A method for fabricating TBC solar cells using photoresist patterning
By replacing laser equipment with photoresist patterning technology, the problems of high equipment cost and difficult waste liquid treatment in TBC battery manufacturing have been solved, realizing efficient and environmentally friendly battery production and improving battery performance and environmental performance.
Patent Information
- Application Number
- CN202611500941.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-24
- Publication Date
- 2026-11-17
AI Technical Summary
Existing laser patterning methods in TBC battery fabrication suffer from high equipment investment, high operation and maintenance costs, difficulties in treating acid etching waste liquid, and edge residue problems, leading to decreased battery efficiency and significant environmental impact.
Photoresist patterning technology is used, replacing laser equipment with photoresist printing and ultraviolet exposure equipment. Combined with photoresist masks, patterns are precisely defined, and alkaline and acidic solutions are used for etching to form clear P-region and N-region structures, reducing acid consumption and waste liquid generation.
It reduced equipment investment and operation and maintenance costs, reduced waste liquid discharge, improved battery efficiency and consistency, reduced leakage risk, and optimized the environmental load of production.
Abstract
Description
Technical Field
[0001] This invention relates to the field of photovoltaic module technology, specifically a method for fabricating TBC solar cells using photoresist patterning. Background Technology
[0002] TBC (TOPCon Back-Contact) cells combine the tunneling oxide passivation contact technology of TOPCon with the advantages of IBC's interdigitated back electrode structure, which can eliminate the light loss of the front grid line and improve the carrier collection efficiency.
[0003] In the fabrication of TBC cells, back-side patterning (selectively forming P-type and N-type regions on the back of the silicon wafer) is the core and challenging aspect of the technology. The current mainstream approach involves selectively modifying the deposited doped polycrystalline silicon layer twice using lasers, followed by alkaline / acid etching to define the pattern. The typical process flow is: polishing → primary deposition and doping (e.g., P-type poly deposition) → primary laser treatment → alkaline treatment → secondary deposition and doping (e.g., N-type poly deposition) → secondary laser treatment → acid treatment → alkaline treatment and texturing… and other core processes. However, the laser patterning approach has the following drawbacks in actual mass production: 1. The investment cost of laser equipment is high. Furthermore, core components of laser equipment, such as galvanometers and light sources, have limited lifespans and require periodic replacement, increasing maintenance costs. In addition, acid etching is an indispensable process in laser solutions, and acid treatment increases chemical consumption and wastewater treatment burdens.
[0004] 2. Laser energy is prone to scattering or uneven absorption at material interfaces, resulting in micron-sized residual passivation layers at the edges of the open film, creating a "half-open" state. This is especially true in high-concentration boron-doped P-poly regions, where laser film removal is further degraded, leading to more pronounced residue problems. These residues hinder subsequent metallization processes, creating leakage channels that directly reduce the battery's pFF, increase leakage current, and decrease its photoelectric conversion efficiency.
[0005] 3. Existing laser solutions are highly dependent on acid etching. The waste liquid generated by acid etching (such as a mixed waste liquid containing high concentrations of hydrofluoric acid and nitric acid) is hazardous waste, which has high treatment costs and a great environmental impact.
[0006] Therefore, how to overcome the above-mentioned defects has become an urgent problem to be solved by those skilled in the art. Summary of the Invention
[0007] To address the technical problems in the background art, this invention discloses a method for fabricating TBC solar cells using photoresist patterning.
[0008] This invention provides a method for fabricating TBC solar cells using photoresist patterning, comprising the following steps: S1. Polish the silicon wafer substrate on one or both sides to remove the cutting damage layer; S2. A tunneling oxide layer and a boron-doped polysilicon layer are deposited on the back side of the silicon wafer to form a P-type doped region; S3. On the back side of the silicon wafer after poly deposition in the P-region, perform operations S31-S34 sequentially: S31. Cover the back of the silicon wafer with a layer of photoresist; S32. Use a mask to selectively expose the photoresist, causing cross-linking or de-chaining reactions in specific areas of the photoresist. S33. Dissolve the photoresist in the exposed or unexposed area with a developer to expose the surface of the poly layer in the P-area that needs to be etched below. S34. Clean and remove developing residue to form a clear photoresist mask pattern; S4. Use an alkaline solution to etch the silicon wafer to remove the P-region poly layer that is not protected by photoresist, exposing the silicon substrate surface. S5. Remove the residual photoresist to expose the remaining P-region poly layer and the silicon substrate with etched openings; S6. A tunneling oxide layer and a phosphorus-doped polysilicon layer are deposited on the back side of the silicon wafer. This layer covers both the retained P-region poly layer and the silicon substrate in the opening region. S7. On the back side of the silicon wafer after N-region poly deposition, perform operations S71-S74 sequentially: S71. Cover the back of the silicon wafer with a layer of photoresist; S72. Use a mask to selectively expose the photoresist, causing cross-linking or de-chaining reactions in specific areas of the photoresist. S73. Dissolve the photoresist in the exposed or unexposed areas with a developer to expose the surface of the N-region poly layer that needs to be etched below. S74. Clean and remove developing residue to form a clear photoresist mask pattern; S8. Use an acidic solution to etch away the N-region poly layer that is not protected by photoresist, forming an interdigitated separation structure between the P-region and the N-region; S9. Remove residual photoresist; S10. A pyramidal textured surface structure is formed on the light-receiving surface of the silicon wafer by anisotropic etching with alkaline solution. S11. Deposit aluminum oxide layers on both sides of a silicon wafer to achieve efficient chemical passivation and field-effect passivation; S12. On top of the aluminum oxide layer, a silicon nitride layer is deposited on both sides as an anti-reflection layer and a bulk passivation layer. S13. Screen print metal paste on the alternating patterned areas of P and N regions on the back of the battery, and co-sinter to form metal electrodes, which form ohmic contacts with the P and N regions respectively. S14. Under light and heating conditions, perform light injection treatment to passivate body defects and interface defects.
[0009] Further, in step S2, a tunneling oxide layer and a boron-doped polycrystalline silicon layer are deposited on the back side of the silicon wafer using PECVD or LPCVD.
[0010] Furthermore, in steps S31 and S71, a layer of photoresist is applied to the back of the silicon wafer by screen printing or spin coating.
[0011] Furthermore, in steps S32 and S72, if the photoresist is a negative photoresist, a cross-linking reaction occurs; if the photoresist is a positive photoresist, a chain-breaking reaction occurs.
[0012] Furthermore, if the photoresist is negative, the unexposed areas are dissolved by the developer; if the photoresist is positive, the exposed areas are dissolved by the developer.
[0013] Further, in steps S34 and S74, deionized water is used to wash away developing residues.
[0014] Furthermore, in steps S5 and S9, residual photoresist is removed using a photoresist stripping solution or plasma cleaning.
[0015] Further, in step S11, an aluminum oxide layer is deposited on both sides of the silicon wafer by atomic layer deposition.
[0016] Further, in step S12, a silicon nitride layer is deposited on both sides by PECVD.
[0017] The beneficial effects of this invention are: 1. This invention replaces expensive laser patterning equipment with photoresist printing and ultraviolet exposure equipment, reducing overall equipment investment by more than 40% compared to laser solutions. Simultaneously, the core components of the photoresist patterning equipment have a longer lifespan and lower maintenance costs, and it eliminates the need for high-power laser equipment and complex optical path systems, thus reducing factory cleanliness requirements and equipment footprint. This equipment architecture is fully compatible with existing TOPCon production line equipment, facilitating upgrades to TBC production lines with limited modification costs.
[0018] 2. In this invention, the acid etching step is performed only on specific areas without mask protection after the second photoresist patterning. The amount of acid used is reduced by more than 60% compared to the global acid washing method of the laser solution. The developing waste liquid and stripping waste liquid generated by the photoresist patterning process have mature recycling and treatment technologies. The waste acid treatment cost can be reduced by more than 40% through the waste liquid recycling system, reducing hazardous waste emissions by tens of thousands of tons per year. The overall environmental impact is significantly lower than that of the laser solution.
[0019] 3. Photolithography precisely defines the processing area through steps of coating, exposure, and development, and achieves patterning by combining it with etching, thus solving the edge residue problem caused by uneven energy scattering or absorption in laser processes. This significantly reduces battery leakage, improves open-circuit voltage and fill factor, creating room for efficiency improvement; at the same time, it allows for increasing the boron doping concentration of the P-poly layer to reduce contact resistance without worrying about residue and cleaning problems caused by high doping.
[0020] 4. This invention uses a photomask to physically define the pattern. The pattern accuracy is determined by the photomask manufacturing accuracy and the alignment accuracy of the exposure machine, and is not affected by power attenuation caused by long-term equipment aging, resulting in better mass production consistency. The coating and stripping of photoresist are both mature and stable chemical processes, and the yield of each step can be consistently maintained at a high level.
[0021] 5. Consumables such as photoresist and developer have a mature supply chain in the semiconductor industry and a high degree of localization, with procurement costs decreasing year by year; the supporting waste liquid recycling technology can further reduce the cost of waste acid treatment by more than 40%, further optimizing long-term operating costs. Detailed Implementation
[0022] This invention provides a method for fabricating TBC solar cells using photoresist patterning, comprising the following steps: S1. Polish the silicon wafer substrate on one or both sides to remove the cutting damage layer and obtain a flat surface. S2. A tunneling oxide layer and a boron-doped polysilicon layer are deposited on the back side of the silicon wafer using PECVD or LPCVD to form a P-type doped region. S3. On the back side of the silicon wafer after poly deposition in the P-region, perform operations S31-S34 sequentially: S31. Apply a layer of photoresist to the back of the silicon wafer by screen printing or spin coating. S32. Selective exposure of photoresist using a mask to cause cross-linking or de-linking reactions in specific areas of the photoresist; wherein the exposure method is ultraviolet light irradiation. If the photoresist is negative, a cross-linking reaction occurs, and the unexposed areas are dissolved by the developer; if the photoresist is positive, a chain-breaking reaction occurs, and the exposed areas are dissolved by the developer. S33. Dissolve the photoresist in the exposed or unexposed area with a developer to expose the surface of the poly layer in the P-area that needs to be etched below. S34. Use deionized water to clean away the developer residue and form a clear photoresist mask pattern; S4. Use an alkaline solution to etch the silicon wafer. Utilize the protective effect of the photoresist mask to selectively remove the P-region poly layer that is not protected by the photoresist, exposing the silicon substrate surface and forming the opening region of the N-region. S5. Use photoresist stripping solution or plasma cleaning to remove residual photoresist and expose the remaining P-region poly layer and the silicon substrate with etched openings. S6. A tunneling oxide layer and a phosphorus-doped polysilicon layer are deposited on the back side of the silicon wafer. This layer covers both the retained P-region poly layer and the silicon substrate in the opening region. S7. On the back side of the silicon wafer after N-region poly deposition, form a mask to protect the areas where N-region poly needs to be retained, and then perform operations S71-S74 sequentially: S71. A layer of photoresist is applied to the back of the silicon wafer by screen printing or spin coating. S72. Selective exposure of photoresist using a photomask to cause cross-linking or de-linking reactions in specific areas of the photoresist; wherein the exposure method is ultraviolet light irradiation. If the photoresist is negative, a cross-linking reaction occurs, and the unexposed areas are dissolved by the developer; if the photoresist is positive, a chain-breaking reaction occurs, and the exposed areas are dissolved by the developer. S73. Dissolve the photoresist in the exposed or unexposed areas with a developer to expose the surface of the N-region poly layer that needs to be etched below. S74. Use deionized water to clean away the developer residue and form a clear photoresist mask pattern; S8. Use an acidic solution to etch and remove the N-region poly layer that is not protected by photoresist, forming an interdigitated separation structure between the P-region and the N-region; wherein the N-region poly layer that is not protected by photoresist is the N-region poly layer above the opening area of the P-region; since the acid etching in this step only acts on the local area that is not protected by the mask, the amount of acid used can be significantly reduced compared with the conventional global acid washing scheme. S9. Use photoresist stripping solution or plasma cleaning to remove residual photoresist; S10. A pyramidal textured surface structure is formed on the light-receiving surface of the silicon wafer by anisotropic etching with alkaline solution. S11. Alumina layers are deposited on both sides of a silicon wafer by atomic layer deposition (ALD) to achieve efficient chemical passivation and field effect passivation. S12. On the aluminum oxide layer, a silicon nitride layer is deposited on both sides by PECVD as an anti-reflection layer and a bulk passivation layer. S13. Screen print metal paste on the alternating patterned areas of P and N regions on the back of the battery, and co-sinter to form metal electrodes, which form ohmic contacts with the P and N regions respectively; in this embodiment, the metal paste is silver paste or silver-aluminum paste. S14. Under light and heating conditions, perform light injection treatment to passivate body defects and interface defects.
[0023] Compared to existing technologies, the advantages of this embodiment are: 1. This invention uses photoresist printing and ultraviolet exposure equipment to replace expensive laser patterning equipment, reducing overall equipment investment by more than 40% compared to laser solutions. Simultaneously, the core components of the photoresist patterning equipment have a longer lifespan and lower maintenance costs, and there is no need to configure high-power laser equipment and complex optical path systems, reducing factory cleanliness requirements and equipment footprint. This equipment architecture is fully compatible with existing TOPCon production line equipment, facilitating the upgrade of the production line to a TBC production line with limited modification costs. 2. The acid etching step in this invention only performs targeted etching on specific areas without mask protection after the second photoresist patterning, reducing acid consumption by approximately 60% compared to the global acid washing of laser solutions. The developing and stripping wastewater generated by the photoresist patterning process has mature recycling and treatment technologies, which can reduce waste acid treatment costs by more than 40% through a wastewater recycling system, reducing hazardous waste emissions by tens of thousands of tons annually, resulting in a significantly lower overall environmental impact than laser solutions. 3. Photolithography precisely defines the processing area through steps of resist coating, exposure, and development, combined with etching to achieve patterning, solving the edge residue problem caused by uneven energy scattering or absorption in laser processes. This significantly reduces battery leakage, improves open-circuit voltage and fill factor, creating room for efficiency improvement; it also allows for increasing the boron doping concentration of the P-poly layer to reduce contact resistance without worrying about residue and cleaning difficulties caused by high doping. 4. This invention uses a physical mask to define the pattern. The pattern accuracy is determined by the mask manufacturing accuracy and the alignment accuracy of the exposure machine, and is not affected by power decay caused by long-term equipment aging, resulting in better mass production consistency. The coating and stripping of photoresist are mature and stable chemical processes, and the yield of a single step can be consistently maintained at a high level. 5. Consumables such as photoresist and developer have a mature supply chain in the semiconductor industry and a high degree of domestic production, with procurement costs decreasing year by year; the supporting waste liquid recycling technology can further reduce waste acid treatment costs by more than 40%, further optimizing long-term operating costs.
[0024] Based on the above-described preferred embodiments of the present invention, and through the foregoing description, those skilled in the art can make various changes and modifications without departing from the inventive concept. The technical scope of this invention is not limited to the contents of the specification, but must be determined according to the scope of the claims.
Claims
1. A method for fabricating a TBC solar cell by patterning a photoresist, characterized in that, Includes the following steps: S1. Polish the silicon wafer substrate on one or both sides to remove the cutting damage layer; S2. A tunneling oxide layer and a boron-doped polysilicon layer are deposited on the back side of the silicon wafer to form a P-type doped region; S3. On the back side of the silicon wafer after poly deposition in the P-region, perform operations S31-S34 sequentially: S31. Cover the back of the silicon wafer with a layer of photoresist; S32. Use a mask to selectively expose the photoresist, causing cross-linking or de-chaining reactions in specific areas of the photoresist. S33. Dissolve the photoresist in the exposed or unexposed area with a developer to expose the surface of the poly layer in the P-area that needs to be etched below. S34. Clean and remove developing residue to form a clear photoresist mask pattern; S4. Use an alkaline solution to etch the silicon wafer to remove the P-region poly layer that is not protected by photoresist, exposing the silicon substrate surface. S5. Remove the residual photoresist to expose the remaining P-region poly layer and the silicon substrate with etched openings; S6. A tunneling oxide layer and a phosphorus-doped polysilicon layer are deposited on the back side of the silicon wafer. This layer covers both the retained P-region poly layer and the silicon substrate in the opening region. S7. On the back side of the silicon wafer after N-region poly deposition, perform operations S71-S74 sequentially: S71. Cover the back of the silicon wafer with a layer of photoresist; S72. Use a mask to selectively expose the photoresist, causing cross-linking or de-chaining reactions in specific areas of the photoresist. S73. Dissolve the photoresist in the exposed or unexposed areas with a developer to expose the surface of the N-region poly layer that needs to be etched below. S74. Clean and remove developing residue to form a clear photoresist mask pattern; S8. Use an acidic solution to etch away the N-region poly layer that is not protected by photoresist, forming an interdigitated separation structure between the P-region and the N-region; S9. Remove residual photoresist; S10. A pyramidal textured surface structure is formed on the light-receiving surface of the silicon wafer by anisotropic etching with alkaline solution. S11. Deposit aluminum oxide layers on both sides of a silicon wafer to achieve efficient chemical passivation and field-effect passivation; S12. On top of the aluminum oxide layer, a silicon nitride layer is deposited on both sides as an anti-reflection layer and a bulk passivation layer. S13. Screen print metal paste on the alternating patterned areas of P and N regions on the back of the battery, and co-sinter to form metal electrodes, which form ohmic contacts with the P and N regions respectively. S14. Under light and heating conditions, perform light injection treatment to passivate body defects and interface defects.
2. The method for fabricating a TBC solar cell using photoresist patterning according to claim 1, characterized in that: In step S2, a tunneling oxide layer and a boron-doped polycrystalline silicon layer are deposited on the back side of the silicon wafer using PECVD or LPCVD.
3. The method for fabricating a TBC solar cell using photoresist patterning according to claim 1, characterized in that: In steps S31 and S71, a layer of photoresist is applied to the back of the silicon wafer by screen printing or spin coating.
4. The method for fabricating a TBC solar cell using photoresist patterning according to claim 1, characterized in that: In steps S32 and S72, if the photoresist is a negative photoresist, a cross-linking reaction occurs; If the photoresist is a positive photoresist, a chain reaction will occur.
5. The method for fabricating a TBC solar cell using photoresist patterning according to claim 4, characterized in that: If the photoresist is a negative photoresist, the unexposed areas will be dissolved by the developer; If the photoresist is a positive photoresist, the exposed area will be dissolved by the developer.
6. The method for fabricating a TBC solar cell using photoresist patterning according to claim 1, characterized in that: In steps S34 and S74, deionized water is used to wash away developing residues.
7. The method for fabricating a TBC solar cell using photoresist patterning according to claim 1, characterized in that: In steps S5 and S9, residual photoresist is removed using a photoresist stripping solution or plasma cleaning.
8. The method for fabricating a TBC solar cell using photoresist patterning according to claim 1, characterized in that: In step S11, an aluminum oxide layer is deposited on both sides of the silicon wafer by atomic layer deposition.