Welded structure, top cover assembly, individual battery cells and battery pack
By designing a welding structure in battery assembly to reduce the cross-sectional width of the molten pool along the direction from the electrode post to the welded part, and using laser welding to connect the electrode post, connecting piece and electrode tab, the problem of battery short circuit caused by metal spatter contacting the core pack is solved, simplifying the production process and reducing costs.
Patent Information
- Application Number
- CN202522380797.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-07
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-11-07
AI Technical Summary
During battery assembly, metal spatter generated when welding the connecting pieces to the tabs can easily come into contact with the battery pack, causing a short circuit. Furthermore, existing technologies require the connecting pieces to be sanded, which increases production costs and complexity.
Design a welding structure in which the molten pool of the pole and the weldment has a decreasing cross-sectional width along the direction from the pole to the weldment, the welding position is set away from the core package, and the pole, the connecting piece and the electrode lug are connected by laser welding to avoid metal spatter contacting the core package and to simplify the production process of the connecting piece.
It effectively prevents short circuits in the battery caused by metal spatter contacting the core pack during welding, simplifies the production process of the connecting piece, reduces production costs, and improves the reliability and efficiency of welding.
Smart Images

Figure CN224986580U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of battery technology, specifically to a welding structure, a top cover assembly, a single battery cell, and a battery pack. Background Technology
[0002] In related technologies, during the assembly process of batteries using connecting tabs, the connecting tabs are first welded to the electrode tabs, and then the connecting tabs are welded to the terminals from the side of the connecting tabs closest to the cell pack. Before welding, the connecting tabs need to be sanded. At the same time, metal spatter is easily generated during the welding process, and if the metal spatter comes into contact with the cell pack, it may cause a short circuit in the battery. Utility Model Content
[0003] The embodiments of this utility model provide a welding structure, a top cover assembly, a single cell, and a battery pack, which can prevent metal spatter contaminants from contacting the cell pack during the welding process and causing a short circuit in the battery, thereby at least partially solving the above-mentioned technical problems.
[0004] In a first aspect, embodiments of the present invention provide a welding structure, comprising: pole; The welded component is welded to the pole post and forms a molten pool inside both, and the molten pool has a decreasing cross-sectional width along the direction from the pole post to the welded component.
[0005] This prevents metal spatter from welding from coming into contact with the battery pack and causing a short circuit.
[0006] In one embodiment, the welded component includes a first weld layer and a second weld layer, the pole post, the first weld layer and the second weld layer are stacked sequentially, and the first weld layer is welded to the second weld layer and the first weld layer is welded to the pole post, wherein one of the first weld layer and the second weld layer is a tab and the other is a connecting piece.
[0007] Therefore, there is no need to perform sanding pretreatment on the connecting pieces, which simplifies the production process and reduces the production cost of the connecting pieces.
[0008] In one embodiment, the first welding layer is ultrasonically welded to the second welding layer, and the first welding layer is laser-welded to the electrode.
[0009] This ensures reliable welding between the first and second welding layers, as well as reliable welding between the first welding layer and the pole.
[0010] In one embodiment, the end of the molten pool away from the pole extends into the first weld layer, or the end of the molten pool away from the pole extends into the second weld layer.
[0011] This ensures a reliable connection between the pole, connecting piece, and pole tab.
[0012] In one embodiment, the pole includes a first metal layer and a second metal layer, the second metal layer being located between the first metal layer and the first welding layer, wherein the first metal layer and the second metal layer have different melting points.
[0013] This allows the formation of metallic compounds after welding, increasing hardness and tensile strength.
[0014] In one embodiment, the melting point of the first metal layer is lower than that of the second metal layer, and / or the melting point of the second metal layer is the same as that of the first weld layer.
[0015] Therefore, the laser needs to penetrate metal layers with different melting points in the first and second metal layers, but the laser does not need to penetrate metal layers with different melting points in the second metal layer and the first weld.
[0016] In one embodiment, the molten pool includes a first molten pool portion, a second molten pool portion, and a third molten pool portion connected in sequence. The first molten pool portion is located within the first metal layer, the second molten pool portion is located within the second metal layer, one end of the third molten pool portion is located within the second metal layer and covers the second metal layer, and the other end extends into the first welding layer or into the second welding layer.
[0017] This ensures that the molten pool can reliably connect the pole, lug, and connecting piece, guaranteeing welding quality and connection strength.
[0018] In one embodiment, the longitudinal section of the first molten pool portion is square, and / or the longitudinal section of the second molten pool portion is inverted conical, and / or the longitudinal section of the third molten pool portion is inverted conical.
[0019] This ensures welding quality and connection strength.
[0020] In one embodiment, the first welding layer has an ultrasonic welding area for ultrasonic welding with the second welding layer and a laser welding area for laser welding with the electrode, wherein the projection of the ultrasonic welding area and the projection of the laser welding area at least partially overlap along the direction from the electrode to the welded part.
[0021] This can improve connection strength and welding effect, and shorten the current path.
[0022] In one embodiment, a groove is formed at the end of the pole away from the weldment, and the bottom surface of the groove serves as the welding surface, which is the working surface of the welding equipment.
[0023] This allows for a reduction in the thickness of the electrode laser welding area, a decrease in laser power, and enables the welding equipment to quickly and accurately identify the welding surface, thereby improving welding efficiency and precision.
[0024] In one embodiment, the distance from the bottom surface of the groove to the welded part is b, and the height of the pole post is h, satisfying: 5%≤b / h≤40%.
[0025] This ensures that the groove can be formed and that the laser can pass through the pole.
[0026] In one embodiment, the welded component includes a connecting piece and a tab, the connecting piece being located between the pole post and the tab, wherein the distance from the bottom surface of the groove to the welded component is b, and the thickness of the connecting piece is c, satisfying: 0 < b / c ≤ 1 / 3.
[0027] This ensures that the connecting piece can be stably melted through, thereby ensuring the connection strength and welding effect of the laser welding of the pole, connecting piece and tab.
[0028] In one embodiment, along the direction from the pole post to the weldment, the sidewall of the groove is inclined in a direction away from the axis of the pole post, wherein the inclination angle of the sidewall of the groove is θ, satisfying: 5°≤θ≤60°.
[0029] This facilitates the demolding of the pole.
[0030] Secondly, embodiments of the present invention provide a top cover assembly, including the welding structure as described above.
[0031] This prevents metal spatter from welding from coming into contact with the battery pack and causing a short circuit.
[0032] Thirdly, embodiments of this utility model provide a single battery cell, including the top cover assembly as described above.
[0033] This prevents metal spatter from welding from coming into contact with the battery pack and causing a short circuit.
[0034] Fourthly, embodiments of the present invention provide a battery pack, including the single battery cell as described above.
[0035] This prevents metal spatter from welding from coming into contact with the battery pack and causing a short circuit.
[0036] The beneficial effects of the embodiments of this utility model are as follows: In embodiments of this invention, the electrode and the weldment are welded on the side of the electrode away from the weldment to form a molten pool inside the electrode and the weldment. This molten pool exhibits a decreasing cross-sectional width along the direction from the electrode to the weldment. Because welding is performed on the side of the electrode away from the weldment, the weld surface is located away from the cell pack and outside the cell. This prevents metal spatter generated during welding from contacting the cell pack and causing a short circuit in the battery. Attached Figure Description
[0037] To more clearly illustrate the technical solutions in the embodiments of this utility model, the drawings used in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this utility model. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0038] Figure 1 This is a schematic diagram of the structure of a single battery cell provided in an embodiment of this utility model; Figure 2 This is an exploded view of a single battery cell provided in an embodiment of this utility model; Figure 3 This is a cross-sectional view of a single battery cell at the positive electrode position provided in an embodiment of this utility model; Figure 4 This is a partial cross-sectional view of a molten pool structure at the positive electrode position of a single battery cell provided in an embodiment of this utility model; Figure 5 This is a partial cross-sectional view of another molten pool structure at the positive electrode position of a single battery cell provided in an embodiment of this utility model; Figure 6 This is a partial cross-sectional view of a single battery cell at the positive electrode position provided in an embodiment of this utility model; Figure 7 This is a cross-sectional view of a single battery cell at the negative terminal position provided in an embodiment of this utility model; Figure 8 This is a partial cross-sectional view of a molten pool structure at the negative electrode position of a single battery cell provided in an embodiment of this utility model; Figure 9 This is a partial cross-sectional view of another molten pool structure at the negative electrode position of a single battery cell provided in an embodiment of this utility model; Figure 10 This is a partial cross-sectional view of a single battery cell at the negative terminal position provided in an embodiment of this utility model; Figure 11 This is another cross-sectional view of a single battery cell provided in an embodiment of this utility model; Figure 12This is a schematic diagram of the welding process provided in an embodiment of this utility model.
[0039] Explanation of reference numerals in the attached figures: 1. Pole post; 11. First metal layer; 12. Second metal layer; 13. Groove; 2. Welded component; 21. First weld layer; 22. Second weld layer; 3. Molten pool; 31. First molten pool section; 32. Second molten pool section; 33. Third molten pool section; 4. Polar ears; 5. Connecting piece; 6. Individual battery cell. Detailed Implementation
[0040] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present utility model. In addition, it should be understood that the specific embodiments described herein are only for illustration and explanation of the present utility model and are not intended to limit the present utility model. In the present utility model, unless otherwise stated, directional terms such as "upper" and "lower" generally refer to the upper and lower positions of the device in actual use or operation, specifically the drawing directions in the accompanying drawings; while "inner" and "outer" refer to the outline of the device.
[0041] This application provides a battery pack. The battery pack includes a battery case and battery modules disposed within the battery case. The battery modules include multiple individual battery cells 6. The battery case provides a space for accommodating the individual battery cells 6, and the battery case can adopt various structures. In some embodiments, the battery case includes a casing and a cover that overlap each other. The casing and the cover together define an accommodating space for accommodating the individual battery cells 6. The casing can be a hollow structure, and the cover can be a plate-like structure, with the cover covering the opening side of the casing so that the cover and casing together define the accommodating space. Both the casing and the cover can be hollow structures with an opening on one side, with the opening of the cover covering the opening side of the casing. Of course, the battery case formed by the cover and casing can be of various shapes, such as a cylinder, a cuboid, etc.
[0042] In a battery pack, multiple individual battery cells 6 can be configured. These cells can be connected in series, parallel, or in a hybrid configuration. A hybrid configuration means that multiple individual battery cells 6 are connected in both series and parallel connections. Multiple individual battery cells 6 can be directly connected in series, parallel, or in a hybrid configuration, and then the entire assembly of these cells 6 is housed within a battery box. Alternatively, the battery pack can consist of multiple individual battery cells 6 first connected in series, parallel, or in a hybrid configuration to form battery modules, and then these battery modules are connected in series, parallel, or in a hybrid configuration to form a whole, which is then housed within a battery box. The battery pack may also include other structures; for example, it may include a busbar component for electrical connection between the multiple individual battery cells 6.
[0043] Each individual cell 6 can be a secondary battery or a primary battery; it can also be a lithium-sulfur battery, a sodium-ion battery, or a magnesium-ion battery, but is not limited to these. The individual cell 6 can be cylindrical, flat, cuboid, or other shapes.
[0044] like Figure 1 and Figure 2 As shown in the illustration, this application also provides a single battery cell 6. The single battery cell 6 includes a housing, a top cover assembly, and electrode assemblies and other functional components located within the housing.
[0045] This application also provides a top cover assembly. The top cover assembly includes a pole post 1, a connecting piece 5, and a tab 4. The connecting piece 5 is located between the pole post 1 and the tab 4, and the connecting piece 5 and the tab 4 are ultrasonically welded, while the pole post 1 and the connecting piece 5 are laser-through welded. Alternatively, the tab 4 is located between the pole post 1 and the connecting piece 5, and the connecting piece 5 and the tab 4 are ultrasonically welded, while the pole post 1 and the tab 4 are laser-through welded.
[0046] like Figures 3 to 11 As shown in the figure, this application embodiment also provides a welding structure. The welding structure includes a pole post 1 and a weldment 2. The weldment 2 is welded to the pole post 1 and a molten pool 3 is formed inside both. Along the direction from the pole post 1 to the weldment 2, the molten pool 3 has a decreasing cross-sectional width.
[0047] In this embodiment, the electrode post 1 and the weldment 2 are welded on the side of the electrode post 1 away from the weldment 2 to form a molten pool 3 inside the electrode post 1 and the weldment 2. The molten pool 3 has a decreasing cross-sectional width along the direction from the electrode post 1 to the weldment 2. Since the welding is performed on the side of the electrode post 1 away from the weldment 2, the welding surface is located away from the cell pack and outside the cell. This prevents metal spatter generated during welding from contacting the cell pack and causing a short circuit in the battery.
[0048] Understandably, since the cross-sectional width of the molten pool 3 decreases along the direction from the electrode post 1 to the weldment 2, welding is performed on the side of the electrode post 1 furthest from the weldment 2. That is, the side of the electrode post 1 furthest from the weldment 2 serves as the welding surface, which is also the working surface of the welding equipment. The welding equipment welds the electrode post 1 and the weldment 2 from this welding surface, and the welding method includes laser welding. During the laser welding process of the electrode post 1 and the weldment 2, a molten pool 3 can be formed inside both. The molten pool 3 gradually extends from the welding surface into the interior of both, eventually reaching the weldment 2, thus achieving laser penetration welding between the electrode post 1 and the weldment 2.
[0049] During the laser welding process of electrode 1 and weldment 2, since laser welding is performed from the side of electrode 1 away from weldment 2, as the laser loses energy and the effective power density decreases during the penetration process, the molten pool 3 can have a decreasing cross-sectional width along the direction from electrode 1 to weldment 2.
[0050] It should be noted that the cross-sectional width of the molten pool 3 can decrease linearly or exponentially along the direction from the pole post 1 to the weldment 2. For example, the molten pool 3 can be set in the shape of a teardrop or an inverted cone. Of course, the cross-sectional width of the molten pool 3 can also remain unchanged initially along the direction from the pole post 1 to the weldment 2, and then decrease linearly.
[0051] like Figure 3 , Figure 7 and Figure 11 As shown, in some embodiments, the welded component 2 includes a first weld layer 21 and a second weld layer 22. The pole post 1, the first weld layer 21 and the second weld layer 22 are stacked in sequence, and the first weld layer 21 is welded to the second weld layer 22 and the first weld layer 21 is welded to the pole post 1. In this case, one of the first weld layer 21 and the second weld layer 22 is a tab 4 and the other is a connecting piece 5.
[0052] Understandably, after the tab 4 and connecting piece 5 are welded, all three are welded together on the welding surface of the pole 1. Since the welding position is far from the connecting piece 5, there is no need to perform a sanding pretreatment on the connecting piece 5. Therefore, the connecting piece 5 can be directly stamped without sanding pretreatment, which simplifies the production process of the connecting piece 5 and reduces its production cost.
[0053] When the first welding layer 21 is the connecting piece 5 and the second welding layer 22 is the tab 4, the connecting piece 5 is located between the terminal post 1 and the tab 4. The tab 4, the connecting piece 5 and the terminal post 1 are directly connected, which can reduce the battery impedance and meet the requirements of high current overcurrent.
[0054] When the first welding layer 21 is the tab 4 and the second welding layer 22 is the connecting piece 5, the connecting piece 5 is located on the side of the tab 4 away from the pole post 1. At this time, the connecting piece 5 can act as an auxiliary welding piece, which can increase the strength during ultrasonic welding and prevent the tab 4 from deforming.
[0055] In some embodiments, the first welding layer 21 and the second welding layer 22 are ultrasonically welded, and the first welding layer 21 is laser welded to the electrode 1.
[0056] Understandably, after the tab 4 and connecting piece 5 are ultrasonically welded, the three are then laser-welded onto the welding surface of the pole 1. Since the welding position is far from the connecting piece 5, there is no need to perform a sanding pretreatment on the connecting piece 5. Therefore, the connecting piece 5 can be directly stamped without sanding pretreatment, which simplifies the production process of the connecting piece 5 and reduces its production cost.
[0057] In some embodiments, the end of the molten pool 3 away from the pole post 1 extends into the first weld layer 21, or the end of the molten pool 3 away from the pole post 1 extends into the second weld layer 22.
[0058] It is understandable that the molten pool 3 extends inward from the welding surface, which can extend into the first welding layer 21 or the second welding layer 22, so that the pole post 1, the connecting piece 5 and the pole lug 4 can form a reliable connection.
[0059] like Figure 4 As shown, electrode post 1 is the positive electrode post 1, the first welding layer 21 is the connecting piece 5, and the second welding layer 22 is the electrode tab 4. The molten pool 3 extends from the welding surface of the positive electrode post 1 into the connecting piece 5. For example, the molten pool 3 extends from the welding surface of the positive electrode post 1 to the junction of the connecting piece 5 and the electrode tab 4. At this time, although the molten pool 3 does not show a macroscopic connection with the electrode tab 4, it has a bonding force at the microscopic level, which enables the electrode tab 4 to form a bonding force with the electrode post 1 and the connecting piece 5 under the action of laser penetration welding, ensuring reliable welding of the three.
[0060] like Figure 5 As shown, electrode post 1 is the positive electrode post 1, the first welding layer 21 is the connecting piece 5, and the second welding layer 22 is the electrode tab 4. The molten pool 3 extends from the welding surface of the positive electrode post 1 into the electrode tab 4. For example, the molten pool 3 extends from the welding surface of the positive electrode post 1 to the middle position of the electrode tab 4 in the height direction. In this case, the molten pool 3 directly and reliably welds the positive electrode post 1, the connecting piece 5, and the electrode tab 4 at the macroscopic level.
[0061] It should be noted that the connection strength of the molten pool 3 extending from the welding surface of the positive electrode post 1 to the junction of the connecting piece 5 and the tab 4 is greater than the connection strength of the molten pool 3 extending from the welding surface of the positive electrode post 1 to the middle position of the tab 4 in the height direction.
[0062] like Figure 8 As shown, electrode post 1 is the negative electrode post 1, the first welding layer 21 is the connecting piece 5, and the second welding layer 22 is the electrode tab 4. The molten pool 3 extends from the welding surface of the negative electrode post 1 into the connecting piece 5. For example, the molten pool 3 extends from the welding surface of the negative electrode post 1 to the middle of the connecting piece 5, or to the junction of the connecting piece 5 and the electrode tab 4. When the molten pool 3 extends to the junction of the connecting piece 5 and the electrode tab 4, although the molten pool 3 does not show a macroscopic connection with the electrode tab 4, it has a bonding force at the microscopic level, so that the electrode tab 4 forms a bonding force with the electrode post 1 and the connecting piece 5 under the action of laser penetration welding, ensuring reliable welding of the three.
[0063] like Figure 9 As shown, electrode post 1 is the negative electrode post 1, the first welding layer 21 is the connecting piece 5, and the second welding layer 22 is the electrode tab 4. The molten pool 3 extends from the welding surface of the negative electrode post 1 into the electrode tab 4. For example, the molten pool 3 extends from the welding surface of the negative electrode post 1 to the middle position of the electrode tab 4 in the height direction. In this case, the molten pool 3 directly and reliably welds the negative electrode post 1, the connecting piece 5, and the electrode tab 4 at the macroscopic level.
[0064] It should be noted that the connection strength of the molten pool 3 extending from the welding surface of the negative electrode post 1 to the junction of the connecting piece 5 and the tab 4 is greater than the connection strength of the molten pool 3 extending from the welding surface of the negative electrode post 1 to the middle position of the tab 4 in the height direction.
[0065] In some embodiments, the pole post 1 includes a first metal layer 11 and a second metal layer 12, the second metal layer 12 being located between the first metal layer 11 and the first welding layer 21, wherein the first metal layer 11 and the second metal layer 12 have different melting points.
[0066] When electrode 1 is the negative electrode electrode 1, it adopts a composite material of a first metal layer 11 and a second metal layer 12. The first and second metal layers 12 are located between the first metal layer 11 and the first welding layer 21. Generally, when the single cell 6 is placed vertically, the first metal layer 11 is located above the second metal layer 12. The first metal layer 11 and the second metal layer 12 have different melting points. During the laser welding process, it is necessary to penetrate the metal layers with different melting points, which can form a metal compound after welding, thereby increasing the hardness and tensile strength.
[0067] In some embodiments, the first metal layer 11 is an aluminum layer and the second metal layer 12 is a copper layer.
[0068] In some embodiments, the melting point of the first metal layer 11 is lower than the melting point of the second metal layer 12, and / or the melting point of the second metal layer 12 is the same as the melting point of the first weld layer 21.
[0069] Understandably, the melting point of the first metal layer 11 is lower than that of the second metal layer 12. During laser welding, this interface needs to penetrate metal layers with different melting points. The melting point of the second metal layer 12 is the same as that of the first welding layer 21, so this interface does not need to penetrate metal layers with different melting points during laser welding. Because the melting point of the first metal layer 11 is lower than that of the second metal layer 12, laser welding requires a higher power density to penetrate the second metal layer 12.
[0070] In some embodiments, the first metal layer 11 is made of aluminum, and the second metal layer 12 and the first weld layer 21 are both made of copper.
[0071] like Figure 8 and Figure 9 As shown, in some embodiments, the molten pool 3 includes a first molten pool portion 31, a second molten pool portion 32 and a third molten pool portion 33 connected in sequence. The first molten pool portion 31 is located in the first metal layer 11, the second molten pool portion 32 is located in the second metal layer 12, one end of the third molten pool portion 33 is located in the second metal layer 12 and covers the second metal layer 12, and the other end extends into the first welding layer 21 or into the second welding layer 22.
[0072] It is understandable that when laser welding sequentially penetrates the first metal layer 11, the second metal layer 12, the first welding layer 21, and the second welding layer 22, a first molten pool portion 31 can be formed within the first metal layer 11, a second molten pool portion 32 within the second metal layer 12, and a third molten pool portion 33 within the second metal layer 12 and the first welding layer 21, or a third molten pool portion 33 can be formed within the second metal layer 12, the first welding layer 21, and the second welding layer 22. This allows the molten pool 3 to reliably connect the electrode post 1, the electrode tab 4, and the connecting piece 5, ensuring welding quality and connection strength.
[0073] In some embodiments, the first metal layer 11 is made of aluminum, and the second metal layer 12 is made of copper. The first molten pool portion 31 is made of aluminum, the second molten pool portion 32 is also made of aluminum, and the third molten pool portion 33 is a copper-aluminum composite material. For example, the third molten pool portion 33 is a copper-aluminum alloy or a copper-aluminum oxide alloy. Because the third molten pool portion 33 is a copper-aluminum composite material, it has the characteristics of high hardness and high melting point, which can significantly improve tensile strength.
[0074] like Figure 8 and Figure 9 As shown, in some embodiments, the longitudinal section of the first molten pool portion 31 is set to square, and / or the longitudinal section of the second molten pool portion 32 is set to inverted conical, and / or the longitudinal section of the third molten pool portion 33 is set to inverted conical.
[0075] Understandably, since the melting point of the first metal layer 11 is lower than that of the second metal layer 12, laser welding requires a higher power density to penetrate the second metal layer 12, resulting in a higher temperature for the first metal layer 11 and thus a square longitudinal section for the first molten pool portion 31. With energy loss and a decrease in effective power density during laser penetration, the second molten pool portion 32 and the third molten pool portion 33 can then form a structure with an inverted conical longitudinal section.
[0076] In some embodiments, the first welding layer 21 has an ultrasonic welding area for ultrasonic welding with the second welding layer 22 and a laser welding area for laser welding with the electrode 1. Along the direction from the electrode 1 to the weldment 2, the projection of the ultrasonic welding area and the projection of the laser welding area at least partially overlap.
[0077] Understandably, along the direction from pole 1 to weldment 2 (height direction), the projection of the ultrasonic welding zone and the projection of the laser welding zone at least partially overlap. On the one hand, this can improve the connection strength of the first welding layer 21, the second welding layer 22, and pole 1, thus improving the welding effect. On the other hand, when current flows through the second welding layer 22, the first welding layer 21, and pole 1, it can flow directly from the ultrasonic welding zone into the laser welding zone without the need for current transmission within the connecting piece 5, thereby shortening the current path.
[0078] In some embodiments, the projection of the ultrasonic welding zone and the projection of the laser welding zone completely coincide along the height direction.
[0079] In some embodiments, along the height direction, the projection of the ultrasonic welding zone is greater than the projection of the laser welding zone, and the projection of the ultrasonic welding zone covers the projection of the laser welding zone.
[0080] In some embodiments, along the height direction, the projection of the ultrasonic welding zone is smaller than the projection of the laser welding zone, and the projection of the laser welding zone covers the projection of the ultrasonic welding zone.
[0081] In some embodiments, along the height direction, the projections of the ultrasonic welding zone and the laser welding zone have overlapping areas that intersect each other.
[0082] like Figure 8 and Figure 9 As shown, in some embodiments, a groove 13 is formed at the end of the pole post 1 away from the weldment 2, and the bottom surface of the groove 13 serves as the welding surface.
[0083] It is understandable that by forming a groove 13 at the end of the electrode 1 away from the weldment 2, and using the bottom surface of the groove 13 as the welding surface, the thickness of the laser welding area of the electrode 1 can be reduced, the laser power can be lowered, thereby reducing welding costs and welding difficulty. At the same time, the groove 13 can also facilitate the positioning of the electrode 1 by the welding equipment, enabling the welding equipment to quickly and accurately confirm the welding surface, which is beneficial to improving welding efficiency and welding accuracy.
[0084] It should be noted that regardless of whether the pole 1 is used as the positive pole 1 or the negative pole 1, a groove 13 is formed at the end away from the welding part 2.
[0085] like Figure 6 and Figure 10 As shown, in some embodiments, the distance from the bottom surface of the groove 13 to the welded part 2 is b, and the height of the pole post 1 is h, satisfying: 5%≤b / h≤40%.
[0086] It is understandable that the distance from the bottom surface of the groove 13 to the weldment 2 is the thickness of the thinnest area of the pole post 1, and this area is the welding area of the pole post 1. The ratio of the thickness of the thinnest area of the pole post 1 to the height of the pole post 1 is set in the range of 5% to 40% to ensure that the groove 13 can be formed and that the laser can pass through the pole post 1.
[0087] When the ratio of the thickness of the thinnest region of electrode 1 to the height of electrode 1 is less than 5%, the groove depth of groove 13 is too large, making it difficult to process and shape groove 13. When the ratio of the thickness of the thinnest region of electrode 1 to the height of electrode 1 is greater than 40%, the groove depth of groove 13 is too small, resulting in a large thickness of the thinnest region of electrode 1, making it difficult for the laser to penetrate electrode 1.
[0088] In some embodiments, the ratio of the thickness of the thinnest region of the pole post 1 to the height of the pole post 1 is 3%. In this case, the groove depth of the groove 13 is too large, and the groove 13 is difficult to process and form.
[0089] In some embodiments, the ratio of the thickness of the thinnest region of the electrode post 1 to the height of the electrode post 1 is 50%. In this case, the groove depth of the groove 13 is too small, resulting in a large thickness of the thinnest region of the electrode post 1, making it difficult for the laser to penetrate the electrode post 1.
[0090] In some embodiments, the ratio of the thickness of the thinnest region of the pole post 1 to the height of the pole post 1 is 25%. In this case, on the one hand, the groove 13 can be formed, and on the other hand, the laser can pass through the pole post 1.
[0091] In some embodiments, the ratio of the thickness of the thinnest region of the pole post 1 to the height of the pole post 1 is set to 5%, 10%, 15%, 20%, 25%, 30%, 35%, 40%, or any value between the two.
[0092] It should be noted that when the electrode post 1 is the negative electrode post 1, the electrode post 1 includes a first metal layer 11 and a second metal layer 12. The groove 13 is located in the first metal layer 11. The distance from the bottom surface of the groove 13 to the weldment 2 is equal to the sum of the distance from the groove 13 to the second metal layer 12 and the thickness of the second metal layer 12.
[0093] like Figure 6 and Figure 10 As shown, in some embodiments, the welded part 2 includes a connecting piece 5 and a tab 4. The connecting piece 5 is located between the pole post 1 and the tab 4. The distance from the bottom surface of the groove 13 to the welded part 2 is b, and the thickness of the connecting piece 5 is c, satisfying: 0 < b / c ≤ 1 / 3.
[0094] It is understandable that when the connecting piece 5 is located between the pole post 1 and the tab 4, the ratio of the thickness of the thinnest area of the pole post 1 to the thickness of the connecting piece 5 is less than or equal to 1 / 3, so as to ensure that the connecting piece 5 can be stably melted through, thereby ensuring the connection strength and welding effect of the laser welding of the pole post 1, the connecting piece 5 and the tab 4.
[0095] Meanwhile, since the ratio of the thickness of the thinnest region of pole post 1 to the thickness of connecting piece 5 is less than or equal to 1 / 3, connecting piece 5 can also be thinner, further reducing the production cost of connecting piece 5.
[0096] In some embodiments, the ratio of the thickness of the thinnest region of the pole post 1 to the thickness of the connecting piece 5 is set to 1 / 7, 1 / 6, 1 / 5, 1 / 4, 1 / 3, or any value between the two.
[0097] like Figure 6 and Figure 10 As shown, in some embodiments, along the direction from the pole post 1 to the weldment 2, the sidewall of the groove 13 is inclined in a direction away from the axis of the pole post 1, wherein the inclination angle of the sidewall of the groove 13 is θ, which satisfies: 5°≤θ≤60°.
[0098] It is understandable that the inclination angle of the groove wall of the groove 13 is set in the range of 5° to 60° in order to facilitate the demolding of the pole post 1.
[0099] In some embodiments, the inclination angle of the groove wall surface of the groove 13 is set to 5°, 10°, 15°, 20°, 25°, 30°, 35°, 40°, 45°, 50°, 55°, 60°, or any value between any two.
[0100] like Figure 12 As shown in the embodiments of this application, a welding method is also provided for forming the welded structure as described above. The welding method includes: S100. Ultrasonic welding is performed between the tab 4 and the connecting piece 5 to form the welded part 2. S200, Laser penetration welding is performed on the side of electrode 1 away from weldment 2.
[0101] It is understandable that if laser penetration welding is performed on the side of the electrode 1 away from the welding component 2, the welding area is located outside the cell. This can prevent metal spatter generated during welding from contacting the cell pack and causing a short circuit in the battery.
[0102] The embodiments of this utility model have been described in detail above. Specific examples have been used to illustrate the principles and implementation methods of this utility model. The description of the above embodiments is only for the purpose of helping to understand the method and core ideas of this utility model. At the same time, for those skilled in the art, there will be changes in the specific implementation methods and application scope based on the ideas of this utility model. Therefore, the content of this specification should not be construed as a limitation of this utility model.
Claims
1. A welded structure, characterized in that, include: pole (1); The weldment (2) is welded to the pole post (1) and forms a molten pool (3) inside both. Along the direction from the pole post (1) to the weldment (2), the molten pool (3) has a decreasing cross-sectional width.
2. The welded structure according to claim 1, characterized in that, The welded component (2) includes a first weld layer (21) and a second weld layer (22). The pole post (1), the first weld layer (21) and the second weld layer (22) are stacked in sequence, and the first weld layer (21) is welded to the second weld layer (22) and the first weld layer (21) is welded to the pole post (1). In this case, one of the first weld layer (21) and the second weld layer (22) is a tab (4) and the other is a connecting piece (5).
3. The welded structure according to claim 2, characterized in that, The first welding layer (21) is ultrasonically welded to the second welding layer (22), and the first welding layer (21) is laser welded to the pole (1).
4. The welded structure according to claim 2, characterized in that, The end of the molten pool (3) away from the pole post (1) extends into the first welding layer (21), or the end of the molten pool (3) away from the pole post (1) extends into the second welding layer (22).
5. The welded structure according to claim 2, characterized in that, The pole post (1) includes a first metal layer (11) and a second metal layer (12), the second metal layer (12) being located between the first metal layer (11) and the first welding layer (21), wherein the first metal layer (11) and the second metal layer (12) have different melting points.
6. The welded structure according to claim 5, characterized in that, The melting point of the first metal layer (11) is lower than that of the second metal layer (12), and / or the melting point of the second metal layer (12) is the same as that of the first weld layer (21).
7. The welded structure according to claim 5, characterized in that, The molten pool (3) includes a first molten pool portion (31), a second molten pool portion (32) and a third molten pool portion (33) connected in sequence. The first molten pool portion (31) is located in the first metal layer (11), the second molten pool portion (32) is located in the second metal layer (12), one end of the third molten pool portion (33) is located in the second metal layer (12) and covers the second metal layer (12), and the other end extends into the first welding layer (21) or into the second welding layer (22).
8. The welded structure according to claim 7, characterized in that, The longitudinal section of the first molten pool (31) is square, and / or the longitudinal section of the second molten pool (32) is inverted conical, and / or the longitudinal section of the third molten pool (33) is inverted conical.
9. The welded structure according to any one of claims 1 to 8, characterized in that, The pole post (1) has a groove (13) formed at the end away from the weldment (2), and the bottom surface of the groove (13) serves as the welding surface, which is the working surface of the welding equipment.
10. The welded structure according to claim 9, characterized in that, The distance from the bottom surface of the groove (13) to the welded part (2) is b, and the height of the pole (1) is h, satisfying: 5%≤b / h≤40%.
11. The welded structure according to claim 9, characterized in that, The welded part (2) includes a connecting piece (5) and a tab (4). The connecting piece (5) is located between the pole post (1) and the tab (4). The distance from the bottom surface of the groove (13) to the welded part (2) is b, and the thickness of the connecting piece (5) is c, satisfying: 0 < b / c ≤ 1 / 3.
12. The welded structure according to claim 9, characterized in that, Along the direction from the pole post (1) to the welded part (2), the side wall of the groove (13) is inclined in a direction away from the axis of the pole post (1), wherein the inclination angle of the side wall of the groove (13) is θ, which satisfies: 5°≤θ≤60°.
13. A top cover assembly, characterized in that, Includes the welded structure as described in any one of claims 1 to 12.
14. A single-cell battery (6), characterized in that, Includes the top cover assembly as described in claim 13.
15. A battery pack, characterized in that, Includes the single cell (6) as described in claim 14.