A display panel and display device

By setting multiple light extraction layers for different light-emitting elements in the OLED display panel, the problem that the light extraction layer cannot take into account the luminous efficiency of different wavelengths is solved, achieving efficient light extraction and viewing angle consistency, reducing power consumption and extending lifespan.

CN123124600APending Publication Date: 2026-11-17XIAMEN TIANMA DISPLAY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611307640.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-26
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In existing OLED display technology, the light extraction layer cannot simultaneously meet the optimal luminous efficiency requirements of light-emitting elements of different wavelengths, resulting in light extraction efficiency loss and viewing angle bias.

Method used

By setting different numbers and/or different thicknesses of light extraction layers for different light-emitting elements, the light extraction layers of different color light-emitting elements are decoupled. The optical microcavity phase interference conditions of each sub-pixel are controlled by a multi-layer structure, allowing some light-emitting elements to adopt a multi-layer high and low refractive index structure, and some to adopt a single-layer high refractive index structure.

Benefits of technology

It significantly improves the overall luminous efficiency of white light and various monochromatic lights, reduces power consumption, extends the lifespan of the display panel, improves color accuracy and viewing angle consistency, reduces production costs, and improves process stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124600A_ABST
    Figure CN123124600A_ABST
Patent Text Reader

Abstract

This disclosure provides a display panel and display device, relating to the field of display technology. The panel includes a substrate, light-emitting elements, and a light extraction layer. The light-emitting elements include a first light-emitting element and a second light-emitting element, wherein the emission wavelength of the first light-emitting element is shorter than that of the second light-emitting element. The light extraction layer includes a first light extraction layer and a second light extraction layer, wherein the first light extraction layer is located on the side of the first light-emitting element facing away from the substrate, and the second light extraction layer is located on the side of the second light-emitting element facing away from the substrate. At least one of the first and second light extraction layers includes at least two dimming layers, and the number of dimming layers included in the first and second light extraction layers is different, and / or the thicknesses of the first and second light extraction layers are different. In this way, the optical microcavity coherent interference conditions of each sub-pixel are precisely controlled, significantly improving the light extraction efficiency of the display panel while reducing power consumption and improving viewing angle color shift.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure relates to the field of display technology, and more particularly to a display panel and display device. Background Technology

[0002] With the continuous development of science and technology, more and more display products, such as mobile phones, tablets, laptops and smart wearable devices, are being widely used in people's daily lives and work, bringing great convenience to people's daily lives and work, and becoming an indispensable tool for people today.

[0003] With the continuous development of organic light-emitting diode (OLED) display technology, improving the outcoupling efficiency of display devices is one of the key means to reduce power consumption and extend the lifespan of displays. In the OLED device structure, the capping layer (CPL) located above the cathode plays a crucial role in optimizing the microcavity effect and increasing the outcoupling efficiency. However, current CPL design schemes cannot perfectly meet the optimal luminous efficiency requirements of light-emitting elements at different wavelengths. Therefore, there is an urgent need for an outcoupling layer design scheme that can precisely control the microcavity for light-emitting elements at different wavelengths and maximize the outcoupling efficiency across the entire color spectrum. Summary of the Invention

[0004] To address the aforementioned technical issues, this disclosure provides a display panel and display device. By differentially matching the number and / or thickness of the dimming layer of the light extraction layer for light-emitting elements with different emission wavelengths, the optical microcavity coherent interference conditions of each sub-pixel are precisely controlled. This significantly improves the light extraction efficiency of the display panel while reducing power consumption and improving viewing angle distortion.

[0005] In a first aspect, this disclosure provides a display panel, including: Substrate; A light-emitting element is disposed on one side of a substrate, including a first light-emitting element and a second light-emitting element, wherein the emission wavelength of the first light-emitting element is shorter than the emission wavelength of the second light-emitting element; The light extraction layer includes a first light extraction layer and a second light extraction layer, wherein the first light extraction layer is located on the side of the first light-emitting element away from the substrate, and the second light extraction layer is located on the side of the second light-emitting element away from the substrate; At least one of the first light extraction layer and the second light extraction layer includes at least two dimming layers, the number of dimming layers included in the first light extraction layer and the second light extraction layer are different, and / or the thicknesses of the first light extraction layer and the second light extraction layer are different.

[0006] Secondly, based on the same inventive concept, this disclosure provides a display device, including the display panel provided in the first aspect of this disclosure.

[0007] The technical solution provided in this disclosure has the following advantages compared with the prior art: This solution overcomes the bottleneck of single-layer or uniformly thick light extraction layers failing to achieve full-band efficiency by setting different numbers and / or thicknesses of light extraction layers for different light-emitting elements. This allows light of various wavelengths to reach optimal constructive interference points, significantly improving the overall luminous efficiency of white light and various monochromatic lights. Considering that color shift at large viewing angles is mainly due to the change in microcavity interference phase with the observation angle, resulting in inconsistent attenuation of light intensity at different wavelengths, this disclosure decouples the light extraction layers of different color light-emitting elements, giving the first and second light extraction layers independent degrees of freedom for thickness or multi-layer structure adjustment. This allows for optimization of normal (front) light extraction efficiency while simultaneously optimizing the spectral phase at large viewing angles for specific wavelengths (such as wavelengths sensitive to color shift), effectively suppressing color shift at different viewing angles and improving color accuracy and viewing angle consistency.

[0008] Furthermore, while multi-layer structures in the light extraction layer offer superior optical performance, increased layers require more evaporation cycles, longer production cycles, and higher manufacturing costs. This solution allows for different numbers of layers in the first and second light extraction layers (e.g., a multi-layer high-low refractive index structure in one part, and a single-layer high refractive index structure in another). For example, multi-layer dimming layers can be used for sub-pixels sensitive to efficiency gain or with shorter wavelengths; while fewer layers or a single dimming layer can be used for sub-pixels with good inherent efficiency or those where a single layer is sufficient for microcavity requirements (e.g., green light). This approach optimizes overall screen optical performance while reducing unnecessary evaporation processes, lowering production costs, and improving process stability.

[0009] Furthermore, to achieve the same light output brightness in a display panel, higher light extraction efficiency results in lower driving current required by the light-emitting elements. By optimizing the light extraction layer structure of each color light-emitting element, the overall light extraction efficiency is improved. This significantly reduces the power consumption of the light-emitting devices while maintaining the same display brightness. The reduction in driving current also helps alleviate the thermal aging of the light-emitting layer material, indirectly extending the lifespan of the display panel. Attached Figure Description

[0010] The accompanying drawings, which are incorporated in and form a part of this specification, illustrate embodiments consistent with this disclosure and, together with the description, serve to explain the principles of this disclosure.

[0011] To more clearly illustrate the technical solutions in the embodiments of this disclosure or the prior art, the accompanying drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, for those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0012] Figure 1 The image shown is a plan view of a display panel provided in an embodiment of this disclosure; Figure 2 As shown Figure 1 A cross-sectional view of the display panel along the CC' direction; Figure 3 As shown Figure 1 Another cross-sectional view of the display panel along the CC' direction; Figure 4 As shown Figure 1 Another cross-sectional view of the display panel along the CC' direction; Figure 5 As shown Figure 1 Another cross-sectional view of the display panel along the CC' direction; Figure 6 As shown Figure 1 Another cross-sectional view of the display panel along the CC' direction; Figure 7 As shown Figure 1 Another cross-sectional view of the display panel along the CC' direction; Figure 8 As shown Figure 1 A schematic diagram of a film layer of the three light-emitting elements in a display panel; Figure 9 As shown Figure 1 A schematic diagram of another film layer of the three light-emitting elements in the display panel; Figure 10 As shown Figure 1 A schematic diagram of another film layer of the three light-emitting elements in the display panel; Figure 11 As shown Figure 1 A schematic diagram of another film layer of the three light-emitting elements in the display panel; Figure 12 As shown Figure 1 A schematic diagram of another film layer of the three light-emitting elements in the display panel; Figure 13 The diagram shown is a planar structural schematic of a display device provided in an embodiment of this disclosure. Detailed Implementation

[0013] To better understand the above-mentioned objectives, features, and advantages of this disclosure, the solutions disclosed herein will be further described below. It should be noted that, unless otherwise specified, the embodiments and features described herein can be combined with each other.

[0014] Numerous specific details are set forth in the following description in order to provide a full understanding of this disclosure, but this disclosure may also be implemented in other ways different from those described herein; obviously, the embodiments in the specification are only some, and not all, of the embodiments of this disclosure.

[0015] In OLED device structures, the capping layer (CPL) located above the cathode plays a crucial role in optimizing the optical microcavity effect and increasing light extraction efficiency. During their research, the inventors discovered that when a single-layer high-refractive-index material is uniformly vapor-deposited into a capping layer, the thickness of the capping layer covering different color light-emitting elements is identical. However, because the emission wavelengths of red, green, and blue light-emitting elements are different, and the refractive index-wavelength curve of the single-layer capping layer material is fixed, the single-layer capping layer with a single thickness and refractive index cannot simultaneously match the optimal light extraction position for different emission wavelengths, resulting in a significant loss of light extraction efficiency.

[0016] Further research by the inventors revealed that when a multilayer light extraction layer is formed by combining materials with different refractive indices (such as alternating layers of high / low refractive index materials), although the multilayer light extraction layer takes into account the optical characteristics of different wavelengths to a certain extent, the matching rate is still not ideal because the structure and thickness of the light extraction layer film in the regions where different color light-emitting elements are located remain consistent. In particular, when taking into account the optimization design of the apparent color bias, there will still be a problem of light extraction efficiency loss.

[0017] Therefore, this disclosure provides a display panel, Figure 1 The diagram shown is a plan view of a display panel provided in an embodiment of this disclosure. It should be noted that... Figure 1 This illustration only shows one arrangement of different light-emitting elements in the display panel and does not limit the actual arrangement, shape, or number of light-emitting elements in the display panel. Figure 2 As shown Figure 1 This is a CC'-direction cross-sectional view of a display panel. This view only illustrates the key film layers in the display panel and does not limit the actual number or size of the film layers contained within the display panel. Please refer to [reference needed]. Figure 1 and Figure 2 The display panel 100 provided in this embodiment includes: Substrate 00; The light-emitting element 90 is disposed on one side of the substrate 00 and includes a first light-emitting element 91 and a second light-emitting element 92. The light-emitting wavelength of the first light-emitting element 91 is smaller than the light-emitting wavelength of the second light-emitting element 92. The light extraction layer 000 includes a first light extraction layer 10 and a second light extraction layer 20. The first light extraction layer 10 is located on the side of the first light-emitting element 91 that is away from the substrate 00, and the second light extraction layer 20 is located on the side of the second light-emitting element 92 that is away from the substrate 00. At least one of the first light extraction layer 10 and the second light extraction layer 20 includes at least two dimming layers tg, the number of dimming layers tg included in the first light extraction layer 10 and the second light extraction layer 20 is different, and / or the thickness of the first light extraction layer 10 and the second light extraction layer 20 is different.

[0018] The display panel provided in this embodiment is an Organic Light-Emitting Diode (OLED) display panel. The display panel includes a pixel definition layer 40 and light-emitting elements 90. The pixel definition layer 40 includes a plurality of pixel openings K0, and the light-emitting elements 90 are located at least in the pixel openings K0. Exemplarily, the light-emitting element 90 includes an anode 90-1, a light-emitting material layer 90-2, and a cathode 90-3. The light-emitting material layer 90-2 is located between the anode 90-1 and the cathode 90-3, and the anode 90-1 is located on the side of the light-emitting material layer 90-2 facing the substrate 00. When electrical signals are provided to the anode 90-1 and the cathode 90-3, the anode 90-1 injects holes into the light-emitting material layer 90-2, and the cathode 90-3 injects electrons into the light-emitting material layer 90-2. The recombination of electrons and holes stimulates the light-emitting material layer 90-2 to emit light, thereby enabling the corresponding light-emitting element 90 to be displayed. Optionally, an array layer 01 is also provided between the substrate 00 and the light-emitting element 90, and the anode 90-1 of the light-emitting element 90 is electrically connected to the array layer 01 to obtain a driving signal.

[0019] OLEDs are typical microcavity structures where light reflects back and forth between the anode 90-1 and the cathode 90-3, causing interference. By covering the cathode 90-3 with a light extraction layer of specific thickness and refractive index, the optical path from the light-emitting center to the upper surface of the device and the phase of the interface reflection can be precisely adjusted, enabling constructive interference of light of a specific wavelength in the emission direction, thereby greatly increasing the luminous intensity.

[0020] There is a significant refractive index difference between the cathode 90-3 material and the overlying dielectric (encapsulation layer or air). Without the light extraction layer 000, a large amount of light would undergo total internal reflection at the cathode 90-3 / air or cathode 90-3 / encapsulation layer interface, becoming trapped inside the device and converted into waveguide mode, ultimately resulting in heat loss. When the light extraction layer 000 is introduced, it acts as a refractive index transition buffer layer (similar to an anti-reflection film), widening the critical angle for total internal reflection and extracting more internal light, thus improving light extraction efficiency.

[0021] The light-emitting mechanism of OLEDs is dominated by the optical microcavity effect, and the constructive interference condition for optimal light extraction efficiency strongly depends on the wavelength of the light and the optical thickness of the light extraction layer 000. Since the wavelengths of the first light-emitting element 91 (such as a blue / green light-emitting element) and the second light-emitting element 92 (such as a red light-emitting element) are different, this solution breaks through the bottleneck that a single-layer or uniformly thick light extraction layer 000 cannot achieve full-band efficiency by setting different numbers and / or different thicknesses of light extraction layers 000 for different light-emitting elements 90. This allows light of various wavelengths to reach a better constructive interference point, significantly improving the overall luminous efficiency of white light and various monochromatic lights.

[0022] Considering that color shift at large viewing angles is mainly due to the change in microcavity interference phase with the observation angle, resulting in inconsistent attenuation of light intensity at different wavelengths, this disclosure decouples the light extraction layers 000 of different color light-emitting elements 90, giving the first light extraction layer 10 and the second light extraction layer 20 independent degrees of freedom for thickness or multilayer structure adjustment. This allows for optimization of the normal (front) light extraction efficiency while simultaneously optimizing the spectral phase at large viewing angles for specific wavelengths (such as wavelengths sensitive to color shift), effectively suppressing color shift at different viewing angles and improving color accuracy and viewing angle consistency.

[0023] Furthermore, while a multi-layer structure in the light extraction layer 000 offers superior optical performance, an increase in the number of layers necessitates more evaporation cycles, longer production cycles, and higher manufacturing costs. This solution allows the first light extraction layer 10 and the second light extraction layer 20 to employ different numbers of layers (e.g., a portion using a multi-layer high-low refractive index structure, and another portion using a single-layer high-refractive-index dimming layer structure). For example, for light-emitting elements sensitive to efficiency gain or with shorter wavelengths, multi-layer dimming layers can be used for dimming; for light-emitting elements with inherently good efficiency or where a single layer is sufficient to meet microcavity requirements, fewer layers or a single-layer dimming layer can be used for dimming. While ensuring optimized overall screen optical performance, this solution also helps reduce unnecessary evaporation processes, lower production costs, and improve process stability.

[0024] Furthermore, under the requirement of achieving the same light output brightness in the display panel, the higher the light extraction efficiency, the lower the driving current required by the light-emitting element 90. By optimizing the light extraction layer 000 structure of each of the different colored light-emitting elements 90, the overall light extraction efficiency is improved, thereby significantly reducing the power consumption of the light-emitting device while maintaining the same display brightness. The reduction in driving current also helps to alleviate the thermal aging of the light-emitting layer material, indirectly extending the service life of the display panel.

[0025] Please continue to refer to this. Figure 2 In one optional embodiment of this disclosure, the display panel includes a pixel definition layer 40, which includes a plurality of pixel openings K0. Different light-emitting elements 90 are located in different pixel openings K0, and a light extraction layer 000 is located in the pixel opening K0 corresponding to the light-emitting element 90 and extends to the periphery of the pixel opening K0.

[0026] In this disclosure, the light extraction layer 000 is not only disposed inside the pixel opening K0 corresponding to the light-emitting element 90, but also extends to the peripheral area of ​​the pixel opening K0 (i.e., covering the side of the pixel definition layer 40 facing away from the substrate 00). During fine evaporation using a mask, due to the angular scattering of the evaporation source and the alignment tolerance between the mask and the substrate, it is difficult to achieve precise and absolute alignment between the evaporation material and the edge of the pixel opening. Extending the light extraction layer 000 to the periphery of the pixel opening allows for a certain process margin. This ensures that even with evaporation alignment deviations or edge shading effects, the interior of the pixel opening (i.e., the effective light-emitting area) can be completely and uniformly covered with the light extraction layer 000 of a predetermined thickness, avoiding damage to the optical microcavity and uneven light emission caused by the absence or thinning of the light extraction layer 000 at the opening edge.

[0027] In a display panel, light emitted from organic light-emitting materials not only travels vertically upwards but also propagates at a large angle towards the edge of the pixel aperture. If the light extraction layer 000 is confined to the inside of the pixel aperture, the aperture edge will create a vertical boundary interruption between the light extraction layer 000 and the upper medium (such as the encapsulation layer), forming a boundary with a sudden change in refractive index. When the light extraction layer 000 extends to the side of the pixel definition layer 40 facing away from the substrate 00, light rays emitted obliquely from the edge of the pixel aperture can still pass through the continuous and gentle light extraction layer 000, maintaining consistent optical matching conditions. This reduces total internal reflection and scattering losses at the aperture edge during oblique light propagation, effectively improving the light extraction efficiency in large-angle and edge regions.

[0028] The pixel definition layer 40 has a noticeable step (sloping surface) between the pixel opening and the top of the barrier. If the pixel definition layer 40 breaks only at the bottom of the pixel opening, it will exacerbate the unevenness of the step. Therefore, the light extraction layer 000 crosses the pixel opening slope and extends above the pixel definition layer 40, acting as a ramp and smoothing the step transition. This provides a smoother substrate surface for the subsequent encapsulation layer fabrication, reducing the risk of stress concentration and cracking caused by steep steps, and improving the sealing reliability of the water and oxygen barrier.

[0029] Please continue to refer to this. Figure 2 In one optional embodiment of this disclosure, the first light extraction layer 10 includes at least one first dimming layer 101 and at least one second dimming layer 102. The first dimming layer 101 and the second dimming layer 102 are stacked along the thickness direction of the display panel. The refractive index of the first dimming layer 101 is less than the refractive index of the second dimming layer 102. The second light extraction layer 20 includes a third dimming layer 203. The refractive index of the third dimming layer 203 is greater than or equal to the refractive index of the second dimming layer 102.

[0030] The short-wavelength light-emitting element 90 (first light-emitting element 91, such as a blue light-emitting element) has a short microcavity period and is extremely sensitive to changes in the refractive index of the medium. By setting a multi-layer medium interface between a low-refractive-index dimming layer (first dimming layer 101) and a high-refractive-index dimming layer (second dimming layer 102) in the first light extraction layer 10, the electromagnetic field can be redistributed using multi-level thin-film interference, significantly increasing the light extraction gain for short wavelengths. For the second light-emitting element 92 (such as a green light-emitting element) with a longer wavelength or different optical microcavity requirements, this embodiment directly matches a third dimming layer 203 with a high refractive index or even higher refractive index. This effectively extends the optical path and amplifies the interference phase of long-wavelength light, eliminating the defect that a single refractive index material cannot simultaneously handle short or long wavelengths. This allows the light-emitting elements 90 of different wavelengths to reach their theoretical interference limits, effectively improving the light extraction efficiency for both white and monochromatic light.

[0031] A significant refractive index difference exists between the high-refractive-index cathode and the upper low-refractive-index medium (such as the encapsulation layer / air), which can easily lead to severe interfacial total internal reflection. In this embodiment, the first light extraction layer 10 adopts an alternating structure of low-refractive and high-refractive-index layers, introducing a gradient / stepped optical transition layer (similar to an anti-reflection film). This increases the critical angle for total internal reflection and reduces the interface reflectivity when light crosses different medium interfaces, thereby extracting more total internally reflected light that was originally trapped inside the device, further improving the light extraction efficiency.

[0032] In this disclosure, the second light extraction layer 20 employs a third dimming layer 203 with an independently designed and higher refractive index, allowing designers to individually fine-tune the spectral half-width and center wavelength of the second light-emitting element 92. This not only optimizes spectral stability at wide viewing angles (reducing viewing angle spectral bias) but also improves color purity by narrowing the emission spectral peak, thereby widening the overall color gamut of the display panel.

[0033] Forcing all sub-pixels across the entire screen to stack extremely high refractive index or extremely multiple dimming layers could lead to a surge in the cost of vapor deposition materials, and the high refractive index characteristics of some materials would increase the difficulty of production control. This solution allows for a division of labor in materials and structure between the first light extraction layer 10 (a composite structure of multiple high and low refractive index dimming layers) and the second light extraction layer 20 (a high refractive index single-layer dimming layer structure). While achieving the benefits of high light extraction, it avoids the need for a complex vapor deposition process across the entire screen, achieving a balance between extremely high optical performance and production cycle time / cost.

[0034] Figure 3 As shown Figure 1 Please refer to another CC' section view of the display panel. Figure 3 In one optional embodiment of this disclosure, the thickness H1 of the first dimming layer 101 is less than the thickness H2 of the second dimming layer 102, and the thickness H3 of the third dimming layer 203 is greater than the thickness H2 of the second dimming layer 102.

[0035] In this disclosure, in a scheme where the light extraction layer 000 includes multiple dimming layers, the low-refractive-index layer (first dimming layer 101) mainly functions to change the optical phase of the interface and introduce an anti-reflection interface, requiring a relatively small optical thickness; while the high-refractive-index layer (second dimming layer 102) is the core layer controlling the constructive interference position of the main microcavity. By setting the thickness of the low-refractive-index layer (first dimming layer 101) to a relatively small value (e.g., 50 Å to 200 Å) and the high-refractive-index layer (second dimming layer 102) to a relatively large thickness (e.g., 400 Å to 850 Å), the thinner low-refractive-index layer can provide accurate phase modulation without introducing additional extinction and dispersion losses due to excessive thickness. The thinner low-refractive-index layer can also significantly shorten the evaporation and deposition time of the film, increase the production cycle, and reduce the consumption and cost of low-refractive-index materials.

[0036] According to the microcavity constructive interference formula, the optimal physical thickness required for light output constructive interference is proportional to the wavelength of the light. For the second light-emitting element 92 with a longer wavelength (such as a red light-emitting element), the thickness of the light extraction layer 000 required to achieve optimal constructive interference is necessarily greater. In this embodiment, the thickness of the third dimming layer 203 corresponding to the second light-emitting element 92 is designed to be greater than the thickness of the second dimming layer 102, precisely meeting the optical interference requirements of long-wavelength light and significantly improving the external quantum efficiency of long-wavelength monochromatic light. For the first light-emitting element 91 with a shorter wavelength (such as a blue light-emitting element), maintaining a relatively thin second dimming layer 102 avoids phase misalignment and destructive interference of short-wavelength light due to excessive thickness, ensuring efficient extraction of short-wavelength light.

[0037] Figure 4 As shown Figure 1 Please refer to another CC' section view of the display panel. Figure 4 In one optional embodiment of this disclosure, the first light extraction layer 10 includes two first dimming layers 101 and one second dimming layer 102. Along the thickness direction of the display panel, the first dimming layer 101 is located on both sides of the second dimming layer 102.

[0038] In this embodiment, in the first light extraction layer 10, along the thickness direction of the display panel, the second dimming layer 102 (high refractive index) is sandwiched between two first dimming layers 101 (low refractive index), forming a symmetrical or quasi-symmetrical three-layer dimming structure consisting of a bottom low refractive index layer, a middle high refractive index layer, and a top low refractive index layer. The second light extraction layer 20 adopts a single-layer high refractive index structure for the third dimming layer 203.

[0039] When light exits from the light-emitting device to the light extraction layer and then to the upper film layer (such as the encapsulation layer), it continuously passes through the dielectric gradient of the low-refractive-index layer, high-refractive-index layer, and low-refractive-index layer. The bottom low-refractive-index first dimming layer 101 forms a transition interface between the cathode 90-3 and the high-refractive-index layer, smoothing out the abrupt change in refractive index and reducing the reflection loss of light at the cathode 90-3 interface. The top low-refractive-index layer (first dimming layer 101, with a refractive index of, for example, around 1.45-1.65) is introduced between the high-refractive-index layer (second dimming layer 102) and the upper encapsulation layer (e.g., with a refractive index of around 1.7-1.8), constructing a function similar to an optical anti-reflection film. This three-layer symmetrical structure significantly increases the light output efficiency across the entire wavelength range, achieving additional light extraction gain compared to a single-layer high-refractive-index structure. Simulation results show that the white light efficiency can be improved by up to 3.5%.

[0040] The second light-emitting element 92 (such as a green light-emitting element) typically accounts for a large proportion of the energy in the display panel. Simulations show that a green light-emitting element can achieve extremely high light extraction efficiency with a single high-refractive-index layer (the third dimming layer 203). If the green light-emitting element 90 is also forcibly made into a multi-layer dimming layer structure, it will increase the number of mask registration and evaporation steps. Simulations show that designing the second light extraction layer 20 corresponding to the second light-emitting element 92 as a single high-refractive-index layer, while the first light extraction layer 10 corresponding to the first light-emitting element 91 adopts a three-layer dimming layer design, can significantly improve the overall white light efficiency by about 3.5% compared to the structure of a single light extraction layer across the entire screen, and by about 2.4% compared to the design of introducing a multi-layer dimming layer of uniform thickness across the entire screen. In this way, unnecessary multi-layer evaporation is avoided in the area of ​​the second light-emitting element 92, greatly reducing the amount of evaporation material used, reducing the mask switching frequency, and shortening the production cycle, achieving the optimal balance between improving white light performance and mass production cost.

[0041] If each region corresponding to a different light-emitting element undergoes independent evaporation with multiple layers of complex film thickness, the accumulated alignment tolerances and shadow effects can easily lead to abnormal film thickness at the sub-pixel boundaries. An asymmetric combination scheme, using a three-layer dimming layer for the region corresponding to the first light-emitting element 91 and a single-layer dimming layer for the region corresponding to the second light-emitting element 92, significantly simplifies the mask control for the region containing the second light-emitting element 92. Even with minor alignment deviations during evaporation, the larger process window of the single-layer dimming layer can effectively tolerate edge coverage errors, thereby improving process stability and yield during large-area mass production of panels.

[0042] In one alternative embodiment of this disclosure, please refer to Figure 4 The second light extraction layer 20 consists of only one third dimming layer 203; or, please refer to Figure 5 The second light extraction layer 20 has a multi-layer structure, and further includes at least one first dimming layer 101 (i.e., simultaneously including a third dimming layer 203 and the first dimming layer 101). The first dimming layer 101 and the third dimming layer 203 are stacked along the thickness direction of the display panel. Figure 5 As shown Figure 1 Another CC' cross-sectional view of the display panel.

[0043] For the first scheme in this embodiment, please refer to Figure 4The second light extraction layer 20 consists of only one third dimming layer 203. That is, the first light-emitting element 91 uses three or more dimming layers, while the second light-emitting element 92 uses only one high-refractive-index third dimming layer 203. The second light-emitting element 92 (such as a green light-emitting element) has a higher proportion of light emission and efficiency weight in the display panel. Using a single dimming layer can accurately match the microcavity interference constructive conditions of green light and avoid adding multiple layers of evaporation processes for the second light-emitting element 92. Simulation shows that the white light estimated efficiency is about 3.5% higher than that of the traditional single layer, improving the overall light extraction efficiency with minimal process complexity. The green light band is more sensitive to the reflection phase of the multi-layer interference interface. The single-layer dimming layer structure avoids the green light intensity attenuation that may be caused by complex multi-layer interfaces when considering color offset design at large viewing angles, ensuring high color purity and viewing angle stability. It reduces the number of evaporation processes and material consumption of the mask in the area where the green light-emitting element is located, significantly improving the production efficiency and product yield of mass production.

[0044] For the second solution in this embodiment, please refer to... Figure 5 The second light extraction layer 20 also includes at least one first dimming layer 101. When the first dimming layer 101 and the third dimming layer 203 are stacked along the thickness direction of the display panel, both the first light-emitting element 91 and the second light-emitting element 92 adopt a multi-layer dimming layer structure (for example, the area of ​​the second light-emitting element 92 also introduces a stacked structure of a low-refractive-index first dimming layer 101 and a high-refractive-index third dimming layer 203). For the microcavity interference of the second light-emitting element 92 (such as a green light-emitting element), by adjusting the film thickness of the low-refractive-index and high-refractive-index dimming layers, the green color point can be further fine-tuned, and its microcavity efficiency can be pushed to the limit. Simulation estimates suggest that the white light efficiency improvement can reach as high as 4.9%~5%, breaking through the upper limit of light emission performance of a single-layer dimming layer scheme. In this embodiment, both the first light-emitting element 91 and the second light-emitting element 92 have the freedom to adjust the multi-layer interface. Designers can perform independent interference phase compensation for the large viewing angle optical path difference of green light, thereby achieving more precise viewing angle color deviation control across the entire color range and comprehensively improving image quality performance at large viewing angles. When the difference in high refractive / low refractive film thickness between red and green light is small, the same refractive index film layers corresponding to the first light-emitting element 91 and the second light-emitting element 92 can be combined for vapor deposition, so as to optimize some vapor deposition processes while pursuing high optical gain.

[0045] Figures 2 to 5 The embodiments illustrate a scheme in which the number of dimming layers included in the second light extraction layer 20 is less than the number of dimming layers included in the first light extraction layer 10. However, this disclosure is not limited thereto. In some other embodiments of this disclosure, the number of dimming layers included in the first light extraction layer 10 and the second light extraction layer 20 can also be set to be the same. For example, please refer to... Figure 6 , Figure 6 As shown Figure 1Another CC' cross-sectional view of the display panel. In an optional embodiment of this disclosure, the second light extraction layer 20 has a multi-layer structure, and the second light extraction layer 20 further includes at least one first dimming layer 101; the number of dimming layers included in the second light extraction layer 20 is equal to the number of dimming layers included in the first light extraction layer 10.

[0046] In this embodiment, both the second light extraction layer 20 (corresponding to the second light-emitting element 92, such as a green light-emitting element) and the first light extraction layer 10 (corresponding to the first light-emitting element 91, such as a red light-emitting element or a blue light-emitting element) adopt a multi-layer dimming layer structure (both include a low-refractive-index first dimming layer 101 and a high-refractive-index dimming layer). The first light extraction layer 10 and the second light extraction layer 20 contain the same number of dimming layers, for example, both adopt a three-layer structure, specifically including two low-refractive-index dimming layers and one high-refractive-index dimming layer, with the two low-refractive-index dimming layers located on both sides of the high-refractive-index dimming layer.

[0047] Considering that if the number of light extraction layers 000 of adjacent light-emitting elements 90 is inconsistent, a break in the number of film layers and a significant step difference will appear in the crossing area at the edge of the pixel definition layer 40, which may cause stress concentration. In this embodiment, the first light-emitting element 91 and the second light-emitting element 92 are kept to have the same number of dimming layers (e.g., uniformly 3 layers), so that the entire area where the first light-emitting element 91 and the second light-emitting element 92 are located has a consistent film layer stacking structure. This helps to eliminate the layer break at the sub-pixel junction, greatly smooths the stress distribution inside the film layer, avoids the risk of coating peeling or cracking, and significantly improves the flatness and moisture-proof sealing reliability of subsequent thin film encapsulation.

[0048] In this embodiment, a dimming layer with the same number of layers as the first light-emitting element 91 is introduced into the region of the second light-emitting element 92. Based on this, the thickness of the high-refractive-index layer in different light-emitting elements 90 can be finely adjusted. For example, the thickness of the third dimming layer 203 in the second light-emitting element 92 can be set differently from the thickness of the second dimming layer 102 in the first light-emitting element 91 (when the second light-emitting element 92 is a green light-emitting element, the thickness of the third dimming layer 203 is, for example, 600 Å; when the first light-emitting element 91 is a red light-emitting element, the thickness of the second dimming layer 102 is, for example, 650 Å; when the first light-emitting element 91 is a blue light-emitting element, the thickness of the second dimming layer 102 is, for example, 550 Å; in this case, the thickness of the first dimming layer 101 corresponding to different light-emitting elements can all be set to 150 Å). Without compromising the spectral purity of green light, the monochromatic efficiency of green light is further increased (in simulations, the efficiency of the green light-emitting element is increased from 100% of a single layer to 96.1%~103.6%). The precise adjustable range of the dimming layer makes the overall white light efficiency stably improved by about 3% compared to a single dimming layer.

[0049] When the number of dimming layers for different colored light-emitting elements is the same and the thickness of some layers is extremely similar (e.g., the high refractive index layer of a red light-emitting element (650 Å) differs from that of a green light-emitting element (600 Å) by only 50 Å), it exhibits strong compatibility in mass production coating processes. For dimming layers with minimal thickness differences (e.g., low refractive index layers with the same thickness at both ends), the dimming layers corresponding to different colored light-emitting elements 90 can be uniformly deposited in a single operation using the same set of masks. Only the high refractive index layers with differences require independent mask adjustments or partial merging of the deposition process. This significantly reduces the frequent switching and registration steps of fine masks, effectively controlling deposition costs and production cycle while enjoying the optical gains brought by multi-layer dimming layers.

[0050] The foregoing embodiments illustrate a scheme in which the number of dimming layers included in the second light extraction layer 20 is less than or equal to the number of dimming layers included in the first light extraction layer 10. However, this disclosure is not limited thereto. Please refer to [the relevant documentation]. Figure 7 , Figure 7 As shown Figure 1 Another CC' cross-sectional view of the display panel. In an optional embodiment of this disclosure, the second light extraction layer 20 has a multi-layer structure, and the second light extraction layer 20 further includes at least one first dimming layer 101; the number of dimming layers included in the second light extraction layer 20 is greater than the number of dimming layers included in the first light extraction layer 10.

[0051] In this embodiment, both the second light extraction layer 20 (corresponding to the second light-emitting element 92, such as a green light-emitting element) and the first light extraction layer 10 (corresponding to the first light-emitting element 91, such as a blue light-emitting element) adopt a multi-layer dimming layer structure. The number of dimming layers included in the second light extraction layer 20 is greater than the number of dimming layers included in the first light extraction layer 10. For example, the first light extraction layer 10 (such as the light extraction layer corresponding to the blue light-emitting element) adopts a 3-layer dimming layer structure (with thicknesses of, for example, 150 / 550 / 150 Å for low-reflection / high-reflection / low-reflection), while the second light extraction layer 20 (such as the light extraction layer corresponding to the green light-emitting element) adopts a structure with up to 5 dimming layers (with thicknesses of, for example, 150 / 550 / 150 / 550 / 150 Å for low-reflection / high-reflection / low-reflection / high-reflection / low-reflection).

[0052] The emission wavelength of the second light-emitting element 92 (such as a green light-emitting element) is located in the core region of the visible light band, and its emission energy accounts for a large proportion of the overall white light brightness. By superimposing more dimming layers (such as 5 layers of alternating high and low refraction) on the second light extraction layer 20, multiple reflections and multi-level interference interfaces are constructed, which can more precisely control the electromagnetic field distribution and constructive interference conditions in the green light band. Simulation data shows that in this embodiment, the efficiency of the green light-emitting element is significantly increased to 103.6%, and the efficiency of the red light-emitting element is increased to 104.59%, resulting in an estimated overall white light efficiency increase of 4.9%~5% compared to a single dimming layer across the entire screen (and an increase of approximately 2.4% compared to a uniform three-layer dimming layer across the entire screen).

[0053] A full-screen structure with a uniform thickness of three or a single dimming layer often results in broadening of the emission spectrum or a shift in the center wavelength when pursuing extremely high light extraction efficiency for green light, thus sacrificing color gamut and color purity. This embodiment increases the number of dimming layers in the second light extraction layer 20 (e.g., a five-layer structure), providing more dimensions for phase and amplitude control of the green light spectrum. This allows designers to precisely fine-tune the color trajectory / color point position of the light emitted by the green light-emitting element while increasing light extraction efficiency, avoiding color shift and color distortion caused by efficiency improvements, achieving a balance between high efficiency and high color saturation.

[0054] When light emitted from the light-emitting layer and cathode 90-3 passes through the thick light extraction layer, if the interface is uniform, total internal reflection can easily occur at the interface between the top and upper encapsulation layers, causing the light to get stuck inside the device. By stacking up to five alternating low-refractive / high-refractive / low-refractive / high-refractive / low-refractive dimming layers, an optical buffer band similar to a gradient refractive index is formed. This further widens the critical angle for total internal reflection of light emission, extracting more light rays traveling at large angles from inside the device and significantly improving the light extraction efficiency at large angles.

[0055] Figure 8 and Figure 9 The following are respectively shown Figure 1 Please refer to the schematic diagram of one film layer of the three light-emitting elements 90 in the display panel. Figure 8 or Figure 9 In one optional embodiment of this disclosure, the light-emitting element 90 further includes a third light-emitting element 93, and the light extraction layer further includes a third light extraction layer 30 disposed on the side of the third light-emitting element 93 facing away from the substrate 00. The emission wavelength of the third light-emitting element 93 is greater than the emission wavelength of the second light-emitting element 92. The number of dimming layers in the third light extraction layer 30 is the same as the number of dimming layers in the first light extraction layer 10.

[0056] The three light-emitting elements 90 satisfy the following condition: the emission wavelength of the third light-emitting element 93 (e.g., a red light-emitting element) > the emission wavelength of the second light-emitting element 92 (e.g., a green light-emitting element) > the emission wavelength of the first light-emitting element 91 (e.g., a blue light-emitting element). The third light extraction layer 30 contains the same number of dimming layers as the first light extraction layer 10. For example, both the third light extraction layer 30 and the first light extraction layer 10 have three dimming layers. Based on this, the second light extraction layer 20 corresponding to the second light-emitting element 92 can further include one dimming layer (e.g., a red light-emitting element). Figure 9 It may also include multiple dimming layers (such as...) Figure 8 ).

[0057] Both short-wavelength blue light emitters and long-wavelength red light emitters are extremely sensitive to the reflection phase at the microcavity interference interface, located at opposite ends of the spectrum. By unifying the short-wavelength blue light emitters and the long-wavelength red light emitters into a multi-layered structure (e.g., three layers of low-refractive / high-refractive / low-refractive dimming layers), and utilizing the anti-reflection and phase modulation capabilities provided by the multi-layered high- and low-refractive-index interfaces, the extraction efficiency of both long-wavelength and short-wavelength light can be simultaneously increased. Simulation data shows that… Figure 8 and Figure 9 In the corresponding scheme, the efficiency of the red light-emitting element 90 can be increased to 104.3%, and the efficiency of the blue light-emitting element 90 can be increased to 104.6%. The simultaneous and significant improvement in the emission efficiency of light at both wavelengths directly leads to a significant increase of 3% to 3.5% in the overall white light prediction efficiency.

[0058] If three different colored light-emitting elements 90 use three completely different numbers of dimming layers, it will lead to a sharp increase in the number of mask switching operations and an accumulation of registration and alignment tolerances. In this embodiment, the third light extraction layer 30 and the first light extraction layer 10 have the same number of dimming layers. For example, the thickness of the top and bottom low-refractive-index layers (e.g., 150 Å) in the third light extraction layer 30 and the first light extraction layer 10 is exactly the same as the material, so the same set of masks can be used for unified evaporation, which greatly reduces the number of evaporation steps. The thickness difference of the high-refractive-index layer can be controlled by adjusting the deposition time / evaporation amount (e.g., the thickness of the high-refractive-index layer in the third light extraction layer 30 is 650 Å, and the thickness of the high-refractive-index layer in the first light extraction layer 10 is 550 Å). This significantly reduces manufacturing costs and increases production cycle time while ensuring that the red and blue colors achieve optimal microcavity matching.

[0059] In display panels, red and blue light-emitting elements are alternately distributed in the pixel array. If the number of dimming layers corresponding to the two differs too much, it will cause frequency differences in layer number and uneven stress between pixels. In this embodiment, the number of dimming layers corresponding to the red and blue light-emitting elements is kept the same, so that the pixel area, which accounts for the majority of the panel area, has a consistent film layer stacking structure. This isomorphic design makes the physical stress distribution of the entire screen more uniform, avoids the risk of film peeling caused by multi-layer evaporation, and provides a smooth and continuous substrate for the subsequent inorganic encapsulation layer, further ensuring the moisture-proof sealing and yield of the panel.

[0060] Figure 8 and Figure 9 The embodiments illustrate a scheme in which the third light extraction layer 30 contains the same number of dimming layers as the first light extraction layer 10, but this disclosure is not limited thereto. Figure 10 As shown Figure 1 Please refer to the schematic diagram of another film layer of the three light-emitting elements 90 in the central display panel. Figure 10 In one optional embodiment of this disclosure, the light-emitting element 90 further includes a third light-emitting element 93, and the light extraction layer further includes a third light extraction layer 30 disposed on the side of the third light-emitting element 93 facing away from the substrate 00. The emission wavelength of the third light-emitting element 93 is greater than the emission wavelength of the second light-emitting element 92. The number of dimming layers included in the third light extraction layer 30 is greater than the number of dimming layers included in the first light extraction layer 10, and the number of dimming layers included in the third light extraction layer 30 is equal to the number of dimming layers included in the second light extraction layer 20.

[0061] In this embodiment, the emission wavelength of the third light-emitting element 93 (e.g., a red light-emitting element) is greater than that of the second light-emitting element 92 (e.g., a green light-emitting element), and the emission wavelength of the second light-emitting element 92 is greater than that of the first light-emitting element 91 (e.g., a blue light-emitting element). The first light-emitting element 91 has the shortest emission wavelength and requires the smallest constructive optical thickness. Therefore, only a small number of dimming layers (e.g., a single dimming layer or a combination of few dimming layers) are needed to achieve the optimal interference peak, while avoiding extinction absorption caused by excessive film thickness. The emission wavelengths of the second light-emitting element 92 and the third light-emitting element 93 are longer, requiring a larger optical thickness. By setting the second light extraction layer 20 and the third light extraction layer 30 to the same number of multi-layer dimming layers (e.g., both are set to a 5-layer structure with alternating low-refractive-index and high-refractive-index layers), the total optical thickness of both is increased synchronously, matching the long-wavelength constructive interference condition.

[0062] If the third light-emitting element 93 and the second light-emitting element 92 use the same single-layer or fewer-layer dimming layer as the first light-emitting element 91, their optical microcavity path may be insufficient, which may cause the interference peak to deviate from the main peak of the emission spectrum. In this embodiment, the number of dimming layers corresponding to the second light-emitting element 92 and the third light-emitting element 93 is increased and kept consistent, which can provide sufficient interference phase compensation for medium and long wavelengths, eliminate the microcavity undermatch between the second light-emitting element 92 and the third light-emitting element 93, and help improve the external quantum efficiency and color purity of the light emitted by the second light-emitting element 92 and the third light-emitting element 93.

[0063] Theoretically, if three light extraction layers with different numbers of layers / materials are independently customized for the three wavelength light-emitting elements, three independent mask evaporation processes are required. This solution simplifies and unifies the number of dimming layers corresponding to the third light-emitting element 93 and the second light-emitting element 92. The light extraction layer structures of the third light-emitting element 93 and the second light-emitting element 92 can share the same evaporation mask (or share some evaporation steps under the same mask opening), reducing the original three mask processes to two, significantly saving mask process costs, reducing screen changing and positioning time, and greatly improving panel production line yield.

[0064] If the number of dimming layers above different color light-emitting elements is not the same, there will be a large number of steep steps above the pixel definition layer. By unifying the number of dimming layers of the third light-emitting element 93 and the second light-emitting element 92, the height difference of the top step of the entire display panel is reduced from a complex 3 levels to 2 levels (low-layer area and high-layer area). This reduces the abrupt change in film thickness at the pixel junction, significantly releases the internal stress during thin-film encapsulation deposition, and avoids microcracks in the inorganic encapsulation layer caused by excessively steep steps.

[0065] Considering the significant spectral energy weight of red and green light in the display image, the same number of refractive index modulation layers are used to ensure that the phase shift patterns of red and green light emitted at an angle are consistent. When viewing the display screen at a wide angle, the brightness attenuation and wavelength drift of red and green light remain synchronized, effectively avoiding the reddish or greenish bias that occurs after color mixing, and significantly improving the color temperature stability of the entire viewing angle.

[0066] Please continue to refer to this. Figure 10 In one optional embodiment of this disclosure, the third light extraction layer 30 includes at least one first dimming layer 101 and at least one second dimming layer 102; the second dimming layer 102 in the first light extraction layer 10, the third dimming layer 203 in the second light extraction layer 20, and the second dimming layer 102 in the third light extraction layer 30 have the same thickness. That is, the thickness of the high-refractive-index dimming layer in the region where the three types of light-emitting elements 90 are located is equal.

[0067] In the vapor deposition production of display panels, high-refractive-index materials typically require pixel-level alignment vapor deposition using fine masks to control different thicknesses for different pixels. If the high-refractive-index layer thicknesses corresponding to the three light-emitting elements 90 are different, frequent mask changes / alignments are required for each vapor deposition. This embodiment designs the high-refractive-index layer thicknesses of the light extraction layers corresponding to the three light-emitting elements 90 to be exactly the same, allowing the high-refractive-index material to be uniformly vapor-deposited across the entire screen in a single operation using a single mask. This eliminates the cumbersome steps of independently vapor-depositing the three high-refractive-index layers, eliminates the switching and registration waiting time for fine masks, greatly shortens the production cycle, and reduces material waste and mask registration costs.

[0068] Considering that partial evaporation of the photomask can easily lead to uneven film thickness at pixel edges due to photomask deformation, shadow effects, or alignment deviations, causing color shifts or efficiency fluctuations between different light-emitting elements, this embodiment directly eliminates the thickness steps and shadow differences of the high-refractive-index layer at the pixel edges because the high-refractive-index layer thickness is consistent across the entire screen. This significantly reduces the sensitivity of the process to photomask alignment accuracy, significantly improves the uniformity and reproducibility of the evaporated film thickness, and enhances the overall yield of display panels in large-area mass production.

[0069] In this embodiment, although the thickness of the high-refractive-index layer in the light extraction layer is fixed and uniform, differentiated optical phase compensation can be provided for light-emitting elements of different wavelengths by adjusting the thickness or number of low-refractive-index layers (first dimming layer 101). While enjoying the extremely low production cost brought by full-screen through-plating, it is still possible to achieve near-optimal microcavity interference constructive conditions for light-emitting elements of different wavelengths through independent fine-tuning of the low-refractive-index layer, thus achieving the dual benefits of optimal process cost and improved light emission efficiency.

[0070] It should be noted that in the foregoing embodiments, when the light extraction layer includes a multi-layer dimming layer with alternating high and low refractive index layers, the layer in contact with the cathode 90-3 can be either a high refractive index layer or a low refractive index layer, and this disclosure does not limit this.

[0071] Please continue to refer to this. Figure 10 In one optional embodiment of this disclosure, the refractive index of the first dimming layer 101 mentioned in this disclosure ranges from 1.45 to 1.65, and the refractive indexes of the second dimming layer 102 and the third dimming layer 203 range from 2.0 to 2.2.

[0072] The interference and reflection amplitudes of optical thin films directly depend on the refractive index difference between adjacent media. The greater the refractive index difference, the stronger the intensity of coherent reflected light generated at the interface, and the more significant the ability to control the phase of the microcavity. By controlling the refractive index of the low-refractive layer at 1.45~1.65 and raising the refractive index of the high-refractive layer to 2.0~2.2, a large refractive index step difference (up to 0.75) is formed. This high-contrast refractive index combination can provide extremely strong coherent interference gain with extremely thin film thickness, extracting most of the total internal reflection light trapped inside the device and significantly improving the external quantum efficiency.

[0073] There is a significant optical impedance mismatch between the translucent metal cathode (typically with a high refractive index) and the thin-film encapsulation layer (such as an inorganic encapsulation layer with a refractive index typically around 1.7 to 1.8) in the display panel. When the high-refractive-index layer (approximately 2.0 to 2.2 refractive index) in the light extraction layer is placed close to the cathode 90-3 or serves as the master modulation layer, it can effectively extend the optical path and match the microcavity compatibility point of the light-emitting layer. The low-refractive-index layer (1.45 to 1.65) serves as a transition or top layer, and can construct a function similar to an antireflection / reflection coating between the high-refractive-index layer and the encapsulation layer above, breaking the critical angle limitation of total internal reflection between the high-refractive-index medium and the encapsulation interface, and significantly reducing interface total internal reflection loss.

[0074] In actual mass production, organic materials with a refractive index higher than 2.2 typically have extremely large molecular weights, require high thermal evaporation temperatures, and are prone to decomposition; while materials with a refractive index lower than 1.45 often have poor mechanical strength or are prone to moisture absorption. Therefore, setting the refractive index range to 1.45~1.65 and 2.0~2.2, materials within this range have moderate evaporation temperatures, low risk of thermal degradation, good film-forming properties and adhesion, and are not prone to crystallization or particle defects; thus, they balance ideal optical performance with the feasibility of large-area evaporation processes and high yield.

[0075] Please refer to this appropriately. Figure 3 In one optional embodiment of this disclosure, the thickness of the first dimming layer 101 is H1, the thickness of the second dimming layer 102 is H2, and the thickness of the third dimming layer 203 is H3, wherein H3 ≥ H2 ≥ k × H1, and 1 < k ≤ 4. It should be noted that, except... Figure 3 Apart from this embodiment, the thicknesses of the first dimming layer 101, the second dimming layer 102, and the third dimming layer 203 in other embodiments can be set with reference to this embodiment.

[0076] In this embodiment, the thickness of the high refractive index dimming layer is at least k times the thickness of the low refractive index dimming layer. For the third dimming layer 203 with a longer emission wavelength (such as red light), its thickness is not less than the thickness of the second dimming layer 102.

[0077] In the interference model of the multi-layer dimming layer, the high refractive index layer mainly functions to provide a sufficient optical path to achieve constructive microcavity interference, which requires a relatively large physical thickness; while the low refractive index layer is mainly used to introduce a refractive index step difference and an anti-reflection interface, and an excessively thick layer will cause light extinction and phase misalignment. The thickness ratio of the high refractive index layer to the low refractive index layer is limited to 1<k≤4 (for example, when H1 is 150Å, H2 is in the range of 200Å to 600Å). When k>1, it is ensured that the high refractive index layer occupies a dominant position, so that the core energy for interference enhancement will not be diluted by the low refractive index layer; when k≤4, high-order interference destructive or spectral broadening at a large angle that may be caused by an excessively thick high refractive index layer is restricted, and the optical interference of the entire waveband is precisely locked within the strongest light output gain window.

[0078] According to the microcavity constructive interference formula, the longer the light wavelength (for example, the wavelength of red light is greater than that of blue / green light), the larger the required optical thickness of the light extraction layer. By defining H3≥H2, the physical thickness of the third dimming layer 203 corresponding to the long-wavelength light-emitting element 90 can increase synchronously with the wavelength, which precisely compensates for the defect that long-wavelength light cannot achieve complete constructive interference in a relatively thin dimming layer, and greatly improves the external quantum efficiency of red light and long-wavelength bands.

[0079] Low refractive index materials have a high vapor deposition rate but are sensitive to the total thickness, while high refractive index materials have a slow film formation rate but determine the main optical gain. In this embodiment, by limiting k≤4, blindly stacking an excessively large thickness of the high refractive index layer is avoided (the upper limit of the thickness of the film layer that takes the longest vapor deposition time is controlled). On the premise of obtaining high light extraction efficiency, the vapor deposition time of high refractive index materials is greatly shortened, the cost of vapor deposition materials is reduced, and the production tact for large-area mass production of display panels is improved.

[0080] If the thickness ratio of the light extraction layers 000 corresponding to adjacent light-emitting elements 90 is excessively large (for example, k>4), the film thickness step difference at the edge of the pixel opening will be excessively steep. By constraining the thickness proportional coefficient k to an upper limit of 4, the thickness variation between the light-emitting elements 90 of different colors and the multi-layer dimming layer falls within a gentle gradient range. This eliminates the internal stress concentration caused by local abrupt change of film thickness, avoids cracking of the vapor-deposited film layer, provides a gentle and flat growth substrate for subsequent thin film encapsulation, and improves the moisture-proof sealing performance and yield of the panel.

[0081] Optionally, 2≤k≤3, or 1.2≤k≤3.5, or 1.8≤k≤3.6, etc., the present disclosure does not make specific limitations in this regard.

[0082] Please continue to refer to Figure 3 , in an optional implementation manner of the present disclosure, the thickness H1 of the first dimming layer 101 satisfies: 50Å≤H1≤200Å.

[0083] Considering that when H1 < 50 Å, in the thermal evaporation process, a film thickness of less than 50 Å (only about a few molecular layers thick) is prone to discontinuous film formation, pinholes, or local defects due to island-like growth. A low-refractive-index layer that is too thin cannot form an effective extinction interference and phase coherence interface, nor can it break the total internal reflection barrier between the high-refractive-index layer and the overlying dielectric, resulting in a significant decrease in light extraction efficiency gain. It is also difficult to effectively isolate the cathode 90-3 from the high-refractive-index material, making it difficult to prevent interfacial micro-stress and molecular interdiffusion. Therefore, setting H1 ≥ 50 Å ensures that the low-refractive-index material can form a flat, continuous, and pinhole-free uniform ultrathin film layer. This establishes a stable high-low refractive-index optical interface and provides a good interface buffering effect, improving the physical stability and yield of multilayer coatings.

[0084] Considering that when H1 > 200 Å, the optical path length of the low-refractive-index medium is too long, disrupting the constructive interference condition of the main microcavity (primarily high-refractive-index layer), leading to increased destructive interference and a significant loss in light extraction efficiency. An excessively thick low-refractive-index layer introduces an excessive phase difference at oblique viewing angles, causing severe spectral peak shift at side-view angles and exacerbating image quality degradation. Increasing the deposition thickness of the low-refractive-index material unnecessarily directly lengthens the deposition time, increasing material consumption and production costs. Therefore, setting H1 ≤ 200 Å allows the low-refractive-index layer to focus on anti-reflection and phase fine-tuning functions without diluting the constructive interference effect of the high-refractive-index master layer. This precisely locks in the optimal constructive interference phase window, achieving an extremely high external quantum efficiency. Furthermore, H1 ≤ 200 Å avoids excessive optical path differences from large-angle oblique incidence, effectively suppressing spectral broadening and peak shift at large angles, and significantly improving viewpoint spectral distortion at large viewing angles. While achieving excellent optical performance, the coating thickness was greatly controlled, the evaporation process time was shortened, the consumption of low-refractive materials was reduced, and the production capacity and production cost were optimized.

[0085] Alternatively, 60Å≤H1≤150Å, or 100Å≤H1≤180Å, or 90Å≤H1≤120Å, etc., are not specifically limited in this disclosure.

[0086] Please continue to refer to this. Figure 10 In one optional embodiment of this disclosure, the total physical thickness of the third light extraction layer 30 is H30, the total physical thickness of the second light extraction layer 20 is H20, and the total physical thickness of the first light extraction layer 10 is H10; wherein, the thickness ratio of the third light extraction layer 30 to the second light extraction layer 20 satisfies: 1≤H30 / H20≤2; the thickness ratio of the third light extraction layer 30 to the first light extraction layer 10 satisfies: 1≤H30 / H10≤2.

[0087] Optionally, the total physical thickness H10 of the first light extraction layer 10 ranges from 400 Å to 800 Å; the total physical thickness H20 of the second light extraction layer 20 ranges from 600 Å to 1100 Å; and the total physical thickness H30 of the third light extraction layer 30 ranges from 700 Å to 1300 Å.

[0088] By limiting the total thickness of the light extraction layer 000 of the three light-emitting elements 90 to the above-mentioned matching ratio range, the microcavity interference constructive condition of the main peak wavelengths of the three primary colors of red, green and blue is precisely matched. Without destroying the uniformity of the emitted light spot, the positive external quantum efficiency of the three colors of the first light-emitting element 91, the second light-emitting element 92 and the third light-emitting element 93 reaches the peak simultaneously, avoiding color drift caused by undermatch or overmatch of monochromatic interference.

[0089] Figure 11 As shown Figure 1 Please refer to the schematic diagram of another film layer of the three light-emitting elements 90 in the central display panel. Figure 11 In one optional embodiment of this disclosure, the display panel further includes an encapsulation layer 70 located on the side of the light extraction layer 000 facing away from the substrate 00. The encapsulation layer 70 includes a first inorganic encapsulation layer 71 covering the light extraction layer. The refractive index of the first inorganic encapsulation layer 71 on the side of different light-emitting elements 90 facing away from the substrate 00 is equal. That is, the entire screen uses a first inorganic encapsulation layer 71 with a single refractive index and uniform coverage.

[0090] The first inorganic encapsulation layer 71, as the first line of defense for thin-film encapsulation close to the light-emitting device, directly determines its water and oxygen barrier capability through its density and compactness. The refractive index is usually closely related to the film layer's density (for example, silicon nitride films with high refractive indices have higher density). By unifying the refractive index of the first inorganic encapsulation layer 71 in the regions where the three different light-emitting elements 90 are located (e.g., controlling it within a specific medium range of 1.7 to 1.85), it ensures that the film layer has uniform and dense water and oxygen barrier capability across the entire screen. Furthermore, by fixing the optical refractive index of the interface with the underlying multilayer / single-layer dimming layer, it reduces parasitic reflections and light loss at the interface between the dimming layer and the inorganic encapsulation layer.

[0091] Depositing inorganic encapsulation layers with different refractive indices for different light-emitting elements 90 requires multi-step, zoned deposition using masks or repeated adjustments to the reactive gas ratio. This not only makes the encapsulation process extremely complex but also introduces microscopic interface defects. A first inorganic encapsulation layer 71 with a uniform refractive index across the entire screen allows for a single, large-area continuous deposition process. This completely eliminates the mask registration and zoned adjustments required in thin-film encapsulation processes, significantly shortens the encapsulation process time, eliminates particulate contamination defects introduced by multiple depositions, and significantly improves the yield and production efficiency of large-area mass production.

[0092] In this embodiment, the first inorganic encapsulation layer 71, with a uniform refractive index across the entire screen, provides a completely consistent and stable upper boundary optical environment for the light extraction layers in each region of the display panel. This reduces the physical variable dimension of the dimming layer design, allowing designers to focus solely on optimizing the thickness and number of layers of the dimming layer itself. This enables precise fine-tuning of the microcavity interference constructive point and viewpoint color deviation of each monochromatic light, which helps eliminate the problem of uneven color across the entire screen caused by fluctuations in the refractive index of the encapsulation layer.

[0093] Please continue to refer to this. Figure 11 In one optional embodiment of this disclosure, the first light extraction layer 10 includes at least one first dimming layer 101 and at least one second dimming layer 102. The first dimming layer 101 and the second dimming layer 102 are stacked along the thickness direction of the display panel. The refractive index of the first dimming layer 101 is less than the refractive index of the second dimming layer 102. The refractive index of the first inorganic encapsulation layer 71 is greater than the refractive index of the first dimming layer 101 and less than the refractive index of the second dimming layer 102.

[0094] If a high-refractive-index dimming layer directly contacts the interface of a medium with a low refractive index, the large abrupt change in refractive index will result in a small critical angle for total internal reflection. A large amount of obliquely propagating light will undergo total internal reflection at the interface, becoming trapped inside the device and lost in waveguide mode. By introducing a low-refractive-index first dimming layer 101 (e.g., 1.45~1.65) and a first inorganic encapsulation layer 71 with a medium refractive index (e.g., 1.7~1.85), when light exits from the second dimming layer 102 (high-refractive-index layer), it passes through an optical buffer gradient consisting of a high-refractive-index layer, a low-refractive-index layer, and a first inorganic encapsulation layer with a medium refractive index, or vice versa. This step-like refractive index transition significantly increases the critical angle for total internal reflection at the interface, extracting more light that was originally trapped at large angles and greatly improving the external quantum efficiency of the display panel.

[0095] The Fresnel reflectivity of the interface between two media is proportional to the difference in refractive index between them. The greater the refractive index difference, the more intense the interface reflection, which easily generates optical stray light and destructive interference. By designing the refractive index of the first inorganic encapsulation layer 71 between the low-refractive-index layer and the high-refractive-index layer, excellent optical impedance matching is achieved. As an intermediate refractive index medium, the first inorganic encapsulation layer 71 reduces the reflection amplitude at the interface between the high-refractive-index layer and the upper inorganic encapsulation layer, constructing a highly efficient anti-reflection / anti-reflection thin film interference effect, reducing parasitic reflection losses, and simultaneously improving the light output in both the normal and oblique directions.

[0096] When the refractive index of the first inorganic encapsulation layer 71 is too high (higher than the high refractive index layer in the dimming layer) or too low (lower than the low refractive index layer in the dimming layer), the optical path difference of light rays emitted at large angles will fluctuate drastically, causing spectral shift and viewing angle distortion of the display screen at side viewing angles. The refractive index of the centrally located first inorganic encapsulation layer 71 constrains the phase transition range of the high-low refractive layer interface, making the phase difference change of light rays emitted at large angles smoother. This effectively suppresses the drift of the central emission wavelength at large viewing angles, ensuring color fidelity and image quality stability at side viewing angles.

[0097] Figure 12 As shown Figure 1 The diagram shows another layer of the three light-emitting elements 90 in the display panel. Optionally, the encapsulation layer 70 also includes an organic encapsulation layer 72 and a second inorganic encapsulation layer 73. The organic encapsulation layer 72 is located on the side of the first inorganic encapsulation layer 71 facing away from the substrate 00, and the second inorganic encapsulation layer 73 is located on the side of the organic encapsulation layer facing away from the substrate 00. Optionally, the second inorganic encapsulation layer 73 is typically made of deposited silicon nitride or aluminum oxide. It is mainly used to isolate water and oxygen, and also serves as the last optical medium environment of the refractive index control system of the dimming layer. The organic encapsulation layer 72 is typically deposited using an inkjet printing process with an acrylic organic resin. The film thickness is relatively thick (micrometer level). It is used to fill the pixel step difference caused by the underlying anode 90-1, pixel definition layer 40, and light extraction layers with different numbers of layers, and to encapsulate the particles generated during the evaporation process. The second inorganic encapsulation layer 73 is again deposited with dense inorganic material, forming an interface barrier with the first inorganic encapsulation layer 71, which greatly extends the path of water and oxygen through microscopic defects, thereby improving the encapsulation reliability of the light-emitting elements 90.

[0098] Based on the same inventive concept, this disclosure also provides a display device. Figure 13 The diagram shown is a planar structural schematic of a display device 200 provided in an embodiment of this disclosure. Please refer to it. Figure 13 The display device 200 includes the display panel 100 provided in any of the foregoing embodiments of the present disclosure.

[0099] The display device 200 provided in this embodiment can be any electronic device with display function, such as a touch screen, mobile phone, tablet computer, laptop computer, e-reader, or television. It can also be a large-size splicing display device, such as a command center screen. The display device 200 provided in this embodiment has the beneficial effects of the display panel 100 provided in this embodiment. For details, please refer to the specific descriptions of the display module in the above embodiments. These descriptions will not be repeated here.

[0100] Understandably, attached Figure 13The rounded rectangle structure is used as an example to illustrate one shape of the display device 200. In some other embodiments of this disclosure, the display device 200 may also be circular, elliptical, fan-shaped or any other feasible shape, and this disclosure does not specifically limit it.

[0101] It should be noted that, in this document, relational terms such as "first" and "second" are used merely to distinguish one entity or operation from another, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Furthermore, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Without further limitations, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes said element.

[0102] The above description is merely a specific embodiment of this disclosure, enabling those skilled in the art to understand or implement it. Various modifications to these embodiments will be readily apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of this disclosure. Therefore, this disclosure is not to be limited to the embodiments described herein, but is to be accorded the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A display panel, characterized in that, include: Substrate; A light-emitting element is disposed on one side of the substrate, including a first light-emitting element and a second light-emitting element, wherein the light emission wavelength of the first light-emitting element is smaller than the light emission wavelength of the second light-emitting element; The light extraction layer includes a first light extraction layer and a second light extraction layer, wherein the first light extraction layer is located on the side of the first light-emitting element away from the substrate, and the second light extraction layer is located on the side of the second light-emitting element away from the substrate; At least one of the first light extraction layer and the second light extraction layer includes at least two dimming layers, and the number of dimming layers included in the first light extraction layer and the second light extraction layer is different, and / or the thickness of the first light extraction layer and the second light extraction layer is different.

2. The display panel according to claim 1, characterized in that, The display panel includes a pixel definition layer, which includes multiple pixel openings. Different light-emitting elements are located in different pixel openings. The light extraction layer is located in the pixel opening corresponding to the light-emitting element and extends to the periphery of the pixel opening.

3. The display panel according to claim 1, characterized in that, The first light extraction layer includes at least one first dimming layer and at least one second dimming layer, which are stacked along the thickness direction of the display panel. The refractive index of the first dimming layer is less than that of the second dimming layer. The second light extraction layer includes a third dimming layer, which has a refractive index greater than or equal to that of the second dimming layer.

4. The display panel according to claim 3, characterized in that, The thickness of the first dimming layer is less than the thickness of the second dimming layer, and the thickness of the third dimming layer is greater than the thickness of the second dimming layer.

5. The display panel according to claim 3, characterized in that, The first light extraction layer includes two first dimming layers and one second dimming layer. Along the thickness direction of the display panel, the first dimming layer is located on both sides of the second dimming layer.

6. The display panel according to claim 3, characterized in that, The second light extraction layer includes only one third dimming layer; or, the second light extraction layer is a multi-layer structure, and the second light extraction layer also includes at least one first dimming layer, with the first dimming layer and the third dimming layer stacked along the thickness direction of the display panel.

7. The display panel according to claim 3, characterized in that, The second light extraction layer has a multi-layer structure, and the second light extraction layer further includes at least one of the first dimming layers; the number of dimming layers included in the second light extraction layer is equal to the number of dimming layers included in the first light extraction layer.

8. The display panel according to claim 3, characterized in that, The second light extraction layer has a multi-layer structure, and the second light extraction layer further includes at least one layer of the first dimming layer; the number of dimming layers included in the second light extraction layer is greater than the number of dimming layers included in the first light extraction layer.

9. The display panel according to claim 6 or 7, characterized in that, The light-emitting element further includes a third light-emitting element, and the light extraction layer further includes a third light extraction layer disposed on the side of the third light-emitting element away from the substrate. The emission wavelength of the third light-emitting element is greater than the emission wavelength of the second light-emitting element. The number of dimming layers in the third light extraction layer is the same as the number of dimming layers in the first light extraction layer.

10. The display panel according to claim 8, characterized in that, The light-emitting element further includes a third light-emitting element, and the light extraction layer further includes a third light extraction layer disposed on the side of the third light-emitting element away from the substrate. The emission wavelength of the third light-emitting element is greater than the emission wavelength of the second light-emitting element. The number of dimming layers included in the third light extraction layer is greater than the number of dimming layers included in the first light extraction layer, and the number of dimming layers included in the third light extraction layer is equal to the number of dimming layers included in the second light extraction layer.

11. The display panel according to claim 10, characterized in that, The third light extraction layer includes at least one first dimming layer and at least one second dimming layer; the second dimming layer in the first light extraction layer, the third dimming layer in the second light extraction layer, and the second dimming layer in the third light extraction layer have the same thickness.

12. The display panel according to claim 3, characterized in that, The refractive index of the first dimming layer is in the range of 1.45 to 1.65, and the refractive index of the second dimming layer and the third dimming layer is in the range of 2.0 to 2.

2.

13. The display panel according to claim 3, characterized in that, The thickness of the first dimming layer is H1, the thickness of the second dimming layer is H2, and the thickness of the third dimming layer is H3, wherein H3≥H2≥k×H1, and 1<k≤4.

14. The display panel according to claim 13, characterized in that, 50Å≤H1≤200Å。 15. The display panel according to claim 1, characterized in that, The display panel further includes an encapsulation layer located on the side of the light extraction layer facing away from the substrate; the encapsulation layer includes a first inorganic encapsulation layer covering the light extraction layer, and the refractive index of the first inorganic encapsulation layer on the side of the light-emitting element facing away from the substrate is equal.

16. The display panel according to claim 15, characterized in that, The first light extraction layer includes at least one first dimming layer and at least one second dimming layer, the first dimming layer and the second dimming layer are stacked along the thickness direction of the display panel, and the refractive index of the first dimming layer is less than the refractive index of the second dimming layer; The refractive index of the first inorganic encapsulation layer is greater than that of the first dimming layer and less than that of the second dimming layer.

17. A display device, characterized in that, Includes the display panel described in any one of claims 1 to 16.