Device for preparing binder pitch for granulation of lithium ion battery cathode material

Through a device composed of a pressurized reactor and a molecular distillation process, a binder asphalt with high coking value, low QI, and high β resin is prepared, which solves the compatibility and structural uniformity problems of lithium-ion battery anode materials and significantly improves improve battery performance and adhesion.

CN221797380UActive Publication Date: 2024-10-01SINOSTEEL ANSHAN RES INST OF THERMO ENERGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420167623.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-24
Publication Date
2024-10-01
Estimated Expiration
2034-01-24

AI Technical Summary

Technical Problem

Artificial graphite, the existing negative electrode material for lithium ion batteries, has poor compatibility when lithium ions are inserted/extracted, resulting in a short battery cycle life, and the uneven microstructure affects the specific capacity and rate performance, and the quality of the binder pitch is difficult to meet. Requirements for high coking value, low QI, and high beta resin.

Method used

A device composed of a pressurized reactor, an oxidation device and a short-range molecular distiller is used to prepare binder pitch with high coking value, low QI and high β resin through pressurized polymerization, oxidative cross-linking and molecular distillation processes to ensure graphite The lamellar skeletons are interconnected to form a uniform and stable void structure.

Benefits of technology

It improves the adhesion and performance indicators of the negative electrode material, reduces volatile emissions, increases the coking value and β-resin content, and significantly improves the applicability and battery performance of the negative electrode material.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221797380U_ABST
    Figure CN221797380U_ABST
Patent Text Reader

Abstract

The utility model relates to a device for preparing binder pitch for granulation of a lithium ion battery cathode material, which comprises a pressurized reaction kettle, an oxidation device, a short-path molecular distiller and a polymerization reaction kettle, a discharge port of the pressurized reaction kettle is connected with a feed port of the oxidation device, a discharge port of the oxidation device is connected with a feed port of the short-path molecular distiller, and a discharge port of the polymerization reaction kettle is connected with a discharge port of the short-path molecular distiller. A heavy component outlet of the short-path molecular distiller is connected with a polymerization reaction kettle, and a discharge hole of the polymerization reaction kettle is connected with a raw material collecting device. According to the utility model, the asphalt is subjected to condensation polymerization through raw material mixing and pressurized polymerization processes, the softening point is greatly reduced under the condition that the coking value of the asphalt is not changed after reaction, and the coking value is greatly improved compared with the conventional process after the softening point is improved through the molecular distillation process. The increase of the coking value shows that less volatile components are discharged in the granulation process of the negative electrode material, and the yield is increased. The content of beta resin is increased through the oxidation process, and the cohesiveness is greatly improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of asphalt, and in particular relates to a device for preparing binder asphalt for granulating negative electrode materials of lithium ion batteries. Background Art

[0002] Binder asphalt is an important raw material for the production of carbon products. Binder asphalt has a high carbon content and excellent bonding properties. The quality of binder asphalt directly affects the strength, thermal shock resistance, electrical and thermal conductivity of the product and other technical indicators. With the rapid development of the metallurgical industry, the quality requirements of carbon products are also constantly improving, and the quality requirements of asphalt binders are also increasing accordingly. Improving the quality of asphalt binders can reduce the resistivity of products, improve the mechanical strength, oxidation resistance and thermal stability of products. There are two requirements for binders used in the production of carbon materials. One is to give the paste a certain plasticity during the kneading and molding process; the other is to form a carbon film bonding bridge between the particle aggregates during the roasting process, which combines the fixed carbon particles into a whole and gives it a certain mechanical strength. Among the various items of binder asphalt, the most important indicators are TI and QI. The β resin truly represents the bonding component.

[0003] In lithium-ion batteries, the negative electrode material is one of the important factors affecting the battery capacity and service life. The negative electrode material is mainly artificial graphite. Artificial graphite is not very compatible with the electrolyte in lithium-ion batteries. When lithium ions are inserted / extracted, solvent molecules will co-embed, resulting in a low cycle life of the battery. At the same time, due to the differences in the microstructure during the artificial graphite process, the graphite microcrystalline structure cannot be completely formed during the graphitization process, and many active sites will be generated on the surface, which seriously affects the specific capacity of the negative electrode material and reduces its applicability. In addition, the relatively complete layered structure of artificial graphite means that lithium ions can only be inserted in a direction perpendicular to the Z axis, increasing the migration path of lithium ions and showing poor rate performance. At this time, a binder for granulating negative electrode materials with high coking value, low QI, high β resin and low ash content can be prepared in a directional manner. On the basis of ensuring that the graphite sheet skeleton is interconnected, artificial graphite secondary particles with uniform and stable void structure and excellent micromorphology can be prepared. Utility Model Content

[0004] The utility model provides a device for preparing binder asphalt for granulating negative electrode materials of lithium ion batteries, so as to prepare binder asphalt for granulating negative electrode materials with high coking value, low QI, high β resin and low ash content, and to prepare artificial graphite secondary particles with uniform and stable void structure and excellent microscopic morphology on the basis of ensuring that the skeletons of graphite sheets are interconnected.

[0005] In order to achieve the above purpose, the utility model adopts the following technical solutions:

[0006] The device for preparing binder asphalt for granulating negative electrode materials of lithium-ion batteries comprises a pressure reactor, an oxidation device, a short-range molecular distiller, and a polymerization reactor. The discharge port of the pressure reactor is connected to the feed port of the oxidation device, the discharge port of the oxidation device is connected to the feed port of the short-range molecular distiller, the heavy component outlet of the short-range molecular distiller is connected to the polymerization reactor, and the discharge port of the polymerization reactor is connected to a raw material collecting device.

[0007] It also includes a light component collection tank and a by-product collection tank. The gas phase outlet of the oxidation device is connected to the light component collection tank, and the light component outlet of the short-range molecular distillation device is connected to the by-product collection tank.

[0008] The oxidation device is a reactor with a stirrer, and the bottom of the reactor is connected to an air pump.

[0009] Compared with the existing technology, the beneficial effects of the utility model are:

[0010] 1) The utility model uses a process of mixing raw materials and pressurizing polymerization to cause a polycondensation reaction of asphalt. After the reaction, the softening point of the asphalt is greatly reduced while the coking value remains unchanged. After the softening point is increased by a molecular distillation process, the coking value is greatly improved compared with the conventional process. The improvement in the coking value is reflected in the emission of less volatiles during the granulation of the negative electrode material and the increase in the yield. The oxidation process increases the β resin content and greatly improves the bonding property.

[0011] 2) The production raw materials of the utility model are medium-low temperature coal tar and ethylene tar, which are easy to obtain, low in price, and high-adhesive binder asphalt materials for lithium-ion battery granulation, so that asphalt can be used with high added value. The obtained binder asphalt product has low quinoline insoluble content, good adhesion, and high coking value. After granulation, the performance of negative electrode material products is significantly improved. The process is simple, the product quality is good, and the enterprise profit is high. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 This is the process route diagram of the utility model.

[0013] In the figure: 1-pressure reactor, 2-oxidation device, 3-light component collection tank, 4-short-range molecular distiller, 5-by-product collection tank, 6-polymerization reactor, 7-raw material collection device, 8-air pump. DETAILED DESCRIPTION

[0014] The present invention is further described below by way of examples, but the present invention is not limited to the scope of the examples. Based on the examples in the present invention, all other examples obtained by ordinary technicians in the field without creative work are within the scope of protection of the present invention.

[0015] The invention discloses a method for preparing a binder asphalt for granulating negative electrode materials of lithium ion batteries. The method uses a mixture of coal-based asphalt and oil-based tar for granulation in the production process of negative electrode materials. With medium-low temperature coal tar asphalt and ethylene tar as raw materials and polyacrylic acid as a modifier, a binder asphalt for granulating lithium ion batteries with high adhesion is obtained through pressure polymerization, oxidative crosslinking and molecular distillation processes. In the mixture of medium-low temperature coal tar and ethylene tar, ethylene tar accounts for 10wt% to 30wt% of the medium-low temperature coal tar. The amount of the modifier polyacrylic acid is 0.5wt% to 2wt% of the mixture of medium-low temperature coal tar and ethylene tar.

[0016] The specific steps include the following:

[0017] 1) Add ethylene tar to medium-low temperature coal tar, place in a pressure reactor and stir at 180-200° C. for 1-1.5 hours to obtain a mixed asphalt.

[0018] 2) The mixed asphalt is pressurized and polymerized in a pressure reactor. The temperature is raised to 350-400°C at a heating rate of 3-5°C / min. Nitrogen is introduced and the pressure is increased to 0.5-1.0 MPa. The polymerization reaction is kept at a constant temperature for 2-8 hours to obtain pressurized polymerized asphalt.

[0019] 3) The pressurized polymerized asphalt obtained in step 2) is further subjected to oxidative cross-linking at a temperature of 330-380° C. The gas flow rate is regulated according to the total amount of material (100 L / min-600 L / min) and the oxidation time is 2-6 hours to obtain oxidized asphalt.

[0020] 4) The mixed oxidized asphalt obtained in step 3) is molecularly distilled through a molecular distillation device at a temperature of 230-280°C, and the vacuum pressure of the short-range molecular distiller is controlled. The mixed oxidized asphalt is distilled under rotation to obtain a high-adhesive high-softening point asphalt material by molecular distillation; the vacuum pressure of the short-range molecular distiller is 30-200 Pa, and the rotation speed is 200-400 rpm.

[0021] 5) Adding a modifier, polyacrylic acid, to the high softening point asphalt material obtained in step 4) and mixing them at a mixing temperature of 220° C. to 270° C. for a mixing time of 0.5 to 2 h, a binder asphalt for lithium-ion battery granulation is obtained.

[0022] The prepared binder asphalt for lithium ion battery granulation has a softening point of 170° C. to 250° C., a QI value of less than 1%, a TI value of more than 31%, a CV of more than 60%, a moisture content of less than 1%, and an ash content of less than 1%.

[0023] like Figure 1As shown, the device used in the method for preparing the binder asphalt for granulation of negative electrode materials of lithium-ion batteries includes a pressure reactor 1, an oxidation device 2, a short-range molecular distiller 4, and a polymerization reactor 5. The discharge port of the pressure reactor 1 is connected to the feed port of the oxidation device 2, the discharge port of the oxidation device 2 is connected to the feed port of the short-range molecular distiller 4, the heavy component outlet of the short-range molecular distiller 4 is connected to the polymerization reactor 6, and the discharge port of the polymerization reactor 6 is connected to the raw material collecting device 7.

[0024] It also includes a light component collecting tank 3 and a by-product collecting tank 5. The gas phase outlet of the oxidation device 2 is connected to the light component collecting tank 3, and the light component outlet of the short-range molecular distiller 4 is connected to the by-product collecting tank 5.

[0025] The oxidation device 2 is a reactor with a stirrer. The bottom of the reactor is connected to an air pump 8, and air is supplied into the oxidation device 2 through the air pump 8.

[0026] The method of the utility model will be further described below through several embodiments.

[0027] Embodiment 1:

[0028] Take a certain mass of medium and low temperature coal tar and ethylene tar accounting for 20wt% of medium and low temperature coal tar, mix them evenly, place them in a pressure reactor 1, stir them at 180℃ for 1.5h, and ensure that the two raw materials are fully mixed. The mixed asphalt is pressurized and polymerized in a pressure reactor 1, and the temperature is raised to 380℃ at a rate of 5℃ / min. Nitrogen is introduced and pressurized to 1Mpa for polymerization reaction for 2 hours to obtain pressurized polymerized asphalt. The pressurized polymerized asphalt is oxidatively cross-linked, with an air flow rate of 100L / min, an oxidative cross-linking temperature of 370℃, and a constant temperature of 3h to obtain oxidized asphalt. The oxidized asphalt is added to a short-range molecular distiller 5, the temperature is set to 250℃, the vacuum pressure of the short-range molecular distiller 5 is controlled to 100Pa, the speed is 200rpm, and the distillation time is 3h. A high-softening point asphalt material with high adhesion is obtained by molecular distillation. Polyacrylic acid accounting for 1wt% of the raw asphalt is added to the high softening point asphalt material and mixed at 250℃ to obtain a binder asphalt for lithium-ion battery granulation. The performance indicators are shown in Table 1. The performance indicators of the asphalt and petroleum coke after granulation are shown in Table 2 (particle size in Table 2), prepared into negative electrode materials and assembled into button-type lithium-ion batteries for electrochemical testing, and compared with the negative electrode materials prepared from ordinary granulated asphalt. The battery test results are shown in Table 2.

[0029] Embodiment 2:

[0030] Take a certain mass of medium and low temperature coal tar and ethylene tar accounting for 25wt% of medium and low temperature coal tar, mix them evenly, place them in a pressure reactor 1, stir them at 190℃ for 1h, and ensure that the two raw materials are fully mixed. The mixed asphalt is pressurized and polymerized in a pressure reactor 1, and the temperature is raised to 370℃ at a rate of 4℃ / min. Nitrogen is introduced and pressurized to 0.9Mpa for polymerization reaction for 6 hours to obtain pressurized polymerized asphalt. The pressurized polymerized asphalt is oxidatively cross-linked, with an air flow rate of 200L / min, an oxidative cross-linking temperature of 360℃, and a constant temperature of 5h to obtain oxidized asphalt. The oxidized asphalt is added to a short-range molecular distiller 5, the temperature is set to 270℃, the vacuum pressure of the short-range molecular distiller 5 is controlled to 150Pa, the speed is 300rpm, and the distillation time is 3h. A high-softening point asphalt material with high adhesion is obtained by molecular distillation. Polyacrylic acid accounting for 1.5wt% of the raw asphalt is added to the high softening point asphalt material and mixed at 240℃ to obtain a binder asphalt for lithium-ion battery granulation. The performance indicators of the asphalt and petroleum coke after granulation are shown in Table 2. The negative electrode materials are prepared and assembled into button-type lithium-ion batteries for electrochemical testing. The battery test results are compared with the negative electrode materials prepared with ordinary granulated asphalt and are shown in Table 2.

[0031] Embodiment 3:

[0032] Take a certain mass of medium and low temperature coal tar and ethylene tar accounting for 15wt% of medium and low temperature coal tar, mix them evenly, place them in a pressure reactor 1, stir them at 185℃ for 1.5h, and ensure that the two raw materials are fully mixed. The mixed asphalt is pressurized and polymerized in a pressure reactor 1, and the temperature is raised to 360℃ at a rate of 5℃ / min. Nitrogen is introduced and pressurized to 0.8Mpa for polymerization reaction for 4 hours to obtain pressurized polymerized asphalt. The pressurized polymerized asphalt is oxidatively cross-linked, with an air flow rate of 100L / min, an oxidative cross-linking temperature of 380℃, and a constant temperature of 6h to obtain oxidized asphalt. The oxidized asphalt is added to a short-range molecular distiller 5, the temperature is set to 260℃, the vacuum pressure of the short-range molecular distiller 5 is controlled to 90Pa, the speed is 250rpm, and the distillation time is 3h. A high softening point asphalt material with high adhesion is obtained by molecular distillation. The high softening point asphalt material is added to polyacrylic acid accounting for 0.9wt% of the raw asphalt and mixed at 230℃ to obtain a binder asphalt for lithium ion battery granulation. The performance indicators of the asphalt and petroleum coke after granulation are shown in Table 2. The negative electrode materials are prepared and assembled into button-type lithium-ion batteries for electrochemical testing. The battery test results are compared with the negative electrode materials prepared with ordinary granulated asphalt and are shown in Table 2.

[0033] Embodiment 4:

[0034] Take a certain mass of medium and low temperature coal tar and ethylene tar accounting for 28wt% of medium and low temperature coal tar, mix them evenly, place them in a pressure reactor 1, stir them at 195℃ for 1.5h, and ensure that the two raw materials are fully mixed. The mixed asphalt is placed in a pressure reactor for pressure polymerization, and the temperature is raised to 390℃ at a rate of 3℃ / min. Nitrogen is introduced and pressurized to 0.5Mpa for polymerization reaction for 1 hour to obtain pressurized polymerized asphalt. The pressurized polymerized asphalt is oxidatively cross-linked, with an air flow rate of 300L / min, an oxidative cross-linking temperature of 350℃, and a constant temperature of 4h to obtain oxidized asphalt. The oxidized asphalt is added to a short-range molecular distiller 5, the temperature is set to 240℃, the vacuum pressure of the short-range molecular distiller 5 is controlled to 80Pa, the speed is 400rpm, and the distillation time is 3h. A high-softening point asphalt material with high adhesion is obtained by molecular distillation. The high-softening point asphalt material is added to polyacrylic acid accounting for 1.8wt% of the raw asphalt and mixed at 260℃ to obtain a binder asphalt for lithium-ion battery granulation. The performance indicators of the asphalt and petroleum coke after granulation are shown in Table 2. The negative electrode materials are prepared and assembled into button-type lithium-ion batteries for electrochemical testing. The battery test results are compared with the negative electrode materials prepared with ordinary granulated asphalt and are shown in Table 2.

[0035] Table 1 Performance index of the embodiment

[0036] Serial number Softening point / ℃ QI / % TI / % CV / % Moisture / % Ash / % 1 180.9 0.10 31.2 66.2 0.04 0.02 2 183.0 0.13 36.5 68.1 0.03 0.05 3 201.7 0.21 37.0 72.3 0.03 0.03 4 186.2 0.68 32.2 67.1 0.02 0.03

[0037] Table 2 Performance indicators of negative electrode materials after granulation and assembly into button batteries

[0038]

[0039] The above description is only a preferred embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the profession can make equivalent substitutions or changes within the technical scope disclosed by the present invention according to the technical solution and the utility model concept of the present invention, which still falls within the protection scope of the present invention.

Claims

1. A device for preparing binder asphalt for granulating negative electrode materials for lithium-ion batteries, characterized in that: The invention comprises a pressure reactor, an oxidation device, a short-range molecular distiller and a polymerization reactor, wherein the discharge port of the pressure reactor is connected to the feed port of the oxidation device, the discharge port of the oxidation device is connected to the feed port of the short-range molecular distiller, the recombinant component outlet of the short-range molecular distiller is connected to the polymerization reactor, and the discharge port of the polymerization reactor is connected to a raw material collecting device.

2. The device for preparing binder asphalt for granulating negative electrode materials for lithium ion batteries according to claim 1, characterized in that: It also includes a light component collection tank and a by-product collection tank. The gas phase outlet of the oxidation device is connected to the light component collection tank, and the light component outlet of the short-range molecular distillation device is connected to the by-product collection tank.

3. The device for preparing binder asphalt for granulating negative electrode materials for lithium ion batteries according to claim 1, characterized in that: The oxidation device is a reactor with a stirrer, and the bottom of the reactor is connected to an air pump.