FRP impeller mold aluminum alloy mold

By using the concentric column and concentric hole design of the aluminum alloy mold, the FRP impeller is precisely positioned and pressurized, solving the problems of runout and thermal deformation, and improving product consistency and production efficiency.

CN224952284UActive Publication Date: 2026-11-10SUZHOU DINGYU ENERGY EFFICIENT EQUIP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522253544.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-10-24
Publication Date
2026-11-10
Estimated Expiration
2035-10-24

AI Technical Summary

Technical Problem

The existing FRP impeller molds lack effective positioning methods during assembly, which leads to wobble, insufficient connection strength, heat accumulation causing deformation, and non-compliant product dimensions.

Method used

The front cover mold, blade mold, and base plate mold are made of aluminum alloy. The design of concentric columns and concentric holes enables precise positioning and pressurization, and the thermal conductivity of aluminum alloy is used to evenly conduct heat.

Benefits of technology

This solved the runout problem of FRP impellers, improved the concentricity and connection strength of the products, avoided deformation caused by thermal stress, and improved the dimensional stability and pass rate of the products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224952284U_ABST
    Figure CN224952284U_ABST
Patent Text Reader

Abstract

This utility model discloses an aluminum alloy mold for FRP impeller assembly, comprising a front cover mold, a blade mold, and a base plate mold. The front cover mold has several weight-reducing ring grooves, and a detachable concentric column is located at its center. The blade mold is concentrically arranged with the front cover mold and the base plate mold. The base plate mold has a positioning boss at its center, and a concentric hole is formed at the center of the positioning boss, which engages with the concentric column. It also includes a pressure plate for applying pressure during blade assembly. This utility model achieves positioning through the concentric column of the front cover mold and the concentric hole of the base plate mold, reducing human alignment errors and solving the problem of FRP impeller sway. Utilizing the thermal conductivity of aluminum alloy, the temperature rise during impeller forming is effectively reduced, making the impeller less prone to deformation due to thermal stress and ensuring product dimensional stability. This utility model integrates positioning and pressurization functions, improving production efficiency and product consistency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of impeller molds, and more particularly to aluminum alloy molds for FRP impeller assembly. Background Technology

[0002] Fiber-reinforced plastic (FRP) impellers are widely used in ventilation, air conditioning, and special-purpose fans due to their advantages such as light weight, high strength, and corrosion resistance. Currently, FRP impellers are mostly molded in molds using processes such as hand lay-up and vacuum induction. However, existing molds and molding processes have the following significant drawbacks:

[0003] First, the impeller is assembled from multiple components such as the front cover, blades, and base plate. The lack of effective and precise positioning methods during assembly, relying primarily on manual alignment, easily leads to severe radial and axial runout in the finished impeller, affecting dynamic balance and causing vibration and noise. Second, to facilitate demolding, traditional mold designs limit the bonding area of ​​components, resulting in insufficient connection strength between impeller parts and a risk of cracking at the bonding points, leading to low reliability. Furthermore, during the curing process of FRP material, the resin cross-linking reaction generates a large amount of heat (temperature rise reaction). Traditional metal molds (such as steel molds) or non-metal molds have poor thermal conductivity, and the accumulated heat causes uneven heating of the FRP components within the mold cavity, generating internal stress, which in turn leads to impeller deformation, dimensional deviations, and a low yield rate.

[0004] Therefore, a new type of mold is needed that can solve the above problems simultaneously. Utility Model Content

[0005] The purpose of this invention is to provide an aluminum alloy mold for FRP impeller assembly that can solve the above-mentioned problems.

[0006] To achieve the above objectives, this utility model provides the following technical solution:

[0007] The FRP impeller assembly mold is an aluminum alloy mold comprising a front cover mold, a blade mold, and a base plate mold. The front cover mold has several weight-reducing ring grooves that penetrate the mold. A detachable concentric column is located at the center of the front cover mold. The impeller mold is positioned above and connected to the base plate mold. The blade mold is concentrically positioned with the front cover mold and the base plate mold. A positioning boss is located at the center of the base plate mold, and a concentric hole is formed at the center of the positioning boss, which engages with the concentric column. The mold also includes a pressure plate for applying pressure during blade assembly.

[0008] Preferably, the front cover mold, the blade mold, and the base plate mold are all made of aluminum alloy.

[0009] Preferably, a plurality of the weight-reducing ring grooves are evenly distributed near the outer edge of the front cover mold.

[0010] Preferably, the cross-section of each of the weight-reducing ring grooves is arc-shaped.

[0011] Preferably, the concentric column and the front cover mold are connected by a threaded connection, an interference fit connection, or a flange connection.

[0012] The beneficial effects of this invention are as follows: This invention achieves positioning through the concentric pillars of the front cover mold and the concentric holes of the bottom plate mold, reducing human alignment errors and solving the problem of FRP impeller runout. Utilizing the thermal conductivity of aluminum alloy effectively reduces the temperature rise during impeller forming, making the impeller less prone to deformation due to thermal stress, resulting in stable product dimensions and a high pass rate. This invention integrates positioning and pressurization functions, improving production efficiency and product consistency. Attached Figure Description

[0013] Figure 1 This is a structural schematic diagram of the front cover mold of this utility model;

[0014] Figure 2 This is a structural schematic diagram of the blade mold and the base plate mold of this utility model;

[0015] Figure 3 This is a schematic diagram of the structure of the pressure plate of this utility model;

[0016] Among them: front cover mold 1, blade mold 2, base plate mold 3, weight reduction ring groove 4, concentric column 5, positioning boss 6, concentric hole 7, pressure plate 8. Detailed Implementation

[0017] The technical solution of this patent will be further described in detail below with reference to specific embodiments.

[0018] In the description of this utility model, it should be noted that the terms "upper", "lower", "inner", "outer", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this utility model and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this utility model.

[0019] like Figures 1 to 3 As shown, this utility model provides an aluminum alloy mold for FRP impeller assembly, which includes a front cover mold 1, a blade mold 2, and a base plate mold 3.

[0020] The working surface profile of the front cover mold 1 is consistent with the preset profile of the impeller front cover. Several weight-reducing ring grooves 4 are formed on the front cover mold 1, penetrating the mold. These grooves are evenly distributed near the outer edge of the front cover mold 1, and each groove has an arc-shaped cross-section. A detachable concentric pillar 5 is located at the center of the front cover mold 1, and the concentric pillar 5 is connected to the front cover mold 1 via a threaded connection, interference fit connection, or flange connection.

[0021] The impeller mold 2 is positioned above the base plate mold 3 and is integrally connected to the base plate mold 3. The working surface profile of the blade mold 2 is consistent with the preset profile of the impeller blade. The blade mold 2 is concentrically positioned with the front cover mold 1 and the base plate mold 3.

[0022] A positioning boss 6 is provided at the center of the base plate mold 3, and a concentric hole 7 is opened at the center of the positioning boss 6. The concentric hole 7 and the concentric column 5 cooperate with each other, playing a key role in pre-positioning when the front cover mold 1 and the base plate mold 3 are combined. During the final mold closing (combining the front cover with the blade and base plate assembly), the concentric column 5 will pass through the central area of ​​the blade mold 2 and be precisely inserted into the concentric hole 7 of the base plate mold 3. This ensures the concentricity between the front cover, blade, and base plate, fundamentally solving the impeller wobble problem.

[0023] This invention also includes a pressure plate 8 for applying pressure to the blade assembly. The pressure plate 8 is mainly used to apply axial pressure to the blade during the blade and base plate assembly process to ensure that the blade can be assembled with the base plate in place and eliminate gaps.

[0024] The front cover mold 1, blade mold 2, and base plate mold 3 of this utility model are all made of aluminum alloy. Aluminum alloy has good thermal conductivity, which can quickly conduct and dissipate the heat generated during the FRP curing process, avoiding local overheating and heat accumulation, making the temperature field inside the cavity more uniform, greatly reducing impeller deformation caused by temperature rise reaction, and ensuring that the product dimensions meet the design requirements.

[0025] In use, the molded base plate is placed on the base plate mold 3. The molded blades are then aligned with the positioning bosses 6 of the base plate mold 3 and lowered down. The blades are initially positioned by the blade mold and the positioning bosses 6 of the base plate mold 3. The pressure plate 4 is then placed on top, and pressure is applied to the pressure plate 8 using an external pressure device to ensure full contact and proper assembly between the blades and the bonding surfaces of the base plate. After the blades and base plate are bonded and cured, a blade-base plate assembly is formed. Finally, the mold is closed, and the concentric column 5 is installed in the center of the front cover mold 1. The molded front cover is placed on the front cover mold 1, allowing the concentric column 5 to pass through the channel in the center of the blade and finally be precisely inserted into the concentric hole 7 of the base plate mold 3. The precise fit between the concentric column 5 and the concentric hole 7 ensures the concentricity of the front cover and the blade-base plate assembly. Then, mold closing pressure is applied to bond the front cover and the blade-base plate assembly. After final curing, demolding yields an FRP impeller product with high concentricity, high connection strength, and precise dimensions.

[0026] This invention achieves positioning through the concentric pillars 5 of the front cover mold 1 and the concentric holes 7 of the base plate mold 3, reducing human alignment errors and solving the problem of FRP impeller sway. Utilizing the thermal conductivity of aluminum alloy, the temperature rise during impeller forming is effectively reduced, making the impeller less prone to deformation due to thermal stress, resulting in stable product dimensions and a high yield rate. This invention integrates positioning and pressurization functions, improving production efficiency and product consistency.

[0027] It will be apparent to those skilled in the art that this invention is not limited to the details of the exemplary embodiments described above, and that it can be implemented in other specific forms without departing from the spirit or essential characteristics of this invention. Therefore, the embodiments should be considered illustrative and non-limiting in all respects, and the scope of this invention is defined by the appended claims rather than the foregoing description. Thus, it is intended that all variations falling within the meaning and scope of equivalents of the claims be included within this invention. No reference numerals in the claims should be construed as limiting the scope of the claims.

[0028] Furthermore, it should be understood that although this specification describes embodiments, not every embodiment contains only one independent technical solution. This narrative style is merely for clarity. Those skilled in the art should consider the specification as a whole, and the technical solutions in each embodiment can also be appropriately combined to form other embodiments that can be understood by those skilled in the art.

Claims

1. An FRP impeller split die aluminum alloy die comprising a front cover die, a blade die and a bottom plate die, characterized in that: The front cover mold is provided with a plurality of weight-reducing ring grooves, the weight-reducing ring grooves penetrate the front cover mold, and the center of the front cover mold is provided with a detachable concentric column; the blade mold is arranged above and connected with the bottom plate mold, the blade mold is concentrically arranged with the front cover mold and the bottom plate mold; the center of the bottom plate mold is provided with a positioning boss, the center of the positioning boss is provided with a concentric hole, and the concentric hole and the concentric column are matched with each other; and the pressure plate is further arranged to apply pressure to the blade assembly.

2. The FRP impeller matched die aluminum alloy die according to claim 1, characterized in that: The front cover mold, the blade mold and the bottom plate mold are all made of aluminum alloy material.

3. The FRP impeller matched die aluminum alloy die of claim 1, wherein: The plurality of weight-reducing ring grooves are uniformly distributed near the outer edge of the front cover mold.

4. The FRP impeller matched die aluminum alloy die according to claim 1 or 3, characterized in that: The cross section of each weight-reducing ring groove is arc-shaped.

5. The FRP impeller matched die aluminum alloy die of claim 1, wherein: The concentric column and the front cover mold are connected through thread connection, interference fit connection or flange connection.

6. The FRP impeller matched die aluminum alloy die of claim 1, wherein: The blade mold is integrally connected with the bottom plate mold.