Compression stabilizer Battery separator

DE102020109571B4Active Publication Date: 2024-10-02CARL FREUDENBERG KG
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
DE102020109571
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-04-06
Publication Date
2024-10-02
Estimated Expiration
2040-04-06

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Battery separator with a substrate, preferably open-pored, in particular a nonwoven fabric according to DIN EN ISO 9092 (2018-02) as the base body, wherein the base body has a coating containing filler particles in a proportion of 80 wt. % to 98 wt. % and binder in a proportion of 2 wt. % to 10 wt. %, each based on the coating weight, wherein the filler particles have a particle size distribution with a d50 according to ISO 21501-3 of 0.05 µm to 10 µm and a particle size distribution range ((d90-d10) / d50) of 0.05 to 3.5, characterized in that the coating has penetrated at least partially into the pores of the base body.
Need to check novelty before this filing date? Find Prior Art

Description

Technical area The invention relates to a battery separator containing filler particles and binder, as well as to its use as a substrate for coating with a laminating binder and as an electrical insulation material in an electrochemical cell. The invention further relates to an electrode separator unit containing the battery separator, as well as to an electrochemical cell containing the electrode separator unit according to the invention. State of the art In electrochemical cells, the positively and negatively charged electrodes are mechanically separated from each other by a non-electrically conductive layer, the battery separator, to prevent internal short circuits. The porous structure of a separator enables the transport of ionic charges, a prerequisite for continuous current draw during battery operation. Fundamental requirements for battery separators include chemical and electrochemical stability with respect to the active electrode materials and the battery electrolyte. At the structural level, high porosity is required to accommodate the electrolyte and ensure high ionic conductivity. At the same time, the pore size and channel structure must effectively suppress the growth of metal dendrites to avoid short circuits, as described in the Journal Power Sources 2007, 164, 351-364. A disadvantage of common battery separators is that they often drastically lose their porosity under pressure loads, as described in Journal of Power Sources 196 (2011) 8147 - 8153, and thus the conductivity of the separator deteriorates. Particularly high compressive loads on the separator occur in electrode pairs with a high volume change during the charging / discharging process, e.g. in silicon-containing anodes and when the separator is laminated onto a battery electrode. EP3357114A4 describes a silicon-carbon composite anode consisting of 40 wt.% to 80 wt.% silicon particles and its use in a lithium-ion battery. This document does not describe how the separator can compensate for the volume increase of the electrodes, especially the anodes, during cycling. A laminated separator is described in EP2750216B1. The battery separator consists of a microporous, multilayer polymer film and exhibits good thermal stability up to 135°C, low areal shrinkage in the xy plane (<20% up to 130°C), and good adhesion to the electrode. However, this separator loses its porosity due to the use of a polyolefin membrane during the lamination process. The polyolefin-based separators described in EP2924781A1 and EP3244475A1 also do not have satisfactory compression resistance. Maintaining the adjusted porosity, even under pressure and temperature loads, is a great advantage, as this is the only way to ensure a permanently low ion transport resistance. This is known as compression stability. In particular, high compression stability must be ensured against the compression forces acting on the separator during the battery cell manufacturing process and during operation. EP 2 978 045 A1 describes a slurry for a porous membrane of a lithium-ion secondary battery, comprising non-conductive particles and a particulate polymer. Also described is a separator for a lithium-ion secondary battery, comprising an organic separator layer and a porous membrane. A porous substrate with micropores can be used as the organic separator layer. Examples of the organic separator layer include microporous membranes and nonwoven fabrics. The nonwoven fabrics are filled with polyolefin resins, such as polyethylene resin, polypropylene resin, or aromatic polyamide resins. The use of a separator layer containing the smallest possible pores (micropores) is important because it can prevent short circuits between the electrodes in a secondary battery.For this reason, substrates that already have micropores (microporous membranes) or nonwovens whose pore size has been reduced by a polymer filling are proposed. It is undesirable for the slurry to penetrate the separator layer, as this would reduce the conductivity of the separator layer, which occurs via the free pores. US 2010 / 0 173 187 A1 describes a separator comprising a microporous polyolefin membrane, at least one surface of which is laminated with a heat-resistant porous layer containing a heat-resistant resin having an inorganic filler. The inorganic filler has an average particle diameter of 0.1 to 1 µm. Smaller particle sizes are disadvantageous, as otherwise the inorganic filler can trickle out of the separator as a powder. The pore sizes of the membrane are specified as 3.0 to 30 nm (0.003 to 0.03 µm). Due to the small pore size of the membrane relative to the inorganic filler, the coating does not penetrate into the pores of the base body, i.e., the polyolefin membrane. Zhang, Sheng Shui, Journal of Power Sources, Vol. 164, 2007, No. 1. pp. 351-364 describes a review of separators for liquid electrolyte Li-ion batteries. The invention is therefore based on the object of providing a separator which makes it possible to adjust the porosity set in it to a defined extent even under high pressure and temperature loads. Description of the invention This object is achieved by a battery separator with a preferably open-pore substrate, preferably a fiber-based substrate, in particular a nonwoven fabric according to DIN EN ISO 9092 (2018-02) as the base body, wherein the base body has a coating which contains filler particles in a proportion of 80 wt.% to 98 wt.% and binder in a proportion of 2 wt.% to 10 wt.%, in each case based on the coating weight, wherein the filler particles have a particle size distribution with a d50 according to ISO 21501-3 (2019-11) of 0.05 µm to 10 µm and a particle size distribution range (SPAN) ((d90-d10) / d50) of 0.05 to 3.5 and wherein the coating has at least partially penetrated into the pores of the base body. Surprisingly, it was discovered according to the invention that the battery separator can maintain its adjusted porosity even under pressure and temperature stresses. This ensures a low ionic conductivity. Furthermore, the specific particle size distribution range in the battery separator according to the invention enables the adjustment of a defined compressibility. Without committing to a specific mechanism, it is assumed that this is made possible by the interaction of the particles and their defined size distribution creating cavities between the particles (interstitial volumes). These cavities are interconnected by particle-to-particle contact and, in the case of fiber-containing base bodies such as nonwovens, particle-to-fiber contact and fiber-to-fiber contact. These cavities do not completely collapse under the temperature and pressure loads typically encountered in battery separators. For example, the battery separator according to the invention is stable up to temperatures of 150°C, more preferably up to 170°C, particularly preferably 200°C, and / or at pressures of up to 0.3 MPa, preferably up to 2.5 MPa, even more preferably up to 5.0 MPa, very particularly preferably up to 15 MPa, and / or pressing forces of up to 500 N, preferably up to 1500 N, particularly preferably up to 4000 N. According to the invention, the term interstitial volume is geometrically distinguished from the pore volume in that the interstitial volume forms concave surfaces at its boundary to the filler particles contained in the battery separator, while a pore volume forms convex surfaces at the interface, each seen from the reference system of the free volume. Electrolyte can be permanently present in these interstitial volumes, which, due to the connected interstitial volumes, leads to a high coherent ionic conductivity across the entire thickness (Z-direction) of the battery separator and promotes a low internal resistance of the cell. Another advantage of the battery separator according to the invention is that it contains a high proportion of filler particles relative to the binder content. Due to the high degree of filling with filler particles, these can form a continuous, coherent particle structure that encloses the substrate. This, in turn, has a beneficial effect on the temperature and pressure stability of the interstitial volume. In particular, the high proportion of filler particles enables the formation of volume elements in the battery separator that, in their z-direction, consist essentially only of filler particles and the interstitial volumes formed thereby. This allows high pressures to be absorbed by the filler particles on one side of the battery separator and transferred directly to the other side without the geometry of the battery separator being undesirably impaired or the porosity completely collapsing. Conversely, an endless, continuous interstitial volume filled with electrolyte can be formed, which is protected from deformation and closure by the temperature and pressure stability of the filler particles and ensures constant ionic conduction between anode and cathode. According to the invention, the base body has a coating. According to the invention, this means that the coating can be present flatly on the base body. According to the invention, the coating also penetrates at least partially into the pores of the base body in the manner of a filling. Particularly preferably, the coating is in the form of a continuous filling. The coating can be present on one or both sides of the base body. In a preferred embodiment of the invention, 10 vol.% to 65 vol.%, more preferably 15 vol.% to 60 vol.%, and in particular 30 vol.% to 50 vol.% of the battery separator according to the invention form volume elements that consist essentially only of filler particles in their z-direction. This increases the compression stability of the battery separator according to the invention. The proportion of these volume elements in the battery separator can be determined using radiometric measurement methods. According to the invention, the battery separator comprises an open-pore substrate. An open-pore substrate is understood to be a substrate that has at least a portion of the pores accessible from the substrate surface. According to the invention, more than 50% of the pores are preferably accessible from the substrate surface. In particular, the pores of the open-pore substrate should be able to accommodate filler particles and / or enable the in-situ deposition of filler. According to the invention, the filler particles have a particle size distribution with a d50 value (measured according to ISO 21501-3 (2019-11)) of 0.05 µm to 10 µm, more preferably from 0.05 µm to 2 µm, more preferably from 0.1 µm to 2 µm, more preferably from 0.1 µm to 1.0 µm, more preferably from 0.2 µm to 1.0 µm, in particular from 0.3 µm to 0.5 µm. Practical tests have shown that these particle size distributions particularly favor the formation of pores with a small mean pore size, measured according to DIN ISO 4003:1990, preferably from 0.01 µm to 1.5 µm, more preferably from 0.1 µm to 0.7 µm, and especially from 0.3 µm to 0.5 µm. The aforementioned particle size distributions and pore diameters are particularly advantageous for preventing dendrite growth in Li-ion batteries while simultaneously ensuring high ionic capability. According to the invention, the filler particles have a particle size distribution range ((d90-d10) / d50) of 0.05 to 3.5, preferably from 0.1 to 3.5, preferably from 0.1 to 3.0, even more preferably from 0.2 to 3.0, even more preferably from 0.2 to 2.5, even more preferably from 1.0 to 2.5, even more preferably from 1.2 to 2.5, in particular from 1.2 to 2.0. Practical tests have shown that particularly high interstitial volumes with a narrow pore size distribution are formed within these particle size distribution ranges. The battery separator according to the invention advantageously has a pore size distribution with an average pore size, measured according to DIN ISO 4003:1990, of 0.25 µm to 0.5 µm. The adjustment of specific particle size distribution ranges can be achieved in various ways, e.g. by sieving for powders or filtering for dispersions. Practical tests have shown that the particle sizes and particle size distribution ranges according to the invention result in a particularly compression-stable battery separator with a high interstitial volume. In a preferred embodiment of the invention, the battery separator has an interstitial volume, as defined in the "Standards and Measurement Methods" section, of more than 25 vol.%, for example, from 25 vol.% to 75 vol.%, more preferably from 40 vol.% to 70 vol.%, and in particular from 45 vol.% to 65 vol.%. The advantage of a high interstitial volume is the high electrolyte uptake of the battery separator, which in turn correlates with a high ionic conductivity of the electrolyte-impregnated battery separator.Without committing to a specific mechanism, it is assumed that the advantageous effects of setting a high interstitial volume result from the fact that, with the particle size distribution ranges according to the invention, smaller particles are less able to settle into the interparticle spaces formed by larger particles, and these spaces can therefore absorb an unusually large amount of electrolyte. The interparticle spaces can be determined using porosity measurements (air permeability according to Gurley). The air permeability according to Gurley correlates with the isobaric air flow through the separator and thus provides information about the porosity of the separator and consequently about its interstitial volume. Another advantage of a high interstitial volume is that solvents, such as water, can escape very easily when the battery separator is dried. This is particularly important for laminated products, e.g.An electrode / battery separator / electrode laminate is relevant. The conductive effect of the battery separator against the solvents is advantageous here. Since the planar diffusion path in the z-direction is not available due to the impermeable conductor materials in these laminates, the planar laminated battery separator can absorb the solvent residues from the electrodes in the laminate and, via its interstitial volumes, conduct them particularly quickly to the laminate edges, from where the solvent residues can escape from the laminate. According to the invention, the battery separator has an open-pore substrate, preferably an open-pore fiber-based substrate, as the base body. In the following, unless stated otherwise, reference is made to the substrate itself, i.e. in the uncoated state. The use of a nonwoven fabric is particularly preferred. However, the use of papers, woven fabrics, knitted and / or crocheted fabrics is also conceivable. Furthermore, the use of foams, membranes, films, in particular stretched films, perforated films, track-etched films, mechanically or laser-perforated films, micro-lithographed films is conceivable. The advantage of using a nonwoven fabric is that low basis weights and low thicknesses can be achieved in a simple manner. Furthermore, an isotropic fiber distribution can be achieved.This is advantageous because the fiber-to-fiber interstitial volumes are also distributed isotropically, and thus the ionic conductivity can also be isotropically achieved through electrolyte deposition. This ensures homogeneous Li-ion migration in the final product. The nonwoven fabric is preferably a wet-laid nonwoven fabric. This is advantageous because the wet-laid process allows for extremely low basis weights and thicknesses while maintaining high homogeneity and mechanical stability. The thickness of the open-pore substrate, in particular the nonwoven fabric, can be further reduced by calendering. Therefore, a calendered nonwoven fabric, in particular a calendered wet-laid nonwoven fabric, is particularly preferred according to the invention. In a preferred embodiment, the thickness of the open-pore substrate is from 2 µm to 50 µm, more preferably from 3 µm to 30 µm, in particular from 5 µm to 15 µm, measured according to EN 29073 - T2. A low thickness is advantageous because it promotes a high volumetric energy density of the battery. The basis weight of the open-pore substrate, preferably the fiber-based substrate, in particular the nonwoven fabric, measured according to EN 29073 - T1, is preferably from 2 g / m2 to 30 g / m2, more preferably from 4 g / m2 to 20 g / m2, even more preferably from 4 g / m2 to 15 g / m2, and in particular from 4 g / m2 to 10 g / m2. A low basis weight of the open-pore substrate is advantageous because it promotes a high gravimetric energy density of the battery. The porosity of the open-pored substrate, preferably the fiber-based substrate, in particular the nonwoven fabric, is preferably from 40 vol.% to 90 vol.%, more preferably from 50 vol.% to 80 vol.%, in particular from 55 vol.% to 70 vol.%. As mentioned above, the porosity refers to the substrate itself, i.e. in the uncoated state. The advantage of high porosity is that large volumes are available for coating with filler particles. This in turn increases compression stability. In a preferred embodiment of the invention, the open-pored substrate has a pore volume in which from 20 vol.% to 75 vol.%, more preferably from 25 vol.% to 65 vol.% and in particular from 30 vol.% to 60 vol.% belong to z-through pores. As mentioned above, the porosity refers to the substrate itself, i.e. in the uncoated state. The open-pore substrate preferably has z-shaped through-pores. Z-shaped through-pores are defined as pores that are uninterrupted by substrate material in the z-direction. This can be determined, for example, using image analysis methods. This is advantageous because it allows volume elements to form in the battery separator that essentially consist only of filler particles in their z-direction, which increases compression stability. The fiber-based substrate, particularly in its embodiment as a wet-laid nonwoven fabric, can comprise staple fibers and / or short-cut fibers. According to the invention, staple fibers are understood to mean fibers with a limited length of preferably 1 mm to 80 mm, more preferably 3 mm to 30 mm, in contrast to filaments, which have a theoretically unlimited length. According to the invention, short-cut fibers are understood to mean fibers with a length of preferably 1 mm to 12 mm, more preferably 3 mm to 6 mm. The average linear density of the fibers of the fiber-based substrate can vary depending on the desired structure of the substrate. The use of fibers with an average linear density of 0.02 dtex to 3.3 dtex, preferably 0.04 dtex to 1.7 dtex, preferably 0.06 dtex to 1.0 dtex, has proven particularly advantageous. The fibers can be formed in a wide variety of shapes, for example, as flat, hollow, round, oval, trilobal, multilobal, bico, and / or island-in-the-sea fibers. According to the invention, the cross-section of the fibers is preferably round or oval, since this inevitably creates a gusset volume at the points of contact between the fiber-fiber and fiber-particle surfaces, regardless of their geometric orientation. According to the invention, the fibers can contain a wide variety of fiber polymers, preferably polyacrylonitrile, polyvinyl alcohol, viscose, cellulose, polyamides, polyimides, especially polyamide 6 and polyamide 6.6, polyesters, especially polyethylene terephthalate and / or polybutylene terephthalate, copolyesters, polyolefins, especially polyethylene and / or polypropylene, and / or mixtures thereof. Polyesters, especially polyethylene terephthalate and / or polybutylene terephthalate, and / or polyolefins, especially polyethylene and / or polypropylene, are preferred. The advantage of using polyesters is that they exhibit high mechanical strength. Advantageously, the fiber-based substrate comprises matrix fibers, i.e., fibers that are essentially unfused in the substrate. The matrix fibers preferably have a melting point of above 160°C, preferably above 200°C, in particular above 250°C, and / or a decomposition point of above 250°C, in particular above 350°C. These improve the structural stability of the fiber-based substrate under pressure and / or temperature loads and lead to low areal shrinkage, preferably down to 200°C. The proportion of matrix fibers in the fiber-based substrate is advantageously from 5 to 70 wt.%, preferably from 5 to 50 wt.%, in particular from 5 to 35 wt.%, based on the total weight of the fiber-based substrate. This is advantageous because in this range, very high geometric stability against the aforementioned loads and very high structural homogeneity are achieved. Practical tests have shown that the at least partial use of matrix fibers with an average linear density of less than 1 dtex, preferably from 0.02 dtex to 1 dtex, has a beneficial effect on the size and structure of the pore sizes and inner surface as well as on the density of the nonwoven fabric. The fiber-based substrate also preferably comprises binding fibers, i.e. fibers that are at least fused in the substrate. The fibers customarily used for this purpose can be used as binding fibers, provided they can be at least partially thermally softened and / or fused. Binding fibers can be uniform fibers or multi-component fibers. Binding fibers that are particularly suitable according to the invention are fibers in which the binding component has a melting point that is below the melting point of the matrix fibers to be bound, preferably below 250°C, more preferably from 70 to 235°C, even more preferably from 125 to 225°C, particularly preferably from 150 to 225°C. Suitable fibers are, in particular, thermoplastic polyesters and / or copolyesters, in particular polybutylene terephthalate (PBTP), polyolefins, in particular polypropylene, polyamides, polyvinyl alcohol, and copolymers and mixtures thereof. In a preferred embodiment, the difference between the melting or decomposition point of the matrix fiber on the one hand and the melting point of the binding fibers on the other hand is at least 30 °C, for example from 30 °C to 60 °C. Particularly suitable binding fibers according to the invention are multi-component fibers, preferably bi-component fibers, in particular core / sheath fibers. Core / sheath fibers contain at least two fiber polymers with different softening and / or melting temperatures. The core / sheath fibers preferably consist of these two fiber polymers. The component with the lower softening and / or melting temperature is found on the fiber surface (sheath), and the component with the higher softening and / or melting temperature is found in the core. In core / sheath fibers, the binding function can be performed by the materials arranged on the surface of the fibers. A wide variety of materials can be used for the sheath. Preferred materials for the sheath according to the invention are polybutylene terephthalate (PBT), polyamide (PA), polyethylene (PE), copolyamides, and / or copolyesters.A wide variety of materials can also be used for the core. According to the invention, preferred materials for the core are polyester (PES), in particular polyethylene terephthalate (PET) and / or polyethylene naphthalate (PEN) and / or polyolefins (PO). The use of core-shell binding fibers is preferred according to the invention, since this allows a particularly homogeneous distribution of the binding agent component in the nonwoven fabric to be achieved. The use of core-shell binder fibers is particularly advantageous. In these fibers, the sheath has a lower melting point than the core. Core-shell binder fibers with a sheath having a melting point below 240°C, preferably between 200°C and 225°C, and a core with a melting point and / or decomposition point above 240°C, preferably between 250°C and 270°C, are preferred. The advantage of a comparatively high melting point is that the battery separator according to the invention can be dried at higher temperatures. Also preferred are core-shell binder fibers having a sheath having a melting point of below 160°C, preferably from 100°C to 150°C, and a core having a melting point of above 160°C, preferably from 160°C to 170°C. The use of undrawn binding fibers is also advantageous. In practical tests, nonwovens with very good properties were obtained using PET-PBT bicomponent fibers and / or PET-CoPES bicomponent fibers. Good results were also achieved with fibers from the polyolefin class, particularly polyethylene-polypropylene bicomponent fibers. PEN-PET bicomponent fibers are also suitable. However, the use of monocomponent binding fibers is also conceivable, provided they can be at least partially thermally softened. The choice of monocomponent binding fibers depends on the matrix fiber used. For example, polyamide 6 binding fibers are suitable for binding polyamide 66 matrix fibers, and copolyester, PBT, or undrawn binding fibers are suitable for binding polyethylene terephthalate fibers. The use of undrawn binding fibers is particularly preferred because they can be used to produce particularly thin nonwovens. The average linear density of the binding fibers can vary depending on the desired structure of the nonwoven fabric. The use of binding fibers with an average linear density of 0.2 to 2.2 dtex, preferably 0.5 to 1.3 dtex, has proven advantageous. The advantage of comparatively thick binding fibers is that during compression in the Z-direction, the binding fibers absorb the majority of the mechanical forces, thus relieving the matrix fibers of the compressive load and preventing the matrix fibers from being pressed into the interstice. This applies particularly to matrix fibers with a lower linear density than the binding fibers. The binding fibers can be bonded to each other and / or to the matrix fibers of the nonwoven fabric by thermofusion. Bonding by means of hot air flow in an oven has proven particularly suitable. The proportion of binding fibers in the fiber-based substrate is advantageously from 95 wt.% to 50 wt.%, preferably from 95 wt.% to 65 wt.%, in particular from 95 wt.% to 65 wt.%, based on the total weight of the fiber-based substrate. This is advantageous because in this range a very high mechanical strength of the entire fiber substrate is achieved, which has a positive effect on compression stability. In an advantageous embodiment, the fiber-based substrate comprises nanofibers. These have diameters of less than 1 µm and are advantageous because they increase the homogeneity of the fiber-based substrate. Furthermore, compared to fibers with a larger titer, they have a larger fiber surface area per weight, which leads to a higher proportion of fiber-fiber and fiber-particle interweaving volumes for a comparable proportion of the substrate. The proportion of nanofibers in the fiber-based substrate is advantageously from 0.1 wt.% to 20 wt.%.%, more preferably from 0.1 wt.% to 10 wt.%, based on the total weight of the fiber-based substrate. This is advantageous because, particularly in the aforementioned ranges, high homogeneity, high mechanical stability, and high geometric stability against pressure and temperature loads can be achieved while simultaneously achieving high additional interlacing volume compared to fibers with a higher titer. The use of semi-crystalline and / or crystalline fibers is particularly advantageous. The crystalline regions in the fibers generally exhibit a higher compression modulus than amorphous fibers, which promotes high compression stability of the fiber-based substrate. In one embodiment of the invention, the fiber-based substrate is bonded with a fiber binder. Preferred fiber binders are crosslinked fiber binders. These can be produced, for example, from crosslinking polymer solutions and dispersions. Crosslinked acrylate-based fiber binders are particularly preferred. The proportion of the fiber binder in the fiber-based substrate is advantageously from 5 wt.% to 50 wt.%, more preferably from 10 wt.% to 40 wt.%, in particular from 15 wt.% to 35 wt.%, based on the total weight of the fiber-based substrate. According to the invention, the battery separator contains filler particles. Filler particles, in contrast to binder particles, are particles that, in isolated form, exhibit no or only insignificant adhesion forces, at least among themselves, i.e., without a binder. The filler particles can be present in and / or on one or both surfaces of the substrate. They are advantageously distributed homogeneously in the xy and / or z directions. This configuration can particularly effectively prevent short circuits and dendrite growth. Furthermore, the battery separator according to the invention can exhibit particularly uniform compression stability. This, in turn, has a positive effect on the battery's cycle stability. It is advantageous if all pores of the open-pore substrate are homogeneously filled with the filler particles. The particles preferably have a particle size distribution in which the d50 value, and more preferably the d90 value, of the filler particles is smaller than the average pore size of the substrate. The filler particles can be organic, inorganic particles, or mixtures thereof. Preferred organic particles are selected from the group consisting of polypropylene, polyvinylpyrrolidone, polyester, polyamide, polytetrafluoroethylene, polyvinylidene difluoride, perfluoroethylene-propylene, polystyrene, polyacrylate, polyimide, and copolymers of the aforementioned polymers and mixtures thereof. Particularly preferred organic particles are selected from the group consisting of polypropylene, polyvinylpyrrolidone, and mixtures thereof. Suitable inorganic filler particles include, for example, metal oxides, metal hydroxides, and silicates. Preferred inorganic particles are selected from the group consisting of aluminum oxide, aluminum oxide hydroxide, silicon oxide, aluminosilicates, zeolites, zirconium oxide, titanium dioxide, magnesium oxide, phosphates, fluorides, and mixtures thereof. Particularly preferred inorganic particles are aluminum oxide, aluminum oxide hydroxide, silicon oxide, zirconium oxide, and mixtures thereof. Very particularly preferred inorganic particles are aluminum oxide, aluminum oxide hydroxide, and zirconium oxide, as these are particularly corrosion-resistant in common battery electrolytes. Chemically doped particles of the above materials are also suitable. The filler particles are preferably Na or Li ion-conductive organic and inorganic materials. The filler particles are preferably at least partially ion-conductive, so that they can make a partial contribution to the overall conductivity of the separator. Hard filler particles that do not reduce the separator's compression stability are particularly preferred. These include, in particular, garnet, nasicon, lisicon materials, and perovskites. Mechanically soft materials such as sulfide glass ceramics are unsuitable. These would reduce compression stability. According to the invention, the filler particles are preferably present in a proportion of 80 wt.% to 98 wt.%, more preferably from 90 wt.% to 98 wt.%, in particular from 92 wt.% to 97 wt.%, based on the total weight of the coating. It has been found that particularly high compression stability can be achieved with these proportions. Further preferably, the filler particles are present in a proportion of 50 wt.% to 90 wt.%, even more preferably from 60 wt.% to 85%, in particular from 65 wt.% to 80 wt.%, based on the total weight of the battery separator according to the invention. In a preferred embodiment of the invention, the Mohs hardness of the filler particles is from 2 Mohs to 10 Mohs, more preferably from 5 Mohs to 10 Mohs, and in particular from 7 Mohs to 9 Mohs. A high Mohs hardness of the filler particles increases the compression stability of the battery separator according to the invention. According to the invention, the coating comprises binder in a proportion of 2 wt.% to 10 wt.%, more preferably from 2 wt.% to 8 wt.%, in particular from 3 wt.% to 7 wt.%, based on the total weight of the coating. The advantage of using binder in a proportion of less than 10 wt.% is that it can create a high interlock volume. In a preferred embodiment, the binder is in particle form. The binder particles preferably have a particle size distribution with a d50 value of the binder particles (measured according to ISO 21501-3) of 0.01 µm to 7 µm, more preferably of 0.02 µm to 2 µm, in particular of 0.05 µm to 1 µm. With the aforementioned values, the average particle size of the binder particles is in the same order of magnitude as that of the filler particles. As a result, filler and binder particles are of a similar size, making geometric differentiation during the formation of the interstitial volume impossible or difficult. Since the binder particles can preferentially occupy the same lattice sites as the filler particles, penetration of the binder particles into the interstitial volume between the filler particles can be reduced. In addition, the binder particles integrated into the lattice structure, due to their inherently higher flexibility, specifically absorb compression loads and thus enable adjustable compressibility of the battery separator according to the invention. Adjustable compressibility is particularly advantageous in combination with highly breathable electrodes, since these are subject to significant volume changes during charging / discharging processes.Due to the adjustable compressibility, the battery separator according to the invention can at least partially compensate for volume changes in the electrodes during battery formation and cycling. This can reduce the mechanical stress in the battery during construction and use. The binder is preferably an organic binder. Preferred binders are selected from the group consisting of polyvinylidene difluoride and its copolymers, polyolefins, for example polyethylene, polyacrylates, for example perfluoropolyacrylate, polymethacrylate, polystyrene-butadiene, acrylonitrile-butadiene copolymers, and mixtures thereof. Preferred organic binders are selected from the group consisting of polypropylene, polyethylene, polystyrene butadiene polypropylene, polyethylene, polyvinylidene difluoride and mixtures thereof. In the case of binder particles, the binder is preferably chemically cross-linked. This is advantageous because it reduces the tendency of the binder to form a film and thus negatively impacts the interlock volume to a lesser extent under thermal or pressure loads. In another embodiment, the binder is a binder applied in the form of a solution, dispersion, and / or emulsion. This is advantageous because the binder in this form can be processed particularly well with the filler particles to form a homogeneous coating paste, which promotes homogeneity in the final product. In a further embodiment of the invention, the binder is present as a mixture of binder particles and binder applied in the form of a solution, dispersion, and / or emulsion. The proportion of binder particles, based on the total weight of the binder, is preferably in the range from 40 wt.% to 95 wt.%, more preferably from 60 wt.% to 90 wt.%, and in particular from 60 wt.% to 80 wt.%. Furthermore, the proportion of binder applied in the form of a solution, dispersion, and / or emulsion, based on the total weight of the binder, is preferably in the range from 5 wt.% to 60 wt.%, more preferably from 10 wt.% to 40 wt.%, and in particular from 20 wt.% to 40 wt.%. Preferred binders, which can be applied in the form of a solution, dispersion, and / or emulsion, are selected from the group consisting of carboxymethylcellulose, polyvinyl alcohol, polycarboxylate, polyacrylic acid, polyvinylpyrrolidone, and mixtures and copolymers thereof. Preferred copolymers are selected from the group consisting of copolymers of polyvinyl alcohol, polycarboxylate, polyacrylic acid, polyethylene oxides, polyethylene glycol, and polyvinylpyrrolidone. Preferably, the battery separator has a thickness, according to DIN EN 29073 - T2, of 3 µm to 70 µm, more preferably of 5 µm to 30 µm, in particular of 8 µm to 25 µm. Thicknesses of more than 10 µm are preferred, as the advantages of adjustable compressibility can be particularly well utilized here. Preferably, the battery separator has a weight, according to DIN EN 29073 - T1, of 3 g / m2 to 50 g / m2, preferably of 5 g / m2 to 35 g / m2, more preferably of 6 g / m2 to 35 g / m2 and in particular of 7 g / m2 to 35 g / m2. Preferably, the battery separator has average pore sizes, measured according to ASTM F 316, of 0.05 µm to 2 µm, preferably of 0.01 µm to 1 µm, more preferably of 0.15 µm to 0.75 µm. Preferably, the battery separator has an elongation in the machine direction, measured according to DIN EN 29073-3 (1992-08), of 5% to 50%, more preferably 6% to 30%, especially 8% to 20%. A low elongation of the battery separator is advantageous because it is more dimensionally stable and thus better retains its gusset volume during processing steps. Preferably, the battery separator has a maximum tensile force in the machine direction, measured according to DIN EN 29073-3 (1992-08), of 10 N / 5 cm to 60 N / 5 cm, more preferably of 10 N / 5 cm to 50 N / 5 cm, in particular of 14 N / 5 cm to 45 N / 5 cm. Preferably, the battery separator has a Gurley air permeability, measured according to ISO 5636-3, of 20 seconds to 350 seconds, more preferably of 30 seconds to 300 seconds, in particular of 50 seconds to 200 seconds. The air permeability according to Gurley correlates with the isobaric air flow through the separator and thus provides information about the porosity of the separator and consequently about its interstitial volume. Preferably, the battery separator, with a square surface, exhibits a surface shrinkage up to 200°C of 0 surface % to 10 surface % (preferably 0 surface % to 2 surface % and even more preferably 0.1 surface % to 1 surface %). A low surface shrinkage is advantageous because it offers safety benefits and the battery separator can also be processed, e.g., laminated and / or dried, at higher temperatures. In a preferred embodiment, the battery separator comprises the filler particles in a proportion of 50 wt.% to 90 wt.%, more preferably from 60 wt.% to 85 wt.%, in particular from 65 wt.% to 80 wt.%, and the binder in a proportion of 1 wt.% to 10 wt.%, more preferably from 1.2 wt.% to 8 wt.%, in particular from 1.3 wt.% to 3 wt.%, in each case based on the total weight of the battery separator. A further battery separator is described which contains filler particles in a proportion of 50 wt.% to 90 wt.%, more preferably from 60 wt.% to 85 wt.%, in particular from 65 wt.% to 80 wt.%, and binder in a proportion of 1 wt.% to 10 wt.%, more preferably from 1.2 wt.% to 8 wt.%, in particular from 1.3 wt.% to 3 wt.%, in each case based on the total weight of the battery separator, wherein the filler particles have a particle size distribution with a d50 according to ISO 21501-3 of 0.05 µm to 10 µm and a particle size distribution range ((d90-d10) / d50) of 0.1 to 3.5. The features described with respect to the further battery separator, in particular the preferred embodiments, can be transferred mutatis mutandis to the further battery separator according to the invention. The advantage of the additional battery separator is that it contains a high proportion of filler particles relative to the total weight of the battery separator. This means that the proportion of substrate and binder is comparatively low. This, in turn, has a positive effect on the temperature and pressure stability of the interstitial volume. A further object of the present invention comprises the use of the battery separator according to the invention as a substrate for coating with a laminating binder. In a preferred embodiment of the invention, the battery separator comprises a laminating binder on one or both surfaces, preferably selected from the group consisting of polyvinylidene difluoride, polyacrylate, perfluoroethylene propylene, carboxymethylcellulose, polyvinylpyrrolidone, polyethylene glycol, polyethylene oxide, and mixtures and copolymers thereof. Preferred copolymers are copolymers of polyvinylidene difluoride. Preferably, the laminating binder is thermoplastic. In this case, the thermoplastic laminating binder preferably has a melting point that is lower than the melting and / or decomposition point of the filler particles and / or, preferably, the fiber-based substrate. The laminating binder may also comprise filler particles, advantageously of the same type as in the coating. In a preferred embodiment, the area coverage of the battery separator surface with the laminating binder is from 0.01 area% to 50 area%, preferably from 5 area% to 35 area%, in particular from 10 area% to 35 area%. The area coverage can be determined by means of optical computer-assisted evaluation of microscopy images. The battery separator preferably comprises the laminating binder with a basis weight of 0.1 g / m2 to 5 g / m2, preferably 0.1 g / m2 to 4 g / m2, particularly preferably 0.2 g / m2 to 3 g / m2, particularly preferably 0.2 g / m2 to 2 g / m2, and in particular 0.5 g / m2 to 2 g / m2. A relatively low proportion of laminating binder is advantageous because, at these amounts, it does not penetrate into the interstice volume under normal laminating conditions and does not completely cover the surface of the battery separator. Both are advantageous because the ionic conductivity of the battery separator is thus less impaired. The laminating binder can be applied to the battery separator using various application methods, preferably coating methods such as doctor blade coating, roller coating, gravure coating, and slot die application. Electrospinning, spraying, electrostatic application, and / or powdering are also suitable. Application can be followed by a drying step. The battery separator provided with the laminating binder can be bonded to electrodes over a large area. For this purpose, a composite can be produced in the first step, consisting of one or more battery separators provided with the laminating binder and one or more electrodes. The battery separators and electrodes are preferably arranged alternately. Simultaneously or subsequently to the formation of the composite, the laminated composite can be laminated by activating the laminating binder, for example, using pressure, temperature, and / or solvent. Practical tests have shown that the battery separator according to the invention is particularly well suited to the stresses occurring during lamination due to its high pressure and temperature stability. The battery separator provided with the laminating binder is suitable for the production of electrode separator laminates. The present invention further provides an electrode-separator unit comprising a battery separator according to the invention and one or more battery electrodes. A battery electrode is an electrode that has a collector as a conductor for the electrical current and at least one active material as a storage device for electrical charge. In a preferred embodiment, the battery separator and one or more battery electrodes are connected to each other by means of a laminating binder. In one embodiment, the laminating binder is introduced into the electrode-separator unit on the electrode side, and in another embodiment, on the battery separator side. Preferred battery electrodes comprise lithium nickel manganese cobalt oxide (NMC), lithium cobalt oxide (LCO), lithium metal phosphates, such as lithium iron phosphate (LFP), lithium manganese oxide spinel (LMS), lithium nickel cobalt aluminum oxide (NCA), lithium and manganese-rich oxides (LMNO), and mixtures thereof as active materials. The aforementioned materials are particularly suitable for lamination with the battery separator and are particularly suitable as cathode material. Preferred battery electrodes include graphite (C), lithium metal (Li), lithium titanium oxide (LTO), silicon (Si), silicon / carbon composites (Si / C), tin (Sn), zinc (Zn), and mixtures thereof as active materials. The aforementioned materials are also particularly suitable for lamination with the battery separator and are particularly suitable as anode material. All of the aforementioned electrode materials can be combined with the battery separator according to the invention, even without the use of a laminating binder, to form an electrochemical cell. The use of the battery separator according to the invention in conjunction with silicon (Si) and silicon / carbon composite (Si / C) electrodes is particularly advantageous, as these exhibit a large volume change during a charge / discharge process, which in turn exerts high pressure on the battery separator. A further object of the present invention comprises the use of the battery separator according to the invention as an electrical insulation material in an electrochemical cell. Suitable electrochemical cells include Li- and / or Na-ion batteries, Prussian blue analog electrochemical cells and Li-ion capacitors. The present invention further relates to an electrochemical cell comprising the electrode-separator unit according to the invention and an electrolyte. The electrolyte can contain one or more organic or aqueous, preferably organic, solvents, one or more conducting salts, and one or more electrolyte additives. Liquid or gel-like electrolytes can be used. The use of the battery separator according to the invention is particularly advantageous when filling the electrochemical cell with the electrolyte, since the large and dimensionally stable interstitial volume enables rapid and uniform distribution of the electrolyte in the electrode-separator unit. This can significantly reduce the production time of the electrochemical cell. In a preferred embodiment, the electrochemical cell is designed as a fast-charging cell. A fast-charging cell is understood to be a cell that can be charged at charging rates (C-rate) of 2 C to 20 C, preferably from 3 C to 10 C, in particular from 4 C to 8 C. Since the cell temperature can rise significantly during such rapid charging, the battery separator according to the invention is particularly suitable for use in such fast-charging cells due to its thermal stability. A further advantage of using the battery separator according to the invention for the production of an electrochemical cell is its high temperature stability, which enables simple and rapid drying and thus high process speeds. This is particularly advantageous for integrated drying in the cell production process, since water residues can be reliably and quickly removed at high temperatures, e.g., 170°C. Standards and methods Measurement methods: With regard to the measurement methods, unless otherwise stated, reference is made in this description to the version valid on 1 March 2020 or, if no valid version is available at that time, to the most recently valid version. Basis weight: Based on test specification EN 29073 - T1, to determine the basis weights, three 100mm x 100mm samples are punched out, the samples are weighed and the measured value is multiplied by 100. Thickness: The thicknesses are measured according to test specification EN 29073 - T2. The measuring area is 2 cm2, and the measuring pressure is 1000 cN / cm2. Particle sizes and distribution: Performed according to ISO 21501-2:2019-11, without ultrasonic treatment. The measured light scattering was evaluated using Mie theory. Porosity: The porosities (P) in % are calculated according to the following formula: Here, the δ bulk density corresponds to the density of the separator calculated using the basis weight and thickness. The δpure density corresponds to the average density δaverage of the materials used according to their weight fraction in the separator, assuming 0% porosity. The average density can be calculated from the relative weight of the coating substrate, the relative weight of the coating layer, and the coating composition. Gusset volume: The gusset volume is determined according to ASTM D7854-16. Pore size: The pore sizes of the substrate, such as the mean pore size, are measured according to ASTM F 316. Air permeability according to Gurley: The air permeabilities are determined according to ISO 5636-3. Shrinkage: To determine the area shrinkage, 100 mm x 100 mm samples are punched out and stored for one hour at 150°C or 200°C in a Mathis Labdryer. The area shrinkage of the samples is then determined. Maximum tensile force: The maximum tensile strength (HZK) of the materials is determined according to EN 29073 T3. Melting point: Melting points and glass transition points are determined according to DIN 53765 (1994-03). C-Rate: The "C-rate" is a term used to specifically describe the charging and discharging process of a battery, independent of its capacity in Ah and the flowing current in amperes. A discharge rate of "1C" means the battery is completely discharged within one hour. A discharge rate of "2C" corresponds to a discharge within half an hour; a discharge rate of "10C" corresponds to a discharge within six minutes. Examples The invention is explained in more detail below using several examples. Example 1 - Production of several battery separators according to the invention and comparison battery separators Coating solution 1 (B1): To 160 parts of a 65% aluminum oxide dispersion (Al2O3) (d50 = 0.45 µm, SPAN = 1.5), 5 parts of a particulate binder dispersion (solids content = 25%), 10 parts of dissolved binder (20% solids content), and 38 parts of deionized water were added with stirring. The solution was stirred for 2 hours and tested for stability for at least 24 hours. The viscosity of the resulting solution was 80 mPa*s. Coating solution 2 (B2): To 148.5 parts of a 65% aluminum oxide dispersion (Al2O3) (d50 = 0.45 µm, SPAN = 1.62), 4.3 parts of a particulate binder dispersion (solids content = 25%), 12.3 parts of dissolved binder (20% solids content), and 38 parts of deionized water were added with stirring. The solution was stirred for 2 hours and tested for stability for at least 24 hours. The viscosity of the resulting solution was 50 mPa*s. Comparison coating solution 1 (VB1): To 141 parts of a 65% aluminum oxide dispersion (Al2O3) (d50 = 0.5 µm, SPAN = 7.8), 15 parts of a particulate binder dispersion (solids content = 50%), 10 parts of dissolved binder (10% solids content), and 38 parts of deionized water were added with stirring. The solution was stirred for 2 hours and tested for stability for at least 24 hours. The viscosity of the resulting solution was 61 mPa*s. Comparison coating solution 2 (VB2): To 136 parts of a 65% aluminum oxide dispersion (Al2O3) (d50 = 0.58 µm, SPAN = 3.8), 20 parts of a particulate binder dispersion (solids content = 50%), 6.5 parts of dissolved binder (20% solids content), and 47 parts of deionized water were added with stirring. The solution was stirred for 2 hours and tested for stability for at least 24 hours. The viscosity of the resulting solution was 140 mPa*s. Example 1A An 80 cm wide, wet-laid PET nonwoven fabric (thickness: 17 µm, basis weight: 8 g / m²) was continuously coated with coating solution 1 using a roll coating process and dried at a temperature gradient from 125°C to 165°C. A coated nonwoven fabric with a basis weight of 33 g / m² and a thickness of 22 µm was obtained. The mean pore size (MFP) of the coated nonwoven fabric was 0.35 µm. The Gurley value (100 ml) was 98 seconds. Example 1B An 80 cm wide, wet-laid PET nonwoven fabric (thickness: 15 µm, basis weight: 6 g / m²) was continuously coated with coating solution 1 using a roll coating process and dried at a gradient from 125°C to 160°C. A coated nonwoven fabric with a basis weight of 27 g / m² and a thickness of 19 µm was obtained. The mean pore size (MFP) of the coated nonwoven fabric was 0.4 µm. The Gurley value was 75 seconds (100 ml). Example 2A An 80 cm wide, wet-laid PET nonwoven fabric (thickness: 15 µm, basis weight: 8 g / m²) was continuously coated with coating solution 2 using a roll coating process and dried at a gradient from 125°C to 165°C. A coated nonwoven fabric with a basis weight of 33 g / m² and a thickness of 23 µm was obtained. The mean pore size (MFP) of the coated nonwoven fabric was 0.4 µm. The Gurley value was 90 seconds (100 ml). Example 2B An 80 cm wide, wet-laid PET nonwoven fabric (thickness: 17 µm, basis weight: 9 g / m²) was continuously coated with coating solution 2 using a roll coating process and dried at a gradient from 125°C to 165°C. A coated nonwoven fabric with a basis weight of 35 g / m² and a thickness of 26 µm was obtained. The mean pore size (MFP) of the coated nonwoven fabric was 0.33 µm. The Gurley value was 100 seconds (100 ml). Example 3A: Laminatable Battery Separator. An 80 cm wide battery separator (Example 1A) was continuously coated with a 10% PVDF dispersion using a roller coating process and dried at 135 °C. A coated battery separator with a basis weight of 35 g / m² and a thickness of 23 µm was obtained. The mean pore size (MFP) of the coated nonwoven was 0.35 µm. The Gurley value was 110 seconds (100 ml). Comparative example 1 (VB1A) An 80 cm wide, wet-laid PET nonwoven fabric (thickness: 19 µm, basis weight: 10 g / m2) was continuously coated with reference coating solution VB1 using a roll coating process and continuously dried with a gradient from 125°C to 165 °C. A coated nonwoven fabric with a basis weight of 34 g / m2 and a thickness of 26 µm was obtained. The Gurley value was 360 seconds (100 ml). Comparison example 2 (VB2A) An 80 cm wide, wet-laid PET nonwoven fabric (thickness: 19 µm, basis weight: 10 g / m2) was continuously coated with reference coating solution VB2 using a roll coating process and continuously dried with a gradient from 125°C to 165 °C. A coated nonwoven fabric with a basis weight of 32 g / m2 and a thickness of 29 µm was obtained. The Gurley value was 652 seconds (100 ml). Example 2 - Measurement of relevant physical properties Table 1. Summary of separator manufacturing results. Table 1. Summary of separator manufacturing results. Example 1A1,50,452233980,352612 Example 1B1,50,451927750,41910 Example 2A1,620,452333900,42811 Example 2B1,620,4526351000,333914 Example 3A1,50,4523351100,353012 VB1A7,80,526343600,23714 VB2A3,80,5829326520,164012 Table 1 shows that the inventive examples 1A to 3A have pore size distributions ranging from 0.25 µm to 0.5 µm and basis weights that are in some cases higher than those of the comparative examples, while simultaneously being thinner and having lower Gurley values. This shows that the coating solutions with SPAN values of 0.1 to 3.5, compared to the comparative coating solutions with higher SPAN values, produce a favorable interstitial volume for porosity and thus ionic conductivity. Example 3 - Cell characterization Various electrochemical cells are manufactured from the battery separators prepared in Example 1. All work is carried out in a glove box unless otherwise stated. The separators are dried in a vacuum at 150°C for 24 hours. The electrodes are dried in a vacuum at 80°C for 24 hours. NMC 111 (Al conductor) is used as the cathode, and graphite (Cu conductor) is used as the anode. The cathode capacity is approximately 72 mAh. The electrolyte is LP50 (800 µL). Unlaminated cells: Using battery separators 1A, 2A, 1B, 2B, VB1A, and VB2A, three-layer assemblies are produced, each consisting of an anode, separator, and anode. These are sealed in pouches, leaving one side open. This results in open cells. 800 µL of electrolyte is slowly added to the electrode-separator assembly, and the fourth side of the cells is sealed. After 24 hours, the cells are opened at one point, a vacuum is applied, and the cells are then resealed. Laminated cell (from 3A). The anode, separator, and cathode are laminated together at 160°C and a pressure of 3 bar. The laminate is then transferred to a glove box and dried at 120°C for 24 hours. The remaining procedure is the same as described previously under "unlaminated cells." Formation of cells: Charging cycle: • Charging (CC) with 0.1C to 4.2 Volts • Pause: 2 min • Charging (CV) at 4.2 V to I < 0.02C • Pause: 2 min • Discharging with 0.1C to 3.0V Repeat the charging cycle Cell tests: Cell life tests:The formed cells are charged and discharged in CCCV mode with 1C (3V / 4.2V). The results of the life tests are shown in Fig. 1. It can be seen that the cells manufactured with the battery separators according to the invention, and in particular those with 1A, 2A, and 1B, have a higher cycle stability and a longer lifespan than the comparative examples. It is particularly noteworthy that the cell manufactured with the battery separator 3A according to the invention shows such a good service life because it was laminated onto the electrodes using pressure.

Claims

Battery separator with a preferably open-pored substrate, in particular a nonwoven fabric according to DIN EN ISO 9092 (2018-02) as the base body, wherein the base body has a coating which contains filler particles in a proportion of 80 wt.% to 98 wt.% and binder in a proportion of 2 wt.% to 10 wt.%, in each case based on the coating weight, wherein the filler particles have a particle size distribution with a d50 according to ISO 21501-3 of 0.05 µm to 10 µm and a particle size distribution range ((d90-d10) / d50) of 0.05 to 3.5, characterized in that the coating has at least partially penetrated into the pores of the base body. Battery separator according to claim 1, characterized in that the filler particles have a particle size distribution with a d50 value (measured according to ISO 21501-3) of 0.05 µm to 2 µm, more preferably of 0.1 µm to 1 µm, in particular of 0.3 µm to 0.5 µm. Battery separator according to claim 1 or 2, characterized in that the filler particles have a particle size distribution range ((d90-d10) / d50) of 0.1 to 3.5, preferably from 0.1 to 3.0, more preferably from 0.2 to 3.0, more preferably from 0.2 to 2.5, more preferably from 1.0 to 2.5, more preferably from 1.2 to 2.5, in particular from 1.2 to 2.

0. Battery separator according to one or more of the preceding claims, characterized in that the battery separator has volume elements which in their z-direction consist essentially only of filler particles and the interstitial volumes formed therefrom. Battery separator according to one or more of the preceding claims, characterized in that the battery separator has a pore size distribution with an average pore size, measured according to DIN ISO 4003:1990, of 0.01 µm to 1.5 µm, preferably of 0.1 µm to 0.5 µm and in particular of 0.25 µm to 0.5 µm. Battery separator according to one or more of the preceding claims, characterized in that the battery separator has a gusset volume of 25 vol.% to 75 vol.%, more preferably of 40 vol.% to 70 vol.% and in particular of 45 vol.% to 65 vol.%. Battery separator according to one or more of the preceding claims, characterized in that the substrate is an open-pored substrate, preferably fabric, a foam, a membrane, film, in particular stretched film, perforated film, track-etched film, mechanically or laser-perforated film, microlithographed film, particularly preferably an open-pored fiber-based substrate, even more preferably a nonwoven fabric, in particular a wet-laid nonwoven fabric. Battery separator according to claim 7, characterized in that the fibers of the fiber-based substrate contain polyester. Battery separator according to claim 7 or 8, characterized in that the fibers of the fiber-based substrate have an average titer of 0.06 dtex to 3.3 dtex, preferably of 0.06 dtex to 1.7 dtex, preferably of 0.06 dtex to 1.0 dtex. Battery separator according to one or more of the preceding claims, characterized in that the filler particles are inorganic particles, in particular selected from the group consisting of aluminum oxide, aluminum oxide hydroxide, silicon oxide, aluminosilicates, zeolites, zirconium oxide, titanium dioxide, magnesium oxide and mixtures thereof. Battery separator according to one or more of the preceding claims, characterized in that the Mohs hardness of the filler particles is 2 Mohs to 10 Mohs, more preferably 5 Mohs to 10 Mohs and in particular 7 Mohs to 9 Mohs. Battery separator according to one or more of the preceding claims, characterized in that the filler particles are present in a proportion of 80 wt.% to 98 wt.%, more preferably of 90 wt.% to 98 wt.%, in particular of 92 wt.% to 97 wt.%, based on the total weight of the coating. Battery separator according to one or more of the preceding claims, characterized in that the coating comprises the binder in a proportion of 2 wt.% to 8 wt.%, in particular of 3 wt.% to 7 wt.%, based on the total weight of the coating. Battery separator according to one or more of the preceding claims, characterized in that the binder is present as a mixture of binder particles and binder applied in the form of a solution or dispersion. Battery separator according to one or more of the preceding claims, characterized by a thickness, according to DIN EN 29073 - T2, of 3 µm to 70 µm, more preferably of 5 µm to 30 µm, in particular of 8 µm to 25 µm. Battery separator according to one or more of the preceding claims, characterized by a temperature stability of up to 150 °C, more preferably up to 170 °C, particularly preferably up to 200 °C, and / or a pressure stability of up to 0.3 MPa, preferably up to 2.5 MPa, more preferably up to 5.0 MPa, very particularly preferably up to 15 MPa, and / or pressing force stability of up to 500 N, preferably up to 1500 N, particularly preferably up to 4000 N. Electrode separator unit comprising a battery separator according to one or more of the preceding claims, as well as one or more battery electrodes. Electrode separator unit according to claim 17, characterized in that the battery separator and one or more battery electrodes are connected to one another by means of a laminating binder. Use of a battery separator according to one or more of claims 1 to 16 as electrical insulation material in an electrochemical cell. Use of a battery separator according to one or more of claims 1 to 16 as a substrate for coating with a laminating binder. Electrochemical cell comprising an electrode-separator unit according to claim 17 or 18 and an electrolyte, preferably a liquid or gel-like electrolyte.

Citation Information

Patent Citations

  • Battery separator

    EP2750216B1

  • Method for producing electrode / separator laminate, and lithium-ion rechargeable battery

    EP2924781A1

  • Separation membrane comprising adhesive coating parts with different adhesion forces, and electrode assembly comprising same

    EP3244475A1

  • Silicon-carbon composite anode for lithium-]on batteries

    EP3357114A1

  • Slurry for lithium ion secondary battery porous film, production method therefor, separator for lithium ion secondary battery, and lithium ion secondary battery

    EP2978045A1