DEVICE AND METHOD FOR COMPOSING FIBER-PLASTIC COMPOSITES AT HIGH APPLICATION GRADS
Patent Information
- Application Number
- DE502016016797
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2015-12-16
- Filing Date
- 2016-12-15
- Publication Date
- 2024-12-05
- Estimated Expiration
- 2036-12-15
AI Technical Summary
Current methods for producing composite materials, particularly fiber-plastic composites, face limitations in process speed and uniform heat input, leading to inefficiencies in production and potential material degradation.
A method and system for composing fiber-plastic composites that involves a semi-finished product being moved at a tool center point speed of greater than or equal to 0.5 m/s with a heating device setting a temperature gradient to partially melt the material, and a composition system with a stable base group, drive unit, and heating source to achieve high-speed, uniform application and consolidation.
This approach significantly increases process speed, ensures uniform heat input, and reduces material degradation, enabling the production of high-quality fiber-plastic composites with improved efficiency and reduced cycle times.
Description
Field of the invention
[0001] The invention relates to a method for composing fiber-plastic composites and a corresponding composition plant. Background and general description of the invention
[0002] Components made of composite materials offer numerous advantages, such as their low weight combined with high load-bearing capacity, particularly when fiber materials are embedded in the fiber direction. However, an increase in the process speed for manufacturing composite components would be desirable, especially for series production.
[0003] In working processes for the production and processing of fiber and / or polymer semi-finished products into composite materials in a partially plastic state, the physical parameters pressure, temperature and time (speed) for processing are typically controlled or regulated.
[0004] In the context of the automated production of composite materials through the directionally and positionally variable deposition of unidirectional fiber semi-finished products, processes are referred to differently in international terminology. For example, the terms "tape laying," "tape / tow placement," "fiber placement," "automated fiber placement" (AFP), or "automated tape laying" (ATL) are commonly used. Generally, these processes refer to partially or fully automated processes for the production of composite materials or preforms with continuous fiber reinforcement on curved or flat structures.
[0005] The manufacturing processes originated in the production of complex, lightweight, and corrosion-resistant aircraft fuselage structures. Initially, the focus was on processing thermoset prepregs, which were subsequently expanded to include thermoplastic semi-finished products and constrained materials. Using semi-automated, hand-guided lay-up devices, manual lay-up processes for unidirectional and multiaxial prepregs could be replaced with rotationally symmetric components.
[0006] The AVSD (Automated Variable Strand Dispensing Head) concept is well known. It uses numerical control (NC) technology to deposit pre-impregnated rovings onto flat and slightly curved surfaces. The first commercially viable system was delivered to General Dynamics by The Ingersoll Milling Machine Company in 1978.
[0007] The need to manufacture more complex components gave rise to multi-tape laying processes. Up to 32 pre-impregnated, unidirectional semi-finished products are individually transported and cut in a complexly designed application device. This is achieved using a robot unit and an external rotation axis.
[0008] At the same time, the first systems for processing thermoplastic semi-finished products were set up in the laboratories of research institutes in the early 1980s. The objective of this development was to combine the knowledge gained from thermoset semi-finished products with the advantages of thermoplastic semi-finished products. Compared to thermoset fiber-reinforced plastics, these composites offer virtually unlimited storage life, processability in non-climate-controlled environments, autoclave-free processing through inline consolidation, excellent impact properties, exceptional chemical resistance for semi-crystalline thermoplastics, meltability, formability, weldability, short processing cycles, and solvent-free processing.
[0009] The autoclave-free production is particularly noteworthy, as this eliminates a very time-consuming and cost-intensive production step.
[0010] Due to the complexity of interacting process parameters and the joining mechanisms that still need to be researched, numerous dissertations and scientific papers in this field have been published in Europe and the USA since the mid-1990s. An overview can be found, for example, in the publication "Automation implementation and process development of thermoplastic tape placement for 3-dimensional parts," Steeg et al., SAMPE, 42, 5 (2006), pp. 18-24.
[0011] During the consolidation phase, the substrate and the semi-finished product undergo phase changes (viscoelastic vs. liquid vs. viscoelastic). Various physical models have been developed for this purpose, describing and verifying different constellations of the process parameters pressure, temperature, and time. The focus is on a quantitative and qualitative description and derivation of all key influencing factors of the joining process. This systematic approach applies to all polymers.
[0012] This modeling approach is illustrated for thermoplastic joining mechanisms as an example. Typically, a "bringing-into-contact" model and an "autohesion" model are distinguished. Dara and Loos (Dara, PH; Loos, A.: Thermoplastic Matrix Composite Processing Model. Virginia Polytechnic Institute Report, Report CCMS-85-10, (1985)) described the "bringing-into-contact" of imperfect surfaces with a roughness as rectangles that expand under pressure (consolidation pressure). Others have extended or simplified this model with different time-dependent, material-dependent, or geometric boundary conditions.
[0013] However, the aforementioned physical and theoretical models are not defined for liquid phases, very high heating rates, and / or highly dynamic, transient changes in material properties. Therefore, their potential for adapting control and regulation parameters in processing technology is limited.
[0014] If the contact surfaces are brought together, it is assumed that the polymer chains can diffuse through the interface. The mechanical entanglement / interlocking of the freely moving molecular chains creates a mechanically resilient bond. This polymer-physical phenomenon is called autohesion. However, the mobility of the molecular chains is limited. For example, de Gennes formulates these entanglement and interlocking mechanisms in his reptation models (de Gennes, P.-G.: "Reptation of a polymer chain in the presence of fixed obstacles". The Journal of Chemical Physics, 55, 2 (1971), pp. 572-579).
[0015] The dependencies between contact surfaces and mechanical properties based on material properties, pressure, temperature, and time can also be modeled. The quality of tensile strength and fracture energy are related to the contact time tc. It can be determined that a cohesive sample bonded over time tr can typically no longer be differentiated from a homogeneous polymer. Zugfestigkeit Zugfestigkeit ∞ = t c t r 1 4 Bruchenergie Bruchenergie ∞ = t c t r 1 2
[0016] The degree of autohesion can be determined according to Dara and Loos as follows: D A = D A0 + K T ⋅ t c 1 4 t c = a T ⋅ t c ,ref a T = − C 1 ⋅ T − T ref C 2 + T − T ref Williams − Landel − Ferry D A = K 0 ′ ⋅ a T ⋅ t c ,ref 1 4
[0017] Lee and Springer developed an alternative approach: D A = χ ⋅ t c 1 4 χ = χ 0 ⋅ exp − E a k ⋅ T Arrhenius
[0018] The difference between Dara and Loos and Lee and Springer is the method of determining the pre-exponential factors or proportionality constants. The Williams-Landel-Ferry relationship is more applicable to amorphous plastics, whereas the Arrhenius relationship is applicable to crystalline or semi-crystalline polymers.
[0019] The quality of autohesion can also be linked to the temperature-dependent viscosities in the melt: t c = T c ,ref ⋅ a T η 0 T = η 0 T 0 ⋅ a T η 0 T = η 0 T 0 ⋅ exp E 0 k 1 T − 1 T 0 Arrhenius
[0020] The temperature dependence of polymers can also be described using an Arrhenius model. For rapid processing processes that rely on low viscosities, the highest possible temperature should therefore be chosen.
[0021] Degradation is a natural limitation. Above the melting temperature, there is a temperature range in oxygen exposure in which predominantly oxidative decomposition occurs over a period of time. This is the degradation of the matrix. The degree of degradation and the duration of exposure can be compared. Nam and Seferis, for example, defined in a degradation model that the mechanical properties only decrease significantly with a loss of molecular weight of more than 0.06%.
[0022] The patent DE 10 2012 102 841 B3 shows an automatable process for applying a binder to a semi-finished fiber product using a fuel gas nozzle.
[0023] The publication WO 2013 / 139 834 A1 also points to the processability of staple fibers in automated deposition processes.
[0024] CN 104 985 834 A describes an infrared heating system for high-speed fiber placement in an ATL device. According to CN 104 985 834 A, various speed ranges for fiber placement can be set. However, the known methods or devices do not allow for satisfactory process speeds.
[0025] It is therefore an object of the present invention to provide a composite assembly system for composite materials that eliminates or improves the aforementioned disadvantages. In particular, the present invention aims to significantly increase the process speed.
[0026] A further aspect of the invention is to realize a uniform heat input into the fiber-plastic composite.
[0027] Yet another aspect of the invention is to provide a space-saving device.
[0028] Further tasks arise from the following description or the special advantages achieved with certain embodiments.
[0029] The object is achieved by the subject matter of the independent claims. Advantageous embodiments are the subject matter of the dependent claims.
[0030] In the method according to the invention according to claim 1 for composing fiber-plastic composites, a semi-finished product is first provided in a storage device.
[0031] The semi-finished product may, for example, comprise a fiber semi-finished product, a polymer semi-finished product and / or a self-reinforced polymer or a combination thereof.
[0032] The semi-finished product may further comprise, for example, fully consolidated, partially consolidated, hindered, wetted semi-finished products or combinations thereof.
[0033] Furthermore, the semi-finished product may comprise thermosets, thermoplastics, elastomers, their derivatives and / or combinations thereof.
[0034] In other words, the semi-finished product is typically a fiber-plastic material provided in strip form, in particular in roll form, wherein the fiber-plastic composite to be produced by the method or device is produced by repeated, for example, strip-by-strip and / or layer-by-layer application of layers of fiber-plastic material.
[0035] The semi-finished product provided is fed to an application device for further use according to the method according to the invention.
[0036] The next step of the process involves performing a relative movement between the application device and an application area to which the fiber-plastic composite can be applied using the application device. During this relative movement, the semi-finished product is applied to the application area using the application device.
[0037] In other words, the application or application of the semi-finished product to the application area takes place during a relative movement between the application area and the application device. For example, and preferably, the application device is moved, i.e., in particular, traveled on rails. However, it is also possible for the application area to be moved relative to the application device and, particularly advantageously, for both the application device and the application area to undergo a movement, so that the relative movement between the application device and the application area is achieved by a counter-directional movement of both the application device and the application area.
[0038] According to the invention, the relative movement between the application device and the application area is carried out with a tool center point speed of greater than or equal to 0.5 m / s.
[0039] During application of the semi-finished product to the application area, a heating device can advantageously be adjusted such that a temperature gradient of the heat distribution can be established across the thickness of the semi-finished product. Using the temperature gradient of the heat distribution, the semi-finished product can, for example, be heated in such a way that it is only partially melted.
[0040] It is also possible to adjust the heating device such that the heat energy stored in the semi-finished product is less than 40% of the heat energy required by the semi-finished product for complete melting. Preferably, the heat energy emitted by the heating device and stored in the semi-finished product is set to less than 20% of the heat energy required by the semi-finished product for complete melting.
[0041] The heating device can further be adjusted in such a way that a phase change occurring in the semi-finished product changes the morphology of a polymer of the semi-finished product only in the edge zone.
[0042] A composition plant according to claim 4 for composite materials, which is particularly suitable for carrying out the method described above, firstly comprises a floor assembly which provides the application area. In other words, a floor assembly is provided which is preferably designed to be as stable as possible, i.e. for example is designed to be very heavy, i.e. in particular has a mass which is a factor of 1,000,000 or more greater than the web-related mass of applied semi-finished products and / or is bolted to the floor, so that a corresponding mass and thus a high level of damping against vibrations and movements generated by dynamic loads is maintained. In particular, the floor assembly is considerably heavier than the moving mass of the composition plant (during operation of the composition plant). For example, the floor assembly is a factor of 10, 50 or even 100 heavier than the moving mass of the composition plant.In the simplest example, the moving mass of the composition system is combined in the application device, so that the floor assembly is a factor of 10, 50 or even 100 heavier than the mass of the application device.
[0043] The composition system further includes a storage device for providing a semi-finished product for further processing in the composition system. An application device is provided for applying the semi-finished product to the application area.
[0044] The assembling system further comprises a drive unit for changing the position of the application device relative to the application area, wherein the drive unit provides a tool center point speed for the application device during the time phase during which the semi-finished product is applied to the application area. In other words, the drive unit moves the application device, for example, along rails. In a preferred embodiment, the rails are also adjustable in a plane perpendicular to the direction of extension of the rails, so that the drive unit can move the application device in two preferably mutually perpendicular directions.
[0045] The application device comprises a heating device or a heat source for heating the semi-finished product, so that a local phase change of the semi-finished product into an at least partially plastic state can be induced. The heat source preferably acts on the semi-finished product a few millimeters to centimeters before its application to the application area.
[0046] According to the invention, the drive unit interacts with the application device in such a way that the semi-finished product is applied to the application area in a direction and position variable manner with a tool center point speed of greater than or equal to 0.5 m / s.
[0047] In a preferred embodiment, the drive unit can be configured to keep the tool center point speed (vTCP) constant or substantially constant for the time range during the application of the semi-finished product to the application area. A substantially constant tool center point speed (vTCP) exists, for example, when the vTCP fluctuates by equal to or less than ±2%, less preferably equal to or less than ±5%, or even less preferably equal to or less than ±10%. In other words, a correlation between the speed of the application device and the feed rate of the semi-finished product can be realized such that the semi-finished product is only applied when a constant or substantially constant relative speed exists between the application device and the application area.
[0048] In a preferred embodiment, the heat source is configured to establish a temperature gradient of the heat distribution across a thickness of the semi-finished product when heating the semi-finished product. In other words, in this embodiment, the heat source induces just enough heat energy into the semi-finished product that the heat energy is not evenly distributed across the thickness of the semi-finished product, i.e., does not completely penetrate the semi-finished product. Rather, the heat source induces just enough heat energy to create a melting zone on the surface of the semi-finished product and to heat up the deeper layers of the semi-finished product less than at the surface, so that in particular the deeper layers of the semi-finished product remain in a solid state during application to the application area.
[0049] Alternatively or cumulatively, the heat source may preferably be designed to concentrate the melting zone on the joining surfaces when heating the semi-finished product or even to limit it substantially thereto.
[0050] In a further advantageous embodiment, the drive unit is designed to accelerate the application device with an acceleration of greater than or equal to 8 m / s 2< , more preferably greater than or equal to 20 m / s 2< or particularly preferably greater than or equal to 50 m / s 2<. In other words, the dynamic performance of the drive unit is preferably large enough to accelerate the application device with the aforementioned accelerations. However, the achievable acceleration will probably not be greater than 100 m / s 2<, since excessive accelerations can reduce the service life of the moving or moving parts of the composition system, or angular errors can occur when applying the semi-finished product to the application area.
[0051] Furthermore, the sum of the moving masses of the application device and the drive unit is preferably less than 750 kg. Reducing the moving masses can improve the control of the application device such that very precise placement and coordination of the application device is possible at very high speeds and / or accelerations.
[0052] Furthermore, the sum of the moving masses of the application device and the drive unit together is preferably equal to or less than 250 kg and even more preferably equal to or less than 75 kg.
[0053] The assembly of fiber-reinforced plastic composites from semi-finished products on the application area can preferably take place successively along predefined paths. In other words, a linear path, i.e., a straight deposit piece, can be specified by a controller, with the application device traversing the predefined linear path and depositing the semi-finished product on the application area.
[0054] In one embodiment, the track paths can also be curved in the plane or spherically curved. Thus, the application area can also have a curved surface.
[0055] In one embodiment of the invention, at least one further semi-finished product is included which differs from the semi-finished product. In other words, two different semi-finished products can be stored, for example, in the storage device. The storage device can then in particular provide both semi-finished products, i.e. operate in such an automated manner that the desired semi-finished product can be made available. The storage device can therefore be designed to feed the semi-finished product and the further semi-finished product alternately to the application device, so that fiber-plastic composites can be produced from different semi-finished products. In this way, more than two semi-finished products can be kept in the storage device, so that a selection can be made from a large number of semi-finished products. In a preferred embodiment, the material used for the semi-finished product and / or the dimensions (e.g. width or thickness) of the semi-finished product can differ.
[0056] In a further embodiment, the composition of fiber-reinforced plastic composites is enabled individually for each web path. In other words, before each subsequent web path is controlled by the application device, the semi-finished product provided by the supply device can be selected and applied web by web, for example, alternately.
[0057] In one embodiment, the composition system may comprise a synchronization system for electronically synchronizing the speed of the drive system (tool center point speed) and a feed speed of the semi-finished product.
[0058] In one embodiment, the assembling system is configured to keep the tool center point speed of the semi-finished product essentially constant during the application of the semi-finished product to the application area. In other words, after an acceleration phase, the semi-finished product is applied in a phase without acceleration of the application device, whereby the application of the semi-finished product is terminated before the application device is decelerated after the end of the path. The application device is particularly configured to also keep the feed rate of the semi-finished product essentially constant during the application of the semi-finished product.
[0059] The drive unit can comprise a direct drive. A direct drive can be an electric motor that provides the drive power without an intermediate gear or other intermediate components. The application device can also comprise a direct drive for advancing the semi-finished product. The drive unit and / or the application device, or even preferably all drives of the assembling system, can be equipped with a high-resolution measuring system for measuring the movement.
[0060] The heat source can be controlled and regulated to cause a phase change to a partially plastic state of the polymer components of the semi-finished product. In other words, in one embodiment, the heat source is adjustable, i.e., preferably controllable, in terms of the type of heat penetration (e.g., the firing depth), the heat output, and / or the geometric heat exposure (e.g., the width of the heat exposure). The heat source preferably comprises, for example, a burner nozzle, a plasma source, a halogen, a laser, and / or an LED source, the respective energy density of which is optimized, in particular, for use in the composition system.
[0061] According to the invention, the assembly system comprises an electronic control system for the integrated control of all systems, which preferably provides a cycle time of less than or equal to 1000 µs, in particular for the electronic synchronization of the speed of the drive system (tool center point speed) and the feed rate of the semi-finished product of the application device. The electronic control system preferably implements a joint synchronization of the speed of the drive system, a speed of the cutting unit, and the feed rate of the semi-finished product, which is implemented by the application device.
[0062] The electronic control system preferably comprises a multi-core architecture. In other words, the electronic control system has multiple processing cores that can execute various processes for controlling the composition system in parallel.
[0063] In particular, different tasks can be assigned to different cores. The cycle times of the different tasks can also differ. In a preferred embodiment, a cycle time of less than 100 µs can be provided in at least one task, more preferably less than 50 µs, even more preferably less than 10 µs, and even more preferably less than 2 µs.
[0064] The electronic synchronization of the systems is particularly preferably based on a real-time protocol.
[0065] The drive unit and the application device can be synchronized via a motion control system, which, in conjunction with a controller, ensures quasi-synchronous control. In other words, the drive unit and the application device are electronically coupled to each other in such a way that they are controlled synchronously, so that, in particular, the application speed is similar to or identical to the feed rate.
[0066] In a further embodiment, the application area comprises a thermally insulating medium. A thermally insulating medium is, for example, a medium with a thermal conductivity of less than or equal to 1 W / (m·K) for polymeric materials or 3.5 W / (m·K) for inorganic materials. In this embodiment, at least a first layer or a first web of the semi-finished product is applied directly to the thermally insulating medium.
[0067] In a preferred embodiment, the thermally insulating medium has a planar extent with a thickness in the range between 0.05 mm and 5 mm.
[0068] In yet another embodiment, the base assembly provides a negative pressure, wherein the thermally insulating medium is held to the base assembly by the negative pressure. For example, the base assembly comprises a tool that rests flat against it. In other words, the thermally insulating medium can be held to the tool by negative pressure. The negative pressure can, for example, be adjusted such that the thermally insulating medium is sufficiently fixed during application to prevent any movement relative to the base assembly.
[0069] The base group may alternatively or cumulatively have a fixing device so that the thermally insulating medium is fixed to the base group by means of the fixing device.
[0070] Alternatively or cumulatively, the base group can create an electric field to the thermally insulating medium, so that the thermally insulating medium is fixed to the base group by the electric field.
[0071] Preferably, the thermally insulating medium is a polymer, an elastomer, a composite material or an inorganic material.
[0072] It is therefore preferred that the thermally insulating medium is fixed to the base group.
[0073] A carrier film can be removably applied to the thermally insulating material. The carrier film can be applied, for example, adhesively and / or electrostatically.
[0074] It is advantageous to apply at least a first layer or first web of the semi-finished product directly to the carrier film.
[0075] It is also advantageous if the carrier film can be removed from the thermally insulating material without leaving any residue and / or the carrier film can be removed from the fiber-plastic composite without leaving any residue.
[0076] In a further preferred embodiment, the application area can undergo consolidation or partial consolidation with the semi-finished product applied thereto, so that the semi-finished product is firmly bonded to the application area. In other words, in this embodiment, a fiber-plastic composite is already created by applying the first layer of the semi-finished product to the application area, since the semi-finished product already forms a bond with the application area.
[0077] Using the application device, a semi-finished product can also undergo consolidation or partial consolidation with an already applied semi-finished product and / or with a pre-assembled semi-finished product. This is the case, for example, when the semi-finished product is placed on an already applied semi-finished product. In this case, the semi-finished product is firmly bonded to the already applied semi-finished product, whereby the degree of bonding can be adjusted on a path-specific basis, particularly via adhesion, autohesion, or cross-linking, for example through the flexible control of the physical process variables of pressure (consolidation), temperature, and time (high speed).
[0078] In the semi-finished product, polymer diffusion or cross-linking in the boundary layer can be preferentially induced by the heat source during application.
[0079] In a further preferred embodiment, a second application device is included, which is also movable by the drive unit for the alternate or simultaneous application of two semi-finished products to the application area. The second application device is preferably movable independently of the application device for the simultaneous or staggered application of at least two semi-finished products in the application area.
[0080] Preferably, a plurality of coupled application devices is also used. The plurality of coupled application devices can be coupled by parallel arrangement. Furthermore, the plurality of coupled application devices can be fixedly mounted to the base assembly. In this case, the application area can be rotatably mounted and configured to perform a translation on the base assembly. This ensures that coverage of the application area, in particular full coverage of the application area during traversal, can be achieved.
[0081] The drive unit and the application device are particularly attached to the floor assembly and arranged above the floor assembly, thus ensuring a compact and space-saving design of the composition system.
[0082] The composition system may comprise an input device for entering track start and end points or for entering track paths.
[0083] The composition system can further preferably independently determine parameters for controlling the drive unit and the application device and control the drive unit and the application device based on the parameters.
[0084] In a further embodiment, a tool center point speed of greater than or equal to 0.5 m / s is realized. In other words, the application device moves relative to the application area during application of the semi-finished product at a speed of greater than or equal to 0.5 m / s. Preferably, a tool center point speed of greater than or equal to 2 m / s, more preferably greater than or equal to 5 m / s, and further preferably greater than or equal to 10 m / s is realized.
[0085] The composition system can further comprise at least one position sensor for determining the position of the application device. The position sensor allows feedback, for example, to the control device, so that the position of the application device can be verified.
[0086] The storage device can further comprise a free loop for forming a buffer for the semi-finished product. In one embodiment, this loop can have a voltage control unit. In another embodiment, the charges generated by friction can be dissipated via an electrically conductive brush.
[0087] The storage device can further comprise a dancer unit for forming a semi-finished product buffer. In one embodiment, the dancer unit is force- and displacement-controlled; in a preferred embodiment, it is force- and displacement-controlled.
[0088] The storage device can comprise a catching device for the safe feeding of the semi-finished product into the application device.
[0089] The angle (α) of the heating source to the substrate is adjustable in a preferred embodiment of the heating source, wherein more preferably the angle of the heating source to the substrate (α) is approximately half as large as the angle of the inlet of the semi-finished product onto the substrate (β).
[0090] The heating device can be designed in such a way that, per millimeter of semi-finished product width (mm-Hb), it has a heating device mass of less than 200 g / mm-Hb, preferably less than 120 g / mm-Hb, more preferably less than 100 g / mm-Hb. With the present invention, it is even possible to achieve a heating device mass of equal to or less than 25 g / mm-Hb. A particularly low heating device mass can, for example, further reduce the moving mass of the composing system and thus enable higher accelerations of the moving mass, i.e. in particular of the application device. In other words, the heating device can be adapted depending on the semi-finished product widths expected to be processed so that the most compact and lightweight heating device possible is available.
[0091] The heating device can further be designed to generate a relative power in relation to the semi-finished product width (mm-Hb) of equal to or more than 20 W / mm-Hb multiplied by the tool center point speed (vTCP [m / s]), preferably equal to or more than 100 W / mm-Hb * vTCP, and / or a relative power of up to 300 W / mm-Hb * vTCP.
[0092] The heating device may comprise a fuel gas nozzle. In this case, the heating device is a fuel gas heating device.
[0093] An ignition device may also be included to ignite the fuel gas. In this case, the ignition device can ignite the fuel gas, for example, with an arc and / or an ignition spark.
[0094] The fuel gas flows out, for example, a few millimeters before the ignition point, depending on the path. It is particularly preferred that the fuel mixture can be ignited at the path-related ignition point with a precision of ± 0.5 mm or more. The ignition device is preferably operated at 5 to 30 kV.
[0095] In a preferred embodiment, the fuel gas nozzle can be designed to create a protective gas environment in the area around the joining surfaces during operation using the fuel gas / exhaust gas mixture produced during combustion. In other words, the fluid flow exiting the fuel gas nozzle is directed, directed, or focused in such a way that the fuel gas / exhaust gas mixture is concentrated in the area of the joining surfaces. This creates a low concentration of free oxygen atoms at the joining surfaces. This low concentration of free oxygen atoms, in turn, can reduce the degradation of the semi-finished products and thus potentially increase the service life and / or the load-bearing capacity of the produced composite material.
[0096] In a further embodiment, it has proven advantageous if the semi-finished product comprises spherulites, pigments, and / or embedded fiber materials, since by varying such materials and / or polymer structures in the semi-finished product, a gradient of the heat distribution of the thermal energy introduced into the semi-finished product by the heating device can be better adjusted. In other words, the location and / or shape of the melting zone can be adjusted by using spherulites, pigments, and / or embedded fiber materials.
[0097] In one embodiment, the heating device comprises optical fibers for transporting the thermal energy. In other words, a heat source can be arranged remotely from the semi-finished product or the substrate, wherein the heat can be transported, for example, in the form of waves such as thermal radiation, or also in the form of laser radiation through the optical fiber to the semi-finished product or the substrate. The heating device can preferably comprise at least one laser module, in particular at least one diode laser module. The energy from these modules can be transported via optical fibers. For example, diode laser modules that are used in laser marking systems can be used.
[0098] In one embodiment, the heating device can have several, in particular different, heat sources for adjusting the melting zone. Particularly when changing the semi-finished product, for example, when there is a change in the heat capacity, a change in the melting temperature of the semi-finished product, or changes in the thickness and / or width of the semi-finished product, it is advantageous if the heating device already has several heat sources. This may enable a shorter waiting time when changing semi-finished products and thus - ultimately - a shorter downtime between the application of the semi-finished product to the application area. The compositing system can have several heating devices, which is advantageous, for example, when applying semi-finished products in different directions.
[0099] Preferably, the heating device can generate the melting zone individually for each path. This is particularly advantageous if, for example, the heat source is operated at a different setting for a first path than for a subsequent path.
[0100] In a further embodiment, the translational drives of the drive unit can be arranged in the center of gravity of the mass to be accelerated, i.e., in particular, the application device. The translational drives of the drive unit can preferably also be arranged within a range of ±100 mm around the center of gravity of the mass to be accelerated.
[0101] In summary, one aspect of the present invention is based on the fact that, in conventional methods, one or more semi-finished fiber products with a low mass are processed using a device, whereby the moving mass of the device is many times greater than the semi-finished fiber products. The gantry systems and articulated arm robots typically used in the past, together with the application unit, must precisely accelerate and decelerate a moving mass of between 750 kg and 25 t along the track path. The drive power required for this can be derived using the physical approach force = mass x acceleration. During the acceleration and deceleration phases, the application speed is not constant. This leads either to readjustment of the temperature control or to uneven energy input into the semi-finished products.
[0102] In other words, the lack of dynamic performance of the drive unit, in particular the dynamic performance for accelerating the moving mass of the composition system, can already limit the possible application range that can be used with a constant tool center point speed. It is preferred that the dynamic performance of the composition system defines the dimensions of the application range. It is further preferred that the dynamic performance of the drive unit be configured in such a way that the operable application range is maximized.
[0103] These relationships also result in a strong restriction of the minimum achievable cycle time for manufacturing the component or a preform.
[0104] Another key factor is the thermodynamic controllability of a heat source. For high application speeds and the establishment of a defined melting behavior of the polymer components, it is advantageous to generate high heat energies of, for example, several hundred or thousand watts concentrated on a small area of the melting zone. Studies have shown that it is particularly complex to dynamically control or regulate this energy for an application speed at a varying tool center point speed in order to maintain a constant energy input into the semi-finished product. It is advantageous to digitally switch the heat source with the high energy densities on or off. For a defined consolidation or partial consolidation behavior or crosslinking behavior, the heat source settings for a constant tool center point speed can be determined and these can, for example,must be kept constant for the application of at least one lane.
[0105] Within the scope of the present invention, it was recognized that even higher application and processing speeds can be achieved with a device and method for assembling fiber-plastic composites if the moving masses of the device are advantageously significantly reduced. Therefore, a dynamic, electronic synchronization of the movement of multiple axes was developed, using powerful drives, a powerful control system, and lean PLC programming, which can be used to further improve and develop the present invention.
[0106] The ratio of drive power to moving mass can be advantageously optimized and precisely controlled under the boundary conditions of the stiffness and strength requirements of the fiber-plastic composite.
[0107] These processes enable fiber orientation to be tailored to requirements and a freely selectable positioning of the reinforcement phase in the component.
[0108] It is also possible to use these technologies for local, load path-oriented reinforcement.
[0109] The semi-finished products can have a wide variety of geometries, and the composition of fibers and matrices can be freely selected within the limits of physical possibilities. Furthermore, a distinction is made between binder-enriched, partially consolidated, and fully consolidated semi-finished fiber products based on the impregnation state and the mass and volume ratios.
[0110] The presented invention thus solves the problem of producing a fiber-plastic composite, which can be composed of a wide variety of fiber and / or polymer semi-finished products, self-reinforced polymers and / or pre-stretched polymers, or combinations thereof, in a fully automated, directionally and positionally variable manner. Furthermore, the presented invention has a compact design, allowing for a reduction in space requirements compared to prior art systems.
[0111] The functional principle of the composition of fiber-plastic composites is essentially formed by the translation provided by a drive unit and the deposition of semi-finished products via an application device.
[0112] For this purpose, the operator can define path start points and end points, or path paths, and enter them via a user interface. Alternatively or cumulatively, these can be read in from other devices via an interface. The entry of path start points and end points, or path paths, can preferably also be possible per path or per shift.
[0113] In one embodiment, path-relevant events and / or process parameters are calculated before each path movement based on the entered path start and end points. Process parameters can be both speed-dependent and speed-independent.
[0114] Process parameters include, for example, locations where events can occur or must be triggered. Process parameters can be calculated based on design-specific machine constants. A machine constant, for example, could be the minimum deposition length. Process parameters can be speed-dependent distances in the unit [mm], speed-independent process-relevant locations in the unit [mm], or parameters that remain constant over the course of a path, such as the angle of the application unit around the Z-axis.
[0115] A speed-dependent process parameter can, for example, be the pre-travel distance for starting the semi-finished product transport in order to ensure that the path start point coincides exactly with the required deposition start point.
[0116] Speed-independent process parameters can be, for example, the path-related locations of the cutting process, path start and end points or start and end points. Events can be, for example: Cutting the semi-finished product Starting the semi-finished product transport Stopping the semi-finished product transport Heating source on Heating source off Ignition on Ignition off Lowering the application unit Raising the application unit Selecting the direction of the semi-finished product "duplex"
[0117] All parameters can be stored in a buffer. The calculation can take place before the actual movement.
[0118] Acceleration and deceleration processes of the drive unit can preferably be automatically supplemented by the calculation, so that a constant tool center point speed can be guaranteed during the application of the semi-finished products. High speed, in the context of the present invention, means a constant tool center point speed of 0.5 m / s or more.
[0119] In one embodiment, all events and / or process parameters are converted into machine-relevant parameters. These include, for example, defined axis positions. This procedure can be performed iteratively for all paths and for all positions. The parameters can be stored or saved in a buffer.
[0120] The movement begins with approaching the starting point of the path and aligning all axes to a defined starting position. At the starting point, all relevant axes for applying semi-finished products are fully electronically synchronized.
[0121] For example, the conveyor unit for the semi-finished products is synchronized with the tool center point speed. As a result, synchronous operation is ensured. This synchronous operation is of particular importance for semi-finished product deposit, as it is advantageous if no relative force develops between the semi-finished product and the tool surface, or between the semi-finished product and the semi-finished product. Such a relative force could lead to sliding, incorrect positioning, or poor consolidation quality. For the presented assembly system or process, measurements were able to determine a negligible relative force in the order of < +< / - 0.1 N, for example, for a 20 mm PA6-CF semi-finished product.
[0122] This coupling can be implemented, for example, via a motion control system in conjunction with specially designed controllers that ensure synchronous operation of the drives, i.e., with a relative speed difference within a range of ±2% or less, but also within a range of ±5% or less, or even ±10% or less, even with different gear ratios. This technology can therefore also advantageously replace, for example, traditional cam gears with vertical shafts or rigid mechanical couplings.
[0123] The drives in the application unit for the semi-finished products can be synchronized with the tool center point speed of the drive unit of the composition system in such a way that the result is synchronization in which the relative force acting between the semi-finished product and the thermally insulating material or the carrier film or the tool or the application area or the fiber-plastic composite is less than or equal to 0.01 N / mm-semi-finished product.
[0124] The assembly line can include a semi-finished product changing device for automatically changing the semi-finished product. The magazines or reels used to store the semi-finished products can thus be automatically changed, for example, for automatic feeding of the semi-finished products to the assembly line.
[0125] The acceleration energy of the drive system, or all drives, can be partially utilized, for example, via an energy recovery system. The energy recovery system can be fed, for example, from the energy released during braking. This is achieved, in particular, via the intermediate circuit voltage.
[0126] Process parameters can be both speed-dependent and speed-independent. Process parameters include, for example, locations where events can occur or must be triggered. Process parameters can be calculated based on design-specific machine constants. Process parameters are typically specified in the unit [mm]. The events and process parameters are typically path-dependent, based on the calculation, and stored in the buffer. All events can be executed with a precision of up to + / - 0.005 mm across all tool center point speeds. Lower, i.e., poorer, precisions are also possible.
[0127] Another preferred approach is to execute the events when approaching the end point with high precision and path-dependent via the process parameters. The path position is calculated from the actual data of the axes' position sensors.
[0128] Afterwards, for example, the electronic synchronization can be switched off and a new starting point can be approached.
[0129] This is preferably performed for all webs and layers. The composition of the fiber-reinforced plastic composite can be composed of several individual calculations. A special case is the composition of a fiber-reinforced plastic composite consisting of one web at a time. This allows, for example, the material-specific use of semi-finished products for each web—in other words, the use of different semi-finished materials for consecutive webs.
[0130] The process for assembling fiber-reinforced plastic composites provides, in particular, fiber and / or polymer semi-finished products and / or self-reinforced polymers and / or pre-stretched polymers and / or combinations thereof. The materials to be processed with the assembly system, which have already undergone value creation, are subsequently referred to as semi-finished products.
[0131] Typically, the semi-finished products are wound onto spools. However, other storage options or pre-cut blanks are also suitable for the application. The spools or magazines for the semi-finished products are located above the tool surface in one embodiment and can feed the material manually or automatically, electronically coupled or decoupled from the movement of the drive system and the application device. The feed speed and feed rate are monitored by a sensor.
[0132] In one embodiment, a tensile stress is generated in the longitudinal direction of the semi-finished products by means of a dancer unit to form a semi-finished product buffer. The tensile stress can preferably be adjusted and / or monitored by a sensor.
[0133] The reels or magazines can contain identical or different semi-finished products. In one embodiment, the reels or magazines can be interchanged during the manufacturing process to ensure continuous composition of composite materials. For this purpose, each reel or magazine can be individually driven. In one embodiment, this drive is achieved via a front-end drive mounted on the outside of the reel or magazine housing.
[0134] A wide variety of semi-finished products can be applied. These semi-finished products can be fully consolidated, partially consolidated, impeded, wetted, or a combination thereof. Thermosets, thermoplastics, elastomers, their derivatives, and combinations thereof can be processed as polymer components. Glass fibers, carbon fibers, ceramic fibers, aramid fibers, steel fibers, natural fibers, nylon fibers (e.g., from DuPont), basalt fibers, boron fibers, other fibers, or combinations thereof can be used as load-bearing fiber components.
[0135] In addition, with a suitably adapted application device, piezo fibers, shape memory polymers or alloys, or fiber optic systems for adaptronics, sensors, or data transport can also be automatically embedded into the composition of the composite material.
[0136] These materials typically range in width from 2.5 to 300 mm, preferably 12 to 100 mm, and in thickness from 0.05 to 10 mm, preferably 0.1 to 0.5 mm. Other dimensions are also available depending on the application.
[0137] A catching device can be used to safely feed the semi-finished products conveyed from the reels or magazines to the application device. The catching device centers the materials above the inlet into the application device while the new material is transported into the application device. The interaction of the reels or magazines, the catching device, and the application device allows for quick semi-finished product changes or ensures continuous production. In this embodiment, the reels or magazines for the semi-finished products are advantageously located above the system.
[0138] In a second variant, the system and the tape feed mechanism are positioned at a transfer point for a material change. The tape can be automatically gripped by a gripper head on the feed arm and pushed over the deflection rollers into the head's tape conveyor mechanism. If the tape sensor in the application device detects the presence of material, the gripper is released. This eliminates the need for a second conveyor mechanism in the application device.
[0139] The method and device according to the invention are not restricted to an explicit process parameter configuration due to the flexible controllability of the physical process variables such as pressure (consolidation force), temperature (energy input), and time (speed). The process variables can be material-dependent.
[0140] The consolidation force acts perpendicular to the path tangent and can range from 25 to 5000 N per application unit. In one version, to improve consolidation quality, the consolidation force can be applied in an oscillating manner, with an amplitude of up to 30% of the consolidation force, at a frequency of 60 to 15000 Hz.
[0141] In developing the present invention, it was further recognized and investigated to what extent the formation of a thin melt layer in the semi-finished product, which can be variably adapted to the material and process requirements, enables a novel joining behavior. This novel joining behavior can, for example, enable further process acceleration.
[0142] The energy input can be selected, for example, with a fuel gas nozzle at a correlated power between 100 W and 25 kW. The feed rate can be selected between 0.5 and 10 m / s. For example, for a thermoplastic polyamide-6 carbon fiber semi-finished product with a fiber volume fraction of 55% and a width of 50 mm, partial consolidation (incomplete autohesion) results at 3 m / s with a correlated power of 4.5 kW and full consolidation at a correlated power of 6.8 kW.
[0143] A joining process that achieves very high heating rates with the heating device is particularly advantageous. Examples of effective heating lengths were determined in our own test series, the results of which are presented in Fig. 4 are presented in tabular form.
[0144] With the process according to the invention, two molten polymer phases can be brought into contact. Both the polymeric components of the semi-finished product and the polymeric components of the substrate are already molten shortly before the nip point. The nip point is the point at which the incoming semi-finished product and the previously deposited substrate are in the molten state and are brought into contact by the application of consolidation pressure under the consolidation roller. The "bringing into contact" occurs in the molten phase.
[0145] In a preferred embodiment, the angle of the heating source to the substrate α is half the angle of the inlet of the semi-finished product β.
[0146] By varying α and β, the melting zone can be shifted toward the substrate or the semi-finished product. If β - α > 0.5 β, the melting zone in the semi-finished product is strengthened. If β - α < 0.5 β, the melting zone in the substrate is strengthened.
[0147] In a preferred embodiment, α = 22.5° and β = 45°.
[0148] The position of the heat source X HQ , Y HQ , Z HQ can be adjusted on the application device.
[0149] In another embodiment, the joining process of plastic laser beam joining is based on the absorption of radiation energy from the joining partners and the resulting heating. The absorption is primarily influenced by the wavelength of the radiation source, the material to be joined, and the additives it contains.
[0150] Short-wave laser radiation such as diode lasers has a lower absorption than, for example, the longer-wave radiation of CO2 lasers.
[0151] Amorphous plastics have a lower absorption coefficient than semi-crystalline plastics, as their crystalline structures (e.g., spherulites) can cause scattering effects. Similar effects can be achieved by embedding fiber materials and, if necessary, by pigmentation. The absorption behavior and thus the location and shape of the melting zone can be influenced by these factors.
[0152] For this process, high radiation absorption in the joining surfaces and the associated low penetration depth into the materials to be joined are advantageous. By coordinating the material parameters, processing speed, irradiation areas, radiation power, and power distribution, a high gradient of heat distribution in the thickness direction of the semi-finished product and / or the fiber-reinforced plastic composite or the substrate can be achieved in a particularly advantageous manner. The melting zone can thus be strongly limited locally and the stored heat capacity kept low.
[0153] The heat capacity of these composite materials can be described approximately using the specific properties of density, fiber mass and fiber volume fractions. C p ,FKV = ψ ⋅ C p ,Faser + 1 − ψ ⋅ C p ,Matrix ψ = m Faser m FKV = ρ Faser ⋅ φ ρ Faser ⋅ φ + ρ Matrix ⋅ 1 − φ = Fasermassenanteil φ = Faservolumenanteil
[0154] Using CF-PA6 as an example with a fiber volume content of 50%, the C p , FKV is approximately 1130 J / kgK.
[0155] For example, for semi-finished products with dimensions of 20 mm wide and 0.13 mm thick, and an effective heating length of 23 mm achieved with the heating device, a heat quantity of approximately 37 J can be calculated for a semi-finished product heated to 400 °C at a processing speed of 0.1 m / s. At 1 m / s, this results in 11.5 J, and at 4 m / s, only 5.7 J. The heat energies introduced according to the invention are much lower than with existing technologies.
[0156] In this embodiment, the total mass of the heat source, including the mounting bracket, ignition device, and fuel gas supply, is less than 2250 g. Per millimeter of semi-finished product width, this results in a cumulative heat source mass of less than 120 g / mm semi-finished product and a relative power of up to 185 W / mm semi-finished product relative to the semi-finished product width.
[0157] From the contact point of the interfaces (nip point) of semi-finished product and substrate under the consolidation roller, direct heating by radiation no longer takes place and the resulting homogenization of the heat distribution leads to a phase change and thus to the joining of the materials.
[0158] In a further preferred embodiment, a plurality of laser modules, such as those used in laser marking systems, can be placed at a favorable location in the system, i.e. in particular away from the semi-finished product or the substrate, by means of fiber coupling using optical fibers. The optical fibers can then be combined in a holder close to the heating zone, for example in columns or rows. The geometric division and the controllability and adjustability, in particular of the output power, of the individual modules therefore make it possible to control the power input and distribution of the energy input into the substrate and semi-finished product, and thus advantageously influence the location and shape of the melting zone. In other words, the holder of the heating device is designed in such a way that the melting zone is concentrated on the joining surfaces when the semi-finished product is heated.In the case of the use of laser radiation, it is preferred if equal to or more than 65% of the heat energy, more preferably equal to or more than 75%, even more preferably equal to or more than 85% of the heat energy is concentrated on the joining surface in such a way that the intended melting zone, ie the effective heating length of 23 mm, is heated.
[0159] When using short-wave laser radiation, such as diode lasers, and the associated high divergence of the radiation after leaving the fiber optic cable, it is possible to build heating units without beam-shaping optics. This design allows for the construction of compact, space-optimized heating units, which can be mounted close to the heating zone. Furthermore, the mass of the heat source, including the fiber optic cable and the mounting bracket, can be kept low.
[0160] For example, for PA-6 made of carbon fibers with a 50% fiber volume content and a width of 20 mm, six modules are coupled for high-speed joining. These modules have an output power of up to 6 kW. The total mass of the six modules, including the fiber optic cable and mounting bracket, is 3750 g. In this embodiment, this results in a cumulative heat source mass of less than 200 g / mm of semi-finished product per millimeter of semi-finished product width and a relative power of up to 300 W / mm of semi-finished product width.
[0161] The implemented heat sources provide high energy densities with high heating output.
[0162] The method according to the invention achieves good heat transfer in the joining partners, ie in particular semi-finished product or substrate.
[0163] This results in high heating rates. Due to the high application speeds, the high temperatures lead to low degradation, as the exposure time can be kept short. In a variant embodiment, the exposure time can be influenced by the effective length of the temperature.
[0164] This is achieved in particular by positioning the heat source, in other words the emitter of the high-energy-density heat output, close to the nip point. In one embodiment, the heat energy exit point is less than 85 mm from the nip point. In a preferred embodiment, the heat energy exit point is less than 55 mm.
[0165] The process according to the invention can utilize lower viscosities of the polymer melt through an extended temperature range. The process according to the invention achieves the lower viscosity level in particular through higher processing temperatures. For thermoplastic polymers, the viscosities can be derived, for example, using an Arrhenius relationship. For thermosetting systems, the viscosity curve can be predicted, for example, from reaction kinetics over the molecular weight buildup through polyaddition and polycondensation of linear polymers, also using an Arrhenius approach with activation energies and an empirically determined pre-exponential factor and the degree of polymerization.
[0166] To prevent degradation due to oxidative decomposition, one embodiment can use a protective atmosphere in the area where heat is introduced into the semi-finished product. In the embodiment with a fuel gas nozzle, the highly superheated fluids from the combustion process themselves form a protective atmosphere.
[0167] In another embodiment, the heating device does not heat the entire thickness of the substrate or semi-finished product, but rather, particularly due to the high processing speed, only brings the surfaces into a molten state. Since the entire thickness is not heated, the energy bound in the form of heat is low.
[0168] If the bound energy in the form of heat is low, it can be rapidly dissipated within the substrate and into the environment during and after the joining process through heat conduction and convection. In other words, high cooling rates are possible. Part of the energy can be absorbed directly during the phase transition or, as is the case with thermoplastics, during endothermic crystallization.
[0169] In fiber-reinforced plastic composites, heat conduction along the fiber direction may be greater than heat conduction across the fiber direction, especially for carbon fibers. This allows the energy to be quickly distributed after application. Rapid distribution against the process direction allows the energy to be quickly conducted into the substrate and dissipated directly, for example, through convection. This enables very high cooling rates.
[0170] The heat conduction across the fiber direction in the thickness of the semi-finished product can be described by the following equation: λ quer , FKV = λ Matrix ⋅ 1 + ξ ⋅ κ ⋅ φ 1 − κ ⋅ φ ξ = log − 1 ⋅ 3 ⋅ log Faserquerschnitt in Wärmeleitrichtung Faserquerschnitt quer zur Wärmeleitrichtung ξ Kreis = 1 κ = λ Faser λ Matrix − 1 λ Faser λ Matrix − ξ
[0171] Since only the surface is heated to a high degree, the application of stretched and self-reinforced semi-finished products is also possible, since the typical morphology of the stretching is retained inside the semi-finished product.
[0172] The degree of autohesion can be adjusted using the process parameters of pressure, temperature, and time, even in the extended temperature and viscosity ranges of high-speed joining. Cohesive joining is possible at high speed with a homogeneous, polymeric surface of the semi-finished product. Adhesion is effective with different joining partners or, in most cases, with chemical additives.
[0173] In summary, this results in a joining process with a definable degree of autohesion or adhesion, which enables high-speed joining of at least two joining partners with a feed speed of the semi-finished product and / or translation speed of the application device of greater than or equal to 0.5 m / s.
[0174] The application device can, for example, accommodate the conveyed semi-finished products. A sensor ensures that the processing materials are provided correctly. In a preferred design, the feed is represented by a funnel-shaped opening. In a preferred design, the semi-finished product is directly picked up by a retractable and disengageable conveyor mechanism and fed to the second conveyor mechanism of the application device. This can accelerate the semi-finished product changeover.
[0175] The correct feeding and the correctly executed cut of the semi-finished product can be monitored by a sensor or by a separate sensor in one embodiment. Furthermore, the temperature of the consolidation roller can be monitored.
[0176] The application device features a heating device for creating the partially plastic state of the polymer components. The combination of pressure, temperature, and time can be individually set for each path.
[0177] In a preferred version, this involves a fuel gas nozzle that burns a fuel gas / oxygen mixture to generate energy. The fluid quantities can be electronically controlled, for example, and temperature and power can be adjusted by varying the stoichiometric ratios and / or the flow rate.
[0178] Heat input can occur, for example, via radiation, but also cumulatively, or alternatively via the particle flow of the combustion product. Hydrogen-oxygen combustion produces a highly superheated H2O mixture.
[0179] In one embodiment, the flow of the fuel gas atmosphere can significantly reduce the degradation of the polymer due to high temperatures, as the free oxygen atoms are bound for oxidation. This creates a protective gas environment.
[0180] In one embodiment, the ignited fuel gas mixture is fed to the semi-finished product via a flow channel. In a preferred embodiment, the flow channel is made of ceramic materials. In other words, the heating device, e.g. by means of the flow channel, concentrates the melting zone on the joining surfaces when heating the semi-finished product. When using the fuel gas nozzle, it is preferred if equal to or more than 40% of the heat energy generated by the heating device, more preferably equal to or more than 50%, even more preferably equal to or more than 60% of the heat energy is concentrated on the joining surface in such a way that the intended melting zone, i.e. the effectively acting heating length of 23 mm, is heated.
[0181] One embodiment of the fuel gas nozzle uses an electric ignition device that ignites the fuel gas with an arc and / or an ignition spark. The fuel gas flows out a few millimeters before the ignition point, depending on the path, and the fuel gas mixture can be ignited precisely at the path-related ignition point with a precision of up to + / -0.001 mm, relative to the path, across all tool center point speeds. Lower precisions are also possible, of course.
[0182] The ignition device is preferably operated at 5 to 30 kV.
[0183] Other physical heating principles, such as plasma, laser, LED, can also be used.
[0184] The semi-finished products are placed on the tool surface via the application device, which can move in the Z-direction relative to the drive unit. An electric, pneumatic, or magnetic actuator generates the controllable and adjustable consolidation force.
[0185] The guide elements for the semi-finished products in the application device are designed with a concave or convex curve perpendicular to the conveying direction of the semi-finished products. This design utilizes the self-centering effect. Furthermore, application precision is increased because the width tolerance of the semi-finished products is converted into a uniform bend of the semi-finished product, thus eliminating the need to consider the absolute width of the guide with a high tolerance. Furthermore, a deflection in the semi-finished product improves the inherent rigidity of the semi-finished product against deflections in unguided, free passages.
[0186] The applicator's attachments are designed to utilize the Coanda effect to support flow formation and thus improve temperature control. This directs the energy flow as centrally as possible to the consolidation point (nip point).
[0187] The design of the attachments determines the effective effective length of the heat source and thus the effective temperature range. In other words, the attachments concentrate the melting zone on the joining surfaces when heating the semi-finished product.
[0188] The application device can be designed in a compact form. The total mass of the application unit, including heating sources, can be 40 kg or less, and in a preferred embodiment, even 25 kg or less.
[0189] The drives of the application device can be connected to the frame of the application device via axles containing the drive stator. The axles can preferably be hollow axles. The drives of the application device can also be arranged inside the rotor of the drive.
[0190] Furthermore, power connections, for example for the drives and / or a data connection of the measuring systems, can preferably be routed through the axis.
[0191] In a further preferred embodiment, the drives of the application device can be external rotors.
[0192] The base unit of the device serves, in particular, to precisely accommodate the drive unit and a tool. In a preferred embodiment, it comprises machined granite or concrete with a high degree of precision in terms of flatness, plane-parallelism, and angular deviation. In a preferred embodiment, it has a mass that is 15 to 1,000 times greater than the moving mass.
[0193] The tool for applying the semi-finished products, i.e., the application area, can be made of metal or plastic, for example. The application area can be temperature-controlled.
[0194] In a preferred design, the application area comprises a thermally insulating carrier medium, which, for example, rests on a receiving tool and has a thermal conductivity of < 1 W / (m K) for polymeric materials and < 3.5 W / (m K) for inorganic materials, and a density of < 3.5 g / cm^3. In a preferred design, the material has a flat or spherical extension with a thickness of 0.05 mm to 25 mm.
[0195] In a preferred design, the thermally insulating material is affixed to the tool as a carrier using negative pressure. It can also be fixed by force or form-fitting. Another possible fixation option is to generate an electrical voltage between the tool platform and the thermally insulating material. In another embodiment, no heat source is required for the first layer, since the adhesion mechanism is generated by the tool itself via a negative pressure.
[0196] In a preferred embodiment, the thermally insulating material is fixed to the tool using negative pressure. A carrier film is adhesively bonded to the thermally insulating material. The semi-finished products are applied to the carrier film during the process. After the semi-finished products have been applied, the carrier film can be removed from the thermally insulating material, particularly without leaving any residue. By adjusting the degree of autohesion, adhesion, or cross-linking, it is possible, for example, to remove the carrier film from the semi-finished products without leaving any residue, or to feed the carrier film together with the semi-finished products to further processes.
[0197] Thanks to the flexible control of the physical process variables pressure (consolidation), temperature, and time (high speed), as well as the material selection of the carrier medium, semi-finished products can form an adhesion, autohesion, cohesive, or chemical bond with the thermally insulating carrier medium. After the composite material has been formed, the carrier medium and composite material can be removed together.
[0198] Thanks to the flexible controllability of the physical process variables pressure (consolidation), temperature, and time (high speed), as well as the material selection of the carrier medium, semi-finished products can form partial adhesion, partial autohesion, or an incomplete chemical bond with the thermally insulating carrier medium. After the composite material has been formed, the carrier medium and composite material can be separated from each other if necessary.
[0199] Thanks to the flexible control of the physical process variables pressure (consolidation), temperature, and time (high speed), as well as the material selection, semi-finished products can form adhesion, auto-hesion, cohesive, or chemical bonds. The semi-finished products may subsequently be irreparable.
[0200] Thanks to the flexible control of the physical process parameters pressure (consolidation), temperature, and time (high speed), as well as the material selection, semi-finished products can form partial adhesion, partial autohesion, or an incomplete chemical bond. The semi-finished products can then be separated from each other if necessary.
[0201] In a preferred version, the drive unit is designed in a gantry portal design. The degrees of freedom can include two translations and one rotation of the application device. In a preferred version, direct drives are used for the translational and rotational movements of the drive unit. The force achievable with the direct drives for a translational movement can be up to 12,000 N per drive and up to 175,000 Nm for rotary direct drives. All drives can be equipped with high-resolution measuring systems.
[0202] The total moving masses are particularly preferably reduced to less than 250 kg. In one embodiment, the drive components can be made of composite materials, whereby the moving masses can be reduced, for example, to less than 75 kg.
[0203] As a result, the invention allows accelerations of > 100 m / s2 to be achieved if necessary. This acceleration capability allows the system to be accelerated to a target speed in very short periods of time. Once the target speed is reached, the semi-finished products are applied at a constant, high application speed, and the application device is then decelerated with a high negative acceleration. According to the invention, the performance of the drives makes it possible to implement the system in a compact design.
[0204] In one embodiment, the translational drives are located in the center of gravity of the mass to be accelerated. This design principle minimizes the high moments during acceleration and deceleration.
[0205] By parallelizing the compact application devices, the mass input of the semi-finished products can be increased, thus reducing cycle times. Individual material feed to each application device enables path-specific selection of the semi-finished product, even in parallel configuration.
[0206] The process and device can be operated, for example, via an industrial PC-based controller. Open interfaces enable the integration of a wide variety of electronic technologies in real time. The system can feature extensive CNC functionality with high-speed options for axis interpolation to achieve the highest dynamic performance.
[0207] The PLC program, for example, is written in a high-level language and can be executed in a few microseconds.
[0208] The process and device can, for example, produce a fiber-reinforced plastic composite web by web according to control specifications. The composite material can consist of a single semi-finished product type, or, depending on the specifications, a specific material can be selected for each web path. This composite composition option allows for advantageous isotropic and anisotropic material properties. The high application and material changeover speed significantly increases capacity and cost-effectiveness.
[0209] In the following, the invention is explained in more detail using exemplary embodiments and with reference to the figures, wherein identical and similar elements are partly provided with the same reference numerals and the features of the various exemplary embodiments can be combined with one another without departing from the scope of the claims. Short description of the characters
[0210] They show:Fig. 1 Functional principle of the application of semi-finished products and designation of selected path points, Fig. 2 Deposition movement of the application device and feed of the semi-finished product, Fig. 3 Process steps for controlling the composition system, Fig. 4 Heating rates depending on the set feed rate, Fig. 5 Effect of the heating device on a substrate, Fig. 6 Side view of an embodiment of the application device Fig. 7 Viscosity field for PA-6 and PEEK, Fig. 8 Effect of the heat exposure time generated by the heating device on the substrate temperature, Fig. 9 Exposure time for different effective effective lengths of the temperature, Fig. 10 Functional principle of high-speed joining, Fig. 11a Measurement results and calculation of the heat energy distribution achievable with the heating device in the semi-finished product or in the substrate, Fig. 11b Calculation of the achievable viscosity distribution in the semi-finished product or in the substrate, Fig.11cMeasurement results and calculation of the temperature distribution in the semi-finished product or in the substrate, Fig. 12alike 11a but with changed surface temperature, Fig. 12blike 11b, but with changed surface temperature, Fig. 12clike 11b, but with changed surface temperature, Fig. 13Embodiment of the application device, Fig. 14further embodiment of the application device, Fig. 15another embodiment of the application device, Fig. 16with. Fig. 16a and 16b Embodiment of the application device with representation of the drive systems, Fig. 17with Fig. 17a and 17b further embodiment of the application device with representation of a further drive system, Fig. 18Application device with guide elements, Fig. 18aSection through the plane AA of the Fig. 18, Fig. 19 Representation of the consolidation area, Fig. 20 Heating device with ignition device, Fig. 21 Application area with carrier medium, Fig. 21b Application area with additional carrier medium, Fig. 22 Example of a deposition process, Fig. 23 Second example of a deposition process, Fig. 24 Third example of a deposition process, Fig. 25 Fourth example of a deposition process, Fig. 26 Fifth example of a deposition process, Fig. 27 Sixth example of a deposition process, Fig. 28 Seventh example of a deposition process, Fig. 29 Drive configurations of possible system concepts of the drive unit, Fig. 30 Overall view of the composition system, Fig. 31 Semi-finished product holder, Fig. 32 Base group with tool and carrier medium, Fig. 33 Application device with feed device, Fig. 34 Drive unit in Gantry version, Fig. 35Variant of the feeding device, Fig. 36Further view of the previous variant of the composition system, Fig.Fig. 37Example path structure of identical semi-finished products that can be applied with the composition system, Fig. 38Example path structure of different semi-finished products that can be applied with the composition system. Detailed description of the invention
[0211] Fig. 1shows an example of a functional principle for the application of semi-finished products 20 by means of the application device 50 at high speed with two events, the path start point BSP (X2, Y2, Z2) and the path end point BEP (X3, Y3, Z3), between which the semi-finished product 20 can be deposited in an application area 100. The movement starts with the approach to the start point SP (X1, Y1, Z1) of the path and the alignment of all axes into a defined starting position. At the start point SP, all relevant axes for the application of semi-finished products 20 are fully electronically synchronized. The path movement ends with the reaching of the end point EP (X4, Y4, Z4). Preferably, upon reaching the end point EP, the approach and subsequent depositing of another path can begin immediately, so that the movement of the application device 50 can be continued if necessary.smoothly transitions into the start of the next path, which can be laid, for example, in the opposite direction to the previously laid path within the boundaries of the application area 100.
[0212] In the lower part of the Fig. 1 A path-speed diagram of the distance traveled by the application device 50 is shown. In this example, the application device is accelerated in the area between the starting point SP and the path starting point BSP, and the application device 50 is decelerated between the path end point BEP and the path end point EP. In the section of the path between the path starting point BSP and the path end point BEP, the application device 50 has a constant tool center point speed vTCP.
[0213] Fig. 2demonstrates fundamental relationships between the deposition movement of the application device 50 and the feed of the semi-finished product 20 therein in one embodiment. For example, the feed of the semi-finished product 20 can be synchronized with the tool center point speed vTCP. As a result, synchronization between the movement of the application device 50 and the feed of the semi-finished product 20 is ensured. This synchronization can be particularly advantageous during semi-finished product deposition, since no or only a very low relative force arises between the semi-finished product 20 in the first layer and a tool surface 101 or, in a further layer (2 to N-1), between the semi-finished product 20 and the semi-finished product 20. This could potentially lead to sliding, incorrect positioning, or poor consolidation quality. The measurements showed that a negligible force of < +< / - 0.1 N can be achieved for one embodiment of the invention.
[0214] Fig. 3shows steps of an exemplary procedure for controlling the composition system 1. In this example, before each movement, 300 data are calculated in a calculation phase and stored in a buffer.
[0215] In a first step 301, for example, a process software or a control system is activated, e.g. started up.
[0216] In a second step 302, various first path parameters that influence the subsequent application of the semi-finished products 50 to the application area 100 can be entered by a user using an operating console or read in via an interface. Examples of the first parameters are path start and path end points for the path j = 1..n for each layer i = 1..m. The exemplary method initially begins in the second step 302 with the input or reading in of the first parameters for the first path j of the first layer i.
[0217] In a third step 303, for example, the calculation of path-relevant process parameters of path j can be carried out on the basis of the entered first parameters, in particular the entered path start and path end points.
[0218] Process parameters can be both speed-dependent and speed-independent. Process parameters include, for example, locations where events can occur or must be triggered. Process parameters can be calculated depending on design-specific machine constants. A machine constant, for example, could be the minimum deposition length. Process parameters can be speed-dependent distances (typically in the unit [mm]), speed-independent process-relevant locations (typically in the unit [mm]), or constant parameters over the course of a path, such as the angle of the application unit around the Z-axis.
[0219] A speed-dependent process parameter can, for example, be the pre-travel distance for starting the semi-finished product transport in order to ensure that the path start point coincides exactly with the required deposition start point.
[0220] Speed-independent process parameters can be, for example, the path-related locations of the cutting process, path start and end points or start and end points.
[0221] Events can be, for example: Cutting the semi-finished product Starting the semi-finished product transport Stopping the semi-finished product transport Heating source on Heating source off Ignition on Ignition off Lowering the application unit Raising the application unit Selecting the direction of the semi-finished product "duplex"
[0222] All parameters can be stored or saved in a buffer.
[0223] In a step 305, a query is made as to whether another path j+1 should be applied in the current layer i. If another path j+1 or another path j+n should be applied, a compensation path of the application device 50 from the end point EP of path j to the starting point SP of path j+1 can be calculated in an intermediate step 306. Subsequently, steps 302, 303, 305 are repeated for all paths j of the current layer i.
[0224] Once all paths j of the current layer i have been calculated, step 307 queries whether a further layer i+1 with semi-finished product 20 should be deposited on the application area 100. If so, the first parameters of the paths j of the further layer i+1 can now be entered again in step 302 for the further path i+1.
[0225] If all trajectories i=1..n of all positions j=1 ..m have been precalculated, the calculation can be completed in step 308. All trajectory- and position-relevant data can be stored or saved in a buffer.
[0226] Pre-calculation 300 can be used for execution 310, so that potentially complex calculations are not required during execution and the execution process can be completed more quickly. The execution calculation is typically determined during a movement of drive unit 10.
[0227] In a step 311 of execution 310, the movement of the composition system 1 is started.
[0228] The composition system 1, or the application device 50, moves to the starting point SP of the path in step 312. Likewise, the system is brought into the starting position for the current path j of position i. All axes can be coordinated with one another in step 312 using electronic precision synchronization.
[0229] According to step 313, the path j of the layer i is traversed and semi-finished product 20 is applied.
[0230] According to step 314, the end point EP of the path j of the layer i is approached after the application of semi-finished product 20 for the layer i has been completed.
[0231] According to step 315, the electronic precision synchronization of the axes can be deactivated.
[0232] According to step 316, a query is made as to whether the last path j of the current layer i has been applied. If not, i.e., if another path j+1 is to be applied, execution 310 continues with step 317. In step 317, the compensation path is traversed, in particular the compensation path calculated in step 306. Furthermore, according to step 318, the path index is subsequently incremented by one counter to j+1, and according to step 312, the approach to the starting point of path j+1 is initiated.
[0233] If, however, the last path j of layer i has been deposited on the application area, a query is made in step 319 as to whether the last layer i has also been deposited or whether another layer i+1 is to be deposited. If another layer is to be deposited, the layer index is incremented to i+1 in step 320, the stored data 300 is read from the memory, and the starting point of path j of the next layer i+1 is approached in step 310.
[0234] If the last layer i has been deposited, the processing is terminated with step 321.
[0235] The Fig. 4 Table 1 shows, within the scope of the present invention, measured values and calculated temperature curves with the corresponding heating rates as a function of the set feed rate, which were determined in our own test series, for an effective heating length of 23 mm.
[0236] Fig. 5schematically shows the action of the heating device 65 on the substrate 28 consisting of fused layers 21, 22, 23, 24, wherein the semifinished product 20 is fused to the uppermost layer 21 at the nip point 29b. Two molten polymer phases 29 are brought into contact. Both the polymeric components of the semifinished product and the polymeric components of the uppermost layer 21 of the substrate are already molten shortly before the nip point 29b. The "bringing into contact" at the contact point 30 occurs in the molten phase.
[0237] The angle of the heating source 65 to the substrate 28 can be adjustable; In the embodiment of the Fig. 5 α is half the angle of the inlet of the semi-finished product β.
[0238] By varying α and β, i.e., by changing the angle of the heat source 65, the melting zone 29 can be shifted toward the substrate 28—i.e., typically downward, with more heat applied to the substrate 28—or toward the semifinished product 20, with more heat applied to the semifinished product 20 to be applied. If β - α > 0.5 β, then the melting zone in the semifinished product is intensified. If β - α < 0.5 β, then the melting zone in the substrate is intensified.
[0239] In a preferred embodiment, α = 22.5° and β = 45°.
[0240] The position of the heat source X HQ , Y HQ , Z HQ can be adjusted on the application device 50.
[0241] Fig. 6 shows a schematic side view of the application device 50 above the application area 100 with activated heating device 65.
[0242] Fig. 6ashows an overall view of the application device 50. In one embodiment, the heating device 65 with several diode laser modules 70 and coupled optical fibers 68 are shown. Diode laser modules 70 are placed at a location in the system where the required installation space is conveniently available. The output power of the diode laser modules 70 is adjustable. In one embodiment, the output power of the diode laser modules 70 is controllable or regulatable. For example, diode laser modules 70 can be used and modified if necessary, as they are used in laser marking systems. The optical fibers 68 can then be combined near the melting zone 29 in a holder 72, for example in columns and rows. The modules 70 can be designed and geometrically divided in such a way that the power input and distribution into substrate 28 and semi-finished product 20 can be controlled and thus the location and shape of the melting zone 29 can be influenced.
[0243] Fig.6b shows a side view of an applicator 50. The optical fibers 68, grouped in columns and rows, are shown with a divergence angle of approximately 25° and with a resulting beam cone 73. The holder 72 can be adjusted in its position relative to the applicator 50 in X HQ, Y HQ, Z HQ and in its angle relative to the substrate 28 or in its angle relative to the applicator 50.
[0244] Fig.6c shows a sectional view of the application device 50. The optical fibers 68, arranged in columns and rows, are shown with a divergence angle of approximately 25° and with a resulting beam cone 73. The energy density can be adjusted by geometrically distributing the optical fibers 68 in holders 72.
[0245] Fig. 7shows the viscosity behavior for PA-6 and PEEK. In one variant, the process according to the invention can utilize a lower viscosity level of the polymer melt by using higher temperatures. Compared to established processes, the higher processing temperatures reduce the viscosity several times over. This improves the autohesion, crosslinking, and adhesion behavior.
[0246] Fig. 8 shows the relationship between the heat exposure time generated by the heating device 65 and the temperature set in the substrate 28 and / or the semi-finished product 20 for PEEK and PA-6. The joining process can be completed in a few milliseconds. Preferably, the parameters of the assembly system 1 are set so that the high-speed joining for PA-6 or PEEK is carried out for an effective effective temperature length of 23 mm in a temperature range between approximately 450°C and approximately 900°C and an exposure time of up to approximately 0.06 seconds.
[0247] Fig. 9 shows the exposure time for the semi-finished product 20 versus the effective effective length of the temperature for a feed rate of the semi-finished product 20 that can be set as a parameter of the composition system 1 and / or adjustable vTCP—in other words, with different processing speeds. The effective effective length of the temperature is predetermined by the design and can be adjusted if necessary. The vTCP of the application device 50 is shown at 1 m / s, 2 m / s, and 4 m / s. With an effective effective length of 23 mm and a vTCP of 2 m / s, the exposure time corresponds to approximately 12 ms.
[0248] Fig. 10 shows the functional principle and elements of the high-speed joining 400. Basis of the functional chain according to Fig. 10is a high heating power 401 achievable through the advantageous design of the heating device 65. The high heating power 401 can be converted into a good heat transfer 402 through the advantageous geometric arrangement and design of the heating device 65, so that high heating rates 403 can be realized in the substrate 28 and / or in the semi-finished product 20. This is achieved in particular by the fact that the heat source, in other words the emitter of the heating power with high energy density, is mounted directly in front of the nip point 29b.
[0249] The high heating rates 403 would per se lead to a high energy input into the substrate. However, it has been found within the scope of the present invention that it is particularly preferred if—for example, in combination with a high feed rate of the semi-finished product 20 and / or a high vTCP, and thus only a short exposure time 407—a thin-film melt 404 is initiated. The low stored heat 405 that can be achieved in this way—which may only be stored in the surface of the semi-finished product 20 or the substrate 28—preferably leads to a low cooling requirement. In other words, the low heat input, i.e., the low total applied heat energy per volume (or per mass) of the semi-finished product 20, enables a distribution and equalization of the heat energy over the entire mass, and thus ultimately to a high cooling rate 406 at the location of the melt 29.
[0250] The high local temperature at the melt location 29 leads to a high mobility of the macromolecules 408, i.e., a low viscosity at the melt location 29. The degree of autohesion, adhesion, or crosslinking can be adjusted via pressure, temperature, and time (high speed) according to the schematic diagram 409. The aforementioned factors lead—as discovered within the scope of the invention—to an improvement in, or form the basis for, the realization of, high-speed joining 410.
[0251] Fig. 11a , b , and c as well as Fig. 12a , b and c show measurement results and calculations that were carried out within the scope of the present invention using the semi-finished product 20 CF-PA6 with 50 fiber volume percent and an effective heating length of 23 mm. Figures 11a , b , c The surface temperature of the semi-finished product 20 was set at 400 °C. Figures 12a , b , cIn contrast, a surface temperature of 600 °C was set for semi-finished product 20. The melting point of PA-6 is 225 °C and is shown in dashed lines.
[0252] Fig. 11a shows the isotherms in the semi-finished product 20 - ie the penetration depth of the thermal energy in the semi-finished product 20 - for different processing or process speeds. Fig. 11b shows the lines of equal viscosity in Pas of the same semi-finished product 20.
[0253] Fig. 11c Finally, the graph shows the temporal progression of the isotherms over the penetration depth in the semi-finished product 20 at a processing speed of 1 m / s and an effective heating length of 23 mm.
[0254] The Figures 12a , b , c each show the same object as the Figures 11a , b , c Wherein the surface temperature of the semi-finished product 20 of the Figures 12a , b , c was set to 600 °C.
[0255] Fig. 13 shows a first embodiment of the application device 50 with a variant of the semi-finished product guide. The semi-finished product 20 is transported into the conveyor unit 506 via a feed device 504 monitored by a feed sensor 502. The semi-finished product 20 is then transported into the cutting unit 510 monitored by a cutting sensor 508 and under the consolidation roller 512, where the semi-finished product can be applied within the boundaries of the application area 100. In this embodiment, the consolidation roller 512 is monitored by the consolidation sensor 514. The heating source 65 is arranged to the side of the consolidation roller 512.
[0256] Fig. 14 shows a further embodiment of an application device 50 with a "duplex design." The application device 50 has at least two tape feeds on the roll as well as a double heating device 65, 65'—and possibly a double ignition device.
[0257] In the design of the Fig. 14 the application direction of the semi-finished product 20 and thus the deposition direction 35 for the application device 50 can be selected, which offers the possibility of saving cycle time by avoiding empty runs or pivoting movements when approaching the path starting points.
[0258] The semi-finished product 20 is fed to the cutting unit 510 by a belt drive 506. In this embodiment, the cutting unit 510 is monitored by a first cutting sensor 508 and a belt switch sensor 528, ensuring optimal monitoring of the cutting process and direction control in both deposition directions 35 of the semi-finished product 20. Behind the cutting unit 510 is a belt switch 516, through which one of the two belt feeds 561 on the roll and thus the deposition direction 35 of the semi-finished product 20 can be selected.
[0259] In Fig. 14In other words, the semi-finished product 20 is fed via the monitored feed device 504 into the conveyor unit 506, then into the monitored cutting unit 510, into a monitored semi-finished product switch 516 for left- or right-side transport under the consolidation roller 512.
[0260] In Fig. 15 Two semi-finished products 20, 20' are guided separately. The first semi-finished product 20 is transported via a feed device 504 monitored by a feed sensor 502 into the conveyor unit 506, through the monitored cutting unit 510, which is monitored by a cutting sensor 508, and under the consolidation roller 512, where the semi-finished product 20 can be applied within the boundaries of the application area 100. The consolidation roller 512 is monitored by the consolidation sensor 514. The first heating source 65 for the first semi-finished product 20 is arranged to the side of the consolidation roller 512.
[0261] The second semi-finished product 20' is transported into the second conveyor unit 506 via a second feed device 524 monitored by a feed sensor 522. The semi-finished product 20' is then transported into the second cutting unit 530 monitored by a second cutting sensor 528 and under the consolidation roller 512, where the semi-finished product can be applied to the application area 100. The consolidation roller 512 is monitored by the consolidation sensor 514. The second heating source 65' for the second semi-finished product 20' is also arranged to the side of the consolidation roller 512.
[0262] In other words, in the execution of the Fig. 15 the first semi-finished product 20 and the second semi-finished product 20' are finally guided via separate conveyor units 504, 524 to two monitored and separate cutting units 510, 530, optionally on the right or left side, under the common consolidation roller 512.
[0263] Thus, in the head area of the application device 50, there are two complete guide lines for the first and second semi-finished products 20, 20', each consisting of a belt drive 506, 526, a cutting unit 510, 530, and guides. The semi-finished products 20, 20' are also provided in duplicate.
[0264] In addition to the previous embodiments, this variant allows the downtimes of the system to be halved, e.g. due to material changes of the semi-finished product 20, 20' and / or maintenance of the cutting unit 510, 530, and the thermal load on the drives in the head area of the application device 50 to be reduced.
[0265] Fig. 16a, 16b shows an embodiment of the application device 50 with a drive system 56 mounted laterally on a frame 54 of the application device 50 and coupled to the conveyor mechanism via a shaft. The above the partial figures Fig. 16a or Fig. 16bThe coordinate systems shown illustrate that the figure part of the Fig. 16a a first side view of the application device 50 in the perspective known from the previous figures. Fig. 16a therefore only serves to clarify the position of the drives on the application device 50. The left part of the figure Fig. 16b shows a second side view of the application device 50 rotated by 90°.
[0266] The conveyor unit 506 has two driven rollers 506a, 506b. Roller 506a is driven by the drive 546a mounted on the side of the frame 54 via the shaft 547a. Roller 506b is driven by the drive 546b mounted on the side of the frame 54 via the shaft 547b.
[0267] Similarly, the cutting unit 510 is driven by the side-mounted drive 550 via the shaft 551; the consolidation roller 512 is driven by the side-mounted drive 552 via the shaft 553.
[0268] In a further embodiment of the Fig. 17a, 17b The drives are integrated as direct drives in a complete functional unit in the application device. As in the previous figure, the Fig. 17a to better illustrate the position of the drives, since the relative position in the z-direction is shown in the Figs. 17a and 17b is identical.
[0269] The driven rollers 506a, 506b of the conveyor unit 506 are driven by the drives 546a, 546b integrated into the rollers. The rollers are each mounted in the frame 54 by an axle or shaft 547a, 547b.
[0270] The cutting unit 510 is driven by the drive 550 integrated into the cutting unit 510, with the cutting unit 510 being supported by the axle or shaft 551. The consolidation roller 512 is driven by the integrated drive 552, with the consolidation roller 512 being supported by the axle or shaft 553.
[0271] For example, connecting cables for the power and the angle measuring system can be routed to the outside through the respective shaft or axis. This particularly compact design enables further miniaturization of the application device 50. Furthermore, the miniaturization of the individual application device 50 simplifies the parallelization or parallel operation of multiple application devices 50.
[0272] The conveyor mechanism 506 may, for example, comprise a drive wheel 506a. The conveyor mechanism may alternatively or cumulatively comprise a belt drive 506a and a counter-body 506b. It is advantageous to evaluate the viscoelastic properties of the conveyor mechanism for the synchronized conveying of the semi-finished product 20 and to incorporate them into the calculation of the semi-finished product feed rate, because the most accurate determination of a "neutral fiber of the semi-finished product" can be used to calculate the most accurate conveyor speed. This can also be used for the Fig. 13 , 14 , 15 , 16a , 16b , 17a , 17b and 18 presented embodiments are taken into account.
[0273] Another function is the fully electronically synchronized cutting of the semi-finished products. In a preferred design, a servo-electric drive with a measuring system or a direct drive with a measuring system is used as a rotary cutter. During the cutting process of the conveyed semi-finished products on a counter body, the cutting blade is electronically synchronized to maintain the same, constant speed at the cutting point. This can also be used for the Fig. 13 , 14 , 15 , 16a , 16b , 17a , 17b and 18 presented embodiments are taken into account.
[0274] The consolidation roller 512 can optionally be electronically synchronized and driven by a servo motor or direct drive. The sensor 514 can, in particular, monitor the temperature of the consolidation roller 512. If necessary, the temperature of the consolidation roller 512 is controlled internally or externally by a fluid. This can also be used for the Fig. 13 , 14 , 15 , 16a , 16b , 17a , 17b and 18 presented embodiments are taken into account.
[0275] Fig. 18shows a further embodiment of the application device 50 with guide elements 561 and 562. The semi-finished product 20 is placed onto the tool surface 101 or the carrier media 102 or 102b via the application device 50, which can perform a movement in the Z direction relative to the drive unit 10. An electric, pneumatic, or magnetic actuator generates the controllable and adjustable consolidation force when the semi-finished product 20 is deposited.
[0276] The guide elements 561, 562 for the semi-finished product 20 in the application device 50 are designed in this embodiment in a concave or convex curved design transverse to the conveying direction of the semi-finished product 20. This design advantageously utilizes a self-centering effect of the semi-finished product 20. Furthermore, the application precision can be increased, since the width tolerance with respect to the semi-finished product 20 is converted into a uniform bend of the semi-finished product 20 and thus the absolute width of the guide does not have to be considered with a high tolerance. Furthermore, a deflection in the semi-finished product 20 ensures that the inherent rigidity of the semi-finished product 20 is improved with respect to deflections in unguided, free passages. This can also be used for the Fig. 13 , 14 , 15 , 16a , 16b , 17a , 17b and 18 presented embodiments are taken into account.
[0277] Fig. 18a shows a section along the AA axis of the Fig. 18 to show the bending of the semi-finished product 20.
[0278] Fig. 19 shows a further embodiment of the consolidation area with consolidation roller 512 and incoming semi-finished product 20, wherein attachment elements 571 of the application device 50 are designed in such a way that they utilize the Coanda effect to support the flow formation and thus the temperature control for the heating device 65. Thus, the energy flow is directed as centrally as possible into the contact point 30. The design of the attachment elements 571 modifies the effective effective length of the heat source 65 and thus the effective effective temperature range.
[0279] For example, the attachment elements 571 can form a flow channel so that, for example, an ignited fuel gas mixture from the heating device 65 is efficiently guided via the flow channel to the semi-finished product 20. In a preferred embodiment, the attachment elements 571 forming the flow channel are made of ceramic materials.
[0280] Fig. 20 shows a preferred embodiment of the heating device 65 with an optional ignition device 66.
[0281] In this preferred version, a fuel gas heating device 65 is used, which burns a fuel gas to generate energy. The fluid quantities can be electronically controlled, for example, and adjusted in temperature and power by varying the stoichiometric ratios and / or the volume flow.
[0282] To ignite the mixture, the fuel gas heating device 65 has an ignition device 66 for igniting the fuel gas. In the illustrated embodiment, the heating device 65 has a ground connection 64. The ignition device 66 can be controlled such that, for example, an ignition spark 67a or an arc 67b is generated. As soon as the ignition spark 67a or the arc 67b of the ignition device 66 is applied, the already escaping fuel gas is ignited.
[0283] For example, hydrogen-oxygen combustion produces a highly superheated H2O mixture. In one embodiment, the flow of the fuel gas and / or exhaust gas atmosphere can significantly reduce the degradation of the polymer due to high temperatures, as the free oxygen atoms are bound for oxidation. This creates a protective gas environment.
[0284] In one embodiment of the heating device 65, an electrical ignition device 66 is used, which ignites the fuel gas with an arc and / or an ignition spark. The fuel gas can flow out a few millimeters before the ignition point, depending on the path, and the fuel gas mixture is ignited exactly at the path-related ignition point with a precision of, for example, + / - 0.001 mm, relative to the path, across all tool center point speeds vTCP. Lower, i.e., poorer, precisions are also possible.
[0285] The ignition device is preferably operated at 5 to 30 kV.
[0286] In the with Fig. 21aIn the embodiment shown, the application area 100 comprises a tool 101 and a thermally insulating carrier medium 102, which lies, for example, on a receiving tool 101 and has a thermal conductivity of < 1 W / (m · K) for polymeric materials and < 3.5 W / (m · K) for inorganic materials and a density of < 3.5 g / cm^3. The carrier medium 102 has a flat or spherical extension with a thickness of 0.05 mm to 25 mm. Other, identical objects are provided with the same reference numerals as the previous figures; a repeated description will not be given. The carrier medium 102 can be fixed to the base group 2, for example, by means of negative pressure. It can also be fixed to the base group 2 in a force-fitting or form-fitting manner or electrostatically.
[0287] In the with Fig. 21bIn the embodiment shown, the application area 100 comprises a tool 101 and a thermally insulating carrier medium 102, which lies, for example, on the receiving tool 101, as well as a carrier medium 102b, which lies, for example, on the thermally insulating carrier medium 102. Both the thermally insulating carrier medium 102 and the carrier medium 102b have a thermal conductivity of < 1 W / (m · K) for polymeric materials and < 3.5 W / (m · K) for inorganic materials.
[0288] In a preferred embodiment, the carrier medium 102 has a planar or spherical extension with a thickness of 0.05 mm to 25 mm. In a preferred embodiment, the carrier medium 102b has a thickness of 0.025 to 1 mm.
[0289] The carrier media 102 and 102b can be removed from the application area 100 and the tool 101 without leaving any residue. The carrier medium 102 can also be removed from the carrier medium 102b without leaving any residue. These removal processes can be automated.
[0290] Other identical items are provided with the same reference numerals as the previous figures; a repeated description will not be repeated. The carrier medium 102 and the carrier medium 102b can be fixed to the base assembly 2, for example, by means of negative pressure. They can also be fixed force-fitting, form-fitting, or electrostatically.
[0291] Fig. 22 shows a first example of a deposition process of the semi-finished product 20 on, for example, a carrier medium 102. A single application device 50 is used, for example the one shown in Fig. 13shown application device 50. All webs are laid down in the same laying direction 35. However, a composition of the type shown is of course also possible with the Fig. 14 or Fig. 15 shown designs of the application device 50 are possible.
[0292] Fig. 23 shows a second example of a deposition process of the semi-finished product 20 on, for example, a carrier medium 102. A duplex-capable application device 50 is used, for example the one shown in Fig. 14 The webs are laid down successively and alternately. This saves travel for the application device 50, thus saving time for the entire application process. This composition is also compatible with the Fig. 15 and Fig. 13 shown designs are possible, whereby in an application with the design of the Fig. 13 a 180° rotation of the application device 50 relative to the drive unit 10 must be possible.
[0293] Fig. 24 shows a third example of a deposition process of various semi-finished products 20, 20' on, for example, a carrier medium 102. Preferably, a duplex-capable application device 50 is used, for example the one shown in Fig. 15 The webs are deposited successively and alternately, with the semi-finished product 20 of type 1 being deposited in a first direction, and the semi-finished product 20' of type 2 being deposited in the opposite direction. This pattern can also be deposited with the other embodiments of the application device 50, although this may require a change of semi-finished product for each web.
[0294] Fig. 25shows a fourth example of a deposition process of a semi-finished product 20 on, for example, a carrier medium 102 with respect to a composition option for producing interrupted fiber-plastic composites 28. In this example, the webs are successively laid down alternately every second web.
[0295] Fig. 26 shows a fifth example of a deposition method for semi-finished products 20 on, for example, a carrier medium 102, with respect to a composition option for producing fiber-plastic composites 28 with a web-by-web change of the semi-finished product using semi-finished products of different types. Types 1, 2, 3, 4, and 5 are shown, which can be deposited alternately in webs or layers. The use of all shown variants of the application device 50 is possible.
[0296] Fig. 27ashows a sixth example of a deposition method of a semi-finished product 20 on, for example, a carrier medium 102 with respect to a composition option for producing fiber-plastic composites 28 with multiple application devices 50 in a composition system 1. For example, webs 1, 2, 3, n-6, and n-5 can be deposited next to one another in a single step in a layer of the substrate 28 by multiple simultaneously operated application devices 50. Furthermore, for example, webs n-4, n-3, n-2, n-1, and n can then be deposited simultaneously thereafter, preferably in the opposite direction to the deposition of the previous webs.
[0297] Fig. 27bshows a further embodiment of the previous example of a deposition method of a semi-finished product 20 on, for example, a carrier medium 102 with respect to a composition option for producing fiber-plastic composites 28 with a plurality of application devices 50 in a composition system 1. For example, all webs can be deposited next to one another in a single step in one layer of the substrate 28 by a plurality of simultaneously operated application devices 50.
[0298] Fig. 28 finally shows an example of a deposition process of a semi-finished product 20 on, for example, a carrier medium 102 with regard to a composition option for producing fiber-plastic composites 28 with several application devices 50 with web-by-web semi-finished product allocation.
[0299] Of course, all previously shown examples of the deposition process can be freely selected in terms of material selection and direction and position variable deposition.
[0300] Fig. 29 shows an excerpt of various drive configurations for the drive unit 10 and / or the application device 50 with regard to the possible degrees of freedom. In the lower part of the Fig. 29A further embodiment of the application area 100 is shown, wherein the application area 100 is rotatably mounted and can perform a translation on the base group 2, so that a movement of the application area 100 is possible and the application device 50 can reach all positions on the application area 100 through the interaction of a movement of the application area 100 with the drive unit 10. In a further embodiment, the application area 100 is rotatably mounted and can perform a translation on the base group 2, so that a full coverage of the application area is possible via a parallel arrangement of application units 50.
[0301] Fig. 30shows a schematic drawing in an overall view of a composition system 1 with a base assembly 2, on which the drive unit 10 is mounted laterally. The drive unit 10 has several guide rails, among other things, for guiding and moving the application device 50. The application device 50 is thus freely movable above the application area 100 by means of the drive unit 10.
[0302] Various semi-finished products 20 are stored above the application device 50 on a semi-finished product holder 40, so that the respective semi-finished product to be used can be lowered into a feed device 504 and fed to the application device 50. A substrate 28 is shown in the composition, which is applied to a carrier medium 102, wherein the carrier medium 102 is fixed to a tool 101. The tool 101 is in turn fixed to the base assembly 2.
[0303] Fig. 31shows a schematic drawing of the semi-finished product holder 40 or the device 40 for providing the semi-finished products 20. The semi-finished product holder 40 has a catching device 42. The catching device 42 centers the semi-finished products 20 above the inlet or feed device 504 of the application device 50 while another, possibly new or different semi-finished product 20, is transported or introduced into the application device 50. Through the interaction of spools 44 (or magazines) in which the semi-finished products 20 are stored, the catching device 42, and the application device 50, rapid semi-finished product changes can be carried out or continuous production can be ensured. The spools 44 can be individually controlled via the drives of the spools or magazines 45.
[0304] Fig. 32shows an embodiment of a base group 2 with tool 101 and a fixed carrier medium 102, with already applied substrate 28, which are arranged on the application area 100.
[0305] Fig. 33 shows a sketch of a detailed view of an application device 50 with feed device 504, drives 546 and 550, and heating devices 65, 65'. Reference is made to the explanations of the previous examples of the application device 50.
[0306] Fig. 34shows an example of a drive unit 10 in a "gantry design." An applicator holder 12 serves to accommodate the applicator 50. The drive unit has lateral mounting surfaces 14, which are provided for lateral mounting on the base assembly 2. A first linear guide 16 enables the translation of the drive unit 10 or the applicator 50 in a first horizontal direction; a second linear guide 18 enables the translation of the applicator 50 in a second horizontal direction perpendicular to the first horizontal direction. A rotation unit 19, consisting of a bearing and drive, with a central semi-finished product feed 20 via a hollow shaft 19b, enables the free rotation of the applicator unit 50.
[0307] Fig. 35shows a variant of the composition system 1. The coils or magazines 44 for the semi-finished product 20 can be held laterally of the base group 2 and fed to the application device 50 by means of the device 40b.
[0308] For a material change of the semi-finished product 20, the drive unit 10 positions the application device 50 and the belt feed mechanism 40 at a transfer point. The semi-finished product 20 can be automatically gripped, for example, by a gripper head on the feed arm and pushed over the deflection rollers 46 into the feed device 504 of the application unit 50. If the belt sensor 502 in the application device 50 detects that the semi-finished product 20 has been inserted, the gripper is released. A second conveyor mechanism in the feed device 504 can thus be dispensed with, and the application device 50 can be constructed even more compactly.
[0309] Fig. 36 shows the design of the Fig. 35from a further view side, whereby the storage of the semi-finished product 20 in the roll 44 is more clearly visible. The reels 44 can be individually controlled via the drives of the reels or magazines 45.
[0310] Fig. 37 shows an example of a web structure achievable with composition system 1 using the same semi-finished product types 20.
[0311] Fig. 38 Finally, Figure 1 shows an example of a web structure achievable with the assembly system 1, consisting of various semi-finished product types 20, 20' with different directionally and positionally variable structures. The semi-finished product types 20, 20' can vary, for example, in their material properties and in the dimensions of width, thickness, and cross-sectional geometry. This variability can also be transferred to a layered structure consisting of several superimposed webs using the assembly system 1.
[0312] It will be apparent to those skilled in the art that the embodiments described above are to be understood as examples and that the invention is not limited to them, but can be varied in many ways without departing from the scope of the claims. List of reference symbols:
[0313] 1 Composition system 2 Floor assembly 10 Drive unit 12 Application device holder 14 Side mounting surface 16 First linear guide 18 Second linear guide 19 Rotation unit 19b Hollow shaft of the rotation unit 20 Semi-finished product 21 Top layer of the substrate 22 Second layer of the substrate 23 Third layer of the substrate 24 Fourth layer of the substrate 25 Bottom layer of the substrate 28 Substrate 29 Melting zone 29b Nip point 30 Contact point 35 Deposition direction 40 Semi-finished product holder or device for storing the semi-finished products 40b Variant of the semi-finished product holder or device for storing the semi-finished products 42 Catch device 44 Reel or magazine 45 Drive reel or magazine 46 Deflection pulley 50 Application device 54 Frame 56 Drive system 64 Ground connection 65Heating device 66Ignition device 67aIgnition spark 67bArc 68Fiber coupling,Optical fiber 70 Laser modules 72 Holder 73 Beam cone 100 Application area 101 Tool 102 Carrier medium 102b Carrier medium 300 Calculation phase 301 First step of the calculation phase 302 Second step of the calculation phase 303 Third step of the calculation phase 304 Fourth step of the calculation phase 305 Fifth step of the calculation phase 306 Intermediate step 307 Step of the calculation phase 308 Step of the calculation phase 310 Execution phase 311 to 321 Steps of the execution phase 400 High-speed joining 401 Heating power 402 Heat transfer 403 Heating rate 404 Thin-film melt 405 Stored heat 406 Cooling rate 407 Exposure time 408 Mobility of macromolecules 409 Schematic diagram 410 High-speed joining 502 Feed sensor 504 Feed device 506 Conveyor unit, belt drive 508 Cutting sensor 510 Cutting unit 512 Consolidation roller 514 Consolidation sensor 516 Belt switch 522 Second feed sensor 524 Second feed device 526 Second conveyor unit,Belt drive 528Belt switch sensor 530Second cutting unit 546Drive 546aDrive 546bDrive 547aShaft 547bShaft 550Drive 551Shaft 552Drive 553Shaft 561Guide element 562Guide element 571Attachment element,
Claims
1. Method for the composition of fibre / plastics composites, comprising the steps of: - providing a semi-finished product (20, 20') in a supply device (40, 40b, 44), - feeding the semi-finished product to an application device (50), - heating the semi-finished product (20, 20') by means of a heating device such that a local phase change of the semi-finished product (20, 20') into an at least partially plastic state is induced, - performing a relative movement between the application device (50) and an application region (100), and - applying the semi-finished product (20), in a manner variable in terms of direction and position, to the application region (100) by means of the application device (50) while the relative movement between the application device (50) and the application region (10) is being performed, wherein the relative movement between the application device (50) and the application region (100) is performed at a tool centre point velocity (vTCP) of greater than or equal to 0.5 m / s.
2. Method for the composition of fibre / plastics composites according to claim 1, wherein during the application of the semi-finished product (20, 20') to the application region (100) by means of a heating device (65) a temperature gradient of the heat distribution over the thickness of the semi-finished product is set in such a way that - the semi-finished product is melted on only in part, and / or - the heat energy stored in the semi-finished product is set to less than 40%, preferably less than 20%, based on the heat energy required by the semi-finished product for complete melting on.
3. Method for the composition of fibre / plastics composites according to claim 2, wherein a phase change appearing in the semi-finished product (20, 20') changes the morphology of a polymer of the semi-finished product only in the edge region.
4. Composition facility (1) for composite materials (28), in particular for carrying out the method according to any of claims 1 to 3, comprising: - a base group (2) for providing an application region (100); - a supply device (40, 40b, 44) for providing a semi-finished product (20, 20') for further processing in the composition facility; - an electronic controller (400) for integrated control of all the systems; - an application device (50) for applying the semi-finished product (20, 20') to the application region (100), comprising - a heating device (65) for heating the semi-finished product (20, 20'), which is controlled so as to induce a local phase change of the semi-finished product (20, 20') into an at least partially plastic state; - a drive unit (10) for changing the position of the application device (50) relative to the application region (100); wherein the drive unit (10) is controlled to provide a tool centre point velocity (vTCP) for the application device (50) for the time phase during the application of the semi-finished product (20, 20') onto the application region (100), and interacts with the application device (50) in such a way that the semi-finished product (20, 20') is applied to the application region (100), in a manner variable in terms of direction and position, at the tool centre point velocity (vTCP) of greater than or equal to 0.5 m / s.
5. Composition facility (1) according to the preceding claim, wherein the drive unit (10) is designed to keep the tool centre point velocity (vTCP) constant or substantially constant for the time range during the application of the semi-finished product (20, 20') onto the application region.
6. Composition facility (1) according to the preceding claim, - wherein the heating device (65) is designed to set a temperature gradient of the heat distribution over the thickness of the semi-finished product during heating of the semi-finished product (20, 20'), and / or - wherein the heating device (65) is designed to concentrate the melting zone, during heating of the semi-finished product, on the joint surfaces (29, 29b, 30), and / or - wherein the heating device (65) can be controlled for a phase change into a partially plastic state of the polymer components of the semi-finished product (20, 20'), and / or - wherein the heating device (65) preferably comprises a burner nozzle, plasma, halogen, laser or an LED source.
7. Composition facility (1) according to any of claims 4 to 6, - wherein the drive unit (10) is designed to accelerate the application device (50) at an acceleration of greater than or equal to 8 m / s2, preferably greater than or equal to 20 m / s2, more preferably greater than or equal to 50 m / s2, and / or - wherein the sum of the moving masses of the application device (50) and the drive unit (10) together is less than 750 kg, preferably less than or equal to 250 kg, and more preferably less than or equal to 75 kg.
8. Composition facility (1) according to any of claims 4 to 7, wherein the semi-finished product (20, 20') includes a semi-finished fibre product, a semi-finished polymer product, and / or a self-reinforced polymer, or combinations thereof, wherein in particular fully consolidated, partially consolidated, bonded, wetted semi-finished products or the combinations thereof, and / or semi-finished products comprising thermosetting plastics, thermoplastics, elastomers, the derivatives thereof, and / or combinations thereof are included.
9. Composition facility (1) according to any of claims 4 to 8, wherein the composition of fibre / plastics composites (28) on the application region (100) takes place from semi-finished products (20, 20') successively along predetermined orbital paths and wherein the composition of fibre / plastics composites is possible individually for each orbital path.
10. Composition facility (1) according to any of claims 4 to 9, further comprising at least one further semi-finished product (20') which differs from the semi-finished product (20), wherein the supply device (40, 40b, 44) is designed to feed the semi-finished product (20) and the further semi-finished product (20') to the application device (50) alternately, such that it is possible to produce fibre / plastics composites (28) from different semi-finished products.
11. Composition facility (1) according to any of claims 4 to 10, wherein the heating device (65) comprises a combustion gas nozzle and further comprises an ignition device (66), wherein the ignition device (66) ignites the combustion gas with an electric arc (67b) and / or an ignition spark (67a).
12. Composition facility (1) according to any of claims 4 to 11, wherein the electronic controller (400) preferably provides a cycle time of less than or equal to 1000 µs for electronic synchronisation of the velocity of the drive system (tool centre point velocity, vTCP) and the feed rate of the semi-finished product (20, 20') to the application device (50).
13. Composition facility (1) according to any of claims 4 to 12, wherein the tool centre point velocity (vTCP) is greater than or equal to 1 m / s, preferably greater than or equal to 2 m / s, more preferably greater than or equal to 5 m / s, and further preferably greater than or equal to 10 m / s.
14. Composition facility (1) according to any of claims 4 to 13, wherein the application device (50) for applying the semi-finished product (20, 20') in the application region (100), including the heating device (65), is of a mass of less than 40 kg, preferably of less than 25 kg.
15. Composition facility (1) according to any of claims 4 to 14, further comprising a semi-finished product changing device for automatically changing the semi-finished product (20, 20').