Battery module welding pin and welding equipment

By designing battery module soldering pins with an eccentric structure, using aluminum oxide copper materials and rectangular contact surfaces, the problems of low efficiency and uncomfortable installation of existing soldering pins are solved, achieving efficient welding and stable current, and improving the efficiency of battery module welding. success rate.

CN221870623UActive Publication Date: 2024-10-22ROYPOW TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420888520.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-25
Publication Date
2024-10-22
Estimated Expiration
2034-04-25

AI Technical Summary

Technical Problem

The existing battery module welding pins are inefficient during the welding process and cannot cover two solder joints at the same time, resulting in increased welding times, low efficiency, and the design of the welding pins cannot meet the installation requirements.

Method used

Design a battery module welding pin, including a clamping part and a discharge part. The discharge part and the clamping part are not coaxial and form an eccentric structure. The contact surface covers two solder joints. The clamping part and the discharge part are made of C15760 alumina copper. Material, rectangular cross-section, increased contact area to improve current stability.

Benefits of technology

By increasing the contact area, the soldering pins can cover two soldering points at the same time, reducing the number of welding times, improving the welding efficiency and success rate, meeting the installation requirements of the soldering pins, and avoiding the problem of virtual soldering.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221870623U_ABST
    Figure CN221870623U_ABST
Patent Text Reader

Abstract

The utility model discloses a battery module welding pin and welding equipment, the battery module welding pin comprises a clamping part and a discharge part, the discharge part is connected with one end of the clamping part, one end face of the discharge part far away from the clamping part forms a contact surface, and the contact surface covers two welding spots during welding. By increasing the area of the contact surface, when the welding needle is used for welding the welding spots, the contact surface of the welding needle can cover the two welding spots at the same time, so that one welding needle discharges electricity to the two welding spots at the same time, the welding of the two welding spots is completed, the battery welding frequency is reduced, and the welding efficiency is effectively improved. And meanwhile, the magnitude of current passing through the discharge part instantly is effectively improved, so that the current is more stable, the pseudo soldering problem is avoided, and the success rate of welding the battery and the substrate is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of battery module welding machines, and in particular to a battery module welding pin and welding equipment. Background Art

[0002] In the production process of battery modules, the negative electrode of each battery needs to be welded to the substrate so that multiple batteries are connected in series through the substrate. During the welding process, one end of the welding needle is installed on the connection port of the welding equipment, and the other end of the welding needle contacts the battery module. The welding mechanism discharges through the welding needle to the preset cold solder joints between the substrate and the battery.

[0003] Each battery is connected to the substrate through four welding points. The traditional welding method is to use a single welding needle to weld the welding points. Please refer to Figure 1 , Figure 1 The welding pin of the prior art includes a connecting portion 10 and a welding portion 20, wherein the welding portion 20 is connected to one end of the connecting portion 10, and the connecting portion 10 and the welding portion 20 are coaxial. By setting two cylindrical welding pins, the circular surface of each welding pin welding portion 20 covers a corresponding welding spot, and the two welding pins perform spot welding twice to weld four welding spots, and the welding efficiency is low. In addition, since the distance between the two welding pins is very small, and the distance between the two connection ports of the welding equipment is relatively large, the welding pin of the prior art cannot meet the installation requirements. Utility Model Content

[0004] In view of the deficiencies in the prior art, a battery module welding pin and welding equipment are provided.

[0005] To achieve the above-mentioned purpose, the utility model provides a battery module welding pin, including a clamping part and a discharge part, wherein the discharge part is connected to one end of the clamping part, and an end surface of the discharge part away from the clamping part forms a contact surface, and during welding, the contact surface covers two welding points.

[0006] According to one embodiment of the present invention, the contact surface area S is in the range of 14.1 mm 2 ≤S≤14.3mm 2 .

[0007] According to an embodiment of the present invention, the central axis of the clamping portion and the central axis of the discharge portion are not collinear.

[0008] According to an embodiment of the present invention, the clamping portion and the discharge portion are integrally formed.

[0009] According to one embodiment of the present invention, the clamping portion and the discharge portion are made of alumina copper with a specification of C15760.

[0010] According to an embodiment of the present invention, the cross-section of the discharge portion is in a rectangular shape.

[0011] According to an embodiment of the present invention, the cross-sectional shape of the clamping portion is different from the cross-sectional shape of the discharge portion.

[0012] According to an embodiment of the present invention, the clamping portion has a first clamping surface and a second clamping surface that are arranged opposite to each other, the first clamping surface and the second clamping surface are parallel to each other, and both the first clamping surface and the second clamping surface are planes.

[0013] The utility model also provides a battery module welding device, comprising any of the above-mentioned battery module welding needles.

[0014] The beneficial effect of the utility model is that, by increasing the area of ​​the contact surface, when the welding needle is used to weld the welding point, the contact surface of the welding needle can cover two welding points at the same time, so that one welding needle discharges the two welding points at the same time, completes the welding of the two welding points, reduces the number of battery welding, and effectively improves the welding efficiency. At the same time, by increasing the area of ​​the contact surface, the amount of current passing through the discharge part instantly is effectively increased, making the current more stable, avoiding the problem of cold welding, and improving the success rate of welding the battery and the substrate. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:

[0016] Figure 1 It is a schematic diagram of a welding pin in the prior art;

[0017] Figure 2 is a schematic diagram of a battery module welding pin in an embodiment;

[0018] Figure 3 is a top view of a battery module welding pin in an embodiment;

[0019] Figure 4 2 is a cross-sectional view of the clamping portion in the embodiment.

[0020] Description of Reference Numerals

[0021] 1-clamping part; 11-first clamping surface; 12-second clamping surface; 2-discharging part; 21-contact surface; 10-connecting part; 20-welding part. DETAILED DESCRIPTION

[0022] The following will disclose multiple embodiments of the present invention with drawings. For the purpose of clear description, many practical details will be described together in the following description. However, it should be understood that these practical details should not be used to limit the present invention. In other words, in some embodiments of the present invention, these practical details are not necessary. In addition, in order to simplify the drawings, some conventional structures and components will be depicted in a simple schematic manner in the drawings.

[0023] In addition, in the present utility model, the descriptions of "first", "second", etc. are only used for descriptive purposes, and do not specifically refer to the order or sequence, nor are they used to limit the present utility model. They are only used to distinguish components or operations described with the same technical terms, and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the technical solutions between the various embodiments can be combined with each other, but they must be based on the ability of ordinary technicians in this field to implement them. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such a combination of technical solutions does not exist and is not within the scope of protection required by the present utility model.

[0024] Please refer to Figure 2 , Figure 2 Schematic diagram of a battery module welding pin in this embodiment. This embodiment provides a battery module welding pin, which includes a clamping portion 1 and a discharge portion 2. The discharge portion 2 is connected to one end of the clamping portion 1, and the axes of the clamping portion 1 and the discharge portion 2 are parallel to each other. The clamping portion 1 is used to connect with the discharge device, and the discharge portion 2 is used to contact with the substrate and the welding point of the battery module. When in use, the discharge device discharges to the clamping portion 1, and conducts the current to the discharge portion 2 through the clamping portion 1. Finally, the current is accurately released to the welding point of the battery module and the substrate through the discharge portion 2, thereby welding the battery module to the substrate.

[0025] The end surface of the discharge part 2 away from the clamping part 1 forms a contact surface 21. During welding, the contact surface 21 can cover two welding points at the same time, so that one welding needle discharges the two welding points at the same time, reducing the number of spot welding and effectively improving the welding efficiency. At the same time, by increasing the area of ​​the contact surface 21, the amount of current passing through the discharge part 2 instantly is effectively increased, making the current more stable, avoiding the problem of cold welding, and improving the success rate of welding between the battery and the substrate.

[0026] Furthermore, the area S of the contact surface 21 is in the range of 14.1 mm 2 ≤S≤14.3mm 2 , so that the contact surface 21 can cover two welding points at the same time.

[0027] In this embodiment, the contact surface area is 14.3 mm 2 The battery module welding pin in this embodiment is used for the welding production of 18650 battery modules. During installation, two welding pins are installed on the discharge device, and the clamping parts 1 of the two welding pins are respectively plugged into the two connection ports of the discharge device. During welding, the contact surface 21 of each welding pin covers two adjacent welding points, and the clamping part 1 receives the current of the discharge device. The current passes through the clamping part 1 and is then transmitted to the discharge part 2, and finally discharged to the welding point through the contact surface 21. Therefore, by setting two welding pins, welding is completed for four welding points each time, which improves the welding efficiency and effectively improves the welding quality.

[0028] Furthermore, the contact surface 21 is a rectangular surface, so that the contact surface 21 can cover two welding points at the same time, while reducing the contact area with other parts of the substrate, resulting in pressure damage to other parts of the substrate.

[0029] Furthermore, the clamping portion 1 and the discharge portion 2 are integrally formed, so that the welding pin structure is more stable.

[0030] Please refer to Figure 2 and Figure 3 , Figure 3 In addition, the clamping portion 1 and the discharge portion 2 are not coaxial, and the two form an eccentric structure, that is, the central axis of the clamping portion 1 and the central axis of the discharge portion 2 are not located on the same straight line.

[0031] Since the two connection ports of the discharge device are spaced relatively large, while the spacing between the two welding points is relatively small, the clamping portion 1 and the discharge portion 2 are not arranged coaxially, and the installation requirements of the welding pin are met without changing the connection port of the welding device. In addition, when the two welding pins are installed at the connection port of the welding device, by setting the welding pins as an eccentric structure, the cross-sectional area of ​​the clamping portion 1 can be effectively expanded while the installation positions of the two discharge portions 2 remain unchanged, so that the welding pins meet the conditions of high hardness and high wear resistance while having better conductivity.

[0032] Furthermore, the cross-sectional shape of the clamping portion 1 is different from the cross-sectional shape of the discharge portion 2. To meet both installation and welding requirements, in this embodiment, the cross-sectional shape of the clamping portion 1 matches the shape of the connection port, and the cross-sectional shape of the discharge portion 2 is rectangular.

[0033] Please refer to Figure 4 , Figure 41 is a cross-sectional view of the clamping portion. In addition, the clamping portion 1 has a first clamping surface 11 and a second clamping surface 12, which are arranged on opposite sides of the clamping portion 1, the first clamping surface 11 and the second clamping surface 12 are parallel to each other, and the first clamping surface 11 and the second clamping surface 12 are both planes. By providing the first clamping surface 11 and the second clamping surface 12, the contact area between the discharge device and the clamping portion 1 is effectively increased to prevent the welding needle from slipping.

[0034] Furthermore, to ensure the high conductivity of the welding needle, the clamping part 1 and the discharge part 2 are made of aluminum oxide copper material with specification model C15760. Model C15760 aluminum oxide copper material has the characteristics of high conductivity, heat resistance, wear resistance, and non-stick welding. It can effectively improve the qualified rate of battery module welding, reduce the rework rate and scrap rate of products, greatly improve the productivity of battery modules, and reduce the production cost of enterprises.

[0035] In summary, by increasing the area of ​​the contact surface, when the welding needle is used to weld the welding point, the contact surface 21 of the welding needle can cover two welding points at the same time, so that one welding needle discharges the two welding points at the same time, completes the welding of the two welding points, reduces the number of battery welding, and effectively improves the welding efficiency. At the same time, by increasing the area of ​​the contact surface 21, the amount of current passing through the discharge part 2 instantly is effectively increased, making the current more stable, avoiding the problem of cold welding, and improving the success rate of welding between the battery and the substrate. In addition, by setting the welding needle to an eccentric structure, the welding needle meets the installation requirements.

[0036] The above description is only an embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent substitution, improvement, etc. made within the spirit and principle of the present invention shall be included in the scope of the claims of the present invention.

Claims

1. A battery module welding pin, characterized in that: include: A clamping portion (1) and a discharge portion (2), wherein the discharge portion (2) is connected to one end of the clamping portion (1), and an end surface of the discharge portion (2) away from the clamping portion (1) forms a contact surface (21); during welding, the contact surface (21) covers two welding points.

2. The battery module welding pin according to claim 1, characterized in that: The area S of the contact surface (21) is in the range of 14.1 mm 2 ≤S≤14.3mm 2 .

3. The battery module welding pin according to claim 1, characterized in that: The central axis of the clamping portion (1) and the central axis of the discharge portion (2) are not collinear.

4. The battery module welding pin according to claim 1, characterized in that: The clamping portion (1) and the discharging portion (2) are integrally formed.

5. The battery module welding pin according to claim 1, characterized in that: The clamping portion (1) and the discharge portion (2) are made of alumina copper with a specification of C15760.

6. The battery module welding pin according to claim 1, characterized in that: The cross-section of the discharge portion (2) is in the shape of a rectangle.

7. The battery module welding pin according to claim 1, characterized in that: The cross-sectional shape of the clamping portion (1) is different from the cross-sectional shape of the discharge portion (2).

8. The battery module welding pin according to claim 1, characterized in that: The clamping portion (1) comprises a first clamping surface (11) and a second clamping surface (12) which are arranged opposite to each other, the first clamping surface (11) and the second clamping surface (12) are parallel to each other, and the first clamping surface (11) and the second clamping surface (12) are both planes.

9. A battery module welding device, characterized in that: Comprising the battery module welding pin described in any one of claims 1-8.