Metal powder for use in a selective laser beam melting process and selective laser beam melting process
A metal powder with an aluminum oxide particle shell enhances mechanical strength and conductivity in selective laser beam melting, addressing cost and defect issues in existing aluminum powders, producing high-strength, conductive 3D workpieces suitable for automotive and aviation.
Patent Information
- Application Number
- DE102023002159
- Authority / Receiving Office
- DE · DE
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-26
- Publication Date
- 2024-11-28
AI Technical Summary
Existing aluminum-based metal powders for selective laser beam melting face challenges such as high cost, oxidation, reflection, and softness, leading to defects and reduced mechanical and electrical properties in the resulting 3D workpieces.
A metal powder composed of an aluminum metallic phase with a surrounding aluminum oxide phase, where the oxide phase forms a particle shell that breaks upon laser fusion, creating strong particle fragments embedded in the metal lattice, enhancing mechanical strength and maintaining electrical conductivity.
The solution results in 3D workpieces with high strength and conductivity, suitable for automotive and aviation applications, while being cost-effective and recyclable, with minimal reduction in electrical properties and no oxide layer defects.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[0001] The invention relates to a metal powder for use in a selective laser beam melting process and to a selective laser beam melting process.
[0002] Additive manufacturing based on a previously generated 3D CAD model is known as such in various technologies. One technology gaining rapidly increasing importance is the layer-by-layer fusion of metal powders using a laser beam to produce a 3D workpiece. An important variant of this technology is the SLM (Selective Laser Melting) process, which produces a 3D workpiece directly and without subsequent sintering. The SLM process is also known as selective laser melting or powder-bed-based laser melting.
[0003] The mechanical, chemical and physical properties of the 3D workpiece, such as strength, surface quality, density or electrical conductivity, are significantly influenced by both the metal powder used and by laser process parameters such as laser power, laser speed, laser focusing, path guidance or the thickness of the respective layer.
[0004] To achieve good flow properties and a high packing density when preparing the layer to be fused in the powder bed, it is known that the metal powder particles should be formed as spherically as possible. To achieve this, the particles are held in an air vortex during atomization for as long as possible until solidification, allowing a substantially spherical shape to develop.
[0005] Due to advantageous properties of aluminum, such as low density enabling lightweight construction, good electrical and thermal conductivity as well as comparatively good and cost-effective availability, there is a high practical need for the production of aluminum 3D workpieces and thus for aluminum metal powders.
[0006] To achieve desired properties, aluminum alloy metal powders are known, which can be in the form of, for example, aluminum-copper, aluminum-copper-manganese, aluminum-silicon, aluminum-manganese-silicon, or aluminum-tin-manganese-copper alloys. The disadvantages of these alloying elements and the high costs of producing the alloys are their high cost.
[0007] Pure aluminum metal powders must be laboriously produced in an inert atmosphere to avoid oxide layers. Disadvantages of their use in a selective laser melting process include high reflection, undesirably high heat dissipation, and oxidation during laser melting. Increasing the laser power to compensate for the high heat dissipation can adversely lead to localized overheating, which, in addition to the fire hazard, can also lead to unwanted gas inclusions and defects. The resulting 3D workpieces are also very soft.
[0008] The object of the invention is to provide an aluminum-based metal powder for use in a selective laser beam melting process that can be produced cost-effectively, allowing an aluminum-based 3D workpiece with advantageous mechanical and electrical properties to be produced. Furthermore, according to a further aspect, the object of the invention is to provide a manufacturing method for producing an aluminum-based molded body.
[0009] The problem is solved with respect to the use by the features listed in patent claim 1. Preferred developments are set out in the subclaims. Furthermore, the problem is solved with respect to the manufacturing method by the features listed in patent claim 5.
[0010] The metal powder for use according to the invention in a selective laser beam melting process for producing a shaped body is an aluminum-based metal powder.
[0011] A selective laser beam melting process in the sense of the present invention is understood to be a method of additive manufacturing in which, on the basis of a previously created 3D CAD model and 2D layers derived therefrom of the shaped body to be produced, a melting takes place layer by layer in a powder bed of metal powder by means of a laser beam and thus a shaped body is obtained by the layers that are simultaneously melted together, also referred to as layers.
[0012] In the sense of the present invention, the shaped body is understood to be the 3D workpiece that was created by the selective laser beam melting process and was materially formed by the metal powder used.
[0013] The metal powder is formed by a multitude of powder particles. The powder particles preferably have a particle size of 30 µm (micrometers) to 65 µm. Particularly preferably, the powder particles are composed of fractions of different particle sizes, so that, when producing a powder bed, a high packing density with a multitude of contact points between the particles and a low proportion of air inclusions is advantageously provided.
[0014] According to the invention, the metal powder has an aluminum metallic phase and an aluminum oxide phase. For use in a selective laser welding process, the properties and interaction of the two phases are crucial for the advantageous process properties and the properties of the resulting molded body.
[0015] The aluminum metallic phase is preferably formed by aluminum without the addition of alloying elements. It is preferably 99.5% to 99.9% aluminum, hereinafter also referred to as pure aluminum. Such pure aluminum is the commercially available base material for aluminum alloys.
[0016] For the purposes of the present invention, the aluminum metallic phase is also understood to mean an aluminum with a higher proportion of accompanying elements or an aluminum alloy with alloying elements such as silicon, magnesium, manganese, copper and zinc.
[0017] For the sake of simplicity, pure aluminum, aluminum with a higher proportion of accompanying elements, and aluminum alloy are collectively referred to as aluminum below, unless expressly stated otherwise.
[0018] The aluminum metallic phase forms the basic body of the powder particles, hereinafter also referred to as the particle core.
[0019] The aluminum-based metal powder for use according to the invention is further characterized by an aluminum oxide phase.
[0020] According to the invention, the aluminum oxide phase is formed by an aluminum oxide layer that surrounds the particle core as a particle shell. This is, in particular, a particle shell with a predominant proportion of Al2O3.
[0021] The aluminum oxide phase is therefore not distributed homogeneously over the volume of the particle bodies, but has an area of higher concentration in the particle shell.
[0022] The aluminum oxide particle shell advantageously forms a support structure in the molded body obtained by the selective laser beam melting process. As a result of the laser beam melting, the particle shell is broken up, resulting in small-sized, finely distributed particle shell fragments that act as a support structure. The particle shell fragments form an aluminum oxide phase in the resulting molded body, and the mass fraction arising from the particle core forms an aluminum-metallic phase.
[0023] It was surprisingly found that, contrary to the efforts known from the prior art to provide a metal powder that is as oxide-free or low in oxide as possible, the following advantages in particular can be provided by using an aluminum-based metal powder with an aluminum oxide phase in the form of a particle shell.
[0024] The aluminum oxide particle coating on the surface absorbs the laser beam well. The disadvantage of strong reflection, which occurs with state-of-the-art aluminum-metallic surfaces, is thus advantageously overcome without the need for additional measures.
[0025] Due to the different thermal expansion coefficients of the aluminum in the particle core and the aluminum oxide particle shell, the rapid heating by the laser beam unexpectedly causes a spontaneous rupture of the particle shell, so that the now suddenly emerging molten aluminum metallic phase of the neighboring particles comes into immediate contact before surface oxidation can occur. In this way, after solidification, a largely undisturbed metal lattice structure is formed by the particle cores, while the particle shell fragments created by the rupture of the particle shell remain and are now enclosed by or embedded in the aluminum metallic phase.
[0026] The particle shell fragments exhibit high strength and are embedded in the metal lattice of the aluminum. Due to their size, which is preferably in the micrometer range or smaller, they create higher-strength bodies in the surrounding metal lattice that counteract deformation and thus increase the strength of the molded body compared to a workpiece made of aluminum without an aluminum oxide phase. This is further supported by the largely homogeneous distribution of the particle fragments both within a layer and between the layers of the resulting molded body. As a result, the particle shell fragments are incorporated as macroscopic, high-strength bodies in the aluminum, which in this respect forms a matrix material. The particle shell fragments therefore do not form closed regions.
[0027] Rather, the aluminum's metallic lattice penetrates the spaces between the particle shell fragments without the lattice defects necessary for strength. The increase in strength is therefore not primarily due to solid solution strengthening, but primarily to the mechanical properties of the particle shell fragments in their mutual support. As aluminum oxide, the particle fragments exhibit mechanically advantageous ceramic properties.
[0028] In contrast to samples from the state of the art, no boundary layers between the particles of the metal powder are visible in the microscopic images of the micrographs of the obtained molded bodies.
[0029] Although aluminum oxide has very low electrical conductivity, the inventive use of the aluminum-based metal powder in a selective laser beam melting process has the particular advantage of providing a shaped body whose electrical conductivity is only slightly reduced compared to pure aluminum. It has been found that the largely homogeneous distribution of the particle fragments and thus of the aluminum oxide phase only insignificantly impairs the metal lattice structure, despite the embedding of the particle shell fragments in the metal lattice of the aluminum. Thus, the shaped body exhibits very high conductivity while simultaneously being high in strength, something unattainable with aluminum alloys of comparable strength. A shaped body obtained in this way is therefore also advantageously suitable for the production of components for electrical circuits.Components produced in this way are particularly suitable for use in the automotive or aviation sectors, as they offer not only advantageous electrical and mechanical properties but also low weight. Their use is particularly advantageous in the field of electromobility.
[0030] Another advantage of the resulting molded body is both chemically and thermally stable. Even at temperatures exceeding 300 degrees Celsius, its strength is largely retained.
[0031] Another advantage is the very simple production of the metal powder; in this regard, reference is made to the description of the manufacturing process according to the invention. In particular, it is advantageous that no expensive and sometimes very limited alloying elements are required for production.
[0032] Another particularly advantageous feature is the significantly lower cost of production compared to other, particularly alloy-based, state-of-the-art metal powders. In this context, it is advantageous that secondary aluminum, i.e., aluminum obtained from aluminum scrap, can also be used. Conversely, the metal powder according to the invention, as well as molded articles obtained therefrom using a selective laser beam melting process, advantageously exhibit very good recycling suitability, since the aluminum is not contaminated by alloying metals, or at most, only in traces.
[0033] According to a first advantageous development of the use of the metal powder in a selective laser melting process for producing a molded body, the metal powder is characterized in that the aluminum oxide phase has a mass fraction of 0.03% to 0.3%. The mass specification according to this development refers to the total mass without differentiation according to zones of higher and lower concentration, such as the particle shell and the particle core.
[0034] It was found that with such a mass fraction, on the one hand, a significant increase in elongation at break and strength can be achieved, and on the other hand, the electrical conductivity is only slightly reduced compared to aluminum or pure aluminum.
[0035] According to a next advantageous development of the use of the metal powder in a selective laser melting process for producing a shaped body, the metal powder is characterized in that the aluminum oxide phase has a mass fraction of 10% to 90% in the particle shell and a mass fraction of less than 1% in the particle core.
[0036] Advantageously, by means of a strongly different concentration of the aluminum oxide particles in the ranges specified according to this further development, a low mass fraction relative to the total mass can be achieved and at the same time high strength and high electrical conductivity can be provided.
[0037] According to a further advantageous development of the use of the metal powder in a selective laser melting process for producing a molded body, the metal powder is characterized by the powder particles having a spherical shape. Spherical shape is a well-established technical term that describes a shape that is as spherical as possible with a smooth surface. The opposite of this can be described as a spiky shape, i.e., with an irregular and jagged surface.
[0038] The spherical shape ensures particularly good flowability, also known as pourability, of the metal powder. This is advantageous when using the selective laser beam melting process, especially when performed as laser powder bed fusion.
[0039] For example, the powder particles in this case have a size of 32 to 64 micrometers. The size refers to the approximate diameter of the powder particles, thus describing their size. It has been found that using a metal powder with powder particles of this size, molded articles can be obtained that exhibit high electrical conductivity without significantly reducing the strength increase provided by the particle shell fragments.
[0040] A further aspect of the invention relates to a selective laser melting process for producing a shaped body, which comprises the following process steps. a) Providing a metal powder according to one of claims 1 to 4 by spraying, blowing, stirring or shaking an aluminium melt in an oxygen-containing atmosphere, b) producing a first layer of a powder bed from the metal powder, c) linearly applying a laser beam to the first layer of the powder bed, fusing the particles in the first layer in a first surface area, d) Creating another layer of the powder bed from the metal powder, e) linearly impinging on the further layer of the powder bed with the laser beam, fusing the particles in the further layer in a further surface area, f) repeating process steps d) and e) and obtaining the shaped body
[0041] The contents of the description of the use of a metal powder according to the invention apply to the method according to the invention in a corresponding manner and taking into account the following aspects.
[0042] The inventive method steps a) to f) are preceded by the creation of a three-dimensional digital model – also called a 3D CAD model – of the molded body to be manufactured. A plurality of superimposed, plane-parallel 2D section planes are formed from the 3D CAD model. The 2D section plane can also be expressed in a spatial coordinate system of the 3D CAD model as an x-coordinate and y-coordinate, and the distance between the 2D section planes as a z-coordinate.
[0043] In process step a), the aluminum-based metal powder is provided. Such aluminum-based metal powders are known in the art and are also referred to herein as aluminum grit. Preferably, the metal powder is produced according to the process according to the invention with powder particles in the size range of 0.01 to 1.0 mm, and particularly preferably in the size range of 0.03 to 0.06 mm, which are also referred to as grit.
[0044] To produce aluminum shot, liquid aluminum is first prepared and then sprayed, blown, atomized, stirred, or shaken to form shot. The aluminum shot can have different shapes and different size fractions. The shapes and size fractions of the bodies influence the properties of the aluminum composite material to be produced and can be determined during production of the aluminum shot and, if necessary, by grading curves. The aluminum shot preferably has a spherical shape. A spherical shape can be achieved in particular by stirring and shaking. Furthermore, a spherical shape can also be achieved by blowing or atomizing, in which the particles are set in rotation and kept suspended for as long as possible using suitable air flow, in particular swirling.
[0045] Process step a) is further characterized in particular by the fact that the powder formation takes place in an oxygen-containing atmosphere. During this process, the aluminum reacts with the oxygen on the hot surface, particularly to form Al2O3. This, according to the invention, creates the aluminum oxide shell of the powder particles of the metal powder.
[0046] In particular, the oxygen content of the oxygen-containing atmosphere to be provided allows the conversion rate of aluminum to aluminum oxide and thus the thickness of the aluminum oxide particle shell and, as a result, the mass fraction of the aluminum oxide phase in the metal powder to be produced to be advantageously and easily adjusted, so that its properties can be influenced in a targeted manner. An aluminum oxide particle shell within the meaning of the present invention is also understood to mean that, in addition to Al2O3, other compounds or substances are contained in the particle shell. This can be due, for example, to impurities. In advantageous further developments, however, targeted admixtures in the oxygen-containing atmosphere can also be used for this purpose.
[0047] In process step b), a powder bed is created using the metal powder. In a conventional manner, the metal powder is applied in a thin layer to a substrate and removed, leaving a flat, smooth surface. This thin layer forms the first layer.
[0048] Subsequently, in process step c), a zone of the thin layer of metal powder is exposed to a linear laser beam and thus heated to such an intense level that a locally defined and thus selective fusion of the powder particles occurs. The zone to be exposed is defined by one of the 2D cutting planes of the 3D CAD model. The powder particles are heated so that the aluminum oxide powder shell breaks open and the aluminum of the powder core of the neighboring powder particles comes into contact and fuses, forming a metal lattice structure and embedding the remaining powder shell fragments. The metal lattice structure then forms the highly electrically conductive aluminum metallic phase, and furthermore, the powder fragments form the aluminum oxide phase of the molded body to be produced as a strengthening support structure. This creates the first layer of the molded body to be produced.
[0049] In process step d), another thin layer of metal powder is created, and in process step e), the additional thin layer is also exposed to a linear laser beam. As in process step d), the neighboring powder particles within the layer fuse not only with each other, but also with the powder particles of the previous layer. This creates the second layer of the molded body to be manufactured, in addition to the first layer.
[0050] In process step f), process steps d) and e) are repeated until the number of all layers of the molded bodies results in the coordinates x, y, z specified by the 3D CAD model.
[0051] The process steps b) to f) are known as such from the prior art, to the extent that reference can be made to them.
[0052] The process according to the invention is thus characterized by the combination of process step a), namely the formation of a metal powder with the features as described in claims 1 to 4, with the further process steps b) to f) known per se.
[0053] The invention is illustrated by way of example with reference to Fig. 1a Micrograph of a 3D-printed molded body made of pure aluminum 99.7% and Al oxide at 50x magnification Fig. 1b Micrograph of a 3D-printed molded body made of pure aluminum 99.7% and Al oxide at 200x magnification Fig. 2 Microsection of a 3D printed molded body AISi10Mg and Si oxide at 50x magnification (state of the art) explained in more detail.
[0054] Identical reference symbols in the various figures refer to identical features or components. These reference symbols are used in the description even if they are not shown in the respective figure.
[0055] Fig. 1a shows a microsection of a shaped body made of a metal powder according to an embodiment described below.
[0056] In one embodiment, in process step a), pure aluminum (99.7% pure aluminum) was atomized in an oxygen-containing atmosphere under turbulence. This resulted in an aluminum powder with an average particle size of 32 µm to 64 µm, with the particles having an Al2O3 layer on their surface. The mass fraction of Al2O3 in the total mass is approximately 0.1%.
[0057] The metal powder thus obtained is also an example of a metal powder for use in the selective laser beam melting process.
[0058] A shaped body was produced from this metal powder by means of laser powder bed fusion using the method according to the invention.
[0059] For this purpose, in process step b) a first layer of a powder bed made of metal powder was applied and then in process step c) this first layer of the powder bed was linearly exposed to a laser beam by moving a laser head in an x and y axes, thus fusing the particles in the first layer in a first surface area. In process step d) a further layer of the powder bed was created from the metal powder and in process step e) the further layer of the powder bed was linearly exposed to the laser beam, fusing the particles in the further layer in a further surface area. In process step f) the process steps d) and e) were repeated and the shaped body was obtained.
[0060] A microsection was created from this molded body, as shown in 50x magnification in Fig. 1a. This microsection particularly highlights the fine and relatively homogeneous distribution of the particle shell fragments. Furthermore, the microsection shows that no interfaces are formed between the former and now densely fused particles.
[0061] Fig. 1b shows the same sample as Fig. 1a, but at a 200x magnification. The dimensioned areas show cavities, so-called blowholes, which can occur particularly during the layered buildup of the powder bed.
[0062] In contrast, Fig. Figure 2 shows a microsection of a molded article obtained from a metal powder based on an aluminum-silicon-magnesium-silicon oxide alloy using a 3D laser melting process according to the state of the art. The boundary layers between the crosswise applied and fused layers of particles of the metal powder used are clearly visible.
Claims
[1] Use of a metal powder in a selective laser melting process for producing a shaped body, wherein the metal powder comprises a plurality of powder particles, and wherein the metal powder has an aluminum metallic phase and an aluminum oxide phase wherein the aluminum metallic phase comprises aluminum and / or an aluminum alloy and forms a particle core and wherein the aluminum oxide phase comprises Al2O3 and forms a particle shell surrounding the particle core. [2] Use of a metal powder in a selective laser melting process for producing a shaped body according to claim 1, characterized by that the aluminum oxide phase has a mass fraction of 0.1% to 3% [3] Use of a metal powder in a selective laser melting process for producing a shaped body according to one of the preceding claims, characterized bythat the aluminum oxide phase has a mass fraction of 10% to 90% in the particle shell and less than 0.3% in the particle core. [4] Use of a metal powder in a selective laser melting process for producing a shaped body according to one of the preceding claims, characterized by that the powder particles have a spherical shape. [5] Selective laser melting process for producing a shaped body, comprising the following process steps, a) Providing a metal powder according to one of claims 1 to 4 by spraying, blowing, stirring or shaking an aluminium melt in an oxygen-containing atmosphere, b) producing a first layer of a powder bed from the metal powder, c) linearly applying a laser beam to the first layer of the powder bed, fusing the particles in the first layer in a first surface area, d) Creating another layer of the powder bed from the metal powder, e) linearly impinging on the further layer of the powder bed with the laser beam, fusing the particles in the further layer in a further surface area, f) repeating process steps d) and e) and obtaining the shaped body.
Citation Information
Patent Citations
Aluminum alloy for additive techniques
EP3623488A1
Cited By
In-situ conversion porous component based on selective laser melting and manufacturing method thereof