Batch for the production of a coarse ceramic refractory basic product and use of the batch, such product as well as process for its production, lining of an industrial furnace and use of the lining for an industrial furnace
Patent Information
- Application Number
- DE102019220085
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2019-12-18
- Publication Date
- 2024-10-10
- Estimated Expiration
- 2039-12-18
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
The present invention relates to a dry batch for producing a coarse ceramic refractory basic shaped product, its use, such a product and a method for its production and a lining of an industrial furnace and the use of the lining for an industrial furnace. The term "refractory" in the context of the invention should not be limited to the definition according to ISO 836 or DIN 51060, which define a cone drop point of > 1500°C. Refractory products within the meaning of the invention have a compression softening point T0.5 according to DIN EN ISO 1893: 2008-09 of T0.5≥ 600 °C, preferably T0.5≥ 800 °C. Accordingly, refractory or refractory granular materials or grains within the meaning of the invention are those materials or grains that are suitable for a refractory product with the above-mentioned compression softening point T0.5. The refractory products according to the invention are used to protect aggregate structures in aggregates in which temperatures between 600 and 2000 °C, in particular between 1000 and 1800 °C, prevail. Coarse ceramic products are known to be products made from grains with grain sizes up to 6 mm, in special cases even up to 25 mm (see “Gerald Routschka / Hartmut Wuthnow, Practical Handbook “Refractory Materials”, 5th edition, Vulkan-Verlag (hereinafter referred to simply as “Practical Handbook”), Chapter 2). The term "granulation" or "granular material" within the meaning of the invention encompasses a pourable solid consisting of many small, solid grains. If the grains have a grain size of ≤ 200 µm, the grain is a flour or powder. If the grains are produced by mechanical comminution, e.g., crushing and / or grinding, they are crushed granules or broken grains. However, a grain can also comprise granules or pellets, which are produced by granulation or pelletizing without mechanical comminution. The grain size distribution of the grain is generally adjusted by sieving. Unless otherwise stated, the grain sizes specified in this invention are also determined according to DIN 66165-2:2016-08. For the purposes of the invention, grain fractions or grain classes also have grain sizes between the two specified test grain sizes. The term "grain fraction" or "grain class" thus means that no grains remain on the upper sieve and none pass through the lower sieve. Thus, there is no oversize or undersize grain. In contrast, the term “grain group” implies that some grains remain on the upper sieve (oversize grain) and some fall through the lower sieve (undersize grain). Furthermore, the grain fractions or grain groups used in this field contain grains of different sizes. They therefore exhibit a grain distribution or grain size distribution. They are not single-grain fractions or groups. In the case of heavy clay products, a distinction is also made between shaped and unshaped products. Shaped heavy clay products are unfired, tempered, or ceramic-fired products, preferably manufactured in a ceramic factory, particularly bricks or slabs. They have a defined geometry and are ready for installation. Shaping is achieved, for example, by pressing, stamping, ramming, or slip casting. The shaped products, particularly bricks, are then laid with mortar or mortar-free ("crunch"), for example, to form a lining. The production process for shaped heavy clay products is typically divided into the following steps (Practical Handbook, page 15 / Section 2.1): - Preparation - Mixing - Shaping - Drying - (If necessary) Thermal treatment up to 800 °C, firing or sintering - Post-treatment (if necessary) Unformed products are products that are formed into their final shape, usually by the user, from an unformed mass or lumps, e.g., by pouring, vibrating, poking, tamping, or spraying. Unformed products are usually placed behind formwork in larger sections at the site of use and, after hardening, form part of the lining. Examples of unformed products include shotcrete, tamping, casting, vibrating, or potting compounds. Both shaped and unshaped products are manufactured in a conventional manner from a coarse ceramic batch. Furthermore, a distinction is known between non-basic (Practical Handbook, 4.1) and basic refractory products (Practical Handbook, 4.2). According to DIN EN ISO 10081:2005-05, a distinction is made between non-basic and basic refractory products based primarily on their chemical reactivity. The non-basic product group includes materials of the SiO2-Al2O3 series and other materials that cannot be further classified according to their chemical reactivity, such as SiC and carbon products. A key characteristic of most basic products is that the sum of the oxides MgO and CaO predominates. Chromite, picrochromite, spinel, and forsterite bricks are also considered basic products, even though they are virtually neutral.Shaped basic products include, in particular, products containing magnesia, in particular magnesia products, magnesia chromite products, magnesia spinel products, magnesia zirconium products, magnesia pleonaster products, magnesia galaxite products, magnesia hercynite products, and magnesia doloma products (see, for example, the Practical Handbook, p. 99 / 100, Tables 4.26 and 4.27). Basic unshaped products are products whose aggregates consist primarily of magnesia, dolomite, chromium magnesia, chromium ore, and spinel (see, for example, the Practical Handbook, p. 146). Due to their basic nature and the high melting point of MgO, magnesia bricks exhibit high hot strength and good resistance to alkaline foreign substances. However, magnesia bricks are generally very brittle due to their relatively high modulus of elasticity (E-modulus) and unfavorable shear modulus (G-modulus). They are therefore sensitive to stress changes, especially due to thermal shock, and thus have a low thermal shock resistance (TSR). Therefore, efforts are being made to achieve lower elastic moduli to improve thermomechanical durability. For example, adding a so-called elasticizer or elasticizing component to the batch is known. Examples of elasticized products include magnesia chromite, magnesia spinel, magnesia zirconium, magnesia hercynite, and magnesia galaxite products, particularly bricks (Practical Handbook, page 101 / No. 1). The elasticizing component can also create the elasticizing products in the batch during ceramic firing. This is called in situ elasticization. In unfired products, in situ elasticization occurs during use. Elastifiers are granular, refractory, mineral materials, usually based on compounds of the base materials, which are typically contained in the batch in quantities of 3 to 30 mass% (= mass %) based on the sum of the elastifier and the main component. They generally cause microcracking in the matrix or structure of a refractory product formed from the batch at high temperatures and subsequent cooling due to different expansion coefficients. This elastification reduces the elastic modulus and shear modulus, and thus the brittleness of the ceramic product. This increases its resistance to thermal shock. Raw materials whose thermal expansion coefficients are significantly higher or lower than those of magnesia are used as elasticizers. Examples include chromium ores, raw materials from the spinel group (e.g., hercynite, pleonast, MA spinel), zirconium oxide, calcium hexaaluminate, and emery. An example of elasticized products are, as already explained, magnesia spinel bricks. Magnesia spinel bricks are fired basic products that mineralogically consist essentially of periclase (MgO) and spinel (MgO·Al2O3). According to classification, they contain at least 40 mass% MgO to distinguish them from spinel bricks. The MA spinel present in magnesia spinel bricks originates either from separate presynthesis or from in-situ formation from Al2O3 additives (aluminum raw materials) with the MgO of the magnesia raw material, e.g., sintered magnesia, during the brick firing process (Practical Handbook, Section 4.2.4.1). Magnesia, or a magnesia raw material, or a magnesia variety, is a raw material that predominantly (> 50 mass%) contains magnesium oxide (periclase). Magnesium carbonate and MA spinel are therefore not considered magnesia raw materials. Due to their chemical / mineralogical composition, magnesia spinel products are highly resistant to thermal shock. Due to their low Young's modulus and low G modulus compared to pure magnesia products, they are better able to dissipate thermal and mechanical stresses. Magnesia spinel products are therefore used to line the firing zones of rotary and shaft kilns for firing cement, lime, dolomite and magnesite. In this context, US Pat. No. 4,971,934 A discloses a refractory batch comprising at least 70 mass% MgO, 4 to 30 mass% Al2O3, and 1.4 to 7.5 mass% MnO2. At least a major portion of the Al2O3 is in the form of MgAl2O4 spinel, and the proportion of Al2O3 present in another form does not exceed 10 mass%. The magnesia raw material providing the MgO contains at least 90 mass% MgO, preferably 96 to 98 mass% MgO. The aluminum raw material providing the Al2O3 can also be pure alumina and / or bauxite, which is part of the coarse fraction of the batch. In this case, however, the two aforementioned raw materials provide no more than 10 mass% of the Al2O3 content of the total composition. The coarse fraction also has grain sizes of up to 4.7 mm. US 4,954,463 discloses a refractory batch for the in-situ formation of magnesium aluminate spinel, wherein the batch comprises 65 to 99 mass-% magnesia with an MgO content of at least 92 mass-% and 35 to 1 mass-% sintered bauxite with an Al2O3 content of at least 83 mass-% and an SiO2 content of less than 7 mass-%. The total SiO2 content of the batch is less than 4 mass-%. According to the examples in US 4,954,463, the batch contains 10 to 20 mass-% sintered bauxite with a grain size of less than 0.224 mm. DE 43 19 741 C2 discloses a process for producing refractory products based on magnesium oxide, starting from sintered and / or fused magnesia grains containing at least 95 mass% MgO. The magnesia grain is mixed with porous aluminum oxide grains of at least 0.5 mm in size, shaped, and fired. Calcined alumina is preferably used as the aluminum raw material. Tabular alumina and fused corundum are also listed. Preferably, the aluminum raw material also has an Al2O3 content of at least 97 mass%. Due to the high purity, high refractoriness of the bricks produced from it is ensured according to DE 43 19 741 C2. Furthermore, it is known from WO 2004 / 056718 A2 to use a calcium aluminate with a CaO / Al2O3 ratio between 0.14 and 0.2, in particular the chemical formula CaAl12O19, as an elasticizer component. The elasticizer component preferably has the oxide formula CaO·6Al2O3 or the abbreviation formula Ca6. According to WO 2007 / 096246 A2, a forsterite material or a mixture forming a forsterite material is used as an elasticizing additive. The object of the present invention is to provide a batch for producing a coarse ceramic refractory basic shaped product, wherein the product should have good thermal shock resistance and sufficient temperature resistance and should be producible cost-effectively. A further object of the invention is to provide a product made from the backfill, a use of the backfill, a method for its production and a lining of an industrial furnace with such a product and a use of such a lining. These objects are achieved by an offset having the features of claim 1, a use having the features of claim 21, a product having the features of claim 22, a method having the features of claim 34, a delivery having the features of claim 35, and a use having the features of claim 39. Advantageous developments of the invention are characterized in the respective subsequent subclaims. The invention is explained in more detail below using an example drawing. Shown are: Fig. 1: A light micrograph of an elasticizer grain formed from sintered bauxite in a brick according to the invention after the production firing. Fig. 2: Distribution of Al and Mg in an elasticizer grain formed from sintered bauxite in a brick according to the invention (left) and in an elasticizer grain formed from alumina in a brick not according to the invention (right). Fig. 3: Distribution of Ca and Si in the elasticizer grain formed from sintered bauxite in the brick according to the invention (left) and in the elasticizer grain formed from alumina in a brick not according to the invention (right). Within the scope of the invention, it was surprisingly found that it is possible to produce a magnesia spinel product with good mechanical and thermomechanical properties and sufficient refractoriness from a batch containing a mineral dry material mixture which contains an impure, granular magnesia component as the main component if an elasticizer component made of sintered bauxite is used for in situ elasticization. Impure means that the magnesia component consists of at least one magnesia with an MgO content of only < 90 mass%, particularly preferably < 89 mass%. According to the invention, the granular, impure magnesia component is contained in the dry matter mixture of the batch in an amount of ≥ 70 mass%, preferably ≥ 85 mass%. The MgO content of the impure magnesia is therefore preferably 85 to < 90 mass%, preferably 87 to < 89 mass%, according to the invention. Unless otherwise stated, the MgO content, the Al2O3 content, the SiO2 content and the content of accompanying oxides of the raw materials are determined by X-ray fluorescence analysis according to DIN EN ISO 12667:2013-2. Furthermore, at least one magnesia of the impure magnesia component is preferably a crushed grain. Preferably, the magnesia of the impure magnesia component consists exclusively of crushed grain(s). Refractoriness generally decreases when impure raw materials are used. This is because impure raw materials contain a relatively high proportion of accompanying oxides, secondary components, or impurities. Magnesia, in particular, contains CaO, SiO2, and Fe2O3 as accompanying oxides. These impurities can adversely influence the reactions taking place in situ during the firing process. The result is structural defects and reduced refractoriness. Cracking beyond the desired microcracks can lead to strength losses, which cause spalling during use. Therefore, experts are generally discouraged from using impure raw materials, even though they are generally more cost-effective. Within the scope of the invention, it has now surprisingly been discovered that a magnesia spinel product with good mechanical and thermomechanical properties and sufficient refractoriness can be obtained if a granular elasticizer component made of at least one sintered bauxite is used for in-situ MA spinel formation. According to the invention, the elasticizer component is contained in the dry matter mixture of the batch in an amount of 2 to 10 wt.%, preferably 3 to 8 wt.%, particularly preferably 4 to 6 wt.%, based on the dry matter of the dry matter mixture. In addition, according to the invention, the elasticizer component has a grain size according to DIN 66165-2:2016-08 ≤ 2.5 mm, preferably ≤ 2.0 mm. Furthermore, the invention has shown that the proportion of fines in the elasticizer component must not be too high, as the reactive proportion of fines can lead to a change in the mineral phase composition in the binder phase. According to the invention, the elasticizer component comprises grains with a grain size according to DIN 66165-2:2016-08 of ≤ 0.5 mm in a maximum amount of up to 25 mass%, preferably up to 20 mass%, particularly preferably up to 15 mass%. The amount of grains with a grain size according to DIN 66165-2:2016-08 of ≤ 0.5 mm is 0 to 25 mass%, preferably 0 to 20 mass%, particularly preferably 0 to 15 mass%. For the above-mentioned reason, the elasticizer component preferably also comprises grains with a grain size according to DIN 66165-2:2016-08 of ≤ 0.2 mm in a maximum amount of up to 10 mass%, preferably up to 7 mass%, particularly preferably up to 5 mass%. Or, the amount of grains with a grain size according to DIN 66165-2:2016-08 of ≤ 0.2 mm is 0 to 10 mass%, preferably 0 to 7 mass%, particularly preferably 0 to 5 mass%. In addition, the elasticizer component preferably comprises grains with a grain size according to DIN 66165-2:2016-08 of > 2 mm in a maximum amount of ≤ 25 wt.%, preferably ≤ 20 wt.%, particularly preferably ≤ 10 wt.%. The amount of grains with a grain size according to DIN 66165-2:2016-08 of > 2 mm is preferably 0 to 25 wt.%, preferably 0 to 20 wt.%, particularly preferably 0 to 10 wt.%. The above-mentioned quantities naturally refer to the total amount of elasticizer component. Furthermore, the at least one sintered bauxite is preferably also a crushed grain. Preferably, the elasticizer component comprises exclusively crushed grain(s). What was particularly surprising was that it is possible to produce a magnesia spinel product with good mechanical and thermomechanical properties and sufficient refractoriness from two impure raw materials, namely impure magnesia and an impure aluminum raw material, namely sintered bauxite. This is because sintered bauxite itself is an impure aluminum raw material compared to alumina and, according to the invention, has an Al2O3 content of only 70 to 92 mass %, preferably 78 to 91 mass %. Thus, due to the high proportion of accompanying oxides in both the magnesia raw material and the sintered bauxite, it would have been expected that good mechanical, thermomechanical properties and refractoriness could not be achieved. In the context of the invention, it was surprisingly also discovered that good properties cannot be achieved with purer aluminum raw materials. This will be discussed in more detail in the exemplary embodiments. Preferably, the at least one magnesia of the main component is sintered magnesia or fused magnesia. Preferably, it is sintered magnesia. In addition, the at least one magnesia of the main component preferably has the following properties, which can be realized individually or in any combination according to the invention: Table 1: Secondary oxide contents of the magnesia of the main component Table 1: Secondary oxide contents of the magnesia of the main component preferably SiO2 content [W%]0.5 to 30.7 to 2.5 CaO content [W%]0.5 to 41.0 to 3.5 Fe2O3 content [W%]0.2 to 10.00.5 to 9.5 MnO content [W%]0 to 1.50.1 to 0.7 Furthermore, the main component has a grain size distribution that is typical for the production of a coarse ceramic magnesia spinel product, preferably a magnesia spinel brick. This means that the main component has both a fine grain and a coarse grain fraction. Both the fine grain and the coarse grain fraction preferably have a consistent grain size distribution. For the purposes of this invention, the term "fine grain" refers to all grain sizes ≤ 1 mm. The term "coarse grain" refers to grain sizes > 1 mm. Preferably, the main component also has a maximum grain size ≤ 7 mm, preferably ≤ 6.5 mm. It is also advantageous if the impure magnesia has a high Fe2O3 content. It has been found that the magnesioferrite contained in magnesia is a stable phase that does not disrupt the microstructure. This can have a positive effect on strength and build-up behavior. The impure magnesia preferably has an Fe2O3 content of 0.2 to 10 wt.%, more preferably 0.5 to 9.5 wt.%. As already explained, the elasticizer component consists of at least one sintered bauxite (=refractory bauxite). Sintered bauxite is a significantly less pure aluminum raw material than, for example, alumina. It is therefore all the more surprising that the invention has shown that significantly better properties can be achieved in the products manufactured from the backfill using sintered bauxite than using alumina. At the same time, sintered bauxite is also a relatively inexpensive aluminum raw material. The at least one sintered bauxite of the elasticizer component preferably has the following properties, which can be realized individually or in any combination according to the invention: Table 2: Properties of the sintered bauxite of the elasticizer component Table 2: Properties of the sintered bauxite of the elasticizer component preferably SiO2 content [M.-%]4 to 206 to 15 CaO content [W%]0.1 to 1.50.2 to 0.5 Fe2O3 content [W%]0.5 to 40.9 to 2 TiO2 content [W%]0.5 to 42 to 3.5 In principle, it can be assumed that the fire resistance decreases with increasing CaO and / or SiO2 content, so that the expert is actually prevented from using such a raw material as an elasticizing component. In addition, the elasticizer component has a grain size distribution within the specified range. The grain size distribution is preferably continuous. Furthermore, the batch according to the invention can contain, in addition to the main component, another granular magnesia component. The other magnesia component consists of at least one magnesia with a higher MgO content than the MgO content of the main component. The other granular magnesia component is preferably present in the dry matter mixture in an amount of 5 to 28 mass%, more preferably 10 to 22 mass%, based on the dry matter of the dry matter mixture. The average MgO content of all magnesia types of the dry mixture taken together, i.e. the main component and, if present, the other magnesia component taken together, is preferably 85 to 91.5 mass%, preferably 87 to 90 mass%, particularly preferably 87 to 89 mass%. Or the average MgO content of all magnesia types of the dry mixture taken together, i.e. the main component and, if present, the other magnesia component taken together, is according to the invention ≤ 91.5 wt.%, preferably ≤ 90 wt.%, more preferably ≤ 89 wt.%. Furthermore, the at least one magnesia of the further granular magnesia component is also preferably a crushed grain. Preferably, the further granular magnesia component comprises exclusively crushed grain(s). Preferably, the dry material mixture contains only broken grain(s). In particular, all magnesia types taken together—that is, the main component and, if present, the other magnesia component—have a preferably continuous grain distribution typical for the production of a coarse ceramic magnesia spinel product, preferably a magnesia spinel brick. This means that the magnesia types together have both a fine grain and a coarse grain portion. Both the fine grain and the coarse grain portion preferably have a continuous grain distribution. Preferably, the magnesia types also have a maximum grain size of ≤ 7 mm, preferably ≤ 6.5 mm. The CaO / SiO2 ratio of all components of the dry mixture taken together is preferably 1.2 to 3.0, more preferably 1.5 to 2.5. To determine the CaO / SiO2 ratio of all components, the CaO or SiO2 content of the individual components is summed, and the CaO / SiO2 ratio is calculated from this. The average MnO content of all components of the dry batch is preferably < 1.0 mass%, more preferably < 0.8 mass%. Preferably, the batch does not contain any raw material that consists mainly of MnO or MnO2 or Mn2O3. As already explained, it has surprisingly been found that refractory products made from the batch according to the invention have good thermal shock resistance (TSR), low elastic and G moduli as well as good cold compressive strength and good cold bending strength while at the same time being good fire resistance. For the production of the refractory product, the batch according to the invention can contain at least one dry or solid binder in addition to or as an additive to the mineral dry material mixture. "Additive" means that the amount of binder is added additively and refers to the total dry mass of the dry material mixture. The batch according to the invention preferably contains the dry binder in a total amount of 0 to 4 mass%, preferably 0 to 3 mass%, based on the dry mass of the dry substance mixture. At least one dry binder is a binder suitable for refractory products. These binders are listed, for example, in the practical handbook, page 28, section 3.2. In addition, the batch may also contain, in addition to or in addition to the mineral dry material mixture, at least one dry additive for refractory materials, preferably in a total amount of < 5 mass% (= 0 to < 5 mass%), preferably < 3 mass% (= 0 to < 3 mass%), based on the dry material mixture. The dry additive is an additive suitable for refractory products. The additive can be mineral or chemical. Suitable additives are listed, for example, in the practical handbook, page 28 / section 3.3. They are used to improve workability or formability or to modify the structure of the products and thus achieve special properties. However, the batch preferably contains no additive. It goes without saying that the proportion of the dry matter mixture in the batch is sufficiently high to produce a magnesia spinel product. The batch according to the invention preferably consists of at least 90 wt.%, preferably at least 95 wt.%, particularly preferably at least 98 wt.%, and in particular 100 wt.% of the dry matter mixture, based on the total mass of the batch. For the production of shaped magnesia spinel products, in particular magnesia spinel bricks, from the batch according to the invention, a mixture or molding compound or fresh batch compound is prepared from the dry batch with at least one liquid binder and / or water. If the batch contains a liquid binder, the addition of water is not necessary but possible. Furthermore, the addition of a liquid binder is not necessary but possible if the batch contains at least one dry binder. The total amount of liquid binder in the fresh batch mass or pressing mass is preferably 2 to 6 mass%, preferably 3 to 5 mass%, based on the dry mass of the dry material mixture. Preferably, the at least one liquid binder is a binder from the following group: thermosetting synthetic resin binder, in particular phenol-formaldehyde resin, or molasses or ligninsulfonate, or a sulfur-free binder, in particular a binder based on dextrose, an organic acid, sucrose, an Al2O3 binder, phosphoric acid, a phosphate binder, water glass, ethyl silicate, or a sulfate, e.g. magnesium sulfate or aluminum sulfate, or a sol-gel system. If necessary, at least one liquid additive can also be added, which is also added to the dry substance mixture. The liquid additive is, for example, a wetting agent. The total amount of liquid additive in the fresh batch mass is preferably < 1.0 M% (= 0 to < 1 M%), preferably < 0.5 M% (= 0 to < 0.5 M%), based on the dry mass of the dry substance mixture. For optimal distribution of the binder(s) and / or water and, if applicable, at least one additive, mixing is carried out for 3 to 10 minutes. The mixture is poured into molds and pressed to form molded bodies. The pressing pressures are within the usual ranges, e.g., 60-180 MPa, preferably 100-150 MPa. Preferably, drying is carried out after pressing, e.g., between 60 and 200 °C, in particular between 90 and 140 °C. Drying is preferably carried out to a residual moisture content of between 0.1 and 0.6 mass %, in particular between 0.2 and 0.5 mass %, determined in accordance with DIN 51078:2002-12. The molded bodies according to the invention, in particular the bricks, can be used unfired, tempered, or fired. However, they are preferably used fired. The green pressed bricks are tempered in a ceramic kiln, e.g. a tunnel kiln, between 200 and 800 °C, especially between 500 and 800 °C. For firing, the preferably dried, pressed bricks are ceramically fired in a ceramic kiln, e.g., a tunnel kiln, preferably between > 800 and 1800 °C, especially between 1400 and 1700 °C. Oxidative firing is preferred, but depending on the material composition, a reducing firing may also be advantageous. The fired, shaped products, in particular the bricks, have a very good cold compressive strength according to DIN EN 993-5:1998-12, preferably from 40 to 120 MPa, in particular 50 to 90 MPa. The cold bending strength according to DIN EN 993-6:1995-04 of the fired, shaped products according to the invention, in particular the bricks, is preferably 3 to 10 MPa, in particular 4 to 7 MPa. In addition, the fired, shaped products, in particular the bricks, preferably have a compression softening point T0.5 according to DIN EN ISO 1893: 2008-09 of 1100 to 1750 °C, preferably 1200 to 1600 °C. Furthermore, the fired, shaped products, in particular the bricks, preferably have a compression Zmax at 1700°C according to DIN EN ISO 1893: 2008-09 of 0.5 to 5 lin%, preferably 1 to 4 lin%. In addition, the fired, shaped products according to the invention, in particular the bricks, preferably have an E-modulus (elasticity modulus) of 15 to 35 GPa, preferably of 18 to 30 GPa. The G-modulus (shear modulus) of the fired, shaped products according to the invention, in particular the bricks, is preferably 7 to 16 GPa, more preferably 8 to 14 GPa. The E-modulus and G-modulus were determined using the GrindoSonic MK6. The thermal shock resistance determined according to DIN EN 993-11:2008-03 with air at an elevated test temperature of 1200 °C of the fired, shaped products according to the invention, in particular the bricks, is preferably > 30 quenching cycles, in particular > 50 quenching cycles. The fired, shaped products, in particular the bricks, also preferably have an open porosity of 12 to 28 vol.%, preferably 13 to 20 vol.%, determined according to DIN EN 993-1:1995-04. And / or they preferably have a bulk density of 2.60 to 3.15 g / cm3, in particular of 2.75 to 3.10 g / cm3, determined according to DIN 993-1:1995-04. All of the above-mentioned properties of the products according to the invention are inventive individually and in any combination. The good mechanical and thermal properties result primarily from the fact that no structural defects occur during firing. This is also demonstrated by the fact that no significant volume increase occurs during firing. The invention is illustrated by the following examples: In a first series of tests, bricks made from two different types of magnesia with an MgO content of > 94 mass% were produced as comparative examples. Clay (BSA = Brown Sintered Alumina) with an Al2O3 content of 96.5 mass% was used as the elasticizer component. In a second series of tests, bricks made from impure magnesia with an MgO content of < 88 wt.% were used as further comparison examples. Alumina with an Al2O3 content of 96.5 wt.% was again used as the elasticizer component. In a third series of tests, bricks made from the two pure magnesia grades and the impure magnesia were produced as comparative examples. Two different sintered bauxites with an Al2O3 content of 90.5 wt.% and 79.6 wt.%, respectively, and a grain size of 0-1 mm were used as the elasticizer component. In a fourth series of experiments, bricks according to the invention were produced from the impure magnesia and the two sintered bauxites with grain fractions according to the invention. The properties of the raw materials used are listed in the following tables: Table 3: Properties of the magnesia raw materials used Table 3: Properties of the magnesia raw materials used Grain density Dg / cm 33,283,193,33 chemical analysis mass-% SiO20.892.110.58 Al2O30,140,480,26 Fe2O30,840,998,05 Cr2O30,010,020,01 MnO0.080.070.46 TiO20,010,020,01 P2O50,180,110,05 CaO2,201,682,57 MgO95.5894.4887.95 Na2O0.020.020.02 G-Loss0,110,120,18 C+S3,093,793.15 C / S2,470,804.43 Table 4: Properties of the aluminum raw materials used Table 4: Properties of the aluminum raw materials used Grain density Dg / cm 33,503,203,07 chemical analysis mass-% SiO20.904.5713.57 Al2O396.5090.4779.64 Fe2O30.151.641.81 MnO0.010.010.01 TiO21,202,903,20 P2O50,020,070,29 CaO0.010,030.55 MgO0.300.050.22 Na2O0.300.020.06 G-Loss0.050.120.18 The bricks were manufactured as follows: A molding compound was prepared from the respective batch. Mixing was carried out for 4 minutes to ensure optimal distribution of the binder. The molding compound was poured into molds and pressed to form bricks. After pressing, they were dried at 110 °C for 8 hours to a residual moisture content of 0.1 mass%, determined according to DIN 51078:2002-12. The bricks were then fired using oxidation. The batches used and the properties of the resulting bricks are listed in the following tables. For sintered bauxite and alumina, the specified grain sizes are grain fractions, while for magnesia, they are grain groups: Table 5: Batches and results of test series 1 Table 5: Batches and results of test series 1 Firing temperature 1430°C 1430 °C Offset No.:V1aV1b Binder: Lignosulfonate (45% conc.) 3,6 3,6 Formatmm70 / 65x200x22070 / 65x200x220 Press pressureMPa180180 DBM12-427.0 DBM11-220.0 DBM10-114.0 DBM1 Flour 34.0 DBM22-427.0 DBM21-220.0 DBM20-114.0 DBM2 flour 34.0 Clay 96.50.5-1.05,05,0 CommentSTATE OF THE ART no cracksSTATE OF THE ART no cracks Finished density g / cm 32,922,80 E ModulGPa24.0216.04 G ModulGPa11,418,15 KDFMPa87,2551,45 KBFMPa6,144,36 PorosityVol%16.6819.23 TWB, air, 1200°C cycles1 / - / >301 / - / >30 Shrinkagelin%-0.28-1.84 DE:Dmaxlin%1,791,51 T0°C15561331 T06°C-1471 T1°C-1523 T2°C-1601 T5°C-- Zmax (1700 °C)lin%0.214.76 Table 6: Offsets and results of test series 2 Table 6: Offsets and results of test series 2 Firing temperature 1430°C 1430°C 1430°C 1430°C Offset No.:V2aV2bV2cV2d BinderLignosulfonate (45% conc.)3,63,63,63,6 Formatmm70 / 65x200x22070 / 65x200x22070 / 65x200x22070 / 65x200x220 Press pressureMPa180180180180 DBM 2 Flour 20,020,020,020,0 DBM 32-428,028,028,028,0 DBM 31-223,023,023,023,0 DBM 30-114,015,016,017,0 DBM 3 Flour 10,010,010,010,0 Bauxite 10.5-1.6 Bauxite 10.5-1.0 Clay 96.50.5-1.05,04,03,02,0 Comment UNSTABLE STONE STRUCTURES / STONE DAMAGE slight cracks Finished density g / cm 32,932,922,922,98 E ModuleGPa14,1114,7815,3823,27 G Modulus GPa 7,437,678,0911,67 KDFMPa47,0048,6544,1562,30 KBFMPa3,913,403,954,56 PorosityVol%17.4517.3918.1516.62 TWB. Air, 1200°C cycles1 / - / >301301301 / - / >30 Shrinkagelin%-1.06-1.64-1.44-0.56 DE:Dmaxlin%1.51n. bnbnb T0°C1298 (not determined due to structural defects / cracks) T05°C1449 T1°C1499 T2°C1565 T3°C Zmax (1700 °C)lin%4.72 Table 8: Offsets and results of test series 4 Table 8: Offsets and results of test series 4 Firing temperature 1430°C 1430°C 1430°C 1430°C 1430°C 1430°C 1430°C Offset No.:V4aV4bV4cV4dV4eV4fV4g Binder: Lignosulfonate (45% conc.) 3,63,63,63,43,63,63,6 Formatmm70 / 65x200x22070 / 65x200x22070 / 65x200x22070 / 65x200x22070165x200x22070 / 65x200x22070 / 65x200x220 Pressing pressureMPa180180180120180180180 DBM 2Flour20,020,020,020,020,020,020,0 DBM 32-428,028,028,028,028,028,028,0 DBM 31-223,023,021,523,022,023,023,0 DBM 30-116,014,514,516,012,014,014.0 DBM 3Flour10,010,010,010,010,010,010,0 Bauxite 12-2.51,0 Bauxite 11-21.0 Bauxite 10.5-1.66.0 Bauxite 10.5-14,04,54,08,02,0 Bauxite 10.2-0.51.0 Bauxite 22-2.51,0 Bauxite 21-21.0 Bauxite 20.5-12.0 Bauxite 20.2-0.51.0 INVENTIVE STONES no cracksno cracksno cracksno cracksno cracksno cracksno cracksno cracks FRDg / cm 33,043,033,022,972,993,033.02 E ModuleGPa25,3622,2819,1021,0616,4323,3723,38 G ModuleGPa12,8811,5810,1810,689,4613,7414,08 KDFMPa102,9595,5083,4075,3085,5599,3595,10 KBFMPa5,885,234,684,634,715,705,58 PorosityVol%14.9214.5614.8517.0216.0514.9114.86 TWB, air, 1200 C cycles1 / - / >302 / - / >302 / - / >301 / - / >301 / - / 301 / - / >301 / - / >30 Shrinkagelin%0.130.250.080.33-0.280.210.28 DE:Dmaxlin-%1,761,711,631,801,681,671,65 T0°C1358134213401324136413321328 T0.5°C1578148115241481151315421511 T1°C1653155015331549157216131581 T2°C-164716761633166717001637 T5°C------- Zmax (1700 °C)lin.-%1,532,352,493,833,362,043.47 The results of test series 1 show that bricks with good mechanical properties and good refractoriness could be easily produced from the two pure magnesia types and the alumina. The bricks in test series 2, made from impure magnesia and alumina, surprisingly did not exhibit good mechanical strength. The bricks grew significantly during firing. This led to significant structural defects (cracks). Due to these structural defects, the bricks did not exhibit good strength. In test series 3 it was shown that when using sintered bauxites with too fine grains in combination with impure magnesia, sufficient refractoriness could not be achieved. In test series 4, numerous bricks according to the invention with good mechanical properties and good refractoriness were produced. The sintered bauxite content was varied. Furthermore, only grain fractions with a low proportion of grain sizes < 0.5 mm were used. During the production firing, the bricks according to the invention shrank moderately. The strengths of the bricks according to the invention correspond to typical magnesia spinel bricks. The refractoriness (compression softening) is advantageous for a brick intended for the firing zone of an industrial furnace, as such thermoplastic behavior can be utilized for use in mechanically stressed furnaces. Within the scope of the invention, it is assumed that the surprisingly good properties of the inventive bricks result, among other things, from the formation of a transition zone (=reaction zone) between the MgO matrix and the elasticizer grains. To confirm this, the bricks were examined using light microscopy, X-ray diffraction, and micro-X-ray fluorescence spectrometry. Analysis of the individual elasticizer grains using micro-X-ray fluorescence spectrometry allows spatial resolution of the elemental distribution. Figure 1 shows a light micrograph of an elasticizer grain 1 formed from sintered bauxite with 90.5 wt.% Al2O3 in an MgO matrix 2 of a brick according to the invention. Clearly visible are an inner ring 3 and an outer ring 4, which have formed around the elasticizer grain 1 and form the transition zone and reaction zone, respectively. Pores 5 are also visible. The results of X-ray powder diffraction are shown in the following table: Test CommentV2a not according to the inventionV4b according to the invention Periclase (M)++++++++ Spinel (MA)++ Corundum (A)±± Magnesioferrite (MF)++ Belite (C2S)±± Merwinite (C3MS2)±± Hibonite (CA6)±- ++++ = main phase + = detected ± = trace - = not detected From the results of X-ray diffraction and micro-X-ray fluorescence spectrometry, it can be deduced that the inner ring 3 contains spinel, which formed during firing through a reaction between the magnesia and the elasticizer grain 1 at its edge. The outer ring also contains the impurities and accompanying oxides contained in the sintered bauxite. It is assumed that the reaction between the elasticizer grain 1 and the magnesia is stopped due to the formation of the outer ring 4, thus preventing the volume increase during firing and thus preventing damage to the bricks. X-ray powder diffraction also showed that, due to the high CaO content in the brick with the alumina, not only in-situ spinel but also hibonite (CA6) was formed. The formation of hibonite (CA6) is generally undesirable because it leads to an increase in volume. The results of micro-X-ray fluorescence spectrometry indicate that hibonite (CA6) was formed in the transition zone. In contrast, no hibonite (CA6) was detectable in the brick according to the invention. Figures 2 and 3 show the distribution of Al, Mg, Ca, and Si in and around an elasticizer grain made of sintered bauxite with 90.5 wt.% Al2O3 (left) and in and around an elasticizer grain made of alumina (left) after ceramic firing at 1430 °C, determined by micro-X-ray fluorescence spectrometry. For comparability, the same scale (at.%) was used to represent the respective elements in both cases. Depending on the aluminum raw material used, differences in the formation of the respective transition zone can be seen. In the case of alumina, the area between the chemically almost unchanged core and the outer ring of spinel is significantly wider than in the case of sintered bauxite. In the case of alumina, an enrichment of CaO and SiO2 is particularly noticeable in the transition zone. In the alumina, a calcium aluminate zone (10-14% CaO) has also developed, which is surrounded by a CaO-free rim of MA spinel (34% MgO). SiO2 is enriched in the calcium aluminate zone (up to 2.8%), but not in the surrounding ring of MA spinel. In sintered bauxite, a continuous decrease in SiO2 content can be observed from the center to the edge. The enrichment of CaO in the transition zone is significantly less pronounced than in alumina. Here, too, a ring of MA spinel is present. The SiO2 content within the elasticizer grain in sintered bauxite varies between 12 and 22%. Comparatively low Al2O3 contents indicate that, in addition to the X-ray-detected MA spinel phase, significant amounts of melilite (C2AS) and merwinite (C3MS2) were formed, which may be present as a melt phase at the selected firing temperatures. In the case of sintered bauxite, the activity of CaO is presumably reduced by the SiO2 content in the raw materials through the formation of melt phases and / or calcium magnesium silicates or calcium aluminum silicates. This prevents the undesirable formation of hibonite (CA6) and prevents an increase in volume during firing.The sintered bauxite buffers the reaction to hibonite (CA6) through the formation of secondary phases and is therefore less reactive.
Claims
Dry batch for the production of a coarse ceramic, refractory, shaped, fired or unfired magnesia spinel product, comprising a dry material mixture consisting of a) a granular magnesia component of at least one magnesia with an MgO content of < 90 wt.% as the main component in an amount of ≥ 70 wt.%, b) a granular elasticizer component in an amount of 2 to 10 wt.% of at least one sintered bauxite with an Al2O3 content of 70 to 92 wt.%, wherein the elasticizer component has a grain size according to DIN 66165-2:2016-08 ≤ 2.5 mm, and the elasticizer component contains grains with a grain size according to DIN 66165-2:2016-08 of ≤ 0.5 mm, maximum in an amount of ≤ 25 wt.% andc) optionally a further granular magnesia component comprising at least one magnesia having a higher MgO content than the main component, the average MgO content of all magnesia types of the dry substance mixture taken together being ≤ 91.5 mass%. Batch according to claim 1, characterized in that the MgO content of the at least one magnesia of the main component is < 89 mass%. Batch according to claim 1 or 2, characterized in that the main component is contained in the dry substance mixture in an amount ≥ 85 mass%. Batch according to one of the preceding claims, characterized in that the elasticizer component is contained in the dry substance mixture in an amount of 3 to 8 mass%, preferably 4 to 6 mass%. Offset according to one of the preceding claims, characterized in that the elasticizer component has a grain size according to DIN 66165-2:2016-08 of ≤ 2 mm. Batch according to one of the preceding claims, characterized in that the elasticizer component has grains with a grain size according to DIN 66165-2:2016-08 of ≤ 0.5 mm in a maximum amount of ≤ 20 mass%, preferably ≤ 15 mass%. Batch according to one of the preceding claims, characterized in that the elasticizer component has grains with a grain size according to DIN 66165-2:2016-08 of ≤ 0.2 mm in a maximum amount of ≤ 10 mass%, preferably ≤ 7 mass%, more preferably ≤ 5 mass%. Batch according to one of the preceding claims, characterized in that the elasticizer component has grains with a grain size according to DIN 66165-2:2016-08 of > 2 mm in a maximum amount of ≤ 25 mass%, preferably ≤ 20 mass%, more preferably ≤ 10 mass%. Batch according to one of the preceding claims, characterized in that the MgO content of the at least one magnesia of the main component is 85 to < 90 mass%, preferably 87 to < 89 mass%. Batch according to one of the preceding claims, characterized in that the at least one sintered bauxite has an Al2O3 content of 78 to 91 mass%. Batch according to one of the preceding claims, characterized in that the average MgO content of all magnesia types of the dry material mixture taken together is 85 to 91.5 mass%, preferably 87 to 90 mass%, particularly preferably 87 to 89 mass%. Batch according to one of the preceding claims, characterized in that the average MgO content of all magnesia types of the dry material mixture taken together is ≤ 90 mass%, preferably ≤ 89 mass%. Batch according to one of the preceding claims, characterized in that the CaO / SiO2 ratio of all components of the dry substance mixture taken together is 1.2 to 3.0, preferably 1.5 to 2.
5. Batch according to one of the preceding claims, characterized in that the dry substance mixture comprises the further magnesia component in an amount of 5 to 28 mass%, preferably 10 to 22 mass%. Batch according to one of the preceding claims, characterized in that the batch does not contain any MnO, MnO2, or Mn2O3 raw material. Batch according to one of the preceding claims, characterized in that the batch comprises at least one dry binder and / or at least one dry additive in addition to the dry substance mixture. Batch according to one of the preceding claims, characterized in that the batch consists of at least 90 wt.%, preferably at least 95 wt.%, more preferably at least 98 wt.%, particularly preferably 100 wt.%, of the dry substance mixture, based on the total dry mass of the batch. Offset according to one of the preceding claims, characterized in that the elasticizer component comprises exclusively broken grain(s). Batch according to one of the preceding claims, characterized in that the dry material mixture comprises exclusively broken grain(s). Batch according to one of the preceding claims, characterized in that the grain size distribution of the main component and / or the grain size distribution of the elasticizer component and / or the grain size distribution of the further granular magnesia component and / or the grain size distribution of all magnesia types of the dry material mixture taken together is continuous. Use of a batch according to one of the preceding claims for producing a coarse ceramic, refractory, shaped, fired or unfired magnesia spinel product, in particular a magnesia spinel product of a working lining or backing of a large-volume industrial furnace, preferably a cement kiln plant, a lime shaft or lime rotary kiln, a magnesite or dolomite kiln, or a heating furnace or a furnace for energy generation or a furnace for steel production or a furnace for the non-ferrous metal industry. Coarse ceramic, refractory, shaped or unshaped, fired or unfired magnesia spinel product, in particular for a working lining or backing of a large-volume industrial furnace, preferably a cement kiln plant, a lime shaft kiln or lime rotary kiln, a magnesite kiln or dolomite kiln, or a heating furnace or a furnace for energy generation or a furnace for steel production or a furnace in the non-ferrous metal industry, characterized in that the product is made from a molding compound containing the batch according to one of claims 1 to 20 and at least one liquid binder and / or water. Product according to claim 22, characterized in that the liquid binder is a binder from the following group: a thermosetting synthetic resin binder, in particular phenol-formaldehyde resin or molasses or ligninsulfonate, or a sulfur-free binder, in particular a binder based on dextrose, an organic acid, an Al2O3 binder, phosphoric acid, a phosphate binder, water glass, ethyl silicate, or a sulfate, e.g. magnesium sulfate or aluminum sulfate, or a sol-gel system. Product according to claim 22 or 23, characterized in that the shaped product is a green, in particular pressed, shaped body, preferably a stone. Product according to claim 22 or 23, characterized in that the shaped product is a tempered shaped body, preferably a stone. Product according to claim 22 or 23, characterized in that the shaped product is a fired shaped body, preferably a stone. Product according to claim 26, characterized in that the fired shaped body, preferably the stone, has an E-modulus of 15 to 35 GPa, preferably 18 to 30 GPa. Product according to claim 26 or 27, characterized in that the fired shaped body, preferably the stone, has a G-modulus of 7 to 16 GPa, preferably of 8 to 14 GPa. Product according to one of claims 26 to 28, characterized in that the fired shaped body, preferably the stone, has a cold compressive strength according to DIN EN 993-5:1998-12 of 40 to 120 MPa, in particular of 50 to 90 MPa. Product according to one of claims 26 to 29, characterized in that the fired shaped body, preferably the stone, has a cold bending strength according to DIN EN 993-6:1995-04 of 3 to 10 MPa, in particular of 4 to 7 MPa. Product according to one of claims 26 to 30, characterized in that the fired shaped body, preferably the stone, has a compression softening point T0.5 according to DIN EN ISO 1893: 2008-09 of 1100 to 1750 °C, preferably of 1200 to 1600 °C. Product according to one of claims 26 to 31, characterized in that the fired shaped body, preferably the stone, has an open porosity of 12 to 28 vol.%, preferably 13 to 20 vol.%, determined according to DIN EN 993-1:1995-04. Product according to one of claims 26 to 32, characterized in that the fired shaped body, preferably the stone, has a compression Zmax at 1700°C according to DIN EN ISO 1893: 2008-09 of 0.5 to 5 lin%, preferably 1 to 4 lin%. A process for producing a refractory shaped product according to any one of claims 22 to 33, characterized by the following process steps: a) mixing the batch with at least one liquid binder and / or water to form a molding compound, b) molding, in particular pressing, the molding compound to form a green molded body, c) preferably drying the green molded body, preferably to a residual moisture content of between 0.1 and 0.6 mass%, in particular between 0.2 and 0.5 mass%, determined in accordance with DIN 51078:2002-12, d) preferably tempering or firing the green molded body. Lining of a large-volume industrial furnace, preferably a kiln in the non-metal industry, preferably a cement kiln plant, a lime shaft kiln or lime rotary kiln, a magnesite kiln or dolomite kiln, or a heating furnace or a furnace for energy generation or a furnace for steel production or a furnace in the non-ferrous metal industry, characterized in that the lining comprises at least one product according to one of claims 22 to 33 and / or manufactured according to claim 34. A lining according to claim 35, characterized in that the lining comprises a working lining which comprises the at least one refractory product. Delivery according to claim 36, characterized in that the working lining is installed in a single or multi-layer masonry. A lining according to any one of claims 35 to 37, characterized in that the lining comprises an insulating backing which comprises the at least one refractory product. Use of a lining according to one of claims 35 to 38 for a large-volume industrial furnace, preferably a kiln in the non-metal industry, preferably a cement kiln plant, a lime shaft kiln or lime rotary kiln, a magnesite kiln or dolomite kiln, or a heating furnace or a furnace for energy production or a furnace for steel production or a furnace in the non-ferrous metal industry.
Citation Information
Patent Citations
Process for the production of refractory products based on magnesium oxide
DE4319741C2
Refractory composition
US4971934A
Heavy ceramic moulded body, method for producing said body and use of the same
WO2004056718A2
Fire-resistant ordinary ceramic batch, and fire-resistant product therefrom
WO2007096246A2
Magnesium aluminate spinel refractory
US4954463A