Perovskite thin film coating device and perovskite solar cell production system

By setting the overlapping area of ​​the first groove and the second groove in the perovskite film coating device to block the solution transmission path, the problem of perovskite solution flow pollution is solved and the performance of the solar cell is improved.

CN221934454UActive Publication Date: 2024-11-01BEI JING SHUO WEI GUANG DIAN KE JI YOU XIAN GONG SI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420512866.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-15
Publication Date
2024-11-01
Estimated Expiration
2034-03-15

AI Technical Summary

Technical Problem

During the perovskite film coating process, the perovskite solution easily flows from the edge of the substrate to the back, resulting in back contamination and affecting the film formation quality and solar cell performance.

Method used

A perovskite film coating device is designed, and the stage is provided with a first groove with an opening facing upwards near the edge of the base and a second groove with an opening facing downwards near the edge of the base to form an overlapping area to separate the solution transmission path. , collect excess solution dropped on the sides and back of the substrate to reduce contamination.

Benefits of technology

It effectively reduces the pollution of perovskite solution on the back of the substrate, improves the film formation quality, and improves the performance of solar cells.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221934454U_ABST
    Figure CN221934454U_ABST
Patent Text Reader

Abstract

The utility model provides a perovskite thin film coating device and a production system of a perovskite solar cell, and relates to the field of perovskite thin film preparation equipment. The perovskite film coating device comprises a carrying table and a substrate for coating a perovskite film, the substrate is placed on the upper surface of the carrying table, a first groove with an upward opening is formed in the periphery, close to the edge of the substrate, of the carrying table, and a second groove with a downward opening is formed in the periphery, close to the edge of the substrate, of the back face of the substrate. The first groove and the second groove have an overlapping region. Wherein the first groove and the second groove can cut off a transmission path of a solution on the surface of the carrying table and the back face of the substrate, the solution entering the second groove can flow into the first groove through an overlapping area of the first groove and the second groove, and the first groove collects redundant solution falling from the side edge and the back face of the substrate and is convenient to clean; pollution of the perovskite solution to the back of the substrate is reduced, the film forming quality is improved, and the performance of the solar cell is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of perovskite film preparation equipment, in particular to a perovskite film coating device and a perovskite solar cell production system. Background Art

[0002] Perovskite materials are neither calcium nor titanium, but a general term for a class of "ceramic oxides" with the same crystal structure, with a molecular formula of ABX3, such as Figure 1 As shown. A stands for "large radius cation", B stands for "metal cation", and X stands for "halogen anion". These three ions can present many magical physical properties, including but not limited to insulation, ferroelectricity, antiferromagnetism, giant magnetic effect, etc., through the arrangement and combination of different elements, or adjusting the distance between each other. Perovskite, as the most promising new material, can be used as the absorption layer of solar cells. It has many excellent optoelectronic properties, such as adjustable band gap, high absorption coefficient, low exciton binding energy, high carrier mobility, high defect tolerance, etc.; and the preparation process of perovskite is simple, which can achieve semi-transparency, ultra-light, ultra-thin, and flexible; the raw materials of perovskite are widely available and rich in content. These advantages make perovskite solar cells a new generation of technology that subverts crystalline silicon and thin-film solar cells.

[0003] At present, the perovskite light-absorbing layer is mostly prepared by the solution method, that is, the prepared perovskite powder is added to the solvent to make a perovskite precursor solution, and the perovskite precursor solution is evenly coated on the substrate surface by spin coating, slit coating, scraping or micro-concave coating technology to form a liquid film. The liquid film sample is removed from the coating device and placed in a VCD (Vacuum concentrate drying) vacuum flash evaporation device for rapid vacuuming (10 seconds to reach 20Pa) to quickly evaporate the low-boiling point solvent, and finally a high-temperature annealing on a heating table is performed to form a polycrystalline perovskite film. Figure 2 As shown, during the coating process, the existing substrate 2 of the sample is placed on the surface of the existing stage 1 of the coating device and fixed by vacuum adsorption; the perovskite solution 3 is evenly covered on the surface of the substrate by the coating device, but the perovskite solution 3 is very easy to flow from the edge of the existing substrate 2 to the back of the existing substrate 2, and continuously spread to the inside of the back of the existing substrate 2 along the gap between the back of the existing substrate 2 and the existing stage 1, causing the back of the existing substrate 2 to be contaminated, which will affect the film quality during high-temperature annealing and crystallization; the contaminated part on the back may also affect the light absorption and reduce the efficiency; it may also affect the flatness of the subsequent coated substrate, and ultimately affect the performance of the perovskite solar cell.

[0004] In view of this, the present utility model is proposed. Utility Model Content

[0005] The utility model aims to provide a perovskite film coating device and a perovskite solar cell production system.

[0006] The embodiment of the utility model is achieved as follows:

[0007] In a first aspect, the utility model provides a perovskite film coating device, which includes a carrier and a substrate for coating the perovskite film, the substrate is placed on the upper surface of the carrier, the carrier is provided with a first groove opening upward around the edge of the substrate, the back side of the substrate is provided with a second groove opening downward around the edge of the substrate, and the first groove and the second groove have an overlapping area.

[0008] In an optional embodiment, the first groove has a depth H1 and a width L1, wherein 0<L1≤5cm, 0

[0009] In an optional embodiment, the second groove has a depth H2 and a width L2, wherein 0<H2≤3mm, 0<L2≤5mm.

[0010] In an optional embodiment, the width of the outer edge of the second groove from the edge of the substrate is L3, wherein 0<L3≤5cm.

[0011] In an optional embodiment, the width of the overlapping area is L4, where 0<L4<5cm.

[0012] In an optional embodiment, the cross-section of the first groove and the second groove is a quadrilateral, a semicircular, or a structure with a quadrilateral opening and an arc-shaped bottom.

[0013] In an optional embodiment, when the cross-sections of the first groove and the second groove are structures with a quadrilateral opening and an arc-shaped bottom, the ratio of the depth of the quadrilateral opening to the depth of the arc-shaped bottom is 1:0.4-0.5.

[0014] In an optional embodiment, the number of the second grooves is at least one. When the number of the second grooves is plural, the width between any two adjacent second grooves is greater than 0 and less than 5 cm.

[0015] In an optional embodiment, a vacuum adsorption mechanism is disposed in the carrier, and the substrate is disposed on the carrier through the vacuum adsorption mechanism.

[0016] In a second aspect, the utility model provides a production system for a perovskite solar cell, which includes a perovskite thin film coating device as described in any one of the aforementioned embodiments.

[0017] The beneficial effects of the embodiments of the utility model are: ​

[0018] The perovskite film coating device provided by the utility model is provided with a first groove opening upward around the carrier near the edge of the substrate, and a second groove opening downward is provided around the back side of the substrate near the edge of the substrate, wherein the first groove can block the transmission path of the solution on the carrier surface, and the second groove can block the transmission path of the solution on the back side of the substrate. The solution entering the second groove can also flow into the first groove through the overlapping area of ​​the first groove and the second groove. The first groove collects the excess solution dropped from the side and back side of the substrate for easy cleaning. This solution can reduce the contamination of the back side of the substrate by the perovskite solution, improve the film forming quality, and enhance the performance of the solar cell. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] In order to more clearly illustrate the technical solutions of the embodiments of the utility model, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the utility model and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other relevant drawings can be obtained based on these drawings without paying creative work.

[0020] Figure 1 A schematic diagram of the crystal structure of the perovskite material mentioned in the background technology of the present utility model;

[0021] Figure 2 It is a structural schematic diagram of the existing coating device mentioned in the background technology of the present utility model;

[0022] Figure 3 A schematic structural diagram of a perovskite thin film coating device provided in the first embodiment of the utility model;

[0023] Figure 4 for Figure 3 The enlarged view of point A in the middle;

[0024] Figure 5 A schematic structural diagram of a perovskite thin film coating device provided in the second embodiment of the utility model;

[0025] Figure 6 A schematic structural diagram of a perovskite thin film coating device provided in the third embodiment of the utility model;

[0026] Figure 7 This is a schematic structural diagram of a perovskite thin film coating device provided in the fourth embodiment of the present utility model.

[0027] Icons: 1-existing stage; 2-existing substrate; 3-perovskite solution;

[0028] 100 - perovskite thin film coating device; 110 - carrier; 111 - first groove; 120 - substrate; 121 - second groove. DETAILED DESCRIPTION

[0029] In order to make the purpose, technical scheme and advantages of the embodiments of the utility model clearer, the technical scheme in the embodiments of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiments of the utility model. Obviously, the described embodiments are part of the embodiments of the utility model, not all of the embodiments. Generally, the components of the embodiments of the utility model described and shown in the drawings here can be arranged and designed in various different configurations.

[0030] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the present invention to be protected, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0031] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.

[0032] In the description of the present utility model, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inside", "outside", etc. indicate the orientation or position relationship based on the orientation or position relationship shown in the accompanying drawings, or the orientation or position relationship in which the utility model product is usually placed when in use, which is only for the convenience of describing the utility model and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present utility model. In addition, the terms "first", "second", "third", etc. are only used to distinguish the description, and cannot be understood as indicating or implying relative importance.

[0033] In addition, the terms "horizontal", "vertical" and the like do not mean that the components are required to be absolutely horizontal or suspended, but can be slightly tilted. For example, "horizontal" only means that its direction is more horizontal than "vertical", and does not mean that the structure must be completely horizontal, but can be slightly tilted.

[0034] In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "set", "install", "connect", and "connect" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0035] Please refer to Figure 3-Figure 7 The utility model provides a perovskite film coating device 100, which includes a carrier 110 and a substrate 120 for coating the perovskite film, the substrate 120 is placed on the upper surface of the carrier 110, specifically, a vacuum adsorption mechanism is provided in the carrier 110, and the substrate 120 is set on the carrier 110 through the vacuum adsorption mechanism.

[0036] The stage 110 is provided with a first groove 111 opening upward around the edge of the base 120 , and the back side of the base 120 is provided with a second groove 121 opening downward around the edge of the base 120 . The first groove 111 and the second groove 121 have an overlapping area.

[0037] In the utility model, the first groove 111 can block the transmission path of the solution on the surface of the carrier 110, and the second groove 121 can block the transmission path of the solution on the back of the substrate 120. At the same time, the first groove 111 can also collect excess solution dropped from the side and back of the substrate 120 for easy cleaning; this solution can reduce the contamination of the perovskite solution on the back of the substrate 120, improve the film formation quality, and enhance the performance of solar cells.

[0038] The first groove 111 has a depth H1 and a width L1, 0

[0039] The second groove 121 has a depth H2 and a width L2, wherein 0<H2≤3 mm, 0<L2≤5 mm.

[0040] The width of the outer edge of the second groove 121 from the edge of the substrate 120 is L3, where 0<L3≤5cm. The width of the overlapping area is L4, where 0<L4<5cm.

[0041] ​In the utility model, the cross-sectional shape of the first groove 111 and the second groove 121 can have a variety of shapes, including but not limited to a quadrilateral, a semicircular or a quadrilateral opening with an arc-shaped bottom structure. It should be understood that the depth and width of the first groove 111 and the second groove 121 can be adaptively adjusted according to the selection of the cross-sectional shape of the first groove 111 and the second groove 121. As long as it is possible to separate the transmission path of the solution on the surface of the carrier 110 and the transmission path of the solution on the back of the substrate 120. Among them, when the cross-section of the first groove 111 and the second groove 121 is a quadrilateral opening with an arc-shaped bottom structure, the arc-shaped bottom can be an arc or a semicircle, and the ratio of the depth of the quadrilateral opening to the depth of the arc-shaped bottom is 1:0.4-0.5.

[0042] In other embodiments of the present invention, the number of the second grooves 121 is at least one, and when the number of the second grooves 121 is multiple, the width between any two adjacent second grooves 121 is greater than 0 and less than 5 cm. Multiple second grooves 121 can better isolate the transmission path of the perovskite solution on the back of the substrate 120, further improve the film quality, and improve the battery performance.

[0043] In addition, the utility model also provides a production system of a perovskite solar cell, which includes the above-mentioned perovskite thin film coating device 100.

[0044] The working principle of the above-mentioned perovskite thin film coating device 100 is: a first groove 111 with an opening upward is arranged around the edge of the carrier 110 near the substrate 120, and a second groove 121 with an opening downward is arranged around the back side of the substrate 120 near the edge of the substrate 120, wherein the first groove 111 can block the transmission path of the solution on the surface of the carrier 110, and the second groove 121 can block the transmission path of the solution on the back side of the substrate 120. The solution entering the second groove 121 can also flow into the first groove 111 through the overlapping area of ​​the first groove 111 and the second groove 121. The first groove 111 collects the excess solution dropped from the side and back side of the substrate 120 for easy cleaning; this solution can reduce the contamination of the perovskite solution on the back side of the substrate 120, improve the film forming quality, and improve the performance of solar cells.

[0045] The invention is further explained below with reference to specific embodiments.

[0046] First embodiment

[0047] Please refer to Figure 3 and Figure 4 This embodiment provides a perovskite thin film coating device 100 , which includes a carrier 110 and a substrate 120 for coating the perovskite thin film, and the substrate 120 is placed on the upper surface of the carrier 110 .

[0048] The first groove 111 with an opening facing upward is arranged around the edge of the carrier 110 near the base 120. The cross-sectional shape of the first groove 111 is a structure with a quadrilateral opening and an arc-shaped bottom. The first groove 111 has a depth H1 and a width L1, 0

[0049] The back side of the substrate 120 is provided with a second groove 121 with an opening facing downward near the edge of the substrate 120. The cross-sectional shape of the second groove 121 is a structure with a quadrilateral opening and an arc-shaped bottom. The second groove 121 has a depth H2 and a width L2, 0<H2≤3mm, 0<L2≤2mm. At this time, the ratio of the depth of the quadrilateral opening to the depth of the arc-shaped bottom is 1:0.5. The width of the outer edge of the second groove 121 from the edge of the substrate 120 is L3, where 0<L3≤5cm. In this embodiment, when the cross-sectional shape of the second groove 121 is defined as a structure with a quadrilateral opening and an arc-shaped bottom, the size range of H2 and L2 should be within 0<H2≤3mm, 0<L2≤2mm. This is because the maximum value of H2 of the structure with a quadrilateral opening and an arc-shaped bottom increases, and the width should be correspondingly reduced to avoid the setting of the second groove 121 affecting the strength of the substrate 120.

[0050] The first groove 111 and the second groove 121 have an overlapping area, and the width of the overlapping area is L4, wherein 0<L4<5cm.

[0051] Second embodiment

[0052] Please refer to Figure 5 This embodiment provides a perovskite thin film coating device 100 , which includes a carrier 110 and a substrate 120 for coating the perovskite thin film, and the substrate 120 is placed on the upper surface of the carrier 110 .

[0053] The first groove 111 with an opening facing upward is arranged around the edge of the carrier 110 near the base 120. The cross-sectional shape of the first groove 111 is a structure with a quadrilateral opening and an arc-shaped bottom. The first groove 111 has a depth H1 and a width L1, 0

[0054] ​​A second groove 121 with an opening downward is provided on the back side of the substrate 120 near the edge of the substrate 120. The cross-sectional shape of the second groove 121 is semicircular. The second groove 121 has a depth H2 and a width L2, 0<H2≤2mm, 0<L2≤5mm. The width of the outer edge of the second groove 121 from the edge of the substrate 120 is L3, wherein 0<L3≤5cm. In this embodiment, when the cross-sectional shape of the second groove 121 is semicircular, the size range of H2 and L2 is defined as 0<H2≤2mm, 0<L2≤5mm. This is because the maximum value of H2 of the semicircular structure is reduced, and the width adaptability is increased, so that the size of the second groove 121 is expanded without affecting the strength of the substrate 120 due to the setting of the second groove 121.

[0055] The first groove 111 and the second groove 121 have an overlapping area, and the width of the overlapping area is L4, wherein 0<L4<5cm.

[0056] Third embodiment

[0057] Please refer to Figure 6 This embodiment provides a perovskite thin film coating device 100 , which includes a carrier 110 and a substrate 120 for coating the perovskite thin film, and the substrate 120 is placed on the upper surface of the carrier 110 .

[0058] The first groove 111 with an opening facing upward is arranged around the edge of the carrier 110 near the base 120. The cross-sectional shape of the first groove 111 is a structure with a quadrilateral opening and an arc-shaped bottom. The first groove 111 has a depth H1 and a width L1, 0

[0059] A second groove 121 with an opening downward is provided on the back side of the substrate 120 near the edge of the substrate 120. The cross-sectional shape of the second groove 121 is a quadrilateral. The second groove 121 has a depth H2 and a width L2, 0<H2≤2mm, 0<L2≤4mm. The width of the outer edge of the second groove 121 from the edge of the substrate 120 is L3, wherein 0<L3≤5cm. In this embodiment, it is defined that when the cross-sectional shape of the second groove 121 is a quadrilateral, the size range of H2 and L2 should be within 0<H2≤2mm, 0<L2≤4mm. This is because when the width is constant, the area of ​​the quadrilateral is greater than the area of ​​the semicircle. Therefore, in this embodiment, the maximum value of L2 is slightly reduced compared to the second embodiment, and the size of the second groove 121 is expanded under the premise of avoiding the setting of the second groove 121 affecting the strength of the substrate 120.

[0060] The first groove 111 and the second groove 121 have an overlapping area, and the width of the overlapping area is L4, wherein 0<L4<5cm.​

[0061] Fourth embodiment

[0062] Please refer to Figure 7 This embodiment provides a perovskite thin film coating device 100 , which includes a carrier 110 and a substrate 120 for coating the perovskite thin film, and the substrate 120 is placed on the upper surface of the carrier 110 .

[0063] The first groove 111 with an opening facing upward is arranged around the edge of the carrier 110 near the base 120. The cross-sectional shape of the first groove 111 is a structure with a quadrilateral opening and an arc-shaped bottom. The first groove 111 has a depth H1 and a width L1, 0

[0064] The back side of the substrate 120 is provided with second grooves 121 opening downward near the edges of the substrate 120. The number of the second grooves is 2. The cross-sectional shape of the second grooves 121 is a structure of a quadrilateral opening and an arc-shaped bottom. The second grooves 121 have a depth H2 and a width L2, 0<H2≤3mm, 0<L2≤2mm. At this time, the ratio of the depth of the quadrilateral opening to the depth of the arc-shaped bottom is 1:0.5. The width of the outer edge of the second groove 121 from the edge of the substrate 120 is L3, wherein 0<L3≤5cm.

[0065] The first groove 111 and the second groove 121 have an overlapping area, and the width of the overlapping area is L4, wherein 0<L4<5cm.

[0066] In summary, the perovskite thin film coating device 100 provided by the utility model is provided with a first groove 111 opening upward around the edge of the carrier 110 near the substrate 120, and a second groove 121 opening downward is provided around the back side of the substrate 120 near the edge of the substrate 120, wherein the first groove 111 can block the transmission path of the solution on the surface of the carrier 110, and the second groove 121 can block the transmission path of the solution on the back side of the substrate 120. The solution entering the second groove 121 can also flow into the first groove 111 through the overlapping area of ​​the first groove 111 and the second groove 121. The first groove 111 collects the excess solution dropped from the side and back side of the substrate 120 for easy cleaning; this solution can reduce the contamination of the back side of the substrate 120 by the perovskite solution, improve the film forming quality, and improve the performance of solar cells.

[0067] ​The above description is only the preferred embodiment of the utility model, and is not intended to limit the utility model. For those skilled in the art, the utility model can have various modifications and changes. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the utility model shall be included in the protection scope of the utility model.

Claims

1. A perovskite thin film coating device, characterized in that: It includes a carrier and a substrate for coating the perovskite film, the substrate is placed on the upper surface of the carrier, the carrier is provided with a first groove opening upward around the edges of the substrate, the back side of the substrate is provided with a second groove opening downward around the edges of the substrate, and the first groove and the second groove have an overlapping area.

2. The perovskite thin film coating device according to claim 1, characterized in that: The first groove has a depth H1 and a width L1, wherein 0<H1≤7.5cm, 0<L1≤5cm.

3. The perovskite thin film coating device according to claim 1, characterized in that: The second groove has a depth H2 and a width L2, wherein 0<H2≤3mm, 0<L2≤5mm.

4. The perovskite thin film coating device according to claim 1, characterized in that: The width of the outer edge of the second groove from the edge of the substrate is L3, wherein 0<L3≤5cm.

5. The perovskite thin film coating device according to claim 1, characterized in that: The width of the overlapping area is L4, wherein 0<L4<5cm.

6. The perovskite thin film coating device according to any one of claims 1 to 5, characterized in that: The cross-sections of the first groove and the second groove are quadrilateral, semicircular, or quadrilateral with an opening and an arc-shaped bottom.

7. The perovskite thin film coating device according to claim 6, characterized in that: When the cross-sections of the first groove and the second groove are structures with a quadrilateral opening and an arc-shaped bottom, the ratio of the depth of the quadrilateral opening to the depth of the arc-shaped bottom is 1:0.4-0.

5.

8. The perovskite thin film coating device according to any one of claims 1 to 5, characterized in that: The number of the second grooves is at least one. When the number of the second grooves is plural, the width between any two adjacent second grooves is greater than 0 and less than 5 cm.

9. The perovskite thin film coating device according to any one of claims 1 to 5, characterized in that: A vacuum adsorption mechanism is arranged in the carrier, and the substrate is arranged on the carrier through the vacuum adsorption mechanism.

10. A production system for perovskite solar cells, characterized in that: It comprises the perovskite thin film coating device as described in any one of claims 1 to 9.