Flaring die for steel strip reinforced polyethylene corrugated pipe
By setting up shunt channels and temperature control in the expansion mold of the steel strip reinforced polyethylene corrugated pipe, the problem of poor molding effect caused by the long flow distance of the injection molding material is solved, and faster and more stable filling and connection effects are achieved.
Patent Information
- Application Number
- CN202322930603.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-10-30
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2033-10-30
AI Technical Summary
When the existing expansion mold is used, the flow distance of the injection molding material is large and the flow time is long, resulting in a drop in melt temperature and fluidity, resulting in poor expansion molding effect.
An expanded mold is designed that includes a mold base, a mold cavity and a mold core. A first runner and a second runner are provided inside the mold cavity. The melt enters the two ends from the runner opening and flows into the cavity until the melt is in the cavity. The middle is filled together, and the mold cavity can be optionally equipped with pouring inserts and compression inserts to improve filling efficiency, and temperature sensors are set on the mold cavity and core to control the temperature.
By diverting the injection molding material, the filling speed is faster, preventing the melt from cooling too quickly, improving the molding effect of the expansion, ensuring that the melt can completely fill the cavity, and enhancing the stability of the connection.
Smart Images

Figure CN221793582U_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of steel-belt reinforced polyethylene corrugated pipes, and more specifically, to a flaring die for steel-belt reinforced polyethylene corrugated pipes. Background Art
[0002] Steel belt reinforced polyethylene corrugated pipe is a double-wall spiral corrugated pipe with high-density polyethylene (PE) as the base, with steel belt coated with adhesive resin on the surface to form a waveform as the main supporting structure, and wrapped with polyethylene material to form a whole. When in use, when two steel belt reinforced polyethylene corrugated pipes need to be connected, in order to ensure stability, such as Figure 7 As shown, it is often necessary to use a flaring mold to produce a flare at the connection end of the steel-reinforced polyethylene corrugated pipe by injection molding.
[0003] Specifically, the flaring mold includes a mold base, a mold cavity and a flaring mold core. The mold cavity is installed on the mold base, and a flow channel is arranged on the mold cavity, so that the melt of the injection molding material can flow into the inner side of the mold cavity through the flow channel. After the flaring mold core is inserted into the mold cavity, the steel belt reinforced polyethylene corrugated tube is sleeved on the protruding end of the flaring mold core, so that the steel belt reinforced polyethylene corrugated tube extends into the mold cavity formed between the inner wall of the mold cavity and the outer wall of the flaring mold core. And the steel belt reinforced polyethylene corrugated tube is clamped between the mold cavity and the flaring mold core. At this time, the injection molding material is melted and flows into the molding cavity between the mold cavity and the flaring mold core through the flow channel, and the melt covers the protruding end of the steel belt reinforced polyethylene corrugated tube. After the melt solidifies, a flare is formed at the protruding end of the steel belt reinforced polyethylene corrugated tube.
[0004] In the existing flaring mold, the flow channels on the mold base and the mold cavity are connected to one end of the cavity. The injection material melt flows from one end of the cavity to the other end and fills the cavity. The flow distance is large and the flow time is long. As time goes by, the temperature of the melt gradually decreases, resulting in reduced fluidity of the melt, poor mold filling effect, and easily causing the problem of poor flaring molding effect. Utility Model Content
[0005] In order to overcome the problems existing in the related art to a certain extent, the purpose of the present application is to provide a flaring die for steel-strip reinforced polyethylene corrugated pipes, which can solve the problem that the flow distance and flow time of the injection material in the existing flaring die are large when filling the mold, which easily leads to poor flaring molding effect. The various technical effects that can be produced by the preferred technical solution among the various technical solutions provided in the present application are described in detail below.
[0006] The present application provides a flaring die for a steel-belt reinforced polyethylene corrugated pipe, comprising:
[0007] Die base;
[0008] A mold cavity is fixedly arranged on the mold base, and a flow channel is arranged on the mold cavity;
[0009] A mold core is inserted into the mold cavity. A step is provided on the outer wall of the insertion end of the mold core. A mold cavity is formed between the step and the inner wall of the mold cavity. The steel belt reinforced polyethylene corrugated pipe can be inserted into the mold cavity from the insertion end of the mold core.
[0010] The mold cavity is provided with a first flow channel and a second flow channel, both of which are connected to the flow channel opening, the first flow channel is connected to the first end of the mold cavity, and the first flow channel is connected to the second end of the mold cavity.
[0011] Optionally, the mold cavity comprises:
[0012] A mold cavity template, fixedly disposed in the mold base, wherein the first flow channel and the second flow channel are disposed in the mold cavity template;
[0013] A casting insert is fixedly arranged at the first end of the mold cavity template, wherein a casting hole communicating with the first flow channel is arranged in the casting insert, and the casting hole is communicated with the first end of the mold cavity;
[0014] A clamping insert is fixedly arranged at the second end of the mold cavity template. A pouring channel connected to the second flow channel is arranged in the clamping insert, and the pouring channel is connected to the second end of the mold cavity.
[0015] Optionally, a plurality of the pouring holes are arranged along the circumference of the inner wall of the pouring insert, an annular channel communicating with the first flow channel is arranged in the pouring insert, and the pouring holes are all communicated with the annular channel.
[0016] Optionally, the inner wall of the clamping insert is spirally provided with connected U-shaped grooves and spiral through grooves in sequence from the outside to the inside, the casting channel is connected to the spiral through groove, the spiral through groove is connected to the second end of the cavity, and the U-shaped groove is matched with the outer corrugation of the steel belt reinforced polyethylene corrugated pipe.
[0017] Optionally, the two first flow channels are respectively arranged at the upper and lower sides inside the mold cavity, the two second flow channels are respectively arranged at the upper and lower sides inside the mold cavity, and the two flow channel openings are respectively arranged at the upper and lower sides of the mold cavity.
[0018] Optionally, an exhaust hole is provided on the inner wall of the mold cavity.
[0019] Optionally, a first temperature sensor is provided on the outer wall of the mold base.
[0020] Optionally, a cooling water channel for introducing cooling water is provided inside the mold core.
[0021] Optionally, a second temperature sensor is provided on the inner wall of the mold core.
[0022] Optionally, the inner diameters of the flow channel openings decrease sequentially along the reverse direction of inflow.
[0023] The technical solution provided by this application may have the following beneficial effects:
[0024] 1. The present application provides a flaring die for a steel-strip reinforced polyethylene corrugated pipe, wherein the runner opening on the die cavity is connected to the first end and the second end of the die cavity through the first runner and the second runner respectively, and the melt of the injection molding material flows from the runner opening into the first runner and the second runner respectively. The melt flows into the die cavity from both ends of the die cavity through the first runner and the second runner respectively, until the melt converges in the middle of the die cavity and fills the die cavity. The melt flows into the die cavity from both ends, which makes it easier to fill the die cavity and fills faster, thereby preventing the melt from cooling too quickly and failing to completely fill the die cavity, thereby affecting the flaring molding effect.
[0025] 2. The mold cavity includes a mold cavity template and a casting insert and a pressing insert installed at both ends of the mold cavity template. On the inner wall of the pressing insert, a U-shaped groove and a spiral through groove are arranged in sequence from the outside to the inside. The shape of the U-shaped groove is matched with the outer corrugation of the steel belt reinforced polyethylene corrugated pipe. During installation, the steel belt reinforced polyethylene corrugated pipe can be screwed into the U-shaped groove and put into the mold core. At this time, the steel belt reinforced polyethylene corrugated pipe is pressed in the clamping U-shaped groove, and the connection is more stable and reliable.
[0026] It should be understood that the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the present application and, together with the description, serve to explain the principles of the present application.
[0028] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0029] Figure 1 is a schematic structural diagram of a flaring die for a steel-belt reinforced polyethylene corrugated pipe according to some exemplary embodiments;
[0030] Figure 2 is a schematic diagram showing a mold cavity installed on a mold base according to some exemplary embodiments;
[0031] Figure 3 is a schematic diagram of a half structure of a mold cavity according to some exemplary embodiments;
[0032] Figure 4 is a schematic diagram of the other half of the structure of the mold cavity according to some exemplary embodiments;
[0033] Figure 5 is a schematic diagram of a casting insert structure according to some exemplary embodiments;
[0034] Figure 6 is a schematic diagram of a mold core structure according to some exemplary embodiments;
[0035] Figure 7 is a schematic diagram of connecting two steel-belt reinforced polyethylene corrugated pipes according to some exemplary embodiments.
[0036] In the figure: 1. mold base; 2. first water channel; 3. mold cavity; 31. mold cavity template; 32. casting insert; 33. pressing insert; 4. runner outlet; 5. mold core; 6. step; 7. mold cavity; 8. first runner; 9. second runner; 10. pouring hole; 11. pouring channel; 12. spiral groove; 13. exhaust hole; 14. first temperature sensor; 15. cooling water channel; 16. second temperature sensor; 17. annular channel; 18. U-shaped groove; 19. gate; 20. second water channel. DETAILED DESCRIPTION
[0037] In order to make the purpose, technical solution and advantages of the utility model clearer, the technical solution of the utility model will be described in detail below. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other implementation methods obtained by ordinary technicians in this field without creative work belong to the scope of protection of the utility model.
[0038] The following is an explanation of the embodiments with reference to the accompanying drawings. In addition, the embodiments shown below do not limit the contents of the utility model described in the claims. In addition, the entire contents of the structures represented by the following embodiments are not limited to the solutions required as the utility model described in the claims.
[0039] refer to Figure 1-7This specific embodiment provides a flaring die for a steel-reinforced polyethylene corrugated pipe, characterized in that it includes: a die base 1, a die cavity 3 and a die core 5. The die cavity 3 is fixedly mounted on the die base 1, and the die core 5 is inserted into the die cavity 3 from the first end of the die cavity 3. Two steps 6 are pre-arranged on the outer wall of the end where the die core 5 is inserted into the die cavity 3. When the die core 5 is inserted into the die cavity 3, a cavity 7 is formed between the steps 6 and the inner wall of the die cavity 3. A first flow channel 8 and a second flow channel 9 are arranged inside the die cavity 3, so that the first flow channel 8 is connected to the first end of the die cavity 7, and the second flow channel 9 is connected to the other end of the die cavity 7. In this way, the liquid in the first flow channel 8 and the liquid in the second flow channel 9 can enter the die cavity 7 from both ends respectively and fill the die cavity 7.
[0040] A runner opening 4 is arranged on the outer wall of the mold cavity 3, so that the runner opening 4 is connected with both the first runner 8 and the second runner 9. In this way, the injection material melt can enter the first runner 8 and the second runner 9 respectively through the runner opening 4. The inner diameter of the runner opening 4 decreases from the outside to the inside.
[0041] Insert the steel-belt reinforced polyethylene corrugated pipe into the mold core 5 and insert it into one end of the mold cavity 3, so that the steel-belt reinforced polyethylene corrugated pipe enters the mold cavity 7, and the outer wall of the steel-belt reinforced polyethylene corrugated pipe is clamped with the inner wall of the mold cavity 3. After the melt of the injection molding material is melted, it flows into the first runner 8 and the second runner 9 respectively. The melt flows into the mold cavity 7 from both ends of the mold cavity 7 through the first runner 8 and the second runner 9 respectively, until the melt converges in the middle of the mold cavity 7 and fills the mold cavity and the annular groove. At this time, the melt is coated on one end of the steel-belt reinforced polyethylene corrugated pipe entering the mold cavity 7. After the melt cools and solidifies, a flare is formed at one end of the steel-belt reinforced polyethylene corrugated pipe, and the melt in the annular groove solidifies to form a reinforcing rib for the flare connection. With this arrangement, the melt flows into the mold cavity 7 from both ends, which is easier to fill the mold cavity 7, and the filling speed is faster, preventing the melt from cooling too fast and failing to completely fill the mold cavity, thereby affecting the flaring molding effect.
[0042] It is worth noting that the mold cavity 3 and the mold core 5 should both be configured as a half-type, that is, the mold cavity 3 and the mold core 5 are composed of two half-shaped bodies, which is convenient for opening the mold and taking it out.
[0043] As an optional embodiment, the mold cavity 3 comprises: a mold cavity template 31, a casting insert 32 and a pressing insert 33. The casting insert 32 and the pressing insert 33 are respectively arranged at two ends of the mold cavity template 31.
[0044] The first flow channel 8 and the second flow channel 9 are arranged in the mold cavity template 31. The first flow channel 8 and the second flow channel 9 both penetrate the inner wall of the mold cavity template 31.
[0045] For the casting insert 32, a casting hole 10 is preset on the casting insert 32, so that the casting hole 10 is connected with the first end of the cavity 7. After the casting insert 32 is installed at the first end of the cavity template 31, the casting hole 10 is aligned with the first flow channel 8 and connected.
[0046] Among them, an annular channel 17 is arranged in the casting insert 32, so that the pouring hole 10 penetrates the inner wall of the annular channel 17 and communicates with the annular channel 17. Multiple pouring holes 10 are evenly arranged along the circumference of the inner wall of the casting insert 32. Multiple pouring holes 10 are all communicated with the annular channel. Multiple pouring holes 10 are arranged along the circumference of the inner wall of the casting insert 32, so that all pouring holes 10 are communicated with the annular channel 17. A gate 19 connected to the annular channel 17 is arranged on the casting insert 32, so that the gate 19 is aligned and communicated with the second runner 9. In this way, the injection material melt can enter from the gate 19 and then be diverted to all pouring holes 10 through the annular channel 17, and finally flow into the mold cavity 7 from all pouring holes 10 at the same time, and the filling is more uniform.
[0047] The pouring hole 10 is formed on the inner wall of the pouring insert 32, and the pouring hole 10 is U-shaped. The pouring insert 32 can be a half-shaped one, that is, the pouring insert 32 is composed of two half-shaped bodies. With such a configuration, installation is more convenient, and the direction of the pouring hole 10 can be set according to needs.
[0048] In some embodiments, a first water channel 2 is provided in the mold cavity template 31, and the first water channel 2 runs through the mold cavity template 31. A second water channel 20 is provided on the casting insert 32, and a plurality of second water channels 20 are arranged in a ring shape and run through the casting insert 32. The first water channel 2 and the second water channel 20 are connected. After the injection molding material melt fills the mold cavity 7, cooling water is passed into the first water channel 2 and then flows through the second water channel 20 and runs through the mold cavity 3, thereby quickly reducing the temperature of the mold cavity 3, so that the injection molding material melt is quickly cooled and solidified.
[0049] It is worth noting that before the injection molding material melt is introduced into the mold cavity 7, hot water can be introduced into the first water channel 2 and then flow through the second water channel 20 to pass through the mold cavity 3, thereby quickly raising the temperature of the mold cavity 3. After the mold cavity 3 is raised to a certain temperature, the injection molding material melt is introduced into the mold cavity 7. At this time, the injection molding material melt is not easy to cool and solidify under the action of high temperature, and has better fluidity, which facilitates the injection molding material melt to fill the mold cavity 7.
[0050] For the compression insert 33, a pouring channel 11 is provided in the compression insert 33. The pouring channel 11 is connected to the second end of the cavity 7 and penetrates the outer wall of the compression insert 33. After the compression insert 33 is installed at the second end of the cavity template 31, the pouring channel 11 is aligned with the second runner 9 and connected.
[0051] A U-shaped groove 18 is firstly formed on the inner wall of the pressing insert 33 from the outside to the inside, and the U-shaped groove 18 is spirally arranged along the inner wall of the pressing insert 33. Then, a spiral through groove 12 is formed immediately thereafter, and the spiral through groove 12 is spirally arranged along the inner wall of the pressing insert 33. At this time, the U-shaped groove 18 is connected with the spiral through groove 12, and the cross-sectional size of the U-shaped groove 18 is smaller than the cross-sectional size of the spiral through groove 12, and the spiral through groove 12 becomes a part of the cavity 7.
[0052] When setting, the shape of the U-shaped groove 18 is matched with the outer corrugation of the steel-belt reinforced polyethylene corrugated pipe. The steel-belt reinforced polyethylene corrugated pipe is screwed into the U-shaped groove 18. As the steel-belt reinforced polyethylene corrugated pipe is screwed in, the steel-belt reinforced polyethylene corrugated pipe is sleeved on one end of the mold core 5 inserted into the mold cavity 3, and is pressed in the clamping U-shaped groove 18, which is more stable and reliable.
[0053] The spiral groove 12 is connected to the second end of the cavity 7 and becomes a part of the cavity 7, and the pouring channel 11 is connected to the spiral groove 12. After the steel-belt reinforced polyethylene corrugated pipe is screwed in, the inner wall of the corrugated pipe fits with the U-shaped groove 18, so there is a gap between the outer wall of the part of the inner wall of the corrugated pipe that passes through the U-shaped groove 18 and the inner wall of the spiral groove 12, so the melt can enter the cavity 7 through the gap after entering the spiral groove 12. At the same time, since the cross-sectional size of the U-shaped groove 18 is smaller than the cross-sectional size of the spiral groove 12, and the inner wall of the corrugated pipe fits with the U-shaped groove 18, the seal is ensured to prevent the melt in the spiral groove 12 from flowing out.
[0054] When the steel-reinforced polyethylene corrugated pipe is screwed into place, the melted injection material flows into the first flow channel 8 and the second flow channel 9 from the runner port 4. The melt flows through the first flow channel 8, the annular channel 17 and the pouring hole 10 and enters the first end of the cavity 7. At the same time, the melt flows through the second flow channel 9, the pouring channel 11 and the spiral groove 12 and enters the second end of the cavity 7 until the melt converges in the middle of the cavity 7 and fills the cavity and the annular groove. At this time, the melt covers one end of the steel-reinforced polyethylene corrugated pipe entering the cavity 7. After the melt cools and solidifies, a flared mouth is formed at one end of the steel-reinforced polyethylene corrugated pipe.
[0055] It is worth noting that the clamping insert 33 should be set as a half-shaped one, that is, the clamping insert 33 is composed of two half-shaped bodies, which is convenient for opening the mold and taking it out. In addition, a vent hole 13 should be set in the middle position of the inner wall of the mold cavity 3 for gas to be discharged to ensure that the melt can fill the mold cavity.
[0056] As an optional embodiment, two first runners 8, two second runners 9 and two runner openings 4 are each provided. The two first runners 8 are respectively opened on the upper and lower sides of the mold cavity 3 and are symmetrically arranged. The two second runners 9 are respectively opened on the upper and lower sides of the mold cavity 3 and are symmetrically arranged. The two runner openings 4 are respectively opened on the upper and lower sides of the mold cavity 3 and are symmetrically arranged. With such an arrangement, when the injection molding material melt is introduced, it can be introduced from the two runner openings 4 respectively, and then diverted to the corresponding first runners 8 and second runners 9 before entering the mold cavity 7, and the introduction efficiency is higher.
[0057] As an optional embodiment, it is characterized in that a first temperature sensor 14 is provided on the outer wall of the mold cavity 3. The first temperature sensor 14 can be a thermocouple, and the first temperature sensor 14 is connected to the temperature control module signal. After the first temperature sensor 14 detects the temperature of the mold base 1, the temperature signal is sent to the temperature control module, and the temperature control module sends the display signal to the display to display the temperature information after processing. During the injection molding process, it is convenient for the operator to monitor the real-time temperature of the mold cavity 3.
[0058] In some embodiments, a cooling water channel 15 is provided inside the mold core 5. The cooling water channel 15 may be a spiral water trough. The two ends of the cooling water channel 15 are connected to a water inlet and a water outlet, respectively. After the injection molding material melt fills the mold cavity 7, cooling water is introduced from the water inlet into the cooling water channel 15, and the cooling water exchanges heat with the mold core 5, thereby quickly reducing the temperature of the injection molding material melt, so that the injection molding material melt is quickly cooled and solidified.
[0059] It is worth noting that before the injection molding material melt is introduced into the cavity 7, hot water can be introduced into the cooling water channel 15 from the water inlet, and the hot water exchanges heat with the mold core 5, thereby quickly raising the temperature of the mold core 5. After the mold core 5 is raised to a certain temperature, the injection molding material melt is introduced into the cavity 7. At this time, the injection molding material melt is not easy to cool and solidify under the action of high temperature, and has better fluidity, which facilitates the injection molding material melt to fill the cavity 7.
[0060] In some embodiments, a second temperature sensor 16 is provided on the inner wall of the mold core 5. The second temperature sensor 16 can be a thermocouple to connect the second temperature sensor 16 to the temperature control module signal. After the second temperature sensor 16 detects the temperature of the mold core 5, it sends the temperature signal to the temperature control module. After the temperature control module processes, it sends the display signal to the display to display the temperature information. During the injection molding process, the temperature of the mold core 5 is the temperature of the injection material melt. It is convenient for the operator to monitor the temperature of the injection material melt in real time.
[0061] It should be noted that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", etc. used herein to indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation, and therefore cannot be understood as a limitation on the present invention. In addition, the terms "first", "second", "third", etc. are used for descriptive purposes only and cannot be understood as indicating or implying relative importance.
[0062] In the description of this article, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "installation", "connection" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in this utility model can be understood according to the specific circumstances.
[0063] Although the embodiments of the present application have been shown and described above, it is understood that the above embodiments are exemplary and cannot be construed as limitations of the present application. A person of ordinary skill in the art may change, modify, replace and modify the above embodiments within the scope of the present application. It is understood that the same or similar parts in the above embodiments may refer to each other, and the contents not described in detail in some embodiments may refer to the same or similar contents in other embodiments. The multiple schemes provided in the present application include the basic schemes themselves, which are independent of each other and do not restrict each other, but they may also be combined with each other without conflict to achieve a plurality of effects to be realized together.
Claims
1. A flaring die for a steel-reinforced polyethylene corrugated pipe, characterized in that: include: Mold base (1); A mold cavity (3) is fixedly arranged on the mold base (1), and a flow channel opening (4) is arranged on the mold cavity (3); A mold core (5) is inserted into the mold cavity (3); a step (6) is provided on the outer wall of the insertion end of the mold core (5); a mold cavity (7) is formed between the step (6) and the inner wall of the mold cavity (3); and the steel-reinforced polyethylene corrugated pipe can be inserted into the mold cavity (7) by inserting the insertion end of the mold core (5). The mold cavity (3) is provided with a first flow channel (8) and a second flow channel (9), the first flow channel (8) and the second flow channel (9) are both connected to the flow channel opening (4), the first flow channel (8) is connected to the first end of the mold cavity (7), and the first flow channel (8) is connected to the second end of the mold cavity (7).
2. The expansion die for steel-strip reinforced polyethylene corrugated pipe according to claim 1, characterized in that: The mold cavity (3) comprises: A mold cavity template (31) is fixedly arranged on the mold base (1), and the first flow channel (8) and the second flow channel (9) are arranged in the mold cavity template (31); A casting insert (32) is fixedly arranged at the first end of the mold cavity template (31), and a casting hole (10) communicating with the first flow channel (8) is arranged in the casting insert (32), and the casting hole (10) is communicated with the first end of the mold cavity (7); A clamping insert (33) is fixedly arranged at the second end of the mold cavity template (31), and a pouring channel (11) connected to the second flow channel (9) is arranged in the clamping insert (33), and the pouring channel (11) is connected to the second end of the mold cavity (7).
3. The expansion die for steel-strip reinforced polyethylene corrugated pipe according to claim 2, characterized in that: The plurality of pouring holes (10) are arranged along the circumference of the inner wall of the pouring insert (32), an annular channel (17) communicating with the first flow channel (8) is arranged in the pouring insert (32), and the pouring holes (10) are all communicated with the annular channel (17).
4. The expansion die for steel-strip reinforced polyethylene corrugated pipe according to claim 2, characterized in that: The inner wall of the clamping insert (33) is provided with a U-shaped groove (18) and a spiral through groove (12) which are connected in a spiral manner from the outside to the inside, the casting channel (11) is connected with the spiral through groove (12), the spiral through groove (12) is connected with the second end of the cavity (7), and the U-shaped groove (18) is arranged in coordination with the outer corrugation of the steel-reinforced polyethylene corrugated pipe.
5. The expansion die for steel-strip reinforced polyethylene corrugated pipe according to claim 2, characterized in that: The two first flow channels (8) are respectively arranged on the upper and lower sides of the mold cavity (3), the two second flow channels (9) are respectively arranged on the upper and lower sides of the mold cavity (3), and the two flow channel openings (4) are respectively arranged on the upper and lower sides of the mold cavity (3).
6. The expansion die for steel-reinforced polyethylene corrugated pipe according to claim 1, characterized in that: An exhaust hole (13) is provided on the inner wall of the mold cavity (3).
7. The expansion die for steel-strip reinforced polyethylene corrugated pipe according to claim 1, characterized in that: A first temperature sensor (14) is arranged on the outer wall of the mold cavity (3).
8. The expansion die for steel-reinforced polyethylene corrugated pipe according to claim 1, characterized in that: A cooling water channel (15) for passing cooling water is arranged inside the mold core (5).
9. The expansion die for steel-strip reinforced polyethylene corrugated pipe according to claim 8, characterized in that: A second temperature sensor (16) is arranged on the inner wall of the mold core (5).
10. The expansion die for steel-reinforced polyethylene corrugated pipe according to claim 1, characterized in that: The inner diameters of the flow channel openings (4) decrease in sequence along the reverse direction of the inflow direction.
Citation Information
Cited By
Flaring die for steel strip reinforced polyethylene corrugated pipe
CN117341127A