Mold structure to improve shrinkage cavity phenomenon in thick parts of aluminum alloy die castings

By introducing a hydraulically driven insert device into the mold cavity, the thick parts of the aluminum alloy die casting are dynamically segmented, solving the shrinkage problem caused by thermal cavities, and improving product quality and structural strength. It is suitable for mold modification of various aluminum alloy castings.

CN224950959UActive Publication Date: 2026-11-10DONGGUAN BOCK FURNITURE PROD CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522254632.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-10-24
Publication Date
2026-11-10
Estimated Expiration
2035-10-24

AI Technical Summary

Technical Problem

In existing aluminum alloy die castings, hot spots are prone to form in thick sections during filling and solidification, leading to shrinkage cavities and porosity defects, which affect product quality and yield. Furthermore, the newly designed mold structure is complex and costly, making it difficult to promote in small and medium-sized enterprises.

Method used

A hydraulically driven insert device is introduced into the mold cavity to dynamically insert and divide the thick parts, disperse and concentrate heat, and achieve synchronous solidification of the thick parts and the surrounding areas, thus avoiding the formation of internal shrinkage cavities.

Benefits of technology

It effectively avoids shrinkage cavities inside castings, ensuring the appearance, strength, and airtightness of the product. It has a simple structure, is easy to upgrade and modify molds, and is suitable for various aluminum alloy castings.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224950959U_ABST
    Figure CN224950959U_ABST
Patent Text Reader

Abstract

This utility model discloses a mold structure for improving the shrinkage phenomenon in thick sections of aluminum alloy die castings, comprising: a front mold with a gate; a rear mold forming a mold cavity with the front mold, the mold cavity including a first cavity area and at least one second cavity area that are interconnected, the left-right width, top-bottom width, and front-back thickness of the first cavity area being greater than corresponding set values, and the front-back thickness of the second cavity area being less than corresponding set values; a mounting cavity extending into the mold cavity is recessed forward at the rear of the rear mold; and a hydraulic cylinder insert device, comprising an insert, a hydraulic cylinder, and a connector, the hydraulic cylinder driving the connector to move the insert along the front-back direction, so that the insert is inserted into the first cavity area of ​​the mold cavity after mold closing, and is withdrawn from the first cavity area after product forming. It can actively and controllably intervene in the formation of hot spots, and its simple structure makes it suitable for upgrading and modifying molds for various aluminum alloy castings, with strong practicality and easy promotion and implementation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of aluminum alloy die casting technology, and in particular to a mold structure for improving the shrinkage phenomenon in thick parts of aluminum alloy die castings. Background Technology

[0002] In the pressure casting industry, thick parts of aluminum alloy die castings (such as reinforcing ribs, bosses, wall thickness transition areas, and accessory installation areas) tend to have concentrated heat during the filling and solidification process, which can easily lead to hot spots. Due to the large amount of molten metal and slow heat dissipation in the hot spot area, it solidifies last, while the surrounding areas solidify before the hot spot area. This results in internal shrinkage that cannot be effectively compensated by the molten metal, leading to defects such as shrinkage cavities and porosity.

[0003] After the hot spot is machined by CNC, the dense layer on the surface of the thick part is removed, and the internal shrinkage cavities are exposed on the surface, which affects the appearance quality, structural strength and airtightness of the product. In particular, as customers have higher and higher requirements for product quality, such defects lead to low product qualification rate and increased production costs.

[0004] For molds requiring a completely new design, improving hot spots can be achieved by changing the location, size, and number of gates to improve the flow path and temperature distribution of the molten metal. Additionally, cooling water channels can be installed at the corresponding hot spots to accelerate cooling. However, this inevitably leads to a more complex overall mold structure and higher design costs. A completely new mold design differs significantly from the existing mold structure, and scrapping the existing mold results in waste. Therefore, the high cost of these newly designed molds, involving gates, runners, and water cooling, is an expense that many companies and factories cannot afford, especially small and medium-sized enterprises. Moreover, some products, limited by their structure, still struggle to effectively eliminate hot spots even with completely new mold designs involving gates, runners, and water cooling.

[0005] Therefore, a new technical solution needs to be researched to address the above problems. Utility Model Content

[0006] In view of this, the present invention addresses the deficiencies of the existing technology, and its main purpose is to provide a mold structure that improves the shrinkage phenomenon in thick parts of aluminum alloy die castings. It can actively and controllably intervene in the formation of hot spots, and its structure is simple. It is suitable for upgrading and modifying molds for various aluminum alloy castings, has strong practicality, and is easy to promote and implement.

[0007] To achieve the above objectives, the present invention adopts the following technical solution: A mold structure for improving shrinkage cavities in thick sections of aluminum alloy die-cast parts, comprising: Front mold; the front mold is provided with a gate; The rear mold is located below the front mold. The front mold and the rear mold form a mold cavity, which includes a first cavity area and at least one second cavity area that are in contact with each other. The left-right width, top-bottom width, and front-back thickness of the first cavity area are all greater than corresponding set values. The front-back thickness of the second cavity area is less than the corresponding set value, and at least one of its left-right width and top-bottom width is also less than the corresponding set value. The rear part of the rear mold is recessed forward to form an installation cavity that extends into the mold cavity. A hydraulic cylinder insert device is provided corresponding to the mounting cavity. It includes an insert pin, a hydraulic cylinder, and a connector. The insert pin is connected to the connector. The hydraulic cylinder drives the connector to move the insert pin in the front-back direction, so that the insert pin is inserted into the first cavity area of ​​the mold cavity after the mold is closed, and is pulled out from the first cavity area after the product is formed.

[0008] As a preferred embodiment, the connector head is connected to two or more insert pins arranged side by side with a spacing, so that after the product is formed, two or more pre-set inner holes are formed, and a connecting wall is retained between adjacent pre-set inner holes.

[0009] As a preferred embodiment, the insert includes a first needle body and a second needle body connected coaxially from the outside to the inside, wherein the cross-sectional area of ​​the second needle body is smaller than that of the first needle body; after mold closing, the inner ends of the second needle body and the first needle body are inserted into the first cavity area, so that a stepped pre-set inner hole is formed after the product is formed.

[0010] As a preferred embodiment, the cylinder insert device is also equipped with a limit switch for controlling the movement stroke of the insert.

[0011] As a preferred embodiment, the limit switch includes a front limit switch and a rear limit switch, which are respectively connected to a PLC. The PLC is also respectively connected to the solenoid valve of the hydraulic cylinder, the injection mechanism of the mold, and the mold opening / closing mechanism.

[0012] As a preferred embodiment, the rear mold has a rear mold core mounting groove recessed at the front, and a rear mold core is detachably mounted in the rear mold core mounting groove. The rear mold core has second rear cavities corresponding to multiple second cavity areas. A rear insert is also detachably mounted in the rear mold core. The front of the rear insert is recessed to form a first rear cavity corresponding to the first cavity area. The rear of the rear insert has a pin hole that extends forward through the first rear cavity and rearward through the mounting cavity. The pin passes through the pin hole and extends into the first cavity area. The rear part of the front mold is recessed forward to form a front mold core mounting groove. An upper insert is detachably installed in the front mold core mounting groove. The rear part of the upper insert is recessed forward to form a first front cavity corresponding to the first cavity area. The first front cavity and the first rear cavity are combined to form the first cavity. The rear part of the front mold is combined with the second rear cavity to form the second cavity.

[0013] As a preferred embodiment, there is one first cavity area and three second cavity areas. The three second cavity areas are arranged at intervals and connected to the outer periphery of the first cavity. The end of one of the second cavity areas that is away from the first cavity serves as the gate inlet connection end.

[0014] As a preferred embodiment, the length of the second cavity region where the gate feed connection end is located is smaller than the length of other second cavity regions. The length refers to the distance between the end far from the first cavity and the end close to the first cavity.

[0015] As a preferred embodiment, at least one of the left-right width dimension and the top-bottom width dimension of the second cavity region is also smaller than the corresponding set value.

[0016] As a preferred embodiment, the cylinder insert device is located inside the mounting cavity, and a recess extends from the side of the mounting cavity to the outer side of the rear mold, with the oil pipe connected to the cylinder hidden inside the recess.

[0017] Compared with the prior art, this utility model has significant advantages and beneficial effects. Specifically, as can be seen from the above technical solution, it mainly involves adding a mounting cavity that extends forward from the rear of the rear mold, connecting to the mold cavity, based on the original mold. A hydraulically driven insert pin is added, which dynamically inserts into the first cavity area before the aluminum alloy liquid is filled. This divides the originally continuous thick section into multiple thinner sections, thereby dispersing and eliminating heat concentration hotspots, improving heat dissipation, and enabling the thick section of the casting to solidify synchronously or substantially synchronously with its surrounding area. This effectively avoids the formation of internal shrinkage cavities. Thus, after CNC machining, the thick section of the casting will not have exposed internal holes, ensuring the product's appearance, strength, and airtightness. It can actively and controllably intervene in the formation of hotspots, and its simple structure makes it suitable for upgrading and modifying molds for various aluminum alloy castings. It is highly practical and easy to promote and implement.

[0018] To more clearly illustrate the structural features and effects of this utility model, the following detailed description of this utility model is provided in conjunction with the accompanying drawings and specific embodiments. Attached Figure Description

[0019] Figure 1This is a perspective view of a mold structure for improving shrinkage cavities in thick sections of aluminum alloy die-cast parts, according to an embodiment of this utility model. Figure 2 This is another perspective view of the mold structure for improving the shrinkage cavity phenomenon in thick parts of aluminum alloy die castings, according to an embodiment of this utility model. Figure 3 This is an exploded view of the mold structure (including aluminum alloy die casting 40) for improving the shrinkage phenomenon in thick parts of aluminum alloy die castings according to an embodiment of the present invention. Figure 4 This is a cross-sectional view of a mold structure for improving shrinkage cavities in thick sections of aluminum alloy die castings, according to an embodiment of this utility model. Figure 5 This is a perspective view of the cylinder insert device 30 (including aluminum alloy die casting 40) according to an embodiment of the present utility model. Figure 6 This is a partial cross-sectional view of an embodiment of the present utility model. Detailed Implementation

[0020] Please refer to Figures 1 to 6 As shown, it illustrates the specific structure of an embodiment of the present invention.

[0021] In the description of this utility model, it should be noted that the terms "upper", "lower", "left", "right", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this utility model and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this utility model.

[0022] A mold structure for improving shrinkage cavities in thick sections of aluminum alloy die-cast parts, comprising: Front mold 10; the front mold 10 is provided with a gate; Rear mold 20; the rear mold 20 is located below the front mold 10; the front mold 10 and the rear mold 20 form a mold cavity, the mold cavity includes a first cavity area and at least one second cavity area that are in contact with each other, the left and right width, the top and bottom width and the front and back thickness of the first cavity area are all greater than the corresponding set values, the front and back thickness of the second cavity area is less than the corresponding set value, and at least one of its left and right width and top and bottom width is also less than the corresponding set value; the rear part of the rear mold 20 is recessed forward and provided with a mounting cavity 201 that is in contact with the mold cavity, for accommodating the hydraulic cylinder insert device 30; A hydraulic cylinder insert device 30 is provided corresponding to the mounting cavity 201. It includes an insert 31, a hydraulic cylinder 32, a connector 33, an oil pipe 34, and a limit switch 35. The hydraulic cylinder insert device is located within the mounting cavity 201. A recessed groove 202 extends from the side of the mounting cavity 201, penetrating to the outer side of the rear mold 20. The oil pipe 34, connected to the hydraulic cylinder 32, is hidden within the recessed groove 202. Hydraulic oil in the oil pipe 34 enters the hydraulic cylinder 32. The insert 31 is connected to the connector 33. The hydraulic cylinder 32 drives the connector 33 to move the insert 31 in a front-to-back direction, causing the insert 31 to insert into the first cavity area of ​​the mold cavity after mold closing and to be withdrawn from the first cavity area after product molding.

[0023] Thus, based on the original mold, an insert pin 31 driven by a hydraulic cylinder 32 is added. This insert pin 31 is dynamically inserted into the first cavity area before the aluminum alloy liquid is filled, dividing the originally continuous thick part into several thinner sections. This disperses and eliminates heat concentration points, improves heat dissipation, and allows the thick part of the casting to solidify synchronously or nearly synchronously with its surrounding area, effectively preventing the formation of internal shrinkage cavities. This ensures that after CNC machining, the thick part of the casting will not have exposed internal holes, thus guaranteeing the product's appearance, strength, and airtightness. The insert pin 31 is withdrawn after the aluminum alloy casting has cooled, solidified, and stabilized in shape. This avoids ejection damage and achieves active and precise intervention in the solidification process. The hydraulic cylinder drive provides ample power and smooth movement, overcoming the clamping force of the aluminum alloy liquid and ensuring smooth insertion and withdrawal of the insert pin 31.

[0024] In this embodiment, the connector 33 is connected to two or more insert pins 31 arranged side by side with a spacing, so that after the product is formed, two or more pre-set inner holes are formed, and a connecting wall 413 is retained between adjacent pre-set inner holes. In comparison, a single insert pin is suitable for localized, small-scale thick spots. For large-area thick parts, the dispersion effect of a single insert pin is limited. However, by setting multiple insert pins 31, a large-area thick region can be divided to form multiple pre-set inner holes inside the thick part of the casting. This divides the entire thick part into a grid-like structure composed of multiple connecting walls. The thickness of these connecting walls is much smaller than the original thickness of the thick part, thereby decomposing a large hot spot into countless tiny hot spots, achieving homogeneous dispersion of the hot spots, with a more significant and reliable effect. In actual design and manufacturing, multiple insert pins 31 can be installed on the slider seat to form a whole module. All insert pins 31 move through the same slider seat, ensuring that their insertion and withdrawal are synchronized, avoiding casting deformation or tearing caused by asynchronous movements. Moreover, the modular design simplifies the mold assembly process and facilitates subsequent disassembly, replacement or maintenance.

[0025] In this embodiment, the insert pin 31 includes a first pin body 311 and a second pin body 312 connected coaxially from the outside to the inside. The cross-sectional area of ​​the second pin body 312 in the vertical sliding direction is smaller than the cross-sectional area of ​​the first pin body 311 in the vertical sliding direction. After mold closing, the inner ends of the second pin body 312 and the first pin body 311 are inserted into the first cavity area, so that a stepped pre-set inner hole is formed after the product is formed. Thus, the pre-set inner hole formed inside the thick part of the product also has two hole segments: from the inside to the outside, the first hole segment 411 and the second hole segment 412. The cross-sectional area of ​​the first hole segment 411 is smaller than the cross-sectional area of ​​the second hole segment 412. Compared to a through hole, the stepped pre-set inner hole forms an internal reinforcing rib structure on the hole wall, which helps to compensate for the overall strength loss that may be caused by the opening, so that the casting still maintains high mechanical strength after material removal. On the other hand, the stepped structure helps to vent air and reduce local vacuum during the needle pulling process, making the needle pulling action smoother. Moreover, for some products, this thick part serves as a connection part, and the second hole section 412 of the pre-set inner hole can serve as a basis for post-processing, reducing the difficulty of post-processing.

[0026] Furthermore, the rear mold 20 has a rear mold core mounting groove recessed at its front, and a rear mold core 21 is detachably mounted in the rear mold core mounting groove. The rear mold core 21 has second rear cavities corresponding to multiple second cavity areas. A rear insert 22 is also detachably mounted in the rear mold core 21. The front of the rear insert 22 is recessed to form a first rear cavity corresponding to the first cavity area. The rear of the rear insert 22 has a pin hole that extends forward through the first rear cavity. The pin hole extends rearward through the mounting cavity; the insert pin 31 passes through the insert pin hole and extends into the first cavity area; the rear part of the front mold 10 is recessed forward to form a front mold core mounting groove, and an upper insert 11 is detachably installed in the front mold core mounting groove. The rear part of the upper insert 11 is recessed forward to form a first front cavity corresponding to the first cavity area. The first front cavity and the first rear cavity are combined to form the first cavity. The rear part of the front mold 10 is combined with the second rear cavity to form the second cavity. There is one first cavity area and three second cavity areas. The three second cavity areas are arranged at intervals and connected to the outer periphery of the first cavity. The end of one second cavity area away from the first cavity serves as the gate inlet connection end. The length dimension of the second cavity area where the gate inlet connection end is located is smaller than the length dimension of the other second cavity areas. The length dimension refers to the distance between the end away from the first cavity and the end close to the first cavity.

[0027] The workflow is briefly described as follows: After the die-casting mold closes, and before die casting, the hydraulic cylinder 32 is connected to the hydraulic system via the oil pipe 34, driving the connector 33 to move upward, causing the insert pin 31 to be inserted forward into the predetermined thick portion (first cavity area) of the mold cavity. At this time, molten metal is injected into the mold cavity through the gate of the front mold 10. Due to the presence of the insert pin 31, part of the space in the first cavity area is occupied by it, reducing the actual thickness of the molten metal filling and effectively dispersing the heat. After solidification, the hydraulic cylinder 32 moves in the reverse direction, pulling the insert pin 31 out of the partially solidified casting. Finally, the mold opens, and the ejector mechanism ejects the finished casting.

[0028] Furthermore, the hydraulic cylinder insert device 30 is also equipped with a limit switch 35 to control the movement stroke of the insert 31. As a position sensor, the limit switch can precisely set and limit the insertion depth and retraction endpoint of the insert, ensuring that the insert reaches the predetermined position in each production run, thereby guaranteeing the consistency of the preset inner hole depth and shape and improving product dimensional accuracy. It can also prevent over-stroke damage to the mold or insert from the hydraulic cylinder, improving overall operational reliability and safety.

[0029] Limit switches are typically installed along the movement path of the cylinder body of hydraulic cylinder 32 or connector 33, and include a front limit switch and a rear limit switch. The limit switches, including the front and rear limit switches, are respectively connected to a PLC. The PLC is also connected to the solenoid valve of the hydraulic cylinder, the injection mechanism of the mold, and the mold opening / closing mechanism. The PLC is configured as follows: 1. After the mold opening / closing mechanism completes mold closing, the PLC sends a signal to the solenoid valve controlling the hydraulic cylinder, causing hydraulic oil to enter the hydraulic cylinder 32 through the oil pipe 34 and insert the insert pin 31; 2. Upon receiving the signal from the front limit switch, the PLC controls the injection mechanism of the mold to inject molten metal into the mold cavity; 3. After the die-casting process is completed (after a preset pressure holding / cooling time), the PLC sends a reverse signal to the solenoid valve, thereby retracting the insert pin 31; 4. Upon receiving the signal from the rear limit switch, the PLC controls the mold opening / closing mechanism to perform the mold opening action. Specifically: After the die-casting mold is closed, and before die-casting, the PLC sends a signal to the solenoid valve controlling the hydraulic cylinder, causing hydraulic oil to enter the hydraulic cylinder 32 through the oil pipe 34, pushing the piston rod to extend, thereby driving the connector 33 and the insert pin 31 to be inserted forward into the first cavity area. When the insert pin 31 is inserted into the correct position, the forward limit switch (or pin insertion position switch) is triggered, sending a signal to the PLC indicating that the insert pin has reached the correct working position. Only after receiving this signal can the PLC immediately start or allow the next action, namely, injecting molten metal into the mold cavity. This ensures that the insert pin is in the correct position to eliminate heat spots before the molten metal is filled, avoiding scrap caused by the insert pin not being in the correct position. After the die casting process is completed and the casting has initially solidified (after a preset pressure holding / cooling time), the PLC sends a reverse signal to the solenoid valve to change the oil circuit, causing the oil cylinder 32 to drive the connector 33 and the insert pin 31 to be pulled downwards. When the insert pin 31 is completely withdrawn from the casting and mold cavity, the backward limit switch (or pin withdrawal position switch) is triggered, sending a signal to the PLC indicating that the insert pin has been completely withdrawn. Only after receiving this withdrawal position signal will the PLC allow the execution of the next action (mold opening), preventing forced mold opening before the insert pin is completely withdrawn, thus avoiding accidents such as tearing the product and damaging the mold. Therefore, the PLC receives the limit switch signal and decides whether to execute the next action (e.g., injection, mold opening) accordingly, thereby ensuring that the production actions of each mold are precise and consistent, improving production efficiency and product quality stability.

[0030] Of course, in addition to electrical control, mechanical blocking structures can also be set. For example, a mechanical blocking structure can be designed at the end of the piston stroke inside the cylinder or at the end of the movement groove of the connector 33. Even if the limit switch or electrical system fails unexpectedly, the mechanical blocking structure can prevent the cylinder from moving excessively and prevent damage to the insert, connector and other components.

[0031] The key design feature of this invention lies in its addition of a mounting cavity, recessed forward at the rear of the rear mold and extending into the mold cavity, based on the original mold. A hydraulically driven insert pin is added, dynamically inserted into the first cavity area before the aluminum alloy liquid is filled. This divides the originally continuous thick section into multiple thinner sections, thereby dispersing and eliminating heat concentration points, improving heat dissipation, and ensuring that the thick section of the casting solidifies synchronously or nearly synchronously with its surrounding area. This effectively prevents the formation of internal shrinkage cavities. Consequently, after CNC machining, the thick section of the casting will not have exposed internal holes, thus guaranteeing the product's appearance, strength, and airtightness. It can actively and controllably intervene in heat point formation, and its simple structure makes it suitable for upgrading and modifying molds for various aluminum alloy castings. It is highly practical and easy to promote and implement.

[0032] The above description is merely a preferred embodiment of the present utility model and does not constitute any limitation on the technical scope of the present utility model. Therefore, any minor modifications, equivalent changes and alterations made to the above embodiments based on the technical essence of the present utility model shall still fall within the scope of the technical solution of the present utility model.

Claims

1. A mold structure for improving shrinkage cavities in thick sections of aluminum alloy die-cast parts, characterized in that, include: Front mold (10); the front mold (10) is provided with a gate; Rear mold (20); the rear mold (20) is located below the front mold (10); the front mold (10) and the rear mold (20) form a mold cavity, the mold cavity includes a first cavity area and at least one second cavity area that are in contact with each other, the left and right width dimension, the up and down width dimension and the front and back thickness dimension of the first cavity area are all greater than the corresponding set values, and the front and back thickness dimension of the second cavity area is less than the corresponding set values; the rear part of the rear mold (20) is recessed forward to provide an installation cavity that extends into the mold cavity; Hydraulic cylinder insert device (30); The hydraulic cylinder insert device (30) is set in the mounting cavity and includes insert (31), hydraulic cylinder (32) and connector (33). The insert (31) is connected to the connector (33). The hydraulic cylinder (32) drives the connector (33) to move the insert (31) in the front-back direction, so that the insert (31) is inserted into the first cavity area of ​​the mold cavity after the mold is closed, and is pulled out from the first cavity area after the product is formed.

2. The mold structure for improving shrinkage cavities in thick sections of aluminum alloy die-cast parts according to claim 1, characterized in that, The connector (33) is connected to two or more inserts (31) arranged side by side with a spacing, so that after the product is formed, two or more pre-set inner holes are formed, and a connecting wall (413) is retained between adjacent pre-set inner holes.

3. The mold structure for improving shrinkage cavities in thick sections of aluminum alloy die-cast parts according to claim 2, characterized in that: The insert (31) includes a first needle body (311) and a second needle body (312) connected coaxially from the outside to the inside. The cross-sectional area of ​​the second needle body (312) is smaller than that of the first needle body (311). After the mold is closed, the inner ends of the second needle body (312) and the first needle body (311) are inserted into the first cavity area, so that a stepped pre-set inner hole is formed after the product is formed.

4. The mold structure for improving shrinkage cavities in thick sections of aluminum alloy die-cast parts according to claim 1, characterized in that, The cylinder insert device (30) is also equipped with a limit switch (35) for controlling the movement stroke of the insert (31).

5. The mold structure for improving shrinkage cavities in thick sections of aluminum alloy die-cast parts according to claim 4, characterized in that, The limit switch (35) includes a front limit switch and a rear limit switch, which are respectively connected to a PLC. The PLC is also respectively connected to the solenoid valve of the oil cylinder, the injection mechanism of the mold, and the mold opening / closing mechanism.

6. The mold structure for improving shrinkage cavities in thick sections of aluminum alloy die-cast parts according to claim 1, characterized in that, The rear mold (20) has a rear mold core mounting groove recessed at the front. A rear mold core (21) is detachably mounted in the rear mold core mounting groove. The rear mold core (21) has a second rear cavity corresponding to a plurality of second cavity areas. A rear insert (22) is also detachably mounted in the rear mold core (21). The rear insert (22) has a first rear cavity corresponding to the first cavity area formed by a rearward recess at the front. The rear of the rear insert (22) has a pin hole that extends forward through the first rear cavity. The pin hole extends backward through the mounting cavity. The pin (31) passes through the pin hole and extends into the first cavity area. The rear part of the front mold (10) is recessed forward to form a front mold core mounting groove. An upper insert (11) is detachably installed in the front mold core mounting groove. The rear part of the upper insert (11) is recessed forward to form a first front cavity corresponding to the first cavity area. The first front cavity and the first rear cavity are combined to form the first cavity. The rear part of the front mold (10) is combined with the second rear cavity to form the second cavity.

7. The mold structure for improving shrinkage cavities in thick sections of aluminum alloy die-cast parts according to claim 1, characterized in that, There is one first cavity area and three second cavity areas. The three second cavity areas are arranged at intervals and connected to the outer periphery of the first cavity. The end of one of the second cavity areas away from the first cavity serves as the gate inlet connection end.

8. The mold structure for improving shrinkage cavities in thick sections of aluminum alloy die-cast parts according to claim 7, characterized in that, The length of the second cavity region where the gate feed connection end is located is smaller than the length of other second cavity regions. The length refers to the distance between the end far from the first cavity and the end close to the first cavity.

9. The mold structure for improving shrinkage cavities in thick sections of aluminum alloy die-cast parts according to claim 1, characterized in that, At least one of the left-right width dimension and the top-bottom width dimension of the second cavity region is also less than the corresponding set value.

10. The mold structure for improving shrinkage cavities in thick sections of aluminum alloy die-cast parts according to claim 1, characterized in that, The cylinder insert device (30) is located in the mounting cavity. A recess extends from the side of the mounting cavity to the outer side of the rear mold (20). The oil pipe (34) connected to the cylinder (32) is hidden in the recess.