Cavity device for synthesizing colorless diamond large single crystals by using double graphite electrodes
By using components such as graphite cups and copper cups in the diamond large single crystal cavity device, the synthetic resistance and heat preservation performance are improved, the problems of high power consumption and difficult to control temperature differences in traditional devices are solved, and a more stable diamond large single crystal cavity device is achieved. crystal growth.
Patent Information
- Application Number
- CN202323400061.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-13
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2033-12-13
AI Technical Summary
Traditional diamond large single crystal cavity devices have problems such as low synthetic resistance, high power consumption, local overheating, difficult to control temperature differences, unstable resistance due to over-burning of dolomite, and uneven temperature of the top hammer, especially the selection of dolomite ring forming density. It has a greater impact on high-grade large single crystals.
Dual graphite electrodes are used to synthesize a colorless diamond large single crystal cavity device. By using graphite cups as heating electrodes, increasing graphite sheets and copper cups to uniform the hammer temperature, increasing the dolomite ring forming density, and using ceramic sheets to avoid dolomite overshooting. Burn, adjust the temperature difference to control the growth rate, and improve the synthetic resistance and heat preservation performance.
The synthetic resistance is increased, power consumption is reduced, local overheating is avoided, resistance stability and temperature difference control are ensured, and the stability and heat preservation performance of the diamond large single crystal cavity device are enhanced.
Smart Images

Figure CN221797728U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a double-graphite electrode synthesis colorless diamond large single crystal cavity device, belonging to the technical field of equipment for manufacturing diamond large single crystals. Background Art
[0002] There are two different growth methods for colorless diamond large single crystals. One is called thin film growth (FG): in the diamond stable zone, the nucleation growth of diamond is achieved by crystallization of graphite through molten metal film deposition at a constant temperature. The other is the temperature gradient method (TGG): the carbon source in the high temperature zone is transported to the surface of the seed in the low temperature zone. Generally speaking, the maximum size of diamonds grown by the thin film method does not exceed 3mm. The crystals grown by the temperature gradient method are of good quality and easy to control. The crystal size depends on the size of the high-pressure reaction vessel. It is currently the main growth method for large-grained single crystals.
[0003] The heating method is indirect heating. The carbon source is spectrally pure graphite powder, diamond powder or a mixture of graphite powder and diamond powder can also be used. The carbon source is placed in the middle of the reaction chamber where the temperature is the highest. The solvent metal is inserted between the carbon source and the seed crystal. A platinum sheet is inserted between the seed crystal and the solvent to prevent the solvent metal from dissolving the seed crystal before being saturated with carbon. The temperature gradient method is used to grow large single crystals, with a growth temperature of 1430-1500℃ and a growth pressure of 5.5-6.0GPa, and a growth cycle of tens to hundreds of hours. The solvent metal is Ni, Ni-based alloy, Co and Fe, etc.
[0004] In the actual production process, the traditional assembly structure has problems such as low synthetic resistance, high power consumption, local overheating at both ends, poor control of temperature difference and growth rate, unstable resistance due to overburning of dolomite, and uneven top hammer temperature. In particular, the selection of dolomite ring forming density has an important influence on the synthesis of high-grade large single crystals.
[0005] Long-term practice shows that using single pyrophyllite as a pressure transmission medium has some weaknesses, mainly manifested in: pyrophyllite undergoes phase change under high temperature and high pressure. Under the condition of 5.5-6.0GPa, when the temperature is 1620-1720K, the water in the pyrophyllite causes the pyrophyllite to transform into kyanite + coesite. This phase change and the accompanying volume shrinkage make the thermal insulation and pressure transmission performance worse, thus causing a significant change in the diamond growth environment in the synthesis cavity, resulting in unstable diamond crystal quality. Compared with pyrophyllite, dolomite has a larger thermal expansion coefficient, a smaller thermal conductivity coefficient, and does not contain water, so it does not undergo phase change under high temperature and high pressure.
[0006] In view of the above reasons, a composite pressure transmission medium more suitable for diamond growth is now used, which is composed of dolomite and pyrophyllite. The internal friction coefficient of dolomite is smaller than that of pyrophyllite, so the dolomite is made into a sleeve and installed inside the pyrophyllite cavity, which is conducive to improving the uniformity of pressure transmission. The dolomite sleeve does not play a sealing role, but only plays a heat preservation role. By increasing the molding density of the dolomite ring, the heat preservation performance can be further improved, and the effect of the volume shrinkage of pyrophyllite due to long-term high temperature and high pressure on the synthesis of large single diamond crystals can be further improved. In combination with the adjustment of other structural accessories, the stability of the diamond large single crystal cavity device can be further improved. Summary of the invention
[0007] In order to solve the above problems, the utility model provides a double graphite electrode synthesis colorless diamond large single crystal cavity device.
[0008] The utility model is implemented according to the following technical solutions:
[0009] A double graphite electrode synthesis colorless diamond large single crystal cavity device, comprising:
[0010] A pyrophyllite block, the middle of which is provided with a through hole penetrating the upper and lower surfaces thereof;
[0011] Two pyrophyllite rings, pyrophyllite ring one is placed at the upper end of the through hole in the middle of the pyrophyllite block, and pyrophyllite ring two is placed at the lower end of the through hole in the middle of the pyrophyllite block;
[0012] Two copper cups, copper cup one is placed in pyrophyllite ring one, and copper cup two is placed in pyrophyllite ring two;
[0013] Two copper plates, copper plate one is placed in copper cup one, and copper plate two is placed in copper cup two;
[0014] Two dolomite rings, dolomite ring one is placed in copper cup one, and dolomite ring two is placed in copper cup two;
[0015] Two alumina rings a, alumina ring a-1 is placed at the lower end of the dolomite ring, and alumina ring a-2 is placed at the upper end of the dolomite ring;
[0016] Two graphite cups a, graphite cup a1 is placed in copper cup a, and graphite cup a2 is placed in copper cup two;
[0017] The magnesium oxide tube is placed in the through hole of the pyrophyllite block and is located between the first alumina ring and the second alumina ring;
[0018] Two alumina rings b are placed in the magnesium oxide tube, with alumina ring b1 placed at the lower end of alumina ring a and alumina ring b2 placed at the upper end of alumina ring a2;
[0019] Two graphite cups b, graphite cup b1 is placed in alumina ring b1 and is located at the lower end of graphite cup a, and graphite cup b2 is placed in alumina ring b2 and is located at the upper end of graphite cup a1;
[0020] Two graphite sheets, graphite sheet one is placed at the lower end of graphite cup b, and graphite sheet two is placed at the upper end of graphite cup b2;
[0021] A graphite tube is placed in the magnesium oxide tube and located between the first graphite sheet and the second graphite sheet;
[0022] An insulating tube placed in a graphite tube;
[0023] The ceramic sheet, the nitrogen removal sheet, the carbon source, the catalyst and the crystal bed are all placed in an insulating tube and located between the first graphite sheet and the second graphite sheet.
[0024] In some embodiments, the dolomite ring one is composed of a small dolomite ring one and a large dolomite ring one, and the dolomite ring two is composed of a small dolomite ring two and a large dolomite ring two; the large dolomite ring one is placed at the lower end of the small dolomite ring, and the large dolomite ring two is placed at the upper end of the small dolomite ring two.
[0025] In some embodiments, the graphite cup a1 and the graphite cup a2 are both filled with dolomite.
[0026] In some embodiments, the graphite cup b1 and the graphite cup b2 are both filled with alumina cores.
[0027] In some embodiments, the ceramic sheet is placed at the lower end of the graphite sheet, the crystal bed is placed at the upper end of the graphite sheet, the denitrification sheet is placed at the lower end of the ceramic sheet, the catalyst is placed at the upper end of the crystal bed, and the carbon source is placed between the denitrification sheet and the catalyst.
[0028] In some embodiments, a seed crystal is disposed on the crystal bed.
[0029] In some embodiments, the thickness of the second graphite sheet is greater than the thickness of the first graphite sheet.
[0030] In some embodiments, the openings of the graphite cup a1 and the graphite cup a2 are both inwardly facing.
[0031] In some embodiments, the graphite cup b1 and the graphite cup b2 are both opened inward.
[0032] In some embodiments, the outer diameter of the graphite cup b is greater than the outer diameter of the graphite cup a.
[0033] Compared with the prior art, the utility model has the following beneficial effects:
[0034] The existing steel cap material is replaced with graphite cup a, and graphite cup a is used as a heating electrode to improve the synthetic resistance and reduce power consumption; the outer diameter of graphite cup b as a secondary heating graphite electrode is larger than that of graphite cup a (primary heating cup) to avoid local overheating, and the graphite heating cup is used twice to heat and improve resistance; graphite sheet 1 and graphite sheet 2 are adjusted to control the growth rate at the same time; ceramic sheets prevent dolomite from being overburned to ensure stable resistance. The copper cup and copper sheet are used to evenly balance the top hammer temperature, and the density of dolomite ring molding is increased to improve thermal insulation and reduce power consumption. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] The accompanying drawings are part of the present invention and are used to provide a further understanding of the present invention. The schematic embodiments of the present invention and their descriptions are used to explain the present invention, but do not constitute an improper limitation on the present invention. Obviously, the accompanying drawings described below are only some embodiments. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without creative work.
[0036] In the attached picture:
[0037] Figure 1 This is a main cross-sectional view of a double graphite electrode synthesis colorless diamond large single crystal cavity device of the utility model.
[0038] Figure identification: 1- pyrophyllite block, 2- pyrophyllite ring, 3- copper cup, 4- copper sheet, 5- graphite cup a, 6- dolomite core, 7- small dolomite ring, 8- large dolomite ring, 9- alumina ring a, 10- graphite cup b, 11- alumina ring b, 12- alumina core, 13- graphite sheet one, 14- ceramic sheet, 15- nitrogen removal sheet, 16- carbon source, 17- catalyst, 18- magnesium oxide tube, 19- graphite tube, 20- insulating tube, 21- crystal bed, 21-1- seed crystal, 22- graphite sheet two.
[0039] It should be noted that these drawings and textual descriptions are not intended to limit the conceptual scope of the present invention in any way, but rather to illustrate the concept of the present invention for those skilled in the art by referring to specific embodiments. Implementation
[0040] In order to make the purpose, technical solutions and advantages of the embodiments of the utility model clearer, the technical solutions in the embodiments will be clearly and completely described below in conjunction with the drawings in the embodiments of the utility model. The following embodiments are used to illustrate the utility model but are not used to limit the scope of the utility model.
[0041] In the description of the present invention, it should be noted that the terms "upper", "lower", "front", "back", "left", "right", "vertical", "inside", "outside", etc. indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction. Therefore, they cannot be understood as limitations on the present invention.
[0042] like Figure 1 As shown, a double graphite electrode synthesis colorless diamond large single crystal cavity device includes a pyrophyllite block 1, two pyrophyllite rings 2, two copper cups 3, two copper sheets 4, a graphite cup a5, a dolomite core 6, two dolomite rings, two alumina rings a9, two graphite cups b10, two alumina rings b11, an alumina core 12, a graphite sheet 1 13, a ceramic sheet 14, a nitrogen removal sheet 15, a carbon source 16, a catalyst 17, a magnesium oxide tube 18, a graphite tube 19, an insulating tube 20, a crystal bed 21, and a graphite sheet 22.
[0043] The connection relationship of the above components is given below:
[0044] Continue to refer to Figure 1 As shown, the middle part of the pyrophyllite block 1 is provided with a through hole penetrating the upper and lower surfaces thereof; the pyrophyllite ring 1 of the two pyrophyllite rings 2 is placed at the upper end of the through hole in the middle part of the pyrophyllite block 1, and the pyrophyllite ring 2 is placed at the lower end of the through hole in the middle part of the pyrophyllite block 1; the copper cup 1 of the two copper cups 3 is placed in the pyrophyllite ring 1, and the copper cup 2 is placed in the pyrophyllite ring 2; the copper sheet 1 of the two copper sheets 4 is placed in the copper cup 1, and the copper sheet 2 is placed in the copper cup 2; the dolomite ring 1 of the two dolomite rings is placed in the copper cup 1, and the dolomite ring 2 is placed in the copper cup 2; the alumina ring a1 of the two alumina rings a9 is placed at the lower end of the dolomite ring, and the alumina ring a2 is placed at the upper end of the dolomite ring 2; the graphite cup a1 of the two graphite cups a5 is placed in the copper cup 1, and the graphite cup a2 is placed in the copper cup 2; the magnesium oxide tube 18 is placed in the through hole of the pyrophyllite block 1, and is located at the alumina ring one and between alumina rings b11; two alumina rings b11 are both placed in the magnesium oxide tube 18, alumina ring b1 is placed at the lower end of alumina ring a, and alumina ring b2 is placed at the upper end of alumina ring a2; the graphite cup b1 of the two graphite cups b10 is placed in the alumina ring b1 and is located at the lower end of graphite cup a, and the graphite cup b2 is placed in the alumina ring b2 and is located at the upper end of graphite cup a1; graphite sheet 13 is placed at the lower end of graphite cup b, and graphite sheet 22 is placed at the upper end of graphite cup b2; graphite tube 19 is placed in the magnesium oxide tube 18 and is located between graphite sheet 13 and graphite sheet 22; insulating tube 20 is placed in graphite tube 19; ceramic sheet 14, denitrification sheet 15, carbon source 16, catalyst 17, crystal bed 21 are all placed in insulating tube 20 and are located between graphite sheet 13 and graphite sheet 22.
[0045] Further solutions: continue to refer to Figure 1 As shown, the dolomite ring is composed of a small dolomite ring 7 and a large dolomite ring 8, specifically: dolomite ring 1 is composed of a small dolomite ring 1 and a large dolomite ring 1, and dolomite ring 2 is composed of a small dolomite ring 2 and a large dolomite ring 2; the large dolomite ring 1 is placed at the lower end of the small dolomite ring, and the large dolomite ring 2 is placed at the upper end of the small dolomite ring 2. The internal friction coefficient of dolomite is smaller than that of pyrophyllite, so the dolomite is made into a sleeve and installed inside the pyrophyllite cavity, which is conducive to improving the uniformity of pressure transmission. The dolomite ring does not play a sealing role, but only plays a heat preservation role. By increasing the molding density of the dolomite ring, the heat preservation performance can be further improved, and the effect of the volume shrinkage of pyrophyllite due to long-term high temperature and high pressure on the synthetic diamond large single crystal can be further improved.
[0046] Further solutions: continue to refer to Figure 1 As shown, both graphite cup a1 and graphite cup a2 are filled with dolomite core 6. Both graphite cup b1 and graphite cup b2 are filled with alumina core 12. Using graphite cup a as a heating electrode improves the synthetic resistance and reduces power consumption; graphite cup b as a secondary heating graphite electrode has a larger outer diameter than graphite cup a (primary heating cup) to avoid local overheating, and using the graphite heating cup twice for heating to improve resistance.
[0047] Further solutions: continue to refer to Figure 1 As shown, the ceramic sheet 14 is placed at the lower end of the graphite sheet 1 13 , the crystal bed 21 is placed at the upper end of the graphite sheet 2 22 , the denitrification sheet 15 is placed at the lower end of the ceramic sheet 14 , the catalyst 17 is placed at the upper end of the crystal bed 21 , and the carbon source 16 is placed between the denitrification sheet 15 and the catalyst 17 .
[0048] Further solutions: continue to refer to Figure 1 As shown, a seed crystal 21 - 1 is provided on the crystal bed 21 .
[0049] Further solutions: continue to refer to Figure 1 As shown, the thickness of the second graphite sheet 22 is greater than that of the first graphite sheet 13. The temperature difference between the first graphite sheet 13 and the second graphite sheet 22 is adjusted to control the growth rate; the ceramic sheet prevents the dolomite from being over-burned to ensure the stability of the resistance.
[0050] Further solutions: continue to refer to Figure 1 As shown, the openings of graphite cup a1 and graphite cup a2 are both facing inwards. The openings of graphite cup b1 and graphite cup b2 are both facing inwards. The outer diameter of graphite cup b10 is greater than the outer diameter of graphite cup a5.
[0051] In summary, the existing steel cap material is replaced with graphite cup a, and graphite cup a is used as a heating electrode to improve the synthetic resistance and reduce power consumption; the outer diameter of graphite cup b as a secondary heating graphite electrode is larger than that of graphite cup a (primary heating cup) to avoid local overheating, and the graphite heating cup is used twice to heat and improve the resistance; the temperature difference of graphite sheet 1 and graphite sheet 2 is adjusted at the same time to control the growth rate; the ceramic sheet avoids overburning of dolomite and ensures stable resistance. The copper cup and copper sheet evenly balance the top hammer temperature, increase the density of dolomite ring molding, improve thermal insulation, and reduce power consumption.
[0052] In the description provided herein, a large number of specific details are described. However, it is understood that embodiments of the present invention can be practiced without these specific details. In some instances, well-known methods, structures and techniques are not shown in detail so as not to obscure the understanding of this description.
[0053] In addition, those skilled in the art will understand that, although some embodiments described herein include certain features included in other embodiments but not other features, the combination of features of different embodiments also means being within the scope of protection of the present utility model and forming different embodiments. For example, in the above embodiments, those skilled in the art can use them in combination according to the known technical solutions and the technical problems to be solved by the present application.
[0054] The above is only a preferred embodiment of the utility model, and does not limit the utility model in any form. Although the utility model has been disclosed as a preferred embodiment as above, it is not used to limit the utility model. Any technician familiar with this patent can make some changes or modify the technical content suggested above into an equivalent embodiment with equivalent changes without departing from the scope of the technical solution of the utility model. However, any simple modification, equivalent change and modification made to the above embodiment based on the technical essence of the utility model without departing from the content of the technical solution of the utility model still falls within the scope of the solution of the utility model.
Claims
1. A double graphite electrode synthesis colorless diamond large single crystal cavity device, characterized in that: include: A pyrophyllite block, the middle of which is provided with a through hole penetrating the upper and lower surfaces thereof; Two pyrophyllite rings, pyrophyllite ring one is placed at the upper end of the through hole in the middle of the pyrophyllite block, and pyrophyllite ring two is placed at the lower end of the through hole in the middle of the pyrophyllite block; Two copper cups, copper cup one is placed in pyrophyllite ring one, and copper cup two is placed in pyrophyllite ring two; Two copper plates, copper plate one is placed in copper cup one, and copper plate two is placed in copper cup two; Two dolomite rings, dolomite ring one is placed in copper cup one, and dolomite ring two is placed in copper cup two; Two alumina rings a, alumina ring a-1 is placed at the lower end of the dolomite ring, and alumina ring a-2 is placed at the upper end of the dolomite ring; Two graphite cups a, graphite cup a1 is placed in copper cup a, and graphite cup a2 is placed in copper cup two; The magnesium oxide tube is placed in the through hole of the pyrophyllite block and is located between the first alumina ring and the second alumina ring; Two alumina rings b are placed in the magnesium oxide tube, with alumina ring b1 placed at the lower end of alumina ring a and alumina ring b2 placed at the upper end of alumina ring a2; Two graphite cups b, graphite cup b1 is placed in alumina ring b1 and is located at the lower end of graphite cup a, and graphite cup b2 is placed in alumina ring b2 and is located at the upper end of graphite cup a1; Two graphite sheets, graphite sheet one is placed at the lower end of graphite cup b, and graphite sheet two is placed at the upper end of graphite cup b2; A graphite tube is placed in the magnesium oxide tube and located between the first graphite sheet and the second graphite sheet; An insulating tube placed in a graphite tube; The ceramic sheet, the nitrogen removal sheet, the carbon source, the catalyst and the crystal bed are all placed in an insulating tube and located between the first graphite sheet and the second graphite sheet.
2. A double graphite electrode synthesis colorless diamond large single crystal cavity device according to claim 1, characterized in that: The dolomite ring one is composed of a small dolomite ring one and a large dolomite ring one, and the dolomite ring two is composed of a small dolomite ring two and a large dolomite ring two; the large dolomite ring one is placed at the lower end of the small dolomite ring, and the large dolomite ring two is placed at the upper end of the small dolomite ring two.
3. A double graphite electrode synthesis colorless diamond large single crystal cavity device according to claim 1, characterized in that: The graphite cup a1 and the graphite cup a2 are both filled with dolomite.
4. The double graphite electrode synthesis colorless diamond large single crystal cavity device according to claim 1, characterized in that: The graphite cup b1 and the graphite cup b2 are both filled with alumina cores.
5. The double graphite electrode synthesis colorless diamond large single crystal cavity device according to claim 1, characterized in that: The ceramic sheet is placed at the lower end of the graphite sheet, the crystal bed is placed at the upper end of the second graphite sheet, the denitrification sheet is placed at the lower end of the ceramic sheet, the catalyst is placed at the upper end of the crystal bed, and the carbon source is placed between the denitrification sheet and the catalyst.
6. The double graphite electrode synthesis colorless diamond large single crystal cavity device according to claim 1, characterized in that: A seed crystal is arranged on the crystal bed.
7. The double graphite electrode synthesis colorless diamond large single crystal cavity device according to claim 1, characterized in that: The thickness of the second graphite sheet is greater than the thickness of the first graphite sheet.
8. The double graphite electrode synthesis colorless diamond large single crystal cavity device according to claim 1, characterized in that: The graphite cup a1 and the graphite cup a2 are both opened inwards.
9. The double graphite electrode synthesis colorless diamond large single crystal cavity device according to claim 1, characterized in that: The graphite cup b1 and the graphite cup b2 both have openings facing inwards.
10. The double graphite electrode synthesis colorless diamond large single crystal cavity device according to claim 1, characterized in that: The outer diameter of the graphite cup b is greater than the outer diameter of the graphite cup a.
Citation Information
Cited By
Colorless diamond and preparation method thereof
CN119656978A
Colorless diamond and preparation method therefor
WO2026123536A1