sidewall 22 with the remaining thickness of the first sidewall 14 in unit area i exposed at a height of the second sidewall 22.
[0022] refer to Figure 3 After removing the gate mask layer 15 at the bottom of the first opening 17 and the bottom of the second opening 18, the process further includes: removing the remaining thickness of the first sidewall 14 to expose the second sidewall 22.
[0023] refer to Figure 4 After removing the remaining thickness of the first sidewall 14 to expose the second sidewall 22, in the barrier layer 16 (as Figure 3 Under the blocking effect shown, the first opening 17 is removed. Figure 3 (a) shows the bottom and the second opening 18 [as shown in] Figure 3 (b) The remaining thickness of the first sidewall 14 at the bottom forms a trench 23 between adjacent word line gate structures 12 and on the side of the peripheral gate structure 11.
[0024] Continue to refer to Figure 4 The step of removing the remaining thickness of the first sidewall 14 at the bottom of the first opening 17 and the bottom of the second opening 18 also includes removing the barrier layer 16.
[0025] refer to Figure 5 After removing the barrier layer 16, in the peripheral gate structure 11 [as shown] Figure 5 (b) shows the top and the top of the word line gate structure 12 [as shown in] Figure 5 A metal silicide layer 25 is formed on the top of (a) shown.
[0026] refer to Figure 6 After forming the metal silicide layer 25, in the word line gate structure 12 [as shown] Figure 6 (a) shown] and peripheral gate structure 11 [as shown in] Figure 6 (b) A first dielectric layer 26 is formed on the top of the trench 23, and an air gap 27 is formed between adjacent word line gate structures 12 and on the side of the peripheral gate structure 11.
[0027] It should be noted that the formation process of the first dielectric layer 26 includes plasma-enhanced chemical vapor deposition (PECVD), and the reaction gas in PECVD includes silane.
[0028] Reference Figure 7 , Figure 7 Is adopted Figures 1 to 6 The log-normal distribution of negative bias temperature instability in the semiconductor structure formed by the method is shown, where the horizontal axis represents failure time in years, the vertical axis represents the cumulative failure distribution function (CDF), the straight line L1 parallel to the vertical axis represents the standard value of negative bias temperature instability, and the solid line L2 represents the distribution of negative bias temperature instability in the aforementioned semiconductor structure. Figure 7 As can be seen, a portion of the solid line L2 is located on one side of the straight line L1, while the remaining portion of the solid line L2 is located on the other side of the straight line L1, indicating that the negative bias temperature stability of the aforementioned semiconductor structure is poor.
[0029] Research has revealed that because the first sidewall 14 on the sidewall of the peripheral gate structure 11 is removed, the peripheral gate structure 11 is susceptible to the influence of the formation process of the first dielectric layer 26 during its formation. For example, the reactive gas used to form the first dielectric layer 26 includes silane. Therefore, during the formation process of the first dielectric layer 26, the silicon-hydrogen bonds in the silane break, allowing hydrogen ions to easily enter the peripheral gate structure 11. This results in instability in the negative bias temperature of the semiconductor structure, thereby reducing the yield of the semiconductor structure.
[0030] To address the aforementioned technical problems, embodiments of the present invention provide a method for forming a semiconductor structure, comprising: providing a substrate, the substrate including a cell region and a peripheral region, a peripheral gate structure formed on the substrate of the peripheral region, a word line gate structure formed on the substrate of the cell region, and a first sidewall formed on the sidewall of the peripheral gate structure and between adjacent word line gate structures; forming a barrier layer on top of the first sidewall of the peripheral region, the barrier layer having a first opening located in the cell region, and the first opening being located above the first sidewall between adjacent word line gate structures; under the blocking effect of the barrier layer, removing the first sidewall at the bottom of the first opening, forming a trench between adjacent word line gate structures; after removing the first sidewall at the bottom of the first opening, forming a first dielectric layer on top of the word line gate structure, the first sidewall, and the peripheral gate structure, the first dielectric layer sealing the top of the trench, forming an air gap between adjacent word line gate structures.
[0031] In the solution disclosed in the embodiments of the present invention, since the sidewall of the peripheral gate structure has a first sidewall, the first sidewall can protect the peripheral gate structure during the process of forming the first dielectric layer, reduce the impact of the process on the peripheral gate structure, thereby improving the problem of negative bias temperature instability and improving the yield of semiconductor structure.
[0032] To make the above-mentioned objects, features and advantages of the embodiments of the present invention more apparent and understandable, the specific embodiments of the present invention will be described in detail below with reference to the accompanying drawings.
[0033] Figures 8 to 13 These are schematic diagrams of the structures corresponding to each step in an embodiment of the semiconductor structure formation method of the present invention, wherein (a) represents a schematic diagram of the unit region, and (b) represents a schematic diagram of the peripheral region. Figure 14 This is a log-normal distribution diagram of the negative bias temperature instability of a semiconductor structure formed using a method according to an embodiment of the present invention.
[0034] refer to Figure 8 A substrate 100 is provided, the substrate 100 including a cell region I [e.g. Figure 8 (a) shown) and outer area II [as shown in] Figure 8 As shown in (b), a peripheral gate structure 101 is formed on the substrate 100 of the peripheral region II, a word line gate structure 102 is formed on the substrate 100 of the unit region I, and a first sidewall 103 is formed on the sidewall of the peripheral gate structure 101 and between adjacent word line gate structures 102.
[0035] Substrate 100 is used to provide a process platform for subsequent flash memory fabrication processes. Specifically, substrate 100 is used to form NAND flash memory.
[0036] In this embodiment, the substrate 100 is made of silicon. In other embodiments, the substrate may be made of other materials such as germanium, silicon germanide, silicon carbide, gallium arsenide, or indium gallium bismuth. The substrate may also be a silicon-on-insulator substrate or a germanium-on-insulator substrate, or other types of substrates. The substrate material may be suitable for process requirements or easy to integrate.
[0037] The word line gate structure 102 is used as a cell structure for storing data in a memory.
[0038] In this embodiment, as Figure 8 As shown in (a), the word line gate structure 102 includes: a first tunneling oxide layer 120 located on the substrate 100 of the cell region I; a first floating gate layer 121 located on the first tunneling oxide layer 120; a first inter-gate dielectric layer 122 located on the first floating gate layer 121; and a first control gate layer 123 located on the first inter-gate dielectric layer 122.
[0039] The first tunneling oxide layer 120 serves as an insulating layer between the first floating gate layer 121 and the substrate 100, allowing electrons to enter the first floating gate layer 121 via the tunneling effect during NAND flash memory operation. In this embodiment, the material of the first tunneling oxide layer 120 is silicon oxide. The first floating gate layer 121 serves to store electrons during the formation of the NAND flash memory, thereby enabling the NAND flash memory to perform data storage functions. In this embodiment, the material of the first floating gate layer 121 is polysilicon. The first inter-gate dielectric layer 122 serves as an insulating layer between the first floating gate layer 121 and the first control gate layer 123. In this embodiment, the material of the first inter-gate dielectric layer 122 is one or both of silicon oxide and silicon nitride. The first control gate layer 123 serves as part of the word line gate structure 102 of the NAND memory. In this embodiment, the material of the first control gate layer 123 is polysilicon.
[0040] By applying voltage to the word line gate structure 102 through the peripheral gate structure 101, the word line gate structure 102 can complete the write or erase operation.
[0041] Therefore, in this embodiment, as Figure 8 As shown in (b), the peripheral gate structure 101 includes: a second tunneling oxide layer 130 located on the substrate 100 of the peripheral region II; a second floating gate layer 131 located on the second tunneling oxide layer 130; a second inter-gate dielectric layer 132 located on the second floating gate layer 131, and the second inter-gate dielectric layer 132 exposes a portion of the top of the second floating gate layer 131; and a second control gate layer 133 located on the second inter-gate dielectric layer 132 and in contact with the exposed second floating gate layer 131.
[0042] In this embodiment, as Figure 8 As shown in (a), in the step of providing substrate 100, a selection gate structure 107 is formed on substrate 100 at the edge position of cell region I, and the selection gate structure 107 is spaced apart from word line gate structure 102.
[0043] By selecting the gate structure 107, the problem of over-erasing of NAND flash memory devices can be effectively avoided during the erase operation, thereby preventing data misinterpretation.
[0044] Therefore, in this embodiment, the selected gate structure 107 includes: a third tunneling oxide layer 140 located on the substrate 100 at the edge of the cell region I; a third floating gate layer 141 located on the third tunneling oxide layer 140; a third inter-gate dielectric layer 142 located on the third floating gate layer 141, and the third inter-gate dielectric layer 142 exposes a portion of the top of the third floating gate layer 141; and a third control gate layer 143 located on the third inter-gate dielectric layer 142 and in contact with the exposed third floating gate layer 141.
[0045] It should be noted that, in order to reduce process steps, shorten manufacturing time, and save costs, the peripheral gate structure 101, word line gate structure 102, and select gate structure 107 are formed in the same process step.
[0046] Specifically, the first tunneling oxide layer 120, the second tunneling oxide layer 130, and the third tunneling oxide layer 140 are formed in the same process step and are made of the same material; the first floating gate layer 121, the second floating gate layer 131, and the third floating gate layer 141 are formed in the same process step and are made of the same material; the first inter-gate dielectric layer 122, the second inter-gate dielectric layer 132, and the third inter-gate dielectric layer 142 are formed in the same process step and are made of the same material; the first control gate layer 123, the second control gate layer 133, and the third floating gate layer 141 are formed in the same process step and are made of the same material.
[0047] In this embodiment, during the step of providing the substrate 100, a gate mask layer 104 is formed on the top of the peripheral gate structure 101 and the top of the word line gate structure 102.
[0048] The gate mask layer 104 is used as an etching mask for forming the peripheral gate structure 101 and the word line gate structure 102, and also protects the top of the peripheral gate structure 101 and the word line gate structure 102 in subsequent processes.
[0049] It should be noted that since the peripheral gate structure 101, word line gate structure 102 and select gate structure 107 are formed in the same process step, the gate mask layer 104 is also located on the select gate structure 107.
[0050] The first sidewall 103 is used to protect the sidewalls of the peripheral gate structure 101 and the word line gate structure 102, and also to define the location of the region where the source and drain doped layers are subsequently formed.
[0051] The material of the first sidewall 103 includes one or more of silicon nitride, silicon carbide, silicon carbonitride, silicon oxynitride, boron nitride, and boron carbonitride. In this embodiment, the material of the first sidewall 103 is silicon nitride. It should be noted that silicon nitride has good chemical inertness and high density; therefore, silicon nitride can play a good role in protecting the peripheral gate structure 101 in the subsequent formation of the first dielectric layer.
[0052] It should be noted that the first sidewall 103 is also formed on the sidewall of the selected gate structure 107.
[0053] In this embodiment, during the step of providing the substrate 100, a second sidewall 105 is formed between the peripheral gate structure 101 and the first sidewall 103, and between the word line gate structure 102 and the first sidewall 103.
[0054] The second sidewall 105 is used to protect the sidewalls of the peripheral gate structure 101 and the word line gate structure 102.
[0055] The material of the second sidewall 105 includes one or both of silicon oxide and silicon oxynitride.
[0056] Therefore, the material of the second sidewall 105 and the material of the first sidewall 103 have an etching selectivity ratio, which is beneficial to reduce the probability of damage to the second sidewall 105 in the subsequent process of removing the first sidewall 103. Thus, the second sidewall 105 can play the role of protecting the gate structure 107, the word line gate structure 102 and the peripheral gate structure 101.
[0057] In this embodiment, the material of the second sidewall 105 is silicon oxide. It should be noted that silicon oxide has relatively stable physical and chemical properties, and it is not easily removed in subsequent processes, thus providing effective protection.
[0058] It should be noted that the second sidewall 105 is also formed between the select gate structure 107 and the first sidewall 103.
[0059] In this embodiment, during the step of providing the substrate 100, a second dielectric layer 106 is formed on the substrate 100 on the side of the first sidewall 103, and the second dielectric layer 106 covers the sidewall of the first sidewall 103.
[0060] The second dielectric layer 106 is used to isolate the adjacent peripheral gate structure 101 and the adjacent select gate structure 107.
[0061] In this embodiment, the material of the second dielectric layer 106 includes silicon oxide. In other embodiments, the material of the second dielectric layer may also be a material containing silicon, such as silicon nitride.
[0062] refer to Figures 8 to 9 A barrier layer 108 is formed on top of the first sidewall 103 of the outer perimeter area II. Figure 9 As shown in (b), the barrier layer 108 has a first opening 109 located in the unit region I. Figure 9 As shown in (a), the first opening 109 is located above the first sidewall 103 between adjacent word line gate structures 102.
[0063] The barrier layer 108 is used to protect the first sidewall 103 of the outer perimeter area II, reducing the probability that the first sidewall 103 of the outer perimeter area II will be removed in subsequent process steps.
[0064] It should be noted that the first opening 109 is located above the first sidewall 103 between adjacent word line gate structures 102, which helps to reduce the difficulty of removing the first sidewall 103 between adjacent word line gate structures 102.
[0065] In this embodiment, during the step of forming a barrier layer 108 on top of the first sidewall 103 of the peripheral region II, the first opening 109 is also located on top of the word line gate structure 102, and the barrier layer 108 also has a second opening 110 located on top of the peripheral gate structure 101 [e.g.] Figure 9 (b) is shown.
[0066] It should be noted that the first opening 109 is located at the top of the word line gate structure 102, which facilitates the subsequent removal of the gate mask layer 104 at the top of the word line gate structure 102; the second opening 110 is located at the top of the peripheral gate structure 101, which facilitates the subsequent removal of the gate mask layer 104 at the top of the peripheral gate structure 101.
[0067] In this embodiment, in the step of forming a barrier layer 108 on top of the first sidewall 103 of the peripheral region II, the barrier layer 108 is also located on top of the first sidewall 103 on the sidewall between adjacent select gate structures 107. This helps to reduce the probability of the first sidewall 103 on the sidewall between adjacent select gate structures 107 being removed, thereby reducing the probability of bridging problems between the interconnect structure (not shown) on the source / drain doped layer on the side of the select gate structure 107 and the interconnect structure (not shown) on the select gate structure 107.
[0068] In this embodiment, during the step of forming the barrier layer 108 on top of the first sidewall 103 of the peripheral region II, the width of the second opening 110 should not be too large or too small. If the width of the second opening 110 is too large, it will increase the probability that the second opening 110 exposes the first sidewall 103 of the peripheral region II, thereby increasing the probability that the first sidewall 103 will be removed in subsequent processes. This will result in poor protection of the peripheral gate structure 101 during the subsequent formation of the first dielectric layer. If the width of the second opening 110 is too small, it will increase the difficulty of removing the gate mask layer 104 on top of the peripheral gate structure 101. Therefore, in this embodiment, during the step of forming the barrier layer 108 on top of the first sidewall 103 of the peripheral region II, the width of the second opening 110 is 1 micrometer to 1.3 micrometers.
[0069] like Figure 9 As shown, in this embodiment, in the step of forming a barrier layer 108 on the top of the first sidewall 103 of the peripheral area II, the barrier layer 108 includes a first barrier layer 111 and a second barrier layer 112 located on the first barrier layer 111.
[0070] Both the first barrier layer 111 and the second barrier layer 112 are used to protect the first sidewall 103 of the peripheral region II, and the first barrier layer 111 serves as a stop layer for the first sidewall 103 and the second barrier layer 112 of the subsequent removal unit region I. Therefore, there is an etching selectivity ratio between the first barrier layer 111 and the second barrier layer 112.
[0071] In this embodiment, the material of the first barrier layer 111 includes silicon oxide, and the material of the second barrier layer 112 includes silicon nitride.
[0072] It should be noted that there is an etching selectivity between silicon oxide and silicon nitride. Therefore, in the subsequent process of removing the first sidewall 103 and the second barrier layer 112 of the unit region I, silicon oxide can be used as a stop layer.
[0073] As an example, the first sidewall 103 is made of silicon nitride, the first barrier layer 111 is made of silicon oxide, and the second barrier layer 112 is made of silicon nitride. The first sidewall 103 and the second barrier layer 112 are made of the same material so that the first sidewall 103 and the second barrier layer 112 can be removed in the same step, simplifying the process. Furthermore, the first sidewall 103 and the second barrier layer 112 have an etching selectivity ratio with respect to the first barrier layer 111. Consequently, during the subsequent removal of the first sidewall 103 and the second barrier layer 112, the probability of the first barrier layer 111 being removed is reduced, thereby reducing the probability of the first sidewall 103 in the peripheral region II being removed.
[0074] Specifically, the step of forming a barrier layer 108 on top of the first sidewall 103 of the outer perimeter area II includes: (Refer to...) Figure 8 A barrier material layer 108a is formed on the top of the first sidewall 103, the top of the peripheral gate structure 101, and the top of the word line gate structure 102; Continuing to refer to Figure 8 A pattern definition layer 113 is formed on top of the barrier material layer 108a, and the pattern definition layer 113 has a third opening 114 [e.g.] Figure 8 (a) shown] and the fourth opening 115 [as shown] Figure 8 (b) shows that the third opening 114 exposes the barrier material layer 108a on top of the word line gate structure 102 and the barrier material layer 108a on top of the first sidewall 103 between adjacent word line gate structures 102, and the fourth opening 115 exposes the barrier material layer 108a on top of the peripheral gate structure 101; Reference Figure 9 (a) and Figure 9 (b) Define layer 113 graphically (e.g.) Figure 8 (As shown) is a mask. The barrier material layer 108a exposed by the third opening 114 and the fourth opening 115 is removed, and the remaining barrier material layer 108a serves as the barrier layer 108.
[0075] The barrier material layer 108a is used to form the barrier layer 108. Accordingly, in this embodiment, the barrier material layer 108a includes a first barrier material layer (not shown) and a second barrier material layer (not shown) located on the first barrier material layer. The first barrier material layer is used to form the first barrier layer 111, and the second barrier material layer is used to form the second barrier layer 112.
[0076] The graphic definition layer 113 is used as a mask to form the blocking layer 108.
[0077] The graphic definition layer 113 has a third opening 114 and a fourth opening 115, which facilitate the removal of the exposed barrier material layer 108a along the third opening 114 and the fourth opening 115.
[0078] In this embodiment, the material of the pattern definition layer 113 includes photoresist. Photoresist has high resolution, allowing for precise control of the opening sizes of the third opening 114 and the fourth opening 115; simultaneously, photoresist is easy to remove, thereby reducing process complexity and improving production efficiency. In other embodiments, the mask layer may also be made of other materials that can serve as etching masks and are easily removable.
[0079] In this embodiment, in the step of forming a pattern definition layer 113 on top of the barrier material layer 108a, the thickness of the pattern definition layer 113 should not be too large or too small. If the thickness of the pattern definition layer 113 is too large, the resolution of the pattern will easily decrease, thereby increasing the difficulty of forming the third opening 114 and the fourth opening 115; if the thickness of the pattern definition layer 113 is too small, the effect of the pattern definition layer 113 as a mask for forming the barrier layer 108 will be poor. Therefore, in this embodiment, in the step of forming a pattern definition layer 113 on top of the barrier material layer 108a, the thickness of the pattern definition layer 113 is 3400 angstroms to 3700 angstroms.
[0080] In this embodiment, the process of removing the barrier material layer 108a exposed by the third opening 114 and the fourth opening 115 includes a wet etching process.
[0081] It should be noted that the wet etching process has the characteristics of a high etching rate, thereby reducing the process time for removing the barrier material layer 108a exposed by the third opening 114 and the fourth opening 115, and thus increasing the throughput. Moreover, the wet etching process has the characteristics of high etching selectivity, which completely removes the barrier material layer 108a exposed by the third opening 114 and the fourth opening 115. At the same time, it also reduces the probability of damage to the pattern definition layer 113, thereby reducing the probability of damage to the barrier material layer 108a covered by the pattern definition layer 113.
[0082] refer to Figure 9 After forming the barrier layer 108 on top of the first sidewall 103 in the outer perimeter area II, and before removing the first sidewall 103 at the bottom of the first opening 109, the forming method further includes: removing the first opening 109 [e.g., ...]. Figure 9 (a) shows the bottom and the second opening 110 [as shown in] Figure 9 (b) shows the bottom gate mask layer 104.
[0083] It should be noted that removing the gate mask layer 104 at the bottom of the first opening 109 and the bottom of the second opening 110 exposes the top of the word line gate structure 102, the select gate structure 107 and the peripheral gate structure 101, which facilitates the subsequent formation of a metal silicide layer on the top of the word line gate structure 102, the select gate structure 107 and the peripheral gate structure 101.
[0084] Furthermore, removing the gate mask layer 104 at the bottom of the first opening 109 and the bottom of the second opening 110 before removing the first sidewall 103 at the bottom of the first opening 109 is beneficial because the first sidewall 103 can protect the sidewalls of the word line gate structure 102, the select gate structure 107, and the peripheral gate structure 101 during the process of removing the gate mask layer 104.
[0085] refer to Figures 9 to 11 Under the blocking effect of the blocking layer 108, the first sidewall 103 at the bottom of the first opening 109 is removed, forming a trench 116 between adjacent word line gate structures 102 (e.g., Figure 11 (As shown).
[0086] Groove 116 is used to provide space for the subsequent formation of air gaps.
[0087] In this embodiment, the step of removing the first sidewall 103 at the bottom of the first opening 109 includes: referring to Figure 9 Remove a portion of the thickness of the first sidewall 103 at the bottom of the first opening 109, exposing a portion of the height of the second sidewall 105; Reference Figure 11 Remove the remaining thickness of the first sidewall 103.
[0088] It should be noted that removing part of the thickness of the first sidewall 103 at the bottom of the first opening 109 and exposing part of the height of the second sidewall 105 helps to reduce the difficulty of removing the exposed second sidewall 105 in the subsequent process; at the same time, in the process of removing the exposed second sidewall 105, the remaining thickness of the first sidewall 103 can protect the remaining second sidewall 105 from being removed.
[0089] It should also be noted that the first sidewall 103, which removes the remaining thickness, is used to form a trench 116 between the word line gate structures 102.
[0090] In this embodiment, the process of removing a portion of the thickness of the first sidewall 103 at the bottom of the first opening 109 includes a wet etching process. By controlling parameters such as etching time and solution concentration, the thickness of the first sidewall 103 removed can be precisely controlled, thereby precisely controlling the height of the exposed second sidewall 105 to meet the actual process design requirements.
[0091] In this embodiment, the process for removing the remaining thickness of the first sidewall 103 includes a wet etching process. The wet etching process has a high etching selectivity, therefore, it can completely remove the remaining thickness of the first sidewall 103, while also reducing the probability of damage to the second sidewall 105.
[0092] refer to Figure 10 (a) and Figure 10 (b) After the second sidewall 105 with a portion of its height is exposed, and before the first sidewall 103 with the remaining thickness is removed, the method further includes: removing the second sidewall 105 exposed by the first sidewall 103 with the remaining thickness.
[0093] It should be noted that removing the remaining thickness of the first sidewall 103 exposes the second sidewall 105, that is, the sidewalls of the word line gate structure 102, the select gate structure 107 and the peripheral gate structure 101 are exposed. In the process of forming metal silicide, it is convenient for the metal reaction source to contact the top and sidewalls of the word line gate structure 102, the select gate structure 107 and the peripheral gate structure 101 to form a metal silicide of a certain thickness.
[0094] In this embodiment, the process for removing the exposed second sidewall 105 from the remaining thickness of the first sidewall 103 includes a wet etching process. The wet etching process has a high etching selectivity, therefore, it can completely remove the exposed second sidewall 105 from the remaining thickness of the first sidewall 103. Simultaneously, it reduces the probability of damaging the remaining thickness of the first sidewall 103, thereby lowering the probability of the remaining second sidewall 105 being removed.
[0095] refer to Figure 11 (a) and Figure 11 (b) After removing the gate mask layer 105 at the bottom of the first opening 109 and the bottom of the second opening 110, and before forming the first dielectric layer, the formation method further includes: removing the barrier layer 108.
[0096] It should be noted that since the steps of removing the barrier layer 108 and removing the first sidewall 103 at the bottom of the first opening 109 both occur after removing the gate mask layer 105 and before forming the first dielectric layer, the barrier layer 108 is likely to remain in the process of removing the first sidewall 103 at the bottom of the first opening 109. This helps the barrier layer 108 to protect the first sidewall 103 of the peripheral region II and reduces the probability that the first sidewall 103 of the peripheral region II will be removed.
[0097] In this embodiment, the steps of removing the first sidewall 103 at the bottom of the first opening 109 and removing the blocking layer 108 include: using the first blocking layer 111 as a stop layer, removing the first sidewall 103 and the second blocking layer 112 in the same step; after removing the first sidewall 111 and the second blocking layer 103, removing the first blocking layer 111.
[0098] It should be noted that there is an etching selectivity between the first barrier layer 111 and the second barrier layer 112, and between the first barrier layer 111 and the first sidewall 103. Compared with the scheme of using the first barrier layer 111 as the barrier layer 108, the embodiment of the present invention reduces the process time for removing the first sidewall 103 and the barrier layer 108, thereby improving production efficiency.
[0099] In this embodiment, the process of removing the first sidewall 103 and the second barrier layer 112 in the same step, using the first barrier layer 111 as the stop layer, includes a wet etching process. The wet etching process has a high etching selectivity, thus it can completely remove the first sidewall 103 and the second barrier layer 112, while also reducing the probability of damage to the first barrier layer 111, thereby reducing the probability of the first sidewall 103 in the peripheral region II being removed.
[0100] In this embodiment, after removing the first sidewall 111 and the second barrier layer 103, the process for removing the first barrier layer 111 includes a wet etching process. Specifically, the wet etching process can efficiently remove the first barrier layer 111 by changing the etching solution, without the need for additional dry etching or complex masking processes, thereby simplifying the process flow and improving production efficiency.
[0101] In this embodiment, during the step of removing the first sidewall 103 and the second barrier layer 112 in the same step, the etching selectivity ratio of the first sidewall 103 and the first barrier layer 111 should not be too small. If the etching selectivity ratio of the first sidewall 103 and the first barrier layer 111 is too small, the first barrier layer 111 is also easily removed during the removal of the first sidewall 103 and the second barrier layer 112, thereby increasing the probability that the first sidewall 103 of the peripheral region II will be removed. Therefore, in this embodiment, during the step of removing the first sidewall 103 and the second barrier layer 111 in the same step, the etching selectivity ratio of the first sidewall 103 and the first barrier layer 112 is greater than 7:1.
[0102] In this embodiment, removing the first sidewall 103 and the second barrier layer 112 in the same step includes: removing the remaining thickness of the first sidewall 103.
[0103] It should be noted that the removal of the first sidewall 103 is divided into two stages: First, in the process of removing the gate mask layer 104, a portion of the thickness of the first sidewall 103 at the bottom of the first opening 109 is removed; then, in the process of removing the second barrier layer 112, the remaining thickness of the first sidewall 103 is removed.
[0104] refer to Figure 12 (a) and Figure 12 (b) After removing the barrier layer 108, a metal silicide layer 117 is formed on top of the peripheral gate structure 101 and the word line gate structure 102.
[0105] By using the metal silicide layer 117, the gate resistance of the NAND flash memory is reduced, thereby improving the programming capability and efficiency of the NAND flash memory, enhancing the repetitive read / write capability of the NAND flash memory device, and improving RC (Resistance Capacitance) latency, thus improving the performance of the NAND flash memory.
[0106] It should be noted that the metal silicide layer 117 is also formed on top of the selected gate structure 107.
[0107] refer to Figure 13 (a) and Figure 13 (b) After removing the first sidewall 103 at the bottom of the first opening 109, a first dielectric layer 118 is formed on top of the word line gate structure 102, the first sidewall 103, and the peripheral gate structure 101. The first dielectric layer 118 seals the top of the trench 116, forming an air gap 119 between adjacent word line gate structures 102. Figure 13 (a) is shown.
[0108] The first dielectric layer 118 is used to seal the top of the trench 116, thereby forming an air gap 119 with the word line gate structure 102 and the substrate 100.
[0109] It should be noted that, compared with the scheme where the adjacent word line gate structures 102 are separated by a first sidewall 103, the dielectric constant of air is smaller. Therefore, the setting of the air gap 119 can reduce the capacitance between adjacent word line gate structures 102, thereby improving the crosstalk problem of NAND flash memory during programming and the repeated read / write capability of NAND flash memory.
[0110] It should also be noted that, due to the presence of a first sidewall 103 on the sidewall of the peripheral gate structure II [e.g.] Figure 13 As shown in (b), therefore, in the process of forming the first dielectric layer 118, the first sidewall 103 can protect the peripheral gate structure 101, reduce the impact of the process on the peripheral gate structure 101, thereby improving the problem of negative bias temperature instability and improving the yield of semiconductor structure.
[0111] Reference Figure 14 , Figure 14 This is a log-normal distribution diagram of the negative bias temperature instability of a semiconductor structure formed using the formation method of an embodiment of the present invention. The horizontal axis represents the failure time in years, the vertical axis represents the cumulative failure distribution function, the straight line l1 parallel to the vertical axis represents the standard value of the negative bias temperature instability, and the solid line l2 represents the distribution of the negative bias temperature instability of the aforementioned semiconductor structure. Figure 14 As can be seen, solid line 12 is located on the same side of straight line 11, which means that the semiconductor structure formed by the method of the present invention has good negative bias temperature stability.
[0112] In this embodiment, the material of the first dielectric layer 108 includes silicon oxide. It should be noted that silicon oxide has the characteristic of fast lateral growth rate. Therefore, during the formation of the first dielectric layer 118 on the top of the word line gate structure 102, the first sidewall 103 and the peripheral gate structure 101, the silicon oxide can be quickly clamped and sealed to form an air gap 119.
[0113] In other embodiments, the material of the first dielectric layer may also be a material containing silicon, such as silicon nitride.
[0114] In this embodiment, the formation process of the first dielectric layer 118 includes plasma enhanced chemical vapor deposition (PECVD), and the reaction gas of the plasma enhanced chemical vapor deposition process includes silane (SiH4).
[0115] Plasma-enhanced chemical vapor deposition has poor hole-filling performance, especially when the opening size of trench 116 is small. The first dielectric layer 118 can only fill a portion of the depth near the top of trench 116. This allows the first dielectric layer 118 to seal the top of trench 116 while avoiding occupying too much space in trench 116. As a result, the air gap 119 can effectively reduce the capacitance between adjacent word line gate structures 102.
[0116] It should be noted that silanes have high process compatibility, are low-cost in semiconductor manufacturing processes, and have a relatively small impact on the overall process flow.
[0117] Accordingly, embodiments of the present invention also provide a semiconductor structure. Figure 15 This is a schematic diagram of a semiconductor structure according to an embodiment of the present invention, wherein (a) shows a schematic diagram of the cell region and (b) shows a schematic diagram of the peripheral region.
[0118] The semiconductor structure includes: a substrate 500, which includes a peripheral region II' and a cell region I'; and a peripheral gate structure 501 [e.g., ...]. Figure 15 (b) As shown, on the substrate 500 located in the peripheral region II'; word line gate structure 502 [as shown] Figure 15 As shown in (a), on the substrate 500 located in cell region I', and adjacent word line gate structures 502 and substrate 500 form a trench (not shown); a first sidewall 504 is located on the sidewall of the peripheral gate structure 501; a first dielectric layer 505 is located on top of the word line gate structure 502, the first sidewall 504 and the peripheral gate structure 501, the first dielectric layer 505 seals the top of the trench, and the first dielectric layer 505, adjacent word line gate structures 502 and substrate 500 form an air gap 506.
[0119] Substrate 500 serves as a process platform for subsequent flash memory fabrication processes. Specifically, substrate 500 is used to form NAND flash memory.
[0120] In this embodiment, the relevant description of the substrate 500 can be referred to the corresponding description of the foregoing embodiment, and will not be repeated here.
[0121] The word line gate structure 502 is used as a cell structure for storing data in a memory.
[0122] In this embodiment, as Figure 15 As shown in (a), the word line gate structure 502 includes: a first tunneling oxide layer 520 located on the substrate 500 of the cell region I'; a first floating gate layer 521 located on the first tunneling oxide layer 520; a first inter-gate dielectric layer 522 located on the first floating gate layer 521; and a first control gate layer 523 located on the first inter-gate dielectric layer 522.
[0123] The first tunneling oxide layer 520 serves as an insulating layer between the first floating gate layer 521 and the substrate 500, allowing electrons to enter the first floating gate layer 521 via the tunneling effect during NAND flash memory operation. In this embodiment, the material of the first tunneling oxide layer 520 is silicon oxide. The first floating gate layer 521 serves to store electrons during the formation of the NAND flash memory, thereby enabling the NAND flash memory to perform data storage functions. In this embodiment, the material of the first floating gate layer 521 is polysilicon. The first inter-gate dielectric layer 522 serves as an insulating layer between the first floating gate layer 521 and the first control gate layer 523. In this embodiment, the material of the first inter-gate dielectric layer 522 is one or both of silicon oxide and silicon nitride. The first control gate layer 523 serves as part of the word line gate structure 502 of the NAND memory. In this embodiment, the material of the first control gate layer 523 is polysilicon.
[0124] By applying voltage to the word line gate structure 502 through the peripheral gate structure 501, the word line gate structure 502 can complete the write or erase operation.
[0125] Therefore, in this embodiment, as Figure 15 As shown in (a), the peripheral gate structure 501 includes: a second tunneling oxide layer 530 located on the substrate 500 of the peripheral region II'; a second floating gate layer 531 located on the second tunneling oxide layer 530; a second inter-gate dielectric layer 532 located on the second floating gate layer 531, and the second inter-gate dielectric layer 532 exposes a portion of the top of the second floating gate layer 531; and a second control gate layer 533 located on the second inter-gate dielectric layer 532 and in contact with the exposed second floating gate layer 531.
[0126] In this embodiment, the semiconductor structure further includes a selected gate structure 507, located on the substrate 500 at the edge of the cell region II'.
[0127] By selecting gate structure 507, over-erasing of NAND flash memory devices can be effectively avoided during the erase operation, thereby preventing data misinterpretation.
[0128] Therefore, in this embodiment, as Figure 15 As shown in (a), the selected gate structure 507 includes: a third tunneling oxide layer 540 located on the substrate 500 at the edge of the cell region I'; a third floating gate layer 541 located on the third tunneling oxide layer 540; a third inter-gate dielectric layer 542 located on the third floating gate layer 541, and the third inter-gate dielectric layer 542 exposes a portion of the top of the third floating gate layer 541; and a third control gate layer 543 located on the third inter-gate dielectric layer 542 and in contact with the exposed third floating gate layer 541.
[0129] Specifically, the materials of the first tunneling oxide layer 520, the second tunneling oxide layer 530, and the third tunneling oxide layer 540 are the same; the materials of the first floating gate layer 521, the second floating gate layer 531, and the third floating gate layer 541 are the same; the materials of the first inter-gate dielectric layer 522, the second inter-gate dielectric layer 532, and the third inter-gate dielectric layer 542 are the same; and the materials of the first control gate layer 523, the second control gate layer 533, and the third floating gate layer 541 are the same.
[0130] The groove is used to provide space for the formation of the air gap 506.
[0131] The first sidewall 504 is used to protect the sidewall of the peripheral gate structure 501 and also to define the location of the region where the source and drain doped layers are subsequently formed.
[0132] The material of the first sidewall 504 includes one or more of silicon nitride, silicon carbide, silicon carbonitride, silicon oxynitride, boron nitride, and boron carbonitride. In this embodiment, the material of the first sidewall 504 is silicon nitride. It should be noted that silicon nitride has good chemical inertness and high density; therefore, silicon nitride can play a good role in protecting the peripheral gate structure 501 in the formation of the first dielectric layer 505.
[0133] It should be noted that the first sidewall 504 is also formed on the sidewall of the selected gate structure 507.
[0134] It should also be noted that since the peripheral gate structure 501 has a first sidewall 504 on its sidewall, the first sidewall 504 can protect the peripheral gate structure 501 during the process of forming the first dielectric layer 505, reduce the impact of the process on the peripheral gate structure 501, thereby improving the problem of negative bias temperature instability and increasing the yield of semiconductor structure.
[0135] In this embodiment, the semiconductor structure further includes a second sidewall 508, located between the peripheral gate structure 501 and the first sidewall 504, and on the sidewall of the word line gate structure 502.
[0136] The second sidewall 508 is used to protect the sidewalls of the peripheral gate structure 501 and the word line gate structure 502.
[0137] The material of the second sidewall 508 includes one or both of silicon oxide and silicon oxynitride.
[0138] Therefore, the material of the second sidewall 508 and the material of the first sidewall 504 have an etching selectivity ratio, which helps to reduce the probability of damage to the second sidewall 508 during the process of removing the first sidewall 504. Thus, the second sidewall 508 can protect the gate structure 507, the word line gate structure 502 and the peripheral gate structure 501.
[0139] In this embodiment, the material of the second sidewall 508 is silicon oxide. It should be noted that silicon oxide has relatively stable physical and chemical properties, and it is not easily removed in subsequent process steps, thus providing effective protection.
[0140] In this embodiment, the second sidewall 505 is also formed between the selected gate structure 507 and the first sidewall 504, which helps to reduce the probability of bridging problems between the interconnect structure (not shown) on the source / drain doped layer located on the side of the selected gate structure 507 and the interconnect structure (not shown) on the selected gate structure 507.
[0141] In this embodiment, the semiconductor structure further includes a second dielectric layer 509 located on the substrate 500 on the side of the first sidewall 507, and the second dielectric layer 509 covers the sidewall of the first sidewall 507.
[0142] The second dielectric layer 509 is used to isolate the adjacent peripheral gate structure 501 and the adjacent select gate structure 507.
[0143] In this embodiment, the material of the second dielectric layer 509 includes silicon oxide. In other embodiments, the material of the second dielectric layer may also be a material containing silicon, such as silicon nitride.
[0144] In this embodiment, the semiconductor structure further includes a metal silicide layer 510, located on top of the peripheral gate structure 501 and the word line gate structure 502.
[0145] By using the metal silicide layer 510, the gate resistance of the NAND flash memory is reduced, thereby improving the programming capability and efficiency of the NAND flash memory, enhancing the repetitive read / write capability of the NAND flash memory device, and improving RC latency, thus improving the performance of the NAND flash memory.
[0146] It should be noted that the metal silicide layer 510 is also located on top of the gate selection structure 507.
[0147] The first dielectric layer 505 is used to seal the top of the trench, thereby forming an air gap 506 with the word line gate structure 502 and the substrate 500.
[0148] It should be noted that, compared with the scheme where the adjacent word line gate structures 502 are separated by a first sidewall 504, the dielectric constant of air is smaller. Therefore, the setting of air gap 506 can reduce the capacitance between adjacent word line gate structures 502, thereby improving the crosstalk problem of NAND flash memory during programming and the repeated read / write capability of NAND flash memory.
[0149] The material of the first dielectric layer 505 includes silicon oxide. It should be noted that silicon oxide has the characteristic of fast lateral growth rate. Therefore, during the process of forming the first dielectric layer 505 on the top of the word line gate structure 502, the first sidewall 504 and the peripheral gate structure 501, the silicon oxide can be quickly clamped and sealed to form an air gap 506.
[0150] In other embodiments, the material of the first dielectric layer may also be a material containing silicon, such as silicon nitride.
[0151] It should be noted that the semiconductor structure of this embodiment can be formed by the formation method of the foregoing embodiment, or by other formation methods. For the description of the semiconductor structure of the embodiment of the present invention, please refer to the relevant content in the foregoing formation method.
[0152] While the present invention has been disclosed above, it is not limited thereto. Any person skilled in the art can make various modifications and alterations without departing from the spirit and scope of the invention; therefore, the scope of protection of the present invention should be determined by the scope defined in the claims.
Claims
1. A method for forming a semiconductor structure, characterized in that, include: A substrate is provided, the substrate including a cell region and a peripheral region, a peripheral gate structure is formed on the substrate of the peripheral region, a word line gate structure is formed on the substrate of the cell region, and a first sidewall is formed on the sidewall of the peripheral gate structure and between adjacent word line gate structures; A barrier layer is formed on top of the first sidewall of the peripheral area, the barrier layer having a first opening located in the cell area, and the first opening being located above the first sidewall between adjacent word line gate structures; Under the blocking effect of the blocking layer, the first sidewall at the bottom of the first opening is removed, forming a trench between adjacent word line gate structures; After removing the first sidewall at the bottom of the first opening, a first dielectric layer is formed on top of the word line gate structure, the first sidewall, and the peripheral gate structure. The first dielectric layer seals the top of the trench, forming an air gap between adjacent word line gate structures.
2. The method for forming a semiconductor structure as described in claim 1, characterized in that, In the step of providing the substrate, a gate mask layer is formed on top of the peripheral gate structure and the word line gate structure; In the step of forming the barrier layer on top of the first sidewall of the peripheral region, the first opening is also located on top of the word line gate structure, and the barrier layer also has a second opening located on top of the peripheral gate structure; After forming the barrier layer on top of the first sidewall of the peripheral area and before removing the first sidewall at the bottom of the first opening, the forming method further includes: removing the gate mask layer at the bottom of the first opening and the bottom of the second opening; After removing the gate mask layers at the bottom of the first opening and the bottom of the second opening, and before forming the first dielectric layer, the formation method further includes: removing the barrier layer; and after removing the barrier layer, forming a metal silicide layer on top of the peripheral gate structure and the word line gate structure.
3. The method for forming a semiconductor structure as described in claim 2, characterized in that, In the step of forming a barrier layer on top of the first sidewall of the peripheral area, the width of the second opening is 1 micrometer to 1.3 micrometers.
4. The method for forming a semiconductor structure as described in claim 2, characterized in that, In the step of forming a barrier layer on top of the first sidewall of the peripheral area, the barrier layer includes a first barrier layer and a second barrier layer located on the first barrier layer; The steps of removing the first sidewall at the bottom of the first opening and removing the barrier layer include: using the first barrier layer as a stop layer, removing the first sidewall and the second barrier layer in the same step; After removing the first sidewall and the second barrier layer, remove the first barrier layer.
5. The method for forming a semiconductor structure as described in claim 4, characterized in that, In the step of removing the first sidewall and the second barrier layer in the same step, the etching selectivity ratio of the first sidewall and the first barrier layer is greater than 7:
1.
6. The method for forming a semiconductor structure as described in claim 4, characterized in that, The material of the first sidewall includes silicon nitride, the material of the first barrier layer includes silicon oxide, and the material of the second barrier layer includes silicon nitride.
7. The method for forming a semiconductor structure as described in claim 2, characterized in that, The step of forming a barrier layer on top of the first sidewall of the peripheral region includes: forming a barrier material layer on top of the first sidewall, on top of the peripheral gate structure, and on top of the word line gate structure; A pattern definition layer is formed on top of the barrier material layer. The pattern definition layer has a third opening and a fourth opening. The third opening exposes the barrier material layer on top of the word line gate structure and the barrier material layer on top of the first sidewall between adjacent word line gate structures. The fourth opening exposes the barrier material layer on top of the peripheral gate structure. Using the graphic definition layer as a mask, the barrier material layer exposed by the third and fourth openings is removed, and the remaining barrier material layer serves as the barrier layer.
8. The method for forming a semiconductor structure as described in claim 7, characterized in that, In the step of forming the pattern definition layer on top of the barrier material layer, the thickness of the pattern definition layer is 3400 angstroms to 3700 angstroms.
9. The method for forming a semiconductor structure as described in claim 7, characterized in that, The process for removing the barrier material layer exposed by the third and fourth openings includes a wet etching process.
10. The method for forming a semiconductor structure as described in claim 4, characterized in that, In the step of providing the substrate, a second sidewall is formed between the peripheral gate structure and the first sidewall, and between the word line gate structure and the first sidewall; The step of removing the first sidewall at the bottom of the first opening includes: removing a portion of the thickness of the first sidewall at the bottom of the first opening to expose a portion of the height of the second sidewall; and removing the remaining thickness of the first sidewall. After exposing a portion of the height of the second sidewall, and before removing the remaining thickness of the first sidewall, the process further includes: removing the remaining thickness of the first sidewall to expose the second sidewall; Removing the first sidewall and the second barrier layer in the same step includes: removing the remaining thickness of the first sidewall.
11. The method for forming a semiconductor structure as described in claim 10, characterized in that, The material of the second sidewall includes silicon dioxide.
12. The method for forming a semiconductor structure as described in claim 1, characterized in that, In the step of providing the substrate, a second dielectric layer is formed on the substrate on the side of the first sidewall, and the second dielectric layer covers the sidewall of the first sidewall.
13. The method for forming a semiconductor structure as described in claim 1, characterized in that, The material of the first dielectric layer includes silicon oxide.
14. The method for forming a semiconductor structure as described in claim 1 or 13, characterized in that, The formation process of the first dielectric layer includes a plasma-enhanced chemical vapor deposition process, wherein the reaction gas of the plasma-enhanced chemical vapor deposition process includes silane.
15. A semiconductor structure, characterized in that, include: Substrate, the substrate including a peripheral region and a cell region; A peripheral gate structure is located on the substrate of the peripheral region; A word line gate structure is located on the substrate of the cell region, and adjacent word line gate structures and the substrate form a trench; The first sidewall is located on the sidewall of the peripheral gate structure; A first dielectric layer is located on top of the word line gate structure, the first sidewall, and the peripheral gate structure. The first dielectric layer seals the top of the trench, and the first dielectric layer, the adjacent word line gate structure, and the substrate form an air gap.
16. The semiconductor structure as described in claim 15, characterized in that, The semiconductor structure further includes: a metal silicide layer located on top of the peripheral gate structure and on top of the word line gate structure; The second sidewall is located between the peripheral gate structure and the first sidewall, and on the sidewall of the word line gate structure.
17. The semiconductor structure as claimed in claim 16, characterized in that, The material of the first sidewall includes silicon nitride; the material of the second sidewall includes silicon oxide.
18. The semiconductor structure as claimed in claim 15, characterized in that, The word line gate structure includes: a first tunneling oxide layer located on the substrate of the cell region; a first floating gate layer located on the first tunneling oxide layer; a first inter-gate dielectric layer located on the first floating gate layer; and a first control gate layer located on the first inter-gate dielectric layer. The peripheral gate structure includes: a second tunneling oxide layer located on the substrate of the peripheral region; a second floating gate layer located on the second tunneling oxide layer; a second inter-gate dielectric layer located on the second floating gate layer, wherein the second inter-gate dielectric layer exposes a portion of the top of the second floating gate layer; and a second control gate layer located on the second inter-gate dielectric layer and in contact with the exposed second floating gate layer.
19. The semiconductor structure as described in claim 15, characterized in that, The material of the first dielectric layer includes silicon oxide.
20. The semiconductor structure as claimed in claim 15, characterized in that, The semiconductor structure further includes a second dielectric layer located on the substrate at the side of the first sidewall, the second dielectric layer covering the sidewall of the first sidewall.