Control unit for a wire position-controlled short arc process

The control device adjusts wire feed rate and current based on the wire electrode's position to address uneven heat inputs in arc welding, achieving a uniform welding process with controlled droplet formation and arc lengths.

DE202025004168U1Active Publication Date: 2026-05-21EWM GMBH
View PDF 2 Cites 0 Cited by

Patent Information

Authority / Receiving Office
DE · DE
Patent Type
Utility models
Current Assignee / Owner
EWM GMBH
Filing Date
2025-08-29
Publication Date
2026-05-21

AI Technical Summary

Technical Problem

Existing arc welding processes with short-circuit phases and arc phases suffer from uneven heat inputs due to varying short-circuit durations, leading to inconsistencies in the welding process, including non-uniformity and difficulties in controlling droplet formation and arc length.

Method used

A control device for a welding apparatus that adjusts the wire electrode feed rate and welding current based on the current position of the wire electrode relative to the weld pool, using a microprocessor and memory to control the welding process, allowing for precise control of heat input and droplet formation during short-circuit and arc phases.

Benefits of technology

This approach achieves a more uniform welding process by controlling the wire electrode's position, ensuring consistent arc lengths and heat input, promoting favorable droplet formation and transition, and enabling high deposition rates.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Control device (114) for a welding device (100) with at least one microprocessor (115) and at least one memory (116) containing instructions, the execution of which on the at least one microprocessor causes an arc welding process to be carried out, in accordance with a method for arc welding with a consumable wire electrode (152) comprising a plurality of welding cycles (SC), each having a short-circuit phase (SC) and an arc phase (ARC). - wherein in the process the wire electrode (152) is moved at a variable conveying speed (v F (t)) is promoted and - where the conveying speed (v) is used in the process F (t)) and / or the welding current (I(t)) is changed depending on a value (x(t)) for the current position of the wire electrode (152), in particular when the value (x(t)) for the current position of the wire electrode (152) is a predetermined position (xc, xD ) reached, in particular exceeding or falling short of.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present invention relates to a control device for a welding device and to a welding device with such a control device.

[0002] Arc welding processes with welding cycles that each have a short-circuit phase and an arc phase are generally known as short-arc processes.

[0003] EP 1 563 938 B1, for example, describes a short-arc process in which a counter-voltage is applied towards the end of the short-circuit phase to prevent spattering during short-circuit resolution. EP 3 509 784 B2 also describes a short-arc process in which a reverse terminal velocity of the wire electrode is reached before the short-circuit resolution.

[0004] Many well-known welding processes share the common feature that the speed of the wire electrode is adjusted depending on the short-circuit signal from the welding device. Due to uneven short-circuit durations, this results in varying heat inputs, which also prevent a high degree of uniformity in the welding process.

[0005] Against this background, the present invention is based on the objective of providing a control device for a welding apparatus and a welding device that enables a better welding process, in particular reducing or avoiding disadvantages of the prior art.

[0006] The above-mentioned problem is solved according to the invention by a control device for a welding apparatus with at least one microprocessor and at least one memory containing instructions, the execution of which on the at least one microprocessor causes an arc welding process to be carried out, according to a method for arc welding with a consumable wire electrode comprising a plurality of welding cycles, each having a short-circuit phase and an arc phase, wherein in the method the wire electrode is fed at a variable feed rate and wherein in the method the feed rate and / or the welding current is changed depending on a value for the current position of the wire electrode, in particular is changed when the value for the current position of the wire electrode reaches a predetermined position, in particular exceeds or falls below it.

[0007] In this way, the welding process can be controlled, for example, depending on the distance of the wire electrode to the weld pool. This allows, in particular, control of the welding process with specified distances. Various welding parameters, especially the acceleration of the wire electrode or current shaping, can be controlled depending on the position of the wire electrode relative to the weld pool. This can, for example, achieve high uniformity of the welding process, allow for targeted control of heat input in the short-circuit and / or arc phases, and / or, depending on the application, achieve minimal immersion depths of the wire electrode in the weld pool and / or consistent arc lengths. Furthermore, by controlling the position of the droplets on the wire electrode, it is possible to shape them in such a way as to promote short-circuit transition or to enable adapted heat input at high deposition rates.

[0008] Such a welding process, guided by the wire electrode position, is particularly advantageous compared to a welding process guided solely by the wire electrode speed.

[0009] The process is for arc welding with a consumable wire electrode. The process is preferably carried out under a shielding gas. Accordingly, the process is preferably a metal inert gas welding process (MIG welding process), for example a metal inert gas welding process (MIG welding process) or a metal active gas welding process (MAG welding process).

[0010] The process comprises a plurality of welding cycles, each with a short-circuit phase and an arc phase. Preferably, the welding cycles of the plurality of welding cycles follow one another. The sequence of welding cycles of the plurality of welding cycles can be interrupted by one or more other intermediate welding cycles, for example, pulse process welding cycles. A hybrid welding process is also conceivable, in which sequences of one or more welding cycles, each with a short-circuit phase and an arc phase, alternate with sequences of one or more intermediate welding cycles without a short-circuit phase.

[0011] Each welding cycle consists of a short-circuit phase and an arc phase. The short-circuit phase begins, in particular, when a short circuit occurs between the wire electrode and the weld pool and lasts until the short circuit is subsequently cleared. The arc phase also begins, in particular, when the short circuit is cleared and lasts until the next short circuit occurs. During the arc phase, a welding arc burns, in particular, between the wire electrode and a workpiece.

[0012] The arc phase preferably comprises an arc withdrawal phase, in which the wire electrode is moved away from (retracted from) the molten pool. The arc phase further preferably comprises an arc approach phase, in which the wire electrode is moved towards the molten pool. Preferably, the arc approach phase of the arc phase follows the arc withdrawal phase of the arc phase.

[0013] The short-circuit phase preferably comprises a short-circuit approach phase, in which the wire electrode is moved towards the melt pool. The short-circuit phase further preferably comprises a short-circuit removal phase, in which the wire electrode is moved away from the melt pool. Preferably, the short-circuit removal phase follows the short-circuit approach phase of the short-circuit phase.

[0014] In this process, the wire electrode is conveyed at a variable conveying speed. The conveying speed v F is therefore preferably a function of time, v F (t). The conveying speed corresponds - except for negligible differences due to slippage - to the wire speed of the wire electrode.

[0015] In this process, the feed rate and / or the welding current is changed depending on a value for the current position of the wire electrode.

[0016] In particular, the feed rate can be changed depending on a value for the current position of the wire electrode. In this way, the feed rate can be adjusted, for example, depending on the distance of the wire electrode to the weld pool, to ensure reliable droplet transfer, prevent the wire electrode from being immersed too deeply in the weld pool, or to increase the welding speed.

[0017] Additionally or alternatively, the welding current can be changed depending on a value for the current position of the wire electrode. In this way, for example, the welding current can be synchronized with the wire movement, for instance to achieve a more uniform weld seam.

[0018] The feed rate and / or the welding current can be changed, in particular, if the value for the current position of the wire electrode reaches a predetermined position, especially if it exceeds or falls below a predetermined distance between the wire electrode and the weld pool, for example, if it reaches or falls below a predetermined distance.

[0019] The value for the current position of the wire electrode is preferably a calculated value.

[0020] In particular, the value for the current position of the wire electrode can be determined depending on a reference position of the wire electrode and the conveying speed or conveying path. The reference position specifies and / or defines the position of the wire electrode at a particular reference time, for example, to a predetermined reference value such as zero. The reference position, especially at the reference time, preferably relates to the actual position of the wire electrode, preferably in terms of the distance of the wire electrode from the weld pool surface.

[0021] The value for the current position can then be calculated, for example, starting from the reference position by integrating the time-dependent conveying speed from the reference time to the current time. For integrating the conveying speed, target values ​​can be used, or, to increase accuracy, measured conveying speed values ​​can be used, for example, by means of a rotary velocity sensor installed on a wire electrode conveying device.

[0022] Furthermore, the value for the current position can be calculated from the reference position by adding a conveying distance. To determine the conveying distance traveled since the reference time, signals to or from a stepper motor of the wire electrode conveying device can be used, or, to increase accuracy, measured values ​​for the distance can be acquired, for example, by means of a displacement sensor, such as a rotary angle sensor, provided on the wire electrode conveying device. If, for example, the stepper motor or rotary angle sensor delivers a pulse after each sweep of a specific angle Δγ, then x(t) can be incrementally calculated by adding or subtracting a corresponding differential displacement (e.g., r). Rolle · Δγ, where r Rolle the radius of the corresponding wire feed roller of the wire feed device is determined at each pulse.

[0023] When determining the value for the current position, the melting of the wire electrode can optionally be taken into account, for example by integrating a melting rate, defined by a characteristic curve, from the reference time to the current time. However, the melting of the wire electrode can also be omitted, for example by appropriately selecting the predefined position and regularly choosing a new reference position, such as at the beginning of each welding cycle.

[0024] The reference position can be determined based on the position of the wire electrode at the time of short-circuit inception and / or resolution during the current and / or a previous welding cycle. Specifically, the position of the wire electrode at the time of short-circuit inception (or resolution) can be used as the reference position. For example, a predetermined value, such as zero, can be set for the position of the wire electrode at the time of short-circuit inception (or resolution). The time of short-circuit inception (or resolution) can then be used as the reference point for calculating the value for the current position of the wire electrode.

[0025] The above-mentioned problem is further solved according to the invention by a welding device comprising the control device described above or an embodiment thereof.

[0026] The welding device includes in particular a welding power source, wherein the control device may preferably be a control device of the welding power source.

[0027] The welding device preferably further comprises a welding torch.

[0028] The welding device includes, in particular, a wire feeder for conveying a wire electrode. The wire feeder is preferably arranged on or integrated into the welding torch. This enables highly dynamic wire feeding with variable feed speed, allowing the feed speed of the wire electrode to be reliably controlled in a time-dependent manner within the individual welding cycles.

[0029] The welding device can further include a wire feeder with an additional wire feeder located upstream of the wire feeder. This additional wire feeder can, for example, be configured and / or controlled by the control unit such that the wire electrode is fed at one or more intermediate feed speeds. Adjusting the feed speed within a welding cycle can then be achieved by the wire feeder located downstream of the additional wire feeder. To compensate for differences between the feed speeds of the additional wire feeder and the main wire feeder, a wire accumulator can be provided between the additional wire feeder and the main wire feeder.The wire storage unit can, in particular, comprise one or more movable rollers around which the wire electrode is guided, so that mechanical stresses in the wire electrode caused by differences in conveying speeds can be compensated by moving the rollers. It is also conceivable to omit the wire storage unit, especially when using a wire guide that has a sufficiently large inner cross-section compared to the outer cross-section of the wire electrode guided therein, preferably a wire guide whose inner diameter is at least 5 mm larger than the diameter of the wire electrode.

[0030] The wire conveying device and / or the further wire conveying device may in particular have one or more opposing rollers between which the wire electrode is guided, wherein at least one, preferably at least two, opposing rollers are driven.

[0031] To accurately measure the conveying speed and / or the conveying distance, the welding device preferably includes a conveying speed measuring device and / or a conveying distance measuring device, particularly on the wire feeder. The conveying speed measuring device can, for example, include a rotary speed sensor on a roller of the wire feeder. The conveying distance measuring device can, for example, include a rotary angle sensor on a roller of the wire feeder. A rotary encoder can be provided as the rotary speed sensor and / or rotary angle sensor.

[0032] The wire feeder and the feeder speed and / or feeder distance measuring device are connected to the control unit, for example via a wired or wireless communication link.

[0033] The following describes various embodiments of the control unit and the welding device, with each embodiment applying independently to the control unit and the welding device. Furthermore, the individual embodiments can be combined with one another as desired.

[0034] In one embodiment, the arc phase includes an arc approach phase in which the wire electrode is fed towards a weld pool, with the feed rate and / or welding current being changed during the arc approach phase depending on a value for the current position of the wire electrode. In this way, the short circuit can be prepared in a position-dependent manner.

[0035] Preferably, the feed rate and / or the welding current are changed when the value for the current position of the wire electrode reaches, in particular falls below, or exceeds a predetermined distance value. The predetermined distance value is, in particular, a predetermined distance value relative to the reference position, which, for example, can correspond to the position of the weld pool surface at the reference time.

[0036] In particular, the conveying speed can be reduced to a lower absolute value once the predetermined distance value is reached. This prevents the wire electrode from being immersed too deeply in the melt pool during the subsequent short-circuit phase. Furthermore, this method facilitates favorable droplet formation and detachment.

[0037] Alternatively, the feed rate can be increased to a higher absolute value once the specified distance value has been reached. This allows the welding current to be increased without premature droplet detachment from the wire electrode. Furthermore, a short circuit can be mechanically induced in this way.

[0038] In addition to or as an alternative to changing the feed rate, the welding current can also be changed depending on the current position of the wire electrode, particularly when the predefined distance is reached or fallen below. For example, an increase in current can be synchronized with a distance-dependent acceleration of the wire electrode to increase the welding energy without premature droplet detachment. Furthermore, a decrease in current can be initiated when the wire electrode reaches a predefined position to cause droplet detachment.

[0039] In one embodiment, the short-circuit phase includes a short-circuit removal phase in which the wire electrode is conveyed away from the melt bath, wherein the conveying speed of the wire electrode is increased in magnitude during the course of the short-circuit removal phase, preferably at a decreasing rate.

[0040] By increasing the feed rate during the short-circuit removal phase, the wire electrode is pulled out of the weld pool more quickly, allowing the short-circuit phase to end sooner and the welding process to proceed faster, particularly at a higher frequency. The preferably decreasing rate of increase in feed rate, i.e., the decreasing acceleration of the wire electrode, prevents excessive speed during short-circuit resolution and thus reduces the deceleration of the wire electrode.

[0041] In one embodiment, the feed rate of the wire electrode is increased during the short-circuit removal phase until a predetermined time has elapsed since the short circuit occurred, or, if the short circuit is resolved before the predetermined time has elapsed, until the short circuit is resolved. If the predetermined time expires before the short circuit is resolved, the feed rate can then remain constant, decrease, or increase until the short circuit is resolved. Alternatively, the feed rate of the wire electrode can be increased during the short-circuit removal phase until a predetermined distance has been covered since the short circuit occurred, or, if the short circuit is resolved before the predetermined distance has been covered, until the short circuit is resolved.Once the wire electrode has traversed the predetermined distance before the short circuit is resolved, the conveying speed can then remain constant, decrease, or increase until the short circuit is resolved. This ensures that the wire electrode is accelerated over a sufficiently long period or distance to resolve the short circuit more quickly.

[0042] In one embodiment, the arc phase includes an arc removal phase in which the wire electrode is moved away from the molten pool, with the wire electrode's conveying speed being reduced during the arc removal phase until the direction reversal. In this way, after the short circuit clears, the wire electrode is retracted further to a top dead center upon reaching the direction reversal, resulting in the formation of a stable arc. Preferably, the wire electrode's conveying speed is reduced during the arc removal phase only from a point in time dependent on the current position of the wire electrode, for example, when the current position of the wire electrode reaches, and in particular exceeds, a predetermined position value.If the value for the current position of the wire electrode exceeds the specified position value at the beginning of the arc removal phase, the feed rate of the wire electrode is preferably reduced in magnitude from the beginning of the arc removal phase.

[0043] In this way, the top dead center can be precisely set when the direction of the wire electrode is reversed, especially at a constant distance to the weld pool, resulting in a more uniform welding process.

[0044] In one embodiment, the rate at which the feed rate of the wire electrode is reduced during the arc removal phase until the direction reversal is set such that the direction reversal is reached after a predetermined time since the short circuit was cleared. In this way, the top dead center of the wire electrode can be reached at a desired time, thus enabling a more uniform welding process.

[0045] In one embodiment, the feed rate of the wire electrode is maintained at a value less than or equal to a predetermined velocity value for a predetermined duration during the reversal of direction. The predetermined velocity value can, in particular, be zero; that is, the wire electrode is preferably held at top dead center for a predetermined duration during the reversal of direction. In this way, the melt pool can be stabilized.

[0046] In one embodiment, the method features a plurality of pulse process welding cycles without a short-circuit phase.

[0047] The process can therefore be a mixed process in which, within a welding operation, there is a change between a short-arc process, i.e., a welding process with a short-circuit phase, and another welding process, in particular a pulse process.

[0048] Preferably, one or more parameters of a welding cycle without a short-circuit phase following a welding cycle with a short-circuit phase, in particular a pulsed welding cycle, are set depending on the value for the current position of the wire electrode. In this way, the value for the current position of the wire electrode, which is easily determined during the short-circuit process, can be used to set the subsequent welding cycle, in which the value for the current position would be more difficult to determine due to the absence of a short-circuit phase.

[0049] In particular, one or more welding cycles following a welding cycle with a short-circuit phase can be operated without a short-circuit phase using transition values ​​for one or more parameters that differ from the values ​​for the one or more parameters of the subsequent welding cycles without a short-circuit phase. The number of welding cycles operated with the transition values ​​depends on the current position of the wire electrode. For example, the welding cycles following a welding cycle with a short-circuit phase can be operated with the transition values ​​until the wire electrode has been advanced by the stickout point during the welding cycle with a short-circuit phase.In this way, the heating of this stickout by the short-circuit current during the short-circuit phase can be taken into account in the subsequent first welding cycles without a short-circuit phase, until a piece of wire not subjected to the short-circuit current has advanced.

[0050] In one embodiment, a counter-voltage is applied in series with the welding voltage during the short-circuit phase, particularly when a predefined condition for the welding voltage value is reached. This accelerates the resolution of the short circuit and reduces weld spatter. The predefined condition could, for example, be exceeding a predetermined welding voltage threshold or a predetermined welding voltage change.

[0051] Further features and advantages of the control device and the welding apparatus will become apparent from the following description of exemplary embodiments, with reference to the attached drawing.

[0052] The drawing shows Fig. 1 an embodiment of the control device and the welding device, Fig. 2 an example of a wire storage device, Fig. 3. Several diagrams over a common time axis to illustrate an exemplary embodiment of the process controlled by the control device. Fig. 4 further diagrams over a common time axis illustrating the exemplary implementation of the method controlled by the control unit. Fig. 3 and Fig. 5 further diagrams over a common time axis illustrating the exemplary implementation of the method controlled by the control unit. Fig. 3.

[0053] Fig. Figure 1 shows a schematic representation of an embodiment of the control device and the welding apparatus. The welding apparatus 100 is designed for metal inert gas (MIG) welding, for example, metal inert gas (MIG) or metal active gas (MAG) welding.

[0054] The welding device 100 comprises a welding power source 110 for providing a welding current, a power unit 112, and a control unit 114. The control unit 114 has a microprocessor 115 and a memory 116 containing instructions. The control unit 114 is configured to control the welding power source 110 and, in particular, controls the power unit 112. For this purpose, the memory 116 contains, in particular, corresponding instructions, the execution of which on the microprocessor 115 effects the control of the welding power source. The power unit 112 is configured to provide a welding current for welding via an electrical output 118 of the welding power source 110.

[0055] The welding device 100 further comprises a wire feeder 150 for transporting a wire electrode 152. The wire feeder 150 has a wire electrode supply 154 in the form of a wire electrode drum, a primary wire electrode conveying device 156, which preferably includes driven rollers for controlled conveying of the wire electrode 152, and a control device 160, which is designed to control the wire feeder 150.

[0056] The wire feeder 150 further comprises an electrical input 162 for supplying the welding current provided by the welding power source 110, which is connected to the electrical output 118 of the welding power source via an electrical line 119 for operation. The wire feeder 150 also comprises a shielding gas inlet 164 for supplying a shielding gas, which is connected to a shielding gas source 166, such as a gas cylinder, via a gas line 165 for operation.

[0057] The wire feeder 150 further features a torch connection 168 for connecting a welding torch 180 of the welding device 100. The wire electrode 152 fed by the primary wire electrode feeder 156, the welding current supplied by the welding power source 110, and the shielding gas supplied by the shielding gas source 166 are provided to the welding torch 180 via the torch connection 168.

[0058] The control unit 160 is specifically designed to control the primary wire electrode feed unit 156. Furthermore, the control unit 160 can be configured to control the shielding gas flow supplied at the burner connection 168. For this purpose, the wire feeder 150 can have, for example, a controllable valve 169 between the shielding gas inlet 164 and the burner connection 168, with which the shielding gas flow can be adjusted.

[0059] The control unit 114 of the welding power source 110 and the control unit 160 of the wire feeder 150 are preferably connected to each other via a communication link, for example via line 119 or via a separate data line, so that one of the two control units 114, 160 can transmit control commands to the other of the two control units 114, 160. In this way, for example, the control unit 114 can be configured to control both the welding power source 110 and the wire feeder 150.

[0060] A user interface 122, 172 is preferably provided on the welding power source 110 and / or on the wire feeder 150, via which the user can read operating information and / or enter control commands.

[0061] The welding torch 180 comprises a torch section 182 and a hose assembly 184. The hose assembly 184 is connected to the torch connection 168 of the wire feeder 150, so that during operation the wire electrode 152 fed by the primary wire electrode feeder 156 is guided via the torch connection 168 through a wire guide 185 running through the hose assembly 184 in the form of a hollow line to the torch section 182, and the welding current supplied by the welding power source 110 and looped through the wire feeder 150 is further guided via the torch connection 168 through an electrical line running through the hose assembly 184 to the torch section 182, where the welding current is directed to the wire electrode 152 via a contact.

[0062] A secondary wire electrode feeder 186 is arranged in the burner section 182. This feeder preferably includes driven rollers for the controlled feeding of the wire electrode 152 and allows precise and dynamic adjustment of the feed rate at which the wire electrode 152 exits the burner section 182. The secondary wire electrode feeder 186 is also controlled by the control unit 114, for example via a data line integrated into the hose assembly 184.

[0063] During operation, the wire electrode 152 is fed by the primary wire electrode conveying device 156 at a variable primary conveying speed v. F (t) and from the secondary wire electrode conveying device 186 with a variable secondary conveying speed v F(t) conveyed. The primary conveying speed can, in particular, be an average conveying speed. The actual exit speed of the wire electrode 152 from the torch part 182, which can change several times or continuously within a welding cycle, corresponds to the secondary conveying speed. The conveying speed v F (t) can be positive or negative. Under a positive flow rate v F (t), i.e. v F (t) > 0 m / min., is understood here to mean that the wire electrode 152 is moved out of the torch part 182, i.e., when welding a workpiece 200, it is moved towards the weld pool 202 (arrow 204). Under a negative feed rate v F (t), i.e. v F(t) < 0 m / min., is understood here to mean that the wire electrode 152 is moved into the torch part 182, i.e., when welding a workpiece 200, it is moved away from the weld pool 202 (arrow 206).

[0064] The conveying of the wire electrode 152 with the wire electrode conveying device 156 results in a conveying path SF (t). At a positive conveying velocity v F (t) the conveying path takes s F (t) to, at a negative conveying velocity v F (t) the conveying path takes s F (t) off.

[0065] To accurately measure the conveying speed v F (t) or of the conveying path s F (t) a conveying speed and / or conveying distance detection device 187, for example in the form of a rotary encoder on one of the driven rollers, is provided on the secondary wire electrode conveying device 186.

[0066] Differences between the primary and secondary conveying speed can be compensated by an optional wire storage unit 190 connected between the primary and secondary wire electrode conveying device 156, 186. Fig. Figure 2 shows a schematic representation of such a wire storage unit 190, which has a clearance of spring-loaded rollers 192 around which the wire electrode 152 is guided. Alternatively, sufficient clearance for the wire electrode to compensate for differences in the primary and secondary conveying speed can be provided by a wire guide 185 with an inner diameter larger than the outer diameter of the wire electrode 152.

[0067] Furthermore, during operation, the shielding gas flow provided at the burner connection 168 is directed through a shielding gas line running through the hose package 184 to the burner part 182 in order to create a shielding gas jacket for the welding process.

[0068] Finally, a torch button 188 is provided on the torch part 182 for starting a welding process.

[0069] The following will be based on the Fig. 3 A method for arc welding with the welding device 100 is described. The method is controlled by the control unit 114 of the welding power source 110, for example when the torch trigger 188 is activated.

[0070] Fig. Figure 3 shows several diagrams over a common time axis to illustrate an exemplary embodiment of the method.

[0071] Diagram (a) shows the welding current I(t), diagram (b) shows the welding voltage U(t), diagram (c) shows the short-circuit phase (0) or the arc phase (1) as a digital signal, diagram (d) shows the conveying speed v measured by the conveying speed detection device 187 F(t) of the wire electrode 152 and the diagram (e) shows a value x(t) for the position of the wire electrode, which is obtained from a reference position by adding a measured conveying path s(t) or by integrating the conveying velocity v F (t) is determined. For the sake of clarity, the sign for v is F (t) is chosen such that positive velocity values ​​correspond to a movement towards the melt pool and negative velocity values ​​to a movement away from the melt pool, and furthermore, the sign for x(t) is chosen such that when the melt pool surface is at zero, positive values ​​are above the melt pool surface (outside the melt pool) and negative values ​​are below the melt pool surface (inside the melt pool). This choice of sign results in a sign reversal between x(t) and v. F (t), i.e. a positive velocity value v F(t) leads to a change of x(t) towards the negative and vice versa.

[0072] Above the diagrams, a schematic representation of wire electrode 152, workpiece 200 and melt bath 202 is shown for some selected times (t1 to t7) at the respective times.

[0073] The welding process comprises a plurality of successive welding cycles SZ, of which in Fig. Figure 3 shows one. Each welding cycle (SZ) has a short-circuit phase (KSP) and an arc phase (LBP). Furthermore, the short-circuit phase (KSP) has a short-circuit approach phase (KS-AP) and a short-circuit removal phase (KS-EP). The arc phase (LBP) has, accordingly, an arc removal phase (LB-EP) and an arc approach phase (LB-AP).

[0074] During the short-circuit approach phase KS-AP and the arc approach phase LB-AP, the wire electrode 152 is conveyed towards the melt pool 202. During the short-circuit removal phase KS-EP and the arc removal phase LB-EP, the wire electrode 152 is conveyed away from the melt pool 202.

[0075] The control unit 114 uses appropriate measuring devices to detect the welding current I(t) supplied by the welding power source 110, which flows from the wire electrode 152 to the workpiece 200 during welding, and the welding voltage U(t) supplied by the welding power source 110, which is present between the wire electrode 152 and the workpiece 200 – except for minor voltage losses due to line resistances. The control unit 114 is configured to detect the short-circuit event (t1 in) depending on the welding voltage U(t). Fig. 3) and the short-circuit resolution (t3 in Fig. 3) to detect. If the welding voltage U(t) during the arc phase drops below a predefined threshold, e.g., 10 V, the control unit 114 detects the short circuit. If the welding voltage U(t) during the short circuit phase rises above a predefined threshold, e.g., 15 V, the control unit 114 detects the short circuit resolution. The control unit 114 also continuously receives the conveying velocity v measured by the conveying velocity and / or conveying distance detection unit 187. F (t) of the wire electrode 152 or the measured conveying distance s F (t) of the wire electrode 152, for example via the data line integrated into the hose package 184.

[0076] The control unit 114 is configured to adjust the secondary wire electrode feeder 186's feed rate v. F(t) and the power unit 112 to adjust the welding current I(t), in particular depending on a value x(t) for the current position of the wire electrode.

[0077] The control unit 114 can determine the value x(t) for the current position of the wire electrode 152 based on the conveying speed v. F (t) or of the conveying path s F(t) and a reference position. For example, the control unit 114 can use the position of the wire electrode 152 at the time of the short circuit as the reference position. The time of the short circuit is then the reference time. To do this, the control unit 114 can set the value x(t1) for the position of the wire electrode 152 at the time of the short circuit (at t1) to a predefined value, for example x(t1) = 0 mm, and store the time t1 of the short circuit as the reference time. The control unit can then, for example, adjust the value x(t) for the current position of the wire electrode 152 depending on the conveying speed v. F (t) can be calculated using the following formula (the minus sign in front of the integral results from the previously described choice of signs for x(t) and v). F (t)): x(t)=x(t1)−∫t1t(vF(t)−C(I(t)))dt, or depending on the funding method s F(t) can be calculated using the following formula (the minus sign before the s) F The (t)-term is obtained in this case by the previously described choice of signs for x(t) and s F (t): x(t)=x(t1)−(sF(t)−sF(t1))−∫t1tC(I(t))dt, where C(I(t)) represents a phenomenologically determined melting rate of the wire electrode 152, dependent on the current I(t), which can be stored, for example, in the memory of the control unit 114. The melting rate can, in particular, take into account that the melting material of the wire forms a droplet at the wire end, the diameter of which is smaller than the length of the wire segment melted to form it. For simplification, a melting rate independent of the current C(I(t)) = const. can also be assumed, or the melting rate can be neglected, i.e., C(I(t)) = 0 m / min.

[0078] Since it can be assumed that the wire electrode 152 is just touching the melt 202 at the time of the short circuit, the values ​​x(t) calculated with the above formula for the respective current position of the wire electrode 152 correspond approximately to the distance of the wire electrode 152 to the melt bath surface.

[0079] Neglecting the melting rate leads to a continuous deviation between the calculated value of x(t) and the actual position of the wire electrode tip relative to the melt pool. However, this deviation can be compensated for by appropriately selecting the predetermined position. Furthermore, the reference position can be regularly recalculated, for example, upon each short circuit, so that the values ​​of x(t) are regularly calibrated and / or adjusted to the actual position of the melt pool surface.

[0080] As an alternative to the position at short-circuit inception, another reference position can be used, for example, the position of the wire electrode 152 at short-circuit resolution, a position averaged from the positions of the wire electrode 152 at short-circuit inception and short-circuit resolution, or a position averaged over the position of the wire electrode at short-circuit inception and / or short-circuit resolution of several past welding cycles. These different reference positions typically differ slightly from one another, for example, due to the dynamics of the weld pool, the arc pressure, or surface tension effects during the interaction of the weld pool and the wire electrode 152.

[0081] Controlling the conveying speed v F (t) and the welding current I(t) through the control unit 114 in the individual phases of the welding cycle is now described below: Short-circuit approach phase KS-AP (Phase 1):

[0082] The welding cycle begins with the short-circuit phase and thus with the occurrence of the short circuit (time t1 in Fig. 3) At the time of the short circuit and also for a certain time after the short circuit occurs, the wire electrode 152 moves towards the melt pool 202 and thus immerses itself in the melt pool 202.

[0083] In this short-circuit approach phase KS-AP, the control unit 114 controls the wire electrode feeder 186 after detection of the short circuit so that the feed rate v F(t) is reduced until the direction reverses, thus decelerating the wire electrode 152. Furthermore, as previously described, the control unit 114 stores x(t1) as the reference position of the wire electrode 152 at the reference time t1, or sets x(t1) to a predetermined value in order to subsequently calculate the respective value x(t) for the current position of the wire electrode 152 starting from the reference time t1. The control unit 114 can, for example, set the reference position x(t1) to zero, as shown in Fig. Figure 3 shows that x(t) represents the position relative to the reference position x(t1). The melting rate is neglected in the calculation of x(t), i.e., C(I(t)) = 0 m / min.

[0084] At time t2, the conveying velocity v F (t2) = 0 m / min. is reached and the wire electrode 152 is at bottom dead center UT, where the wire electrode 152 is immersed deepest in the melt bath 202. Short-circuit removal phase KS-EP (Phase II):

[0085] After bottom dead center UT (time t2), the control device 114 causes a further change in the conveying speed v. F (t) into the negative, so that the wire electrode 152 moves away from the melt pool 152. In this short-circuit removal phase KS-EP, the wire electrode 152 is therefore pulled out of the melt pool 152 until the short circuit is resolved (time t3).

[0086] During the short-circuit removal phase, the control device 114 causes a continuously decreasing (negative) acceleration of the wire electrode, resulting in a continuously increasing feed rate, whereby the rate of increase in feed rate, i.e., the acceleration of the wire electrode, decreases. The decrease in the rate of change of feed rate is preferably set such that the (negative) feed rate continues to increase in magnitude over a predetermined distance traveled by the wire electrode since the short circuit occurred, determined by x(t), or over a predetermined time period since the short circuit occurred. The predetermined time period can, for example, be at least 3 ms, more preferably at least 3.5 ms. In this way, the wire electrode is moved away from the melt pool at an ever-increasing speed over a sufficiently long distance or time period to clear the short circuit.If the short circuit has not resolved itself by the end of the period, the conveying speed may increase. F (t) will be further increased, decreased or maintained until the short circuit clears. Arc removal phase LB-EP (Phase III):

[0087] With the short-circuit resolution (time t3) the arc ignites between wire electrode 152 and workpiece 200, and the wire electrode 152 moves away from the melt pool until reaching a top dead center (TDC), at which the wire electrode 152 has the greatest distance to the melt pool.

[0088] Upon detection of the short-circuit resolution, the control unit 114 continuously compares the value x(t) for the current position of the wire electrode 152 with a predetermined distance value xc (phase IIIa). Only when the value x(t) for the current position reaches or exceeds the distance value xc, i.e., a predetermined position, does the control unit 114 cause the (negative) conveying velocity v to change. F (t) is reduced in magnitude, i.e., the wire electrode 152 is slowed down (Phase IIIb). If xc is already exceeded at the time of short-circuit resolution, the control device 114 causes the conveying speed to be reduced in magnitude immediately after short-circuit resolution.

[0089] This position-dependent control of the conveying speed ensures that the wire electrode 152 is moved quickly away from the melt pool to a predetermined minimum distance. This positively influences the melt pool dynamics. The control device 114 then further reduces the conveying speed v by a specific amount. F (t) until the direction changes, i.e. until the top dead center (TDC) is reached.

[0090] Additionally or alternatively, the control unit 114 can control the conveying speed v F (t) after short-circuit resolution, depending on x(t), also control such that the top dead center (TDC) occurs at a given value x OT is achieved.

[0091] In addition to or as an alternative to the conveying speed v F(t) After reaching or exceeding the distance value xc, the control unit 114 can also change the welding current I(t), in particular trigger a melting current pulse to melt the wire electrode, optionally after a predetermined time period has elapsed since reaching or exceeding the distance value xc. In this way, the melting current pulse for melting a droplet can be synchronized to the wire position.

[0092] Preferably, the control device 114 adjusts the rate of change of conveying speed, i.e. the acceleration of the wire electrode 152, such that the top dead center is reached after a predetermined time period (Δt). OT ) is achieved after short-circuit resolution (t3), resulting in a more uniform welding process. Arc approach phase LB-AP (Phase IV):

[0093] After reaching top dead center (TDC), the control device 114 causes a (further) increase in the conveying speed v.F (t), so that the wire electrode 152 moves back towards the melt pool 202, optionally after a predetermined holding time of the wire electrode 152 at the dead center. The rate of increase in conveying velocity, i.e., the acceleration of the wire electrode towards the melt pool 202, can be constant or variable.

[0094] In particular, the wire electrode 152 can be accelerated up to a first predetermined velocity v. F_1 accelerates and then remains constant at v F_1 be held.

[0095] From the reversal of direction at top dead center OT (phase IVa), the control unit 114 compares the value x(t) for the current position of the wire electrode 152 with a predetermined distance value x. D If the value x(t) for the current position is the distance value x D , i.e., when a predetermined position is reached or falls below, the control device 114 causes the conveying speed v to change. F(t) is changed in amount (Phase IVb). The conveying rate v F (t) can be changed in a targeted manner if the wire electrode 152 is at a predetermined distance from the melt bath 202.

[0096] The conveying speed v F (t) can be reduced in particular during phase IVb, for example as in Fig. 3 shown at a predetermined lower speed value v F_2The electrode is lowered. This allows for a greater distance between the wire and the workpiece, preventing the wire electrode from being unnecessarily immersed in the molten pool during the impending short circuit. Furthermore, decelerating the wire electrode causes the liquid phase on the wire to move towards the molten pool faster than the solid phase of the decelerated wire electrode due to its inertia. This stretches the liquid phase on the wire, facilitating droplet detachment. The increased velocity of the liquid phase compared to the solid phase also leads to a rapid spreading of the contact surfaces between the droplet and the molten pool. F_2 For example, it can be in the range of 15 - 60 m / min.

[0097] Alternatively, the conveying speed v F(t) in phase IVb can also be increased, for example to a predetermined higher velocity value. In this way, the short circuit can be actively initiated mechanically. In addition, the increase in the conveying velocity also leads to a higher final velocity of the droplet, thus ensuring a secure bond between the droplet and the melt pool, resulting in rapid expansion of the contact area between the droplet and the melt pool.

[0098] By reducing or increasing the conveying speed v F (t) In phase IVb, the dynamics and shape of the liquid phase at the wire electrode or the droplet can be influenced in order to positively affect the subsequent short-circuit phase. In particular, a high velocity of the liquid phase can be achieved through these measures.

[0099] The control unit 114 can be configured to determine the time t6 at which the value x(t) for the current position equals the distance value x D to predict when the value is reached or exceeded, and to predict the change in the conveying velocity v. F (t), i.e., the acceleration of wire end 152, in phase IVa is adjusted such that time t6 lies within a predetermined range, for example, relative to the short-circuit resolution (t3). In this way, for example, the duration of the arc phase LBP can be kept largely constant. Furthermore, the kinetic energy used to initiate the short circuit can be controlled in this way.

[0100] In addition to or as an alternative to the conveying speed v F (t) the control unit 114 can after reaching or falling below the distance value x DThe welding current I(t) can also be changed. In this way, the welding current intensity can be influenced by the wire position and / or the wire acceleration, i.e., the rate of change of v. F (t), also on dv F (t) / dt, can be synchronized. For example, when the distance value x is reached or fallen below, it can be synchronized. D The termination of an ongoing melting current pulse is initiated to prevent premature droplet detachment.

[0101] Phase IV or IVb ends with the next short circuit (time t7). The welding cycle also ends with the end of phase IV or IVb, and the next welding cycle begins with phase I (so). Since the melting of the wire electrode 152 is neglected when determining x(t), meaning that the actual position of the wire end shortly before the short circuit deviates from the calculated value x(t), and since a droplet transfer occurs at the moment of the short circuit, further shortening the wire electrode, the short circuit only occurs at a position x(t7) < 0 mm. By using the short circuit start point t7 as the new reference position and, for example, setting x(t7) = 0 mm, the control unit again provides a fairly accurate value for the wire position in the subsequent welding cycle.

[0102] Will v FIncreasing the current (t) in phase IVb leads to an upward shift of the liquid phase at the wire electrode. This allows for the use of a high melting current without any droplets detaching from the wire electrode. The shift of the liquid phase thus enables the use of higher arc currents. In this way, the heat input to the melt pool can be adjusted, resulting in, among other things, higher melting rates.

[0103] Additionally, the current shape of the melting current pulse can be changed in such a way that position-dependent influences can be compensated for, depending on the value for the current wire position.

[0104] Furthermore, the control unit 114 can change the welding current I(t) during the short-circuit phase depending on the value for the current position of the wire electrode. For example, the short-circuit current can be regulated in this way depending on the position of the wire in the weld pool in order to influence the pinch forces on the wire.

[0105] Fig. 4 shows further welding cycles SZ n , SZ n+1 of the welding process Fig. 3. Diagrams (a) to (e) in Fig. 4 correspond to diagrams (a) to (e). Fig. 3. The control unit 114 continues to control the procedure as above. Fig. 3 described. The phases and distinguished points in Fig. 4 are labelled with the same names as the corresponding phases and points in Fig. 3.

[0106] As already mentioned Fig. As described in section 3, the control unit 114 activates every time a short circuit occurs (in Fig. 4 at time tKSn , t KSn+1 or t KSn+2 ) the current wire position is set as the new reference position and the value x(t) at the respective short-circuit time t KSn , t KSn+1 or t KSn+2 equals 0 mm. In this way, x(t) is calibrated and adjusted to the position of the weld pool surface at the time of the short circuit at the beginning of each welding cycle. As before to Fig. As explained in section 3, the melting of the wire electrode and the droplet transfer during the short circuit, which are not taken into account when determining x(t), lead to deviations between x(t) and the actual position of the wire end relative to the weld pool surface throughout the welding cycle. Therefore, x(t) shows in Fig. 4 each one jump to the short circuit occurrence, since the control device x(t KS ) sets to zero.

[0107] In Fig. 4 is the position-dependent control of the conveying speed v F(t) is clearly visible in Phase IV. As explained above for Phase IV, the control unit 114 compares the value x(t) for the current position of the wire electrode 152 with a predetermined distance value x from the top dead center OT onwards. D and changes, in particular reduces, the conveying speed v F (t) if x(t) has the distance value x D falls below the threshold. How the comparison of welding cycles SZ n and SZ n+1 in Fig. As shown in section 4, this method achieves the conveying speed v. F (t) is reduced at approximately a constant distance to the subsequent short-circuit occurrence, regardless of the height of the TDC. This is in contrast to the TDC of the welding cycle SZ. n higher OT of the welding cycle SZ n+1 The position-dependent control allows the conveying speed to remain constant for a longer period before it is reduced. This ensures a uniform welding process.

[0108] At the beginning of phase III, the specified position xc is reached during the welding cycles SZ. n and SZ n+1 The threshold has already been reached or exceeded. Therefore, after the short circuit is resolved, the control unit 114 immediately transitions to phase IIIb.

[0109] Fig. 5 shows further welding cycles SZ m , SZ m+1 of the welding process Fig. 3 or Fig. 4. Diagrams (a) to (e) in Fig. 5 correspond to diagrams (a) to (e). Fig. 3. The control unit 114 continues to control the procedure as above. Fig. 3 described. The phases and distinguished points in Fig. 4 are labelled with the same names as the corresponding phases and points in Fig. 3.

[0110] As previously described, the control unit 114 sets up a short circuit every time it occurs (in Fig. 5 at time t KSm , t KSm+1 or t KSm+2) the current wire position is set as the new reference position and the value x(t) at the respective short-circuit time t KSm , t KSm+1 or t KSm+2 equals 0 mm.

[0111] In Fig. 5 is the position-dependent control of the conveying speed v F (t) is clearly visible in Phase III. As above. Fig. As described in section 3, in phase III, after short-circuit resolution, the control unit 114 compares the value x(t) for the current position of the wire electrode 152 with a predetermined distance value xc and reduces the conveying speed v. F (t) in absolute value, if x(t) exceeds the distance value xc. For the welding cycles SZ m and SZ m+1 in Fig. In step 5, the short-circuit phase is quite short. This leads to the specified distance value xc (compared to the welding cycles SZ) being exceeded. n and SZ n+1 in Fig. 4) is only achieved after a longer period of time and the absolute reduction in the conveying speed v F (t) accordingly delayed. As the comparison of welding cycles SZ m and SZ m+1 in Fig. 5 shows that this duration is at SZ m and SZ m+1 of different lengths, as the wire electrode is used in the welding cycle SZ. m at the time of short-circuit resolution, it still has to travel a longer distance than during the welding cycle SZ. m+1 , to reach the specified position x c to reach.

[0112] In Fig. 4 and Fig. Figure 5 further illustrates the position-dependent control of the welding current I(t). As above. Fig. As described in section 3, in phase III, the control device 114 triggers a melting current pulse to melt the wire electrode after a predetermined time period has elapsed since reaching or exceeding the distance value xc by x(t), and in phase IV, after a predetermined time period has elapsed since reaching or falling below the distance value x D Terminating the melting current pulse to prevent premature droplet detachment.

[0113] At the welding device 100 in Fig. 1. The present document concerns a welding device for manual welding. However, the teaching described here is not limited to welding devices for manual welding; rather, the welding device can also be a welding device for automated welding, for example, using a welding robot. The same applies to the described control device and the described method. Reference symbol list: 100 welding devices 110 welding power source 112 Power section 114 Control unit 115 microprocessor 116 storage 118 electrical output 119 Management 122 User interface 150 wire feeder 152 Wire electrode 154 wire electrode stock 156 primary wire electrode feeder 160 Control unit Entrance 162 164 Admission 165 Gas pipeline 166 Shielding gas source 168 Burner connection 169 Valve 180 welding torches 182 Burner part 184 Hose package 185 Wire guide 186 secondary wire electrode conveying device 187 Conveyor speed and / or conveying path detection device 188 burner buttons 190 wire storage 192 spring-loaded roller 200 workpieces 202 Melt bath QUOTES INCLUDED IN THE DESCRIPTION

[0000] This list of documents cited by the applicant was automatically generated and is included solely for the reader's convenience. The list is not part of the German patent or utility model application. The DPMA accepts no liability for any errors or omissions. Cited patent literature

[0000] EP 1 563 938 B1

[0003] EP 3 509 784 B2

[0003]

Claims

Control device (114) for a welding device (100) with at least one microprocessor (115) and at least one memory (116) containing instructions, the execution of which on the at least one microprocessor causes an arc welding process to be carried out, in accordance with a method for arc welding with a consumable wire electrode (152) comprising a plurality of welding cycles (SC), each having a short-circuit phase (SC) and an arc phase (ARC), wherein in the method the wire electrode (152) is fed at a variable feed rate (vF(t)) and wherein in the method the feed rate (vF(t)) and / or the welding current (I(t)) is changed depending on a value (x(t)) for the current position of the wire electrode (152), in particular when the value (x(t)) for the current position of the wire electrode (152) reaches, in particular exceeds or falls below, a predetermined position (xc, xD). Control device according to claim 1, characterized in that the arc phase (LBP) has an arc approach phase (LB-AP) in which the wire electrode (152) is conveyed towards a melt pool (202), and during the arc approach phase (LB-AP) the conveying speed (vF(t)) and / or the welding current (I(t)) is changed depending on a value (x(t)) for the current position of the wire electrode (152). Control device according to claim 1 or 2, characterized in that in the method the value (x(t)) for the current position of the wire electrode (152) is determined depending on a reference position of the wire electrode (152) and the conveying speed (vF(t)) or a conveying path (sF(t)). Control device according to one of claims 1 to 3, characterized in that in the method the reference position is determined depending on the position of the wire electrode (152) at the time of short-circuit inception and / or short-circuit resolution of the current and / or a previous welding cycle (SC). Control device according to one of claims 1 to 4, characterized in that the short-circuit phase (KSP) has a short-circuit removal phase (KS-EP) in which the wire electrode (152) is conveyed away from the melt bath (202), wherein in the method the conveying speed (vF(t)) of the wire electrode (152) is increased in magnitude during the course of the short-circuit removal phase (KS-EP), preferably with decreasing acceleration. Control device according to claim 5, characterized in that in the method the conveying speed (vF(t)) of the wire electrode (152) is increased in magnitude during the course of the short-circuit removal phase (KS-EP) until the expiry of a predetermined time since the occurrence of the short circuit or, if a short-circuit resolution occurs before the expiry of the predetermined time, until the short-circuit resolution. Control device according to one of claims 1 to 6, characterized in that the arc phase (LBP) has an arc removal phase (LB-EP) in which the wire electrode (152) is conveyed away from the melt bath (202), wherein in the method the conveying speed (vF(t)) of the wire electrode (152) is reduced in magnitude during the course of the arc removal phase (LB-EP) until the direction is reversed, preferably only from a time point which depends on the value (x(t)) for the current position of the wire electrode (152). Control device according to claim 7, characterized in that in the method the rate at which the conveying speed (vF(t)) of the wire electrode (152) is reduced in magnitude during the course of the arc removal phase (LB-EP) until the reversal of direction is set such that the reversal of direction is achieved after a predetermined time period since short circuit resolution. Control device according to claim 7 or 8, characterized in that in the method the conveying speed (vF(t)) of the wire electrode (152) in the area of ​​the direction reversal is kept in magnitude less than or equal to a predetermined speed value for a predetermined period of time. Control device according to one of claims 1 to 9, characterized in that the method has a plurality of pulse process welding cycles without short-circuit phase (KSP), wherein preferably a parameter of a pulse process welding cycle following a welding cycle (SZ) with short-circuit phase (KSP) is set depending on the value (x(t)) for the current position of the wire electrode (152). Welding device (100) comprising a control device (114) according to one of claims 1 to 10 .