Battery cell busbars and photovoltaic modules
By employing a combination structure of a busbar layer and a flexible insulating coating between the busbar and the solar cell, the problem of poor insulation performance in existing technologies is solved, achieving reliable insulation and a simplified process, thereby improving the production efficiency of photovoltaic modules.
Patent Information
- Application Number
- CN202522306255.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-10-29
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-10-29
AI Technical Summary
The existing insulation structure between the busbar and the solar cell has poor insulation performance, which can easily lead to short circuits. In addition, the existing insulation process is complicated and affects the production efficiency of photovoltaic modules.
The combined structure of the busbar and flexible insulating coating is adopted. The flexible insulating coating is located on the first side of the busbar and is used to abut the back of the battery cell. The second side of the busbar is connected to the solder strip, which connects to the conductive structure on the front of the battery cell to form an integrated design, achieving reliable insulation without the need for additional lamination process.
It improves the insulation reliability between the busbar and the solar cell, simplifies the process, and enhances the production efficiency and insulation performance of photovoltaic modules.
Smart Images

Figure CN224987917U_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of photovoltaic cell technology, and in particular to a cell busbar and a photovoltaic module. Background Technology
[0002] To increase the utilization area of solar cells within a given size and thus improve the power of photovoltaic modules, the common practice is to use busbar folding technology. This involves folding the busbars to the back of the solar cells, thus saving the area originally used for the busbars on the photovoltaic modules. This allows for further increases in the size of the solar cells and improves their detection power.
[0003] When the busbar is folded to the back of the battery cell, to prevent a short circuit after the busbar comes into contact with the battery cell, insulation is usually applied between the busbar and the battery cell. However, existing insulation structures are not very effective and can easily lead to insulation failure between the busbar and the battery cell. Utility Model Content
[0004] Therefore, it is necessary to provide a cell busbar and photovoltaic module to address the problem of low insulation performance of existing insulation structures.
[0005] In a first aspect, this application provides a battery cell busbar, comprising:
[0006] The busbar has a first surface and a second surface that are positioned opposite to each other.
[0007] A flexible insulating coating is located on the first surface of the busbar layer;
[0008] The first side of the busbar layer is used to abut against the back of the battery cell through the flexible insulating coating; the second side of the busbar layer is used to connect the solder strip and connect the conductive structure located on the front of the battery cell through the solder strip.
[0009] In one embodiment, the flexible insulating coating comprises an inorganic adhesive layer, an organic insulating layer, and a protective layer sequentially stacked in a direction away from the busbar.
[0010] In one embodiment, at least one of the following solutions is included:
[0011] The organic insulating layer comprises a composite layer consisting of an organosilicon resin and an ultraviolet absorber.
[0012] The inorganic bonding layer comprises a composite layer consisting of nano-alumina sol and silane coupling agent;
[0013] The protective layer includes a perfluoropolyether layer;
[0014] The thickness of the flexible insulating coating ranges from 8μm to 50μm.
[0015] In one embodiment, the breakdown strength of the organic insulating layer is ≥35kV / mm.
[0016] In one embodiment, the thickness of the organic insulating layer ranges from 5 μm to 30 μm.
[0017] In one embodiment, the thickness of the inorganic adhesive layer ranges from 2 μm to 10 μm.
[0018] In one embodiment, the thickness of the protective layer ranges from 1 μm to 10 μm.
[0019] In one embodiment, the bus layer includes a conductive layer and a solder layer sequentially stacked in a direction away from the flexible insulating coating;
[0020] Alternatively, the bus layer may include: a conductive layer and a welding layer covering the conductive layer; the flexible insulating coating may be sprayed onto the surface of the welding layer.
[0021] In one embodiment, at least one of the following solutions is included:
[0022] The dimensions of the conductive layer along the length of the battery cell range from 4mm to 10mm.
[0023] The thickness of the conductive layer ranges from 0.2 mm to 1.0 mm;
[0024] The thickness of the weld layer ranges from 10μm to 50μm.
[0025] Secondly, this application provides a photovoltaic module, comprising:
[0026] A battery cell has a front side and a back side disposed opposite to each other, including a conductive structure disposed on the front side and / or the back side;
[0027] Solder strips are used to connect the conductive structure;
[0028] The battery cell busbar described above is located on the back side of the battery cell; wherein the flexible insulating coating surface facing away from the busbar abuts against the back side of the battery cell; the second side of the busbar is connected to the solder strip and is connected to the conductive structure through the solder strip.
[0029] The aforementioned busbar and photovoltaic module, by incorporating a busbar layer and a flexible insulating coating, achieve this by using a first side of the busbar layer. This first side of the busbar layer abuts against the back of the solar cell via the flexible insulating coating. The second side of the busbar layer is used to connect solder strips, which connect to the conductive structure on the front of the solar cell. The busbar layer and the flexible insulating coating are integrally formed, allowing the busbar to function as both a current collector and an insulator. Furthermore, this integral design ensures a tight bond between the busbar layer and the flexible insulating coating, guaranteeing reliable insulation between the busbar layer and the solar cell. Additionally, since the flexible insulating coating is formed on the first side of the busbar layer, when the busbar is folded to the back of the solar cell, the side of the flexible insulating coating away from the busbar layer abuts against the solar cell. This eliminates the need for lamination bonding, achieving insulation between the busbar layer and the solar cell. This simple process effectively improves the production efficiency of photovoltaic modules. Attached Figure Description
[0030] Figure 1 This is a schematic diagram of the structure of an insulating strip in the prior art.
[0031] Figure 2 This is a front view of a photovoltaic module with the busbars not folded up, according to one embodiment.
[0032] Figure 3 This is a schematic diagram of the back of a photovoltaic module after the busbar has been folded up, according to one embodiment.
[0033] Figure 4 for Figure 3 Cross-sectional view of AA.
[0034] Figure 5 for Figure 4 Enlarged view of point B in the middle.
[0035] Figure 6 This is a schematic diagram of the structure of a battery cell busbar according to one embodiment.
[0036] Figure 7 This is a schematic diagram of the structure of the battery cell busbar according to another embodiment.
[0037] Instruction manual illustrations:
[0038] First coating layer 11, first coating layer 12, substrate 13, second coating layer 14, second coating layer 15;
[0039] Busbar 100, busbar layer 110, inorganic bonding layer 111, organic insulating layer 112, protective layer 113, flexible insulating coating 120, conductive layer 121, welding layer 122;
[0040] 200 solar cells;
[0041] First welding strip 300;
[0042] The second welding strip is 400. Detailed Implementation
[0043] To make the above-mentioned objectives, features, and advantages of this application more apparent and understandable, the specific embodiments of this application are described in detail below with reference to the accompanying drawings. Many specific details are set forth in the following description to provide a thorough understanding of this application. However, this application can be implemented in many other ways different from those described herein, and those skilled in the art can make similar modifications without departing from the spirit of this application. Therefore, this application is not limited to the specific embodiments disclosed below.
[0044] In the description of this application, it should be understood that if terms such as "center", "longitudinal", "lateral", "length", "width", "thickness", "upper", "lower", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", "clockwise", "counterclockwise", "axial", "radial", "circumferential" appear, these terms indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, and are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this application.
[0045] Furthermore, where the terms "first" and "second" appear, these terms are for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined with "first" or "second" may explicitly or implicitly include at least one of that feature. In the description of this application, where the term "multiple" appears, "multiple" means at least two, such as two, three, etc., unless otherwise explicitly specified.
[0046] In this application, unless otherwise expressly specified and limited, the terms "installation," "connection," "joining," and "fixing," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components, unless otherwise expressly limited. Those skilled in the art can understand the specific meaning of the above terms in this application based on the specific circumstances.
[0047] In this application, unless otherwise expressly specified and limited, the use of descriptions such as "above" or "below" the second feature indicates that the first and second features are in direct contact or indirect contact via an intermediate medium. Furthermore, "above," "on top of," and "over" the second feature can mean that the first feature is directly above or diagonally above the second feature, or simply that the first feature is at a higher horizontal level than the second feature. Similarly, "below," "below," and "under" the second feature can mean that the first feature is directly below or diagonally below the second feature, or simply that the first feature is at a lower horizontal level than the second feature.
[0048] It should be noted that if an element is referred to as being "fixed to" or "set on" another element, it can be directly on the other element or there may be an intervening element. If an element is considered to be "connected to" another element, it can be directly connected to the other element or there may be an intervening element. If so, the terms "vertical," "horizontal," "upper," "lower," "left," "right," and similar expressions used in this application are for illustrative purposes only and do not represent the only possible implementation.
[0049] As described in the background section, in the prior art, to prevent the folded busbar from contacting the back of the battery cell, the busbar needs to be insulated to avoid a short circuit between the busbar and the battery cell. Typically, an insulating strip is used to separate the busbar from the battery cell. Figure 1 As shown, the existing insulating strip includes a first coating layer 11, a first coating layer 12, a substrate 13, a second coating layer 14, and a second coating layer 15, which are stacked sequentially from bottom to top along the thickness direction. The first coating layer 11 is used to bond with the busbar, the second coating layer 15 is used to bond with the battery cell, the first coating layer 12 and the second coating layer 14 are used to block ultraviolet rays, and the substrate 13 is used to provide insulation between the busbar and the battery cell.
[0050] In the prior art, the thickness of the first coating layer 11 is typically in the range of 50μm to 200μm, the thickness of the first coating layer 12 is typically in the range of 5μm to 20μm, the thickness of the substrate 13 is typically in the range of 50μm to 125μm, the thickness of the second coating layer 14 is typically in the range of 5μm to 20μm, and the thickness of the second coating layer 15 is typically in the range of 200μm to 500μm. Since the thickness of the first coating layer 11 and the second coating layer 15 is different from the thickness of the adhesive film used to bond them to the corresponding busbars and battery cells, during the lamination (bonding) process, the first coating layer 11 and the second coating layer 15 are easily affected by process parameters such as lamination temperature and lamination time, which can easily generate bubbles during the lamination process, resulting in a narrow process window and making process control difficult. In addition, during the UV (Ultraviolet) aging test, the substrate 13 is made of PET (Polyethylene terephthalate), which is prone to chemical bond breakage under ultraviolet irradiation, resulting in yellowing or overall powdering. At the same time, in high-temperature aging tests such as hot spots, the insulating strip is prone to generating bubbles, leading to the failure of the insulating strip.
[0051] For the reasons mentioned above, this application provides a battery cell busbar, such as... Figure 2 , Figure 3 , Figure 4 and Figure 5 As shown, a battery cell busbar provided in one embodiment of this application includes a busbar layer 110 and a flexible insulating coating 120. The busbar layer 110 has a first side and a second side disposed opposite to each other. The flexible insulating coating 120 is located on the first side of the busbar layer 110. The first side of the busbar layer 110 is used to abut against the back side of the battery cell 200 through the flexible insulating coating 120. The second side of the busbar layer 110 is used to connect a first solder strip 300 and to connect a conductive structure (not shown) located on the front side of the battery cell 200 through the first solder strip 300.
[0052] The busbar 100 has an overall elongated structure. The length of the busbar 100 extends along the width of the solar cell 200, i.e., the X-axis direction in the figure. The busbar 100 has a certain thickness in the Z-axis direction. The busbar layer 110 and the flexible insulating coating 120 are stacked along the Z-axis direction. The busbar layer 110 is used to collect the photocurrent generated by the solar cell 200. Specifically, the busbar layer 110 is connected to the conductive structure on the front side of the solar cell 200 through the first solder strip 300. After the solar cell 200 detects a light signal, it can generate a photocurrent through photoelectric conversion. The photocurrent is transmitted sequentially through the conductive structure and the first solder strip 300 to the busbar layer 110, thus collecting the photocurrent. The flexible insulating coating 120 is used to insulate the busbar layer 110 and the solar cell 200 when the busbar 100 is folded to the back of the solar cell 200, preventing short circuits caused by contact between the busbar layer 110 and the solar cell 200.
[0053] The first and second surfaces of the bus layer 110 are surfaces that are arranged opposite each other in the Z-axis direction, and the flexible insulating coating 130 is stacked on the first surface of the bus layer 110 along the Z-axis direction. When the busbar 100 is not folded to the back of the battery cell 200, in the illustrated direction, the first surface of the busbar layer 110 and the back of the battery cell 200 are arranged downward along the Z-axis, so that the side surface of the flexible insulating coating 120 away from the busbar layer 110 (the first surface of the flexible insulating coating 120) is also arranged downward along the Z-axis, and the second surface of the busbar layer 110 and the front of the battery cell 200 are arranged upward along the Z-axis. When the busbar 100 is folded to the back of the battery cell 200, the first surface of the busbar layer 110 and the front of the battery cell 200 are arranged upward along the Z-axis, while the second surface of the busbar layer 110 and the back of the battery cell 200 are arranged downward along the Z-axis, so that the first surface of the flexible insulating coating 120 is arranged upward and abuts against the corresponding position of the downward-arranged back of the battery cell 200, thereby achieving insulation between the busbar layer 110 and the battery cell 200.
[0054] In this embodiment, by providing a bus layer 110 and a flexible insulating coating 120, the flexible insulating coating 120 is located on the first side of the bus layer 110, and the first side of the bus layer 110 abuts against the back of the battery cell 200 through the flexible insulating coating 120. The second side of the bus layer 110 is used to connect the first solder strip 300 and to connect the conductive structure located on the front side of the battery through the first solder strip 300. The bus layer 110 and the flexible insulating coating 120 are formed as one piece, so that the bus bar 100 has the functions of collecting current and insulation. At the same time, the integral arrangement between the bus layer 110 and the flexible insulating coating 120 allows the bus layer 110 and the flexible insulating coating 120 to be tightly bonded, so as to ensure reliable insulation between the bus layer 110 and the battery cell 200 by the flexible insulating coating 120. In addition, the flexible insulating coating 120 is formed on the first side of the busbar 110. When the busbar 100 is folded to the back of the cell 200, the side of the flexible insulating coating 120 away from the busbar 110 abuts against the cell 200. The insulation between the busbar 110 and the cell 200 can be achieved without the need for lamination bonding. The process is simple and can effectively improve the production efficiency of photovoltaic modules.
[0055] In one embodiment, such as Figure 6 As shown, the flexible insulating coating 120 includes an inorganic adhesive layer 111, an organic insulating layer 112, and a protective layer 113 sequentially stacked in a direction away from the busbar 110.
[0056] For example, the inorganic adhesive layer, organic insulating layer 112, and protective layer 113 are stacked along the Z-axis. The inorganic adhesive layer is stacked on the first surface of the busbar 110, and is in direct contact with the first surface of the busbar 110, to achieve a reliable connection between the entire flexible insulating coating 120 and the busbar 110. The organic insulating layer 112 is stacked on the side of the inorganic adhesive layer facing away from the busbar 110. As the core insulating film layer of the flexible insulating coating 120, the organic insulating layer 112 can provide insulation between the busbar 110 and the battery cell 200, and can also be used to block ultraviolet rays to improve the UV resistance of the busbar 100. The protective layer 113 is stacked on the side of the organic insulating layer 112 facing away from the inorganic adhesive layer to form a dense protective film layer to prevent the organic insulating layer 112 from being corroded, thereby improving the reliable insulation of the flexible insulating coating 120 for the busbar 110 and the battery cell 200.
[0057] In an optional embodiment, the inorganic adhesive layer 111 comprises a composite layer consisting of nano-alumina sol and a silane coupling agent.
[0058] For example, the inorganic adhesive layer can be formed by mixing a nano-alumina solution and a silane coupling agent and molding it onto the first surface of the busbar layer 110 to form a composite layer. The nano-alumina solution in the composite layer can form a gradient porous structure through the stacking effect of nanoparticles, achieving the dual functions of water vapor barrier and ultraviolet shielding. The silane coupling agent in the composite layer can be used to achieve chemical bonding between particles, connecting the nano-alumina to the busbar layer 110 to form a high-strength chemical bond; specifically, a coupling agent of type KH-550 can be used.
[0059] Optionally, the mixing mass ratio of the nano-alumina solution and the silane coupling agent can be 85%:15%. After fusing the nano-alumina with the silane coupling agent to form a mixed solution, the mixed solution can be sprayed onto the first surface of the busbar layer 110 to increase the chemical bonding force between the inorganic adhesive layer and the first surface of the busbar layer 110. This helps to prevent the flexible insulating coating 120 from peeling off from the first surface of the busbar layer 110 under high temperature, thereby greatly increasing the insulation reliability of the flexible insulating coating 120. Specifically, the inorganic adhesive layer can be formed by electrostatic spraying, and the spraying voltage can be 40kV. After spraying, the sprayed coating can be cured using a gradient curing method. After curing, an inorganic adhesive layer is formed. During gradient curing, the initial temperature can be 120℃ for 1 minute, the ending temperature can be 180℃ for 2 minutes, the heating rate can be 5℃ / min, and the curing transfer rate is 1.5m / min.
[0060] Optionally, the uniformity of the inorganic adhesive layer's film thickness is less than or equal to ±5% to ensure the uniformity of thermal stress distribution between the busbar layer 110 and the flexible insulating coating 120. Based on this, the particle size of the alumina nanoparticles in the alumina nanoparticle solution ranges from 20 nm to 40 nm. For example, the particle size of the alumina nanoparticles can be 20 nm, 25 nm, 30 nm, 40 nm, or any value between these values. Specifically, if the particle size of the alumina nanoparticles is less than 20 nm, agglomeration is likely to occur due to increased particle surface energy, leading to a decrease in the uniformity of the inorganic adhesive layer. If the particle size of the alumina nanoparticles is less than 40 nm, the particle specific surface area decreases, which may affect the adhesion between the inorganic adhesive layer and the busbar layer 110 due to stress concentration.
[0061] In an optional embodiment, the organic insulating layer 112 comprises a composite layer consisting of an organosilicon resin and an ultraviolet absorber.
[0062] For example, the organic insulating layer 112 can be formed by mixing an organosilicon resin and an ultraviolet absorber and molding it onto the surface of the inorganic adhesive layer opposite to the busbar layer 110 to form a composite layer. The organosilicon resin in the composite layer can be used to construct a flexible matrix to increase the overall ductility of the flexible insulating coating 120 and reduce the risk of breakage of the flexible insulating coating 120; specifically, the organosilicon resin can be phenyl-modified methyl silicone resin. The ultraviolet absorber in the composite layer can be used to selectively absorb ultraviolet light to inhibit the photolysis of the organosilicon resin, thereby improving the anti-aging performance of the organic insulating layer 112.
[0063] Optionally, the mixing mass ratio of silicone resin and UV absorber can be 97%:3%. After mixing the silicone resin and UV absorber to form a fusion, the mixed solution can be sprayed onto the surface of the inorganic adhesive layer facing away from the busbar 110, serving as the core of the flexible insulating coating 120 to achieve insulation between the busbar 110 and the battery cell 200. Simultaneously, the UV absorber provides UV protection. Specifically, the organic insulating layer 112 can be formed by high-precision atomization spraying, ensuring that the film thickness CV (Coefficient of Variation) value of the organic insulating layer 112 is less than or equal to 3%. After spraying, the coating can be cured using infrared fast curing under a protective atmosphere. The infrared light temperature is 150℃, the duration is 90s, and the peak wavelength is 2.5μm. The protective atmosphere is nitrogen with a flow rate less than or equal to 100ppm.
[0064] Optionally, the breakdown strength of the organic insulating layer 112 is ≥35kV / mm. In photovoltaic modules, electric field concentration may occur between the bus layer 110 and the back surface of the cell 200 due to local defects (such as pinholes or impurities). If the breakdown strength of the organic insulating layer 112 is insufficient (e.g., <35kV / mm), partial discharge is easily triggered under high voltage, leading to carbonization and perforation of the organic insulating layer 112. Therefore, setting the breakdown strength of the organic insulating layer 112 to ≥35kV / mm can reduce the risk of failure of the organic insulating layer 112 due to partial discharge.
[0065] In an optional embodiment, the protective layer 113 comprises a perfluoropolyether layer.
[0066] For example, the protective layer 113 can be formed by molding perfluoropolyether onto the surface of the organic insulating layer 112 away from the inorganic adhesive layer to form a perfluoropolyether layer. The perfluoropolyether in the perfluoropolyether layer can be used to form a dense coating on the surface of the organic insulating layer 112 away from the inorganic adhesive layer. This dense coating has sufficient surface energy to prevent various acidic substances generated during the aging process of the battery cell 200's encapsulation material from corroding the organic insulating layer 112, thereby improving the resistance of the organic insulating layer 112 to damp heat.
[0067] Optionally, the perfluoropolyether can be formed by spraying a perfluoropolyether nano-dispersion with a particle size of 30 nm onto the surface of the organic insulating layer 112 facing away from the inorganic adhesive layer. Specifically, the protective layer 113 can be formed by atomization spraying, with an atomization pressure of 0.3 MPa and a nozzle height of 15 cm ± 1 cm from the organic insulating layer 112. After spraying, the coating can be cured using infrared fast curing under a protective atmosphere. The infrared light temperature is 200°C, the duration is 90 s, and the peak wavelength is 2.5 μm. The protective atmosphere is nitrogen with a flow rate less than or equal to 100 ppm.
[0068] In an optional embodiment, the thickness of the flexible insulating coating 120 ranges from 8 μm to 50 μm. For example, the thickness of the flexible insulating coating 120 can be 8 μm, 15 μm, 30 μm, 50 μm, or any value between these values. Specifically, if the thickness of the flexible insulating coating 120 is less than 8 μm, the flexible insulating coating 120 is prone to damage / breakdown due to local electric field concentration or mechanical stress, failing to provide reliable insulation. If the thickness of the flexible insulating coating 120 is greater than 50 μm, it will increase the thickness of the entire busbar 100, leading to stress imbalance between the layers of the battery cell 200 or insufficient encapsulation space, affecting the reliability of the battery cell 200. Therefore, setting the thickness of the flexible insulating coating 120 to 8 μm to 50 μm can ensure reliable insulation of the battery cell 200 and the busbar 110 by the entire flexible insulating coating 120.
[0069] Optionally, the thickness of the inorganic adhesive layer 111 can range from 2μm to 10μm. For example, the thickness of the inorganic adhesive layer 111 can be 2μm, 4μm, 7μm, 10μm, or any value between these values. Specifically, if the thickness of the inorganic adhesive layer 111 is less than 2μm, the interfacial bonding strength between the inorganic adhesive layer and the busbar 100 may decrease, leading to the peeling of the entire flexible insulating coating 120 during long-term use. If the thickness of the inorganic adhesive layer 111 is greater than 10μm, stress concentration within the inorganic adhesive layer may cause microcracks to propagate, reducing the connection reliability of the inorganic adhesive layer. Therefore, setting the thickness of the inorganic adhesive layer 111 to 2μm to 10μm ensures the connection strength between the entire inorganic adhesive layer 111 and the busbar 110.
[0070] Optionally, the thickness of the organic insulating layer 112 can range from 5 μm to 30 μm. For example, the thickness of the organic insulating layer 112 can be 5 μm, 10 μm, 20 μm, 30 μm, or any value between these values. Specifically, if the thickness of the organic insulating layer 112 is less than 5 μm, the organic insulating layer 112 may fail due to breakdown. If the thickness of the organic insulating layer 112 is greater than 30 μm, it increases the thickness of the entire flexible insulating coating 120, which may lead to stress imbalance between the layers of the solar cell 200 or insufficient encapsulation space. Therefore, setting the thickness of the organic insulating layer 112 to 5 μm to 30 μm can ensure the reliable insulation of the entire organic insulating layer 112.
[0071] Optionally, the thickness of the protective layer 113 can range from 1 μm to 10 μm. For example, the thickness of the protective layer 113 can be 1 μm, 3 μm, 6 μm, 10 μm, or any value between these values. Specifically, if the thickness of the protective layer 113 is less than 1 μm, the protective effect of the protective layer 113 may be poor, which may lead to corrosion of the organic insulating layer 112 and a reduction in the insulation effect. If the thickness of the protective layer 113 is greater than 10 μm, it may increase the thickness of the entire flexible insulating coating 120. Therefore, setting the thickness of the protective layer 113 to 1 μm can ensure the protective performance of the entire protective layer 113.
[0072] In one embodiment, such as Figure 6 As shown, the bus layer 110 includes a conductive layer 121 and a welding layer 122 sequentially stacked along the direction away from the flexible insulating coating 120.
[0073] For example, the conductive layer 121 and the solder layer 122 are stacked along the Z-axis. The conductive layer 121 is stacked on the surface of the flexible insulating coating 120 opposite to the solar cell 200 (in the folded state of the busbar 100). The conductive layer 121 is used to receive the photocurrent transmitted from the solar cell 200 through the conductive structure and the solder joint, and output the photocurrent to the external circuit. Specifically, the conductive layer 121 is stacked on the surface of the inorganic adhesive layer opposite to the organic insulating side. The conductive layer 121 is in direct contact with the inorganic adhesive layer to achieve a reliable connection between the busbar 110 and the flexible insulating coating 120. The solder layer 122 is stacked on the surface of the conductive layer 121 opposite to the inorganic adhesive layer. The solder layer 122 is used to connect with the first solder strip 300 to achieve the connection between the first solder strip 300 and the busbar 110, thereby transmitting the photocurrent to the conductive layer 121.
[0074] Optionally, the conductive layer 121 can be made of a copper substrate. The copper substrate can be a copper plate or other copper structure cut to a preset size to form the conductive layer 121. The solder layer 122 can be made of a tin-lead solder alloy. The solder layer 122 can be made using a hot-dip galvanizing process combined with a resist plating process, that is, the solder layer 122 is plated on one side surface of the conductive layer 121 to reduce the overall material cost of the bus layer 110.
[0075] In one embodiment, such as Figure 7 As shown, the bus layer 110 includes a conductive layer 121 and a welding layer 122 covering the conductive layer 121; a flexible insulating coating 120 is sprayed onto the surface of the welding layer 122.
[0076] For example, the bus layer 110 is stacked along the Z-axis on the surface of the flexible insulating coating 120 facing away from the solar cell 200 (in the folded state of the busbar 100). The conductive layer 121 is used to receive the photocurrent transmitted from the solar cell 200 through the conductive structure and solder joints, and output the photocurrent. The solder layer 122 is used to connect to an external circuit to provide a current path from the conductive layer 121 to the external circuit. In specific implementation, the solder layer 122 covering the conductive layer 121 means that the solder layer 122 is provided on the outer periphery of the conductive layer 121 to ensure the uniformity of photocurrent transmission. In this embodiment, the bus layer 110 can be an existing structure, so it can be implemented without additional processes, and the process implementation is simple.
[0077] Optionally, the conductive layer 121 can be made of a copper substrate. The copper substrate can be a copper plate or other copper structure cut to a preset size to form the conductive layer 121. The solder layer 122 can be made of a tin-lead solder alloy. When plating the solder layer 122, a hot-dip galvanizing process can be used to directly plate it on the outer periphery of the conductive layer 121 to obtain the solder layer 122.
[0078] In an optional embodiment, the dimension of the conductive layer 121 along the length direction (i.e., the Y-axis direction) of the solar cell 200 ranges from 4mm to 10mm, which is the width of the conductive layer 121. For example, the width of the conductive layer 121 can be 4mm, 5mm, 7.5mm, 10mm, or any value between these. Specifically, if the width of the conductive layer 121 is less than 4mm, the overall conductive cross-sectional area of the busbar 100 may be insufficient, resulting in increased resistance during the transmission of photocurrent and affecting the overall operational stability of the solar cell 200. If the width of the conductive layer 121 is greater than 10mm, it will increase the overall material cost of the busbar 100. Therefore, setting the width of the conductive layer 121 to 4mm to 10mm can reduce the production cost of the solar cell 200 while ensuring sufficient conductive cross-sectional area and reducing photocurrent transmission loss.
[0079] In an optional embodiment, the thickness of the conductive layer 121 ranges from 0.2 mm to 1.0 mm, which is the dimension of the conductive layer 121 in the Z-axis direction. For example, the thickness of the conductive layer 121 can be 0.2 mm, 0.4 mm, 0.65 mm, 1.0 mm, or any value between these values. Specifically, if the thickness of the conductive layer 121 is less than 0.2 mm, it may bend or break due to insufficient mechanical strength. At the same time, a small thickness will result in an excessively small cross-sectional area of the conductive layer 121, leading to increased transmission resistance of the photogenerated current and increased power loss. If the thickness of the conductive layer 121 is greater than 1.0 mm, it will increase the overall material cost of the busbar 100. In addition, an excessively thick conductive layer 121 may also cause mechanical stress damage to the solar cell 200, reducing conductivity reliability. Therefore, setting the thickness of the conductive layer 121 to 0.2 mm to 1.0 mm can balance the mechanical strength and conductivity of the conductive layer 121, avoiding structural fragility and excessive losses caused by excessive thinness, while preventing risks such as increased production costs and stress damage caused by excessive thickness.
[0080] In an optional embodiment, the thickness of the weld layer 122 ranges from 10 μm to 50 μm, which is the dimension of the weld layer 122 in the Z-axis direction. For example, the thickness of the weld layer 122 can be 10 μm, 20 μm, 35 μm, 50 μm, or any value between these values. Specifically, if the thickness of the welding layer 122 is less than 10μm, it may lead to poor contact at the welding interface, forming a local high-resistance area, which will affect the transmission of photocurrent. In addition, if the welding strength is insufficient, the weld joint is prone to cracking and falling off when the ambient temperature changes or vibrates. If the thickness of the welding layer 122 is greater than 50μm, the excess welding material is prone to overflow and accumulation, which makes it easy for bubbles or stress concentration to form inside the welding layer 122 after curing, reducing welding reliability and increasing material costs. Therefore, setting the thickness of the welding layer 122 to 10μm~50μm can ensure that the welding material fully fills the interface gap, realizes a stable and reliable electrical connection between the welding layer 122 and the first welding strip 300, and avoids stress and cost problems, ensuring a stable connection between the busbar 100 and the battery cell 200.
[0081] like Figure 2 , Figure 3 , Figure 4 and Figure 5 As shown, this embodiment provides a photovoltaic module, including a solar cell 200, a first solder ribbon 300, and a solar cell busbar (i.e., busbar 100 as described above) as in the above embodiments. The solar cell 200 has a front and a back side disposed opposite to each other, including conductive structures disposed on the front and / or back sides; the first solder ribbon 300 is used to connect the conductive structures; the solar cell busbar is located on the back side of the solar cell 200; wherein, the surface of the flexible insulating coating 120 facing away from the busbar layer 110 abuts against the back side of the solar cell 200; the second side of the busbar layer 110 is connected to the first solder ribbon 300, and the conductive structures are connected through the first solder ribbon 300.
[0082] The solar cell 200 is used to detect optical signals and generate photocurrent through photoelectric conversion. Multiple solar cells 200 can be provided, and they can be connected to each other through a conductive structure to form a battery string. Optionally, the conductive structure may include a second solder strip 400, grid lines, and / or contact electrodes. Each solar cell 200 can connect its electrodes (e.g., the front electrode to the back electrode of an adjacent solar cell 200) through the second solder strip 400, or through the corresponding overlap, pressing, or welding of the grid lines and contact electrodes, allowing current to be sequentially transmitted between adjacent solar cells 200, thus forming a battery string.
[0083] The first solder strip 300 may include one or more strips. When multiple first solder strips 300 are provided, each first solder strip 300 can be evenly spaced along the X-axis. Correspondingly, when multiple first solder strips 300 are provided, the conductive structure on the solar cell 200 can also be configured one-to-one with the first solder strip 300 to improve the transmission efficiency of the photogenerated current. The first solder strip 300 can be made of a deformable conductive material so that after the solar cell 200 is connected to the solar cell busbar through the first solder strip 300, the first solder strip 300 can be bent toward the back of the solar cell 200, so that the busbar 100 can be folded to the back of the solar cell 200, and the flexible insulating coating 120 abuts against the back of the solar cell 200. In this way, the space originally used for arranging the solar cell busbar on the photovoltaic module can be saved to increase the size of the solar cell 200, thereby increasing the power of the photovoltaic module.
[0084] The technical features of the above embodiments can be combined in any way. For the sake of brevity, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0085] The embodiments described above are merely illustrative of several implementation methods of this application, and while the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the patent application. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of this application, and these all fall within the protection scope of this application. Therefore, the protection scope of this patent application should be determined by the appended claims.
Claims
1. A busbar for a battery cell, characterized in that include: The busbar has a first surface and a second surface that are positioned opposite to each other. A flexible insulating coating is located on the first surface of the busbar layer; The first side of the busbar layer is used to abut against the back of the battery cell through the flexible insulating coating; the second side of the busbar layer is used to connect the solder strip and connect the conductive structure located on the front of the battery cell through the solder strip.
2. The cell tab of claim 1, wherein, The flexible insulating coating comprises: an inorganic bonding layer, an organic insulating layer, and a protective layer sequentially stacked in a direction away from the busbar.
3. The cell tab of claim 2, wherein, The thickness of the flexible insulating coating ranges from 8μm to 50μm.
4. The cell tab of claim 2, wherein, The breakdown strength of the organic insulating layer is ≥35kV / mm.
5. The cell tab of claim 2, wherein, The thickness of the organic insulating layer ranges from 5 μm to 30 μm.
6. The cell tab of claim 2, wherein, The thickness of the inorganic adhesive layer ranges from 2 μm to 10 μm.
7. The cell tab of claim 2, wherein, The thickness of the protective layer ranges from 1 μm to 10 μm.
8. The battery cell busbar according to any one of claims 1 to 7, characterized in that, The bus layer includes: a conductive layer and a welding layer sequentially stacked in a direction away from the flexible insulating coating; Alternatively, the bus layer may include: a conductive layer and a welding layer covering the conductive layer; the flexible insulating coating may be sprayed onto the surface of the welding layer.
9. The battery cell busbar according to claim 8, characterized in that, Including at least one of the following solutions: The dimensions of the conductive layer along the length of the battery cell range from 4mm to 10mm. The thickness of the conductive layer ranges from 0.2 mm to 1.0 mm; The thickness of the weld layer ranges from 10μm to 50μm.
10. A photovoltaic module, characterized in that, include: A battery cell has a front side and a back side disposed opposite to each other, including a conductive structure disposed on the front side and / or the back side; Solder strips are used to connect the conductive structure; The battery cell busbar as described in any one of claims 1 to 9 is located on the back side of the battery cell; wherein the surface of the flexible insulating coating facing away from the busbar abuts against the back side of the battery cell; the second surface of the busbar is connected to the solder strip and connected to the conductive structure through the solder strip.