Semiconductor structure and its formation method, memory

By employing a thin-film deposition-wet etching process to adjust the thickness uniformity of the protective material layer during the semiconductor structure formation of 3D memory, the problem of uneven thickness of the protective material layer is solved, thereby improving the protective performance of the electrode pillar structure and the electrical performance of the semiconductor device.

CN123124365APending Publication Date: 2026-11-17SHENZHEN ZHANGGE INSTR CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202610299080.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-03-11
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In existing technologies, when forming the semiconductor structure of 3D memory, the protective material layer of the conductive pillar structure has poor thickness uniformity, resulting in poor protection effect during etching, which affects the morphological quality of the electrode pillar structure and the electrical performance and reliability of the semiconductor device.

Method used

A protective material layer is formed covering the top, via sidewalls and bottom of the stacked structure by using a single thin film deposition-wet etching process or a multiple thin film deposition-wet etching alternating cycle process, ensuring that its thickness uniformity is greater than or equal to 90%, and serving as an etching stop layer when removing the sacrificial layer to protect the electrode pillar structure.

Benefits of technology

It improves the uniformity of the protective material layer, enhances the protective performance of the electrode post structure, reduces void generation, and improves the electrical performance and reliability of the semiconductor structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124365A_ABST
    Figure CN123124365A_ABST
Patent Text Reader

Abstract

A semiconductor structure and its formation method, and a memory, wherein the semiconductor structure formation method, after forming a through-hole through a stacked structure with a conductive portion as an etch stop layer, employs a single thin film deposition-wet etch-back process or a multiple thin film deposition-wet etch-back alternating cycle process, which can adjust the step coverage of the protective material layer formed on the top, sidewalls and bottom of the stacked structure, so that the thickness uniformity of the protective material layer located on the sidewall of the through-hole is greater than or equal to 90%, which is beneficial to improving the performance of the formed semiconductor structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor manufacturing, and more particularly to a semiconductor structure and a method for forming the same, and a memory. Background Technology

[0002] The structure of a 3D memory consists of multiple conductive plates and dielectric layers stacked in a cross pattern, with numerous conductive pillars that are wider at the top and narrower at the bottom. The surfaces where the conductive plates and pillars meet are arranged as follows: upper electrode – capacitor material – lower electrode. The upper electrode connects to the upper conductive wire within the conductive plate, and the lower electrode connects to the lower conductive wire within the conductive pillar. 3D memory uses a plate-last process, where the conductive pillars are first constructed, and then a wet etching method is used to contact the sacrificial material layer corresponding to each conductive plate through trenches near the conductive pillar matrix. The sacrificial material layer is then completely removed, and finally, the conductive plate material is filled to form the conductive plate. Summary of the Invention

[0003] The problem solved by the embodiments of the present invention is to provide a semiconductor structure and a method for forming the same, as well as a memory, which can improve the performance of the formed semiconductor structure.

[0004] To address the above problems, embodiments of the present invention provide a method for forming a semiconductor structure, comprising: A substrate is provided, the substrate including a plurality of embedded, mutually isolated conductive portions; A stacked structure is formed on the substrate, the stacked structure comprising a first dielectric layer and a sacrificial layer that are alternately stacked longitudinally from bottom to top; Using the conductive portion as an etching stop layer, through-holes are formed that penetrate the stacked structure, the through-holes exposing the conductive portion, and the number of through-holes is the same as the number of conductive portions; A protective material layer is formed covering the top, sidewalls, and bottom of the stacked structure by employing a single thin film deposition-wet etching process or a multiple thin film deposition-wet etching alternating cycle process. The material of the protective material layer includes a conductive material, and the thickness uniformity of the protective material layer located on the sidewalls of the vias is greater than or equal to 90%. The remaining space of the through-hole is filled to form an electrode post material layer on the protective material layer; Remove the protective material layer and the electrode post material layer that are above the top of the stacked structure, and retain the protective material layer located on the sidewall and bottom of the through hole, as well as the electrode post material layer located in the through hole, as the protective layer and the electrode post structure, respectively. Using the protective layer as an etching stop layer, all the sacrificial layers in the stacked structure are removed to form a plurality of trenches spaced apart in the longitudinal direction, the trenches exposing part of the sidewalls of the protective layer and the surface of the first dielectric layer; A dielectric layer is formed covering a portion of the sidewalls of the protective layer exposed in the trench and the surface of the first dielectric layer; A conductive plate structure is formed that covers the dielectric layer and fills the trench.

[0005] Optionally, the step of forming a protective material layer covering the top, sidewalls, and bottom of the stacked structure using a single thin-film deposition-wet etching process or a multiple thin-film deposition-wet etching alternating cycle process includes: An initial protective material layer is formed by using a thin film deposition process to cover the top, sidewalls, and bottom of the stacked structure, wherein the thickness of the initial protective material layer located on the sidewalls of the through holes gradually decreases from top to bottom; When performing a wet etching process on the initial protective material layer, the contact time between the initial protective material layer and the etching solution used in the wet etching process decreases from top to bottom along the longitudinal direction, and the etching amount of the initial protective material layer gradually decreases. Repeat the thin film deposition process and the wet etching process once or multiple times until the initial protective material layer on the sidewall of the via reaches the target size along the surface direction parallel to the substrate and the thickness uniformity of the remaining initial protective material layer on the sidewall of the via is greater than or equal to 90%, thus forming the protective material layer.

[0006] Optionally, the thin film deposition process includes an atomic layer deposition process.

[0007] Optionally, the process parameters of the wet etching process include: the etching solution is a phosphoric acid solution, the volume percentage concentration of the phosphoric acid solution is 70% to 90%, and the process temperature is 150°C to 170°C.

[0008] Optionally, the material of the protective layer includes tantalum nitride.

[0009] Optionally, after the step of removing the protective material layer and the electrode pillar material layer above the top of the stacked structure, retaining the protective material layer located on the sidewall and bottom of the via, and the electrode pillar material layer located within the via, as the protective layer and the electrode pillar structure respectively, and before the step of removing the sacrificial layer in the stacked structure using the protective layer as an etching stop layer to form a plurality of trenches spaced longitudinally, wherein the trenches expose part of the sidewall of the protective layer and the surface of the first dielectric layer, the method for forming the semiconductor structure further includes: A second dielectric layer is formed on the stacked structure, and the second dielectric layer also covers the protective layer and the top surface of the electrode post structure.

[0010] Optionally, the step of filling the remaining space of the through-hole to form an electrode post material layer on the protective material layer includes: A liner material layer is formed by conformally covering the surface of the protective material layer; A core material layer is formed that covers the padding material layer and fills the groove formed by the enclosure of the padding material layer; The electrode post material layer includes the padding material layer and the core material layer; in the step of removing the protective material layer and the electrode post material layer above the top of the stacked structure, the padding material layer and the core material layer above the top of the stacked structure are also removed.

[0011] Optionally, the material of the liner layer includes titanium nitride, and the material of the core material layer includes tungsten.

[0012] Accordingly, embodiments of the present invention also provide a semiconductor structure, comprising: A substrate, the substrate comprising a plurality of embedded, mutually isolated conductive portions; A stacked structure is located on the substrate, the stacked structure comprising a first dielectric layer and a conductive plate structure that are alternately stacked longitudinally from bottom to top; Multiple conductive pillar structures extend longitudinally through the stacked structure. Each conductive pillar structure includes a protective layer and an electrode pillar structure from the outside to the inside. The protective layer covers the sides and bottom of the electrode pillar structure. The thickness uniformity of the protective layer is greater than or equal to 90%, and the bottom surface of the protective layer is in contact with the conductive part. A dielectric layer is located between the conductive plate structure and the protective layer, and between the conductive plate structure and the first dielectric layer.

[0013] Accordingly, embodiments of the present invention also provide a memory, including a semiconductor structure as described above and a plurality of transistors, wherein the number of transistors is consistent with the number of conductive pillars, and the conductive portion is the source or drain of the transistor.

[0014] Compared with the prior art, the technical solution of the embodiments of the present invention has the following advantages: In the semiconductor structure formation method provided in this embodiment of the invention, after forming a through-hole through the stacked structure with the conductive part as the etching stop layer, a single thin film deposition-wet etch-back process or a multiple thin film deposition-wet etch-back alternating cycle process is used to adjust the step coverage capability of the protective material layer formed on the top, sidewall and bottom of the stacked structure, so that the thickness uniformity of the protective material layer on the sidewall of the through-hole is greater than or equal to 90%. This can avoid the large difference in thickness uniformity of the protective layer on the sidewall of the through-hole, which would cause the etching solution used in the process of removing the sacrificial layer in the stacked structure to etch away the thinner protective layer on the sidewall of the through-hole. This can improve the protective performance of the protective material layer on the sidewall of the through-hole for the electrode pillar structure.

[0015] Furthermore, the thickness uniformity of the protective material layer located on the sidewall of the via is greater than or equal to 90%. When the remaining space of the via is filled, an electrode pillar material layer is formed on the protective material layer, which can improve the pore filling performance of the electrode pillar material layer, reduce or avoid the generation of voids, and improve the morphological quality of the formed electrode pillar structure, thereby helping to improve the performance of the formed semiconductor structure. Attached Figure Description

[0016] Figures 1 to 7 A schematic diagram of the corresponding structure for each step in a method for forming a semiconductor structure is shown. Figures 8 to 20 The diagram shows a schematic representation of a key step in an embodiment of the semiconductor structure formation method provided by the present invention. Detailed Implementation

[0017] Forming a protective layer as an etch stop layer for electrode pillar structures within vias with high aspect ratios still faces numerous challenges, leading to structural collapse in the resulting semiconductor structures. This paper analyzes the causes of semiconductor structure collapse in conjunction with a semiconductor structure formation method.

[0018] like Figures 1 to 7 As shown, a schematic diagram of each step in a method for forming a semiconductor structure is illustrated.

[0019] refer to Figure 1 A substrate 10 is provided, which includes a plurality of embedded, mutually isolated conductive portions 11 (only one conductive portion 11 is shown in the figure).

[0020] refer to Figure 2 A stacked structure 12 is formed on the substrate 10, the stacked structure 12 including sacrificial layers 121 and dielectric layers 122 that are stacked alternately from bottom to top in the longitudinal direction. refer to Figure 3Using the conductive part 105 as an etching stop layer, a through hole 13 is formed that penetrates the stacked structure 12, and the through hole 13 exposes the conductive part 11; refer to Figure 4 A protective material layer 14' is formed covering the top, sidewalls and bottom of the laminated structure 12; refer to Figure 5 The remaining space of the through hole 13 is filled to form an electrode post material layer 15' on the protective material layer 14'; refer to Figure 6 Remove the protective material layer 14' and electrode post material layer 15' that are above the top of the stacked structure 12, and retain the protective material layer 15' located on the side wall and bottom of the through hole 13, and the electrode post material layer 15' located in the through hole 13, which serve as the protective layer 14 and the electrode post structure 15, respectively. refer to Figure 7 Using the protective layer 14 as the etching stop layer, all sacrificial layers 121 in the stacked structure 12 are removed, forming a plurality of trenches 16 spaced longitudinally. The trenches 16 expose part of the sidewalls of the protective layer 14 and the surface of the dielectric layer 122. It should be noted that before removing all sacrificial layers 121 in the stacked structure 12, a slit opening is formed penetrating the stacked structure 12. This slit opening is used to provide an etching solution flow channel for the wet etching process, allowing subsequent etching solution to laterally etch and remove all sacrificial layers 121 in the stacked structure 12 through the slit opening.

[0021] When the depth-to-width ratio of the through hole 13 is large, the step coverage of the protective material layer 14' is poor, resulting in the protective material layer 14' forming a shape that is wider at the top and narrower at the bottom on the side wall of the through hole 13. That is, the thickness uniformity of the protective material layer 14' on the side wall of the through hole 13 is poor.

[0022] Accordingly, such as Figure 7 As shown in the dashed box 20, during the wet etching process to remove the sacrificial layer 121 in the stacked structure 12, the etching solution used may remove a portion of the thinner protective layer 14 located on the sidewall of the via 13, and may even cause partial damage to the electrode pillar structure 15 that has lost the protection of the protective layer 14. Furthermore, the protective material layer 14' on the sidewall of the via 13 has a top-wide and bottom-narrow morphology, which will also affect the pore-filling ability of the electrode pillar material layer 15', causing voids to easily form in the lower part of the electrode pillar material layer 15' filled in the via 13, making the formed semiconductor structure prone to collapse, thereby affecting the overall electrical performance and reliability of the formed semiconductor device.

[0023] To address the aforementioned technical problems, embodiments of the present invention provide a method for forming a semiconductor structure, comprising: providing a substrate, the substrate including a plurality of embedded, mutually isolated conductive portions; forming a stacked structure on the substrate, the stacked structure including a first dielectric layer and a sacrificial layer alternately stacked longitudinally from bottom to top; forming vias penetrating the stacked structure using the conductive portions as etching stop layers, the vias exposing the conductive portions, the number of vias being consistent with the number of conductive portions; and forming a protective material layer covering the top, sidewalls, and bottom of the stacked structure using a single thin-film deposition-wet etch-back process or a multiple thin-film deposition-wet etch-back alternating cycle process, the protective material layer comprising a conductive material, the protective material layer located on the sidewalls of the vias being formed. The thickness uniformity of the material layer is greater than or equal to 90%; the remaining space of the via is filled to form an electrode pillar material layer on the protective material layer; the protective material layer and electrode pillar material layer above the top of the stacked structure are removed, and the protective material layer located on the sidewall and bottom of the via, as well as the electrode pillar material layer located in the via, are retained as the protective layer and electrode pillar structure, respectively; using the protective layer as the etching stop layer, all sacrificial layers in the stacked structure are removed to form multiple trenches arranged longitudinally at intervals, the trenches exposing part of the sidewall of the protective layer and the surface of the first dielectric layer; a dielectric layer is formed covering part of the sidewall of the protective layer exposed by the trenches and the surface of the first dielectric layer; a conductive plate structure covering the dielectric layer and filling the trenches is formed.

[0024] In the semiconductor structure formation method provided in this embodiment of the invention, after forming a through-hole through the stacked structure with the conductive part as the etching stop layer, a single thin film deposition-wet etch-back process or a multiple thin film deposition-wet etch-back alternating cycle process is used to adjust the step coverage capability of the protective material layer formed on the top, sidewall and bottom of the stacked structure, so that the thickness uniformity of the protective material layer on the sidewall of the through-hole is greater than or equal to 90%. This can avoid the large difference in thickness uniformity of the protective layer on the sidewall of the through-hole, which would cause the etching solution used in the process of removing the sacrificial layer in the stacked structure to etch away the thinner protective layer on the sidewall of the through-hole. This can improve the protective performance of the protective material layer on the sidewall of the through-hole for the electrode pillar structure.

[0025] Furthermore, the thickness uniformity of the protective material layer located on the sidewall of the via is greater than or equal to 90%. When the remaining space of the via is filled, an electrode pillar material layer is formed on the protective material layer, which can improve the pore filling performance of the electrode pillar material layer, reduce or avoid the generation of voids, and improve the morphological quality of the formed electrode pillar structure, thereby helping to improve the performance of the formed semiconductor structure.

[0026] To make the above-mentioned objects, features and advantages of the present invention more apparent and understandable, specific embodiments of the present invention will be described in detail below with reference to the accompanying drawings.

[0027] Figures 8 to 20This is a schematic diagram of the key steps in one embodiment of the semiconductor structure formation method provided by the present invention.

[0028] Please refer to the reference. Figure 8 A substrate 100 is provided, which includes a plurality of embedded, mutually isolated conductive portions 105 (only one conductive portion 105 is shown in the figure).

[0029] The substrate 100 provides the process basis for the formation process of the semiconductor structure of the present invention.

[0030] In some embodiments, the substrate 100 is a substrate having a semiconductor structure. Exemplarily, the substrate material includes silicon. Silicon is a commonly used material in semiconductor processes; it is compatible with many other materials and mainstream semiconductor manufacturing processes. In other embodiments, the substrate material may also include germanium, silicon germanide, silicon carbide, gallium arsenide, or indium gallium dihydrogen phosphate, etc.

[0031] The conductive part 105 is used for electrical connection with the subsequently formed conductive pillar structure.

[0032] In some embodiments, the conductive portion 105 can be a contact, or it can be the source or drain of a transistor. In other embodiments, the conductive portion can also be a pad or a conductive line, etc.

[0033] In some embodiments, there are multiple conductive parts 105. Specifically, each conductive part 105 is provided in a one-to-one correspondence with a subsequently formed conductive post structure.

[0034] Please refer to the reference. Figure 9 A laminated structure 110 is formed on a substrate 100, the laminated structure 110 including components along the longitudinal direction (e.g., Figure 20 The sacrificial layer 111 and the first dielectric layer 112 are stacked alternately from bottom to top in the Z direction of the stack. It should be noted that the topmost layer of the stacked structure 110 is the first dielectric layer 112.

[0035] The stacked structure 110 is used to provide a foundation for the subsequent formation of conductive pillar structures and conductive plate structures therein.

[0036] The sacrificial layer 111 is used to occupy space for the subsequent formation of the conductive plate structure.

[0037] In some embodiments, the material of the sacrificial layer 111 includes silicon nitride.

[0038] The thickness of the sacrificial layer 111 can be set by those skilled in the art according to actual needs. Specifically, the thickness of the sacrificial layer 111 is sufficient to provide enough space for the subsequent formation of the conductive plate structure, and to ensure that the longitudinal dimension of the formed semiconductor structure is not too large, thereby improving the integration density of the formed semiconductor structure. As an example, the thickness of the sacrificial layer 111 is 10 nm to 200 nm.

[0039] The first dielectric layer 112 is used to achieve electrical isolation between longitudinally adjacent conductive plate structures.

[0040] In some embodiments, the material of the first dielectric layer 112 includes silicon oxide.

[0041] The sacrificial layer 111 is made of silicon nitride, and the first dielectric layer 112 is made of silicon oxide. This results in a large etching selectivity between the sacrificial layer 111 and the first dielectric layer 112 during the subsequent wet etching process to remove the sacrificial layer 111. The etching solution causes little or no damage to the first dielectric layer 112, which is beneficial to improving the performance of the formed semiconductor structure.

[0042] In some embodiments, the thickness of the first dielectric layer 112 is 10 nm to 100 nm to ensure good electrical isolation and to ensure that the space occupied by the semiconductor structure is not too large, thereby improving the integration of the formed semiconductor structure.

[0043] Please refer to the reference. Figure 10 Using the conductive portion 105 as an etching stop layer, through-holes 115 are formed that penetrate the stacked structure 110. The through-holes 115 expose the conductive portion 105, and the number of through-holes 115 is the same as the number of conductive portions 105.

[0044] Through hole 115 is used to provide space for the subsequent formation of conductive pillar structure.

[0045] In the step of forming through-holes 115 through the stacked structure 110 using conductive portion 105 as an etch stop layer, the number of through-holes 115 is the same as the number of conductive portions 105, that is, through-holes 115 and conductive portions 105 are provided in a one-to-one correspondence. Accordingly, in the step of forming through-holes 115 through the stacked structure 110 using conductive portion 105 as an etch stop layer, each through-hole 115 exposes a corresponding conductive portion 105, so that the conductive pillar structure subsequently formed in the through-hole 115 can be electrically connected to the corresponding conductive portion 105.

[0046] In some embodiments, there are multiple conductive portions 105. Correspondingly, in the step of forming through holes 115 through the stacked structure 110 with the conductive portion 105 as the etching stop layer, multiple through holes 115 through the stacked structure 110 are formed with each conductive portion 105 as the etching stop layer, and the multiple through holes 115 expose the corresponding conductive portion 105.

[0047] In some embodiments, in the step of forming a through-hole 115 through the stacked structure 110 with the conductive portion 105 as the etching stop layer, the through-hole 115 exposes the top surface of the conductive portion 105. Subsequently, after a conductive pillar structure is formed in the through-hole 115, the conductive pillar structure contacts the top surface of the conductive portion 105 to achieve electrical connection.

[0048] In some embodiments, the process of forming the via 115 includes a dry etching process.

[0049] In some embodiments, in the step of forming a through hole 115 through the stacked structure 110 with the conductive part 105 as the etching stop layer, the sidewall and bottom of the through hole 115 are in a vertical or nearly vertical state, so that the through hole 115 has a good morphology.

[0050] The via 115 is used for the subsequent formation of a conductive pillar structure, and the opening size of the via 115 is set according to the size of the conductive pillar structure subsequently formed therein. In some embodiments, the opening size of the via 115 is 10 nm to 80 nm.

[0051] It is understandable that the smaller the size of the via 115, the more difficult the process of forming the via 115 is, and the smaller the size of the via 115, the more conducive it is to achieving a higher electrical integration of the formed semiconductor structure.

[0052] Please refer to the reference. Figures 11 to 13 A protective material layer 120' is formed covering the top of the stacked structure 110, the sidewalls of the via 115, and the bottom by using a single thin film deposition-wet etching process or a multiple thin film deposition-wet etching alternating cycle process. The material of the protective material layer 120' includes conductive material, and the thickness uniformity of the protective material layer 120' located on the sidewall of the via 115 is greater than or equal to 90%.

[0053] The protective material layer 120' is used to form a protective layer in the subsequent process of removing the sacrificial layer 111 in the stacked structure 110, so as to protect the electrode pillar structure.

[0054] In the step of forming a protective material layer 120' covering the top, sidewalls and bottom of the through-hole 115 of the stacked structure 110 using a single thin film deposition-wet etching process or a multiple thin film deposition-wet etching alternating cycle process, the protective material layer 120' is made of a conductive material, so that the protective material layer 120' can be used as part of the conductive pillar structure. This eliminates the need to remove the protective material layer 120' of the through-hole 115 in the subsequent process, which helps to simplify the process and does not affect the electrical connection performance between the conductive pillar structure and the conductive part 105, nor does it affect the capacitor structure formed by the conductive pillar structure and the conductive plate structure.

[0055] In the step of forming a protective material layer 120' covering the top, sidewalls, and bottom of the stacked structure 110, using a single thin film deposition-wet etching process or a multiple thin film deposition-wet etching alternating cycle process, if the thickness uniformity of the protective material layer 120' located on the sidewall of the through hole 115 is greater than or equal to 90%, then in the subsequent etching process to remove the sacrificial layer 111 in the stacked structure 110, the etching solution used can avoid etching away the thinner protective material layer 120' on the sidewall of the through hole 115. This helps to ensure the etching stop effect of the protective material layer 120' located on the sidewall of the through hole 115, thereby helping to ensure the protection performance of the subsequently formed electrode post structure.

[0056] Meanwhile, the thickness uniformity of the protective material layer 120' located on the sidewall of the through hole 115 is greater than or equal to 90%, which makes the protective material layer 120' located on the sidewall of the through hole 115 and the protective material layer 120' located at the bottom of the through hole 115 nearly perpendicular or perpendicular to each other. This provides a geometric cavity with a uniform cross section and nearly perpendicular sidewall and bottom for the subsequent electrode post structure formation process, so that seamless and dense filling can be achieved when the electrode post structure is deposited on the protective material layer 120' of the through hole 115.

[0057] In some embodiments, the step of forming a protective material layer covering the top of the stacked structure 110, the sidewalls of the via 115, and the bottom using a single thin-film deposition-wet etch-back process or a multiple thin-film deposition-wet etch-back alternating cycle process includes: (Refer to reference) Figure 11 An initial protective material layer 120'' is formed using a thin-film deposition process, covering the top, sidewalls, and bottom of the stacked structure 110, the via 115, and the via itself. The thickness of the initial protective material layer 120'' located on the sidewalls of the via 115 gradually decreases from top to bottom. (Please refer to the reference.) Figure 12 A wet etching process is performed on the initial protective material layer 120''. Along the vertical direction from top to bottom, the contact time between the initial protective material layer 120'' and the etching solution used in the wet etching process decreases, resulting in a gradually smaller etching amount on the initial protective material layer 120''. Please refer to the reference. Figure 13Repeat the thin film deposition process and wet etching process once or multiple times until the initial protective material layer 120'' on the sidewall of the via 115 reaches the target size along the surface direction parallel to the substrate and the thickness uniformity of the remaining initial protective material layer 120'' on the sidewall of the via 115 is greater than or equal to 90%, thus forming the protective material layer 120'.

[0058] In some embodiments, an initial protective material layer 120'' is formed using an atomic layer deposition (ALD) process to cover the top of the stacked structure 110, the sidewalls of the via 115, and the bottom. The film layer formed by the atomic layer deposition process has good thickness uniformity and good step coverage capability, enabling the initial protective material layer 120'' to cover the top of the stacked structure 110, the sidewalls of the via 115, and the bottom in a well-conformable manner.

[0059] In other embodiments, the process for forming the initial protective material layer covering the top, through-hole sidewalls and bottom of the laminated structure can also employ a low-pressure chemical vapor deposition (LPCVD) process, etc.

[0060] It should be noted that when the depth-to-width ratio of the via 115 is large, due to the limitations of the thin film deposition process, the thickness of the initial protective material layer 120'' formed on the sidewall of the via 115 gradually decreases from top to bottom. That is, the initial protective material layer 120'' on the sidewall of the via 115 has a shape that is wider at the top and narrower at the bottom.

[0061] Therefore, during the wet etching process of the initial protective material layer 120'', the etching solution used flows into the via 115 in the longitudinal direction from top to bottom and reacts with the initial protective material layer 120'' located on the sidewall of the via 115. As a result, the contact time between the initial protective material layer 120'' and the etching solution used in the wet etching process decreases in the longitudinal direction from top to bottom, and the etching amount of the initial protective material layer 120'' gradually decreases. This reduces the thickness difference of the initial protective material layer 120'' on the sidewall of the via 115, making it negligible, thereby improving the thickness uniformity of the initial protective material layer 120'' formed on the sidewall of the via 115.

[0062] In addition, the wet etching back process has a relatively low cost and simple operation steps, and can achieve a large etching selectivity, which is beneficial to reduce damage to other film layers during the wet etching back process on the initial protective material layer 120''.

[0063] In some embodiments, the material of the initial protective material layer 120'' is tantalum nitride, and accordingly, the process parameters for performing a wet back etching process on the initial protective material layer 120'' include: the etching solution is a phosphoric acid (HPO) solution, the volume percentage concentration of the phosphoric acid solution is 70% to 90%, and the process temperature is 150°C to 170°C.

[0064] By coordinating the control of the etching solution used in the wet etching process, the volume percentage of the etching solution, and the process temperature, the rate and process of the etching reaction between the etching solution and the initial protective material layer 120'' located on the sidewall of the via 115 can be precisely controlled, thereby improving the thickness uniformity of the initial protective material layer 120'' located on the sidewall of the via 115.

[0065] Depending on the protection requirements for the subsequently formed electrode pillar structure, a single thin-film deposition-wet etch-back process or multiple alternating cycles of thin-film deposition-wet etch-back are performed until the initial protective material layer 120'' on the sidewall of the via 115 reaches the target size along the surface direction parallel to the substrate, and the thickness uniformity of the remaining initial protective material layer 120'' on the sidewall of the via 115 is greater than or equal to 90%, thus forming the protective material layer 120'. As an example, the thickness of the protective material layer 120' is 8 nm to 15 nm.

[0066] Please refer to the reference. Figures 14 to 15 The remaining space in the through hole 115 is filled to form an electrode post material layer 130' on the protective material layer 120'.

[0067] The electrode post material layer 130' is used for subsequent formation of the electrode post structure.

[0068] If the thickness uniformity of the protective material layer 120' located on the sidewall of the through hole 115 is greater than or equal to 90%, the filling process of the electrode post material layer 130' will be smoother and more consistent, so that the filled electrode post material layer 130' can form a dense, void-free conductive column, which is beneficial to fundamentally ensuring the electrical characteristics of the electrode post structure formed by the electrode post material layer 130'.

[0069] In some embodiments, the electrode post material layer 130' includes a pad material layer 131' and a core material layer 132'. Accordingly, the step of filling the remaining space of the through-hole 115 to form the electrode post material layer 130' on the protective material layer 120' includes: (Refer to reference) Figure 14 A liner material layer 131' is formed on the surface of the conformal protective material layer 120'; please refer to the reference. Figure 15 A core material layer 132' is formed, which covers the groove formed by the padding material layer 131'.

[0070] The padding material layer 131' is used to form a subsequent padding layer, serving as a diffusion barrier layer and a nucleation layer for the core material layer 132' subsequently formed in the groove enclosed by the padding material layer 131'. Specifically, as a diffusion barrier layer, the padding layer can effectively prevent adverse reactions, such as diffusion or chemical reactions, between the subsequent core material layer 132' and the substrate material, thereby improving the reliability of the formed semiconductor structure; as a nucleation layer, the padding layer can provide atomic attachment sites for the formation of the core material layer 132', promoting the uniform filling of the core material layer 132' and avoiding the generation of voids or defects.

[0071] In some embodiments, the material of the padding material layer 131' includes titanium nitride (TiN). Titanium nitride has excellent adhesion and diffusion-blocking properties, making it a good material for a padding layer. It is understood that the material of the padding material layer can also be other suitable materials, and no limitation is made herein.

[0072] In some embodiments, the padding material layer 131' is formed using atomic layer deposition (ALD). ALD is a film preparation technique that grows layer by layer at the atomic level. It has the advantages of good bonding strength, consistent film thickness, good compositional uniformity, and good shape retention, which helps to improve the thickness uniformity and film quality of the padding material layer 131'.

[0073] The core material layer 132' is used to form the core part of the conductive pillars in the subsequent 3D memory.

[0074] In some embodiments, the via 115 has a high depth-to-width ratio, and accordingly, a core material layer 132' is formed using chemical vapor deposition (CVD) or atomic layer deposition (ALD). Using CVD or ALD to form the core material layer 132' improves its pore-filling properties, thereby helping to reduce or avoid void formation.

[0075] In some embodiments, the core material layer 132' is made of tungsten. Depending on the specific requirements, the core material layer can also be made of other conductive materials, such as copper or molybdenum, and there is no limitation herein.

[0076] Please refer to the reference. Figure 16 Remove the protective material layer 120' and electrode post material layer 130' that are above the top of the stacked structure 110, and retain the protective material layer 120' located on the side wall and bottom of the through hole 115, and the electrode post material layer 130' located in the through hole 115, which serve as the protective layer 120 and the electrode post structure 130, respectively.

[0077] The protective layer 120 and the electrode pillar structure 130 together form a conductive pillar structure to serve as a conductive pillar for 3D storage.

[0078] In some embodiments, a chemical mechanical polishing (CMP) process is used to remove the electrode post material layer 130' and the protective material layer 120' that extend above the top of the stacked structure 110. The CMP process can effectively remove the electrode post material layer 130' and the protective material layer 120' that extend above the top of the stacked structure 110. Furthermore, by precisely controlling the material removal rate (MRR), the top of the stacked structure 110 after removing the electrode post material layer 130' and the protective material layer 120' can achieve a certain surface morphology.

[0079] In other embodiments, the process of removing the electrode post material layer and the protective material layer above the top of the stacked structure can also be a wet etching process.

[0080] Please refer to the reference. Figure 17 In some embodiments, after removing the electrode pillar material layer 130' and protective material layer 120' above the top of the stacked structure 110, and retaining the protective material layer 120' located on the sidewall and bottom of the via 115, and the electrode pillar material layer 130' located within the via 115 as the protective layer 120 and the electrode pillar structure 130 respectively, the method of forming the semiconductor structure further includes: forming a second dielectric layer 145 on the stacked structure 110, the second dielectric layer 145 also covering the top surface of the protective layer 120 and the electrode pillar structure 130.

[0081] The second dielectric layer 145 covers the top surface of the stacked structure 110, the protective layer 120, and the electrode post structure 130, thereby protecting the top of the stacked structure 110, the protective layer 120, and the electrode post structure 130 in subsequent processes.

[0082] In some embodiments, the material of the second dielectric layer 145 is the same as the material of the first dielectric layer 112; specifically, the material of the second dielectric layer 145 is silicon oxide. It is understood that in other embodiments, the material of the second dielectric layer may also be different from the material of the first dielectric layer.

[0083] In the step of forming a second dielectric layer 145 on the stacked structure 110, wherein the second dielectric layer 145 also covers the top surface of the protective layer 120 and the electrode pillar structure 130, the second dielectric layer 145 is formed by a deposition process such as chemical vapor deposition, physical vapor deposition or atomic layer deposition.

[0084] Please refer to the reference. Figure 18Using the protective layer 120 as the etching stop layer, all sacrificial layers 111 in the stacked structure 110 are removed to form a plurality of trenches 140 arranged longitudinally at intervals. The trenches 140 expose part of the sidewalls of the protective layer 120 and the surface of the first dielectric layer 112.

[0085] The trench 140 is used to provide space for the subsequent formation of dielectric layers and conductive plate structures.

[0086] In some embodiments, a wet etching process is used to remove all sacrificial layers 111 in the stacked structure 110. Specifically, before removing the sacrificial layers 111 using the wet etching process, at least one slit opening (not shown) is formed through the stacked structure 110 with its sidewalls exposed to the sacrificial layers 111, so that the etching solution can be used to etch and remove the sacrificial layers 111 through this slit opening.

[0087] Wet etching, with its isotropic etching characteristics, is advantageous for completely removing all sacrificial layers 111 in the stacked structure 110. Furthermore, wet etching easily achieves a large etching selectivity, thereby reducing damage to other film layers during the removal of the sacrificial layers 111. However, this application is not limited to this; those skilled in the art can select other etching processes with etching selectivity relative to the first dielectric layer 112 and the protective layer 120 to remove the sacrificial layers 111 as needed.

[0088] In some embodiments, the sacrificial layer 111 is made of silicon nitride (SiN), and correspondingly, the etching solution used to remove all sacrificial layers 111 in the stacked structure 110 includes a hot phosphoric acid solution. The process parameters of the hot phosphoric acid solution can be set according to the requirements of etching rate of sacrificial layer 111, process stability and controllability, and avoiding etching loss of other film layers, and are not limited here.

[0089] Please refer to the reference. Figure 19 A dielectric layer 150 is formed covering part of the sidewall of the protective layer 120 exposed in the trench 140 and the surface of the first dielectric layer 112.

[0090] The dielectric layer 150 serves as a storage capacitor material in the 3D memory to store or release charge according to the direction and magnitude of the external electric field. In some embodiments, the dielectric layer 150 is made of a ferroelectric material. Ferroelectric materials become polarized under the influence of an external electric field and retain partial polarization (residual polarization) even after the external electric field is removed. This residual polarization has a potential difference, causing the capacitor electrodes on both sides of the dielectric layer 150—that is, the surfaces of the portions of the dielectric layer 150 closest to the conductive pillar structure and the conductive plate structure, respectively—to induce charges of opposite polarities. Different polarization directions induce different charges, thereby enabling the storage of logic "0" and logic "1". Ferroelectric materials possess spontaneous polarization characteristics and can form two different stable residual polarization states under the influence of an external electric field. By utilizing the aforementioned polarization characteristics of ferroelectric materials to store data "0" or "1", benefits such as high-speed read / write, high durability, and low power consumption can be achieved, making it suitable for various high-performance storage applications.

[0091] In some embodiments, the angle between the sidewall and bottom of the via 115 is a right angle or approximately a right angle. Accordingly, after forming a dielectric layer 150 covering part of the sidewall of the protective layer 120 exposed in the trench 140 and the surface of the first dielectric layer 112, the critical dimensions of the dielectric layer 150 in contact with the protective layer 120 are more uniform. This allows the capacitive electrodes on both sides of the dielectric layer 150 to release equal amounts of charge during data reading, thereby improving the accuracy of data reading and consequently improving the performance of the formed semiconductor structure.

[0092] Please refer to the reference. Figure 20 A conductive plate structure 160 is formed, which covers the dielectric layer 150 and fills the trench 140.

[0093] The conductive plate structure 160 is used as a conductive plate for 3D memory.

[0094] In some embodiments, the conductive plate structure 160 includes an upper electrode covering a dielectric layer 150 and an upper conductor filling a trench 140 and covering the upper electrode, wherein the upper electrode and the upper conductor, together with the dielectric layer, the lower electrode and the lower conductor, form a capacitor structure.

[0095] Specifically, the surfaces in contact with the conductive plate structure 160 and the conductive pillar structure are distributed as an upper electrode-storage capacitor material-lower electrode, i.e., a capacitor layer. The upper electrode is connected to the upper wire in the conductive plate structure 160, and the lower electrode is connected to the lower wire in the conductive pillar structure.

[0096] Accordingly, embodiments of the present invention also provide a semiconductor structure.

[0097] Figure 20 A schematic diagram of a semiconductor structure provided by the technical solution of the present invention is shown. (Referring to the reference...) Figure 20 A semiconductor structure includes: a substrate 100, the substrate 100 including a plurality of embedded, mutually isolated conductive portions 105; a stacked structure 110' located on the substrate 100, the stacked structure 110' including a first dielectric layer 111 and a conductive plate structure 160 alternately stacked from bottom to top along a longitudinal direction (Z direction); a plurality of conductive pillar structures (not shown) extending longitudinally through the stacked structure 110', the conductive pillar structures including a protective layer 120 and an electrode pillar structure 130 from the outside to the inside, the protective layer 120 covering the side and bottom surfaces of the electrode pillar structure 130; wherein the thickness uniformity of the protective layer 120 is greater than or equal to 90%, and the bottom surface of the protective layer 120 is in contact with the conductive portions 105; and a dielectric layer 150 located between the conductive plate structure 160 and the protective layer 120, and between the conductive plate structure 160 and the first dielectric layer 112.

[0098] The substrate 100 provides the process basis for the formation process of the semiconductor structure of the present invention.

[0099] In some embodiments, the substrate 100 is a substrate having a semiconductor structure. Exemplarily, the substrate material includes silicon. Silicon is a commonly used material in semiconductor processes; it is compatible with many other materials and mainstream semiconductor manufacturing processes. In other embodiments, the substrate material may also include germanium, silicon germanide, silicon carbide, gallium arsenide, or indium gallium dihydrogen phosphate, etc.

[0100] The conductive part 105 is used for electrical connection with the conductive post structure.

[0101] In some embodiments, the conductive portion 105 can be a contact, or it can be the source or drain of a transistor. In other embodiments, the conductive portion can also be a pad or a conductive line, etc.

[0102] In some embodiments, there are multiple conductive parts 105, specifically, each conductive part 105 is provided in a one-to-one correspondence with a conductive post structure.

[0103] The stacked structure 110' is used to form multiple conductive plate structures 160 arranged longitudinally at intervals.

[0104] The conductive plate structure 160 is used as a conductive plate in a 3D memory.

[0105] In some embodiments, the conductive plate structure 160 includes an upper electrode covering a dielectric layer 150 and an upper conductor filling the space between longitudinally adjacent first dielectric layers 112 and covering the upper electrode.

[0106] The first dielectric layer 112 is used to achieve electrical isolation between adjacent conductive plate structures 160 in the longitudinal direction.

[0107] In some embodiments, the material of the first dielectric layer 112 includes silicon oxide.

[0108] In some embodiments, the thickness of the first dielectric layer 112 is 10 nm to 100 nm to ensure good electrical isolation and to ensure that the space occupied by the semiconductor structure is not too large, thereby improving the integration of the formed semiconductor structure.

[0109] In some embodiments, the conductive pillar structure includes a protective layer 120 and an electrode pillar structure 130 for use as conductive pillars of a 3D memory.

[0110] The protective layer 120 is used as an etch stop layer to protect the electrode pillar structure 130 during semiconductor manufacturing processes.

[0111] As an example, the material of the protective layer 120 is tantalum nitride (TaN).

[0112] In semiconductor manufacturing processes, a single thin film deposition-wet etching process or a multiple thin film deposition-wet etching alternating cycle process is used to form a protective material layer covering the top, sidewalls, and bottom of the stacked structure. This results in the thickness uniformity of the protective material layer located on the sidewalls of the via being greater than or equal to 90%. Subsequently, the protective material layer on the top of the stacked structure is removed, and the protective material layers located on the sidewalls and bottom of the via are retained as the protective layer 120. Correspondingly, the thickness uniformity of the protective layer 120 located on the side of the electrode pillar structure 130 is greater than or equal to 90%.

[0113] In semiconductor manufacturing processes, a single thin-film deposition-wet etch-back process or a multiple thin-film deposition-wet etch-back alternating cycle process is used to form a protective material layer covering the top, sidewalls, and bottom of the stacked structure. If the thickness uniformity of the protective material layer on the sidewalls of the vias is greater than or equal to 90%, then the subsequent etching process to remove the sacrificial layer in the stacked structure can avoid the etching solution from removing the thinner protective material layer on the sidewalls of the vias. This helps to ensure the etching stop effect of the protective material layer on the sidewalls of the vias, thereby ensuring the protection performance of the subsequently formed electrode pillar structure.

[0114] Meanwhile, the thickness uniformity of the protective material layer on the sidewall of the through hole is greater than or equal to 90%, which makes the protective material layer on the sidewall of the through hole and the protective material layer at the bottom of the through hole almost perpendicular or perpendicular. This provides a geometric cavity with a uniform cross section and almost perpendicular sidewall and bottom for the subsequent electrode post structure formation process, so that seamless and dense filling can be achieved when the electrode post structure is deposited on the protective material layer of the through hole.

[0115] In semiconductor manufacturing processes, a protective material layer covering the top, sidewalls, and bottom of a multilayer structure is formed using a single thin-film deposition-wet etching process or multiple alternating cycles of thin-film deposition-wet etching. In this process, the protective material layer is made of a conductive material, which allows it to be part of the conductive pillar structure. This eliminates the need to remove the protective material layer from the vias later, simplifying the process and not affecting the electrical connection performance between the conductive pillar structure and the conductive parts, nor the capacitor structure formed by the conductive pillar structure and the conductive plate structure.

[0116] Correspondingly, the bottom surface of the protective layer 120 contacts the conductive part 105 for electrical connection, thereby realizing the electrical connection between the conductive pillar structure and the conductive part 105.

[0117] In some embodiments, the electrode post structure 130 includes a liner layer 131 and a core 132.

[0118] The padding layer 131 serves as a diffusion barrier layer and a nucleation layer for the core material layer subsequently formed in the groove enclosed by the padding material layer during semiconductor manufacturing processes. As a barrier layer, the padding layer 131 effectively prevents adverse reactions between the core and the substrate material, such as diffusion or chemical reactions, thereby improving the reliability of the formed semiconductor structure. As a nucleation layer, the padding layer 131 provides attachment sites for atoms in the core material layer during semiconductor manufacturing processes, promoting uniform filling of the core material layer, avoiding voids or defects, and improving the quality of the formed core 132.

[0119] In some embodiments, the material of the liner 131 includes titanium nitride (TiN). Titanium nitride has excellent adhesion and diffusion-blocking properties, making it a good material for the liner 131. In other embodiments, the liner can be made of other suitable materials, which are not limited herein.

[0120] The core 132 is used as the core part of the conductive pillar in the 3D memory.

[0121] In some embodiments, the core 132 is made of tungsten. Depending on the specific requirements, the core can also be made of other conductive materials, such as copper or molybdenum, and there are no limitations on this.

[0122] The dielectric layer 150 serves as the storage capacitor material in the 3D memory to store and release charges according to the direction and magnitude of the external electric field. In some embodiments, the dielectric layer 150 is made of a ferroelectric material. Ferroelectric materials become polarized under the influence of an electric field and retain partial polarization (residual polarization) even after the external electric field is removed. This residual polarization has a potential difference, causing the capacitor electrodes on both sides of the dielectric layer 150—that is, the surfaces of the dielectric layer 150 closest to the conductive pillar structure and the conductive plate structure 160, respectively—to induce charges of opposite polarities. Different polarization directions induce different charges, thereby enabling the storage of logic "0" and logic "1". Ferroelectric materials possess spontaneous polarization characteristics and can form two different stable residual polarization states under the influence of an external electric field. By utilizing the aforementioned polarization characteristics of ferroelectric materials to store data "0" or "1", benefits such as high-speed read / write, high durability, and low power consumption can be achieved, making it suitable for various high-performance storage applications.

[0123] In semiconductor manufacturing processes, during the step of forming a through-hole through a multilayer structure using a conductive portion as an etch stop layer, the angle between the sidewall and bottom of the through-hole is a right angle or approximately a right angle. Correspondingly, after forming a dielectric layer covering part of the sidewall of the protective layer exposed in the trench and the surface of the first dielectric layer, the critical dimensions of the dielectric layer 150 in contact with the protective layer 120 are more uniform. This allows the capacitive electrodes on both sides of the dielectric layer 150 to release equal amounts of charge during data reading, thereby improving the accuracy of data reading and consequently enhancing the performance of the formed semiconductor structure.

[0124] The conductive plate structure 160 is used as a conductive plate for 3D memory.

[0125] In some embodiments, the conductive plate structure 160 includes an upper electrode covering the dielectric layer 150 and an upper conductor filling the trench and covering the upper electrode, the upper electrode and the upper conductor together with the dielectric layer, the lower electrode and the lower conductor forming a capacitor structure.

[0126] Specifically, the surfaces in contact with the conductive plate structure 160 and the conductive pillar structure are distributed as an upper electrode-storage capacitor material-lower electrode, i.e., a capacitor layer. The upper electrode is connected to the upper wire in the conductive plate structure 160, and the lower electrode is connected to the lower wire in the conductive pillar structure.

[0127] Accordingly, embodiments of the present invention also provide a memory, including a semiconductor structure as provided in the embodiments of the present invention and a plurality of transistors, wherein the number of transistors is consistent with the number of conductive pillar structures, and the conductive portion is the source or drain of the transistor. For a description of the semiconductor structure provided in the embodiments of the present invention, please refer to the foregoing section; it will not be elaborated upon here.

[0128] While the present invention has been disclosed above, it is not limited thereto. Any person skilled in the art can make various modifications and alterations without departing from the spirit and scope of the invention; therefore, the scope of protection of the present invention should be determined by the scope defined in the claims.

Claims

1. A method for forming a semiconductor structure, characterized in that, include: A substrate is provided, the substrate including a plurality of embedded, mutually isolated conductive portions; A stacked structure is formed on the substrate, the stacked structure comprising a first dielectric layer and a sacrificial layer that are alternately stacked longitudinally from bottom to top; Using the conductive portion as an etching stop layer, through-holes are formed that penetrate the stacked structure, the through-holes exposing the conductive portion, and the number of through-holes is the same as the number of conductive portions; A protective material layer is formed covering the top, sidewalls, and bottom of the stacked structure by employing a single thin film deposition-wet etching process or a multiple thin film deposition-wet etching alternating cycle process. The material of the protective material layer includes a conductive material, and the thickness uniformity of the protective material layer located on the sidewalls of the vias is greater than or equal to 90%. The remaining space of the through-hole is filled to form an electrode post material layer on the protective material layer; Remove the protective material layer and the electrode post material layer that are above the top of the stacked structure, and retain the protective material layer located on the sidewall and bottom of the through hole, as well as the electrode post material layer located in the through hole, as the protective layer and the electrode post structure, respectively. Using the protective layer as an etching stop layer, all the sacrificial layers in the stacked structure are removed to form a plurality of trenches spaced apart in the longitudinal direction, the trenches exposing part of the sidewalls of the protective layer and the surface of the first dielectric layer; A dielectric layer is formed covering a portion of the sidewalls of the protective layer exposed in the trench and the surface of the first dielectric layer; A conductive plate structure is formed that covers the dielectric layer and fills the trench.

2. The method for forming a semiconductor structure as described in claim 1, characterized in that, The step of forming a protective material layer covering the top, sidewalls, and bottom of the stacked structure using a single thin-film deposition-wet etching process or a multiple thin-film deposition-wet etching alternating cycle process includes: An initial protective material layer is formed by using a thin film deposition process to cover the top, sidewalls, and bottom of the stacked structure, wherein the thickness of the initial protective material layer located on the sidewalls of the through holes gradually decreases from top to bottom; When performing a wet etching process on the initial protective material layer, the contact time between the initial protective material layer and the etching solution used in the wet etching process decreases from top to bottom along the longitudinal direction, and the etching amount of the initial protective material layer gradually decreases. Repeat the thin film deposition process and the wet etching process once or multiple times until the initial protective material layer on the sidewall of the via reaches the target size along the surface direction parallel to the substrate and the thickness uniformity of the remaining initial protective material layer on the sidewall of the via is greater than or equal to 90%, thus forming the protective material layer.

3. The method for forming a semiconductor structure as described in claim 2, characterized in that, The thin film deposition process includes atomic layer deposition.

4. The method for forming a semiconductor structure as described in claim 2, characterized in that, The process parameters of the wet etching process include: the etching solution is a phosphoric acid solution with a volume percentage concentration of 70% to 90%, and the process temperature is 150°C to 170°C.

5. The method for forming a semiconductor structure as described in claim 1, characterized in that, The material of the protective layer includes tantalum nitride.

6. The method for forming a semiconductor structure as described in claim 1, characterized in that, After the step of removing the protective material layer and the electrode pillar material layer above the top of the stacked structure, retaining the protective material layer located on the sidewall and bottom of the via, and the electrode pillar material layer located within the via, as the protective layer and the electrode pillar structure respectively, and before the step of removing the sacrificial layer in the stacked structure using the protective layer as an etching stop layer to form a plurality of trenches spaced longitudinally, wherein the trenches expose part of the sidewall of the protective layer and the surface of the first dielectric layer, the method further includes: A second dielectric layer is formed on the stacked structure, and the second dielectric layer also covers the protective layer and the top surface of the electrode post structure.

7. The method for forming a semiconductor structure as described in claim 1, characterized in that, The step of filling the remaining space of the through-hole to form an electrode post material layer on the protective material layer includes: A liner material layer is formed by conformally covering the surface of the protective material layer; A core material layer is formed that covers the padding material layer and fills the groove formed by the enclosure of the padding material layer; The electrode post material layer includes the padding material layer and the core material layer; in the step of removing the protective material layer and the electrode post material layer above the top of the stacked structure, the padding material layer and the core material layer above the top of the stacked structure are also removed.

8. The method for forming a semiconductor structure as described in claim 7, characterized in that, The material of the liner layer includes titanium nitride, and the material of the core material layer includes tungsten.

9. A semiconductor structure, characterized in that, include: A substrate, the substrate comprising a plurality of embedded, mutually isolated conductive portions; A stacked structure is located on the substrate, the stacked structure comprising a first dielectric layer and a conductive plate structure that are alternately stacked longitudinally from bottom to top; Multiple conductive pillar structures extend longitudinally through the stacked structure. Each conductive pillar structure includes a protective layer and an electrode pillar structure from the outside to the inside. The protective layer covers the sides and bottom of the electrode pillar structure. The thickness uniformity of the protective layer is greater than or equal to 90%, and the bottom surface of the protective layer is in contact with the conductive part. A dielectric layer is located between the conductive plate structure and the protective layer, and between the conductive plate structure and the first dielectric layer.

10. A memory, characterized in that, It includes the semiconductor structure as described in claim 9 and a plurality of transistors, wherein the number of transistors is the same as the number of conductive pillars, and the conductive portion is the source or drain of the transistor.