Semiconductor structure and its preparation method
By combining photolithography and dry etching with plasma-like ashing and ICP etching equipment for shaping processes, the problems of insufficient and uneven etching of hard mask layers in semiconductor manufacturing have been solved, significantly improving the morphology of high aspect ratio trenches or vias and enhancing processing accuracy and quality.
Patent Information
- Application Number
- CN202610911527.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-06-23
- Publication Date
- 2026-11-17
AI Technical Summary
In semiconductor manufacturing, it is difficult to control the morphology of high aspect ratio trenches or vias, especially due to insufficient etching of the hard mask layer and uneven top dimensions, resulting in poor morphology.
After forming the initial hard mask opening pattern using photolithography and dry etching processes, the initial hard mask opening pattern is modified using a plasma-like ashing process to form a patterned hard mask layer. The sidewalls and bottom are then modified using an ICP etching device to ensure the uniformity of the hard mask opening pattern and the morphological quality of the holes and grooves.
It significantly improves the top size uniformity of hard mask aperture patterns and the morphology of holes and grooves, solves the problems of insufficient and uneven etching, and improves the processing accuracy and quality of semiconductor structures.
Smart Images

Figure CN123124688A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of semiconductor technology, and more specifically to a semiconductor structure and its fabrication method. Background Technology
[0002] Semiconductors have been developing for nearly a century. However, due to the limitations of Moore's Law, it has become extremely difficult to further reduce the critical dimension (CD) of semiconductors in a two-dimensional plane. Therefore, semiconductor products such as NAND flash and DRAM (Dynamic Random Access Memory) have gradually transformed from two-dimensional planar structures to three-dimensional structures.
[0003] The development of three-dimensional structures has led to a demand for trenches or vias with high aspect ratios (30:1 to 100:1), making topographic control crucial. For dry etching, the increased complexity of the process makes topographic control of high aspect ratio trenches or vias even more challenging. For example, in high aspect ratio etching, the complexity of the process places stringent requirements on the hard mask layer, resulting in a relatively small process window. This can lead to insufficient etching of the opening pattern and / or uneven top dimensions of the opening pattern within the hard mask layer. Consequently, trenches or vias formed using this hard mask layer often exhibit poor topographic characteristics.
[0004] Therefore, improvements are needed to at least partially address the aforementioned problems. Summary of the Invention
[0005] The summary section introduces a series of simplified concepts, which will be further explained in detail in the detailed description section. The summary section of this invention is not intended to limit the key features and essential technical features of the claimed technical solution, nor is it intended to determine the scope of protection of the claimed technical solution.
[0006] To at least partially solve the above problems, according to a first aspect of the present invention, a method for fabricating a semiconductor structure is provided, comprising: S10: Provide an initial semiconductor structure, wherein the initial semiconductor structure includes a substrate, a plurality of landing portions on the substrate, an etchable layer above the landing portions, and a hard mask layer on the etchable layer, the landing portions are isolated from each other by an isolation layer, the top surface of the landing portions is flush with the top surface of the isolation layer, the etchable layer is a stacked structure of alternating layers, and the thickness of the hard mask layer is greater than or equal to 1 μm; S20: A plurality of initial hard mask opening patterns are formed in the hard mask layer using photolithography and dry etching processes. There is at least one instance of insufficient etching of the initial hard mask opening pattern and / or uneven top size of the initial hard mask opening pattern. The number of the initial hard mask opening patterns corresponds one-to-one with the number of the landing parts. S30: The initial hard mask opening pattern is modified by an etching device through a plasma-like ashing process to form a patterned hard mask layer with a plurality of hard mask opening patterns, wherein the top size uniformity of the hard mask opening pattern is greater than or equal to 95%, and the hard mask opening pattern exposes the layer to be etched. S40: Using the patterned hard mask layer as a mask, etch the layer to be etched to form an initial hole through the layer to be etched to expose the landing part.
[0007] For example, the material of the hard mask layer is amorphous carbon; The ashing gas used in the plasma-like ashing process is a mixture of hydrogen and inert gas, or a mixture of oxygen and inert gas.
[0008] For example, the flatness of the sidewall of the initial slot does not meet the preset requirements; After step S40, the preparation method further includes: S50: Remove the hard mask layer; S60: The sidewall of the initial hole groove is modified using a first shaping process so that the flatness of the sidewall of the initial hole groove meets the preset requirements. The first modification process is performed at least once, and the first modification process includes: S61: A first protective layer is deposited on the upper surface of the layer to be etched and the inner wall of the initial hole through a first deposition process; S62: The sidewalls of the holes in the layer to be etched are etched by an anisotropic first dry etching process; S63: Remove the first protective layer and etching byproducts by a first dry cleaning process.
[0009] For example, the first deposition process, the first dry etching process, and the first dry cleaning process are all performed using an ICP etching device; During the first dry etching process, the source power of the ICP etching equipment is greater than the bias power, and / or the bias power frequency of the ICP etching equipment is 13.56MHz.
[0010] For example, the first protective layer is a polymer layer or a silicon dioxide layer.
[0011] For example, the layer to be etched includes silicon dioxide layers and silicon nitride layers stacked alternately in a cycle; The landing section is made of aluminum oxide or tungsten. The bottom of the initial slot has a tapered opening; After step S40, the preparation method further includes: S70: Remove the hard mask layer; S80: The bottom of the initial groove is modified using a second shaping process to remove the tapered opening; The second shaping process is performed at least once, and the second shaping process includes: S81: A second protective layer is deposited on the upper surface of the layer to be etched and on the inner wall of the initial hole through a second deposition process; S82: The bottom of the holes in the layer to be etched is etched by an anisotropic second dry etching process; S83: Remove the second protective layer and etching byproducts by a second dry cleaning process.
[0012] For example, the second deposition process, the second dry etching process, and the second dry cleaning process are all performed using an ICP etching device; In the second dry etching process, the source power of the ICP etching equipment is less than the bias power, and / or the bias power frequency of the ICP etching equipment is 2MHz.
[0013] For example, the second protective layer is a polymer layer or a silicon dioxide layer.
[0014] For example, prior to step S70, the preparation method further includes: The etching byproducts at the bottom of the initial groove are removed by a third dry cleaning process; The cleaning gas used in the third dry cleaning process includes hydrogen and / or chlorine.
[0015] According to a second aspect of the present invention, a semiconductor structure is provided, which is prepared by the preparation method described above.
[0016] According to the semiconductor structure and its fabrication method of the present invention, after forming a plurality of initial hard mask opening patterns in the hard mask layer by photolithography and dry etching processes, the initial hard mask opening patterns are modified by a plasma-like ashing process using an etching device. This can effectively improve the phenomenon of insufficient etching of the initial hard mask opening patterns and / or the phenomenon of uneven top size of the initial hard mask opening patterns. Thus, the morphology of the initial holes formed by etching the layer to be etched using the hard mask layer as a mask can be significantly improved. Attached Figure Description
[0017] The following figures are included as part of this application for understanding the application. The figures illustrate embodiments of the application and their descriptions, serving to explain the apparatus and principles of the application. In the figures, Figure 1 This is a schematic flowchart of a method for fabricating a semiconductor structure according to an embodiment of this application; Figures 2A-2D This is a cross-sectional schematic diagram of the structure corresponding to each step of a method for fabricating a semiconductor structure according to an embodiment of this application; Figure 3 This is a cross-sectional schematic diagram of a semiconductor structure according to an embodiment of this application; Figure 4 This is a schematic flowchart of a method for fabricating a semiconductor structure according to an embodiment of this application; Figures 5A-5B This is a cross-sectional schematic diagram of the structure corresponding to each step of the method for fabricating a semiconductor structure according to an embodiment of this application; Figure 6 This is a flowchart illustrating the first modification process; Figure 7 This is a cross-sectional schematic diagram of a semiconductor structure according to an embodiment of this application; Figure 8 This is a schematic flowchart of a method for fabricating a semiconductor structure according to an embodiment of this application; Figures 9A-9B This is a cross-sectional schematic diagram of the structure corresponding to each step of the method for fabricating a semiconductor structure according to an embodiment of this application; Figure 10 This is a flowchart illustrating the second modification process.
[0018] Explanation of reference numerals in the attached figures: 100-Substrate, 200-Landing section, 300-Isolation layer, 400-Layer to be etched, 410-Silicon nitride layer, 420-Silicon dioxide layer, 430-Initial via, 500-Hard mask layer, 510-Initial hard mask opening pattern, 520-Hard mask opening pattern. Detailed Implementation
[0019] The following description provides numerous specific details to offer a more thorough understanding of this application. However, it will be apparent to those skilled in the art that this application can be practiced without one or more of these details. In other instances, certain technical features well-known in the art have not been described to avoid confusion with this application.
[0020] It should be understood that this application can be implemented in various forms and should not be construed as limited to the embodiments set forth herein. Rather, providing these embodiments will make the disclosure thorough and complete, and will fully convey the scope of this application to those skilled in the art. In the drawings, for clarity, the dimensions and relative dimensions of layers and regions may be exaggerated. The same reference numerals denote the same elements throughout.
[0021] It should be understood that although the terms first, second, third, etc., may be used to describe various elements, components, areas, layers, and / or parts, these elements, components, areas, layers, and / or parts should not be limited by these terms. These terms are only used to distinguish one element, component, area, layer, or part from another element, component, area, layer, or part. Therefore, without departing from the teachings of this application, the first element, component, area, layer, or part discussed below may be referred to as the second element, component, area, layer, or part.
[0022] Spatial relation terms such as "below," "under," "below," "under," "above," and "above" are used here for convenience to describe the relationship between one element or feature shown in the figure and other elements or features. It should be understood that, in addition to the orientation shown in the figure, spatial relation terms are intended to also include different orientations of devices in use and operation.
[0023] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the scope of this application. When used herein, the singular forms “a,” “an,” and “the” are also intended to include the plural forms unless the context clearly indicates otherwise. It should also be understood that the terms “comprising” and / or “including,” when used in this specification, identify the presence of the stated features, integers, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups. When used herein, the term “and / or” includes any and all combinations of the associated listed items.
[0024] Embodiments of the invention are described herein with reference to cross-sectional views that serve as schematic diagrams of preferred embodiments (and intermediate structures) of this application. Thus, variations in the shown shape are contemplated due to, for example, manufacturing techniques and / or tolerances. Therefore, embodiments of this application should not be limited to the specific shapes shown herein, but include shape deviations due to, for example, manufacturing processes. Consequently, the figures are substantially schematic, and their shapes are not intended to show the actual shape of the device and are not intended to limit the scope of this application.
[0025] See attached document Figure 1 An exemplary method for fabricating a semiconductor structure according to an embodiment of this application will be described, the method comprising the following steps: S10: Provide an initial semiconductor structure. The initial semiconductor structure includes a substrate, a plurality of landing portions on the substrate, an etchable layer above the landing portions, and a hard mask layer on the etchable layer. The landing portions are isolated from each other by an isolation layer. The top surface of the landing portions is flush with the top surface of the isolation layer. The etchable layer is a stacked structure with alternating layers. The thickness of the hard mask layer is greater than or equal to 1 μm.
[0026] S20: Several initial hard mask opening patterns are formed in the hard mask layer using photolithography and dry etching processes. At least one initial hard mask opening pattern exhibits insufficient etching and / or uneven top size of the initial hard mask opening pattern. The number of initial hard mask opening patterns corresponds one-to-one with the number of landing parts.
[0027] S30: The initial hard mask opening pattern is reshaped using an etching device and a plasma-like ashing process to form a patterned hard mask layer with several hard mask opening patterns. The top dimension uniformity of the hard mask opening pattern is greater than or equal to 95%, and the hard mask opening pattern exposes the layer to be etched.
[0028] S40: The layer to be etched is etched using a patterned hard mask layer as a mask to form an initial hole or groove that penetrates the layer to be etched and exposes the landing part.
[0029] According to the semiconductor structure fabrication method of the present application, after forming a plurality of initial hard mask opening patterns in the hard mask layer by photolithography and dry etching processes, the initial hard mask opening patterns are modified by plasma-like ashing process using etching equipment. This can effectively improve the phenomenon of insufficient etching of the initial hard mask opening patterns and / or the phenomenon of uneven top size of the initial hard mask opening patterns. Thus, the morphology of the initial hole and groove formed by etching the layer to be etched with the hard mask layer as a mask can be significantly improved.
[0030] The following is a reference to the appendix. Figures 2A-2D The method for fabricating a semiconductor structure according to an embodiment of this application (i.e., steps S10-S40 described above) will be described in detail below.
[0031] In step S10, see Appendix Figure 2A This provides an initial semiconductor structure. The initial semiconductor structure includes a substrate 100, a plurality of landing portions 200 on the substrate 100, an etchable layer 400 above the landing portions 200, and a hard mask layer 500 on the etchable layer 400. The landing portions 200 are isolated from each other by an isolation layer 300, the top surface of the landing portions 200 is flush with the top surface of the isolation layer 300, and the etchable layer 400 is located on both the landing portions 200 and the isolation layer 300. The etchable layer 400 is a stacked structure with alternating layers. The thickness of the hard mask layer 500 is greater than or equal to 1 μm.
[0032] For example, substrate 100 may be a silicon substrate. In some other embodiments, substrate 100 may also include at least one of the following materials: Si, Ge, SiGe, SiC, SiGeC, InAs, GaAs, InP, InGaAs, or other III / V compound semiconductors. For example, the layer to be etched 400 may include alternating stacked silicon dioxide layers 420 and silicon nitride layers 410, and the bottom and top layers of the stacked structure are both oxide layers (silicon dioxide layer 420). For example, the isolation layer 300 may be made of silicon oxide or silicon nitride. For example, the mask layer may be made of materials including, but not limited to, amorphous carbon. For example, the landing portion 200 may be made of materials including, but not limited to, aluminum oxide, tungsten, etc., and a plurality of landing portions 200 located on substrate 100 may be arranged in an array, for example, in a rectangular array.
[0033] In step S20, see Appendix Figure 2B A plurality of initial hard mask opening patterns 510 are formed in the hard mask layer 500 using photolithography and dry etching processes. That is, a photoresist layer (not shown in the figure) is first formed on the hard mask layer 500 using a coating process such as spin coating; then, the photoresist layer is patterned using photolithography, wherein the patterned photoresist layer has a plurality of openings, the number of which corresponds one-to-one with the number of landing portions 200, and is oriented in the thickness direction of the substrate 100 (i.e.,...). Figure 2B On the top and bottom squares, the center of each opening is aligned with the center of each landing part 200; then, using the patterned photoresist layer as a mask, the hard mask layer 500 is etched by a dry etching process (i.e., anisotropic dry etching process) to form a number of initial hard mask opening patterns 510 in the hard mask layer 500, the number of initial hard mask opening patterns 510 corresponding one-to-one with the number of landing parts 200; then, the photoresist layer is removed.
[0034] In this embodiment, because the hard mask layer 500 is relatively thick (greater than 1 μm), at least one of the initial hard mask opening patterns 510 formed exhibits insufficient etching (i.e., the etched opening pattern does not expose the layer 400 to be etched, such as...). Figure 2BAs shown at point A), and / or, there is an uneven top size of the initial hard mask opening pattern 510 (for example, when the initial hard mask opening pattern 510 is circular in a top view, the top apertures of multiple initial hard mask opening patterns 510 are of different sizes). The above phenomenon occurs partly because the hard mask layer material reacts with the etching gas during the etching process to generate byproducts that are difficult to remove, which remain on the sidewalls and bottom of the initial hard mask opening pattern 510; and partly because a certain amount of loose hard mask material remains in the initial hard mask opening pattern 510 (that is, hard mask material that was not completely etched through during dry etching, which is loose residual carbon in this embodiment).
[0035] In step S30, see Appendix Figure 2CThe initial hard mask opening pattern 510 is reshaped using an etching equipment and a plasma-like ashing process to form a patterned hard mask layer 500 with several hard mask opening patterns. Plasma ashing, commonly known in the semiconductor industry as dry stripping, uses plasma (e.g., oxygen plasma) to oxidize and decompose organic mask materials such as photoresist (PR) into gaseous products such as CO2 and H2O, which are then removed by a vacuum system. This process typically requires a dedicated photoresist stripping machine. The plasma-like ashing process described in this application, however, is performed in an etching equipment. It uses plasma to decompose and remove residual byproducts and loose hard mask material in the initial hard mask opening pattern 510. While similar in principle to existing plasma ashing processes, it does not require a dedicated photoresist stripping machine; it is achieved through the piping integrated into the etching equipment. The initial hard mask opening pattern 510 is reshaped using an etching device and a plasma-like ashing process. Specifically, the etching device removes residual byproducts and loose hard mask material from the initial hard mask opening pattern 510 using a plasma-like ashing process, thereby reshaping the morphology of the initial hard mask opening pattern 510. This reshaping process forms a patterned hard mask layer 500 with several hard mask opening patterns 520. In the reshaped patterned hard mask layer 500, the top dimension uniformity of the hard mask opening patterns 520 is greater than or equal to 95% (thus significantly improving the uneven top dimension phenomenon of the initial hard mask opening pattern 510), and the hard mask opening patterns 520 expose the layer 400 to be etched (thus significantly improving the insufficient etching phenomenon of the initial hard mask opening pattern 510). Therefore, the hard mask opening pattern 520 formed after the reshaping process has a better morphology. For example, in some embodiments, a top dimension uniformity of 95% or more for the hard mask opening pattern 520 can mean that the number of hard mask opening patterns 520 whose critical dimensions (e.g., aperture) fall within a specified standard (preset range) is ≥95%. For example, in some embodiments, a top dimension uniformity of 95% or more for the hard mask opening pattern 520 can also mean that the range of critical dimensions among all hard mask opening patterns 520 does not exceed 5% of the mean of the critical dimensions.
[0036] In this embodiment, the hard mask layer 500 is made of amorphous carbon. During the etching process, the hard mask layer 500 reacts with the etching gas to generate byproducts such as cross-linked fluorocarbon polymers, which remain on the sidewalls and bottom of the initial hard mask opening pattern 510. A certain amount of loose residual carbon will also remain in the initial hard mask opening pattern 510. The ashing gas used in the plasma-like ashing process is a mixture of hydrogen and inert gas (such as nitrogen). In the plasma-like ashing process, the ashing gas is excited by a radio frequency power supply to generate plasma, that is, to generate hydrogen-containing plasma. On the one hand, the hydrogen-containing plasma can break the cross-linking bonds (such as CC, CF, etc.) in the residual byproducts, decomposing the polymer into volatile small molecule hydrocarbons. On the other hand, the hydrogen-containing plasma can decompose and remove the loose residual carbon without easily affecting the dense amorphous carbon hard mask layer 500 (that is, it does not affect the hard mask layer 500 body). For example, the flow ratio of inert gas to hydrogen in the ashing process gas can be from 5:1 to 50:1, and the processing time of the plasma-like ashing process (the reaction time of hydrogen-containing plasma with byproducts and loose residual carbon) can be from 5s to 50s.
[0037] For example, in some other embodiments, the hard mask layer 500 is made of amorphous carbon, and the ashing gas used in the plasma-like ashing process is a mixture of oxygen and inert gas. In the plasma-like ashing process, the ashing gas is excited by a radio frequency power supply to generate plasma, that is, plasma containing oxygen free radicals. This plasma can oxidize byproducts (polymers) and loose carbon residues, generating gaseous small molecules to remove them. It should be noted that when the ashing gas is a mixture of oxygen and inert gas, the reaction rate and reaction time between the oxygen free radicals and the byproducts (polymers) and loose carbon residues need to be strictly and precisely controlled to avoid excessive decomposition and removal of the hard mask layer 500 during this process.
[0038] In step S40, see Appendix Figure 2D The patterned hard mask layer 500 is used as a mask to etch the layer 400 to be etched (using an anisotropic dry etching process) to form an initial via 430 that penetrates the layer 400 to expose the landing portion 200. The initial via 430 corresponds one-to-one with the landing portion 200. For example, the initial via 430 can be a via or a trench, depending on the shape of the hard mask opening pattern 520. For example, the initial via 430 is a via or trench with a high aspect ratio, which can be from 30:1 to 100:1.
[0039] In related technologies, after step S20, the hard mask layer 500 formed in step S20 is usually used directly as a mask to etch the layer 400 to be etched (by an anisotropic dry etching process) to form a hole (through hole or trench) that penetrates the layer 400 to be etched and exposes the landing part 200. Since the initial hard mask opening pattern 510 has a poor morphology (there is at least one initial hard mask opening pattern 510 that is not etched enough, and / or there is an uneven top size of the initial hard mask opening pattern 510), the hole formed by etching also has a poor morphology, such as not exposing the landing part 200, or having a large deviation in key dimensions.
[0040] In this embodiment, after step S20, the initial hard mask opening pattern 510 is first modified in step S30 to give the hard mask opening pattern 520 formed by the modification process a better morphology. Then, the patterned hard mask layer 500 formed in step S30 (that is, the hard mask layer 500 with the opening pattern having a better morphology) is used as a mask to etch the layer 400 to be etched to form an initial hole 430 that penetrates the layer 400 to be etched and exposes the landing portion 200. As a result, the initial hole 430 formed can have a better morphology (especially the top of the initial trench has a better morphology).
[0041] This completes the process steps of the semiconductor structure fabrication method according to an embodiment of this application. It is understood that this fabrication method may include other necessary steps before, during, or after the steps described above. The semiconductor structure formed through the above steps can subsequently be used to fabricate semiconductor devices such as memory, which will not be elaborated upon here.
[0042] For example, see Appendix Figure 3 In some embodiments, the flatness of the sidewalls of the initial slot 430 in the semiconductor structure formed by the above steps does not meet the preset requirements. For example, there is unevenness in some parts of the sidewalls (as shown in the attached figure). Figure 3 (As shown at point A in the diagram). In some other embodiments, the flatness of the sidewall of the initial slot 430 not meeting the preset requirements may also mean that the sidewall is not a smooth straight line but a continuous fine wave or sawtooth undulation, or that the surface roughness of the sidewall does not meet the preset requirements, or that other indicators used to characterize the flatness of the sidewall do not meet the preset requirements, etc. In this case, see Appendix Figure 4 Appendix Figures 5A-5B After step S40, the preparation method further includes: S50: Remove hard mask layer 500.
[0043] For details, please see the appendix. Figure 5AIn step S50, the hard mask layer 500 can be removed using a hard mask layer removal process such as plasma ashing. Removing the hard mask layer 500 can effectively avoid potential contamination and prevent it from affecting the normal operation of subsequent processes.
[0044] S60: The first shaping process is used to shape the sidewall of the initial hole groove 430 so that the flatness of the sidewall of the initial hole groove 430 meets the preset requirements.
[0045] For details, please see the appendix. Figure 5B In step S60, the sidewall of the initial hole 430 is modified using a first shaping process. That is, the uneven parts of the sidewall of the initial hole 430 are modified using the first shaping process to optimize the shape of the sidewall and make the flatness of the sidewall of the initial hole 430 meet the preset requirements. The first shaping process includes at least an etching process for the sidewall of the initial hole 430.
[0046] See appendix Figure 6 In this embodiment, the first shaping process includes: S61: A first protective layer is deposited on the upper surface of the layer to be etched 400 and the inner wall (including the sidewall and bottom of the initial hole 430) by a first deposition process.
[0047] Specifically, the first protective layer can be a polymer layer or a silicon dioxide layer. The polymer layer can be formed using a gas containing C and F, including but not limited to at least one of CH2F2, C4F6, CH4, and CH3F; the silicon dioxide layer can be formed using SiCl4 and O2. The first protective layer is primarily used to protect the top of the layer to be etched 400 and the exposed landing portion 200.
[0048] S62: The sidewalls of the holes in the etching layer 400 are etched using an anisotropic first dry etching process.
[0049] Specifically, in the anisotropic first dry etching process, the etching direction and angle (ejection direction and angle of plasma) can be adjusted by adjusting the etching parameters. Thus, in step S62, the sidewalls of the holes in the etching layer 400 can be etched in a targeted manner by the anisotropic first dry etching process to optimize the morphology of the sidewalls and improve their flatness.
[0050] S63: Remove the first protective layer and etching byproducts by the first dry cleaning process.
[0051] Specifically, in step S63, a specific gas can be introduced to generate plasma, which reacts with the first protective layer and etching byproducts to decompose and remove them, so as to carry out the next round of the first shaping process or subsequent processes.
[0052] The first modification process is performed at least once, and each time it is performed in the order of steps S61 to S63. For example, the first modification process can be performed 1 to 60 times.
[0053] For example, the first deposition process, the first dry etching process, and the first dry cleaning process are all performed using an ICP (Inductively Coupled Plasma) etching device. The ICP etching device uses high-density plasma to etch materials. Its core principle is to excite gas in the reaction chamber through an external radio frequency coil to form plasma. The plasma contains high-energy electrons, ions, and chemically active free radicals. Through a combination of chemical reaction and physical bombardment, the material is precisely removed. The plasma contains high-energy electrons, ions, and chemically active free radicals, and can also dissociate the precursor gas to generate active free radicals and ions, which are adsorbed, reacted, and solidified on the substrate surface to form a film.
[0054] For example, in step S61, the duration of the first deposition process can be 5s-10s. During the first deposition process, the source power (Wb, i.e., source power) of the ICP etching equipment can be 200W-2000W, and the bias power (Wb2, i.e., bias power) of the ICP etching equipment can be 0. CH2F2, C4F6, CH4, CH3F, and Ar gases can be introduced during the deposition process to form a polymer layer. The first deposition process can be an ALD (Atomic Layer Deposition) process or a CVD (Chemical Vapor Deposition) process performed in situ using an ICP etching equipment.
[0055] In step S62, that is, during the first dry etching process, the source power of the ICP etching equipment is greater than the bias power, and / or the bias power frequency of the ICP etching equipment is 13.56MHz. Specifically, the higher the source power of the ICP etching equipment and the lower the bias power, the closer it is to etching the sidewalls. Setting the source power to be greater than the bias power allows for better etching of the sidewalls. At the same time, setting the bias power frequency of the ICP etching equipment to 13.56MHz makes it easier to generate obliquely incident ions, achieving controllable sidewall micro-etching. For example, in step S62, the duration of the first dry etching process can be 5s-60s, the source power of the ICP etching equipment can be 1001W-5000W, the bias power of the ICP etching equipment can be 1000W, the bias power frequency can be 13.56MHz, and Cl2, CH2F2, C4F6, CH3F, and NF3 can be introduced during the etching process.
[0056] In step S63, the duration of the first dry cleaning process can be 5s-60s. During the first dry cleaning process, the source power of the ICP etching equipment can be 2000W-5000W, and the bias power of the ICP etching equipment can be 0. CH4 and O2 can be introduced during the cleaning process. O2 is excited by the radio frequency power supply to generate plasma containing oxygen free radicals, which can react with the polymer to generate gaseous products, while oxidizing residual hydrocarbon byproducts and eliminating potential sources of contamination; CH4 dissociates to generate CH4. x Free radicals react with polymers, reducing the degree of polymer crosslinking and making them easier to oxidize and peel off.
[0057] For example, see Appendix Figure 7 In some embodiments, the layer to be etched 400 includes alternating layers of silicon dioxide 420 and silicon nitride 410, and the landing portion 200 is made of aluminum oxide or tungsten. In the semiconductor structure formed by the above steps S10-S40, the initial trench 430 has a tapered opening (e.g., Figure 7 (As shown at point C). When the bottom of the initial groove 430 with a high aspect ratio consists of two completely different films, such as a silicon dioxide layer 420 and an aluminum oxide layer (tungsten layer) landing section 200, the bottom will form a constricted shape due to the non-volatility of the metal byproducts, i.e., a conical constriction, affecting the morphology of the bottom of the initial groove 430. In this case, see Appendix Figure 8 Appendix Figures 9A-9B After step S40, the preparation method further includes: S70: Remove hard mask layer 500.
[0058] For details, please see the appendix. Figure 9AIn step S70, the hard mask layer 500 can be removed using a hard mask layer removal process such as plasma ashing. Removing the hard mask layer 500 can effectively avoid potential contamination and prevent it from affecting the normal operation of subsequent processes.
[0059] S80: The bottom of the initial groove 430 is modified using a second shaping process to remove the tapered end.
[0060] For details, please see the appendix. Figure 9B In step S80, a second shaping process is used to shape the bottom of the initial hole groove 430. That is, the second shaping process is used to shape the tapered opening at the bottom of the initial hole groove 430 to optimize the morphology of the bottom of the initial hole groove 430. The second shaping process includes at least an etching process for the tapered opening at the bottom of the initial hole groove 430.
[0061] See appendix Figure 10 In this embodiment, the second shaping process includes: S81: A second protective layer is deposited on the upper surface of the layer to be etched 400 and the inner wall (including the sidewall and bottom of the initial hole 430) by a second deposition process.
[0062] Specifically, the second protective layer can be a polymer layer or a silicon dioxide layer. The polymer layer can be formed using a gas containing C and F, including but not limited to at least one of CH2F2, C4F6, CH4, and CH3F; the silicon dioxide layer can be formed using SiCl4 and O2. The second protective layer is primarily used to protect the top of the layer to be etched 400 and the sidewalls of the initial via 430.
[0063] S82: The bottom of the holes in the etching layer 400 is etched by an anisotropic second dry etching process.
[0064] Specifically, in the anisotropic second dry etching process, the etching direction and angle (ejection direction and angle of plasma) can be adjusted by adjusting the etching parameters. Thus, in step S82, the tapered end of the hole at the bottom can be etched specifically by the anisotropic second dry etching process to optimize the morphology of the bottom of the initial hole 430.
[0065] S83: The second protective layer and etching byproducts are removed by a second dry cleaning process.
[0066] Specifically, in step S83, a specific gas can be introduced to generate plasma, which reacts with the second protective layer and etching byproducts to decompose and remove them, so as to carry out the next round of second shaping process or subsequent processes.
[0067] The second modification process is performed at least once, and each time it is performed in the order of steps S81 to S83. For example, the second modification process can be performed 1 to 60 times.
[0068] For example, the second deposition process, the second dry etching process, and the second dry cleaning process are all performed using an ICP etching equipment. The ICP etching equipment uses high-density plasma to etch materials. Its core principle is to excite gas in the reaction chamber through an external radio frequency coil to form plasma. The plasma contains high-energy electrons, ions, and chemically active free radicals. Through a combination of chemical reaction and physical bombardment, the material is precisely removed. The plasma contains high-energy electrons, ions, and chemically active free radicals, and it can also dissociate the precursor gas to generate active free radicals and ions, which are adsorbed, reacted, and solidified on the substrate surface to form a film.
[0069] For example, in step S81, the duration of the second deposition process can be 5s-10s. During the second deposition process, the source power of the ICP etching equipment can be 200W-2000W, and the bias power of the ICP etching equipment can be 0. CH2F2, C4F6, CH4, CH3F, and Ar gases can be introduced during the deposition process to form a polymer layer. The second deposition process can be an ALD process or a CVD process performed in situ using the ICP etching equipment.
[0070] In step S82, that is, during the second dry etching process, the source power of the ICP etching equipment is less than the bias power, and / or the bias power frequency of the ICP etching equipment is 2MHz. Specifically, the smaller the source power of the ICP etching equipment and the larger the bias power, the easier it is to etch the bottom of the via. Setting the source power to be less than the bias power can better etch the tapered end at the bottom of the via to remove the tapered end. At the same time, setting the bias power frequency of the ICP etching equipment to 2MHz can make the ion incident direction highly perpendicular to the wafer normal, bombarding only the bottom of the via perpendicularly. For example, in step S82, the duration of the second dry etching process can be 5s-60s, the source power of the ICP etching equipment can be 500W-999W, the bias power of the ICP etching equipment can be 1000W, the bias power frequency can be 2MHz, and Cl2, CH2F2, C4F6, CH3F, and NF3 can be introduced during the etching process.
[0071] In step S83, the duration of the second dry cleaning process can be 5s-60s. During the second dry cleaning process, the source power of the ICP etching equipment can be 2000W-5000W, and the bias power of the ICP etching equipment can be 0. CH4 and O2 can be introduced during the cleaning process. O2 is excited by the radio frequency power supply to generate plasma containing oxygen free radicals, which can react with the polymer to generate gaseous products, while oxidizing residual hydrocarbon byproducts and eliminating potential sources of contamination; CH4 dissociates to generate CH4. x Free radicals react with polymers, reducing the degree of polymer crosslinking and making them easier to oxidize and peel off.
[0072] For example, in some embodiments, prior to step S70 (or step S50), a third dry cleaning process can be used to remove etching byproducts from the bottom of the initial cavity 430, wherein the cleaning gas used in the third dry cleaning process includes hydrogen and / or chlorine. The third dry cleaning process can effectively reduce the accumulation of polymer and etching byproducts at the bottom of the initial cavity 430, improving the morphology of the bottom of the initial cavity 430.
[0073] For example, in some embodiments, the etchable layer 400 in the initial semiconductor structure includes a silicon dioxide layer 420 and a silicon nitride layer 410 stacked alternately in a cycle. When the landing part 200 is made of aluminum oxide or tungsten, step S80 can be performed after step S60 to further improve the morphology of the bottom of the initial hole 430 after optimizing the morphology of the sidewalls of the hole 430.
[0074] This application also provides a semiconductor structure fabricated by the method described above. This semiconductor structure can subsequently be used to fabricate semiconductor devices such as memory.
[0075] Although exemplary embodiments have been described herein with reference to the accompanying drawings, it should be understood that the above exemplary embodiments are merely illustrative and are not intended to limit the scope of this application. Various changes and modifications can be made therein by those skilled in the art without departing from the scope and spirit of this application. All such changes and modifications are intended to be included within the scope of this application as claimed in the appended claims.
[0076] Numerous specific details are set forth in the specification provided herein. However, it will be understood that embodiments of this application may be practiced without these specific details. In some instances, well-known methods, structures, and techniques have not been shown in detail so as not to obscure the understanding of this specification.
[0077] Similarly, it should be understood that, in order to streamline this application and aid in understanding one or more of the various inventive aspects, features of this application may sometimes be grouped together in a single embodiment, figure, or description thereof in the description of exemplary embodiments of this application. However, this approach should not be construed as reflecting an intention that the claimed application requires more features than are expressly recited in each claim. Rather, as reflected in the corresponding claims, its inventive point lies in solving the corresponding technical problem with features fewer than all features of a single disclosed embodiment. Therefore, the claims following the detailed description are hereby expressly incorporated into that detailed description, wherein each claim itself is a separate embodiment of this application.
[0078] Those skilled in the art will understand that, apart from the mutual exclusion of features, all features disclosed in this specification (including the accompanying claims, abstract, and drawings) and all processes or units of any method or apparatus so disclosed can be combined in any combination. Unless otherwise expressly stated, each feature disclosed in this specification (including the accompanying claims, abstract, and drawings) may be replaced by an alternative feature serving the same, equivalent, or similar purpose.
[0079] Furthermore, those skilled in the art will understand that although some embodiments described herein include certain features but not others included in other embodiments, combinations of features from different embodiments are intended to be within the scope of this application and form different embodiments. For example, in the claims, any one of the claimed embodiments can be used in any combination.
[0080] It should be noted that the above embodiments are illustrative of this application and not restrictive of this application, and that those skilled in the art can devise alternative embodiments without departing from the scope of the appended claims.
Claims
1. A method for fabricating a semiconductor structure, characterized in that, include: S10: Provide an initial semiconductor structure, wherein the initial semiconductor structure includes a substrate, a plurality of landing portions on the substrate, an etchable layer above the landing portions, and a hard mask layer on the etchable layer, the landing portions are isolated from each other by an isolation layer, the top surface of the landing portions is flush with the top surface of the isolation layer, the etchable layer is a stacked structure of alternating layers, and the thickness of the hard mask layer is greater than or equal to 1 μm; S20: A plurality of initial hard mask opening patterns are formed in the hard mask layer using photolithography and dry etching processes. There is at least one instance of insufficient etching of the initial hard mask opening pattern and / or uneven top size of the initial hard mask opening pattern. The number of the initial hard mask opening patterns corresponds one-to-one with the number of the landing parts. S30: The initial hard mask opening pattern is modified by an etching device through a plasma-like ashing process to form a patterned hard mask layer with a plurality of hard mask opening patterns, wherein the top size uniformity of the hard mask opening pattern is greater than or equal to 95%, and the hard mask opening pattern exposes the layer to be etched. S40: Using the patterned hard mask layer as a mask, etch the layer to be etched to form an initial hole through the layer to be etched to expose the landing part.
2. The preparation method according to claim 1, characterized in that, The hard mask layer is made of amorphous carbon. The ashing gas used in the plasma-like ashing process is a mixture of hydrogen and inert gas, or a mixture of oxygen and inert gas.
3. The preparation method according to claim 1, characterized in that, The flatness of the sidewall of the initial slot does not meet the preset requirements; After step S40, the preparation method further includes: S50: Remove the hard mask layer; S60: The sidewall of the initial hole groove is modified using a first shaping process so that the flatness of the sidewall of the initial hole groove meets the preset requirements. The first modification process is performed at least once, and the first modification process includes: S61: A first protective layer is deposited on the upper surface of the layer to be etched and the inner wall of the initial hole through a first deposition process; S62: The sidewalls of the holes in the layer to be etched are etched by an anisotropic first dry etching process; S63: Remove the first protective layer and etching byproducts by a first dry cleaning process.
4. The preparation method according to claim 3, characterized in that, The first deposition process, the first dry etching process, and the first dry cleaning process are all performed using an ICP etching device; During the first dry etching process, the source power of the ICP etching equipment is greater than the bias power, and / or the bias power frequency of the ICP etching equipment is 13.56MHz.
5. The preparation method according to claim 3, characterized in that, The first protective layer is a polymer layer or a silicon dioxide layer.
6. The preparation method according to claim 1, characterized in that, The layer to be etched comprises alternating layers of silicon dioxide and silicon nitride; The landing section is made of aluminum oxide or tungsten. The bottom of the initial slot has a tapered opening; After step S40, the preparation method further includes: S70: Remove the hard mask layer; S80: The bottom of the initial groove is modified using a second shaping process to remove the tapered opening; The second shaping process is performed at least once, and the second shaping process includes: S81: A second protective layer is deposited on the upper surface of the layer to be etched and on the inner wall of the initial hole through a second deposition process; S82: The bottom of the holes in the layer to be etched is etched by an anisotropic second dry etching process; S83: Remove the second protective layer and etching byproducts by a second dry cleaning process.
7. The preparation method according to claim 6, characterized in that, The second deposition process, the second dry etching process, and the second dry cleaning process are all performed using an ICP etching device; In the second dry etching process, the source power of the ICP etching equipment is less than the bias power, and / or the bias power frequency of the ICP etching equipment is 2MHz.
8. The preparation method according to claim 6, characterized in that, The second protective layer is a polymer layer or a silicon dioxide layer.
9. The preparation method according to claim 6, characterized in that, Before step S70, the preparation method further includes: The etching byproducts at the bottom of the initial groove are removed by a third dry cleaning process; The cleaning gas used in the third dry cleaning process includes hydrogen and / or chlorine.
10. A semiconductor structure, characterized in that, The semiconductor structure is prepared by any one of claims 1-9.