Lead frame and chip packaging product

By forming an anti-seepage layer on the periphery of the chip bonding area of ​​the lead frame, the problem of adhesive leakage is solved, the reliability and thermal stability of the chip package are improved, and the problems of non-adhesion of solder joints and weak bonding are avoided. .

CN222088588UActive Publication Date: 2024-11-29ADVANCED ASSEMBLY MATERIALS ANHUI LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323531076.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-22
Publication Date
2024-11-29
Estimated Expiration
2033-12-22

AI Technical Summary

Technical Problem

In the existing chip packaging process, the problem of adhesive oozing in the chip bonding area leads to non-adhesion of solder joints, weak bonding between bonding wires and lead frames, and the packaging material may be delaminated or peeled, reducing the reliability of the packaging. and thermal stability.

Method used

Design a lead frame, which forms an anti-seepage layer on the periphery of the chip bonding area, the width of the anti-seepage layer is smaller than the distance from the base boundary, and includes multiple discrete sub-seepage layers, made of ethylene glycol monoisopropylene A mixture of (3,3,4,4,5,5,6,6,7,7,8,8,8-tridefluorooctyl)phosphate and ammonium salt or disproportionate-α-(nolenide A mixture of ylphenyl)-ω-hydroxy-(polyethylene oxide) and organic acid salts to prevent the adhesive from oozing out.

Benefits of technology

Effectively prevent the adhesive from oozing out in the chip bonding area, improve the overall reliability of the chip package and the bonding force between the packaging material and the lead frame, and ensure high reliability and thermal stability of the packaging products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222088588U_ABST
    Figure CN222088588U_ABST
Patent Text Reader

Abstract

The embodiment of the utility model provides a lead frame and a chip packaging product, the lead frame comprises a base used for placing a chip, the base comprises a chip bonding area, and an impermeable layer is formed on the periphery of at least part of the boundary of the chip bonding area; a first distance is formed between the boundary of the chip bonding area and the boundary of the corresponding base; the impermeable layer has a certain width, and the width of the impermeable layer is smaller than the first distance. By adopting the lead frame provided by the embodiment of the utility model to carry out chip packaging, the adhesive can be prevented from seeping out of the chip bonding area when the chip is bonded, meanwhile, the adverse effect on chip packaging caused by the adhesive seeping out of the chip bonding area can be avoided, and the packaging reliability is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the field of chip packaging, and in particular to a lead frame and a chip packaging product. Background Art

[0002] In the field of chip packaging, a lead frame is usually used as a carrier for mounting the chip, and the pins of the chip and the lead frame are connected by bonding wire welding to connect the electrodes of the chip. At the same time, packaging materials are needed to seal the chip and the bonding wires to protect the chip and the bonding wires from interference and influence of the external environment.

[0003] To mount the chip on the lead frame, it is necessary to apply adhesive to the area on the lead frame that is bonded to the chip, and then adhere the chip to the adhesive, thereby fixing the chip and the lead frame to each other.

[0004] During the die attach process, adhesive tends to seep out of the die bonding area due to the free diffusion of small molecule chemicals under capillary forces. Adhesive seepage may result in non-stick on pads, weak bonding of bond wires to the lead frame, or even delamination or peeling of the packaging material from the die-attach pad of the lead frame, thus reducing the overall reliability of the package.

[0005] In order to solve the problem of adhesive leakage from the chip bonding area, in some practical applications, the adhesive is modified to change its flow properties on the lead frame, specifically, an anti-seepage agent is added to prevent the adhesive from leaking out of the chip bonding area. However, this method is relatively complicated, and different proportions or different types of anti-seepage agents need to be selected for different adhesives. The actual application is relatively complicated and the cost is relatively high.

[0006] In order to solve the problem of adhesive leakage from the chip bonding area, in some practical applications, a die attach film is used to replace the adhesive as a bonding material between the chip and the lead frame. This can solve the problem of adhesive leakage from the chip bonding area to a certain extent. However, the die attach film often has poor corrosion resistance and cannot guarantee the long-term use of the lead frame. At the same time, the die attach film will cause the bonding force between the chip and the lead frame to decrease, the packaging reliability is low, and the thermal stability of the packaged product is reduced. In addition, the cost of forming the die attach film on the lead frame is high.

[0007] Therefore, the existing chip packaging process needs to be further improved to provide a new lead frame or chip packaging product. Utility Model Content

[0008] An embodiment of the present disclosure provides a lead frame, comprising a base for placing a chip, the base comprising a chip bonding area for placing the chip, an impermeability layer being formed around at least part of the boundary of the chip bonding area; a first distance is present between the boundary of the chip bonding area and the corresponding boundary of the base; the impermeability layer has a certain width, and the width of the impermeability layer is less than the first distance.

[0009] In some embodiments, the width of the barrier layer is 0.1 μm to 1100 μm.

[0010] In some embodiments, the barrier layer includes a plurality of discrete sub-barrier layers, the sub-barrier layer closest to the chip bonding region constitutes a first barrier layer, and the width of the first barrier layer ranges from 0.1 μm to 500 μm.

[0011] In some embodiments, the first barrier layer is spaced from the chip bonding region by a distance within 0.1 μm.

[0012] In some embodiments, the anti-seepage layer further includes a second anti-seepage layer closest to the first anti-seepage layer, and the width of the second anti-seepage layer ranges from 0.1 μm to 500 μm.

[0013] In some embodiments, the spacing distance between the second anti-seepage layer and the first anti-seepage layer is 0 μm to 100 μm.

[0014] In some embodiments, the anti-seepage layer further includes a second anti-seepage layer, the second anti-seepage layer and the first anti-seepage layer are respectively located on two opposite sides or adjacent sides of the chip bonding area, and the width of the second anti-seepage layer ranges from 0.1 μm to 500 μm.

[0015] In some embodiments, the material of the first anti-seepage layer includes: ethylene glycol monoisopropyl ether, a mixture of (3,3,4,4,5,5,6,6,7,7,8,8,8-tridecafluorooctyl) phosphate and ammonium salt, or a mixture of disproportionated-α-(nonylphenyl)-ω-hydroxy-(polyethylene oxide) and organic acid salt.

[0016] In some embodiments, the material of the second barrier layer includes: ethylene glycol monoisopropyl ether, a mixture of (3,3,4,4,5,5,6,6,7,7,8,8,8-tridecafluorooctyl) phosphate and ammonium salt, or a mixture of disproportionated-α-(nonylphenyl)-ω-hydroxy-(polyethylene oxide) and organic acid salt.

[0017] In some embodiments, the first barrier layer is ring-shaped, and the first barrier layer surrounds the chip bonding area.

[0018] An embodiment of the present disclosure also provides a chip packaging product, which includes: any of the above lead frames; a chip mounted on the chip bonding area of ​​the lead frame; bonding wires electrically connected to the chip and the lead frame; and packaging material, which encapsulates the chip, the bonding wires, and at least part of the lead frame.

[0019] In some embodiments, the chip packaging product further includes: an adhesive located between the lead frame and the chip, the adhesive being bonded to the lead frame and the chip.

[0020] In some embodiments, the adhesive includes epoxy and silver.

[0021] Compared with the prior art, the technical solution of the embodiment of the present disclosure has the following beneficial effects:

[0022] In the lead frame of the embodiment of the present disclosure, a waterproof layer is formed on the periphery of at least part of the boundary of the chip bonding area. When the chip is bonded to the base by means of an adhesive, the waterproof layer reduces the surface energy between the base surface and the adhesive, thereby effectively preventing the adhesive from seeping out of the chip bonding area when the chip is bonded, thereby avoiding problems such as the solder joints on the lead frame not being bonded, the bonding force between the bonding wire and the lead frame being weak, and even the delamination or peeling of the packaging material from the chip connection pads of the lead frame due to the adhesive seepage, thereby improving the overall reliability of the chip package.

[0023] The anti-seepage layer of the embodiment of the present disclosure has a certain width, and the width of the anti-seepage layer is smaller than the first distance, that is, the anti-seepage layer is only formed on part of the surface of the base except the chip bonding area, thereby avoiding that the area of ​​the lead frame in direct contact with the packaging material is too small due to the anti-seepage layer area being too large, thereby avoiding the resulting decrease in the bonding strength between the lead frame and the packaging material, and ensuring the reliability of the packaging.

[0024] The anti-seepage layer of the embodiment of the present disclosure includes multiple discrete sub-anti-seepage layers, each of which can be formed on the same side, opposite side or adjacent side of the chip bonding area. The distribution of each sub-anti-seepage layer can be set according to the specific purpose or packaging requirements of the lead frame, which has high flexibility. The lead frame is suitable for various chip packaging requirements.

[0025] The chip packaging product of the embodiment of the present disclosure has an anti-seepage layer with a certain width on the lead frame, so no adhesive seeps out of the chip bonding area during the chip bonding process, and the packaging material and the lead frame have sufficient contact area, so the chip packaging product has high packaging reliability. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Other features and advantages of the present disclosure will be better understood through the following detailed description of the optional embodiments in conjunction with the accompanying drawings, in which the same reference numerals represent the same or similar components, wherein:

[0027] Figure 1-Figure 4 A schematic diagram of a top view of a base of a lead frame according to an embodiment of the present disclosure is shown;

[0028] Figure 5 A schematic structural diagram of a chip packaging product according to an embodiment of the present disclosure is shown. DETAILED DESCRIPTION

[0029] Embodiments of the present disclosure are described in detail below, and examples of the embodiments are shown in the accompanying drawings. In the accompanying drawings, the same or similar reference numerals represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present disclosure, and cannot be understood as limiting the present disclosure.

[0030] Unless otherwise defined, the technical terms or scientific terms used herein shall have the usual meanings understood by persons with ordinary skills in the field to which the present disclosure belongs. In the description of the present disclosure, it should be understood that the terms "center", "longitudinal", "lateral", "upper", "lower", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present disclosure and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation to the present disclosure.

[0031] In order to prevent the adhesive from seeping out of the chip bonding area and affecting the packaging reliability when the chip is bonded in the chip bonding area, an embodiment of the present disclosure provides a lead frame, the lead frame includes a base for placing the chip, the base includes a chip bonding area for placing the chip, and an anti-seepage layer is formed on the periphery of at least part of the boundary of the chip bonding area; a first distance is provided between the boundary of the chip bonding area and the corresponding boundary of the base; the anti-seepage layer has a certain width, and the width of the anti-seepage layer is less than the first distance.

[0032] Figure 1-Figure 4 A schematic top view of the structure of a base of a lead frame according to an embodiment of the present disclosure is shown. The lead frame of the embodiment of the present disclosure is described in detail below in conjunction with the accompanying drawings.

[0033] refer to Figure 1The lead frame includes a base 1, and the base includes a chip bonding area 11 for placing the chip during chip packaging. The chip is bonded to the chip bonding area 11 by an adhesive, and the area of ​​the chip bonding area 11 is larger than the area of ​​the chip. The chip bonding area 11 includes a boundary 111, and a first distance S is formed between the boundary 111 and a corresponding boundary 13 of the base 1. An impermeable layer 12 is formed around at least part of the boundary 111 of the chip bonding area 11, and the impermeable layer 12 has a certain width W, and the width of the impermeable layer 12 is less than the first distance S.

[0034] The waterproof layer 12 formed on the periphery of the boundary 111 of the chip bonding area 11 has a certain width, so as to prevent the adhesive from seeping out of the chip bonding area 11 when the chip is bonded; at the same time, the width of the waterproof layer 12 is smaller than the first distance S, that is, the waterproof layer 12 does not completely cover the other parts of the base 1 except the chip bonding area 11, so as to avoid the reduction of the lead frame area in direct contact with the packaging material due to the excessive area of ​​the waterproof layer 12, thereby avoiding the reduction of the bonding force between the lead frame and the packaging material, so that the packaging reliability of the lead frame is high.

[0035] In order to prevent the adhesive from seeping out of the chip bonding area 11 during the chip bonding process and to ensure the contact area between the packaging material and the lead frame during the packaging process, the width W of the anti-seepage layer 12 can be set according to the material of the anti-seepage layer 12 and the type of adhesive. In some embodiments, the width W of the anti-seepage layer 12 is 0.1 μm to 1100 μm; in some embodiments, the width W of the anti-seepage layer 12 is 0.1 μm to 500 μm. In some embodiments, the first distance S is 0.5 μm to 2000 μm and is greater than the width W of the anti-seepage layer 12.

[0036] In some embodiments, the barrier layer 12 includes a plurality of discrete sub-barrier layers, the sub-barrier layer closest to the chip bonding area 11 constitutes a first barrier layer 121, and the width W1 of the first barrier layer 121 ranges from 0.1 μm to 500 μm. The width W of the barrier layer 12 is the sum of the widths of the sub-barrier layers and the spacing therebetween.

[0037] In some embodiments, the first barrier layer 121 is spaced from the chip bonding area 11 by a distance of less than 0.1 μm to prevent adhesive from seeping out near the boundary 111 of the chip bonding area 11 ; in some embodiments, the first barrier layer 121 is spaced from the chip bonding area 11 by a distance of 0 μm.

[0038] The first anti-seepage layer 121 has a certain thickness, and the thickness is related to the formation method of the first anti-seepage layer 121. In some embodiments, the thickness of the first anti-seepage layer 121 is 0.1 nm to 1000 nm.

[0039] In the lead frame of the embodiments of the present disclosure, in some embodiments, the barrier layer 12 further includes a second barrier layer 122 . Figure 2 to Figure 4 An embodiment is shown in which the anti-permeability layer 12 includes a first anti-permeability layer 121 and a second anti-permeability layer 122 .

[0040] refer to Figure 2 In some embodiments, the second anti-seepage layer 122 is closest to the first anti-seepage layer 121 and is located outside the first anti-seepage layer 121 . The second anti-seepage layer 122 and the first anti-seepage layer 121 jointly prevent the adhesive from leaking out.

[0041] The width W2 of the second impermeable layer 122 may be the same as or different from the width W1 of the first impermeable layer 121 . In some embodiments, the width W2 of the second impermeable layer 122 ranges from 0.1 μm to 500 μm.

[0042] In some embodiments, the interval between the second impermeable layer 122 and the first impermeable layer 121 is 0 μm to 100 μm. When the interval between the second impermeable layer 122 and the first impermeable layer 121 is 0 μm, the two are connected to each other. In some embodiments, the interval between the second impermeable layer 122 and the first impermeable layer 121 is not 0 μm, that is, the first impermeable layer 121 and the second impermeable layer 122 are separated from each other.

[0043] In some embodiments, the second impermeable layer 122 located outside the first impermeable layer 121 mainly functions to prevent the adhesive from seeping out when the impermeable effect of the first impermeable layer 121 is not ideal. In some embodiments, the width W2 of the second impermeable layer 122 is smaller than the width W1 of the first impermeable layer 121, thereby reducing the total width of the impermeable layer 12 as much as possible, and avoiding the impermeable layer 12 being too large, resulting in the base area in contact with the packaging material being too small, thereby affecting the packaging strength.

[0044] The second anti-seepage layer 122 has a certain thickness, and the thickness is related to the formation method of the second anti-seepage layer 122. In some embodiments, the thickness of the second anti-seepage layer 122 is 0.1 nm to 1000 nm.

[0045] The barrier layer 12 of the embodiment of the present disclosure includes multiple discrete sub-barrier layers, each of which can be formed on the same side, opposite sides or adjacent sides of the chip bonding area 11. The distribution of each sub-barrier layer can be set according to the specific purpose or packaging requirements of the lead frame, with high flexibility.

[0046] According to the different requirements for preventing adhesive leakage on different sides of the chip bonding area 11, in some embodiments, an anti-seepage layer 12 is formed around part of the boundaries 111 of the chip bonding area 11, and it is not necessary to form an anti-seepage layer around all the boundaries 111, thereby reducing the area of ​​the anti-seepage layer 12, avoiding the anti-seepage layer 12 being too large and resulting in the base area in contact with the packaging material being too small to affect the packaging strength, and also saving the material cost of the anti-seepage layer 12.

[0047] refer to Figure 3 The first anti-seepage layer 121 and the second anti-seepage layer 122 are respectively located at the peripheries of two adjacent boundaries 111 of the chip bonding area 11 . Figure 3 The structure of the impermeable layer shown is only for illustration. In other embodiments, the first impermeable layer 121 and the second impermeable layer 122 may be respectively located at the peripheries of two opposite boundaries 111 of the chip bonding area 11, and the first impermeable layer 121 and / or the second impermeable layer 122 may also be formed at the peripheries of one or three boundaries 111 of the chip bonding area 11. The specific distribution of the first impermeable layer 121 and the second impermeable layer 122 is set according to actual needs, for example, according to the electrode distribution on the chip, the pad distribution on the lead frame, and the pin distribution.

[0048] According to different requirements for preventing adhesive seepage on different sides of the chip bonding area 11, in some embodiments, an anti-seepage layer 12 is formed around all boundaries 111 of the chip bonding area 11, and the number and distribution of sub-anti-seepage layers included in the anti-seepage layer 12 can be set according to actual needs.

[0049] In some embodiments, the periphery of all the boundaries 111 of the chip bonding area 11 is formed with a first impermeable layer 121 and / or a second impermeable layer 122. In some embodiments, the first impermeable layer 121 and the second impermeable layer 122 are respectively located on two opposite sides or adjacent sides of the chip bonding area 11. Figure 4 The first waterproof layer 121 and the second waterproof layer 122 are respectively located on adjacent sides of the chip bonding area 11, that is, the peripheries of the two adjacent boundaries 111 are respectively formed with the first waterproof layer 121 and the second waterproof layer 122, the two first waterproof layers 121 are arranged opposite to each other, and the two second waterproof layers 122 are arranged opposite to each other. Figure 4 The structure of the impermeable layer shown is only for illustration. In other embodiments, two first impermeable layers 121 and two second impermeable layers 122 are respectively formed on four boundaries 111 of the chip bonding area 11, and the first impermeable layer 121 and the second impermeable layer 122 can be respectively formed on opposite sides of the chip bonding area 11. The specific distribution of the first impermeable layer 121 and the second impermeable layer 122 is set according to actual needs, for example, according to the electrode distribution on the chip, the pad distribution on the lead frame, and the pin distribution.

[0050] Continue to refer Figure 4 In some embodiments, there is at most one sub-impermeable layer around any boundary 111 of the chip bonding area 11, such as only the first impermeable layer 121 or only the second impermeable layer 122; in some embodiments, the width of the first impermeable layer 121 ranges from 0.1 μm to 500 μm, and the width of the second impermeable layer 122 ranges from 0.1 μm to 500 μm. In some embodiments, the thickness of the first impermeable layer is 0.1 nm to 1000 nm, and the thickness of the second impermeable layer is 0.1 nm to 1000 nm.

[0051] It should be noted that Figure 2 to Figure 4 The embodiments in the figure are only for illustrating the distribution of the anti-seepage layer 12 and the sub-anti-seepage layers (the first anti-seepage layer 121 and the second anti-seepage layer 122), and do not exhaust all the distribution modes of the anti-seepage layer 12. Figure 2 to Figure 4 It does not constitute a limitation on the technical solutions of the embodiments of the present disclosure.

[0052] In some embodiments, the first impermeable layer 121 is ring-shaped, and the first impermeable layer 121 surrounds the chip bonding area 11 .

[0053] In some embodiments, the second impermeable layer 122 is ring-shaped, and the second impermeable layer 122 surrounds the chip bonding area 11 .

[0054] In some embodiments, the impermeable layer 12 is formed on the periphery of a portion of the boundary 111 of the chip bonding area 11; in some embodiments, the impermeable layer 12 is formed on the periphery of all the boundaries 111 of the chip bonding area 11. The distribution of the impermeable layer 12 and the distribution and number of the sub-impermeable layers are not limited here, and are set according to the structural characteristics of the lead frame, the chip electrode distribution and the electrode connection requirements in the specific embodiment.

[0055] It should be noted that the chip bonding area is an area divided according to the shape and size of the chip for placing the chip. When bonding the chip, when the adhesive does not seep out or only slightly seeps out of the chip bonding area, the adhesive has basically no adverse effect on the subsequent packaging process. Therefore, the shape of the chip bonding area can be changed according to the shape of the chip, and the shape of the anti-seepage layer formed on the periphery of the chip bonding area can also be changed accordingly. The embodiment in the accompanying drawings is based on the case where the chip is rectangular, and thus the chip bonding area is rectangular. It is only for illustration and does not constitute a limitation on the technical solution of the embodiment of the present disclosure.

[0056] In order to effectively prevent the adhesive from seeping out and minimize the width of the anti-seepage layer, it is necessary to select an anti-seepage layer of suitable material to reduce the surface energy between the base surface and the adhesive. The choice of the material of the anti-seepage layer is mainly based on the type of adhesive, while considering the width of the anti-seepage layer and the design of the distribution of the anti-seepage layer on the base.

[0057] To ensure that the anti-seepage layer effectively reduces the surface energy between the adhesive and the base, that is, the surface energy between the anti-seepage layer and the adhesive is lower than the surface energy between the base surface and the adhesive, thereby preventing the adhesive from seeping out, in some embodiments, the material of the anti-seepage layer includes: ethylene glycol monoisopropyl ether, a mixture of (3,3,4,4,5,5,6,6,7,7,8,8,8-tridecafluorooctyl) phosphate and ammonium salt, or a mixture of disproportionated-α-(nonylphenyl)-ω-hydroxy-(polyethylene oxide) and an organic acid salt.

[0058] The materials of the sub-anti-seepage layers of the anti-seepage layer can be the same or different. For the same adhesive, in order to simplify the steps of forming the anti-seepage layer, the materials of the sub-anti-seepage layers are the same while ensuring the anti-seepage effect.

[0059] In some embodiments, the adhesive used to bond the chip includes epoxy resin and silver.

[0060] In some embodiments, the material of the first anti-seepage layer 121 includes: ethylene glycol monoisopropyl ether, a mixture of (3,3,4,4,5,5,6,6,7,7,8,8,8-tridecafluorooctyl) phosphate and ammonium salt, or a mixture of disproportionated-α-(nonylphenyl)-ω-hydroxy-(polyethylene oxide) and organic acid salt.

[0061] In some embodiments, the material of the second barrier layer 122 includes: ethylene glycol monoisopropyl ether, a mixture of (3,3,4,4,5,5,6,6,7,7,8,8,8-tridecafluorooctyl) phosphate and ammonium salt, or a mixture of disproportionated-α-(nonylphenyl)-ω-hydroxy-(polyethylene oxide) and organic acid salt.

[0062] In some embodiments, the barrier layer 12 is in a liquid or solid state.

[0063] In some embodiments of the lead frame of the embodiments of the present disclosure, the impermeable layer 12 can be formed by spraying or soaking, that is, spraying a solution of a compound including the material of the impermeable layer 12 onto the base 1, or soaking the base 1 into a solution of a compound including the material of the impermeable layer 12. During the spraying or soaking process, a mask of a specific shape is kept covering the surface of the base 1, so that the impermeable layer 12 is selectively formed in a partial area on the base 1, that is, the impermeable layer 12 with a specific shape and distribution on the base 1 is formed.

[0064] In some embodiments, the solution used for spraying or immersion includes: anti-silver colloid diffusion agent T14 or anti-silver colloid diffusion agent X5.

[0065] An embodiment of the present disclosure further provides a chip packaging product, which includes the lead frame of any of the above embodiments, or is obtained by packaging a chip using the lead frame of any of the above embodiments.

[0066] Figure 5 FIG. 1 shows a schematic diagram of the structure of a chip packaging product according to an embodiment of the present disclosure. Figure 5 The package product includes: a lead frame including a base 1 and pins 6; a chip 2 mounted on a chip bonding area 11 on the surface of the base 1; a bonding wire 4 electrically connecting the chip 2 and the pins 6; and a packaging material 5, wherein the packaging material 5 packages the chip 2, the bonding wire 4, and at least a portion of the lead frame. The lead frame is the same as the lead frame of any of the above embodiments, and will not be described in detail herein.

[0067] In the chip packaging product of the embodiment of the present disclosure, an impermeable layer 12 is formed on the base 1. In some embodiments, the impermeable layer 12 includes a first impermeable layer 121; in some embodiments, the impermeable layer 12 includes a first impermeable layer 121 and a second impermeable layer 122; the impermeable layer 12, the first impermeable layer 121 and the second impermeable layer 122 are the same as any of the above embodiments, and will not be repeated here.

[0068] In some embodiments, the chip packaging product further includes: an adhesive 3 located between the lead frame 1 and the chip 2 , the adhesive 3 being bonded to the base 1 of the lead frame, and the adhesive 3 being also bonded to the chip 2 , thereby mounting and fixing the chip 2 on the chip bonding area 11 of the base 1 .

[0069] In the process of forming the chip package product, the chip 2 is mounted on the base 1, specifically comprising: providing a lead frame of any of the above embodiments, applying the adhesive 3 to the chip bonding area 11 on the base 1 of the lead frame, and then bonding the chip 2 to the adhesive 3. In the process of bonding the chip 2 to the adhesive 3, the adhesive 3 gradually seeps out of the chip bonding area 11. Since the anti-seepage layer 12 and the adhesive 3 have a lower surface energy, when the adhesive 3 reaches the anti-seepage layer 12, the anti-seepage layer 12 effectively prevents the adhesive 3 from seeping out, thereby preventing the adhesive 3 from seeping out and affecting subsequent bonding or packaging.

[0070] Due to the formation of the anti-seepage layer 12, that is, the lead frame has been improved to prevent the adhesive from seeping out, so when the adhesive 3 is applied to the chip bonding area 11, no other additional operations are required to prevent the adhesive from seeping out, such as mixing the adhesive and the anti-seepage agent with each other before applying them. The adhesive 3 is easy to apply and will not seep out.

[0071] In some embodiments, the adhesive 3 includes epoxy resin and silver.

[0072] In some embodiments, the base 1 and the pins 6 are made of copper alloy or copper.

[0073] The above is only an exemplary embodiment used to illustrate the principle of the present disclosure, and is not intended to limit the scope of protection of the present disclosure. For those of ordinary skill in the art, various modifications and improvements can be made without departing from the spirit and essence of the present disclosure, and these modifications and improvements are also within the scope of protection of the present disclosure.

Claims

1. A lead frame, comprising a base for placing a chip, the base comprising a chip bonding area for placing the chip, characterized in that: An anti-seepage layer is formed around at least part of the periphery of the boundary of the chip bonding area; There is a first distance between the boundary of the chip bonding area and the corresponding boundary of the base; The anti-seepage layer has a certain width, and the width of the anti-seepage layer is smaller than the first distance.

2. The lead frame according to claim 1, characterized in that: The width of the anti-seepage layer is 0.1 μm to 1100 μm.

3. The lead frame according to claim 1, characterized in that: The anti-seepage layer includes a plurality of discrete sub-anti-seepage layers, the sub-anti-seepage layer closest to the chip bonding area constitutes a first anti-seepage layer, and the width of the first anti-seepage layer ranges from 0.1 μm to 500 μm.

4. The lead frame according to claim 3, characterized in that: The first barrier layer is spaced from the chip bonding area within 0.1 μm.

5. The lead frame according to claim 3, characterized in that: The anti-seepage layer further includes a second anti-seepage layer closest to the first anti-seepage layer, and the width of the second anti-seepage layer ranges from 0.1 μm to 500 μm.

6. The lead frame according to claim 5, characterized in that: The interval between the second anti-seepage layer and the first anti-seepage layer is 0 μm to 100 μm.

7. The lead frame according to claim 3, characterized in that: The anti-seepage layer further includes a second anti-seepage layer. The second anti-seepage layer and the first anti-seepage layer are respectively located on two opposite sides or adjacent sides of the chip bonding area. The width of the second anti-seepage layer ranges from 0.1 μm to 500 μm.

8. The lead frame according to any one of claims 3 to 7, characterized in that: The first impermeable layer is ring-shaped and surrounds the chip bonding area.

9. A chip packaging product, characterized in that: include: The lead frame according to any one of claims 1 to 8; a chip mounted on a chip bonding area of ​​the lead frame; A bonding wire electrically connected to the chip and the lead frame; A packaging material is provided to encapsulate the chip, the bonding wires, and at least a portion of the lead frame.

10. The chip packaging product according to claim 9, characterized in that: Also includes: An adhesive is located between the lead frame and the chip, and the adhesive is bonded to the lead frame and the chip.