Flip LED Chip and Its Fabrication Method

By employing an aluminum nitride and boron nitride stacked structure in the sidewall passivation layer of the flip-chip LED, the problem of insufficient sidewall protection under high temperature and high humidity environments is solved, achieving higher reliability and stability.

CN123124530APending Publication Date: 2026-11-17JIANGXI ZHAO CHI SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611164622.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-03
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing flip-chip LEDs have insufficient sidewall protection in high-temperature and high-humidity environments, leading to the intrusion of moisture and impurity ions, which corrode the metal electrodes and affect the chip's reliability and lifespan.

Method used

A sidewall passivation layer with an aluminum nitride and boron nitride stacked structure is used to cover the isolation groove and the sidewall of the N-type GaN via, and a connection hole is formed on the N-type GaN conductive step. Combined with the multilayer metal structure, the reliability of electrical connection and environmental protection are improved.

Benefits of technology

It effectively blocks water, oxygen, and ion penetration, improving the reliability and stability of the chip in high temperature and high humidity environments and extending its service life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124530A_ABST
    Figure CN123124530A_ABST
Patent Text Reader

Abstract

This invention discloses a flip-chip light-emitting diode and its fabrication method, relating to the field of optoelectronic manufacturing technology. It includes a substrate and an epitaxial structure. The epitaxial structure comprises an N-type GaN layer, an active light-emitting layer, and a P-type GaN layer sequentially stacked on the substrate. The epitaxial structure includes an N-type GaN conductive step exposing a portion of the N-type GaN layer and an isolation trench extending downward from the N-type GaN conductive step. The sidewall transitioning from the N-type GaN conductive step to the P-type GaN layer is an N-type GaN via sidewall. A sidewall passivation layer is disposed on the isolation trench and the N-type GaN via sidewall. Using this invention, the sidewall passivation layer provides the advantage of improving the chip's lifespan in high-temperature and high-humidity environments.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of optoelectronic manufacturing technology, and in particular to a flip-chip light-emitting diode and its fabrication method. Background Technology

[0002] Light-emitting diodes (LEDs), as a highly efficient and environmentally friendly solid-state lighting source, have been widely used in displays, backlighting, and general lighting. Flip-chip structures, due to their advantages such as avoiding electrode light blocking, improving light extraction efficiency, and enhancing heat dissipation, have become the mainstream technology for high-performance LED chips. In flip-chip structures, etching processes are required to form mesas or vias for N-type electrode contacts, which exposes the sidewalls of the epitaxial layer.

[0003] These exposed sidewalls, especially the N-type GaN conductive steps and their sidewalls (N-type GaN via sidewalls) and the isolation trench sidewalls used for electrical isolation, are weak points in the chip structure. Under harsh operating environments such as high temperature and high humidity, moisture and impurity ions can easily penetrate the chip interior along these unprotected sidewalls, corroding metal electrodes or causing leakage current, severely compromising the chip's long-term reliability and lifespan. Traditional passivation protective layers (such as SiO2 or SiNx) still have insufficient barrier performance and long-term stability when facing extreme environmental challenges, making it difficult to meet the increasingly stringent reliability requirements.

[0004] Therefore, there is an urgent need in the existing technology for a new flip-chip structure and its fabrication method to solve the problem of insufficient sidewall protection, thereby significantly improving the reliability and stability of the chip in high temperature and high humidity environments. Summary of the Invention

[0005] The problem to be solved by the present invention is to provide a flip-chip light-emitting diode and its preparation method, which can improve the reliability of the flip-chip light-emitting diode in high temperature and high humidity environments.

[0006] To address the aforementioned technical problems, this invention provides a flip-chip light-emitting diode (LED) chip, comprising: a substrate and an epitaxial structure, wherein the epitaxial structure comprises an N-type GaN layer, an active light-emitting layer, and a P-type GaN layer sequentially stacked on the substrate; the epitaxial structure includes an N-type GaN conductive step exposing a portion of the N-type GaN layer and an isolation trench extending downward from the N-type GaN conductive step, wherein the sidewall of the N-type GaN conductive step transitioning to the P-type GaN layer is an N-type GaN via sidewall; A sidewall passivation layer is provided on the isolation groove and the sidewall of the N-type GaN via. The sidewall passivation layer includes an aluminum nitride layer and a boron nitride layer disposed on the aluminum nitride layer. An N-type connection hole is formed above the N-type GaN conductive step by the sidewall passivation layer. A metal reflective layer is disposed on the P-type GaN layer; A first insulating layer is disposed on the P-type GaN layer and the sidewall passivation layer, wherein the first insulating layer disposed on the P-type GaN layer includes a P-type connection hole; a P-type connection metal layer is disposed on the first insulating layer and the P-type connection hole, and an N-type connection metal layer is disposed on the first insulating layer and the N-type connection hole, the P-type connection metal layer and the N-type connection metal layer are indirectly connected; a P-type pad layer is disposed on the P-type connection metal layer, an N-type pad layer is disposed on the N-type connection metal layer, and a second insulating layer is disposed in the area outside the P-type pad layer and the N-type pad layer.

[0007] As an improvement to the above scheme, the thickness of the aluminum nitride layer is 30A-50A, and the total thickness of the boron nitride layer is 900A-1200A; The boron nitride layer includes a first boron nitride layer and a second boron nitride layer, wherein the thickness of the first boron nitride layer is 100 Å-200 Å and the thickness of the second boron nitride layer is 800 Å-1000 Å.

[0008] As an improvement to the above scheme, the deposition pressure of the aluminum nitride layer is 1 Torr-5 Torr, and the deposition temperature is 200℃-250℃; The deposition pressure of the boron nitride layer is 1 Torr-5 Torr, and the deposition temperature is 200℃-250℃; The boron source for the first boron nitride layer is introduced at time T11, and the ammonia gas is introduced at time T12. The boron source is introduced into the second boron nitride layer at time T21, and the ammonia gas is introduced at time T22, satisfying the conditions that T21 > T11 and T22 > T12.

[0009] As an improvement to the above solution, the sidewall passivation layer covers the surface and sidewall of the isolation trench, and covers the sidewall of the N-type GaN via, and partially covers the P-type GaN layer and the N-type GaN layer. The distance between the edge of the sidewall passivation layer and the edge of the N-type GaN via sidewall is L, where L is 2μm-5μm.

[0010] As an improvement to the above scheme, the metal reflective layer includes an ITO layer, an Ag layer, a first Ti layer, a first Ni layer, a first Pt layer, a second Ti layer, a second Ni layer, a second Pt layer, and a third Ti layer stacked sequentially; and / or the thickness of the ITO layer is 50 Å-80 Å; and / or the thickness of the Ag layer is 1200 Å-2000 Å; and / or the thickness of the first Ti layer is 1000 Å-2000 Å; and / or the thickness of the first Ni layer is 1000 Å-2000 Å; and / or the thickness of the first Pt layer is 1000 Å-2000 Å; and / or the thickness of the second Ti layer is 1000 Å-2000 Å; and / or the thickness of the second Ni layer is 1000 Å-2000 Å; and / or the thickness of the second Pt layer is 2000 Å-3000 Å; and / or the thickness of the third Ti layer is 30 Å-50 Å.

[0011] As an improvement to the above scheme, both the P-type connecting metal layer and the N-type connecting metal layer are Cr / Al / Ti / Pt / Ti / Pt / Ti / Au / Pt / Ti stacked structures.

[0012] Both the P-type and N-type pad layers are Al / Ti / Pt / Ni / Au stacked structures.

[0013] Accordingly, the present invention also provides a method for fabricating a flip-chip light-emitting diode, comprising: forming an epitaxial layer on a substrate, the epitaxial layer comprising an N-type GaN layer, an active light-emitting layer and a P-type GaN layer sequentially stacked on the substrate; etching to form an N-type GaN conductive step exposing a portion of the N-type GaN layer, and an isolation trench extending downward from the N-type GaN conductive step, wherein the sidewall of the N-type GaN conductive step transitioning to the P-type GaN layer is an N-type GaN via sidewall; A sidewall passivation layer is provided on the isolation groove and the sidewall of the N-type GaN via. The sidewall passivation layer includes an aluminum nitride layer and a boron nitride layer disposed on the aluminum nitride layer. An N-type connection hole is formed above the N-type GaN conductive step by the sidewall passivation layer. A metallic reflective layer is formed on the P-type GaN layer; A first insulating layer is formed on the P-type GaN layer and the sidewall passivation layer, wherein the first insulating layer on the P-type GaN layer includes a P-type interconnect; a P-type interconnect metal layer is formed on the first insulating layer and the P-type interconnect, and an N-type interconnect metal layer is formed on the first insulating layer and the N-type interconnect, wherein the P-type interconnect metal layer and the N-type interconnect metal layer are indirectly connected; a P-type pad layer is formed on the P-type interconnect metal layer, and an N-type pad layer is formed on the N-type interconnect metal layer; a second insulating layer is disposed in the area outside the P-type pad layer and the N-type pad layer.

[0014] As an improvement to the above scheme, the formation process of the sidewall passivation layer includes: depositing an aluminum nitride layer using the ALD process; depositing an aluminum nitride layer on the isolation trench and the sidewall of the N-type GaN via, wherein the thickness of the aluminum nitride layer is 30 Å-50 Å, the deposition pressure is 1 Torr-5 Torr, and the deposition temperature is 200℃-250℃. A first boron nitride layer is deposited on an aluminum nitride layer, the thickness of the first boron nitride layer being 100 Å-200 Å, the deposition pressure being 1 Torr-5 Torr, and the deposition temperature being 200℃-250℃; A second boron nitride layer is deposited on the first boron nitride layer. The thickness of the second boron nitride layer is 800 Å-1000 Å, the deposition pressure is 1 Torr-5 Torr, and the deposition temperature is 200℃-250℃.

[0015] As an improvement to the above scheme, the deposition of a first boron nitride layer on the aluminum nitride layer includes: Trimethylboron gas is introduced for 0.8s-1s to allow the trimethylboron gas to be adsorbed on the surface of the aluminum nitride layer; Purge with Ar inert gas for 1.5s-2s; Ammonia gas is introduced for 1.2s-1.5s to form the first boron nitride layer; Ar inert gas was introduced for purging, and the purging time was 2.0s-2.5s, to complete the single deposition of the first boron nitride layer; Repeat the above deposition steps until the thickness of the first boron nitride layer is 100 Å-200 Å.

[0016] As an improvement to the above scheme, the deposition of a second boron nitride layer on the first boron nitride layer includes: Trimethylboron gas is introduced for 1.2s-1.4s to allow the trimethylboron gas to be adsorbed on the surface of the first boron nitride layer; Purge with Ar inert gas for 1.5s-2s; Ammonia gas is introduced for 1.8s-2s to generate a second boron nitride layer. Ar inert gas was introduced for purging, and the purging time was 2.0s-2.5s, to complete the single deposition of the second boron nitride layer; Repeat the above deposition steps until the thickness of the second boron nitride layer is 800 Å-1000 Å.

[0017] Implementing this invention has the following beneficial effects: This invention achieves precise regional protection by setting a sidewall passivation layer on the surface and sidewalls of the isolation tank, as well as on the sidewalls of the N-type GaN through holes. At the same time, the sidewall passivation layer forms an N-type connection hole above the N-type GaN conductive step. This structural design can effectively cover and seal the sidewall area most susceptible to environmental corrosion, blocking the longitudinal and lateral penetration of water, oxygen and ions.

[0018] The sidewall passivation layer is a stacked structure of aluminum nitride and boron nitride layers. The aluminum nitride layer, as a transition layer, can form a good interface with the GaN material, reducing interface states and stress. The boron nitride layer, as the main passivation layer, has excellent chemical inertness, high density, and excellent water and oxygen barrier properties. This allows the sidewall passivation layer to not only adhere tightly to the isolation trench and the sidewall of the N-type GaN via, but also to resist external environmental corrosion in a long-term stable manner, greatly extending the lifespan of the chip and thus improving the high-temperature and high-humidity reliability of the flip-chip. Attached Figure Description

[0019] Figure 1 This is a schematic diagram of the structure of the flip-chip light-emitting diode of the present invention; Figure 2 This is a schematic diagram of the first structure of the flip-chip light-emitting diode after step S200 is completed in this invention; Figure 3 This is a schematic diagram of the second structure of the flip-chip light-emitting diode after step S300 is completed in this invention; Figure 4 This is a schematic diagram of the third structure of the flip-chip light-emitting diode after the completion of step S400 in this invention; Figure 5 This is a schematic diagram of the fourth structure of the flip-chip light-emitting diode after the completion of step S500 in this invention; Figure 6 This is a fifth structural schematic diagram of the flip-chip light-emitting diode after step S600 of the present invention is completed; Figure 7 This is a sixth structural schematic diagram of the flip-chip light-emitting diode after the completion of step S700 in this invention; Figure 8 This is a flowchart of the method for fabricating the flip-chip light-emitting diode of the present invention. Detailed Implementation

[0020] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings. It is hereby declared that the directional terms such as up, down, left, right, front, back, inside, and outside used in this text are based solely on the accompanying drawings and are not intended to specifically limit the invention.

[0021] like Figures 1-7As shown, it displays a schematic diagram of an embodiment of a flip-chip light-emitting diode according to the present invention, which includes: Substrate 10 and epitaxial structure, wherein the epitaxial structure includes an N-type GaN layer 111, an active light-emitting layer 112 and a P-type GaN layer 113 sequentially stacked on substrate 10; like Figure 1 and 2 As shown, the epitaxial structure includes an N-type GaN conductive step 116 forming an exposed portion of the N-type GaN layer 111 and an isolation groove 115 extending downward from the N-type GaN conductive step 116. The sidewall of the N-type GaN conductive step 116 transitioning to the P-type GaN layer 113 is an N-type GaN via sidewall 114. like Figure 1 and Figure 3 As shown, a sidewall passivation layer 12 is provided on the isolation groove 115 and the sidewall 114 of the N-type GaN through hole, and an N-type connection hole 18 is formed above the N-type GaN conductive step 116 in the sidewall passivation layer 12. like Figure 1 and Figure 4 As shown, a metal reflective layer 13 is disposed on the P-type GaN layer 113; like Figure 1 and Figure 5 As shown, a first insulating layer 14 is provided on the P-type GaN layer 113 and the sidewall passivation layer 12, wherein the first insulating layer 14 provided on the P-type GaN layer 113 includes a P-type connection hole 19; like Figure 1 and Figure 6 As shown, a P-type connecting metal layer 151 is provided on the first insulating layer 14 and the P-type connecting hole 19, and an N-type connecting metal layer 152 is provided on the first insulating layer 14 and the N-type connecting hole 18. like Figure 1 and Figure 7 As shown, the P-type connection metal layer 151 and the N-type connection metal layer 152 are indirectly connected; a P-type pad layer 171 is provided on the P-type connection metal layer 151, and an N-type pad layer 172 is provided on the N-type connection metal layer 152. A second insulating layer (not shown in the figure) is provided in the area outside the P-type pad layer 171 and the N-type pad layer 172.

[0022] In some embodiments, the sidewall passivation layer 12 is a stacked structure, including an aluminum nitride layer that is in direct contact with the surfaces of the isolation groove 115, the N-type GAN via sidewall 114, etc., and a boron nitride layer deposited on the aluminum nitride layer.

[0023] The aluminum nitride layer serves as a transition layer, forming a good interface with the GaN material and reducing interface states and stress. Its thickness can be 30 Å-50 Å, exemplarily 30 Å, 40 Å, 45 Å, or 50 Å, but is not limited thereto. Preferably, the thickness of the aluminum nitride layer is 35 Å-45 Å.

[0024] The boron nitride layer, serving as the primary passivation and protective layer, exhibits excellent high-temperature stability and water and oxygen barrier capabilities. The total thickness of the boron nitride layer is 900 Å to 1200 Å, exemplarily 900 Å, 950 Å, 1000 Å, 1050 Å, 1100 Å, 1150 Å, and 1200 Å, but is not limited thereto. Preferably, the total thickness of the boron nitride layer is 950 Å to 1100 Å.

[0025] Boron nitride layer, as the main passivation layer, has excellent chemical inertness, high density and excellent water and oxygen barrier properties. This allows the sidewall passivation layer to not only adhere tightly to the isolation trench and the sidewall of the N-type GaN via, but also to resist external environmental corrosion in a long-term stable manner, greatly extending the lifespan of the chip and thus improving the high-temperature and high-humidity reliability of the flip-chip.

[0026] In some embodiments, the boron nitride layer may further include a first boron nitride layer and a second boron nitride layer, formed by a two-stage atomic layer deposition (ALD) process. The boron nitride layer comprises a first boron nitride layer and a second boron nitride layer. The thickness of the first boron nitride layer is 100 Å-200 Å, exemplarily 100 Å, 120 Å, 150 Å, 170 Å, 180 Å, or 200 Å, but is not limited thereto. Preferably, the thickness of the first boron nitride layer is 120 Å-180 Å.

[0027] The thickness of the second boron nitride layer is 800 Å-1000 Å, exemplarily 800 Å, 850 Å, 900 Å, 950 Å, and 1000 Å, but not limited thereto. Preferably, the thickness of the second boron nitride layer is 850 Å-950 Å.

[0028] In some embodiments, the deposition pressure of the aluminum nitride layer is 1 Torr-5 Torr, and the deposition temperature is 200°C-250°C; the deposition pressure of the boron nitride layer is 1 Torr-5 Torr, and the deposition temperature is 200°C-250°C. The boron source is introduced into the first boron nitride layer at time T11 and the ammonia gas is introduced at time T12; the boron source is introduced into the second boron nitride layer at time T21 and the ammonia gas is introduced at time T22, satisfying that T21 > T11 and T22 > T12.

[0029] During the deposition of the second boron nitride layer, the boron source introduction time is longer than that of the first boron nitride layer, and the ammonia gas introduction time of the second boron nitride layer is longer than that of the first boron nitride layer. With this setting, the amount of boron source adsorption in the first deposition can be precisely controlled, the crystallinity of the film layer is moderate, and the bonding force with the underlying aluminum nitride is strong. The boron source adsorption in the second deposition is more uniform, the ammonia gas reaction is more complete, the crystallinity of the film layer is higher, the density is higher, and it is more conducive to improving the high temperature and high humidity performance. In this way, the high temperature and high humidity performance is maximized while ensuring the bonding force.

[0030] In some embodiments, the deposition conditions of the first boron nitride layer are as follows: The deposition pressure is 1 Torr-5 Torr, exemplarily 1 Torr, 2 Torr, 4 Torr or 5 Torr, but not limited thereto; The deposition temperature is 2000℃-250℃, exemplarily 200℃, 210℃, 230℃ or 250℃, but not limited thereto; Trimethylboron (TMB) gas is introduced for 0.8s-1s, exemplarily 0.8s, 0.9s, 0.95s, or 1s, but not limited thereto, to allow the trimethylboron gas to be adsorbed onto the surface of the aluminum nitride layer. Ar inert gas is introduced to purge for 1.5s-2s, for example 1.5s, 1.6s, 1.7s or 2s, but not limited to this, to thoroughly remove excess TMB gas and reaction byproducts that have not been adsorbed in the reaction chamber, and to avoid residual impurities affecting the interlayer bonding force. Ammonia (NH3) gas is introduced for 1.2s-1.5s, exemplarily 1.2s, 1.3s, 1.4s or 1.5s, but not limited thereto, so that NH3 can fully react with TMB adsorbed on the surface to generate a boron nitride film. Ar inert gas is introduced for purging for 2.0-2.5 seconds, exemplarily 2 seconds, 2.1 seconds, 2.3 seconds, or 2.5 seconds, but not limited to these. Unreacted NH3 gas and reaction residue are removed, completing the single deposition of the first boron nitride layer. Repeat the above deposition steps until the thickness of the first boron nitride layer is 100 Å-200 Å.

[0031] In some embodiments, the deposition conditions of the second boron nitride layer are as follows: Trimethylboron (TMB) gas is introduced for 1.2s-1.4s, exemplarily 1.2s, 1.3s, 1.35s or 1.4s, but not limited thereto, to ensure that TMB is uniformly adsorbed on the surface of the first boron nitride layer and to compensate for any minor defects that may exist in the underlying layer. Ar inert gas is introduced to purge for 1.5s-2s, exemplarily 1.5s, 1.6s, 1.7s or 2s, but not limited thereto, to remove excess TMB gas and reaction byproducts that have not been adsorbed in the reaction chamber. Ammonia gas is introduced for 1.8s-2s, exemplarily 1.8s, 1.9s, 1.95s or 2s, but not limited thereto, so that NH3 can fully react with TMB adsorbed on the surface to generate a second boron nitride layer. Ar inert gas is introduced for purging. The purging time is 2.0s-2.5s, exemplarily 2s, 2.1s, 2.3s or 2.5s, but not limited to this. This removes unreacted NH3 gas and reaction residue, completing the single deposition of the second boron nitride layer. Repeat the above deposition steps until the thickness of the second boron nitride layer is 800 Å-1000 Å.

[0032] Furthermore, the sidewall passivation layer 12 covers the surface and sidewall of the isolation groove, and covers the sidewall of the N-type GaN via, and partially covers the P-type GaN layer and the N-type GaN layer; the distance between the edge of the sidewall passivation layer 12 and the edge of the N-type GaN via sidewall 114 is L, where L is 2μm-5μm, exemplarily 2μm, 3μm, 4μm or 5μm, but not limited thereto, to ensure effective protection of the sidewall without affecting the electrical connection.

[0033] It should be noted that, as Figure 3 As shown, the distance between one edge of the sidewall passivation layer 12 and the top edge of the N-type GaN via sidewall 114 is L, and the distance between the other edge and the bottom edge of the N-type GaN via sidewall 114 is L.

[0034] The metal reflective layer 13 is disposed on the upper surface of the P-type GaN layer 113. It reflects photons emitted downwards from the active light-emitting layer 112, causing them to exit from above the chip, thereby improving light extraction efficiency. In one specific embodiment, the metal reflective layer 13, from bottom to top, includes an ITO layer, an Ag layer, a first Ti layer, a first Ni layer, a first Pt layer, a second Ti layer, a second Ni layer, a second Pt layer, and a third Ti layer.

[0035] The thickness of the ITO layer is 50 Å-80 Å, exemplarily 50 Å, 60 Å, 70 Å, or 80 Å, but not limited thereto; the thickness of the Ag layer is 1200 Å-2000 Å, exemplarily 1200 Å, 1500 Å, 1700 Å, or 2000 Å, but not limited thereto; the thickness of the first Ti layer is 1000 Å-2000 Å, exemplarily 1000 Å, 1300 Å, 1500 Å, or 2000 Å, but not limited thereto; the thickness of the first Ni layer is 1000 Å-2000 Å, exemplarily 1000 Å, 1300 Å, 1500 Å, or 2000 Å, but not limited thereto; the thickness of the first Pt layer is 1000 Å-2000 Å, exemplarily 1000 Å, 1300 Å, 1500 Å, or 2000 Å, but not limited thereto; The thickness of the second Ti layer is 1000A-2000A, exemplarily 1000A, 1300A, 1500A or 2000A, but not limited thereto; the thickness of the second Ni layer is 1000A-2000A, exemplarily 1000A, 1300A, 1500A or 2000A, but not limited thereto; the thickness of the second Pt layer is 2000A-3000A, exemplarily 2000A, 2400A, 2700A or 3000A, but not limited thereto; the thickness of the third Ti layer is 30A-50A, exemplarily 30A, 40A, 45A or 50A, but not limited thereto; the ITO layer can be used as an ohmic contact layer, the Ag layer is a high reflectivity metal, and multilayer metals such as Ti / Ni / Pt can be used as an adhesion layer, a diffusion barrier layer and a protective layer.

[0036] The first insulating layer 14 covers the metal reflective layer 13 and the sidewall passivation layer 12. The first insulating layer 14 has two conductive vias: one located above the metal reflective layer 13, serving as a P-type connection hole 19; the other located above the N-type connection hole 18, serving as an N-type connection hole 18. In some embodiments, the material of the first insulating layer 14 may be SiO2, SiNx, Al2O3, or a combination thereof.

[0037] The connecting metal layer forms electrical connections with the underlying metal reflective layer 13 (i.e., the P-type electrode) and the exposed N-type GaN layer 111 (i.e., the N-type electrode) through conductive vias in the first insulating layer 14. Specifically, the P-type connecting metal layer 151 is connected to the metal reflective layer 13 through a P-type connecting hole 19; the N-type connecting metal layer 152 is connected to the N-type GaN layer 111 through an N-type connecting hole 18. The P-type connecting metal layer 151 and the N-type connecting metal layer 152 are insulated from each other in the horizontal direction. Preferably, both the P-type connecting metal layer 151 and the N-type connecting metal layer 152 are Cr / Al / Ti / Pt / Ti / Pt / Ti / Au / Pt / Ti stacked structures, which have good conductivity, adhesion, and anti-electromigration ability.

[0038] The P-type pad layer 171 and N-type pad layer 172 are formed on the P-type connection metal layer 151 and N-type connection metal layer 152, respectively, for subsequent chip packaging bonding. The area outside the P-type pad layer 171 and N-type pad layer 172 is covered by a second insulating layer to achieve insulation and protection.

[0039] In some embodiments, both the P-type pad layer 171 and the N-type pad layer 172 are Al / Ti / Pt / Ni / Au stacked structures, and the thicknesses of the Al / Ti / Pt / Ni / Au stacked structures are 10000-16000 Å, 1000 Å-2000 Å, 1000 Å-2000 Å, 5000-10000 Å, and 200-500 Å, respectively; exemplarily, the thickness of the Al layer is 10000 Å, 12000 Å, and 14000 Å. The thickness of the Ti layer is 1000 Å, 1200 Å, 1400 Å, or 2000 Å, but not limited thereto; the thickness of the Pt layer is 1000 Å, 1200 Å, 1400 Å, or 2000 Å, but not limited thereto; the thickness of the Ni layer is 5000 Å, 7000 Å, 9000 Å, or 10000 Å, but not limited thereto; the thickness of the Au layer is 200 Å, 300 Å, 400 Å, or 500 Å, but not limited thereto.

[0040] Accordingly, the present invention also provides a method for fabricating a flip-chip light-emitting diode, such as... Figure 8 As shown, it includes: S100. An epitaxial layer is formed on the substrate 10, the epitaxial layer comprising an N-type GaN layer 111, an active light-emitting layer 112 and a P-type GaN layer 113 sequentially stacked on the substrate 10. S200: Etching forms an N-type GaN conductive step 116 that exposes a portion of the N-type GaN layer 111 and an isolation trench 115 extending downward from the N-type GaN conductive step 116. The sidewall of the N-type GaN conductive step 116 transitioning to the P-type GaN layer 113 is an N-type GaN via sidewall 114. Figure 1 and 2 As shown.

[0041] S300. A sidewall passivation layer 12 is provided on the isolation groove 115 and the sidewall 114 of the N-type GaN through hole. The sidewall passivation layer 12 forms an N-type connection hole 18 above the N-type GaN conductive step 116. Figure 3 As shown.

[0042] In some embodiments, the sidewall passivation layer 12 is a stacked structure, including an aluminum nitride layer that is in direct contact with the surfaces of the isolation groove 115, the N-type GAN via sidewall 114, etc., and a boron nitride layer deposited on the aluminum nitride layer.

[0043] The aluminum nitride layer serves as a transition layer, forming a good interface with the GaN material and reducing interface states and stress. Its thickness can be 30 Å-50 Å, exemplarily 30 Å, 40 Å, 45 Å, or 50 Å, but is not limited thereto. Preferably, the thickness of the aluminum nitride layer is 35 Å-45 Å.

[0044] The boron nitride layer, serving as the primary passivation and protective layer, exhibits excellent high-temperature stability and water and oxygen barrier capabilities. The total thickness of the boron nitride layer is 900 Å to 1200 Å, exemplarily 900 Å, 950 Å, 1000 Å, 1050 Å, 1100 Å, 1150 Å, and 1200 Å, but is not limited thereto. Preferably, the total thickness of the boron nitride layer is 950 Å to 1100 Å.

[0045] Boron nitride layer, as the main passivation layer, has excellent chemical inertness, high density and excellent water and oxygen barrier properties. This allows the sidewall passivation layer to not only adhere tightly to the isolation trench and the sidewall of the N-type GaN via, but also to resist external environmental corrosion in a long-term stable manner, greatly extending the lifespan of the chip and thus improving the high-temperature and high-humidity reliability of the flip-chip.

[0046] In some embodiments, the boron nitride layer may further include a first boron nitride layer and a second boron nitride layer, formed by a two-stage atomic layer deposition (ALD) process. The boron nitride layer comprises a first boron nitride layer and a second boron nitride layer. The thickness of the first boron nitride layer is 100 Å-200 Å, exemplarily 100 Å, 120 Å, 150 Å, 170 Å, 180 Å, or 200 Å, but is not limited thereto. Preferably, the thickness of the first boron nitride layer is 120 Å-180 Å.

[0047] The thickness of the second boron nitride layer is 800 Å-1000 Å, exemplarily 800 Å, 850 Å, 900 Å, 950 Å, and 1000 Å, but not limited thereto. Preferably, the thickness of the second boron nitride layer is 850 Å-950 Å.

[0048] In some embodiments, the deposition pressure of the aluminum nitride layer is 1 Torr-5 Torr, and the deposition temperature is 200°C-250°C; the deposition pressure of the boron nitride layer is 1 Torr-5 Torr, and the deposition temperature is 200°C-250°C. The boron source is introduced into the first boron nitride layer at time T11 and the ammonia gas is introduced at time T12; the boron source is introduced into the second boron nitride layer at time T21 and the ammonia gas is introduced at time T22, satisfying that T21 > T11 and T22 > T12.

[0049] During the deposition of the second boron nitride layer, the boron source introduction time is longer than that of the first boron nitride layer, and the ammonia gas introduction time of the second boron nitride layer is longer than that of the first boron nitride layer. With this setting, the amount of boron source adsorption in the first deposition can be precisely controlled, the crystallinity of the film layer is moderate, and the bonding force with the underlying aluminum nitride is strong. The boron source adsorption in the second deposition is more uniform, the ammonia gas reaction is more complete, the crystallinity of the film layer is higher, the density is higher, and it is more conducive to improving the high temperature and high humidity performance. In this way, the high temperature and high humidity performance is maximized while ensuring the bonding force.

[0050] In some embodiments, the deposition conditions of the first boron nitride layer are as follows: The deposition pressure is 1 Torr-5 Torr, exemplarily 1 Torr, 2 Torr, 4 Torr or 5 Torr, but not limited thereto; The deposition temperature is 2000℃-250℃, exemplarily 200℃, 210℃, 230℃ or 250℃, but not limited thereto; Trimethylboron (TMB) gas is introduced for 0.8s-1s, exemplarily 0.8s, 0.9s, 0.95s, or 1s, but not limited thereto, to allow the trimethylboron gas to be adsorbed onto the surface of the aluminum nitride layer. Ar inert gas is introduced to purge for 1.5s-2s, for example 1.5s, 1.6s, 1.7s or 2s, but not limited to this, to thoroughly remove excess TMB gas and reaction byproducts that have not been adsorbed in the reaction chamber, and to avoid residual impurities affecting the interlayer bonding force. Ammonia (NH3) gas is introduced for 1.2s-1.5s, exemplarily 1.2s, 1.3s, 1.4s or 1.5s, but not limited thereto, so that NH3 can fully react with TMB adsorbed on the surface to generate a boron nitride film. Ar inert gas is introduced for purging for 2.0-2.5 seconds, exemplarily 2 seconds, 2.1 seconds, 2.3 seconds, or 2.5 seconds, but not limited to these. Unreacted NH3 gas and reaction residue are removed, completing the single deposition of the first boron nitride layer. Repeat the above deposition steps until the thickness of the first boron nitride layer is 100 Å-200 Å.

[0051] In some embodiments, the deposition conditions of the second boron nitride layer are as follows: Trimethylboron (TMB) gas is introduced for 1.2s-1.4s, exemplarily 1.2s, 1.3s, 1.35s or 1.4s, but not limited thereto, to ensure that TMB is uniformly adsorbed on the surface of the first boron nitride layer and to compensate for any minor defects that may exist in the underlying layer. Ar inert gas is introduced to purge for 1.5s-2s, exemplarily 1.5s, 1.6s, 1.7s or 2s, but not limited thereto, to remove excess TMB gas and reaction byproducts that have not been adsorbed in the reaction chamber. Ammonia gas is introduced for 1.8s-2s, exemplarily 1.8s, 1.9s, 1.95s or 2s, but not limited thereto, so that NH3 can fully react with TMB adsorbed on the surface to generate a second boron nitride layer. Ar inert gas is introduced for purging. The purging time is 2.0s-2.5s, exemplarily 2s, 2.1s, 2.3s or 2.5s, but not limited to this. This removes unreacted NH3 gas and reaction residue, completing the single deposition of the second boron nitride layer. Repeat the above deposition steps until the thickness of the second boron nitride layer is 800 Å-1000 Å.

[0052] Furthermore, the sidewall passivation layer 12 covers the surface and sidewall of the isolation groove, and covers the sidewall of the N-type GaN via, and partially covers the P-type GaN layer and the N-type GaN layer; the distance between the edge of the sidewall passivation layer 12 and the edge of the N-type GaN via sidewall 114 is L, where L is 2μm-5μm, exemplarily 2μm, 3μm, 4μm or 5μm, but not limited thereto, to ensure effective protection of the sidewall without affecting the electrical connection.

[0053] It should be noted that, as Figure 3 As shown, the distance between one edge of the sidewall passivation layer 12 and the top edge of the N-type GaN via sidewall 114 is L, and the distance between the other edge and the bottom edge of the N-type GaN via sidewall 114 is L.

[0054] After deposition, the passivation layer in specific areas (such as the N-type interconnect and the central region of the P-type GaN layer) is removed by photolithography and etching processes.

[0055] S400, A metal reflective layer 13 is disposed on the P-type GaN layer 113; like Figure 4 As shown, the metal reflective layer 13 is disposed on the upper surface of the P-type GaN layer 113. It is used to reflect photons emitted downwards from the active light-emitting layer 112, causing them to exit from above the chip, thereby improving light extraction efficiency. In one specific embodiment, the metal reflective layer 13, from bottom to top, includes an ITO layer, an Ag layer, a first Ti layer, a first Ni layer, a first Pt layer, a second Ti layer, a second Ni layer, a second Pt layer, and a third Ti layer.

[0056] S500, A first insulating layer 14 is provided on the P-type GaN layer 113 and the sidewall passivation layer 12, wherein the first insulating layer 14 provided on the P-type GaN layer 113 includes a P-type connection hole 19. like Figure 5 As shown, the first insulating layer 14 covers the metal reflective layer 13 and the sidewall passivation layer 12. The first insulating layer 14 has two conductive vias: one located above the metal reflective layer 13, serving as a P-type connection hole 19; the other located above the N-type connection hole 18, serving as an N-type connection hole 18. In some embodiments, the material of the first insulating layer 14 may be SiO2, SiNx, Al2O3, or a combination thereof.

[0057] S600, a P-type connecting metal layer 151 is provided on the first insulating layer 14 and the P-type connecting hole 19, and an N-type connecting metal layer 152 is provided on the first insulating layer 14 and the N-type connecting hole 18. The P-type connecting metal layer and the N-type connecting metal layer are indirectly connected, such as... Figure 6 As shown.

[0058] S700, A P-type pad layer 171 is provided on the P-type connection metal layer 151, and an N-type pad layer 172 is provided on the N-type connection metal layer 152. A second insulating layer is provided in the area outside the P-type pad layer 171 and the N-type pad layer 172, such as... Figure 7 As shown.

[0059] The present invention will be further described below with reference to specific embodiments: Example 1 This embodiment provides a flip-chip diode, which includes a substrate and an epitaxial structure. The epitaxial structure includes an N-type GaN layer, an active light-emitting layer, and a P-type GaN layer sequentially stacked on the substrate. The epitaxial structure includes an N-type GaN conductive step that exposes a portion of the N-type GaN layer and an isolation trench extending downward from the N-type GaN conductive step. The sidewall of the N-type GaN conductive step transitioning to the P-type GaN layer is an N-type GaN via sidewall. A sidewall passivation layer is provided on the isolation trench and the sidewall of the N-type GaN via. The sidewall passivation layer forms an N-type connection hole above the N-type GaN conductive step. The sidewall passivation layer has a stacked structure, including an aluminum nitride (AlN) layer that is in direct contact with the surfaces of the isolation trench and the sidewall of the N-type GaN via, and a boron nitride (BN) layer deposited on the aluminum nitride layer. The thickness of the aluminum nitride layer is 40 Å. The boron nitride layer includes a first boron nitride layer and a second boron nitride layer. The deposition pressure of the first boron nitride layer is 3 Torr, the deposition temperature is 230°C, and during deposition, trimethylboron is first introduced for 0.8 s, then Ar inert gas is introduced for 1.5 s purging, followed by ammonia for 1.2 s, and finally Ar inert gas is introduced for 2 s purging until the thickness of the first boron nitride layer reaches 150 Å. The deposition pressure of the second boron nitride layer is 3 Torr, the deposition temperature is 230℃, and during deposition, trimethylboron is first introduced for 1.2s, followed by Ar inert gas purging for 1.5s, then ammonia for 1.8s, and finally Ar inert gas purging for 2s, until the thickness of the first boron nitride layer reaches 900 Å; the edge distance of the sidewall passivation layer from the sidewall of the N-type GaN via is controlled at 2 μm.

[0060] A metal reflective layer is disposed on the P-type GaN layer. The metal reflective layer comprises an ITO layer, an Ag layer, a first Ti layer, a first Ni layer, a first Pt layer, a second Ti layer, a second Ni layer, a second Pt layer, and a third Ti layer, stacked sequentially. The thickness of the Ag layer is 1500 Å; the thickness of the first Ti layer is 1500 Å; the thickness of the first Ni layer is 1500 Å; the thickness of the first Pt layer is 1500 Å; the thickness of the second Ti layer is 1500 Å; the thickness of the second Ni layer is 1500 Å; the thickness of the second Pt layer is 2700 Å; and the thickness of the third Ti layer is 45 Å. A first insulating layer is disposed on the P-type GaN layer and the sidewall passivation layer, wherein the first insulating layer disposed on the P-type GaN layer includes a P-type connection hole; A P-type connecting metal layer is provided on the first insulating layer and the P-type connecting hole, and an N-type connecting metal layer is provided on the first insulating layer and the N-type connecting hole. The P-type connecting metal layer and the N-type connecting metal layer are indirectly connected. A P-type pad layer is disposed on the P-type connection metal layer, and an N-type pad layer is disposed on the N-type connection metal layer. A second insulating layer is disposed in the area outside the P-type and N-type pad layers. Both the P-type and N-type pad layers are Al / Ti / Pt / Ni / Au stacked structures. The thickness of the Al layer is 14000 Å; the thickness of the Ti layer is 1400 Å; the thickness of the Pt layer is 1400 Å; the thickness of the Ni layer is 9000 Å; and the thickness of the Au layer is 400 Å.

[0061] Example 2 The difference between this embodiment and Embodiment 1 is that: The deposition pressure of the first boron nitride layer is 3 Torr, and the deposition temperature is 230°C. During deposition, trimethylboron is first introduced for 0.9 s, followed by Ar inert gas purging for 1.8 s, then ammonia for 1.4 s, and finally Ar inert gas purging for 2.3 s, until the thickness of the first boron nitride layer reaches 150 Å. The deposition pressure of the second boron nitride layer is 3 Torr, and the deposition temperature is 230°C. During deposition, trimethylboron is first introduced for 1.3 s, followed by Ar inert gas purging for 1.8 s, then ammonia for 1.9 s, and finally Ar inert gas purging for 2.3 s, until the thickness of the first boron nitride layer reaches 900 Å. The edge distance of the sidewall passivation layer from the sidewall of the N-type GaN via is controlled at 2 μm.

[0062] Example 3 The difference between this embodiment and Embodiment 1 is that: The deposition pressure of the first boron nitride layer is 3 Torr, and the deposition temperature is 230°C. During deposition, trimethylboron is first introduced for 1 second, followed by Ar inert gas purging for 2 seconds, then ammonia for 1.5 seconds, and finally Ar inert gas purging for 2.5 seconds, until the thickness of the first boron nitride layer reaches 150 Å. The deposition pressure of the second boron nitride layer is 3 Torr, and the deposition temperature is 230°C. During deposition, trimethylboron is first introduced for 1.4 seconds, followed by Ar inert gas purging for 2 seconds, then ammonia for 2 seconds, and finally Ar inert gas purging for 2.5 seconds, until the thickness of the first boron nitride layer reaches 900 Å. The edge distance of the sidewall passivation layer from the sidewall of the N-type GaN via is controlled at 2 μm.

[0063] Example 4 The difference between this embodiment and Embodiment 1 is that: The deposition pressure of the first boron nitride layer is 3 Torr, and the deposition temperature is 230°C. During deposition, trimethylboron is first introduced for 1 second, followed by Ar inert gas purging for 2 seconds, then ammonia for 1.5 seconds, and finally Ar inert gas purging for 2.5 seconds, until the thickness of the first boron nitride layer reaches 150 Å. The deposition pressure of the second boron nitride layer is 3 Torr, and the deposition temperature is 230°C. During deposition, trimethylboron is first introduced for 1.4 seconds, followed by Ar inert gas purging for 2 seconds, then ammonia for 2 seconds, and finally Ar inert gas purging for 2.5 seconds, until the thickness of the first boron nitride layer reaches 900 Å. The edge distance of the sidewall passivation layer from the sidewall of the N-type GaN via is controlled at 5 μm.

[0064] Comparative Example 1 This comparative example provides a flip-chip LED, whose basic structure is the same as that of Example 1. The difference between it and Example 1 is: No sidewall passivation layer is provided on the isolation groove and the sidewall of the N-type GaN through hole.

[0065] The flip-chip LEDs of Examples 1-4 and Comparative Example 1 were fabricated into circular chips with a diameter of 1400 μm. These LED chips were placed in a test chamber with a temperature of 60°C and a humidity of 90% RH, and a 1 mA current was continuously applied to the chip to keep it lit. Every 72 hours, a 1 μA current was applied to test its voltage. If the voltage was below 2.1V, the LED chip was considered to have failed, and the current time point was recorded.

[0066] According to the experimental results, Examples 1 to 4 all adopted the technical solution of setting an aluminum nitride / boron nitride stacked structure as a sidewall passivation layer on the isolation groove and the sidewall of the N-type GaN through hole, while Comparative Example 1 did not set any sidewall passivation layer.

[0067] Under the same harsh environment (60°C, 90% RH), the Comparative Example 1 chip without passivation layer protection failed after only 504 hours; while all embodiments with this specific passivation layer achieved an order-of-magnitude improvement in reliability lifetime, ranging from 1584 hours to 1800 hours. This indicates that the structure claimed in this invention, which involves setting a passivation layer in a specific sidewall region to form an N-type interconnect, can significantly improve the long-term reliability of the chip under high temperature and high humidity conditions.

[0068] The above-disclosed embodiments are merely preferred embodiments of the present invention and should not be construed as limiting the scope of the present invention. Therefore, any equivalent variations made in accordance with the claims of the present invention are still within the scope of the present invention.

Claims

1. A flip-chip light-emitting diode, characterized in that, include: Substrate and epitaxial structure, wherein the epitaxial structure comprises an N-type GaN layer, an active light-emitting layer and a P-type GaN layer sequentially stacked on the substrate; The epitaxial structure includes an N-type GaN conductive step forming an exposed portion of the N-type GaN layer and an isolation groove extending downward from the N-type GaN conductive step. The sidewall of the N-type GaN conductive step transitioning to the P-type GaN layer is an N-type GaN via sidewall. A sidewall passivation layer is provided on the isolation groove and the sidewall of the N-type GaN via. The sidewall passivation layer includes an aluminum nitride layer and a boron nitride layer disposed on the aluminum nitride layer. An N-type connection hole is formed above the N-type GaN conductive step by the sidewall passivation layer. A metal reflective layer is disposed on the P-type GaN layer; A first insulating layer is disposed on the P-type GaN layer and the sidewall passivation layer, wherein the first insulating layer disposed on the P-type GaN layer includes a P-type connection hole; A P-type connecting metal layer is provided on the first insulating layer and the P-type connecting hole, and an N-type connecting metal layer is provided on the first insulating layer and the N-type connecting hole. The P-type connecting metal layer and the N-type connecting metal layer are indirectly connected. A P-type pad layer is provided on the P-type connection metal layer, an N-type pad layer is provided on the N-type connection metal layer, and a second insulating layer is provided in the area outside the P-type pad layer and the N-type pad layer.

2. The flip-chip LED as described in claim 1, characterized in that, The thickness of the aluminum nitride layer is 30A-50A, and the total thickness of the boron nitride layer is 900A-1200A; The boron nitride layer includes a first boron nitride layer and a second boron nitride layer, wherein the thickness of the first boron nitride layer is 100 Å-200 Å and the thickness of the second boron nitride layer is 800 Å-1000 Å.

3. The flip-chip light-emitting diode as described in claim 2, characterized in that, The deposition pressure of the aluminum nitride layer is 1 Torr-5 Torr, and the deposition temperature is 200℃-250℃; The deposition pressure of the boron nitride layer is 1 Torr-5 Torr, and the deposition temperature is 200℃-250℃; The boron source for the first boron nitride layer is introduced at time T11, and the ammonia gas is introduced at time T12. The boron source is introduced into the second boron nitride layer at time T21, and the ammonia gas is introduced at time T22, satisfying the conditions that T21 > T11 and T22 > T12.

4. The flip-chip LED as described in any one of claims 1-3, characterized in that, The sidewall passivation layer covers the surface and sidewall of the isolation trench, and also covers the sidewall of the N-type GaN via, and partially covers the P-type GaN layer and the N-type GaN layer; The distance between the edge of the sidewall passivation layer and the edge of the N-type GaN via sidewall is L, where L is 2μm-5μm.

5. The flip-chip LED as described in claim 1, characterized in that, The metallic reflective layer comprises, in sequence, an ITO layer, an Ag layer, a first Ti layer, a first Ni layer, a first Pt layer, a second Ti layer, a second Ni layer, a second Pt layer, and a third Ti layer; and / or The thickness of the ITO layer is 50 Å-80 Å; and / or The thickness of the Ag layer is 1200 Å-2000 Å; and / or The thickness of the first Ti layer is 1000 Å-2000 Å; and / or The thickness of the first Ni layer is 1000 Å-2000 Å; and / or The thickness of the first Pt layer is 1000 Å-2000 Å; and / or The thickness of the second Ti layer is 1000 Å-2000 Å; and / or The thickness of the second Ni layer is 1000 Å-2000 Å; and / or The thickness of the second Pt layer is 2000 Å-3000 Å; and / or The thickness of the third Ti layer is 30A-50A.

6. The flip-chip light-emitting diode as described in claim 1, characterized in that, Both the P-type and N-type connecting metal layers are Cr / Al / Ti / Pt / Ti / Pt / Ti / Au / Pt / Ti stacked structures; and / or Both the P-type and N-type pad layers are Al / Ti / Pt / Ni / Au stacked structures.

7. A method for fabricating a flip-chip light-emitting diode, characterized in that, include: An epitaxial layer is formed on a substrate, the epitaxial layer comprising an N-type GaN layer, an active light-emitting layer and a P-type GaN layer sequentially stacked on the substrate; The etching process forms an N-type GaN conductive step that exposes a portion of the N-type GaN layer, and an isolation trench extending downward from the N-type GaN conductive step. The sidewall of the N-type GaN conductive step transitioning to the P-type GaN layer is an N-type GaN via sidewall. A sidewall passivation layer is provided on the isolation groove and the sidewall of the N-type GaN via. The sidewall passivation layer includes an aluminum nitride layer and a boron nitride layer disposed on the aluminum nitride layer. An N-type connection hole is formed above the N-type GaN conductive step by the sidewall passivation layer. A metallic reflective layer is formed on the P-type GaN layer; A first insulating layer is formed on the P-type GaN layer and the sidewall passivation layer, wherein the first insulating layer on the P-type GaN layer includes a P-type connection hole; A P-type connection metal layer is formed on the first insulating layer and the P-type connection hole, and an N-type connection metal layer is formed on the first insulating layer and the N-type connection hole. The P-type connection metal layer and the N-type connection metal layer are indirectly connected. A P-type pad layer is formed on the P-type connection metal layer, an N-type pad layer is formed on the N-type connection metal layer, and a second insulating layer is disposed in the area outside the P-type pad layer and the N-type pad layer.

8. The method for fabricating a flip-chip light-emitting diode as described in claim 7, characterized in that, The formation process of the sidewall passivation layer includes: An aluminum nitride layer is deposited on the isolation trench and the sidewall of the N-type GaN via. The thickness of the aluminum nitride layer is 30 Å-50 Å, the deposition pressure is 1 Torr-5 Torr, and the deposition temperature is 200℃-250℃. A first boron nitride layer is deposited on an aluminum nitride layer, the thickness of the first boron nitride layer being 100 Å-200 Å, the deposition pressure being 1 Torr-5 Torr, and the deposition temperature being 200℃-250℃; A second boron nitride layer is deposited on the first boron nitride layer. The thickness of the second boron nitride layer is 800 Å-1000 Å, the deposition pressure is 1 Torr-5 Torr, and the deposition temperature is 200℃-250℃.

9. The method for fabricating a flip-chip light-emitting diode as described in claim 8, characterized in that, The deposition of the first boron nitride layer on the aluminum nitride layer includes: Trimethylboron gas is introduced for 0.8s-1s to allow the trimethylboron gas to be adsorbed on the surface of the aluminum nitride layer; Purge with Ar inert gas for 1.5s-2s; Ammonia gas is introduced for 1.2s-1.5s to form the first boron nitride layer; Ar inert gas was introduced for purging, and the purging time was 2.0s-2.5s, to complete the single deposition of the first boron nitride layer; Repeat the above deposition steps until the thickness of the first boron nitride layer is 100 Å-200 Å.

10. The method for fabricating a flip-chip light-emitting diode as described in claim 8, characterized in that, The deposition of the second boron nitride layer on the first boron nitride layer includes: Trimethylboron gas is introduced for 1.2s-1.4s to allow the trimethylboron gas to be adsorbed on the surface of the first boron nitride layer; Purge with Ar inert gas for 1.5s-2s; Ammonia gas is introduced for 1.8s-2s to generate a second boron nitride layer. Ar inert gas was introduced for purging for 2.0s-2.5s to complete the single deposition of the second boron nitride layer; Repeat the above deposition steps until the thickness of the second boron nitride layer is 800 Å-1000 Å.