Low-rebound foam for touch screen and electronic product

By performing matrix punching and multi-layer structure treatment on the foam, the rebound force of the foam is reduced and the cushioning performance is improved, and the problems of excessive rebound force and fiber fall off in existing foam materials in lightweight electronic products are solved, achieving Better usage and screen protection.

CN221940370UActive Publication Date: 2024-11-01SUZHOU HI TECH ELECTRONICS CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420618145.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-28
Publication Date
2024-11-01
Estimated Expiration
2034-03-28

AI Technical Summary

Technical Problem

The existing foam material has too much rebound force after compression, resulting in uneven color of the touch screen, and the fibers fall off and contaminate the screen after long-term use, making it difficult to meet the buffering and sealing needs of light and thin electronic products.

Method used

By laser or die-cutting matrix drilling of foam, a porous structure is formed, and a flexible glue layer and foamed substrate layer are added to its surface to form a multi-layer structure, reducing rebound force and increasing buffering performance, while supporting resistance Scrape the coating to prevent the fiber from falling off.

Benefits of technology

It effectively reduces the compression rebound force of the foam, improves the cushioning and friction resistance, extends the service life of the touch screen, and avoids contamination caused by fiber shedding.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221940370U_ABST
    Figure CN221940370U_ABST
Patent Text Reader

Abstract

The utility model provides low-rebound foam for a touch screen and an electronic product. The low-rebound foam is of a multi-layer structure which is arranged in an attached mode and at least comprises a low-density foam layer and a first buffering structure layer which are arranged in an attached mode. The first buffer structure layer is composed of a first flexible glue layer, a foaming base material layer and a second flexible glue layer which are sequentially arranged in an attached mode. The porous structure comprises a plurality of regularly arranged through holes formed in the thickness direction, and the first buffer structure layer is adhered to the surface of the battery module. According to the utility model, a filling foam material in the prior art adopts a matrix-arranged through hole structure under the condition that the thickness is not changed to reduce the rebound force of the compressed foam, the filling effect is not influenced, and the requirement on the compression rebound force of an assembled electronic product, especially the use scene of a touch screen, is not influenced. The service performance can be improved, and the service life of the electronic product assembly can be prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of adhesive tapes, in particular to a low-rebound super foam cotton used for touch screens and electronic products. Background Art

[0002] With the development of the economy, electronic products in the consumer electronics field are being updated and iterated at an increasingly rapid pace. Electronic products in the 3C industry are becoming thinner and lighter. The market has higher requirements for the lightweight and user experience of electronic products. Therefore, there are higher requirements for the structural design, materials and performance of electronic products.

[0003] Generally, when assembling electronic products with touch functions, such as mobile phones and tablets, the battery module and other bottom components are installed first, and then the entire screen module is fixed directly on the battery module. The gap between the battery module and the screen module is usually filled with foam, which not only plays a role in buffering and sealing, but also can isolate the battery and the touch screen, protect the safety performance and touch feel of the screen during use, thereby improving the service life of the touch screen and customer experience. During installation, the foam material is generally bonded to the battery on one side, and the other side of the foam is in contact with the screen module.

[0004] Furthermore, the traditional 3C industry filling buffer foam is conventional foam, which can be set with single-sided or double-sided adhesive. However, due to the trend of 3C products to be thin and light, the space that can be filled is very small. Generally, the thickness of the gap that can be filled is between 0.1 and 0.5 mm. When the screen module and the battery module are assembled and used, the force causes the foam to be compressed. Since the material of the contact surface is glass, which is relatively fragile, the rebound force of the foam after being compressed cannot be too large. Moreover, the foam material of appropriate thickness is selected according to the size of the gap between the components. During the use of electronic products using this filling material and assembly structure, the screen will be slightly deformed when the finger presses the screen, and the pressing force directly acts on the foam under the screen, causing the foam to deform. The force disappears, and then the original shape is restored according to the resilience of the foam. However, the foam materials currently on the market are difficult to meet this requirement. The foam products available in the prior art generally have a large rebound force generated by compression and rebound after being subjected to external force. Taking 0.35mm foam as an example, the rebound pressure when compressed by 25% is at least 1.4KPa. This rebound pressure causes uneven color on the touch screen when the screen is pressed.

[0005] On the other hand, when electronic products are used for a long time, the expansion caused by the continuous heating of the battery causes the gap between the battery and the screen to become smaller. The foam is compressed by the expanded battery and the rebound force acts on the screen, causing the screen to be partially lifted by external force, resulting in uneven color of the entire screen. Especially for lightweight electronic products, the gap between the battery module and the screen module is even narrower. On the one hand, it is necessary to use a filler with a certain compression rebound force to meet the use needs of the touch screen. On the other hand, it is necessary to reduce the impact of the compression rebound force on the touch screen in the gap of the limited assembly space. Simply reducing the thickness of the filling material cannot meet the buffer sealing function. This requires that the filling material must be thin enough to fill the gap in the middle, and must have a low rebound force when compressed so as not to affect the use of the screen.

[0006] At the same time, the surface of conventional foam is easily damaged after long-term use, or repeated pressing of the screen causes friction between the bottom of the screen module and the foam surface, causing the foam's fiber structure to fall off due to external force to form fiber debris, thereby contaminating the screen and reducing material performance.

[0007] Based on the above-mentioned problems existing in the prior art, the utility model provides a foam material with low density and low rebound force, which can not only solve the ultra-low rebound force effect of the compressed foam, but also has excellent cushioning performance, while also providing the material surface with greater friction resistance, and will not affect the performance of the screen module. Utility Model Content

[0008] In view of this, in order to solve the above problems, the utility model provides a low-rebound ultra-soft foam and electronic product for touch screens. The foam in the prior art is subjected to matrix punching processing by laser or die-cutting to reduce its rebound force, and its cushioning performance is improved by adding a functional layer. The formed foam with a multi-layer structure has the mechanical properties of low rebound performance, and while maintaining the thickness of the foam, it ensures that the gaps between modules are completely filled, and can also improve the performance of the touch screen.

[0009] In order to achieve the above-mentioned purpose, the utility model provides a low-rebound ultra-soft foam for a touch screen, which at least includes a first foam layer and a first buffer structure layer which are laminated together; the first buffer structure layer is composed of a first flexible glue layer-a foaming substrate layer-a second flexible glue layer which are laminated together in sequence; the low-density foam layer has a layered foam material with a porous structure, and the porous structure is composed of a plurality of regularly arranged through holes opened along the thickness direction, and the first buffer structure layer is bonded to the surface of the battery module.

[0010] The first buffer structure layer (first flexible glue layer-foamed substrate layer-second flexible glue layer) of the multi-layer structure arranged at the bottom has a soft structural layer. The flexible glue layer wraps the foamed substrate and can absorb the elastic force transmitted to the bottom due to pressing the touch screen during use, thereby further protecting the touch screen.

[0011] Preferably, the thickness of the low-density foam layer is 0.2-1 mm; the diameter of the through hole is 0.5-2 mm; and the spacing between each through hole is 0.8-1 mm.

[0012] Preferably, the foam substrate layer is a foam material with a thickness of 0.05 to 0.1 mm.

[0013] Preferably, the porous structure is composed of a plurality of straight through holes or oblique through holes at equal distances.

[0014] More preferably, the through holes in the porous structure are arranged in a matrix.

[0015] As a preferred implementation, the inclination angle of the inclined through hole along the horizontal direction of the foam is 45°≤a<90°.

[0016] Preferably, the first flexible glue layer and / or the second flexible glue layer is an elastic acrylic glue layer.

[0017] Preferably, an elastic layer is provided in the acrylic glue layer, and the elastic layer is composed of built-in foamed microspheres.

[0018] Preferably, the foamed microspheres are evenly distributed inside the acrylic glue layer.

[0019] Preferably, the particle size of the foamed microspheres is 20 to 50 μm.

[0020] Preferably, the low-rebound ultra-soft foam comprises a multi-layer structure of a protective functional layer - the low-density foam layer - the first buffer structure layer which is arranged in a close-fitting manner.

[0021] Preferably, the protective functional layer is a scratch-resistant single-sided tape, which is attached to the surface of the low-density foam layer. During the long-term use of electronic products, the friction between modules and other external forces will cause the fiber structure of the foam to fall off due to external forces to form fiber scraps, especially when the foam includes multiple through-hole structures, which increases the contact area between foams, between foams and screens, and between foams and batteries. The friction is further increased compared to the non-perforated foam in the prior art, and it is easier to fall off. The tiny fiber scraps that fall off affect the performance of other components in the electronic product, and the protective functional layer can prevent the friction of the foam surface caused by frequent pressing of the touch screen during use, and prevent the fiber scraps from falling off. In particular, the use of a protective functional layer can shield the porous structure of the foam without affecting the buffering or continuity performance.

[0022] Preferably, a fifth flexible glue layer is further provided between the protective functional layer and the low-density foam layer; the fifth flexible glue layer is an acrylic glue layer. Laminating the surface of the low-density foam layer with an acrylic glue layer can improve the bonding strength between the coating of the protective functional layer and the foam, and further protect the low-density foam layer.

[0023] Preferably, it comprises a multilayer structure of the second buffer structure layer - the low-density foam layer - the first buffer structure layer which are arranged in sequence.

[0024] More preferably, the structure of the second buffer structure layer is the same as that of the first buffer structure layer. The buffer structure layer is arranged on both the upper and lower sides of the first low-density foam layer, which can significantly improve the buffering performance of the entire foam multilayer structure. In particular, the second buffer structure layer also has adhesive properties, which can fix the foam on the touch screen surface or between other modules in special circumstances, thereby broadening the scope of use of the foam.

[0025] The foam provided based on the above technical solution, compared with cotton filling materials of the same thickness and the same material, has a rebound force per unit area reduced by 20% to 50% when compressed by 25%, which can meet the use requirements of the touch screen, and the foam has no effect on the filling of the gap between the battery module and the screen module, and the overall cushioning performance is further improved.

[0026] Beneficial technical effects obtained by the utility model:

[0027] 1. The utility model reduces the rebound force of the foam after compression by using matrix punching or matrix equidistant punching and other methods while maintaining the thickness of the filling foam material in the prior art. Compared with conventional foam, its compression rebound force is reduced by 20-50% without affecting its filling effect. It is suitable for scenarios where there are requirements for the compression rebound force of assembled electronic products, especially touch screen usage scenarios, and can improve their performance and the service life of electronic product components.

[0028] 2. The low-rebound foam material with a multi-layer structure provided by the utility model can select the hardness and thickness of the low-density foam according to the filling requirements, and set the through-hole structure with different arrangements or apertures to meet the design and processing of different rebound forces, and can make full use of the most commonly used foam material with a thickness of 0.2 to 1.0 mm in the existing market electronics industry. There is no need to improve the material itself. Only simple structural processing is required and the appropriate thickness, hole size and hole density can be selected according to the assembly gap and use requirements. The operation is simple, the cost is low, and the effect is excellent.

[0029] 3. In the technical solution adopted by the utility model, the bottom bonding includes a multi-layer structure composed of a foam substrate layer wrapped with an acrylic glue layer, and an elastic layer is arranged in the acrylic glue layer to improve the cushioning performance. While having excellent viscoelastic properties, the cushioning effect can also be further improved. At the same time, the substrate preferably adopts a VHB foam substrate, so that the entire bottom double-sided adhesive also has excellent cushioning performance, absorbs the energy transmitted by the rebound force of the low-density foam, thereby providing compression and cushioning performance for the entire foam multi-layer structure, thereby better protecting the components of electronic products.

[0030] 4. The utility model adheres a scratch-resistant coating + modified acrylic glue to the low-density foam layer after the through holes are set. After contacting with the screen module, it is not only scratch-resistant and does not drop chips, but also can cover the punching position, without affecting the appearance and usage of the foam material. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Figure 1 This is a schematic diagram of the porous structure of the low-density foam layer provided in Example 1 of the present utility model.

[0032] Figure 2 This is a schematic diagram of the multi-layer structure of the low-rebound ultra-soft foam provided in Example 1 of the present invention.

[0033] Figure 3 This is a schematic diagram of the multi-layer structure of the low-rebound ultra-soft foam provided in Example 2 of the present utility model.

[0034] Figure 4 This is a schematic diagram of the multi-layer structure of the low-rebound ultra-soft foam provided in Example 3 of the present utility model.

[0035] Figure 5 This is a schematic diagram of the multi-layer structure of the low-rebound ultra-soft foam provided in Example 4 of the present utility model.

[0036] Figure 6 This is a schematic diagram of the multi-layer structure of the low-rebound ultra-soft foam provided in Example 4 of the present utility model.

[0037] Among them, the accompanying drawings are marked: 10, low-density foam layer; 101, through hole; 20 first buffer structure layer; 201, first flexible glue layer; 202, first foam substrate layer; 203, second flexible glue layer; 30, second buffer structure layer; 301, third flexible glue layer; 302, second foam substrate layer; 303, fourth flexible glue layer 303; 40, protective function layer; 50, fifth flexible glue layer. DETAILED DESCRIPTION

[0038] In order to make the purpose, technical scheme and advantages of the utility model clearer, the technical scheme in the embodiment of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiment of the present application. Obviously, the described embodiment is only a part of the embodiment of the present application, not all of the embodiments.

[0039] The utility model provides a low-rebound ultra-soft foam for a touch screen, which at least comprises a low-density foam layer and a first buffer structure layer which are laminated together; the first buffer structure layer is composed of a first flexible glue layer-a foaming substrate layer-a second flexible glue layer which are laminated together in sequence; the low-density foam layer is a layered foam material with a porous structure, the porous structure comprises a plurality of through holes which are regularly arranged in a matrix and opened in a thickness direction, and the first buffer structure layer is bonded to the surface of the battery module.

[0040] As a preferred embodiment, the porous structure is composed of a plurality of equidistantly distributed through holes.

[0041] Furthermore, the thickness of the low-density foam layer is 0.2-1 mm; in the porous structure, the aperture of the through hole is 0.5-2 mm; the spacing between each through hole is 0.8-1 mm; and the through hole includes an oblique hole or a straight hole.

[0042] As a preferred embodiment, the through holes are arranged in a matrix and are a plurality of through holes perpendicular to the horizontal direction of the foam.

[0043] The porous structure is a plurality of parallel, matrix-arranged inclined holes, and the inclined angle of the inclined holes is 45°≤a<90° along the horizontal direction of the foam.

[0044] The utility model reduces the rebound force of the foam after compression by using matrix punching or matrix equidistant punching while maintaining the thickness of the filling foam material in the prior art. Compared with conventional foam, the compression rebound force is reduced by 20-50% without affecting the filling effect. It is suitable for scenarios where there are requirements for the compression rebound force of assembled electronic products, especially touch screen usage scenarios, and can improve the performance and service life of electronic product components.

[0045] The above technical solution is described in detail below through specific embodiments.

[0046] Example 1

[0047] This embodiment provides a low-rebound ultra-soft foam with a multi-layer structure, which is used between a screen module (touch screen) and a battery module in an electronic product to achieve filling and buffering functions.

[0048] The multilayer structure of low-rebound ultra-soft foam provided in this embodiment at least comprises: a low-density foam layer 10 and a first buffer structure layer 20 which are arranged in a laminated manner, wherein the low-density foam layer adopts foam material in the prior art, and has a thickness of 0.2 to 1 mm, which can be selected according to the thickness of the gap to be filled in the electronic product. The first buffer structure layer 20 is bonded to the surface of the battery module.

[0049] See also Figure 1 The low-rebound ultra-soft foam with a porous structure provided in this embodiment, the low-density foam layer is a layered foam material with a porous structure, and the porous structure is composed of a plurality of regularly arranged through holes 101 opened along the thickness direction.

[0050] Further, see Figure 2 , including a low-density foam layer 10 and a first buffer structure layer 20 which are sequentially laminated, the through holes 101 are straight holes and are equidistantly distributed on the surface of the foam; more preferably, the through holes 101 are arranged in a matrix, and the porous structure is punched by laser or die-cutting to form the through holes 101 arranged in a matrix, and the excess parts are removed.

[0051] Preferably, in the porous structure, the diameter of the through holes is 0.5 to 2 mm; and the spacing between each through hole is 0.8 to 1 mm.

[0052] Preferably, the first buffer structure layer 20 is an integral structure consisting of a first flexible glue layer 201-a first foaming substrate layer 202-a second flexible glue layer 203 which are sequentially bonded together; the first flexible glue layer 201 and / or the second flexible glue layer 203 may be elastic acrylic glue layers; by coating acrylic glue on both sides of the first foaming substrate layer respectively, the first buffer structure layer is formed after curing.

[0053] Preferably, the first foamed substrate layer 202 is made of foam material with a thickness of 0.05-0.1 mm.

[0054] Preferably, an elastic layer is provided in the acrylic glue layer, and the elastic layer is composed of built-in foaming microspheres; the foaming microspheres are evenly distributed inside the acrylic glue layer; more preferably, the particle size of the foaming microspheres is 20 to 50 μm.

[0055] Example 2

[0056] See also Figure 3 The through holes 101 in the porous structure of the low-rebound ultra-soft foam provided in this embodiment are inclined holes, and the inclination angle (along the horizontal direction of the foam) is 45°≤a<90°.

[0057] Example 3

[0058] The low rebound ultra-soft foam with a multi-layer structure provided in this embodiment has a specific structure. Figure 4 , comprising a protective functional layer 40, a low-density foam layer 10 and a first buffer structure layer 20 which are sequentially laminated. Preferably, the protective functional layer is a scratch-resistant single-sided tape laminated on the surface of the low-density foam layer.

[0059] As a preferred embodiment, the first buffer structure layer 20 is composed of a first flexible glue layer 201-a first foaming substrate layer 202-a second flexible glue layer 203 which are sequentially bonded together; the first flexible glue layer 201 and / or the second flexible glue layer 203 can be made of elastic acrylic glue layers.

[0060] Preferably, the first foamed substrate layer 202 is made of foam material with a thickness of 0.05-0.1 mm.

[0061] Preferably, an elastic layer is provided in the acrylic glue layer, and the elastic layer is composed of built-in foaming microspheres; the foaming microspheres are evenly distributed inside the acrylic glue layer; more preferably, the particle size of the foaming microspheres is 20 to 50 μm.

[0062] Example 4

[0063] The low rebound ultra-soft foam with a multi-layer structure provided in this embodiment has a specific structure. Figure 5 , which is different from Example 1, is that a fifth flexible glue 50 is further included between the protective functional layer and the low-density foam layer; the fifth flexible glue layer 50 is an acrylic glue layer.

[0064] Example 5

[0065] The low rebound ultra-soft foam with a multi-layer structure provided in this embodiment has a specific structure. Figure 6, including a multilayer structure of a second buffer structure layer 30 - a low-density foam layer 10 - a first buffer structure layer 20 which are sequentially bonded.

[0066] The structure of the second buffer structure layer 30 is the same as that of the first buffer structure layer 20, and is composed of a third flexible glue layer 301-a second foaming substrate layer 302-a fourth flexible glue layer 303 which are sequentially bonded together; the third flexible glue layer 301 and / or the fourth flexible glue layer 303 can be made of elastic acrylic glue layers.

[0067] Preferably, the second foaming substrate layer 202 is a foam material with a thickness of 0.05-0.1 mm, and the material is preferably VHB material.

[0068] The multilayer structure of this embodiment is adopted, and the bottom adhesive is also composed of modified acrylic glue + VHB foam substrate, so that the tape itself also has compression buffering performance, so that the entire structure has buffering properties, so that the rebound force of the entire product after being compressed will be greatly reduced. Thereby improving the overall performance. We can choose different pore sizes and spacings according to different application requirements to meet different compression rebound forces.

[0069] Furthermore, the low-rebound ultra-soft foam with a multi-layer structure obtained in the above embodiment is used between the touch screen and the battery assembly in the electronic product, the first buffer structure layer 20 with bonding properties is bonded to the battery assembly, and finally the touch screen is installed on the assembled battery assembly.

[0070] In order to illustrate the rebound force of the above-mentioned low-rebound ultra-soft foam with a porous structure, low-density foam layers of 0.35mm and 0.5mm were selected respectively, and the structures of the low-density foam layer 10 and the first buffer structure layer 20 were respectively adopted (Example 1), and the pressure (KPa) before compression and after compression of 25% was carried out according to the through-hole diameter and hole spacing in Table 1 to illustrate the rebound performance of the material. The through-holes are straight holes and arranged in a matrix. The test results of the foam layer before the above results are compared. The results are shown in Table 1.

[0071] Table 1 Test results of through-hole parameters and rebound performance of low-density foam layer

[0072]

[0073] From the results provided in Table 1, it can be seen that the low-density foam layer can have different pore sizes and pore spacings according to product requirements, so that the pressure (rebound force) per unit area when compressed by 25% is reduced by 20% to 50% compared with before compression, thereby greatly improving the product application performance.

[0074] Conventional foam generally only selects ultra-thin and ultra-soft foam. Although the thickness can meet the requirements, the foam is completely attached to the battery. When the material is compressed, the rebound force per unit area of ​​the foam will be very large, causing the back screen film module to be squeezed, thus affecting the color uniformity of the screen. The compression rebound force of the foam itself is relatively large. At the same time, the use space is limited. Generally, the gap between the module and the battery is less than 0.5mm, and the material needs to be fixed. In this way, the tape pasted on the bottom will also lose some thickness, making the compression performance of the entire structure lower, and the rebound force after compression will be greater. If the rebound force is reduced by reducing the thickness, or the size of the foam is reduced and partially attached, although the problem of small rebound force after compression can be solved, the area without foam is suspended between the screen and the battery. When the screen film is compressed, the screen film will deform, thus affecting the color saturation. Based on the above problems, the utility model provides a low-rebound foam layer with a porous structure, and reduces the density of the foam in the prior art by punching holes (the density of the unit-density foam is reduced) to form a low-density foam layer. At the same time, a multi-layer buffer structure layer is provided on the bottom surface of the foam, and the foam material is coated on the outer surface of the foam layer through an acrylic glue layer-a substrate layer-an acrylic glue layer, so as to improve the buffering performance of the buffer structure layer. In particular, the buffer structure layer can absorb the rebound force from external force on the low-density foam layer, reduce the force of the foam layer on the screen, and extend the service life and use effect of the touch screen.

[0075] The above are only preferred embodiments of the present invention, which do not limit the protection scope of the present invention. For those skilled in the art, the present invention can be modified and varied in various ways. Any changes, modifications, integrations and parameter changes to these embodiments within the spirit and principle of the present invention through conventional substitutions or capable of achieving the same functions without departing from the principles and spirit of the present invention shall fall within the protection scope of the present invention.

Claims

1. A low rebound foam for a touch screen, characterized in that: At least comprising a low-density foam layer and a first buffer structure layer that are fitted together; The first buffer structure layer is composed of a first flexible glue layer, a foaming substrate layer, and a second flexible glue layer which are sequentially bonded together; The low-density foam layer is a layered foam material with a porous structure, and the porous structure is composed of a plurality of through holes regularly arranged in a matrix opened along the thickness direction; The first buffer structure layer is bonded to the surface of the battery module.

2. The low rebound foam for touch screen according to claim 1, characterized in that: The thickness of the low-density foam layer is 0.2-1 mm; the aperture of the through hole in the porous structure is 0.5-2 mm; the spacing between each through hole is 0.8-1 mm; the porous structure is composed of a plurality of straight through holes or oblique through holes arranged equidistantly along the horizontal direction of the foam.

3. The low rebound foam for touch screen according to claim 1, characterized in that: The porous structure is a plurality of parallel, equidistantly arranged oblique through holes, and the inclination angle of the oblique through holes along the horizontal direction of the foam is 45°≤ɑ<90°.

4. The low rebound foam for touch screen according to claim 1, characterized in that: The through holes in the porous structure are arranged in a matrix; The foaming substrate layer is a foam material with a thickness of 0.05-0.1 mm.

5. The low rebound foam for touch screen according to claim 1, characterized in that: The first flexible glue layer and / or the second flexible glue layer is an elastic acrylic glue layer.

6. The low rebound foam for touch screen according to claim 5, characterized in that: An elastic layer is provided in the acrylic glue layer, and the elastic layer is composed of built-in foaming microspheres; the foaming microspheres are evenly distributed inside the acrylic glue layer; The particle size of the foamed microspheres is 20-50 μm.

7. The low rebound foam for touch screen according to claim 1, characterized in that: A multilayer structure comprising a protective functional layer, the low-density foam layer, and the first buffer structure layer arranged in a close relationship; The protective functional layer is a scratch-resistant single-sided adhesive tape, which is attached to the surface of the low-density foam layer.

8. The low rebound foam for touch screen according to claim 7, characterized in that: A fifth flexible glue layer is also included between the protective functional layer and the low-density foam layer; The fifth flexible glue layer is an acrylic glue layer.

9. The low rebound foam for touch screen according to claim 1, characterized in that: It comprises a multilayer structure having a second buffer structure layer, the low-density foam layer, and the first buffer structure layer which are sequentially laminated; The structure of the second buffer structure layer is the same as that of the first buffer structure layer.