Batteries and battery packs
By using laser-penetrating welding and a copper-aluminum layered structure, the problem of electrode welding damage was solved, achieving a high-strength, low-internal-resistance battery connection and improving the battery's conductivity and mechanical stability.
Patent Information
- Application Number
- CN202522380722.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-07
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-11-07
AI Technical Summary
In existing technologies, welding damage often occurs when the electrode posts are welded to the battery cell, affecting battery quality and leading to unstable conductivity and insufficient mechanical strength.
Laser penetration welding technology is used to form a molten pool between the electrode and the connector, so that the laser energy is accurately transmitted to the interface of the connector along the thickness direction of the electrode. Combined with the design of heterogeneous metal layers, including the layered structure of aluminum and copper, the welding groove shape and molten pool distribution are optimized.
It improves welding reliability and conductivity stability, reduces the risk of incomplete welding, enhances mechanical strength and fatigue resistance of the welded area, and ensures consistent current conduction and long-term battery reliability.
Smart Images

Figure CN224986579U_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of battery technology, and more particularly to a battery and a battery pack. Background Technology
[0002] Currently, the terminals are a key component of the battery cell, responsible for converting chemical energy into electrical energy or vice versa. The terminal materials are typically composed of copper and aluminum; the combination of copper and aluminum improves conductivity and mechanical strength while reducing internal resistance. In existing technologies, welding damage often occurs during the connection of the terminals to the battery cell, thus affecting battery quality. Utility Model Content
[0003] This application provides a battery and a battery pack to at least partially solve the above-mentioned technical problems.
[0004] To achieve the above objectives, according to a first aspect of this application, a battery is provided, comprising a cell, terminals, and a connector, wherein the connector is disposed on the cell, the terminals are connected to the connector on the side opposite to the cell, and the terminals and the connector are connected by laser welding; wherein... The electrode and the connector form a molten pool under the action of laser welding. Along the thickness direction of the electrode, the molten pool extends from the side of the electrode away from the connector to the interface between the electrode and the connector.
[0005] By employing the above technical solution, a molten pool is formed between the electrode and the connector using laser penetration welding. This allows laser energy to be precisely transmitted along the thickness direction of the electrode and penetrates to the interface of the connector, achieving a high-strength metal bond. This welding method can effectively control the heat input while maintaining the continuity and uniformity of the weld, thereby preventing damage to the connector due to overheating. Compared with traditional surface welding, this structure improves connection reliability, reduces residual welding stress and the risk of incomplete welds, and ensures the stability and consistency of current conduction within the battery cell.
[0006] In one embodiment, the connector includes a tab connected between the battery cell and the terminal post, and the molten pool extends from the side of the terminal post away from the tab to the interface between the terminal post and the tab. Alternatively, the connector includes a tab and a connecting piece, the tab being connected to the battery cell, a first side of the connecting piece being connected to the tab, a second side of the connecting piece being connected to the electrode post, and the molten pool extending from the side of the electrode post away from the connecting piece to the interface between the electrode post and the connecting piece.
[0007] By adopting the above technical solution, when the connector is an electrode tab, the laser energy is precisely transmitted along the thickness direction of the electrode post and penetrates to the electrode tab interface, achieving a high-strength metal bond. This welding method can effectively control the heat input while maintaining the continuity and uniformity of the weld, thereby avoiding damage to the electrode tab due to overheating; and when the connector includes a connecting piece and an electrode tab, the laser welding will directly reach the connecting piece without affecting the electrode tab, making the electrode tab less prone to damage.
[0008] In one embodiment, the pole includes a first metal layer and a second metal layer, the second metal layer being connected to the connector, and the first metal layer being connected to the side of the second metal layer opposite to the connector.
[0009] By adopting the above technical solution, the electrode post is divided into a first metal layer and a second metal layer, achieving a structural division of labor among dissimilar metals. The second metal layer is directly welded to the connector to ensure conductivity, while the first metal layer provides mechanical strength and structural support. This layered design achieves a balance between different functional requirements, concentrating the welding area in a layer with high material compatibility, thereby improving welding reliability and thermal conductivity, and reducing stress concentration caused by thermal mismatch.
[0010] In one embodiment, the second metal layer and the connector are made of the same metal material, while the second metal layer and the first metal layer are made of different metal materials.
[0011] By adopting the above technical solution, designing the second metal layer and the connector to be made of the same metal material can significantly reduce the risk of intermetallic chemical reactions and brittle phase formation during laser welding, and improve the uniformity and ductility of the weld metal bonding. At the same time, the setting of the first metal layer as a dissimilar metal layer enables the overall electrode post to have both excellent conductivity and high structural rigidity, improving the mechanical stability of the battery during charge and discharge cycles.
[0012] In one embodiment, the first metal layer is made of aluminum; and / or, the second metal layer is made of copper.
[0013] By adopting the above technical solution and selecting an aluminum first metal layer and a copper second metal layer, a synergistic optimization of weight and conductivity is achieved. The aluminum layer provides excellent thermal conductivity and lightweight properties, while the copper layer provides high conductivity and weldability. This gives the electrode post a comprehensive performance of low internal resistance, high heat dissipation efficiency, and high mechanical strength, thereby improving the battery's energy density and cycle life. In one embodiment, a welding groove is formed on the first metal layer, the welding groove extends along the thickness direction of the electrode post, the bottom surface of the welding groove is the initial welding position of the laser welding, and the molten pool extends from the bottom surface of the welding groove into the second metal layer.
[0014] By adopting the above technical solution, a welding groove is opened on the first metal layer, allowing the laser beam energy to be focused at the bottom of the welding groove as the initial welding position. This results in higher energy utilization and a more concentrated molten pool. The molten pool extends along the thickness direction to the interface between the second metal layer and the connector, achieving layered deep penetration welding. This structure not only enhances welding strength but also prevents excessive laser energy diffusion through the groove's guiding effect, thereby further avoiding connector ablation and improving welding accuracy and consistency.
[0015] In one embodiment, the molten pool portion includes a first molten pool sub-portion extending from the initial welding position into the second metal layer along the thickness direction of the pole post; The molten pool portion further includes a second molten pool sub-portion, which is connected to the first molten pool sub-portion. Along the thickness direction of the pole post, the second molten pool sub-portion extends from within the first metal layer to the interface between the second metal layer and the pole post.
[0016] By employing the above technical solution, and subdividing the molten pool into a first molten pool sub-section and a second molten pool sub-section, a graded welding zone can be formed in different metal layers, making the weld depth and energy distribution controllable. The first molten pool sub-section is mainly distributed within the first metal layer, forming a stable initial welding base; the second molten pool sub-section extends to the interface between the second metal layer and the connector, ensuring complete weld penetration. This double-layer molten pool structure effectively alleviates the welding thermal gradient and improves weld strength and fatigue resistance.
[0017] In one embodiment, the cross-sectional width of the first molten pool sub-section gradually decreases along the direction from the first metal layer to the second metal layer.
[0018] By adopting the above technical solution, the structure in which the width of the first molten pool subsection gradually decreases along the thickness direction makes the energy distribution of the weld more uniform, forming a natural penetration transition zone and avoiding cracks or voids caused by heat concentration. This gradual shape helps to achieve stepwise heat transfer, reduces stress concentration effects, and thus improves the fatigue life and electrical conductivity stability of the welded joint.
[0019] In one embodiment, the cross-sectional shape of the second molten pool sub-section is crescent-shaped.
[0020] By adopting the above technical solution, the second molten pool subsection forms a crescent-shaped cross-section, which can create a good transition at the molten pool boundary and make the stress distribution at the top and bottom of the weld more uniform. The crescent shape is conducive to the release of shrinkage stress and the stable control of intermetallic flow, thereby reducing the probability of weld porosity and incomplete welds, and improving the density and impact resistance of the welded area.
[0021] In one embodiment, the second molten pool sub-part has a protrusion located within the first metal layer and protruding in a direction away from the second metal layer, and the first molten pool sub-part has a groove in which the protrusion is embedded.
[0022] By adopting the above technical solution, the second molten pool sub-section is provided with a protrusion, and the first molten pool sub-section is provided with a corresponding groove, achieving a fitting connection and forming a mechanical interlocking structure between the two molten pools. This protrusion-concave fit not only improves the shear strength of the fusion interface but also prevents weld peeling. This further enhances the stability of the weld joint surface and improves the weld's vibration resistance and thermal shock resistance.
[0023] In one embodiment, the minimum thickness of the first metal layer in the thickness direction of the pole post is a, where 0 mm < a ≤ 1 mm; And / or, the minimum thickness of the second metal layer in the thickness direction of the pole is b, 0.5a < b ≤ 2a.
[0024] By adopting the above technical solution, and by limiting the thickness range of the first metal layer and the second metal layer, i.e., the ratio of A to B, the welding energy conduction path and penetration depth are controlled within the optimal range. Appropriate thickness matching can ensure conductivity while preventing excessive laser energy transmission, thus avoiding thermal damage to the joint. This dimensional ratio achieves a balance between welding depth and welding strength, improving the stability of the welding process window.
[0025] In one embodiment, the battery further includes a cover plate and a fixing component, wherein the cover plate has a through-hole for mounting, and the fixing component and the terminal post are both embedded in the mounting hole.
[0026] By adopting the above technical solution, and setting up fixing components, cover plates, and mounting holes, the pole posts and fixing components are all embedded in the mounting holes to form a high-precision assembly interface, effectively improving the mechanical fixing strength and the stability of the current output path. This structure also makes the current transmission path inside the cell shorter and the contact resistance lower, thereby improving the overall electrical performance and thermal conductivity of the battery pack.
[0027] In one embodiment, in the thickness direction of the electrode post, the projected area of the welding area formed by the laser welding on the electrode post is S1, and the projected area of the fixing component is S2, where 1 / 3S2≤S1≤4 / 5S2.
[0028] By adopting the above technical solution, the ratio range between the projected area S1 of the laser penetration welding and the projected area S2 of the fixed component is limited, thereby creating an optimal stress distribution relationship between the welding area and the load-bearing area of the fixed component. This ratio control ensures sufficient welding strength while avoiding material waste or thermal deformation caused by an excessively large weld area, thus optimizing mechanical stability and electrical conductivity uniformity.
[0029] In one embodiment, the cover plate includes a bare aluminum sheet and a lower plastic sheet, the lower plastic sheet being connected to the side of the bare aluminum sheet near the connector; The fixing component includes a welding block, an upper plastic and a sealing ring. The sealing ring is sleeved between the outer peripheral wall of the pole and the mounting hole. The aluminum sheet has a mounting groove on the outer periphery of the mounting hole. The upper plastic is embedded in the mounting groove. The surface of the upper plastic facing away from the mounting groove has a pressing groove. The welding block is embedded in the pressing groove.
[0030] By adopting the above technical solution, the cover plate uses a composite structure of a smooth aluminum sheet and a lower plastic layer, which ensures conductivity, protection, and sealing performance while also considering weight and heat resistance. The smooth aluminum sheet improves structural rigidity and heat dissipation capacity, while the lower plastic layer provides electrical insulation and cushioning and shock absorption functions, thereby improving the reliability and safety of battery packaging. By setting mounting grooves on the smooth aluminum sheet and configuring upper plastic, welded pressure blocks, and sealing rings, a multi-layer sealing and fixing structure is achieved. The sealing ring enhances liquid and gas resistance, the upper plastic filling the grooves improves assembly stability, and the welded pressure blocks achieve reliable end-face pressing. This integrated structure can effectively prevent leakage of external gas or electrolyte, ensuring long-term safe use of the battery.
[0031] In one embodiment, the battery further includes an explosion-proof valve and an explosion-proof film. An explosion-proof hole is formed on the aluminum sheet, the explosion-proof valve is installed in the explosion-proof hole, and the explosion-proof film is attached to the side of the explosion-proof valve facing away from the lower plastic.
[0032] By adopting the above technical solutions, including the installation of explosion-proof valves and explosion-proof films, the battery can release pressure in a directional manner when overcharged, overheated, or when internal gas expands, preventing the casing from bursting. The explosion-proof film combines sealing and protection functions, maintaining local isolation after the explosion-proof valve activates, thus improving the battery's safety protection level and meeting the safety design requirements of high-energy-density cells.
[0033] In one embodiment, the battery further includes a casing, a battery cell, a separator, and a support frame. The battery cell is installed inside the casing, the separator is installed between the cover and the connector, and the separator is connected to the support frame and allows a portion of the connector to pass through and overlap.
[0034] By adopting the above technical solution, a stable mechanical support and electrical isolation structure is formed by setting an isolation plate and a support frame between the shell and the cover plate. The isolation plate prevents short circuits caused by direct contact between the connectors and the metal cover plate, while the support frame enhances the positioning accuracy of the battery cells. This structure improves the overall package's vibration resistance and modular assembly accuracy, adapting to the complex operating conditions of vehicles and energy storage scenarios.
[0035] According to a second aspect of this application, a battery pack is provided, including the battery of the first aspect.
[0036] The beneficial effects of the embodiments of this application are as follows: 1. By using laser penetration welding to connect the electrode and the connector, laser energy is fully transferred along the thickness direction of the electrode to the interface region of the connector, thereby forming a continuous and dense molten pool between them. This molten pool is distributed throughout the thickness direction, forming an intermetallic chemical bonding layer between the electrode and the connector at the microscopic level. This significantly reduces the contact interface resistance and improves conductivity. The presence of the molten pool can also alleviate the problem of welding stress concentration to a certain extent, improve the mechanical strength and fatigue resistance of the welded area, and prevent crack propagation in the heat-affected zone. In addition, this structure makes the heat distribution in the welded area more uniform, which helps to suppress excessive melting and material ablation, ensuring the stability and consistency of the welded joint, and providing structural protection for the long-term reliable operation of the battery under high-rate charging and discharging and vibration conditions. 2. By forming a composite molten pool structure consisting of a first molten pool sub-section and a second molten pool sub-section within the laser penetration welding area between the electrode and the connector, the molten metal is distributed in layers and sections along the thickness direction, forming a stable welding transition zone. The first molten pool sub-section extends from the initial welding position into the interior of the second metal layer, undertaking the conduction and diffusion of laser energy. The second molten pool sub-section extends from the interior of the first metal layer to the interface between the electrode and the second metal layer, forming a covering and supporting structural feature. Through this layered metallurgical bonding region, the metal microstructure inside the weld is refined and evenly distributed, and the bonding interface is continuous and stable. This is beneficial to improving the electrical conductivity and mechanical strength of the welded part to a certain extent, while improving the stress transmission path of the weld, reducing thermal stress concentration, and enhancing the reliability and fatigue resistance of the weld under charge-discharge cycles and vibration conditions. Attached Figure Description To more clearly illustrate the technical solutions in the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0037] To gain a more complete understanding of this application and its beneficial effects, the following description will be provided in conjunction with the accompanying drawings, wherein the same reference numerals in the following description denote the same parts.
[0038] Figure 1 This is a schematic diagram of the overall structure of the battery according to an embodiment of this application; Figure 2 This is an internal cross-sectional view of the battery according to an embodiment of this application; Figure 3 This is a structural cross-sectional view of the connection relationship between the pole and the connector in some embodiments of this application; Figure 4 yes Figure 3 An enlarged schematic diagram of part A in the middle; Figure 5 This is a structural cross-sectional view of the connection relationship between the pole and the connector in some other embodiments of this application; Figure 6 yes Figure 5 An enlarged schematic diagram of part B in the diagram; Figure 7 This is a first explosion diagram of the battery according to an embodiment of this application; Figure 8 This is a second explosion diagram of the battery according to an embodiment of this application.
[0039] Explanation of reference numerals in the attached figures: 1. Battery cell; 2. Pole post; 21. First metal layer; 211. Welding groove; 22. Second metal layer; 3. Connector; 31. Electrode; 32. Connecting piece; 4. Molten pool section; 41. First molten pool sub-section; 411. Groove; 42. Second molten pool sub-section; 421. Protrusion; 5. Cover plate; 51. Plain aluminum sheet; 511. Mounting groove; 52. Lower plastic; 53. Mounting hole; 6. Fixing components; 61. Welding blocks; 62. Applying plastic; 63. Pressing groove; 64. Sealing ring; 7. Explosion-proof valve; 71. Explosion-proof film; 8. Shell; 9. Isolation panel; 10. Support frame. Detailed Implementation
[0040] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of this application, and not all of them. All other embodiments obtained by those skilled in the art based on the embodiments of this application without creative effort are within the protection scope of this application.
[0041] This embodiment provides a battery and electrical device designed to improve upon existing problems such as overheating in the welding area, damage to the tabs, incomplete soldering, and excessive contact resistance during the connection of battery cell terminals and tabs. This structure optimizes the metal layering structure of the terminals, the molten pool distribution, and the packaging assembly, making the energy conduction path during laser penetration welding controllable, thereby achieving a functional balance in terms of conductivity, thermal conductivity, and mechanical support.
[0042] Firstly, this application provides a battery, please refer to [link to relevant documentation]. Figure 1 , Figure 2 and Figure 3 The battery includes a cell 1, a terminal post 2, and a connector 3. The connector 3 is located on the upper end of the cell 1, and the terminal post 2 is installed on the side of the connector 3 away from the cell 1. The terminal post 2 and the connector 3 are connected by laser welding.
[0043] For example, the specific method of laser welding connection can be laser penetration welding connection.
[0044] Furthermore, the electrode post 2 and the connector 3 form a molten pool 4 under the action of laser penetration welding. Along the thickness direction of the electrode post 2, the molten pool 4 extends from the electrode post 2 to the interface with the connector 3.
[0045] It is understandable that laser penetration welding, as a high-energy beam welding technology, uses a high-energy-density laser beam to penetrate the metal layer in a very short time to form a weld with a large depth-to-width ratio. Its welding area is small and the heat-affected zone is limited, making it suitable for precision welding of dissimilar metals such as copper and aluminum.
[0046] During laser penetration welding, the laser beam is focused by a focusing lens and incident perpendicularly on the surface of the electrode post 2. The laser energy forms an instantaneous high-temperature melting zone on the surface of the electrode post 2 material, creating a molten pool 4 along the thickness direction of the electrode post 2. This molten pool 4 extends longitudinally from the upper surface of the electrode post 2 to the mating surface of the connector 3. Due to the strong directionality and high energy density of laser penetration welding, the energy is mainly concentrated in the thickness direction of the electrode post 2, and the heat is transferred longitudinally. After reaching the mating interface of the connector 3, the energy gradually decays, preventing the connector 3 from over-melting. In this way, the welding depth can be precisely terminated at the surface layer of the connector 3 under energy control, achieving a conductive connection without damaging the main structure of the connector 3.
[0047] In some implementations, combined with Figure 3 , Figure 4 The connector 3 includes a tab 31, which is connected between the cell 1 and the post 2. The molten pool 4 extends from the side of the post away from the tab 31 to the interface between the post 2 and the tab 31.
[0048] In some implementations, combined with Figure 5 , Figure 6 The connector 3 includes a tab 31 and a connecting piece 32. The tab 31 is connected to the cell 1. The first side of the connecting piece 32 is connected to the tab 31, and the second side of the connecting piece 32 is connected to the pole post 2. The molten pool portion 4 extends from the side of the pole post 2 away from the connecting piece 32 to the interface between the pole post 2 and the connecting piece 32.
[0049] It is understandable that when the connector 3 is the tab 31, the laser energy is precisely transmitted along the thickness direction of the electrode post 2 and penetrates to the interface of the tab 31, achieving a high-strength metal bond. This welding method can effectively control the heat input while maintaining the continuity and uniformity of the weld, thereby avoiding damage to the tab 31 due to overheating. When the connector 3 includes the connecting piece 32 and the tab 31, the laser welding will directly reach the connecting piece 32 without affecting the tab 31, making the tab 31 less prone to damage and thus improving its service life.
[0050] In some implementations, combined with Figure 2 , Figure 3 The pole post 2 includes a first metal layer 21 and a second metal layer 22. The second metal layer 22 is close to the connector 3, and the first metal layer 21 is located above it.
[0051] For example, the second metal layer 22 and the connector 3 are made of the same metal material to improve the welding compatibility between the materials and reduce the thermal stress concentration caused by the difference in thermal expansion coefficients between dissimilar metals. The first metal layer 21 is made of a different metal material than the second metal layer 22, and the two metal layers respectively serve the functions of conducting electricity and structural reinforcement.
[0052] For example, aluminum can be used as the first metal layer 21 and copper as the second metal layer 22. Aluminum has good thermal conductivity and is lightweight, which can be used to disperse heat in the welding area and prevent heat concentration from causing structural deformation; the copper layer has high electrical conductivity to ensure efficient current transmission. Through the composite electrode structure 2 of copper and aluminum, a balance is achieved between electrical performance, thermal conductivity and quality control.
[0053] In some implementations, combined with Figure 2 , Figure 3 A welding groove 211 is provided on the first metal layer 21. The welding groove 211 extends along the thickness direction of the pole post 2. The bottom of the welding groove 211 is the initial welding position for laser penetration welding. The molten pool 4 extends from the initial welding position to the interface between the second metal layer 22 and the connector 3.
[0054] It is understood that, in the specific manufacturing process, a welding groove 211 is formed on the first metal layer 21. The welding groove 211 extends through the electrode post 2 along its thickness direction, and the bottom surface of the welding groove 211 is the initial welding position for laser welding. It is understood that the bottom of the welding groove 211, as the initial welding position for laser penetration welding, can concentrate laser energy, form a stable melting point, and laser weld from top to bottom from the electrode post 2 to the connector 3. During laser penetration welding, the laser beam first generates a high-energy-density region at the bottom of the welding groove 211, where local metal rapidly melts to form an initial molten pool. This initial molten pool extends further downwards along its thickness direction, penetrating the first metal layer 21 and gradually expanding to the interface between the second metal layer 22 and the connector 3, forming an integral molten pool portion 4.
[0055] In some implementations, such as Figure 2 , Figure 3 and Figure 4 As shown, the molten pool portion 4 includes a first molten pool sub-portion 41, which extends from the initial welding position into the second metal layer 22 along the thickness direction of the pole post 2.
[0056] Furthermore, the molten pool section 4 also includes a second molten pool subsection 42, which is connected to the first molten pool subsection 41. Along the thickness direction of the pole post 2, the second molten pool subsection 42 extends from the first metal layer 21 to the interface between the second metal layer 22 and the pole post 2.
[0057] It can be understood that the molten pool section 4 includes two substructures: a first molten pool subsection 41 and a second molten pool subsection 42. The first molten pool subsection 41 is formed within the first metal layer 21 and is the main area affected by laser energy. The second molten pool subsection 42 is distributed at the junction of the second metal layer 22 and the connector 3. After welding, cross-sectional observation using a revealing agent shows that the welding interface between the electrode post 2 and the connector 3 changes from the original two-layer metal structure to a four-layer composite structure, including the first metal layer 21, the second metal layer 22, and the first molten pool subsection 41 and the second molten pool subsection 42 formed during the welding process. The two molten pool subsections are metal compound layers formed after laser welding, and the compound components are products of the diffusion and mixing of the original materials at high temperatures.
[0058] For example, the distribution patterns of the first molten pool sub-section 41 and the second molten pool sub-section 42 exhibit a clear interface layer relationship. The second molten pool sub-section 42 supports and covers the first molten pool sub-section 41, forming an overall composite layer structure. The second molten pool sub-section 42 is distributed in both the upper and lower layers of the copper-aluminum bonding line, and its structural shape is crescent-shaped in cross-section. The crescent-shaped molten pool structure is conducive to forming a flexible thermal stress transition zone, releasing some shrinkage stress during cooling and solidification, and reducing the concentration of residual stress inside the weld.
[0059] For example, along the direction from the first metal layer 21 to the second metal layer 22, the cross-sectional width of the first molten pool sub-section 41 gradually decreases. This gradual cross-section helps control the flow and solidification rate of the molten metal, resulting in a more uniform heat distribution in the weld transition zone. The trend of the weld shape narrowing from wide to narrow effectively disperses the stress gradient in the heat-affected zone, making it less likely for stress concentration points to form in the weld under stress. Furthermore, a metallurgical bonding layer is formed at the interface where the first molten pool sub-section 41 and the second molten pool sub-section 42 contact each other. This bonding layer is composed of a solid solution formed by intermetallic diffusion and has high electrical conductivity and shear strength.
[0060] In some implementations, refer to Figure 3 , Figure 4 The second molten pool sub-part 42 has a protrusion 421, which is located inside the first metal layer 21 and protrudes in a direction away from the second metal layer 22. The first molten pool sub-part 41 has a groove 411, and the protrusion 421 is embedded in the groove 411.
[0061] It is worth noting that, from Figure 4 As can be seen directly, the first molten pool sub-section 41 is divided into two regions with different curvatures by the groove 411.
[0062] It is understood that the second molten pool sub-section 42 forms an upward protrusion 421, and the first molten pool sub-section 41 correspondingly forms a groove 411, with the two interlocking spatially. This convex-concave interlocking structure achieves mechanical interlocking through morphological constraints during welding cooling, giving the welded joint higher shear strength and vibration resistance. The protrusion 421 extends in a direction away from the second metal layer 22, making the overall stress transmission path of the weld smoother and helping to improve the fatigue life of the overall welded structure.
[0063] In some implementations, combined Figure 3 , Figure 4 Regarding the design of the electrode post 2, the minimum thickness of the first metal layer 21 in the thickness direction is set to 'a', ranging from 0 mm to 1 mm, and the minimum thickness of the second metal layer 22 in the thickness direction is set to 'b', ranging from 0.5a to 2a. This thickness ratio ensures the structural strength of the electrode post 2 while allowing the laser energy to gradually attenuate to a reasonable range during the penetration path, thus preventing excessive energy from penetrating the main body of the connector 3. When the first metal layer 21 is relatively thin, the laser energy can be effectively concentrated in the welding area; when the second metal layer 22 is of moderate thickness, the welding heat is evenly distributed, forming a stable metallurgical bonding zone.
[0064] In some implementations, combined Figure 1 , Figure 2 and Figure 7The battery also includes a cover plate 5 and a fixing component 6. The cover plate 5 has a through hole 53, the fixing component 6 is installed in the mounting hole 53, and the terminal post 2 is also embedded in the mounting hole 53 to achieve mechanical fixation and electrical connection.
[0065] For example, the fixing component 6 is generally made of a highly conductive metal, such as copper or nickel-plated copper, and the cover plate 5 can be an aluminum-plastic composite structure. Through the embedded installation method, the pole post 2 and the fixing component 6 form a tight fit, making the contact interface flat and the conductive path short, reducing contact resistance, which is beneficial to the energy output stability during high-rate discharge.
[0066] For example, in the mating relationship between the welded structure and the fixing component 6, in the thickness direction of the pole post 2, the projected area of the welded region formed by laser penetration welding on the pole post 2 is S1, and the projected area of the fixing component 6 is S2. The ratio of the projected area S1 of the laser penetration welding to the projected area S2 of the fixing component 6 is limited to between 1 / 3S2 and 4 / 5S2. This ratio control achieves a balance between welding strength and heat distribution. If the welded area is too small, the connection strength is insufficient; if the area is too large, it may cause the heat-affected zone of the fixing component 6 to expand. By limiting the ratio, the welding energy is evenly distributed within the load-bearing range of the fixing component 6, which is beneficial for the fixing component 6 to maintain consistent deformation during heating and cooling, and prevents interface warping.
[0067] It is worth noting that the fixing component 6 is a combination structure of multiple parts. However, among the multiple parts, the upper plastic 62 has the largest projected area in the thickness direction of the pole post 2. The projected areas of the other parts in the fixing component 6 are all located within the projected area of the upper plastic 62. Therefore, the projected area S2 of the fixing component 6 in the thickness direction of the pole post 2 is actually the projected area of the upper plastic 62 in the thickness direction of the pole post 2.
[0068] For example, the welding area formed by laser penetration welding on the electrode post 2 is annular in shape. The annular welding area is distributed along the thickness direction of the electrode post 2 and arranged around the central axis of the electrode post 2. Further, during welding, the laser beam is focused and penetrates the electrode post 2 within the welding area, so that the energy acts uniformly within the annular welding area, thereby forming a continuous closed molten pool 4 within the electrode post 2 up to the interface between the electrode post 2 and the connector 3. This molten pool 4 extends from the interior of the electrode post 2 along the thickness direction to the interface of the connector 3. The annular distribution of the welding area is beneficial to forming a stable symmetrical stress structure, reducing local thermal stress concentration, and promoting uniform fusion between metals. This structure is beneficial to improving the metallurgical bonding quality, reducing contact resistance, enhancing the fatigue strength and conductivity stability of the weld joint, thereby improving the overall reliability and service life of the battery.
[0069] In some embodiments, the cover plate 5 includes a light aluminum sheet 51 and a lower plastic sheet 52, the lower plastic sheet 52 being connected to the side of the light aluminum sheet 51 near the connector 3.
[0070] It is understood that the cover plate 5 is composed of a composite of a light aluminum sheet 51 and a lower plastic layer 52. The light aluminum sheet 51 is located on the outer side, providing excellent heat dissipation and mechanical rigidity. The lower plastic layer 52 is located on the side of the light aluminum sheet 51 closest to the connector 3, providing electrical insulation and cushioning. The bonding of the light aluminum sheet 51 and the lower plastic layer 52 can be achieved through an injection molding process, enabling the cover plate 5 to simultaneously provide protection, thermal conductivity, and sealing functions. The surface of the light aluminum sheet 51 is anodized to improve its corrosion resistance.
[0071] In some implementations, combined Figure 1 , Figure 2 and Figure 7 The battery also includes a welding block 61, an upper plastic 62, and a sealing ring 64. The sealing ring 64 is fitted between the outer peripheral wall of the terminal post 2 and the mounting hole 53. The aluminum sheet 51 has a mounting groove 511 on the outer periphery of the mounting hole 53. The upper plastic 62 is embedded in the mounting groove 511. The surface of the upper plastic 62 facing away from the mounting groove 511 has a crimping groove 63. The welding block 61 is embedded in the crimping groove 63.
[0072] To enhance the sealing performance and assembly stability between the battery cell 1 and the fixing assembly 6, an installation groove 511 is formed on the outer periphery of the cover plate 5, and an upper plastic structure 62 is embedded in the groove 411. A crimping groove 63 is formed on the side of the upper plastic 62 opposite to the installation groove 511, and a welding pressure block 61 is embedded in the crimping groove 63. A sealing ring 64 is installed between the outer peripheral wall of the terminal post 2 and the mounting hole 53. The sealing ring 64 is made of high-temperature resistant fluororubber, which can maintain its sealing performance during high-temperature welding and subsequent operation. The welding pressure block 61 applies a uniform clamping force to the upper plastic 62, causing the sealing ring 64 to form a radially compressed state, thereby preventing external moisture or electrolyte from penetrating into the welding interface and improving the battery's airtightness.
[0073] In some implementations, combined Figure 1 , Figure 2 and Figure 7 The battery also includes an explosion-proof valve 7 and an explosion-proof film 71. An explosion-proof hole is formed on the aluminum sheet 51, and the explosion-proof valve 7 is installed in the hole. The explosion-proof film 71 is attached to the outside. When the gas inside the cell 1 expands, causing the pressure to rise, the explosion-proof valve 7 opens at a specific pressure value, allowing the gas to escape through the explosion-proof hole. After activation, the explosion-proof film 71 maintains its protective layer state, preventing external particles or sparks from entering the internal space. This structure helps prevent the risk of the cell 1's casing rupture due to overcharging, short circuits, or other abnormalities, improving the battery's safety.
[0074] In some implementations, combined Figure 1 , Figure 7 and Figure 8 The battery also includes a casing 8, battery cells 1, an separator 9, and a support frame 10. The battery cells 1 are installed inside the casing 8. The separator 9 is located between the cover plate 5 and the connector 3, and is connected to the support frame 10. The separator 9 has perforations for the connector 3 to pass through and overlap with the terminal post 2. The separator 9 is made of heat-resistant insulating composite material to prevent direct contact between metal parts. The support frame 10 can be a high-strength engineering plastic or metal skeleton structure, capable of maintaining the stability of the battery cell arrangement under vibration. This multi-layer assembly structure gives the battery cell module high vibration resistance and thermal stability during assembly and operation.
[0075] It is understandable that after the laser penetration welding of cell 1 is completed, microscopic observation can be performed after preparing a cross-section and etching with metallographic reagents. This allows us to observe that the welding interface changes from the original two-layer metal structure to a four-layer composite structure. The newly added first molten pool sub-section 41 and second molten pool sub-section 42 exhibit different grayscale distributions at the microscopic level. The first molten pool sub-section 41 is located in the upper region, fusing with the first metal layer 21 to form a continuous transition zone. The second molten pool sub-section 42 surrounds it and extends to the surface of the connector 3. The boundary region between the two molten pool sub-sections exhibits a transition diffusion morphology, indicating that the two metals underwent mutual dissolution and resolidification under high-temperature welding. After welding, the laser energy attenuates after reaching the surface of the connector 3 and no longer propagates downwards, thus maintaining the integrity of the main structure of the connector 3.
[0076] Through the above structural design, laser penetration welding can not only complete the copper-aluminum composite connection in a very short time, but also form a dense and continuous metallurgical bonding layer between the metals. The weld cross-section is smooth, with few pores and gas pores, and the weld interface has a multi-layer structure, resulting in a short and continuous current conduction path. Hardness testing of the weld metal shows that the microhardness of the weld area is between that of the first metal layer 21 and the second metal layer 22, indicating the formation of a stable intermetallic chemical layer, which is beneficial to improving the uniformity of electrical conductivity.
[0077] Furthermore, the battery uses laser penetration welding to firmly bond the terminal post 2 to the connector 3, which helps improve the overall module's vibration stability and cycle reliability. Laser welding has low heat input and high welding speed, resulting in a narrower heat-affected zone around the weld joint, reducing material coarsening and extending the cycle life of the cell 1.
[0078] After the entire package is assembled, the connection area between the terminal post 2 and the fixing component 6 forms a closed conductive channel. The fixing component 6 is connected to the external circuit via threaded crimping or quick-connect structure. The cover plate 5, the housing 8, and the sealing component form a multi-layer sealing system, isolating the internal environment of the battery from external gases and preventing moisture infiltration that could cause corrosion. The explosion-proof structure has a directional pressure relief function under abnormal operating conditions, ensuring that the battery maintains its structural integrity under high pressure.
[0079] For example, this battery can be integrated into various electrical devices, including electric vehicles, energy storage stations, power tools, and drone systems. Because the electrode post 2 uses laser-through welding, the weld has high conductivity and strong connection strength, maintaining stable electrical performance under high-rate charging and discharging or frequent vibration environments. The overall lightweight design contributes to improved energy density and range.
[0080] In summary, through multiple design methods, including metal layering of the electrode post 2, guidance of the welding groove 211, layering of the molten pool, and structural optimization of the fixing component 6, the welding connection structure of the battery cell 1 has been significantly improved in terms of energy conduction, stress distribution, and thermal management. The laser penetration welding process, while forming a weld with a large depth-to-width ratio, suppresses excessive heat transfer to the main body of the connector 3, enabling the connector 3 to form a dense metallurgical bonding layer on its surface while maintaining structural integrity, resulting in high reliability and engineering applicability.
[0081] Secondly, see Figures 1 to 8 This application also provides a battery pack, including the battery of the first aspect.
[0082] In the description of this application, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more features. In the description of this application, "multiple" means two or more, unless otherwise explicitly specified.
[0083] In the above embodiments, the descriptions of each embodiment have different focuses. For parts not described in detail in a certain embodiment, please refer to the relevant descriptions of other embodiments.
[0084] The embodiments, implementation methods, and related technical features of this application can be combined and substituted for each other without conflict.
[0085] The above are merely preferred embodiments of this application and are not intended to limit this application in any way. Any simple modifications, equivalent changes, and alterations made to the above embodiments based on the technical essence of this application without departing from the scope of the technical solution of this application shall still fall within the scope of the technical solution of this application.
Claims
1. A battery, characterized by, The device includes a battery cell (1), a terminal post (2), and a connector (3). The connector (3) is disposed on the battery cell (1). The terminal post (2) is connected to the connector (3) on the side away from the battery cell (1), and the terminal post (2) and the connector (3) are connected by laser welding. The electrode post (2) and the connector (3) form a molten pool (4) under the action of laser welding. Along the thickness direction of the electrode post (2), the molten pool (4) extends from the side of the electrode post (2) away from the connector (3) to the interface between the electrode post (2) and the connector (3).
2. The battery of claim 1, wherein, The connector (3) includes a tab (31), which is connected between the battery cell (1) and the terminal post (2). The molten pool portion (4) extends from the side of the terminal post (2) away from the tab (31) to the interface between the terminal post (2) and the tab (31). Alternatively, the connector (3) includes a tab (31) and a connecting piece (32), the tab (31) is connected to the battery cell (1), the first side of the connecting piece (32) is connected to the tab (31), the second side of the connecting piece (32) is connected to the pole post (2), and the molten pool portion (4) extends from the side of the pole post (2) away from the connecting piece (32) to the interface between the pole post (2) and the connecting piece (32).
3. The battery of claim 1, wherein, The pole post (2) includes a first metal layer (21) and a second metal layer (22). The second metal layer (22) is connected to the connector (3), and the first metal layer (21) is connected to the side of the second metal layer (22) away from the connector (3).
4. The battery of claim 3, wherein, The second metal layer (22) and the connector (3) are made of the same metal material, while the second metal layer (22) and the first metal layer (21) are made of different metal materials.
5. The battery of claim 3, wherein, The first metal layer (21) is made of aluminum; and / or the second metal layer (22) is made of copper.
6. The battery of claim 3, wherein, A welding groove (211) is provided on the first metal layer (21). The welding groove (211) extends along the thickness direction of the pole post (2). The bottom surface of the welding groove (211) is the initial welding position of the laser welding. The molten pool (4) extends from the bottom surface of the welding groove (211) into the second metal layer (22).
7. The battery of claim 6, wherein, The molten pool portion (4) includes a first molten pool sub-portion (41), which extends from the initial welding position into the second metal layer (22) along the thickness direction of the pole post (2). The molten pool section (4) further includes a second molten pool subsection (42), which is connected to the first molten pool subsection (41). Along the thickness direction of the pole post (2), the second molten pool subsection (42) extends from the first metal layer (21) to the interface between the second metal layer (22) and the pole post (2).
8. The battery of claim 7, wherein, Along the direction from the first metal layer (21) to the second metal layer (22), the cross-sectional width of the first molten pool sub-section (41) gradually decreases.
9. The battery of claim 7, wherein, The cross-sectional shape of the second molten pool sub-section (42) is crescent-shaped.
10. The battery of claim 7, wherein, The second molten pool sub-part (42) has a protrusion (421) located within the first metal layer (21) and protruding in a direction away from the second metal layer (22). The first molten pool sub-part (41) has a groove (411) in which the protrusion (421) is embedded.
11. The battery of any one of claims 3 to 10, wherein, The minimum thickness of the first metal layer (21) in the thickness direction of the pole post (2) is a, where 0 mm < a ≤ 1 mm; And / or, the minimum thickness of the second metal layer (22) in the thickness direction of the pole post (2) is b, 0.5a < b ≤ 2a.
12. The battery according to any one of claims 1 to 10, characterized in that, The battery also includes a cover plate (5) and a fixing component (6). The cover plate (5) has a through hole (53), and the fixing component (6) and the terminal post (2) are both embedded in the mounting hole (53).
13. The battery of claim 12, wherein, In the thickness direction of the pole post (2), the projected area of the welding area formed by the laser welding on the pole post (2) is S1, and the projected area of the fixing component (6) is S2, 1 / 3S2≤S1≤4 / 5S2.
14. The battery of claim 12, wherein, The cover plate (5) includes a light aluminum sheet (51) and a lower plastic sheet (52), wherein the lower plastic sheet (52) is connected to the side of the light aluminum sheet (51) near the connector (3); The fixing component (6) includes a welding pressure block (61), an upper plastic (62), and a sealing ring (64). The sealing ring (64) is fitted between the outer peripheral wall of the pole post (2) and the mounting hole (53). The aluminum sheet (51) has a mounting groove (511) on the outer periphery of the mounting hole (53). The upper plastic (62) is embedded in the mounting groove (511). The surface of the upper plastic (62) facing away from the mounting groove (511) has a crimping groove (63). The welding pressure block (61) is embedded in the crimping groove (63).
15. The battery of claim 14, wherein, The battery also includes an explosion-proof valve (7) and an explosion-proof film (71). An explosion-proof hole is provided on the aluminum sheet (51). The explosion-proof valve (7) is installed in the explosion-proof hole. The explosion-proof film (71) is attached to the side of the explosion-proof valve (7) away from the lower plastic (52).
16. The battery of claim 12, wherein, The battery also includes a housing (8), an isolation plate (9), and a support frame (10). The battery cell (1) is installed inside the housing (8). The isolation plate (9) is installed between the cover plate (5) and the connector (3). The isolation plate (9) is connected to the support frame (10) and allows part of the connector (3) to pass through and overlap.