Semiconductor structure fabrication methods, semiconductor structures

By forming primary and secondary trenches in the semiconductor structure and filling them with thermal oxide and conductive layers, the process incompatibility between the semi-floating gate memory array region and the standard logic device region is solved, achieving control gate height matching and precise definition of the floating gate layer, thereby improving chip yield and device performance.

CN123124361APending Publication Date: 2026-11-17ANHUI UNIV +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611629710.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-21
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

During the fabrication process, the incompatibility between the semi-floating gate memory array region and the standard logic device region due to the difference in control gate height seriously affects chip yield and device performance.

Method used

By forming primary and secondary trenches on the substrate, combined with the filling of thermal oxide layer and conductive layer, the height matching of control gate of memory area and logic area is ensured, and the position of control gate sidewall is defined by the groove in secondary trench, so as to achieve precise definition of floating gate layer and simplify photolithography process.

Benefits of technology

This achieves process compatibility between the semi-floating gate memory array region and the standard logic device region, simplifies the fabrication process, and improves chip yield and device performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124361A_ABST
    Figure CN123124361A_ABST
Patent Text Reader

Abstract

This application relates to a semiconductor structure fabrication method and a semiconductor structure. The method includes: providing a substrate; the substrate including arranged logic regions and memory regions; forming a first trench in the logic regions and a second trench in the memory regions; the second trench including a secondary trench and a primary trench with its top surface in the bottom surface of the secondary trench; forming a thermal oxide layer and a groove located in the secondary trench, exposing a portion of the substrate surface; forming an oxide layer filling the first trench and a first conductive layer filling the second trench; forming a first control gate on the top surface of the logic regions away from the oxide layer, and forming a second control gate on the top surface of the first conductive layer directly above the primary trench; and removing a portion of the first conductive layer based on the second control gate, such that the remaining first conductive layer located directly below the second control gate constitutes a floating gate layer. This method can at least solve the process incompatibility problem caused by the difference in control gate height between the semi-floating gate memory array region and the standard logic device region during fabrication.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of integrated circuit technology, and in particular to a method for preparing a semiconductor structure and the semiconductor structure itself. Background Technology

[0002] As semiconductor device miniaturization continues to advance, embedded memory and logic integrated chips are widely used in various high-end integrated circuit scenarios due to their advantages of high integration, low power consumption, and high adaptability. Semi-floating gate memory devices, as a new type of non-volatile memory device, are compatible with advanced logic process nodes, require no additional capacitor structures, and possess strong miniaturization and fast read / write speeds, making them one of the core development directions of embedded memory integration technology.

[0003] In the chip integration process, the semi-floating gate memory array area and the standard logic device area need to be fabricated simultaneously on the same wafer to achieve the integration of storage function and logic operation function. However, the related integration fabrication process has many unavoidable technical defects, which seriously restrict the chip yield and device performance. Summary of the Invention

[0004] Based on this, it is necessary to provide a method for fabricating a semiconductor structure and a semiconductor structure to address the technical problems in the existing technology, so as to solve the process incompatibility problem caused by the difference in control gate height between the semi-floating gate memory array region and the standard logic device region during the fabrication process.

[0005] In a first aspect, this application provides a method for fabricating a semiconductor structure, comprising: providing a substrate; the substrate including a logic region and a storage region arranged along a first direction parallel to a first surface of the substrate;

[0006] A first trench is formed in the logic region, and a second trench is formed in the storage region; the second trench includes a secondary trench extending into the substrate via a first surface, and a primary trench whose top surface is within the bottom surface of the secondary trench and is fabricated concurrently with the first trench.

[0007] A thermo-oxidative layer is formed covering the inner surfaces of the first trench and the second trench, and a groove is located in the secondary trench, exposing a portion of the substrate surface;

[0008] An oxide layer is formed that fills the first trench, and a first conductive layer is formed that fills the second trench;

[0009] A first control gate is formed on the top surface of the logic region away from the oxide layer, and a second control gate is formed on the top surface of the first conductive layer directly above the primary trench; the orthographic projection of the sidewall of the second control gate in the secondary trench is located inside the bottom surface of the groove.

[0010] Based on the second control gate, a portion of the first conductive layer is removed, so that the remaining first conductive layer located directly below the second control gate constitutes a floating gate layer.

[0011] In some embodiments, a mask structure is provided on the first surface; the mask structure includes a nitride mask layer and an oxide mask layer arranged sequentially along a second direction toward the substrate.

[0012] In some embodiments, forming a second trench includes:

[0013] Based on the same photomask, a first trench and a primary trench are formed extending from the first surface into the substrate;

[0014] The first sacrificial layer is formed in the first trench and the first-level trench;

[0015] The patterned photoresist layer exposes part of the mask structure of the storage area and the top surface of the first sacrificial layer;

[0016] The mask structure and the substrate of the storage area are etched sequentially to form a secondary trench;

[0017] Remove the first sacrificial layer and photoresist layer; the secondary trench and the primary trench constitute the second trench.

[0018] In some embodiments, forming a thermal oxidation layer and a groove includes:

[0019] After forming a thermal oxidation layer using a thermal oxidation process, a second sacrificial layer is formed that covers the logic area and the storage area;

[0020] A third trench is formed that penetrates the second sacrificial layer and the thermo-oxidative layer along the second direction;

[0021] The second sacrificial layer located in the second trench is removed, and the remaining third trench located between the adjacent thermo-oxidative layers forms a groove.

[0022] In some embodiments, forming an oxide layer and a first conductive layer includes:

[0023] Form the first conductive layer covering the logic area and memory area;

[0024] The first conductive layer is etched back so that the top surface of the remaining first conductive layer is not higher than the first surface, and the top surface of the second sacrificial layer is exposed;

[0025] After removing the second sacrificial layer, a deposition process is used to form an oxide layer that fills the first trench and covers the top surface of the nitride mask layer and the first conductive layer.

[0026] Excess oxide layer above the nitride mask layer is removed using a mechanical grinding process.

[0027] In some embodiments, after forming the oxide layer, the process includes:

[0028] Remove the nitride mask layer;

[0029] Chemical dry etching is used to sequentially remove the oxide layer of the storage area and the oxide mask layer of the logic area.

[0030] In some embodiments, forming a first control gate and a second control gate includes:

[0031] An oxide dielectric layer, a second conductive layer, and a barrier layer are sequentially formed to cover the logic area and the storage area.

[0032] A patterned barrier layer is formed, and a second conductive layer and an oxide dielectric layer are etched based on the patterned barrier layer; the remaining second conductive layer and oxide dielectric layer in the logic region form a first control gate, and the remaining second conductive layer and oxide dielectric layer in the storage region form a second control gate.

[0033] In some embodiments, forming a floating gate layer includes:

[0034] A third sacrificial layer is formed to cover the logic region, and its top surface is higher than that of the barrier layer, and a photoresist layer covers the third sacrificial layer;

[0035] Using a photoresist layer and a barrier layer as masks, a portion of the first conductive layer and substrate located in the storage area is etched away, and the remaining first conductive layer forms a floating gate layer.

[0036] In some embodiments, the second trench includes two primary trenches spaced apart along a first direction; the groove is located on the side of the primary trench away from the adjacent primary trench.

[0037] Secondly, this application provides a semiconductor structure prepared by the preparation method described in any of the above embodiments.

[0038] In the above embodiments, the unexpected technical effects that this application can produce include:

[0039] In the fabrication method provided in this application, primary trenches are formed simultaneously with the first trenches of the logic region. Secondary trenches are then formed through an etch-back process to increase the trench depth of the storage region. This ensures that after the first conductive layer is subsequently filled, the top surface height of the first conductive layer in the storage region matches the top surface height of the oxide layer in the logic region, thus creating a flat and consistent process baseline for the synchronous fabrication of the control gates in both regions. Based on this, the first control gate of the logic region and the second control gate of the storage region can be formed in the same deposition and patterning steps, eliminating the need for separate gate fabrication in each region. This effectively solves the process incompatibility problem caused by the difference in control gate height between the semi-floating gate storage array region and the standard logic device region during fabrication.

[0040] In addition, since the orthographic projection of the sidewall of the second control gate in the secondary trench is limited to the bottom surface of the groove, the control gate itself is a self-aligned mask for subsequent etching of the first conductive layer. This allows the outline of the floating gate layer to be precisely defined by the second control gate, forming a uniform floating gate structure without additional photolithography. This effectively eliminates dimensional fluctuations caused by multiple photolithography alignment deviations and simplifies the overall process. Attached Figure Description

[0041] To more clearly illustrate the technical solutions in the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0042] Figure 1 This is a schematic diagram of a partial structure of a chip integrating a semi-floating gate memory structure and standard logic devices in related technologies.

[0043] Figure 2 This is a schematic flowchart of a method for fabricating a semiconductor structure provided in one embodiment of this application;

[0044] Figure 3 This is a schematic cross-sectional view of the structure obtained after forming the mask structure in step S10 of the preparation method provided in one embodiment of this application;

[0045] Figure 4 This is a cross-sectional schematic diagram of the structure obtained after forming the first trench and the primary trench in step S201 of the preparation method provided in one embodiment of this application.

[0046] Figure 5 This is a cross-sectional schematic diagram of the structure obtained after forming the first sacrificial layer in step S202 of the preparation method provided in one embodiment of this application;

[0047] Figure 6 This is a cross-sectional schematic diagram of the structure obtained after forming the second trench in step S203 of the preparation method provided in one embodiment of this application;

[0048] Figure 7 This is a cross-sectional schematic diagram of the structure obtained after forming a thermo-oxidative layer in step S301 of the preparation method provided in one embodiment of this application;

[0049] Figure 8 This is a schematic cross-sectional view of the structure obtained after forming the second sacrificial layer and the third trench in step S302 of the preparation method provided in one embodiment of this application.

[0050] Figure 9This is a schematic cross-sectional view of the structure obtained after forming a groove in step S303 of the preparation method provided in one embodiment of this application;

[0051] Figure 10 This is a cross-sectional schematic diagram of the structure obtained after forming the first conductive layer in step S401 of the preparation method provided in one embodiment of this application;

[0052] Figure 11 This is a cross-sectional schematic diagram of the structure obtained after forming an oxide medium layer in step S402 of the preparation method provided in one embodiment of this application;

[0053] Figure 12 This is a cross-sectional schematic diagram of the structure obtained after forming the second conductive layer and the barrier layer in step S501 of the preparation method provided in one embodiment of this application.

[0054] Figure 13 This is a cross-sectional schematic diagram of the structure obtained after forming the first control gate and the second control gate in step S502 of the preparation method provided in one embodiment of this application;

[0055] Figure 14 This is a schematic cross-sectional view of the structure obtained after forming the third sacrificial layer in step S601 of the preparation method provided in one embodiment of this application;

[0056] Figure 15 This is a cross-sectional schematic diagram of the structure obtained after forming the floating gate layer in step S602 of the preparation method provided in one embodiment of this application;

[0057] Figure 16 For this Figure 15 The diagram shows a cross-sectional view of the structure obtained after the sidewalls and source / drain regions are formed in the structure shown.

[0058] Explanation of reference numerals in the attached figures:

[0059] 100, Substrate; 101, Logic region; 102, Storage region; 110, First trench; 120, Second trench; 130, Third trench; 121, Primary trench; 122, Secondary trench; 200, Mask structure; 220, Nitride mask layer; 210, Oxide mask layer; 310, First sacrificial layer; 320, Second sacrificial layer; 330, Third sacrificial layer; 410, Thermal oxide layer; 420, Trench; 510, First conductive layer; 520, Oxide layer; CG1, First control gate; CG2, Second control gate; 610, Dielectric oxide layer; 620, Second conductive layer; 630, Barrier layer; FG, Floating gate layer. Detailed Implementation

[0060] To facilitate understanding of this application, a more complete description will be provided below with reference to the accompanying drawings, which illustrate preferred embodiments of the application. However, this application may be implemented in many different forms and is not limited to the embodiments described herein. Rather, these embodiments are provided so that the disclosure of this application will be thorough and complete.

[0061] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs. The terminology used herein is for the purpose of describing particular embodiments only and is not intended to be limiting of the application.

[0062] It should be understood that when an element or layer is referred to as "on," "adjacent to," "connected to," or "coupled to" other elements or layers, it may be directly on, adjacent to, connected to, or coupled to other elements or layers, or there may be intervening elements or layers. Conversely, when an element is referred to as "directly on," "directly adjacent to," "directly connected to," or "directly coupled to" other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc., may be used to describe various elements, parts, regions, layers, doping types, and / or portions, these elements, parts, regions, layers, doping types, and / or portions should not be limited by these terms. These terms are only used to distinguish one element, part, region, layer, doping type, or portion from another element, part, region, layer, doping type, or portion. Therefore, without departing from the teachings of this application, the first element, component, region, layer, doping type, or portion discussed below may be represented as a second element, component, region, layer, or portion; for example, the first doping type may be referred to as the second doping type, and similarly, the second doping type may be referred to as the first doping type; the first doping type and the second doping type are different doping types, for example, the first doping type may be P-type and the second doping type may be N-type, or the first doping type may be N-type and the second doping type may be P-type.

[0063] Spatial relation terms such as “below,” “under,” “below,” “under,” “above,” “above,” etc., are used herein to describe the relationship between one element or feature shown in the figure and other elements or features. It should be understood that, in addition to the orientation shown in the figure, spatial relation terms also include different orientations of the device in use and operation. For example, if the device in the figure is flipped, the element or feature described as “below,” “under,” or “below” will be oriented “above” the other element or feature. Therefore, the exemplary terms “below” and “under” can include both above and below orientations. Furthermore, the device may also include other orientations (e.g., rotated 90 degrees or other orientations), and the spatial descriptive terms used herein will be interpreted accordingly.

[0064] When used herein, the singular forms of “a,” “an,” and “the” may also include the plural forms unless the context clearly indicates otherwise. It should also be understood that when the terms “comprise” and / or “comprising” are used in this specification, the presence of the stated feature, integer, step, operation, element, and / or part is established, but the presence or addition of one or more other features, integers, steps, operations, elements, parts, and / or groups is not excluded. Meanwhile, when used herein, the term “and / or” includes any and all combinations of the associated listed items.

[0065] Embodiments of the invention are described herein with reference to cross-sectional views illustrating ideal embodiments (and intermediate structures) of this application, thus allowing for variations in the illustrated shapes due to, for example, manufacturing techniques and / or tolerances. Therefore, embodiments of this application should not be limited to the specific shapes of the regions shown herein, but rather include shape deviations due to, for example, manufacturing techniques. For instance, implantation regions shown as rectangular typically have rounded or curved features at their edges and / or implantation concentration gradients, rather than a binary change from implantation regions to non-implantation regions. Similarly, the buried regions formed by implantation can result in some implantation in the region between the buried region and the surface traversed during implantation. Therefore, the regions shown in the figures are substantially schematic, and their shapes do not represent the actual shapes of regions of the device and do not limit the scope of this application.

[0066] Figure 1 This diagram illustrates a partial structure of a chip integrating a semi-floating gate memory structure and standard logic devices, as shown in related technologies. Figure 1 As shown, since the semi-floating gate memory array region adopts a Poly / OX / Poly composite stacked gate structure, while the standard logic device in the chip logic function region adopts a conventional Poly / OX single-layer gate structure, a fixed gate height difference is formed between the memory region and the logic region. This height difference cannot be prepared simultaneously by conventional etching process and chemical mechanical polishing process, and cannot meet the matching process requirements of integrated memory and logic.

[0067] Based on this, please refer to the following: Figure 2 This application provides a method for fabricating a semiconductor structure, comprising:

[0068] Step S10: Provide a substrate; the substrate includes a logic region and a storage region arranged along a first direction parallel to the first surface of the substrate.

[0069] Step S20: A first trench is formed in the logic region, and a second trench is formed in the storage region; the second trench includes a secondary trench extending into the substrate via a first surface, and a primary trench whose top surface is within the bottom surface of the secondary trench and is fabricated concurrently with the first trench.

[0070] Step S30: Form a thermal oxide layer covering the inner surfaces of the first trench and the second trench, and a groove located in the secondary trench that exposes a portion of the substrate surface.

[0071] Step S40: Form an oxide layer that fills the first trench and a first conductive layer that fills the second trench.

[0072] Step S50: A first control gate is formed on the top surface of the logic region away from the oxide layer, and a second control gate is formed on the top surface of the first conductive layer directly above the primary trench; the orthographic projection of the sidewall of the second control gate in the secondary trench is located inside the bottom surface of the groove.

[0073] Step S60: Based on the second control gate, remove part of the first conductive layer so that the remaining first conductive layer located directly below the second control gate constitutes a floating gate layer.

[0074] It should be understood that, although Figure 2 The steps in the flowchart are shown sequentially as indicated by the arrows, but these steps are not necessarily executed in the order indicated by the arrows. Unless otherwise specified herein, there is no strict order in which these steps are executed, and they can be performed in other orders. Figure 2 At least some of the steps in the process may include multiple steps or multiple stages. These steps or stages are not necessarily completed at the same time, but may be executed at different times. The execution order of these steps or stages is not necessarily sequential, but may be executed in turn or alternately with other steps or at least some of the steps or stages in other steps.

[0075] The following is combined Figures 3-16 The steps of the semiconductor structure fabrication method in this embodiment are described in detail. It should be noted that the films shown in the accompanying drawings as rectangles or other shapes are for illustrative purposes only and are not drawn to the actual scale of the device; they are merely illustrative examples.

[0076] Please see Figure 3In step S10, a substrate 100 is provided. The substrate 100 includes a logic region 101 and a storage region 102 arranged sequentially along a first direction (Y direction in the figure) parallel to the first surface (i.e., the upper surface) of the substrate 100. In this embodiment, the substrate 100 can be a silicon substrate, or a germanium substrate, a germanium-silicon substrate, a silicon carbide substrate, a silicon-on-insulator (SOI) substrate, or a germanium-on-insulator (GOI) substrate, etc., and this application does not impose any special limitations on this.

[0077] like Figure 3 As shown, a mask structure 200 is disposed on the first surface of the substrate 100. The mask structure includes a nitride mask layer 220 and an oxide mask layer 210 arranged sequentially along a second direction toward the substrate 100 (i.e., a direction perpendicular to the first surface, such as the Z direction in the figure). Specifically, the oxide mask layer 210 is located on the first surface of the substrate 100, and the nitride mask layer 220 is located on the top surface of the oxide mask layer 210 away from the substrate 100.

[0078] In this embodiment, the oxide mask layer 210 can be a silicon oxide (SiO2) layer, the nitride mask layer 220 can be a silicon nitride (Si3N4) layer, and the mask structure 200 can be sequentially formed on the surface of the substrate 100 by processes such as chemical vapor deposition (CVD) or thermal oxidation.

[0079] Please see Figures 4-6 In some embodiments, step S20 includes the following sub-steps:

[0080] Please see Figure 4 In step S201, combined with photolithography and etching processes, a first trench 110 and a primary trench 121 extending into the substrate 100 via the first surface are formed in the logic region 101 and the storage region 102, respectively.

[0081] Specifically, the first trench 110 and the primary trench 121 are formed using the same photomask and the same etching process, with their angle controlled at approximately 89°. The first trench 110 of the logic region 101 serves as an isolation trench, used to form a shallow trench isolation (STI) structure, while the primary trench 121 is used to form the portion of the floating gate structure that extends into the substrate. It should be understood that the height design of the floating gate structure needs to be compatible with the depth of the isolation trench. In this embodiment, the width and depth of the first trench 110 and the primary trench 121 are the same.

[0082] It should be understood that, Figure 4 The diagram only shows a partial schematic of adjacent logic regions 101 and memory regions 102 in the semiconductor structure. In the actual arrangement, multiple first trenches 110 are arranged at intervals along the OY direction in the logic region, and multiple first-level trenches 121 are arranged at intervals along the OY direction in the memory region 102.

[0083] Please combine Figure 4 See Figure 5 In step S202, a first sacrificial layer 310 is formed to fill the first trench 110 and the first-level trench 121 and cover the top surface of the nitride mask layer 220. The excess first sacrificial layer 310 above the top surface of the mask structure is removed by etch-back or chemical mechanical polishing process, so that the top surface of the first sacrificial layer 310 is flush with the top surface of the nitride mask layer 220.

[0084] In this embodiment, the first sacrificial layer 310 can be a spin-on carbon (SOC) material, which has good gap-filling ability and planarization characteristics. It can be formed by spin coating process and cured by baking.

[0085] Please see Figure 6 In step S203, the patterned photoresist layer PR is used as a mask to etch back the substrate 100 of the storage region 102, forming secondary trenches 122 extending into the substrate 100 via the first surface on both sides of the first sacrificial layer 310. After removing the first sacrificial layer 310 and the photoresist layer, the primary trench 121 and the secondary trench 122 together constitute the second trench 120.

[0086] In this embodiment, the depth of the secondary trench 122 can be set according to the height of the floating gate structure required by the storage cell. Figure 6 The image shows the second groove 120 as a combination of two primary grooves 121 and a secondary groove 122. In some embodiments, the second groove 120 may also be formed by a primary groove 121 and a secondary groove 122.

[0087] Please see Figures 7-9 In some embodiments, step S30 includes the following sub-steps:

[0088] See Figure 7 Step S301: Remove the first sacrificial layer in the first trench 110 and form a thermal oxidation layer 410 on the inner surface of the first trench 110 and the second trench 120 using a thermal oxidation process.

[0089] In this embodiment, the thickness of the thermal oxidation layer 410 can be set according to the device's operating voltage requirements, and is not specifically limited here. The thermal oxidation layer 410 formed by the thermal oxidation process has a uniform thickness and a low interface defect density, which is beneficial to improving the electrical performance of the device.

[0090] Please combine Figure 7 See Figure 8In step S302, a second sacrificial layer 320 is formed covering the mask structure 200 and the thermal oxide layer 410. Next, a patterned photoresist layer is formed on the top surface of the second sacrificial layer 320, and based on the patterned photoresist layer, the second sacrificial layer 320 is etched back to form a third trench 130 that penetrates the second sacrificial layer 320 and the thermal oxide layer 410 along the OZ direction, so as to expose a portion of the surface of the substrate 100.

[0091] In this embodiment, the second sacrificial layer 320 can also be made of spin-coated carbon (SOC) material and formed by spin coating. The second sacrificial layer 320 has good flowability and can fully fill the first trench 110 and the second trench 120.

[0092] Please see Figure 9 Step S303: Remove the second sacrificial layer 320 and the photoresist layer above it within the second trench. Within the storage region 102, the remaining third trench located between adjacent thermal oxide layers 410 constitutes the recess 420. When the second trench includes two primary trenches, the recess 420 is located on the side of the primary trench away from the adjacent primary trench, which facilitates electrical isolation of subsequent adjacent floating gate layers.

[0093] Please see Figures 10-12 In some embodiments, step S40 includes the following sub-steps:

[0094] Please see Figure 10 Step S401: Form a first conductive layer 510 covering the logic region 101 and the storage region 102 using any deposition process. Then, etch back the first conductive layer 510 so that the top surface of the first conductive layer 510 in the storage region 102 is not higher than the first surface, and the top surface of the second sacrificial layer 320 in the logic region 101 is exposed.

[0095] In this embodiment, the first conductive layer 510 includes doped polycrystalline silicon, which can be formed by atomic layer deposition (ALD) or low-pressure chemical vapor deposition (LPCVD) processes.

[0096] For example, the top surface of the first conductive layer 510 may be flush with or lower than the first surface. In this embodiment, the top surface of the first conductive layer 510 is lower than the first surface.

[0097] Please see Figure 11 In step S402, after removing the second sacrificial layer 320, an oxide layer 520 covering the logic region 101 and the storage region 102 is formed using a deposition process. Next, using a nitride mask layer 220 as a polishing stop layer, a chemical mechanical polishing process is performed on the oxide layer 520. The oxide layer 520 filling the first trench constitutes a shallow trench isolation (STI) structure.

[0098] For example, the material of oxide layer 520 includes silicon oxide (SiO2).

[0099] For example, since the second sacrificial layer 320 is a SOC material, it can be removed by ashing or wet stripping processes without damaging the first conductive layer 510 and the thermo-oxidative layer 410.

[0100] Please see Figures 12-13 In some embodiments, step S50 includes the following sub-steps:

[0101] Please see Figure 12 In step S501, due to the different surface oxide thicknesses, a chemical dry etching (CDE) process is used to sequentially remove the oxide layer 520 of the storage region and the oxide mask layer 210 of the logic region. Subsequently, an oxide dielectric layer 610, a second conductive layer 620, and a barrier layer 630 covering the logic region and the storage region are formed using any deposition process.

[0102] For example, the second conductive layer 620 can be doped polycrystalline silicon or metal materials such as copper (Cu) or aluminum (Al).

[0103] For example, the barrier layer 630 may include silicon oxide (SiO2) or silicon nitride (Si3N4) arranged along the OZ direction.

[0104] Please see Figure 13 In step S502, a patterned barrier layer 630 is formed to create control gate patterns corresponding to the logic region 101 and the memory region 102, respectively. Based on the patterned barrier layer 630, a second conductive layer 620 and an oxide dielectric layer 610 are etched. The etching stops at the surface of the substrate 100 or the top surface of the first conductive layer 510. The remaining second conductive layer 620 and oxide dielectric layer 610 located in the logic region 101 constitute the first control gate CG1 (logic gate), and the remaining second conductive layer 620 and oxide dielectric layer 610 located in the memory region 102 constitute the second control gate CG2.

[0105] In this embodiment, the second control gate CG2 of the storage region 102 is formed on the top surface of the first conductive layer 510 directly above the primary trench, and the orthographic projection of the sidewall of the second control gate CG2 in the secondary trench is located inside the bottom surface of the groove. This positional relationship ensures that when the first conductive layer 510 is subsequently etched back using the second control gate CG2 as a mask, the etching range is limited to inside the groove, thereby realizing the fabrication of the floating gate layer.

[0106] Please see Figures 14-15 In some embodiments, step S60 includes the following sub-steps:

[0107] Please see Figure 14In step S601, a third sacrificial layer 330 with its top surface higher than the barrier layer 630 is formed in the logic region 101 and the storage region 102, and a photoresist layer covering the logic region 101 is formed.

[0108] In this embodiment, the third sacrificial layer 330 also uses spin-coated carbon (SOC) material.

[0109] Please see Figure 15 Step S602: Using the patterned photoresist layer as a mask, after removing the third sacrificial layer of the storage area, a portion of the first conductive layer 510 and the substrate 100 are etched away.

[0110] During the etching process described above, the barrier layer 630 above the second control gate CG2 acts as a hard mask, protecting the second control gate CG2 and the first conductive layer 510 located directly below it from etching. The remaining first conductive layer 510 constitutes the floating gate layer FG. The memory region 102 forms a floating gate structure with a memory cell having the floating gate layer FG and the second control gate CG2 located above the floating gate.

[0111] It should be noted that after step S60, subsequent standard semiconductor process steps such as barrier layer removal, source / drain implantation, sidewall formation, and contact hole formation may also be included. These are well known to those skilled in the art and will not be described in detail here. The resulting structure is as follows: Figure 16 As shown.

[0112] Furthermore, in some other embodiments of this application, a semiconductor structure is also provided, which is fabricated using the fabrication method described in any of the above embodiments. Since this semiconductor structure employs the above-described fabrication method, it has advantages such as good integration of logic and memory region processes, which will not be described in detail here.

[0113] As can be seen from the detailed description of the above specific embodiments, the preparation method provided in this application reserves space for the formation of the floating gate layer through the second trench, ensuring that the starting height of the subsequent control gate deposition is uniform, realizing the synchronous integrated preparation of the control gate of the logic region and the memory region, and solving the compatibility problem between the semi-floating gate process and the logic process.

[0114] The technical features of the above embodiments can be combined in any way. For the sake of brevity, not all possible combinations of the technical features of the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0115] The embodiments described above are merely examples of several implementation methods of this application, and while the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the patent application. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of this application, and these modifications and improvements all fall within the protection scope of this application.

Claims

1. A method for fabricating a semiconductor structure, characterized in that, include: A substrate is provided; the substrate includes a logic region and a storage region arranged sequentially along a first direction parallel to a first surface of the substrate; A first trench is formed in the logic area, and a second trench is formed in the storage area; The second trench includes a secondary trench extending into the substrate via the first surface, and a primary trench whose top surface is within the bottom surface of the secondary trench and is prepared concurrently with the first trench. A thermo-oxidative layer is formed covering the inner surfaces of the first trench and the second trench, and a groove is located in the secondary trench, exposing a portion of the substrate surface; An oxide layer is formed that fills the first trench, and a first conductive layer is formed that fills the second trench; A first control gate is formed on the top surface of the logic region away from the oxide layer, and a second control gate is formed on the top surface of the first conductive layer directly above the primary trench; the orthographic projection of the sidewall of the second control gate in the secondary trench is located inside the bottom surface of the groove. Based on the second control gate, a portion of the first conductive layer is removed, such that the remaining first conductive layer located directly below the second control gate constitutes a floating gate layer.

2. The preparation method according to claim 1, characterized in that, A mask structure is provided on the first surface; the mask structure includes a nitride mask layer and an oxide mask layer arranged sequentially along a second direction toward the substrate.

3. The preparation method according to claim 2, characterized in that, Forming the second trench includes: Based on the same photomask, the first trench and the primary trench are formed extending from the first surface into the substrate; A first sacrificial layer is formed in the first trench and the primary trench; A patterned photoresist layer is formed, exposing part of the mask structure of the storage area and the top surface of the first sacrificial layer; The mask structure and the substrate of the storage area are etched sequentially to form the secondary trench; Remove the first sacrificial layer and the photoresist layer; the secondary trench and the primary trench constitute the second trench.

4. The preparation method according to claim 2, characterized in that, Forming the thermal oxide layer and the groove includes: After the thermal oxidation layer is formed using a thermal oxidation process, a second sacrificial layer is formed covering the logic area and the storage area; A third trench is formed that penetrates the second sacrificial layer and the thermo-oxidative layer along the second direction; The second sacrificial layer located in the second trench is removed, and the remaining third trench located between the adjacent thermo-oxidative layers forms the groove.

5. The preparation method according to claim 4, characterized in that, Forming the oxide layer and the first conductive layer includes: A first conductive layer is formed covering the logic area and the storage area; The first conductive layer is etched back so that the top surface of the remaining first conductive layer is not higher than the first surface, and the top surface of the second sacrificial layer is exposed; After removing the second sacrificial layer, a deposition process is used to form an oxide layer that fills the first trench and covers the top surface of the nitride mask layer and the first conductive layer. Excess oxide layer above the nitride mask layer is removed using a mechanical grinding process.

6. The preparation method according to claim 5, characterized in that, After the oxide layer is formed, it includes: Remove the nitride mask layer; The oxide layer of the storage area and the oxide mask layer of the logic area are removed sequentially by chemical dry etching.

7. The preparation method according to claim 6, characterized in that, Forming the first control gate and the second control gate includes: An oxide dielectric layer, a second conductive layer, and a barrier layer are sequentially formed to cover the logic area and the storage area. The barrier layer is patterned, and the second conductive layer and the oxide dielectric layer are etched based on the patterned barrier layer; the remaining second conductive layer and oxide dielectric layer located in the logic region constitute the first control gate, and the remaining second conductive layer and oxide dielectric layer located in the storage region constitute the second control gate.

8. The preparation method according to claim 7, characterized in that, Forming the floating gate layer includes: A third sacrificial layer is formed, covering the logic region and having a top surface higher than the barrier layer, and a photoresist layer is formed covering the third sacrificial layer; Using the photoresist layer and the barrier layer as masks, a portion of the first conductive layer and the substrate located in the storage area are etched away, and the remaining first conductive layer forms a floating gate layer.

9. The preparation method according to claim 7, characterized in that, The second groove includes two primary grooves spaced apart along the first direction; the groove is located on the side of the primary groove away from the adjacent primary groove.

10. A semiconductor structure, characterized in that, It is prepared by the preparation method described in any one of claims 1-9.