A high-temperature asphalt mortar layered structure for road joints

By designing a high-temperature asphalt mortar layered structure, the problem of easy damage to road joints under high and low temperature conditions is solved. This achieves comprehensive performance improvement in high-temperature extrusion resistance, low-temperature crack resistance, interlayer anti-detachment, and seepage prevention, thus extending the service life of the joint structure.

CN224981997UActive Publication Date: 2026-11-17GUIZHOU ROAD & BRIDGE GRP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522658905.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-16
Publication Date
2026-11-17
Estimated Expiration
2035-12-16

AI Technical Summary

Technical Problem

Existing road surface joints are prone to damage under high and low temperature conditions. Traditional materials cannot simultaneously meet the comprehensive requirements of high temperature resistance to compression, low temperature resistance to cracking, interlayer anti-detachment and seepage prevention, making it difficult to adapt to the long-term stable use requirements of high-grade roads.

Method used

It adopts a high-temperature asphalt sand layered structure, including a high-temperature wear-resistant surface layer, a high-elasticity self-healing intermediate layer, a three-dimensional interlocking reinforcement layer, and an adhesive sealing bottom layer. Through specific layered structure and material combination, it forms a layered synergistic system of wear protection, self-healing buffer, interlocking reinforcement and sealing bonding, which enhances the interlayer connection strength and waterproof performance.

Benefits of technology

It improves the road joint's resistance to rutting at high temperatures, cracking at low temperatures, and interlayer shear peel strength, extends the service life of the joint structure, and achieves waterproof sealing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224981997U_ABST
    Figure CN224981997U_ABST
Patent Text Reader

Abstract

This application discloses a high-temperature asphalt mortar layered structure for road joints, relating to the field of road engineering joint treatment technology. It comprises, from top to bottom, a surface high-temperature abrasion-resistant layer, a high-elasticity self-healing intermediate layer, a three-dimensional interlocking reinforcement layer, an adhesive sealing underlayer, and a peelable silicone anti-sticking membrane. The three-dimensional interlocking reinforcement layer includes a PET grid and modified asphalt impregnated on the PET grid. The PET grid impregnated with modified asphalt is covered with pre-coated ceramic sand. This application achieves the objectives of preventing high-temperature extrusion, low-temperature brittleness, interlayer debonding, and seepage in road joints, thereby improving the overall service life and environmental adaptability of the joint structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of road engineering joint treatment technology, and in particular to a high-temperature asphalt mortar layered structure for road surface joints. Background Technology

[0002] In the field of road engineering, the transverse / longitudinal joints of facilities such as high-grade highways, airport pavements, and bridge decks are key parts of the road surface that are prone to damage due to long-term exposure to vehicle load shearing and environmental thermal expansion and contraction. The treatment effect of these joints directly affects the overall service life of the road.

[0003] For example, most pre-formed joint sealing tapes currently on the market are based on styrene-butadiene rubber (SBS) modified asphalt materials. Although they are easy to apply, their bonding with the road surface mainly relies on van der Waals forces, resulting in limited interfacial bond strength (typically a pull-out strength of less than 0.5 MPa). Under the repeated shearing action of high summer temperatures (road surface temperatures can reach over 70°C) and heavy traffic, they are highly susceptible to interlayer slippage and debonding.

[0004] Traditional on-site heated joint sealants, such as polymer-modified asphalt, while having good initial adhesion, have uniform material properties and cannot simultaneously meet the multiple functional requirements of surface wear resistance, middle layer flexibility, and bottom layer strong adhesion. After long-term use, they are still prone to problems such as high-temperature overflow or low-temperature brittleness. Moreover, their specially designed layered structure lacks a structural design that can achieve mechanical and chemical interlocking between layers, and cannot simultaneously meet the comprehensive requirements of high-temperature extrusion resistance, low-temperature crack resistance, interlayer anti-detachment, and seepage prevention for joints. They are difficult to adapt to the long-term stable use requirements of joints in high-grade roads. Utility Model Content

[0005] To address the existing problems of high-temperature compression resistance, low-temperature crack resistance, interlayer debonding prevention, and seepage prevention in road joints, this application provides a high-temperature asphalt mortar layered structure for road joints.

[0006] The high-temperature asphalt mortar layered structure for road joints provided in this application adopts the following technical solution:

[0007] A high-temperature asphalt mortar layered structure for road joints includes, from top to bottom, a surface high-temperature wear-resistant layer, a high-elasticity self-healing intermediate layer, a three-dimensional interlocking reinforcement layer, an adhesive sealing bottom layer, and a peelable silicone anti-sticking isolation film. The three-dimensional interlocking reinforcement layer includes a PET grid and modified asphalt impregnated on the PET grid. The PET grid impregnated with modified asphalt is covered with pre-coated ceramic sand.

[0008] By adopting the above technical solution, the silicone anti-adhesive release film can be peeled off during transportation and storage to isolate and seal the underlying layer, avoiding the stacking and adhesion of layered structures. During construction, after removing the release film, a hot-pressing process is used to tightly bond the surface high-temperature wear-resistant layer, the high-elastic self-healing intermediate layer, the three-dimensional interlocking reinforcement layer, and the adhesive sealing layer. PET grids serve as the skeleton support, and pre-wrapped ceramic sand fills the gaps between the grids and enhances the physical interlocking with the upper and lower layers, forming a layered synergistic system of "wear protection, self-healing buffer, interlocking reinforcement, and sealing adhesion." Through specific layered structures and material combinations, the structure's resistance to rutting at high temperatures, its resistance to cracking at low temperatures, the shear peel strength between layers, and the overall waterproof sealing performance are improved, thereby potentially extending the service life of the joint structure.

[0009] Preferably, the modified asphalt is composed of SBS block copolymer, waste rubber powder, compatibilizer and base asphalt.

[0010] By adopting the above technical solutions, SBS block copolymers can form an elastic network structure in asphalt, significantly improving the material's high-temperature rheological resistance and preventing the joint structure from softening and extruding under high summer temperatures. Waste rubber powder has both elasticity and wear resistance, which can enhance the material's low-temperature flexibility and improve the surface wear resistance. Sulfur, as a compatibilizer, can promote the interfacial fusion of SBS with the base asphalt and waste rubber powder, avoid component stratification, and ensure uniform material performance. The base asphalt provides basic adhesion and construction fluidity for the whole. The synergistic effect of the four optimizes the comprehensive high and low temperature performance of the modified asphalt, which helps to improve the high-temperature rutting resistance and low-temperature crack resistance of the asphalt sand-rubber layered structure.

[0011] Preferably, the highly elastic self-healing intermediate layer contains a microencapsulated regenerator.

[0012] By adopting the above technical solution, the high-elastic self-healing intermediate layer itself is elastic and can buffer the thermal expansion and contraction stress of the road joint; when cracks occur in the joint, the capsule wall of the microencapsulated regenerator ruptures, releasing the internal regenerator to penetrate into the crack and repair the crack gap, giving the layered structure the ability to self-repair after micro-cracks occur, which helps to inhibit the further expansion of cracks and maintain its waterproof sealing performance.

[0013] Preferably, the surface high-temperature wear-resistant layer is composed of basalt sand and modified bitumen.

[0014] By adopting the above technical solutions, basalt sand has high hardness and wear resistance, and can directly withstand tire friction and external impact. Modified asphalt firmly binds the basalt sand, and at the same time, it resists high temperature softening due to its own high softening point, preventing the basalt sand from loosening and falling off, thus achieving the purpose of wear resistance and high temperature resistance of the road joint surface.

[0015] Preferably, the PET grid has ribs at both the top and bottom.

[0016] By adopting the above technical solution, the top ribs of the PET grid are embedded in the high-elastic self-healing intermediate layer, and the bottom ribs are embedded in the adhesive sealing bottom layer, forming a two-way mechanical anchoring structure. This breaks the traditional "single-sided point-to-line" contact bonding mode, enhances the connection strength between the three-dimensional interlocking reinforcement layer and the upper and lower layers, resists vehicle shear force, achieves the purpose of preventing interlayer debonding, and improves the interlayer shear strength of the layered structure.

[0017] Preferably, the bonding and sealing underlayer is composed of a composite mortar of modified asphalt and cement emulsified asphalt.

[0018] By adopting the above technical solutions, modified asphalt provides elasticity and bonding flexibility to adapt to the slight deformation of road joints; cement emulsified asphalt composite mortar provides rigidity and high strength to ensure a firm bond between the base layer and the subbase. The synergy of rigidity and flexibility prevents the base layer from cracking due to excessive rigidity or detaching due to excessive flexibility, thus achieving the goal of tightly sealing and bonding the road joints with the subbase.

[0019] Preferably, the thickness of the peelable silicone anti-stick release film is 0.04 to 0.06 mm.

[0020] By adopting the above technical solution, the thickness design of the peelable silicone anti-stick release film 5 not only ensures the isolation strength during transportation and storage, preventing the adhesive sealing bottom layer 4 from sticking to other structures, but also ensures that it can be easily removed during construction, and that no residue remains after removal that affects the bonding effect between the adhesive sealing bottom layer 4 and the underlying layer. This achieves the purpose of simplifying the construction process, improving construction efficiency, and reducing the pretreatment time and cost before the construction of layered structures.

[0021] In summary, this application includes at least one of the following beneficial technical effects:

[0022] Through the synergy of a high-temperature wear-resistant surface layer, a high-elasticity self-healing intermediate layer, and a three-dimensional interlocking reinforcement layer, the composite layered structure provided in this application achieves high-temperature non-softening extrusion and low-temperature non-brittleness. The interlayer shear strength is effectively improved compared with traditional joint sealing tape, and it can self-repair when microcracks occur in the structure. Compared with the existing technology of filling or sealing joints using a single modified asphalt material, the composite layered structure provided in this application is expected to achieve significant improvements in key performance indicators such as high-temperature stability, low-temperature flexibility, and interlayer bonding strength. Attached Figure Description

[0023] Figure 1 This is a three-dimensional schematic diagram of the present application;

[0024] Figure 2 This is an enlarged 3D schematic diagram of point A in Figure 1.

[0025] Figure 3This is a three-dimensional schematic diagram of the three-dimensional interlocking reinforcement layer in this application.

[0026] Figure label:

[0027] 1. High-temperature wear-resistant surface layer; 2. High-elasticity self-healing intermediate layer; 3. Three-dimensional interlocking reinforcement layer; 4. Adhesive sealing bottom layer; 5. Peelable silicone anti-stick release film; 6. Ribs. Detailed Implementation

[0028] The following is in conjunction with the appendix Figures 1-3 This application will be described in further detail.

[0029] This application discloses a high-temperature asphalt mortar layered structure for road joints.

[0030] Reference Figure 1 and Figure 2 A high-temperature asphalt mortar layered structure for road joints includes, from top to bottom, a surface high-temperature wear-resistant layer 1, a high-elastic self-healing intermediate layer 2, a three-dimensional interlocking reinforcement layer 3, an adhesive sealing bottom layer 4, and a peelable silicone anti-sticking release film 5. The thickness of the peelable silicone anti-sticking release film 5 is 0.04-0.06 mm, and a transparent silicone film with a thickness of 0.05 mm is selected. The surface is coated with a 0.01 mm thick organic silicone anti-sticking coating to prevent adhesion during transportation and stacking. The three-dimensional interlocking reinforcement layer 3 is composed of PET grid impregnated with modified asphalt. Ribs 6 are provided at the top and bottom of the PET grid. The thickness of the three-dimensional interlocking reinforcement layer 3 is 1.3-1.7 mm. The rib width of the PET grid is 3.8-4.2 mm, the rib thickness is 0.8-1.2 mm, the grid size is (11-13) mm × (11-13) mm, and the particle size of the pre-coated ceramic sand is 0.3-0.6 mm.

[0031] The high-temperature asphalt sand-rubber layered structure has an overall thickness of 7.0–8.0 mm, a width of 50–100 mm, and a length of 3–10 m / roll. It can be cut to any size according to the joint requirements. Modified asphalt is pre-cured to 60%–70% curing degree and embedded with pre-coated ceramic sand to form a "grid-sand-embedded" composite. Each layer is formed in one step by hot pressing at 115–125℃ and 0.5–0.8 MPa. The upper and lower ends of the grid ribs are embedded into the adjacent layers by 0.3–0.6 mm. During construction, after removing the isolation film 5, the asphalt at the interface of each layer is melted and interpenetrated by hot pressing at 115–125℃ and 0.5–0.8 MPa. At the same time, the upper and lower ends of the ribs of the PET grid 31 are embedded into the adjacent layers by 0.3–0.6 mm. The pre-coated ceramic sand fills the grid gaps and enhances the physical interlocking with the upper and lower layers.

[0032] Reference Figure 1Modified asphalt is composed of SBS (styrene-butadiene-styrene) block copolymer, waste rubber powder, compatibilizer, and base asphalt. The SBS block copolymer is added at 4-6%, waste rubber powder (particle size 0.15-0.3 mm) at 10-15%, and compatibilizer (sulfur) at 0.3-0.5%. The base asphalt is road petroleum asphalt with a penetration of 60-80. The base asphalt is heated to 150-160℃, and 5% SBS block copolymer is added and stirred for 30-40 minutes until completely dissolved. Then, 12% waste rubber powder (particle size 0.2 mm) and 0.4% sulfur are added, and the temperature is raised to 165-175℃ and stirred at high speed for 60-80 minutes to produce modified asphalt. Once the mixture is homogeneous, the modified asphalt mixture is obtained.

[0033] Reference Figure 1 The high-elastic self-healing intermediate layer 2 contains 0.5-1.0 wt% of microencapsulated regenerator. The microencapsulated regenerator has an aromatic oil core and a melamine-urea-formaldehyde resin wall with an average particle size of 50-100 μm. The melting point of the microencapsulated regenerator wall is 85-95℃. When the crack width is >0.3 mm, the self-healing rate of the crack in this intermediate layer is ≥80% within 24 hours.

[0034] When microcracks develop at pavement joints due to temperature changes or loads, a high degree of stress concentration occurs at the crack tip during the expansion process. When the microcrack tip extends to the vicinity of the microencapsulated regenerator inside the high-elasticity self-healing intermediate layer 2, this stress concentration effect exceeds the fracture strength of the microcapsule wall (such as melamine-urea-formaldehyde resin), causing the capsule wall to rupture. After the capsule wall ruptures, the liquid regenerator (such as aromatic oil) stored inside is drawn into the microcrack through capillary action, swelling and regenerating the aged asphalt around the crack, restoring its adhesion and fluidity, thereby healing the crack and restoring the sealing and integrity of the structure.

[0035] The surface high-temperature wear-resistant layer 1 has a thickness of 2.8-3.2 mm and is composed of 70% basalt sand and 30% modified asphalt. The surface high-temperature wear-resistant layer 1 is prepared by heating the modified asphalt to 120-125℃ and mixing it with basalt sand (particle size 1.18-2.36 mm) preheated to 80-90℃ at a mass ratio of 3:7 and stirring for 15-20 min.

[0036] Basalt sand with a particle size of 1.18–2.36 mm (70% of the composition) has high hardness and wear resistance, and can directly withstand tire friction and external impact, avoiding surface wear. Modified asphalt 12 (30% of the composition) firmly binds the basalt sand, and at the same time, it resists high-temperature softening due to its high softening point (≥120℃), preventing the basalt sand from loosening and falling off. The thickness design of 2.8–3.2 mm further ensures the surface protection strength, achieving the purpose of wear resistance and high-temperature resistance of the road joint surface.

[0037] The thickness of the bonding and sealing base layer 4 is 0.8-1.2 mm, and it is composed of 50% modified asphalt and 50% cement emulsified asphalt composite mortar. The modified asphalt (120-125℃) and cement emulsified asphalt composite mortar (cement to emulsified asphalt mass ratio 1:2, room temperature) are mixed at a mass ratio of 1:1 and stirred for 10-15 min. The mass ratio of cement to emulsified asphalt in the cement emulsified asphalt composite mortar is 1:2, and the tensile strength of this base layer at 25℃ is ≥2.5 MPa.

[0038] Modified asphalt (50%) provides elasticity and bonding flexibility to accommodate minor deformations at pavement joints; cement emulsified asphalt composite mortar (50%, cement to emulsified asphalt mass ratio 1:2) provides rigidity and high strength to ensure a strong bond between the base layer and the subbase.

[0039] The implementation principle of a high-temperature asphalt mortar layered structure for road joints in this application embodiment is as follows:

[0040] Pre-construction isolation: A peelable silicone anti-stick release film 5 (0.04~0.06mm) is used to cover the bonding and sealing base layer 4 to prevent adhesion during transportation and stacking. It can be directly removed during construction without affecting the adhesion between the base layer and the underlying layer.

[0041] Hot-press interlocking molding: Each layer is hot-pressed once at 115-125℃ and 0.5-0.8MPa, and the interfacial asphalt melts and interpenetrates; the PET grid 31 ribs of the three-dimensional interlocking reinforcement layer 3 are embedded 0.3-0.6mm into the adjacent layers, and the pre-coated ceramic sand 32 fills the gaps, forming a mechanical and chemical double interlocking to prevent interlayer debonding;

[0042] High-temperature wear-resistant protection: The surface high-temperature wear-resistant layer 1 (2.8~3.2mm, 70% basalt sand + 30% modified asphalt 12) directly resists tire friction. The modified asphalt is resistant to high temperature (softening point ≥120℃), and has a dynamic stability of ≥30000 times / mm at 60℃, preventing extrusion at high temperatures in summer.

[0043] Self-healing cracks: When the crack in the joint is >0.3mm, the microencapsulated regenerator 21 (capsule wall melting point 85~95℃) in the high-elastic self-healing intermediate layer 2 ruptures, releasing the regenerator to repair the crack. The self-healing rate is ≥80% in 24 hours, preventing crack expansion and water seepage.

[0044] Bottom layer sealing and bonding: Bonding and sealing bottom layer 4 (0.8~1.2mm, 50% modified bitumen + 50% composite mortar) with rigidity and flexibility, tensile strength ≥2.5MPa at 25℃, firmly bonding to the underlying layer.

[0045] The above are merely optional embodiments of this application and are not intended to limit this application. Various modifications and variations can be made to this application by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this application should be included within the protection scope of this application.

Claims

1. A high temperature asphalt mastic layer for a pavement joint, characterized by, Comprise: From top to bottom, surface high temperature wear resistant layer (1), high elastic self-healing intermediate layer (2), three-dimensional interlocking reinforcing layer (3), adhesive sealing bottom layer (4) and peelable silicone release film (5) are arranged in turn, the three-dimensional interlocking reinforcing layer (3) comprises PET grid and modified asphalt impregnated on the PET grid, the outside of the PET grid impregnated with modified asphalt is sprinkled with pre-wrapped ceramic sand.

2. A high temperature asphalt mastic layered structure for pavement joints according to claim 1, characterized in that: The high elastic self-healing intermediate layer (2) contains microencapsulated regenerant.

3. A high temperature asphalt mastic layered structure for pavement joints according to claim 1, characterized in that: The top and bottom of the PET grid are provided with ribs (6).

4. A high temperature asphalt mastic layered structure for pavement joints according to claim 1, characterized in that: The thickness of the peelable silicone release film (5) is 0.04-0.06 mm.